Magnetic wedge, rotary electric machine and manufacturing method of magnetic wedge

The right-angled trapezoidal magnetic wedge with varying thickness addresses the space inefficiency in conventional designs, ensuring complete slot filling and improved fixation, thereby enhancing the efficiency of rotating electric machines.

JP2024150298AInactive Publication Date: 2024-10-23PROTERIAL LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023063650
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-23
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional magnetic wedges in rotating electric machines have a constant thickness, leading to wasted space at both axial ends of the slot due to the curvature of the coil, which compromises the ability to fully fill the slot opening and reduces the efficiency of the machine.

Method used

A magnetic wedge with a right-angled trapezoidal shape, where the longest side is the oblique side, and a manufacturing method involving press forming and heat treatment to create a magnetic wedge with varying thickness, allowing it to fit the slot opening effectively without gaps.

Benefits of technology

The solution enables the magnetic wedge to fill the slot opening without waste, enhancing the efficiency of the rotating electric machine by reducing gaps and improving fixation, thus increasing the machine's overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024150298000001_ABST
    Figure 2024150298000001_ABST
Patent Text Reader

Abstract

To provide a magnetic wedge effective for filling a slot opening and a manufacturing method of the magnetic wedge.SOLUTION: A magnetic wedge is installed in a slot opening of a stator of a rotary electric machine. With dimensions of the magnetic wedge in a circumferential direction of the rotary electric machine considered as width, a projection shape of the magnetic wedge projected on a plane perpendicular to a direction of the width is a rectangular trapezoid, and the longest side among four sides constituting the rectangular trapezoid is a hypotenuse. A manufacturing method of the magnetic wedge installed in the slot opening of the stator of the rotary electric machine comprises a press molding process of press-molding, with the dimensions of the magnetic wedge in the circumferential direction of the rotary electric machine considered as the width, base powder containing soft magnetic particles in the direction of the width to obtain a compact, and uses a metal mold having an opening in a rectangular trapezoidal shape and a punch which can be inserted into the opening of the metal mold in the press molding process.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a magnetic wedge used in a magnetic circuit of a rotating electric machine, a rotating electric machine, and a method for manufacturing such a magnetic wedge. [Background technology]

[0002] In a typical radial gap type rotating electric machine, the stator and rotor are arranged coaxially, and multiple teeth with coils wound around them are arranged at equal intervals in the circumferential direction on the stator around the rotor. Magnetic wedges may be arranged on the rotor-side tips of the teeth to connect the tips of adjacent teeth. In this case, the magnetic wedges are used without winding a coil around them, unlike coil components, etc.

[0003] By providing such a magnetic wedge, it is possible to magnetically shield the magnetic flux reaching the coil from the rotor, and suppress the eddy current loss of the coil. Also, by providing the magnetic wedge, it is possible to smooth the magnetic flux distribution (particularly the magnetic flux distribution in the circumferential direction) in the gap between the stator and rotor, and reduce the loss (stray load loss) occurring in the rotor. By providing the magnetic wedge in this way, it is possible to obtain a highly efficient rotating electric machine (for example, Patent Document 1).

[0004] A composite material made of ferromagnetic powder such as iron powder and thermosetting resin is known as a conventional magnetic wedge. The manufacturing method of this magnetic wedge is to first make a plate-shaped base material by kneading the ferromagnetic powder and thermosetting resin into a paste, compressing and molding this in the thickness direction of the magnetic wedge while thermally curing it, and then machining it to the dimensions and shape required for the magnetic wedge.

[0005] Such conventional magnetic wedges are usually machined into a long, thin rectangular parallelepiped (rectangle shape) or even into a trapezoid or T-shape in cross section perpendicular to the length direction, and are inserted lengthwise into grooves or the like provided at the tips of the teeth. Since coils are placed between adjacent teeth (these spaces are called slots), the magnetic wedge is pushed inward from behind (the outer diameter side of the motor) by the coils. This force presses the magnetic wedge into the grooves at the tips of the teeth and fixes it in place.

[0006] Conventional magnetic wedges are generally rectangular in shape as described above, and therefore generally have a constant thickness. In other words, the cross section perpendicular to the width direction of the magnetic wedge is basically rectangular. However, in order to make it easier to insert the magnetic wedge into a rotating electric machine, one corner of the rectangle may be chamfered to provide a taper at the end. This taper is also performed by machining. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 3-27745 Summary of the Invention [Problem to be solved by the invention]

[0008] The coil in the slot is usually curved, and at both axial ends of the rotating electric machine, it is slightly behind the slot (on the outer periphery of the rotating electric machine), and near the axial center, it protrudes toward the slot opening side (on the inner periphery of the rotating electric machine). Therefore, the space for inserting the magnetic wedge is wide at both axial ends and narrow near the axial center. Since the thickness of a conventional magnetic wedge is basically constant in the length direction, it is possible to fill the space of the slot opening without any gaps near the axial center, but at both axial ends, there is wasted space behind the magnetic wedge. In particular, when the coil in the slot is curved greatly, it is necessary to make the thickness of the magnetic wedge thin to fit the narrow space near the axial center, which results in the wasted space at both axial ends being further expanded. For this reason, there was a problem that the effect that would have been obtained if the magnetic wedge could fully fill the space of the slot opening could not be obtained.

[0009] SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide a magnetic wedge that is effective for filling a slot opening and a method for manufacturing the magnetic wedge. [Means for solving the problem]

[0010] The present invention relates to a magnetic wedge installed at a slot opening of a stator of a rotating electric machine, wherein if the dimension of the magnetic wedge in the circumferential direction of the rotating electric machine is the width, the projected shape of the magnetic wedge projected onto a plane perpendicular to the width direction is a right-angled trapezoid, and the longest side of the four sides that make up the right-angled trapezoid is the hypotenuse.

[0011] It is also preferable that the corners of the right-angled trapezoid have a radius.

[0012] It is also preferable that the magnetic wedge includes a plurality of soft magnetic particles and an electrically insulating material between the soft magnetic particles.

[0013] In addition, it is preferable that the soft magnetic particles are Fe-based soft magnetic particles, the Fe-based soft magnetic particles contain element M which is more easily oxidized than Fe, the electrically insulating material is an oxide phase containing element M, and the Fe-based soft magnetic particles are bound by the oxide phase.

[0014] Moreover, the element M is preferably at least one selected from the group consisting of Al, Si, Cr, Zr and Hf.

[0015] In the magnetic wedge, the Fe-based soft magnetic particles are preferably Fe-Al-Cr based alloy particles.

[0016] The rotating electric machine of the present invention is a rotating electric machine having a stator for a rotating electric machine having a plurality of teeth and a plurality of slots formed by the plurality of teeth, and a rotor arranged in a position sharing an axis with the stator for the rotating electric machine, in which a plurality of magnetic wedges are inserted in a vertical row in the axial direction into the slot opening of each slot, at least one of which is the magnetic wedge.

[0017] The manufacturing method of a magnetic wedge of the present invention is a manufacturing method for a magnetic wedge to be installed at a slot opening of the stator of a rotating electric machine, and includes a press molding process in which raw material powder containing soft magnetic particles is press-molded in the direction of width to obtain a molded body, where the dimension of the magnetic wedge in the circumferential direction of the rotating electric machine is taken as width, and the press molding process uses a die having an opening in the shape of a right-angled trapezoid and a punch that can be inserted into the opening of the die, and the longest side of the four sides that make up the right-angled trapezoid shape is the hypotenuse.

[0018] It is also preferable that the corners of the opening in the shape of a right-angled trapezoid are rounded.

[0019] Moreover, in the method for manufacturing the magnetic wedge, it is preferable that the raw material powder is a mixed powder of a binder and a powder of Fe-based soft magnetic particles containing element M, which is more easily oxidized than Fe, and that after the press molding process, a heat treatment process is performed to the molded body to form a surface oxide phase of the Fe-based soft magnetic particles between the particles, which bonds the Fe-based soft magnetic particles to each other.

[0020] In the method for producing a magnetic wedge, the element M is preferably at least one selected from the group consisting of Al, Si, Cr, Zr and Hf.

[0021] Furthermore, in the method for producing a magnetic wedge, the Fe-based soft magnetic particles are preferably Fe-Al-Cr based alloy particles. Effect of the Invention

[0022] According to the present invention, the space generated by the curvature of the coil inside the slot can be filled with the magnetic wedge without waste, and it is expected that a more efficient rotating electric machine can be realized. [Brief description of the drawings]

[0023] [Figure 1] 1 is a schematic diagram showing the shape of a magnetic wedge according to an embodiment of the present invention. [Diagram 2] 1 is a schematic diagram showing a case where a magnetic wedge according to an embodiment of the present invention is mounted on a radial gap type rotating electric machine. [Diagram 3] 1 is a schematic cross-sectional view of a magnetic wedge according to an embodiment of the present invention attached to a slot opening of a stator. [Figure 4] FIG. 2 is a schematic diagram of a molding die and upper and lower punches used when manufacturing a magnetic wedge by powder press molding. [Diagram 5] 1 is a schematic diagram showing a case where a magnetic wedge with a constant thickness is attached to a radial gap type rotating electric machine. [Figure 6] FIG. 2 is a schematic cross-sectional view of a constant thickness magnetic wedge installed in a slot opening of a stator. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] Hereinafter, with reference to the drawings, an embodiment of a conventional magnetic wedge will be described, and then an embodiment of the present invention will be described, but the present invention is not limited to this embodiment. Also, the description of overlapping parts will be omitted.

[0025] First, a conventional magnetic wedge will be described. Fig. 5 is a schematic diagram showing a state in which a conventional magnetic wedge 9 is attached to a radial gap type rotating electric machine. The magnetic wedge 9 is inserted in the length direction into a gap (called a slot opening) surrounded by adjacent teeth 34 and coils 33. The shape of a cross section perpendicular to the length direction of the magnetic wedge 9 is such that it can be fitted into the slot opening, as shown in the figure. The magnetic wedge 9 basically has a constant thickness. The length of the magnetic wedge 9 is generally the same as the thickness of the stator 31, but to simplify the magnetic wedge insertion work, multiple magnetic wedges shorter than the thickness of the stator may be inserted vertically. Note that in practice, insulating sheets called slot liners are inserted between the coil 33, the stator 31, and the teeth 34 to ensure electrical insulation, but are omitted in the figure.

[0026] 6 shows a schematic cross-sectional view of a conventional magnetic wedge 9 attached to a slot opening of a stator 31. This figure shows a cross-sectional view of the stator 31 cut near the center between the teeth 34 (near the center of the slot) on a plane including the axis of the rotating electric machine. The left-right direction of the page in this figure is the axial direction of the rotating electric machine, the top of the page is the inner diameter side of the rotating electric machine, and the bottom of the page is the outer diameter side.

[0027] The magnetic wedge 9 is installed on the inner diameter side of the slot as shown in the figure. On the outer diameter side of the magnetic wedge, there is a slot liner 35, and further below that, there is a coil 33. A plurality of coils 33 are installed in the slot. In FIG. 1 described later, for ease of viewing, gaps are drawn between the slot liner 35 and the coils 33, or between the coils 33 themselves, but in reality, they are in close contact with each other. Also, in order to avoid interference with a rotor (not shown) present on the inner diameter side, the coil 33 is usually fixed so as to be pushed outward toward the outer diameter side as shown in the figure on the outside of the slot. Therefore, the coil 33 is curved inside the slot as shown in the figure, protruding toward the inner diameter side near the axial center of the slot, and receding toward the outer diameter side near both ends. The magnetic wedge 9 comes into contact with the slot liner 35 near the center, but gaps are generated between the magnetic wedge 9 and the slot liner 35 near both axial ends of the slot as shown in the figure.

[0028] The schematic cross-sectional diagrams of the schematic diagram of FIG. 6 cut along planes (AA' and BB') perpendicular to the axis of the rotating electric machine are shown below the same figure. The cross sections are at two locations: the axial end (AA' cross section) and the axial center (BB' cross section). The cross section of the magnetic wedge 9 is T-shaped as shown in the figure, and both flanges (both ends of the T-shape) are caught by the protrusions of the teeth 34 so as not to fall off to the inner diameter side of the rotating electric machine. Also, as shown in the BB' cross section, at the axial center portion, the magnetic wedge 9 is pressed against the teeth 34 from the outer diameter side by the coil 33 via the slot liner 35 and fixed. Meanwhile, at the AA' cross section at the slot end, a gap is generated between the magnetic wedge 9 and the slot liner 35.

[0029] Basically, the larger the volume of the magnetic wedge 9 that fills the gap at the slot opening (the smaller the gap at the slot opening), the greater the effect of the magnetic wedge, which is advantageous for increasing the efficiency of the rotating electric machine, so the presence of the gap as shown in the figure is undesirable. Also, although the magnetic wedge 9 and the teeth 34 are bonded and fixed by varnish impregnation, electromagnetic forces are repeatedly applied to the magnetic wedge 9 when the rotating electric machine is in operation, so there is a risk that the adhesion will deteriorate over the long term and the fixation will become loose. If the fixation becomes weak, the magnetic wedge will vibrate due to the electromagnetic force, leading to problems such as wear and breakage, so from this perspective as well, the presence of the gap as shown in the figure is undesirable.

[0030] Next, the magnetic wedge of this embodiment will be described. Figure 1 shows five views of the magnetic wedge 10 according to this embodiment. The basic shape of the magnetic wedge is a strip shape (rod shape) represented by length L, width W, and thickness T, and the thickness T changes from T1 to T2 in the length L direction, so that it has a right-angled trapezoid shape when viewed from the width direction. In addition, when the upper base (side 24) of the right-angled trapezoid is infinitesimally small, such as when the radii are adjacent to each other as described below, the shape when viewed from the width direction becomes close to a right-angled triangle, but this can also be considered as a right-angled trapezoid. However, from the viewpoint of preventing chipping, it is preferable that the upper base has a straight line portion. Conventional magnetic wedges generally have a constant thickness, so the point that this thickness is different at both ends in the longitudinal direction is a major difference from conventional magnetic wedges.

[0031] The front view (center view) of Fig. 1(a) shows the shape of the magnetic wedge 10 as seen from the width direction, which is a right-angled trapezoid. In this case, the height (side 21) of the right-angled trapezoid is longer than the lower base (side 23) and upper base (side 24), and naturally, the oblique side (side 22) is longer than the height (side 21) of the right-angled trapezoid. Therefore, of the four sides constituting the right-angled trapezoid, the longest side is the oblique side.

[0032] Here, side 21 is taken as the reference side. Reference side 21 is parallel to the direction of insertion into the slot opening described in FIG. 5. Side 22 opposite reference side 21 is slanted. This side is called hypotenuse 22. Hypotenuse 22 may be a curved line curving toward reference side 21 as shown in FIG. 1(b), or may be bent in a V shape toward reference side 21 as shown in FIG. 1(c). In other words, hypotenuse 22 may be concave in a direction that narrows the area of ​​the right-angled trapezoid. In other words, anything that can be roughly recognized as a right-angled trapezoid is included in the right-angled trapezoid shape.

[0033] Side 23 (the lower base of the trapezoid) and side 24 (the upper base of the trapezoid) adjacent to reference side 21 are each perpendicular to reference side 21. This right angle does not need to be strictly 90 degrees, and may have a taper or a radius to make it easier to insert into the teeth. Similarly, the corner where side 23 or side 24 meets oblique side 22 may also be tapered or radiused. Shapes such as those described above are also included in right-angled trapezoid shapes.

[0034] Normally, the coil is gently curved, so it is preferable that the hypotenuse 22 of the magnetic wedge is also curved in order to fill the gap with the coil. The inclination angle and curved shape of the hypotenuse 22 can be selected in various ways according to the shape of the slot opening into which the magnetic wedge 10 is inserted.

[0035] The side views (left and right views) in FIG. 1(a) show the shape of the magnetic wedge 10 as viewed in the length direction. The shape of the cross section perpendicular to the length direction may be a simple rectangle, or may be T-shaped as shown in the figure (the T is upside down in the figure). An enlarged view of the left side view is shown at the bottom of the page. Here, the center of the T is called the body, and the part extending laterally (the part protruding in the width direction) is called the flange 25. The thickness of the body is also designated T3. The thickness T of the magnetic wedge 10 changes in the length direction, but the thickness T3 of the body does not change in the length direction and is constant.

[0036] The flange 25 may be tapered to match the shape of the slot opening into which the magnetic wedge 10 is inserted, and the taper angle (θ in FIG. 1) can be 0° or more and less than 90°. However, if the angle θ is close to 0°, stress is concentrated at the base of the flange 25, increasing the risk of the flange 25 breaking. On the other hand, the closer the angle θ is to 90°, the more likely the magnetic wedge 10 is to fall off from the slot opening. From this perspective, the angle θ is more preferably 10° or more and 80° or less, and even more preferably 20° or more and 70° or less.

[0037] Furthermore, dimensions and shapes other than the angle θ can also be selected from a variety of options to match the shape of the slot opening into which the magnetic wedge 10 is inserted. When the magnetic wedge 10 is attached to a typical three-phase induction motor, the width W is in the range of 3 to 15 mm, and the thickness T is in the range of 1 to 5 mm. As will be described later, since it is also possible to insert multiple magnetic wedges in a vertical row into the slot, the length L does not necessarily have to match the thickness of the stator, and can be selected from a variety of options, for example, in the range of 20 to 100 mm.

[0038] The rotating electric machine into which the magnetic wedge of this embodiment is inserted may be any rotating electric machine having a stator having a plurality of teeth and a plurality of slots formed by the plurality of teeth, and a rotor arranged in a position sharing an axis with the stator, and may be either a radial gap type rotating electric machine or an axial gap type rotating electric machine.

[0039] Fig. 2 is a schematic diagram of a case where a magnetic wedge 10 is attached to a radial gap type rotating electric machine. The magnetic wedge 10 is inserted into the slot opening of the rotating electric machine from the thinner side. As shown in the figure, the length direction of the magnetic wedge 10 corresponds to the axial direction of the rotating electric machine, the thickness direction of the magnetic wedge corresponds to the radial direction of the rotating electric machine, and the width direction of the magnetic wedge corresponds to the circumferential direction of the rotating electric machine. On the other hand, when mounting the magnetic wedge 10 to an axial gap type rotating electric machine, the magnetic wedge 10 is inserted from the outer periphery of the stator starting from the thinner end of the magnetic wedge 10. In this case, the length direction of the magnetic wedge corresponds to the radial direction of the rotating electric machine, the thickness direction of the magnetic wedge corresponds to the axial direction of the rotating shaft, and the width direction of the magnetic wedge corresponds to the circumferential direction of the rotating electric machine.

[0040] 3 shows a schematic cross-sectional view of the magnetic wedge 10 according to this embodiment attached to the slot opening of the stator 31. This figure shows a cross-sectional view of the stator 31 cut near the center between the teeth 34 (near the center of the slot) on a plane including the axis of the rotating electric machine. The left-right direction of the paper in this figure is the axial direction of the rotating electric machine, the upper side of the paper is the inner diameter side of the rotating electric machine, and the lower side of the paper is the outer diameter side. The magnetic wedges are installed in a row of three on the inner diameter side of the slot as shown in the figure. Of these, those located at both ends in the axial direction are the magnetic wedges 10 of this embodiment, and the one in the middle is the magnetic wedge 9 with a constant thickness.

[0041] A slot liner 35 is provided on the outer side of the magnetic wedges 9 and 10, and a coil 33 is provided on the outer side of the slot liner 35. A plurality of coils 33 are provided in the slot. For convenience of explanation, FIG. 1 is a schematic diagram in which gaps are provided between the magnetic wedge 10, the slot liner 35, and the coil 33, but in reality, they are in contact with each other or in close contact with each other. In addition, the coil 33 is usually fixed on the outside of the slot in such a way that it is pushed outward toward the outer diameter as shown in the figure in order to avoid interference with a rotor (not shown) present on the inner circumference side. Therefore, the coil 33 is curved inside the slot as shown in the figure, but by providing the magnetic wedges 10 of this embodiment at both ends of the slot axial direction as shown in the figure, unnecessary gaps are eliminated, and the effect of improving the efficiency of the rotating electric machine by the magnetic wedges can be further enhanced.

[0042] A schematic cross-sectional view of the schematic diagram of FIG. 3 cut along a plane perpendicular to the axis of the rotating electric machine is shown at the bottom of the figure. The cross sections are at two locations: the axial end (AA' cross section) and the axial center (BB' cross section). The cross section of the magnetic wedge 10 is T-shaped as shown in the figure, and both flanges (both ends of the T-shape) are caught by the protrusions of the teeth 34 so as not to fall off to the inner diameter side of the rotating electric machine. When the magnetic wedge 10 of this embodiment is used, the magnetic wedge 10 is fixed by being pressed against the teeth 34 from the outer diameter side by the coil 33 via the slot liner 35, even at the axial end (AA' cross section). Furthermore, the magnetic wedge 10 is bonded not only to the teeth 34 but also to the slot liner 35 by the varnish impregnation, so that it is fixed more firmly. As a result, the resistance to vibration caused by electromagnetic force when the rotating electric machine is driven is increased, and the risk of trouble such as wear and breakage of the magnetic wedge can be reduced.

[0043] In addition, FIG. 3 shows an example in which a total of three magnetic wedges 10 of this embodiment are inserted at both axial ends of the slot and a magnetic wedge 9 with a constant thickness is inserted in the center, but the insertion form of the magnetic wedges is not limited to this. For example, when the coil 33 is greatly curved, the magnetic wedges 10 of this embodiment may be inserted from both ends, and two magnetic wedges 10 may be inserted in one slot. In such a case, it is suitable for a small rotating electric machine with a thin stator 31. On the other hand, in a large rotating electric machine with a thick stator 31, it is possible to increase the number of magnetic wedges 9 with a constant thickness in the axial center and insert two magnetic wedges 10 of this embodiment only at both ends of the slot. In this case, the multiple magnetic wedges 9 in the center may be replaced with one relatively long magnetic wedge 9.

[0044] The magnetic wedge 10 can be a compact made of soft magnetic particles (hereinafter also referred to as soft magnetic powder), for example, iron powder or Fe-based soft magnetic alloy powder, or both. By using such a material for the magnetic wedge 10, it can be manufactured by powder press molding, and as a result, the above-mentioned shape can be easily formed without relying on machining, as described below.

[0045] 4 is a schematic diagram of a molding die (die 40) and an upper punch 41 and a lower punch 42 used when manufacturing the compact 11 by powder press molding. The die 40 is provided with a cavity having an opening 43 of a right-angled trapezoid shape equal to the side shape (shape in the center diagram of FIG. 1) of the compact 11 (which will be sintered later to become the magnetic wedge 10). At this time, the shape of the right-angled trapezoid is such that the height is longer than the lower and upper bases of the trapezoid, as with the shape of the magnetic wedge 10 described above, and naturally, the hypotenuse is longer than the height of the right-angled trapezoid. Therefore, of the four sides constituting the right-angled trapezoid, the longest side is the hypotenuse.

[0046] The upper punch 41 and the lower punch 42 have a cross-sectional shape perpendicular to the molding direction (the vertical direction of the paper) that is equal to the side shape of the magnetic wedge 10. However, the upper punch 41 and the lower punch 42 have dimensions that are smaller than the dimensions of the opening 43 by about several μm so that they can be inserted into the opening 43 of the die 40.

[0047] An enlarged view of the lower punch 42 is shown at the bottom of the paper in FIG. 4. As can be seen from this figure, the lower punch 42 has projections and recesses for forming the flange 25 of the magnetic wedge. The reference side 21 of the magnetic wedge 10 described in FIG. 1 is formed on the side 421 of the lower punch 42, the oblique side 22 of the magnetic wedge 10 is formed on the side 422 of the lower punch 42, and the angle θ of the flange 25 of the magnetic wedge 10 is formed by the sides 423 and 424 of the lower punch 42. At this time, the sides 423 and 424 are parallel to the side 421. This means that in the AA′ or BB′ cross section of FIG. 3, the magnetic wedge 10 does not protrude toward the inner diameter side (upper side of the paper) from the teeth 34 (in other words, the tip position of the teeth 34 and the reference surface 21 of the magnetic wedge 10 are at the same height), and this positional relationship is maintained. In other words, the punch faces of the upper and lower punches have projections and recesses, and the contour lines of the projections and recesses are parallel to the long sides of the right-angled trapezoid.

[0048] The manufacturing method for a magnetic wedge that is an embodiment of the present invention is a manufacturing method for a magnetic wedge to be installed at a slot opening of the stator of a rotating electric machine, and includes a press molding process in which raw material powder containing soft magnetic particles is press molded in the direction of width to obtain a molded body, where the dimension of the magnetic wedge in the circumferential direction of the rotating electric machine is taken as width, and in this press molding process, a die having an opening of the same shape as the side shape of the magnetic wedge 10 and a punch that can be inserted into the opening of the die are used.

[0049] Here, in the press molding process, for example, a die and upper and lower punches can be used to obtain a green body 11 of the magnetic wedge 10. The method of molding the magnetic wedge 10 using a die 40, an upper punch 41, and a lower punch 42 is as follows. First, only the lower punch 42 is inserted into the die 40, and raw material powder including soft magnetic powder is filled into the cavity. After that, the upper punch 41 is inserted into the opening 43 of the die and pressurized with a predetermined pressure. At this time, the pressing direction (molding direction) is the width direction of the magnetic wedge 10.

[0050] 4, it is preferable to make the shape of the punch faces of the upper and lower punches the same as the shape of the side portion of the magnetic wedge 10, and to perform pressure molding in the width direction of the magnetic wedge 10. The pressed raw material powder is compacted to become a compact 11 having the shape of the magnetic wedge 10. By subjecting this compact 11 to a heat treatment or the like to solidify it, the magnetic wedge 10 can be easily obtained without performing any additional machining.

[0051] The shape of the cross section perpendicular to the length direction of the magnetic wedge 10 is not limited to the T-shape shown in Fig. 1, but may be any shape in which the width of the magnetic wedge varies in the thickness direction, and may be various shapes such as a trapezoidal shape. In this case, the punch surfaces of the upper punch 41 and the lower punch 42 are also configured to match the side shape of the magnetic wedge 10.

[0052] Furthermore, it is preferable that the side shape of the magnetic wedge 10 (and the shapes of the upper and lower punches) is made of straight lines and curves, and is a shape that smoothly connects them. With such a shape, when the raw material powder in the cavity of the opening of the die is pressed by the upper and lower punches during molding, the raw material powder can move from the high pressure area to the low pressure area along the shape of the punch surface, so that the density uniformity inside the compact 11 can be improved. In addition, by making the punch surface shape like this, it is possible to prevent the stress applied to the punch surface during molding from concentrating on the inflection part, which is also preferable in terms of improving the durability and life of the punch. Furthermore, the magnetic wedge 10 is repeatedly pressed against the teeth by the electromagnetic excitation force when the motor is driven, which generates stress, but by making the side of the magnetic wedge 10 into such a shape, it is possible to prevent the above-mentioned stress from concentrating on the inflection part. Therefore, it is effective in terms of improving the durability and life of the magnetic wedge.

[0053] As a method of pressure molding, a molding method in which compression is simply performed using upper and lower punches (single-stage molding) as shown in Figure 4 can be used, but it is also possible to use a molding method in which one or both of the upper and lower punches are separated and compressed by controlling them independently (multi-stage molding). Of these, the single-stage molding method is preferable because it avoids the need to use complex and large presses and dies, and also because the time required for molding can be relatively short. However, when using the single-stage molding method, care must be taken to ensure that the density difference inside the molded body does not become too large.

[0054] That is, in the cross-sectional shape perpendicular to the length direction of the magnetic wedge 10 shown in FIG. 1, when the length of the upper side is W1 and the length of the lower side is W2, if W1 / W2 is too small, the density of the compact near the upper side is easily increased, while the density of the compact near the lower side is difficult to increase, so that the density difference inside the compact becomes large, and the strength is easily reduced and the magnetic properties are insufficient. From this viewpoint, in the case of one-stage molding, W1 / W2 is preferably 65% ​​or more, more preferably 70% or more, and even more preferably 75% or more. On the other hand, if the value of W1 / W2 becomes 100%, there will be no protrusion in the width direction, and the magnetic wedge cannot be fixed in the form shown in FIG. 3. From this viewpoint, the value of W1 / W2 is preferably 95% or less, more preferably 90% or less, and even more preferably 85% or less.

[0055] On the other hand, due to the structure of the stator, there are cases where the value of W1 / W2 must be set to 65% or less. In such cases, by using the multi-stage forming method, it is possible to create a shape where W1 / W2 is 60% or less, 50% or less, or even 40% or less.

[0056] In principle, the direction of pressure during molding can be the thickness direction or the length direction in addition to the width direction. However, when pressing in the thickness direction, the pressing surface is the largest surface of the magnetic wedge 10, so a large load is required. This requires a large press machine, which causes problems such as high equipment costs. On the other hand, when pressing in the length direction, although the pressing surface is the smallest, it is difficult to form the shape shown in FIG. 1 only through the molding process. Furthermore, it is necessary to prepare a fairly thick die and elongated upper and lower punches, which causes an increase in die costs, including the durability of the die. In this regard, according to the manufacturing method of this embodiment in which pressure is applied in the width direction, pressure can be applied over a relatively small surface area, and the load can be significantly reduced compared to when molding in the thickness direction. Furthermore, the shape of the oblique side 22 of the magnetic wedge can be easily formed by making the opening of the die into an appropriate shape as described above.

[0057] The molding pressure can be adjusted appropriately according to the material and properties of the raw material powder, but if it is too low, the density of the molded body will be too low, resulting in insufficient strength of the molded body, which will cause problems in handling in later processes, and even after heat treatment, the density will be low, resulting in insufficient strength and failure to obtain the desired magnetic properties. Therefore, the molding pressure is preferably 0.1 GPa or more, more preferably 0.2 GPa or more, and more preferably 0.3 GPa or more. On the other hand, if the molding pressure is too high, the load on the mold will increase, making it easier for wear and cracks to occur, and the mold life will be shortened. From this perspective, the molding pressure is preferably 3 GPa or less, more preferably 2 GPa or less, and even more preferably 1 GPa or less.

[0058] In order to extend the life of the die, it is preferable that at least the portions of the die and the upper and lower punches which come into contact with the compact 11 are made of cemented carbide.

[0059] As described above, according to the manufacturing method of this embodiment, the end of the magnetic wedge 10 can be formed with a rounded shape without machining, and the magnetic wedge 10 that can easily improve the efficiency of a rotating electric machine can be manufactured at low cost. Furthermore, the corners of the opening of the die and the corresponding corners of the upper and lower punches may be rounded. This reduces the stress concentration at the corners caused by the molding pressure, and is also effective in improving the life of the die. In order to more reliably enjoy the above-mentioned effects, the radius of the rounded shape is preferably 0.1 mm or more, more preferably 0.2 mm or more, and even more preferably 0.3 mm or more.

[0060] From the viewpoint of ensuring the effective length of the magnetic wedge 10, the radius of the arc is preferably 50% or less of the thickness of the magnetic wedge 10, more preferably 40% or less, and even more preferably 30% or less. On the other hand, by making the arc smaller, the gap between this portion of the magnetic wedge and the tip of the tooth is reduced, the fixation of the magnetic wedge is strengthened, and the disturbance of the magnetic flux distribution occurring around the gap is suppressed, which results in the magnetic wedge contributing to improving the motor efficiency. From this viewpoint as well, the radius of the arc is preferably 50% or less of the thickness of the magnetic wedge 10, more preferably 40% or less, and even more preferably 30% or less.

[0061] The magnetic wedge 10 can also be a composite material made of soft magnetic particles and an electrically insulating substance. The composite material is a material in which an electrically insulating substance is present between multiple soft magnetic particles, bonding the soft magnetic particles together and electrically isolating the particles from each other, and by increasing the electrical resistance of the magnetic wedge 10, the eddy current loss generated in the magnetic wedge 10 can be suppressed.

[0062] The average particle size of the soft magnetic particles (median diameter d50 in the cumulative particle size distribution) is preferably 200 μm or less, more preferably 100 μm or less, and even more preferably 50 μm or less, because if it is too large, the electrical resistance decreases and the eddy current loss increases. On the other hand, in order to maintain high magnetic permeability and enhance the effect of the magnetic wedge, the average particle size of the ferromagnetic particles is preferably 2 μm or more, more preferably 5 μm or more, and even more preferably 10 μm or more.

[0063] As the electrically insulating material, either an organic substance or an inorganic substance can be used, for example, epoxy resin, phenol resin, polyimide, polyphenylene sulfide, polyamide, polyamideimide, silicon resin, colloidal silica, low melting point glass, etc. When using these, after mixing the ferromagnetic powder with the electrically insulating material, it can be produced by the above-mentioned powder press molding, as well as transfer molding, injection molding, hot pressing, etc.

[0064] In the manufacturing method of the magnetic wedge of this embodiment, the raw material powder is a mixed powder of a powder of Fe-based soft magnetic particles containing element M, which is more easily oxidized than Fe, and a binder, and after the press molding process, a heat treatment process is performed to the molded body to form a surface oxide phase of the Fe-based soft magnetic particles between the particles, which bonds the Fe-based soft magnetic particles to each other.

[0065] The magnetic wedge 10 is a compact of a plurality of Fe-based soft magnetic particles 1 containing an element M that is more easily oxidized than Fe. Here, "element M that is more easily oxidized than Fe" means an element whose standard Gibbs energy of oxide formation is lower than that of Fe2O3. As the element M, at least one selected from the group consisting of Al, Si, Cr, Zr, and Hf can be used.

[0066] As one form of the magnetic wedge 10, the soft magnetic particles are an Fe-based alloy containing element M, which is more easily oxidized than Fe, and an oxide phase of element M is generated between the soft magnetic particles to bond the particles together. In order to manufacture the magnetic wedge 10 in this form, the soft magnetic particles are press-molded by the above-mentioned method, and then heat-treated in an atmosphere containing oxygen, so that the oxide phase of element M can grow on the grain boundaries. In this form, the proportion of electrically insulating material on the grain boundaries can be minimized, and the density is increased, resulting in high strength and high magnetic permeability, which is more preferable.

[0067] In order to generate the oxide phase of element M, the heat treatment temperature is preferably 650°C or higher, more preferably 700°C or higher. On the other hand, if the heat treatment temperature is too high, oxidation of Fe proceeds and the magnetic properties deteriorate (reduction in magnetic permeability and increase in iron loss). From this viewpoint, the heat treatment temperature is preferably 850°C or lower, more preferably 800°C or lower. If the heat treatment time is too short, the generation of element M is insufficient and the strength decreases, while if it is too long, oxidation of Fe proceeds and the magnetic properties deteriorate. From this viewpoint, the heat treatment time is preferably in the range of 30 minutes to 6 hours, more preferably in the range of 1 to 3 hours.

[0068] Here, the element M may be selected not only as one type, but also as two or more types in combination, such as Al and Cr, Si and Cr. For example, two types, Al and Cr, may be selected, and the Fe-based soft magnetic particles may be Fe-Al-Cr alloy particles. In this way, the magnetic wedge 10 with high bending strength and electrical resistance can be obtained. The Fe-Al-Cr alloy is an alloy in which the elements with the second highest content after Fe are Cr and Al (in no particular order), and other elements may be contained in smaller amounts than Fe, Cr, and Al. The composition of the Fe-Al-Cr alloy is not particularly limited, but for example, the content of Al is preferably 2.0 mass% or more, more preferably 5.0 mass% or more. From the viewpoint of obtaining a high saturation magnetic flux density, the content of Al is preferably 10.0 mass% or less, more preferably 6.0 mass% or less. Moreover, the content of Cr is preferably 1.0 mass% or more, more preferably 2.5 mass% or more. From the viewpoint of obtaining a high saturation magnetic flux density, the content of Cr is preferably 9.0 mass% or less, more preferably 4.5 mass% or less.

[0069] When two or more elements are selected as the element M, the total content of these elements is preferably 1.0 mass % or more and 20 mass % or less, similarly to the case where one element is selected.

[0070] The Fe-based soft magnetic particles may be surface-treated by a chemical method, heat treatment, etc. Furthermore, the Fe-based soft magnetic particles may be composed of a plurality of types of Fe-based soft magnetic particles having different compositions.

[0071] As described above, according to the present invention, a magnetic wedge that can further increase the efficiency of a rotating electric machine can be obtained, and such a magnetic wedge can be manufactured at low cost without machining. [Explanation of symbols]

[0072] 9: Magnetic wedge (constant thickness) 10: Magnetic wedges (different thicknesses) 11: Molded object (magnetic wedge) 21: Reference edge of magnetic wedge 22: Hypotenuse of magnetic wedge 23: Magnetic Wedge Edge 24: Magnetic Wedge Edge 25: Magnetic wedge flange 31:Stator 32:Rota 33: Coil 34: Teeth 35: Slot Liner 36: Secondary conductor 40: Dice 41: Upper punch 42: Down punch 43: Dice opening L: Length of the magnetic wedge R: Earl T: Thickness of the magnetic wedge T1: Thickness of the magnetic wedge T2: Thickness of the magnetic wedge T3: Thickness of the magnetic wedge body W: Width of the magnetic wedge W1: Length of the top edge of the magnetic wedge W2: Length of the bottom side of the magnetic wedge

Claims

1. A magnetic wedge installed in a slot opening of a stator of a rotating electric machine, comprising: If the dimension of the magnetic wedge in the circumferential direction of the rotating electric machine is the width, A magnetic wedge in which the projected shape of the magnetic wedge when projected onto a plane perpendicular to the width direction is a right-angled trapezoid, and the longest side of the four sides constituting the right-angled trapezoid is the hypotenuse.

2. The magnetic wedge according to claim 1 , wherein the right-angled trapezoid shape has rounded corners.

3. The magnetic material includes a plurality of soft magnetic particles and an electrically insulating material between the soft magnetic particles.

2. The magnetic wedge of claim 1 .

4. the soft magnetic particles are Fe-based soft magnetic particles, The Fe-based soft magnetic particles contain an element M which is more easily oxidized than Fe, the electrically insulating material is an oxide phase containing the element M, 4. The magnetic wedge according to claim 3, wherein the Fe-based soft magnetic particles are bound by the oxide phase.

5. 5. The magnetic wedge according to claim 4, wherein the element M is at least one selected from the group consisting of Al, Si, Cr, Zr and Hf.

6. 6. The magnetic wedge according to claim 5, wherein the Fe-based soft magnetic particles are Fe-Al-Cr alloy particles.

7. A rotating electric machine including a stator for a rotating electric machine having a plurality of teeth and a plurality of slots formed by the plurality of teeth, and a rotor arranged at a position sharing an axis with the stator for the rotating electric machine, A rotating electric machine in which a plurality of magnetic wedges are inserted in a vertical row in the axial direction into the slot opening of each of the plurality of slots, and at least one of the plurality of magnetic wedges is the magnetic wedge of any one of claims 1 to 6.

8. A method for manufacturing a magnetic wedge to be installed in a slot opening of a stator of a rotating electric machine, comprising the steps of: If the dimension of the magnetic wedge in the circumferential direction of the rotating electric machine is the width, A press molding process is provided in which a raw material powder containing soft magnetic particles is press-molded in the width direction to obtain a molded body, In the press molding process, a die having a right-angled trapezoidal opening, Using a punch that can be inserted into the opening of the die, A method for manufacturing a magnetic wedge, in which the longest side of the four sides constituting the right-angled trapezoid shape is the hypotenuse side.

9. The method for manufacturing a magnetic wedge according to claim 8, characterized in that the corners of the opening of the right-angled trapezoid are rounded.

10. The raw material powder is a mixed powder of a powder of Fe-based soft magnetic particles containing an element M that is more easily oxidized than Fe, and a binder, a heat treatment step of subjecting the compact to a heat treatment after the press molding step, to form a surface oxide phase between the Fe-based soft magnetic particles, which bonds the Fe-based soft magnetic particles to each other; The method of claim 9, further comprising the steps of:

11. The method for producing a magnetic wedge according to claim 10, wherein the element M is at least one selected from the group consisting of Al, Si, Cr, Zr and Hf.

12. The method for manufacturing a magnetic wedge according to claim 11, wherein the Fe-based soft magnetic particles are Fe-Al-Cr alloy particles.

Citation Information

Patent Citations

  • Rotary electric machine including slot blocking wedge made of metal filled type garabo woven cloth and method of the same

    JP1991027745A