【0011】 本発明によれば、加工溝の凹凸を低減させ被加工物の品質を向上させることができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024148650000001_ABST
    Figure 2024148650000001_ABST
Patent Text Reader

Abstract

To provide a workpiece processing method capable of reducing unevenness of a processed groove and improving the quality of a workpiece.SOLUTION: A processing method for a workpiece 10 includes: a first processing step of irradiating the workpiece 10 with a first laser beam 67 having a wavelength having absorbency from a surface 12 of the workpiece 10 to form a processed groove 17 of a depth that does not completely divide the workpiece 10; and a second processing step of irradiating the workpiece 10 with a second laser beam 68 having a wavelength absorbency and having a lower energy density per spot than in the first processing step along the processed groove 17 to reduce unevenness on a bottom surface 71 of the processed groove 17.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for machining a workpiece. [Background technology]

[0002] In the processing of workpieces such as semiconductor wafers, there is a process of forming a groove by a laser beam. In order to reduce problems in processing quality such as chipping and delamination (film peeling) when forming the groove, for example, Patent Documents 1 and 2 disclose a technique of forming the groove by punching both ends of the groove with a narrow beam and punching the remaining part with a wide beam. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-092363 A [Patent Document 2] Patent Publication No. 2022-054232 Summary of the Invention [Problem to be solved by the invention]

[0004] In conventional technology, when forming a groove in a workpiece using a laser beam, if the desired depth of the groove is deep, the laser beam must be irradiated multiple times, resulting in a problem of reduced productivity. On the other hand, when a laser beam with a high energy density is irradiated, a deep groove can be formed in a short time, but unevenness occurs on the bottom surface of the groove, resulting in a problem of poor quality in terms of appearance and strength. Therefore, in a method for processing a workpiece, there is a problem of reducing the unevenness of the groove and improving the quality of the workpiece.

[0005] The present invention has been made in consideration of the above points, and has an object to provide a method for processing a workpiece that can reduce unevenness in the processed groove and improve the quality of the workpiece. [Means for solving the problem]

[0006] The method for processing a workpiece of the present invention comprises a first processing step in which a first laser beam having a wavelength absorbed by the workpiece is irradiated from one side of the workpiece to form a processed groove of a depth that does not completely divide the workpiece, and a second processing step in which a second laser beam having a wavelength absorbed by the workpiece and a lower energy density per spot than in the first processing step is irradiated along the processed groove to reduce unevenness in the bottom surface of the processed groove.

[0007] In one embodiment of the present invention, a spot size of the first laser beam is smaller than a spot size of the second laser beam.

[0008] In one aspect of the present invention, the workpiece is a wafer having a functional layer laminated on the surface of a substrate, and the first processing step and the second processing step remove the functional layer to expose the substrate.

[0009] One aspect of the present invention further includes, after the second machining step, a dividing step of dividing the workpiece along the machined groove to produce a plurality of chips.

[0010] According to the above-mentioned configuration, the first laser beam has a higher energy density than the second laser beam, so that a deep groove can be formed quickly. The second laser beam, which has a lower energy density than the first laser beam, can smooth out the unevenness of the bottom surface of the groove caused by the first laser beam. This reduces the unevenness of the groove and improves the quality of the workpiece. Effect of the Invention

[0011] According to the present invention, it is possible to reduce unevenness in the machined groove and improve the quality of the machined product. [Brief description of the drawings]

[0012] [Figure 1] 1 is a perspective view of a workpiece to be processed by a processing method according to an embodiment of the present invention; [Diagram 2] 1 is a diagram showing an example of a processing apparatus for performing a method for processing a workpiece; [Diagram 3] FIG. 2 is a schematic diagram of an optical system of the processing apparatus. [Figure 4] 3A to 3C are diagrams illustrating steps of a method for processing a workpiece performed by the processing apparatus of the first embodiment. [Diagram 5] 3A to 3C are diagrams illustrating steps of a method for processing a workpiece performed by the processing apparatus of the first embodiment. [Figure 6] 10A to 10C are diagrams illustrating steps of a method for processing a workpiece performed by the processing apparatus of the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, a processing apparatus for carrying out the method for processing a workpiece according to the present embodiment will be described with reference to the attached drawings. FIG. 1 is a perspective view of a workpiece to be processed by the processing method. FIG. 2 is a diagram showing an example of a processing apparatus for carrying out the method for processing a workpiece. FIG. 3 is a schematic diagram of an optical system of the processing apparatus. FIGS. 4 to 5 are diagrams for explaining each step of the method for processing a workpiece carried out by the processing apparatus of Example 1. FIG. 6 is a diagram for explaining each step of the method for processing a workpiece carried out by the processing apparatus of Example 2.

[0014] The method for processing a workpiece includes a first processing step and a second processing step, which will be described later. The method for processing a workpiece may further include a dividing step, which will be described later. The workpiece and / or the processing device may have any configuration that allows the method for processing a workpiece of the present embodiment to be carried out, and is not limited to the configurations shown in Figures 1 to 3.

[0015] The X-axis, Y-axis, and Z-axis directions shown in each figure are perpendicular to each other. The X-axis and Y-axis directions are approximately horizontal, and the Z-axis direction is up-down (vertical). In each figure, of the two arrows indicating the X-axis direction, the +X side is the left, and the -X side is the right. Of the two arrows indicating the Y-axis direction, the +Y side is the front, and the -Y side is the rear. Of the two arrows indicating the Z-axis direction, the +Z side is the up, and the -Z side is the down.

[0016] A workpiece 10 shown in Fig. 1 is a disk-shaped semiconductor wafer having a substrate 11 made of, for example, silicon. The substrate 11 has a front surface 12 and a back surface 13. On the front surface 12 side of the substrate 11, chips 15, which are electronic devices, are formed in a plurality of regions partitioned by a plurality of lattice-like dividing lines 14. Fig. 1 illustrates only some of the plurality of lattice-like dividing lines 14. It should be noted that the workpiece 10 to which the present invention is applied is not limited to a semiconductor wafer.

[0017] A functional layer 16 is provided on the surface 12 of a substrate 11 that constitutes the workpiece 10. The functional layer 16 constitutes the surface 12 side of the chip 15. A machined groove 17 is formed on the surface 12 side of the workpiece 10 along the planned division line 14. The machined groove 17 is a groove that penetrates the functional layer 16 and has a shape that is recessed from the surface 12 of the workpiece 10 (recessed from the surface 12).

[0018] The functional layer 16 includes a low dielectric constant insulating film (hereinafter referred to as a low-k film) made of an inorganic film such as SiOF, BSG (Borosilicate Glass) (SiOB), or an organic film such as a polymer film of a polyimide system or a parylene system, and a conductor film made of a conductive metal. The low-k film is laminated with the conductor film to form the chip 15. The conductor film forms the circuit of the chip 15. For this purpose, the chip 15 is composed of the low-k films laminated on each other and the conductor film laminated between the low-k films. The functional layer 16 of the planned division line 14 is composed of the low-k film and does not include a conductor film.

[0019] A central portion of a tape (supporting member) T is attached to the workpiece 10, and a ring-shaped frame (not shown) is attached to the outer periphery of the tape T. The workpiece 10 is carried into the processing device 1 while being supported by the frame via the tape T.

[0020] As shown in FIG. 2, the processing device 1 is configured to perform laser processing on the workpiece 10 by moving a laser beam application means 40 that applies a laser beam and a chuck table 20 that holds the workpiece 10 relative to each other.

[0021] A chuck table moving mechanism 30 that moves the chuck table 20 in the X-axis direction and the Y-axis direction is provided on a base 50 of the processing device 1. The chuck table moving mechanism 30 has a pair of guide rails 31 that are arranged on the base 50 and parallel to the X-axis direction, and a motor-driven X-axis table 33 that is slidably installed on the pair of guide rails 31. The chuck table moving mechanism 30 also has a pair of guide rails 32 that are arranged on the upper surface of the X-axis table 33 and parallel to the Y-axis direction, and a motor-driven Y-axis table 34 that is slidably installed on the pair of guide rails 32.

[0022] Nuts (not shown) are formed on the rear sides of the X-axis table 33 and the Y-axis table 34, respectively, and ball screws 35, 36 are screwed into these nut parts. Drive motors 37, 38 connected to one ends of the ball screws 35, 36 are rotated to move the chuck table 20 in the X-axis and Y-axis directions along the guide rails 31, 32. The chuck table 20 for holding the workpiece 10 is provided on the Y-axis table 34. A holding surface 21 is formed on the upper surface of the chuck table 20, and a clamp (not shown) for clamping and fixing a frame around the workpiece 10 may be provided around the chuck table 20.

[0023] An arm 52 protrudes from a vertical wall 51 at the rear of the chuck table 20, and a laser beam application means 40 is provided at the tip of the arm 52 so as to face the chuck table 20 in the vertical direction. In the processing head 41 of the laser beam application means 40, a laser beam (pulse laser) oscillated from an oscillator 61 (not shown) is irradiated toward the workpiece 10 held on the chuck table 20. The laser beam has a wavelength that is transparent to the workpiece 10, and a pulse mark is formed by focusing the laser beam inside the workpiece 10.

[0024] The workpiece 10 is continuously formed along the dividing lines 14 inside, forming modified layers 18 that serve as dividing starting points in the workpiece 10. That is, dividing starting points that are dividing grooves or modified layers 18 formed inside are formed along the dividing lines 14. The dividing lines 14 are formed in a lattice pattern on the surface 12 of the workpiece 10, and chips 15 are formed in each area partitioned by the dividing lines 14. The modified layer 18 is formed, for example, by irradiating the workpiece 10 along the dividing lines 14 with a laser beam that has a wavelength that transmits the workpiece 10 and has a focusing point positioned inside the workpiece 10. The modified layer 18 refers to a region in which the density, refractive index, mechanical strength, and other physical properties of the inside of the workpiece 10 are different from those of the surrounding area due to irradiation with a laser beam, and the strength is lower than that of the surrounding area. The modified layer 18 may be, for example, a melting treatment area, a crack area, an insulation breakdown area, a refractive index change area, or a mixture of these.

[0025] The laser beam application means 40 performs ablation processing on the workpiece 10 on the chuck table 20. The laser beam application means 40 intensively applies a laser beam of an absorbent wavelength along the planned dividing line 14 of the workpiece 10 to form a processing groove 17. Note that ablation refers to a phenomenon in which, when the irradiation intensity of a laser beam reaches a predetermined processing threshold or more, the laser beam is converted into electronic, thermal, optical, and mechanical energy on the solid surface, resulting in the explosive release of neutral atoms, molecules, positive and negative ions, radicals, clusters, electrons, and light, and the solid surface is etched. In the processing device 1, the chuck table 20 is moved in the processing feed direction relative to the laser beam application means 40, thereby performing ablation processing along the planned dividing line 14 of the workpiece 10.

[0026] An imaging means 42 for imaging the surface 12 of the workpiece 10 is provided on the side of the laser beam application means 40. The machining head 41 and the workpiece 10 are aligned based on the image captured by the imaging means 42. The machining device 1 is also provided with a control means 45 for controlling each part of the device and a storage means 46 for storing related data, which will be described later. The control means 45 and the storage means 46 are composed of a processor for executing various processes, a memory, and the like. The memory is composed of one or more storage media, such as a ROM (Read Only Memory) and a RAM (Random Access Memory), depending on the application. The storage means 46 stores a program for executing the machining method for the workpiece 10. The control means 45 executes the program stored in the storage means 46 to execute the machining method for the workpiece 10.

[0027] An optical system of the processing device 1 is provided in the laser beam application means 40. The optical system of the processing device 1 is not limited to a configuration formed in the laser beam application means 40, and may be configured to be formed across the processing head 41, the vertical wall portion 51, and the arm portion 52.

[0028] Here, the laser beam application means 40 constituting the optical system of the processing device 1 will be described with reference to Fig. 3. Fig. 3 is a schematic diagram of the optical system of the processing device 1.

[0029] 3, the optical system of the processing apparatus 1 includes an oscillator 61 that oscillates a first laser beam 67 and a second laser beam 68 toward the workpiece 10, and a condenser 641 that condenses the first laser beam 67 oscillated by the oscillator 61 and a condenser 642 that condenses the second laser beam 68. In addition to the condensers 641 and 642, a splitter 631, mirrors 632 and 633, and a half mirror 634 are arranged on the optical paths of the first laser beam 67 and the second laser beam 68 oscillated from the oscillator 61.

[0030] The splitter 631 transmits the first laser beam 67 oscillated by the oscillator 61, and reflects the second laser beam 68 oscillated by the oscillator 61 to guide it to the condenser 642. The mirror 632 reflects the first laser beam 67 transmitted through the splitter 631 to guide it to the condenser 641. The mirror 633 reflects the second laser beam 68 condensed by the condenser 642 to guide it to the half mirror 634. The half mirror 634 guides the first laser beam 67 condensed by the condenser 641 to the half mirror 634. The half mirror 634 guides the first laser beam 67 condensed by the condenser 641 to the workpiece, and reflects the second laser beam 68 reflected by the mirror 633 to guide it to the workpiece 10.

[0031] 3, a first laser beam 67 oscillated by an oscillator 61 passes through a splitter 631, is reflected by a mirror 632, is guided to a condenser 641, and is also passed through a half mirror 634 to be focused on a processing point of the workpiece 10. A second laser beam 68 oscillated by the oscillator 61 is reflected by the splitter 631, is guided to a condenser 642, is reflected by a mirror 633, and is then reflected by a half mirror 634 to be focused on a processing point of the workpiece 10. The first laser beam 67 and the second laser beam 68 are irradiated onto the workpiece 10 via different optical paths formed by the condensers 641 and 642, the splitter 631, the mirrors 632 and 633, and the half mirror 634.

[0032] When the first laser beam 67 and the second laser beam 68 are focused on the processing point of the workpiece 10, the workpiece 10 is partially sublimated at the processing point. Then, the processing device 1 processes the workpiece 10 along the planned division line 14 by processing and feeding the chuck table 20 relative to the processing head 41 along the planned division line 14.

[0033] In the above-described embodiment, the optical system includes the splitter 631, but is not limited to this. For example, a shutter (not shown) may be provided instead of the splitter 631. In this case, when the first laser beam 67 is irradiated onto the workpiece 10, the shutter is driven to pass the first laser beam 67. The first laser beam 67 that has passed through is reflected by a mirror 632 and guided to a condenser 641. When the second laser beam 68 is irradiated onto the workpiece 10, the shutter is driven to reflect the second laser beam 68. The reflected second laser beam 68 is guided to a condenser 642.

[0034] As the oscillator 61, various oscillators can be used, such as a solid-state laser using a crystal such as ruby ​​or YAG as a laser medium, a semiconductor laser using a semiconductor such as gallium arsenide or indium gallium arsenide phosphide as a laser medium, a gas laser using a gas such as helium-neon or argon as a laser medium, and an excimer laser using a mixed gas of a rare gas such as argon, krypton, or xenon and a halogen such as fluorine or chlorine as a laser medium. The mode of laser oscillation by the oscillator 61 is preferably pulse oscillation in view of the output characteristics, but continuous oscillation may also be used.

[0035] The condenser 641 is mainly configured to include a condenser lens 621 capable of transmitting and focusing the first laser beam 67, and the condenser 641 is mainly configured to include a condenser lens 622 capable of transmitting and focusing the second laser beam 68. The condenser lenses 621 and 622 may be configured as single lenses or combination lenses, or may be combined with other optical components. There is also no particular limit to the number of optical components that can be used for the condensers 641 and 642, and it is sufficient to adopt a configuration that can appropriately achieve focusing on a processing point of the workpiece 10, which is a work.

[0036] 3, a first laser beam 67 and a second laser beam 68 are oscillated by the same oscillator 61 and irradiated along different optical paths. The first laser beam 67 is irradiated in a first processing step, which will be described later, and the second laser beam 68 is irradiated in a second processing step, which will be described later.

[0037] The characteristics of the first laser beam 67 output in the first processing step are as follows: (Characteristics of the first laser beam) Wavelength: 355nm Output: 16W Frequency: 500kHz Feed speed: 800mm / s Beam width: 10μm

[0038] The characteristics of the second laser beam 68 output in the second processing step are as follows: (Characteristics of the second laser beam) Wavelength: 355nm Output power: 8.4W Frequency: 500kHz Feed speed: 800mm / s Beam width: 65μm

[0039] The wavelength indicates the distance between the peaks of the electromagnetic wave formed by the first laser beam 67 or the second laser beam 68, and a wavelength that is absorbent for the workpiece 10 is selected. The first laser beam 67 and the second laser beam 68 are set to have the same wavelength, but this is not limited, and different wavelengths may be set. The output is the energy density per spot when the first laser beam 67 or the second laser beam 68 is focused, and indicates the power of the laser beam when the first laser beam 67 or the second laser beam 68 reaches a position where it is irradiated to the processing point of the workpiece 10 and is focused. The frequency indicates the frequency oscillated by the oscillator 61. The first laser beam 67 and the second laser beam 68 are set to have the same frequency, but this is not limited, and different frequencies may be set. The feed speed indicates the speed at which the chuck table 20 is fed for processing along the planned division line 14 relative to the processing head 41. The beam width indicates the size of the spot of the first laser beam 67 or the second laser beam 68.

[0040] The size of the spot of the first laser beam 67 is smaller than the size of the spot of the second laser beam 68 irradiated in the second processing step. The size of the spot is the size of the unit area per spot at the processing point of the workpiece 10. Therefore, the area per spot of the first laser beam 67 is formed by an area smaller than the area per spot of the second laser beam 68. Also, the size of the spot of the first laser beam 67 is formed by an area smaller than the spot size of the second laser beam 68. The width of the spot of the first laser beam 67 may be formed by a width smaller than the size of the spot of the second laser beam 68, and the width of the spot of the second laser beam 68 may be formed by a width larger than the size of the spot of the first laser beam 67. Hereinafter, the first laser beam 67 is also called a "narrow beam" and the second laser beam 68 is also called a "wide beam". The shape of the narrow beam spot and / or the shape of the wide beam spot is not limited to a circle, and may be an ellipse, a rectangle, a polygon, etc. In this embodiment, as shown in Figures 4 and 5, the beam width of the first laser beam 67 is set to Wa, and the beam width of the second laser beam 68 is set to Wb. The beam width Wb of the second laser beam 68 is set to be larger than the beam width Wa of the first laser beam 67.

[0041] The first laser beam 67 and the second laser beam 68 are generated by the same oscillator 61 and split into two beams along the optical path. The beam width Wa of the first laser beam 67 and / or the beam width Wb of the second laser beam 68 are adjusted by a combination of focusing lenses 621, 622 and a slit (not shown).

[0042] The output of the first laser beam 67 and / or the second laser beam 68 may be changed by branching. For example, the first laser beam 67 with an output of "16 W" may be branched into four to produce the second laser beam 68 with an output of "4 W" branched into four. This allows the energy density per spot of the second laser beam 68 to be smaller than the energy density per spot of the first laser beam 67.

[0043] As described above, the beam width Wa of the first laser beam 67 and the beam width Wb of the second laser beam 68 are different from each other, but this is not limited to the above. The beam width Wa of the first laser beam 67 and the beam width Wb of the second laser beam 68 may be set to be the same, and only the output of the first laser beam 67 and the second laser beam 68 may be set to be different from each other.

[0044] A method for processing the workpiece 10 by the processing device 1 configured as above will be described. The method for processing the workpiece 10 is performed by a first processing step and a second processing step. The method for processing the workpiece 10 will be described with reference to FIG. 4 for the first processing step and the second processing step according to the first embodiment.

[0045] Example 1 A first processing step and a second processing step performed by the processing method of the workpiece 10 of Example 1 will be described with reference to Fig. 4. Note that the functional layer 16 is omitted in the workpiece 10 of Example 1. Fig. 4(1) shows the first processing step, and Fig. 4(2) shows the second processing step.

[0046] (First processing step) 4(1), in the first processing step of Example 1, a first laser beam 67 having a wavelength absorbed by the workpiece 10 is irradiated from a surface 12 (one side) of a substrate 11 constituting the workpiece 10 to form a processed groove 17 having a depth that does not completely divide the workpiece 10. In this embodiment, in the first processing step, a first laser beam 67 having an output of 16 W, a wavelength of 355 nm, and a beam width of 10 μm is irradiated.

[0047] Specifically, the chuck table 20 is processed and fed relative to the processing head 41 along the intended division line 14, whereby a plurality of recesses 72 are formed on the bottom surface 71 of the processed groove 17 by the spots of the first laser beam 67. A plurality of protrusions 73 that are not sublimated and remain partially are formed between the formed recesses 72. Therefore, the bottom surface 71 of the processed groove 17 is uneven due to the plurality of recesses 72 formed at the depth Da and the plurality of recesses 72 formed at the depth Db. The first laser beam 67 has a higher energy density than the second laser beam 68, and therefore the processed groove 17 can be formed quickly and deeply.

[0048] The first laser beam 67 irradiated in the first processing step is set to have a higher energy density per spot than the second laser beam 68 irradiated in the second processing step. Therefore, by irradiating the first laser beam 67 with a high energy density, a deep processed groove 17 can be formed in a short time. On the other hand, the recesses 72 and the protrusions 73 formed on the bottom surface 71 of the processed groove 17 cause unevenness, which deteriorates the quality of the workpiece 10, such as the appearance and strength. Therefore, in this embodiment, the second processing step is performed after the first processing step. The interval between the recesses 72 and the protrusions 73 depends on the feed speed at which the chuck table 20 is processed and fed along the planned division line 14 relative to the processing head 41.

[0049] (Second processing step) 4(2), in the second processing step of Example 1, a second laser beam 68 having a wavelength absorbed by the workpiece 10 and a lower energy density per spot than in the first processing step is irradiated along the processed groove 17 to reduce unevenness on the bottom surface 71 of the processed groove 17. In this embodiment, in the second processing step, a second laser beam 68 having an output of "8.4 W", a wavelength of "355 nm", and a beam width of "65 μm" is irradiated.

[0050] The output of the second laser beam 68 irradiated in the second processing step, "8.4 W," is set to have a lower energy density per spot than the output of the first laser beam 67 irradiated in the first processing step, "16 W."

[0051] Therefore, the plurality of convex portions 73 that are not sublimated in the first processing step and remain partially can be sublimated by irradiating them with the second laser beam 68 irradiated in the second processing step. By irradiating the bottom surface 71 of the processed groove 17 including the convex portions 73 with the second laser beam 68, the depth Db of the convex portions 73 becomes deeper than the depth Db of the convex portions 73 formed in the first processing step, as shown in FIG. 4(2). As a result, by performing the second processing step after the first processing step, the difference between the depth Db of the concave portions 72 and the depth Da of the convex portions 73 can be reduced. This makes it possible to reduce the unevenness formed by the plurality of concave portions 72 and the plurality of convex portions 73 formed on the bottom surface 71 of the processed groove 17. Therefore, the bottom surface 71 of the processed groove 17 can be smoothed to improve the quality of the workpiece 10, such as the appearance and strength.

[0052] The method for processing the workpiece 10 by the processing apparatus 1 configured as above may further include a dividing step. The dividing step executed by the method for processing the workpiece 10 will be described with reference to Fig. 5 .

[0053] (split step) 5, in the dividing step of Example 1, the workpiece 10 is divided along the processed groove 17 to produce a plurality of chips 15. Specifically, as shown in FIG. 5(1), a third laser beam 69 having a wavelength that is transparent to the substrate 11 of the workpiece 10 that has been irradiated with the first laser beam 67 and the second laser beam 68 in the first and second processing steps is irradiated from the back surface 13.

[0054] 5(2), in the workpiece 10 irradiated with the third laser beam 69 from the rear surface 13, cracks 19 are formed from each modified layer 18 toward the front surface 12. The direction in which the cracks 19 are formed can be controlled by appropriately setting the focal point position of the third laser beam 69 in the thickness direction of the workpiece 10. For example, when the modified layer 18 is formed at a position closer to the front surface 12 in the thickness of the workpiece 10, the cracks 19 are mainly formed toward the front surface 12 close to the modified layer 18.

[0055] After the dividing step, the method for processing the workpiece 10 may further include a step of expanding the tape T to widen the intervals between the chips 15, and / or a step of extending the cracks 19 to at least one of the front surface 12 and the back surface 13 along the dividing starting points that become the modified layers 18 by grinding from the back surface 13 with a grinding wheel. In this way, the workpiece 10 can be divided to produce a plurality of chips 15.

[0056] Example 2 A first processing step and a second processing step performed by the processing method of the workpiece 10 of the second embodiment will be described with reference to Fig. 6. In the workpiece 10 of the second embodiment, a functional layer 16 is formed, unlike the first embodiment described with reference to Fig. 4. Fig. 6(1) shows the first processing step, and Fig. 6(2) shows the second processing step.

[0057] (First processing step) 6(1), in the first processing step of Example 2, as in Example 1, a first laser beam 67 having a wavelength absorbed by the workpiece 10 is irradiated from the surface 12 of a substrate 11 constituting the workpiece 10 to form a processed groove 17 having a depth that does not completely divide the workpiece 10. The characteristics of the first laser beam 67 in Example 2 are similar to those of Example 1.

[0058] In Example 2, similarly to Example 1, a plurality of recesses 72 are formed on a bottom surface 71 of the processed groove 17 by spots of the first laser beam 67. In Example 2, the first laser beam 67 is irradiated onto the workpiece 10 until the depth Db, which is approximately the same as the thickness of the functional layer 16, is reached, thereby removing the functional layer 16 and exposing the substrate 11. Similarly to Example 1, unevenness is generated on the bottom surface 71 of the processed groove 17 in Example 2 by a plurality of recesses 72 formed at a depth Da and a plurality of protrusions 73 formed at a depth Db.

[0059] In the above embodiment, the functional layer 16 is removed in the first processing step, but this is not limited to the above. In the processing method of the workpiece 10 of Example 2, the functional layer 16 may be removed and the substrate 11 may be exposed by the first processing step and the second processing step. The functional layer 16 can be removed by the first processing step and the second processing step, a part of the substrate 11 may be exposed by the first processing step, and the remaining substrate 11 that could not be removed by the first processing step may be exposed by the second processing step. Therefore, it is possible to minimize the thermal damage to silicon and the like constituting the substrate 11 caused by the first laser beam 67 having a high energy density, and the bottom surface 71 of the processed groove 17 can be smoothed by the second laser beam 68 having a low energy density. This reduces the unevenness of the processed groove 17 and improves the quality of the workpiece 10. It is also possible to remove the functional layer 16 only by the first processing step and expose the entire substrate 11. This improves the processing speed. The method for processing the workpiece 10 in the second embodiment may also include a step similar to the dividing step described with reference to FIG.

[0060] In this manner, in this embodiment, the first laser beam 67 irradiated in the first processing step has a higher energy density than the second laser beam 68, and therefore the processed groove 17 can be formed quickly and deeply. Then, the multiple convex portions 73 that are partially left without being sublimated as a result of irradiation with the first laser beam 67 in the first processing step can be sublimated by irradiating them with the second laser beam 68 irradiated in the second processing step. That is, by irradiating the bottom surface 71 of the processed groove 17 including the convex portions 73 with the second laser beam 68, the depth Db of the convex portions 73 becomes deeper than the depth Db of the convex portions 73 formed in the first processing step, as shown in FIG. 4(2). As a result, by performing the second processing step after the first processing step, the difference between the depth Db of the concave portions 72 and the depth Da of the convex portions 73 can be reduced. This makes it possible to reduce the unevenness formed by the multiple concave portions 72 and the multiple concave portions 72 formed on the bottom surface 71 of the processed groove 17. Therefore, the bottom surface 71 of the groove 17 can be smoothed to improve the quality of the workpiece 10, such as its appearance and strength.

[0061] The embodiments of the present invention are not limited to the above-mentioned embodiments and modifications, and may be modified, substituted, or altered in various ways without departing from the spirit of the technical idea of ​​the present invention. Furthermore, if the technical idea of ​​the present invention can be realized in a different way due to technological progress or a derived technology, the present invention may be implemented using that method. Therefore, the claims cover all embodiments that may be included within the scope of the technical idea of ​​the present invention. [Industrial Applicability]

[0062] As described above, the method for processing the workpiece 10 by the processing device 1 of the present invention irradiates the first laser beam 67 in the first processing step to form the processed groove 17, and then irradiates the second laser beam 68, which has a lower energy density per spot than in the first processing step, along the processed groove 17 in the second processing step to reduce the unevenness of the bottom surface 71 of the processed groove 17, thereby reducing the unevenness of the processed groove 17 and improving the quality of the processed workpiece 10. Therefore, it is particularly useful in the field of processing the workpiece 10, which reduces the unevenness of the processed groove 17 and improves the quality of the processed workpiece 10. [Explanation of symbols]

[0063] 1: Processing equipment 10: Workpiece 11: Substrate 12: Surface 13: Back side 14: Planned division line 15: Tip 16: Functional layer 17: Machining groove 18: Modified layer 19: Crack 20: Chuck table 21: Holding surface 30: Chuck table movement mechanism 31: Guide rail 32: Guide rail 33: X-axis table 34: Y-axis table 35: Ball screw 36: Ball screw 37: Drive motor 38: Drive motor 40: Laser beam irradiation means 41: Processing head 42: Imaging means 45: Control means 46: Storage means 50: Foundation 51: Vertical wall 52: Arm section 61: Oscillator 67: First laser beam 68: Second laser beam 69: Third laser beam 71: Bottom 72: Recess 73: Convex 621: Condenser lens 622: Condenser lens 631: Splitter 632: Mirror 633: Mirror 634: Half mirror 641: Concentrator 642: Concentrator T: Tape

Claims

1. Irradiating one surface of the workpiece with a first laser beam having a wavelength that is absorbed by the workpiece; A first machining step of forming a groove having a depth that does not completely divide the workpiece; a wavelength that is absorbent for the workpiece, and a second processing step of irradiating a second laser beam having a lower energy density per spot than that of the first processing step along the processed groove to reduce unevenness on the bottom surface of the processed groove; A method for processing a workpiece, comprising:

2. The size of the spot of the first laser beam is: smaller than the spot size of the second laser beam 2. The method for machining a workpiece according to claim 1.

3. The workpiece is a wafer having a functional layer laminated on the surface of a substrate, The first processing step and the second processing step remove the functional layer to expose the substrate.

2. The method for machining a workpiece according to claim 1.

4. After the second processing step, Along the processed groove, The method further includes a dividing step of dividing the workpiece to produce a plurality of chips.

4. A method for machining a workpiece according to claim 1, wherein the workpiece is machined by a machine tool.

Citation Information

Patent Citations

  • Method of forming identification mark on single crystal substrate made of refractory material, and single crystal substrate made of refractory material

    JP2014031306A

  • Wafer dicing using a hybrid multi-step laser scribing process with plasma etching

    JP2015519732A

  • Element chip manufacturing method

    JP2019175976A

  • Hybrid wafer dicing approach using an adaptive optics-controlled laser scribing process and plasma etch process

    US20160086851A1

  • Dividing method for wafer

    JP2017092363A

Cited By

  • Spatial light modulator-based low dielectric constant material slotting system and method

    CN121104303A

  • Processing method and processing device

    WO2026028963A1

  • Processing method and processing device

    WO2026028964A1