Double shield tig welding method

The method adjusts inner gas flow rate based on welding current and joint shape to control arc rigidity, enhancing welding workability by accommodating individual operator preferences.

JP2024149941AInactive Publication Date: 2024-10-23DAIHEN CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023063127
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-23
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The double shield TIG welding method lacks the ability to adjust arc rigidity to meet the preferences of individual welding operators, affecting welding workability.

Method used

A method that adjusts the flow rate of inner gas in a welding torch based on welding current, electrode diameter, and joint shape to control arc rigidity, using an adjustment unit to increase or decrease the inner gas flow rate.

Benefits of technology

Enables arc rigidity adjustment to match the operator's preference, improving welding workability by providing a hard or soft arc as desired.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149941000001_ABST
    Figure 2024149941000001_ABST
Patent Text Reader

Abstract

To provide a double shield tig welding method, which can adjust rigidity of an arc into a desired state.SOLUTION: A double shield tig welding method, which performs welding by generating an arc 3 between an electrode 1 and a base material 2 and passing welding currents Iw, using a welding torch WT provided with an inner nozzle 4 that jets inner gas 7 and an outer nozzle 5 that jets outer gas 9, sets a flow rate Fi of the inner gas 7 in accordance with a set value Ir of the welding currents Iw, where an adjusting part H4R for adjusting rigidity of the arc 3 is provided, and the adjusting part H4R increases and decreases the set flow rate Fi of the inner gas 7.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a double shielded TIG welding method. [Background technology]

[0002] A double-shielded TIG welding method is commonly used in which welding is performed using a welding torch equipped with an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas (see, for example, Patent Document 1). As the inner gas and the outer gas, inert gases such as argon and helium are used. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-15048 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the double shield TIG welding method, the desired arc stiffness varies from one welding operator to another. Some welding operators prefer a hard arc with strong stiffness, while others prefer a soft arc with weak stiffness. If the stiffness of the arc can be adjusted to the state desired by the welding operator, the welding workability can be improved.

[0005] Therefore, an object of the present invention is to provide a double-shielded TIG welding method capable of adjusting the rigidity of the arc to a desired state. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems, the invention of claim 1 comprises: A welding torch having an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas is used, In a double shield TIG welding method in which an arc is generated between an electrode and a base metal and a welding current is passed through the electrode, A flow rate of the inner gas is set according to a value of the welding current; An adjustment unit for adjusting the stiffness of the arc is provided, The adjustment unit increases or decreases the set flow rate of the inner gas. This is a double shielded TIG welding method characterized by the above.

[0007] The invention of claim 2 is as follows: The flow rate of the inner gas, which is set according to the value of the welding current, is corrected according to the diameter of the electrode and the joint shape of the base metal. 2. The double shielded TIG welding method according to claim 1,

[0008] The invention of claim 3 is as follows: resetting the increase or decrease in the flow rate of the inner gas by the adjustment unit to 0 when at least one of the conditions of the value of the welding current, the diameter of the electrode, and the joint shape of the base metal is changed; 3. The double shielded TIG welding method according to claim 2, Effect of the Invention

[0009] According to the double shielded TIG welding method of the present invention, the stiffness of the arc can be adjusted to a state desired by the welding operator, thereby improving the efficiency of the welding work. [Brief description of the drawings]

[0010] [Figure 1] 1 is a block diagram of a welding apparatus for carrying out a double-shielded TIG welding method according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0012] 1 is a block diagram of a welding apparatus for carrying out a double shielded TIG welding method according to an embodiment of the present invention. Each block will be described below with reference to the diagram.

[0013] The welding torch WT mainly includes an electrode 1, an inner nozzle 4 surrounding the electrode 1, and an outer nozzle 5 surrounding the inner nozzle 4. A tungsten electrode or the like is used for the electrode 1. For example, the inner diameter of the inner nozzle 4 is 5 mm, and the inner diameter of the outer nozzle 5 is 13 mm.

[0014] The start switch ON outputs a start signal On that goes to a high level when it is turned on and goes to a low level when it is turned off. This start switch ON is a torch switch provided on the welding torch WT. The start signal On may also be output from the robot control device.

[0015] The current setting circuit IR outputs a predetermined current setting signal Ir.

[0016] When the diameter of the electrode 1 to be used is selected from 1.6 mm, 2.4 mm, or 3.2 mm, the electrode diameter correction circuit H1R outputs an electrode diameter correction signal H1r such that H1r=-1 when 1.6 mm is selected, H1r=-0.5 when 2.4 mm is selected, and H1r=0 when 3.2 mm is selected.

[0017] When the material of the base material 2 to be used is selected from either steel or aluminum, the base material material correction circuit H2R outputs a base material material correction signal H2r, where H2r=0 when steel is selected and H2r=2 when aluminum is selected.

[0018] When the joint shape correction circuit H3R selects the joint shape of the base material 2 as either a butt joint or a fillet joint, it outputs a base material joint correction signal H3r, which becomes H3r = 0 when a butt joint is selected and H3r = 1 when a fillet joint is selected.

[0019] The inner gas flow rate setting circuit FIR receives the current setting signal Ir, the electrode diameter correction signal H1r, the joint shape correction signal H3r, and the arc rigidity adjustment signal H4r (described later) as inputs, inputs them to a predetermined inner gas flow rate setting function, and outputs the calculated value as an inner gas flow rate setting signal Fir [l / min]. An example of the inner gas flow rate setting function is shown below. Fir=(Ir-75) / 50+3.5+H1r+H3r+H4r (1) formula However, the range is 75≦Ir≦150, and when Ir<75, the value is the same as Ir=75, and when Ir>150, the value is the same as Ir=150.

[0020] The inner gas flow regulator CI is a commonly used mass flow controller that receives the above-mentioned start signal On and the above-mentioned inner gas flow setting signal Fir as inputs, and when the start signal On becomes high level, it adjusts the flow rate Fi of the inner gas 7 from the inner gas cylinder 6 to a value determined by the inner gas flow setting signal Fir and sprays it.

[0021] The outer gas flow rate setting circuit FOR receives the current setting signal Ir and the base material material correction signal H2r as inputs, inputs them to a predetermined outer gas flow rate setting function, and outputs the calculated value as an outer gas flow rate setting signal For [l / min]. An example of the outer gas flow rate setting function is shown below. For = (Ir-75) / 50+5.5+H2r (2) However, the range is 75≦Ir≦150, and when Ir<75, the value is the same as Ir=75, and when Ir>150, the value is the same as Ir=150.

[0022] The outer gas flow regulator CO is a commonly used mass flow controller that receives the above-mentioned start signal On and the above-mentioned outer gas flow setting signal For as inputs. When the start signal On becomes high level, it adjusts the flow rate Fo of the outer gas 9 from the outer gas cylinder 8 to a value determined by the outer gas flow setting signal For and sprays it.

[0023] An inner gas 7 flows through a passage inside the inner nozzle 4. An outer gas 9 flows through a passage outside the inner nozzle 4 and inside the outer nozzle 5. An inert gas such as argon or helium is used as the inner gas 7 and the outer gas 9. The arc 3 is generated with the electrode 1 serving as the negative electrode and the base material 2 serving as the positive electrode.

[0024] The welding power source PS receives as input the above-mentioned start signal On and the above-mentioned current setting signal Ir, and when the start signal On goes to high level, it applies a high frequency high voltage between the electrode 1 and the base material 2, and when an arc 3 is generated, it begins outputting the welding current Iw set by the current setting signal Ir, and when the start signal On goes to low level, it stops outputting the welding current Iw.

[0025] The arc stiffness adjustment circuit H4R is provided on the front panel of the welding power source PS, and receives the current setting signal Ir, the electrode diameter correction signal H1r, and the joint shape correction signal H3r as inputs. The circuit has an increase button and a decrease button, and outputs an arc stiffness adjustment signal H4r that increases by a predetermined value each time the increase button is pressed and decreases by a predetermined value each time the decrease button is pressed. The arc stiffness adjustment signal H4r is reset to 0 when any of the current setting signal Ir, the electrode diameter correction signal H1r, and the joint shape correction signal H3r changes. For example, the predetermined value is 0.1 (l / min). At this time, when the increase button is pressed five times, H4r=0.5 (l / min). After that, when the decrease button is pressed twice, H4r=0.5-0.2=0.3 (l / min).

[0026] Below, we will explain numerical examples in which the flow rates of the inner gas and outer gas are set according to the value of the welding current, the flow rates of the inner gas and / or outer gas are corrected according to the electrode diameter, the material of the base metal, and the joint shape of the base metal, and further the arc rigidity is adjusted. (1) Correction of inner gas flow rate Electrode diameter 3.2mm → Electrode diameter correction signal H1r=0 Joint shape Butt joint → Joint shape correction signal H3r=0 Arc stiffness adjustment signal H4r=0.3 From the above equation (1), the inner gas flow rate Fi is calculated by inputting the current setting signal Ir. Since Fi=(Ir-75) / 50+3.5+H1r+H3r+H4r, When Ir=75A, Fi=3.8(l / min), When Ir=150A, Fi=5.3 (l / min). Here, when the electrode diameter becomes 2.4 mm, the electrode diameter correction signal H1r = -0.5, so The inner gas flow rate Fi is 0.5 (l / min) smaller than the above. When the electrode diameter becomes 1.6 mm, the electrode diameter correction signal H1r = -1, so The inner gas flow rate Fi is 1 (l / min) smaller than the above. If the joint shape becomes a fillet joint, the shape correction signal H3r becomes 1. The inner gas flow rate Fi is 1 (l / min) larger than the above. Here, by adjusting the arc rigidity signal H4r, the above-mentioned automatically set value of the inner gas flow rate can be increased or decreased with respect to the median value.

[0027] (2) Correction of outer gas flow rate Base material Steel Base material correction signal H2r=0 From the above equation (2), the outer gas flow rate Fo is calculated by inputting the current setting signal Ir. Since Fo=(Ir-75) / 50+5.5+H2r, When Ir=75A, Fo=5.5(l / min), When Ir=150A, Fo=7 (l / min). Here, if the base material is aluminum, the base material correction signal H2r=2, so The outer gas flow rate Fo is 2 (l / min) larger than the above.

[0028] The effects of this embodiment will be described below. According to this embodiment, the flow rate of the inner gas is set according to the value of the welding current, and an adjustment unit for adjusting the rigidity of the arc is provided, and the adjustment unit increases or decreases the flow rate of the inner gas that has been set. The welding state can be improved by optimizing the flow rate of the inner gas according to the value of the welding current. In addition, the rigidity of the arc desired by each welding operator is different. Some welding operators prefer a hard arc with strong rigidity, and some prefer a soft arc with weak rigidity. If the rigidity of the arc can be adjusted to a state desired by the welding operator, the welding workability can be improved in this embodiment, which is provided with an adjustment unit for finely adjusting the rigidity of the arc, and the flow rate of the inner gas set according to the value of the welding current can be increased or decreased by this adjustment unit. If the flow rate of the inner gas is increased, the rigidity of the arc becomes strong, resulting in a hard arc. If the flow rate of the inner gas is decreased, the rigidity of the arc becomes weak, resulting in a soft arc. As a result, in this embodiment, the rigidity of the arc can be adjusted to a state desired by the welding operator, and the workability can be improved.

[0029] More preferably, according to this embodiment, the flow rate of the inner gas, which is set according to the value of the welding current, is corrected according to the diameter of the electrode and the joint shape of the base metal, so that the flow rate of the inner gas is optimized according to various combinations of electrode diameters and joint shapes, thereby making it possible to improve the welding condition.

[0030] More preferably, according to this embodiment, when at least one of the conditions of the welding current value, the electrode diameter, and the joint shape of the base metal is changed, the increase or decrease value of the flow rate of the inner gas by the adjustment unit is reset to 0. Even if the increase or decrease value by the adjustment unit is the same depending on the combined conditions of the welding current value, the electrode diameter, and the joint shape of the base metal, the degree of the rigidity of the arc differs. Therefore, when at least one of these conditions is changed, the increase or decrease value is reset to 0 to return the rigidity of the arc to the standard state. After that, the rigidity of the arc is again adjusted to the desired state by the adjustment unit. [Explanation of symbols]

[0031] 1 electrode 2 Base material 3. Arc 4 Inner nozzle 5 Outer nozzle 6 Inner gas cylinder 7. Inner Gas 8 Outer gas cylinder 9. Outer Gas CI Inner Gas Flow Regulator CO outer gas flow regulator Fi Inner gas flow rate FIR inner gas flow rate setting circuit Fir inner gas flow rate setting signal Fo Outer gas flow rate FOR outer gas flow rate setting circuit For outer gas flow rate setting signal H1R Electrode diameter correction circuit H1r Electrode diameter correction signal H2R base material correction circuit H2r Base material correction signal H3R joint shape correction circuit H3r joint shape correction signal H4R Arc stiffness adjustment circuit H4r Arc Stiffness Adjustment Signal IR current setting circuit Ir Current setting signal Iw Welding current ON Start switch On Start signal PS Welding Power Source WT Welding Torch

Claims

1. A welding torch having an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas is used, In a double shield TIG welding method in which an arc is generated between an electrode and a base metal and a welding current is passed through the electrode, A flow rate of the inner gas is set according to a value of the welding current; An adjustment unit for adjusting the stiffness of the arc is provided, The adjustment unit increases or decreases the set flow rate of the inner gas. A double shielded TIG welding method.

2. The flow rate of the inner gas, which is set according to the value of the welding current, is corrected according to the diameter of the electrode and the joint shape of the base metal. The double shielded TIG welding method according to claim 1 .

3. resetting the increase or decrease in the flow rate of the inner gas by the adjustment unit to 0 when at least one of the conditions of the value of the welding current, the diameter of the electrode, and the joint shape of the base metal is changed; The double shield TIG welding method according to claim 2 .

Citation Information

Patent Citations

  • TIG welding torch provided with contracting nozzle

    JP2020015048A