Light emitting device or optical member

The implementation of a ruthenium oxide conductive film in wavelength conversion sections of light emitting devices ensures stability and improved detection accuracy under high temperature and humidity conditions, addressing the challenges of environmental stability in existing technologies.

JP2024150736AActive Publication Date: 2024-10-23NICHIA CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024126105
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-10-23
Estimated Expiration
2040-04-06

AI Technical Summary

Technical Problem

Existing light emitting devices and optical members face challenges in achieving high detection accuracy and stability under varying temperature and humidity conditions, particularly with conductive films used in wavelength conversion sections.

Method used

The use of a conductive film made from ruthenium oxide surrounding the wavelength conversion section, which maintains low resistance changes (less than 2.5%) under high temperature and humidity conditions, ensuring reliable operation and improved detection accuracy.

Benefits of technology

The ruthenium oxide conductive film provides enhanced detection accuracy by minimizing resistance changes, maintaining device performance in harsh environments, and enabling effective abnormality detection in the wavelength conversion section.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024150736000001_ABST
    Figure 2024150736000001_ABST
Patent Text Reader

Abstract

To provide an optical member or a light emitting device with excellent detection accuracy.SOLUTION: An optical member includes a wavelength conversion member that emits light having a wavelength different from that of incident light, and a wiring that surrounds the main light that is incident on the wavelength conversion member, or a light emitting device includes a light emitting element. The wiring is formed using ruthenium oxide. Alternatively, the wiring satisfies at least one of a case in which the wiring is an oxide, or a case in which the wiring has a light transmittance of 60% or less, and satisfies at least one of a case in which the change rate of the wiring resistance is 2.5% or less when it is moved from room temperature to a high-temperature and high-humidity environment of a temperature of 85°C and a humidity of 85% and stored for 100 hours, or a case in which the change rate of the sheet resistance is less than 3% when it is moved from room temperature to an environment of 100°C and stored for 50 hours or 100 hours.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a light emitting device or an optical member. [Background technology]

[0002] Laser light is used for various purposes. When using laser light, safety is also a major consideration. In Patent Document 1, the excitation light, which is a laser beam, is used as light of a different wavelength. and a conductive thin wire for detecting damage to the conversion member. An optical member having such a structure is disclosed. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2019-117827 Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the present invention is to provide an optical member or a light emitting device with excellent detection accuracy. [Means for solving the problem]

[0005] The light emitting device disclosed in the present specification includes a light emitting element and a light emitting device for emitting light. a wavelength conversion unit that converts the light into light of a different wavelength and emits the light to the outside; and an enclosure that surrounds the wavelength conversion unit. and a conductive film provided in the surrounding portion and surrounding the wavelength converting portion. The conductive film is formed using ruthenium oxide.

[0006] The light emitting device disclosed in the present specification includes a light emitting element and a light emitting diode. A wavelength conversion unit converts incoming light into light of a different wavelength and emits the light to the outside. A wavelength conversion member having an enclosure and a conductive film provided on the enclosure and surrounding the wavelength conversion portion. The conductive film is an oxide, and is resistant to a temperature ranging from room temperature to a high temperature of 85°C and a humidity of 85%. When stored in a high humidity environment for 100 hours, the change in wiring resistance is 2.5% or less. It is.

[0007] The light emitting device disclosed in the present specification includes a light emitting element and a light emitting diode. A wavelength conversion unit converts the light entering the wavelength conversion member into light of a different wavelength and emits the light to the outside. a surrounding portion surrounding the surface, and a conductive film disposed in the surrounding portion and surrounding the wavelength conversion portion; a conversion member, and the conductive film has a transmittance of 6. 0% or less, and moved from room temperature to a high-temperature, high-humidity environment of 85°C and 85% humidity. When stored at room temperature for 100 hours, the change in wiring resistance is 2.5% or less.

[0008] The light emitting device disclosed in the present specification includes a light emitting element and a main light emitting element. a wavelength conversion section on which the light from the light emitting element is incident, and a region outside the region on which the light from the light emitting element is incident and a conductive film surrounding the region on the side of the wavelength conversion member. The transmittance of the light emitted from the optical element is 60% or less, and the temperature range is from room temperature to 85℃. Change in wiring resistance when stored for 100 hours in a high-temperature, high-humidity environment with a humidity of 85% The rate is below 2.5%.

[0009] In addition, the optical member disclosed in this specification emits light having a wavelength different from that of the incident light. A base material having a wavelength converting portion and an enclosure portion surrounding a side surface of the wavelength converting portion, and a conductive film disposed on the upper or lower surface of the wavelength conversion portion and surrounding the wavelength conversion portion, the conductive film being made of an acid. It is formed using ruthenium chloride.

[0010] In addition, the optical member disclosed in this specification emits light having a wavelength different from that of the incident light. A base material having a wavelength converting portion and an enclosure portion surrounding a side surface of the wavelength converting portion, and a conductive film disposed on the upper or lower surface of the wavelength conversion portion and surrounding the wavelength conversion portion, the conductive film being made of an acid. It is a compound that has been transferred from room temperature to an environment of 100°C and stored for 50 or 100 hours. When the temperature is increased, the rate of change in sheet resistance is less than 3%.

[0011] In addition, the optical member disclosed in this specification emits light having a wavelength different from that of the incident light. and a conductive film surrounding a predetermined region of the base material, The conductive film has a visible light transmittance of 60% or less, and when moved from room temperature to an environment of 100°C, The sheet resistance change is less than 3% when stored for 50 or 100 hours under this condition. . Effect of the Invention

[0012] According to the present invention, it is possible to provide an optical member or a light emitting device with excellent detection accuracy. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a perspective view of a light emitting device according to an embodiment. [Diagram 2] FIG. 2 is a top view corresponding to FIG. [Diagram 3] FIG. 3 is a cross-sectional view of the light emitting device taken along line III-III in FIG. [Figure 4] FIG. 4 is a perspective view for explaining the internal structure of the light emitting device according to the embodiment. [Diagram 5] FIG. 5 is a top view corresponding to FIG. [Figure 6] FIG. 6 is a perspective view for explaining the internal structure of the light emitting device according to the embodiment. [Figure 7] FIG. 7 is a top view corresponding to FIG. [Figure 8] FIG. 8 is a perspective view of an optical member according to an embodiment. [Figure 9] FIG. 9 is a top view corresponding to FIG. [Figure 10] FIG. 10 is a top view showing the base material of the wavelength conversion member to explain the joint surface between the light-transmitting member and the wavelength conversion member according to the embodiment. [Figure 11] FIG. 11 is a bottom view of the wavelength conversion member according to the embodiment. [Figure 12] FIG. 12 is a top view of the light-transmissive member according to the embodiment. [Figure 13] FIG. 13 is a graph showing the results of an experiment investigating the correlation between the annealing temperature and the sheet resistance of ruthenium oxide. [Figure 14] FIG. 14 is a graph showing the results of an experiment investigating the change in resistance of each ruthenium oxide when ruthenium oxide that had been subjected to heat treatment under different conditions and ruthenium oxide that had not been subjected to heat treatment were stored in a high-temperature environment. [Figure 15] FIG. 15 is a graph showing the results of an experiment investigating the change in resistance of ruthenium oxide and indium tin oxide stored in a high-temperature, high-humidity environment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] In this specification or claims, when referring to polygons such as triangles and quadrilaterals, Polygons and shapes that have been processed with rounded corners, chamfers, corner removal, rounding, etc. are also included. In addition, the shape where processing is applied not only to the corners (edges) but also to the middle part of the edge is also called In other words, the polygon is left as the base, but partial processing is performed. The shapes shown are within the interpretation of "polygon" as used herein and in the claims. It shall be so.

[0015] This also applies to words that represent specific shapes, such as trapezoids, circles, and irregular shapes, not just polygons. The same is true for each edge that forms the shape. Even if the corners or middle parts are processed, the interpretation of the “side” includes the processed parts. In addition, "polygons" and "edges" that are not partially processed are distinguished from processed shapes. In such cases, the word "strict" shall be added, for example, "strict rectangle."

[0016] In addition, in the present specification or claims, the terms "up and down," "left and right," "front and back," "front and back," "front and back," and "back" are used interchangeably. These expressions only describe the relationship of relative position, orientation, direction, etc. For example, the top surface of a part may be aligned with the top surface of the finished product. Even if the component is mounted on the side, the top surface remains the same for that component.

[0017] In addition, in the present specification or claims, the following description will be used to refer to a certain component: When there are multiple things and you want to distinguish between them, you can put “first,” “second,” etc., in front of the component. In addition, the following points are sometimes distinguished in the present specification and the claims: In the case where the subject matter or viewpoint is different, the same notation is used between the present specification and the claims. may not refer to the

[0018] For example, objects that are distinguished by being labeled "first," "second," and "third" in this specification In the case where the claims are written only with respect to the "first" and "third" in the specification, In such cases, the claims may be distinguished by adding "first" and "second" for ease of reading. In this case, the subject matter described as "first" and "second" in the claims may be refers to the objects referred to as "first" and "third" in this specification.

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The embodiments embody the technical ideas of the present invention, but do not limit the present invention. In the following description, the same names and symbols refer to the same or similar components. The drawings show the sizes of the components shown in the drawings. The sheath, positional relationship, etc. may be exaggerated for clarity of explanation.

[0020] <Embodiment> FIG. 1 is a perspective view showing an example of a light emitting device 1 according to an embodiment. FIG. Fig. 3 is a cross-sectional view of the light emitting device 1 taken along line III-III in Fig. 2. FIG. 1 is a perspective view of the light emitting device 1 with a light blocking member 90 removed in order to explain the internal structure. FIG. 5 is a top view in the same state as FIG. 4. FIG. 6 is a diagram showing the internal structure of the device. 7 is a perspective view of the device 1 with the light-transmitting member 82 and the wavelength conversion member 81 removed therefrom. FIG. 8 is a top view in the same state as in FIG. 6. FIG. 9 is a top view in the same state as FIG. 8. FIG. 10 is a perspective view of an example. In order to explain the bonding surface between the optical member 82 and the wavelength conversion member 81, 10 is a top view of the bonding area of ​​the metal film 821 of the light-transmitting member 82. , and the conductive film 813 of the wavelength conversion member 81 are indicated by hatching. 11 is a bottom view of the wavelength conversion member 81 according to the embodiment. 12 is a top view of a light-transmitting member 82 according to an embodiment.

[0021] The light emitting device 1 includes, as its components, a base 10, a light emitting element 20, a submount 30, and a light reflector. A member 40, a protective element 50, a temperature measuring element 60, a wiring 70, an optical member 80, and a light blocking member 90. The light emitting device 1 includes, as its components, at least a light emitting element 20 and , and optical member 80.

[0022] The light emitting device 1 has one or more light emitting elements 20. The light-reflecting member 40 includes one or more protection elements 50. Also, it has one or more temperature measuring elements 60. Also, it has one or more wirings 7 0.

[0023] The optical member 80 includes a wavelength conversion member 81 and a light-transmitting member 82 as components. The optical member 80 includes at least a wavelength conversion member 81 as a component. The light emitting device 1 may further include other components.

[0024] Next, each component will be described. (base 10) The base 10 has a concave shape that is recessed from the top surface to the bottom surface. The recess is formed inside this outer shape. The base 10 has an upper surface 11, a bottom surface 12, and a lower surface 13. 3, one or more inner surfaces 14 and one or more outer surfaces 15. When viewed from above, a frame is formed by the lines where the upper surface 11 and one or more inner surfaces 14 intersect. The recess of part 10 is surrounded by this frame.

[0025] The base 10 also has one or more step portions 16 on the inside of the frame. In the portion 10, two step portions 16 having different heights from the bottom surface 12 are formed. The step portion 16 is composed only of an upper surface and a side surface that intersects with the upper surface and extends downward. The height of the step portion 16 is the height from the bottom surface 12 to the upper surface of the step portion 16. The inner surface 14 includes a side surface that intersects with the upper surface 11 of the base 10 and a side surface of a step portion 16. do.

[0026] Here, of the two step portions 16, the one having a lower height from the bottom surface 12 is referred to as a first step portion 161. The higher one is called the second step portion 162. The first step portion 161 is the entire frame of the base 10. The second step portion 162 is not provided around the entire periphery of the frame of the base portion 10. The base 10 is not provided with a plurality of second step portions 16. 2 is formed.

[0027] The base 10 may be formed mainly of ceramic. Examples of the materials that can be used include aluminum nitride, silicon nitride, aluminum oxide, and silicon carbide. The main material is not limited to ceramic, and may be other insulating materials. good.

[0028] In addition, one or more metal films are provided on the bottom surface 12 of the base 10. One or more metal films are provided on the upper surface of the step portion 162. In the illustrated example of the light emitting device 1, the bottom surface 12 is provided with one or more metal films. Four metal films, one metal film on each of the two second step portions 162, and six gold films on the upper surface 11. A metal membrane is provided.

[0029] In addition, the one or more metal films provided on the bottom surface 12 may include a metal film provided on the top surface 11. The second step portion 162 includes a metal film that is electrically connected to the first step portion 162. The metal film or films include a metal film electrically connected to the metal film provided on the upper surface 11. do.

[0030] (Light emitting element 20) The light emitting element 20 is a semiconductor laser element, although it does not have to be a semiconductor laser element. For example, a light-emitting element such as an LED or an organic EL may be used as the light-emitting element 20 of the light-emitting device 1. In the illustrated example of the light emitting device 1, a semiconductor laser element 20 is used as the light emitting element 20. 0 is adopted.

[0031] The semiconductor laser element 20 shown in the figure has a rectangular outer shape when viewed from above. The side surface intersecting with one of the two short sides is the emitting surface of the light emitted from the semiconductor laser element 20. The upper and lower surfaces of the semiconductor laser element 20 are larger in area than the light emitting end surface. stomach.

[0032] The light (laser light) emitted from the semiconductor laser element 20 has a spreading property. An elliptical far-field pattern (hereafter referred to as "FFP") is formed in a plane parallel to the end face. Here, FFP refers to the shape and light emitted from the light source at a position away from the light output facet. The intensity distribution is shown.

[0033] The shape of the FFP of the light emitted from the semiconductor laser element 20 is determined by the number of semiconductor layers including the active layer. The layer direction is longer than the layer direction, and the perpendicular direction is called the FF. The horizontal direction of P and the stacking direction are called the vertical direction of the FFP.

[0034] Based on the light intensity distribution of the FFP of the semiconductor laser element 20, 1 / e 2 The light having the intensity above this level is called the main part of the light. The angle corresponding to the full width at half maximum of the fabric is called the divergence angle. The spread angle of the FFP in the horizontal direction is called the horizontal spread angle. This is called the bevel angle.

[0035] The light emitting element 20 has a peak emission wavelength of 320 nm to Use a wavelength in the range of 530 nm, typically in the range of 430 nm to 480 nm. As such a semiconductor laser element 20, a semiconductor laser including a nitride semiconductor can be used. Examples of nitride semiconductors include GaN, InGaN, and AlGa N can be used. However, the light emitted from the light emitting element 20 is not limited to this. stomach.

[0036] (Submount 30) The submount 30 is configured in a rectangular parallelepiped shape and has a bottom surface, a top surface, and side surfaces. In addition, the width of the submount 30 in the vertical direction is the smallest. The shape is not limited to a rectangular parallelepiped. The submount 30 is made of, for example, silicon nitride, aluminum nitride, or silicon carbide. It should be noted that other materials may be used. A metal membrane is provided.

[0037] (Light reflecting member 40) The light reflecting member 40 has two light reflecting surfaces 41 that reflect light. In this case, a surface is provided that has a light reflectance of 90% or more for the peak wavelength of the irradiated light. The light reflectance at can be up to or less than 100%.

[0038] The two light reflecting surfaces 41 are planar and inclined with respect to the lower surface. The oblique angles are different. In other words, the two light reflecting surfaces 41 are both perpendicular to the lower surface. The two light reflecting surfaces 41 are not parallel to each other. Form a shooting area.

[0039] Here, the light reflecting surface closer to the bottom surface is called the first reflecting surface 411, and the light reflecting surface further away is called the second reflecting surface 412. In the light reflecting member 40, the inclination angle of the second reflecting surface 412 is larger than that of the first reflecting surface 412. For example, the inclination angle of the first reflecting surface 411 and the second reflecting surface 412 is larger than the inclination angle of the first reflecting surface 411. The difference in the inclination angle is in the range of 10 degrees or more to 60 degrees or less.

[0040] In addition, the light reflecting surface 41 may have three or more light reflecting surfaces 41 that form one integral reflecting area. Also, one light reflecting surface 41 may form one reflecting area. The light reflecting surface 41 may further include a light reflecting surface that is not continuously connected. may be a curved surface rather than a flat surface.

[0041] The light reflecting member 40 may be made of glass, metal, or the like as a main material for forming its outer shape. The main material should be heat-resistant, such as quartz or BK7 (borosilicate glass). Glass, metal such as aluminum, or silicon can be used. The light reflecting surface is e.g. For example, metals such as Ag and Al, Ta2O5 / SiO2, TiO2 / SiO2, Nb2O5 / It can be formed using a dielectric multilayer film such as SiO2.

[0042] (Protection element 50) The protective element 50 is configured to protect a specific element, such as a light-emitting element, from being destroyed by an excessive current flowing therethrough. The protection element 50 is, for example, a Zener diode made of Si. A diode may be used.

[0043] (Temperature measuring element 60) The temperature measuring element 60 is an element used as a temperature sensor for measuring the surrounding temperature. As the temperature measuring element 60, for example, a thermistor can be used.

[0044] (Wiring 70) The wiring 70 is used for electrical connection between the two components. For example, a metal wire can be used.

[0045] (wavelength conversion member 81) The wavelength conversion member 81 has a lower surface, an upper surface, and a side surface. The wavelength converting member 81 has a wavelength converting portion 811. The wavelength converting member 81 also has an enclosure portion 812. The wavelength conversion member 81 includes a conductive film 813. The wavelength conversion member 81 also includes a metal film 814. has.

[0046] The wavelength conversion member 81 is made of a base material having a conductive film 813, a metal film 814, or other That is, the wavelength conversion member 81 is formed by forming a base material of the wavelength conversion member 81. and providing a conductive film 813 on the base material of the wavelength conversion member 81. and providing a metal film 814 on the base material of the wavelength conversion member 81.

[0047] The step of providing the metal film 814 may be performed before the step of providing the conductive film 813. In addition, the base material with the metal film 814 provided on the base material of the wavelength conversion member 81 is You may prepare it by purchasing it, etc.

[0048] The base material is configured in a rectangular parallelepiped flat plate shape. However, the shape is not limited to a rectangular parallelepiped. The surrounding portion 812 is included in the base material of the wavelength conversion member 81. The base material of the wavelength conversion member 81 is an inorganic material that is not easily decomposed by irradiation with light. The main material may be an inorganic material.

[0049] In the wavelength conversion member 81, the wavelength conversion portion 811 and the surrounding portion 812 are integrally formed. The surrounding portion 812 surrounds the wavelength converting portion 811. The inner surface of the surrounding portion 812 is in contact with the side surface of the wavelength converting portion 811, and the outer surface of the surrounding portion 812 is in contact with the side surface of the wavelength converting member 8 The wavelength converting member 81 corresponds to the side surface of the light emitting element 1. The wavelength converting member 81 includes a wavelength converting portion 811 and a surrounding portion 812. It is formed of an integrally sintered body.

[0050] Such an integrated sintered body may include, for example, a wavelength converting portion 811 made of a molded product such as a sintered body, and an envelope. The powder material forming the surrounding portion 812 is molded and sintered to form the base material of the wavelength conversion member 81. In addition, the surrounding portion 812 made of a molded product such as a sintered body and the wavelength conversion material can be formed. The powder material forming the portion 811 is integrally molded and sintered to form the base material of the wavelength conversion member 81. For sintering, for example, the spark plasma sintering method (SPS method) or hot A press sintering method (HP method) or the like can be used.

[0051] The wavelength converting portion 811 has a rectangular parallelepiped shape. In addition, the wavelength conversion unit 811 may convert the light incident on the wavelength conversion unit 811 into a different The wavelength conversion unit 811 converts the light into a different wavelength. The wavelength converting unit 811 outputs the light having the wavelength A part of the light incident on the wavelength converting portion 811 is emitted to the outside of the wavelength converting portion 811 .

[0052] The wavelength conversion portion 811 is formed mainly of ceramics and contains a phosphor. However, the main material may be glass. Alternatively, a multi-crystal phosphor may be used. The wavelength conversion portion 811 may be formed of a single crystal of a phosphor. It is preferable to use a material with a temperature of 1300℃ to 2500℃ as the main material. Even when the heat applied to the length changing portion 811 is taken into consideration, deterioration such as deformation and discoloration is unlikely to occur.

[0053] For example, when ceramics is used as the main material of the wavelength conversion unit 811, phosphor and aluminum oxide The phosphor content can be adjusted by sintering the ceramic with a light-transmitting material such as ceraminium. The content of the filler may be 0.05% by volume to 50% by volume relative to the total volume of the mix. Ceramics consisting essentially of phosphor, obtained by sintering phosphor powder, may also be used.

[0054] The phosphor used was cerium-activated yttrium aluminum garnet (Y AG), cerium-activated lutetium aluminum garnet (LAG), Nitrogen-containing calcium aluminosilicate (CaO-Al) activated with rhodium and / or chromium 2O3-SiO2), europium activated silicate ((Sr,Ba)2SiO4), Examples of such phosphors include α-sialon phosphors and β-sialon phosphors. The YAG phosphor is a phosphor that can emit white light in combination with blue excitation light. It is preferable to use

[0055] The enclosure 812 is a rectangular parallelepiped flat plate having a through hole in the center. The wavelength converting portion 811 is provided in the through hole. In response, the surrounding portion 812 surrounds the side surface of the wavelength converting portion 811 .

[0056] The surrounding portion 812 can be formed mainly using ceramics. However, metal or a composite of ceramics and metal may be used. It is preferable to use a material with high thermal conductivity that can dissipate heat generated by the wavelength conversion portion 811. The surrounding portion 812, which is mainly made of a material having a high thermal conductivity, dissipates heat in the wavelength conversion portion 811. From this viewpoint, it can be regarded as a heat dissipation member in place of the enclosure portion 812. do.

[0057] The surrounding portion 812 contains the light emitted by the semiconductor laser element 20 and the fluorescent light emitted by the phosphor. It is preferable to use a material that reflects light with high reflectance. It is preferable to reflect light in the area surrounding the side surface. A material with high reflectivity is used as the main material. The surrounding portion 812 has high reflectivity for reflecting the irradiated light. From this viewpoint, the surrounding portion 812 It can also be considered as a light reflecting member. Examples of the oxide include alumina (Al2O3).

[0058] The surrounding portion 812 does not have a wavelength conversion function like the wavelength conversion portion 811. The surrounding portion 812 converts the light incident on the surrounding portion 812 into light of a different wavelength and emits the converted light to the outside. In addition, the enclosure 812 cannot convert the light incident on the enclosure 812 and emit it to the outside. For example, the surrounding portion 812 does not contain a phosphor. has a light-blocking property with a transmittance of 5% or less.

[0059] The conductive film 813 is provided on the upper surface side or the lower surface side of the wavelength conversion member 81. 813 is provided on the upper or lower surface of the base material of the wavelength conversion member 81. Alternatively, another thin film (for example, an anti-reflection film) may be interposed. The predetermined area is surrounded by the member 81. is, for example, the region where the main part of the light is incident on the wavelength conversion member 81. By providing the conductive film 813 outside the region where light enters, light can be extracted efficiently.

[0060] The conductive film 813 is provided on the surrounding portion 812. The conductive film 813 is a wavelength conversion film. The conductive film 813 is provided on the outer side of the wavelength converting portion 811. For example, the distance between the wavelength converting portion 811 and the conductive film 813 is 500 mm at the closest position. The conductive film 813 has a thickness of 300 μm or less, and preferably has a thickness of 300 μm or less. The wavelength conversion member 81 shown in the figure is provided so as to surround the linear conductive film 81. 3 surrounds the wavelength conversion portion 811 .

[0061] It is preferable that the conductive film 813 is in a thin line shape and surrounds the wavelength conversion portion 811. For example, when viewed from below, the line width is smaller than the width of the wavelength converting portion 811, and the line length is 11. In addition, for example, the line width is the width of the wavelength conversion portion 811. The width of the wavelength conversion portion 811 here may be, for example, a rectangular shape. For example, if the external shape is an ellipse, it is the width of the minor axis. In the case of the other shapes, the width is substantially specified based on these examples.

[0062] The conductive film 813 can be formed using an oxide. An example of the oxide is ruthenium oxide (RuO2). Compared to metal materials such as gold, silver, and aluminum, it is brittle and prone to cracking.

[0063] In addition, the conductive film 813 is not transparent and is a colored film. Here, the term "light-shielding" means that the transmittance of visible light is 60% or less. The conductive film 813 has a property of absorbing visible light. The conductive film 813 made of ruthenium is black in color and therefore absorbs light and blocks light. It has sexuality.

[0064] In addition to ruthenium oxide, other oxides that can be used for the conductive film include ruthenium oxide. In comparison with indium tin oxide, ruthenium oxide is In this respect, the resistance change due to temperature or humidity is excellent. explain.

[0065] Figure 13 shows the temperature [℃] when ruthenium oxide was annealed, and the time The sheet resistance [Ω / □] of ruthenium oxide was measured after the experiment. A ruthenium oxide film with a thickness of 200 nm was formed by sputtering, and then exposed to the atmosphere. After annealing for one hour under ambient temperature, the specimen was returned to room temperature (approximately 25°C) and then The sheet resistance was measured using a surface resistivity meter Loresta-GP manufactured by Epson Corporation. The temperature at which the test was carried out was changed from 100°C to 500°C in increments of 100°C. The sheet resistance at 100 nm was measured.

[0066] From the results in Figure 13, the sheet resistance of ruthenium oxide increases with the temperature applied to the ruthenium oxide. It can be seen that the sheet resistance changes depending on the temperature of the heat treatment. It can also be seen that the temperature range of 300℃ to 500℃ is higher than that of 100℃ to 300℃. It can be seen that the amount of change in sheet resistance with respect to temperature is larger in the case of

[0067] Figure 14 shows the results of the measurements of each ruthenium oxide measured in Figure 13, when it was transferred from room temperature to an environment of 160°C. The rate of change [%] in sheet resistance [Ω / □] versus storage time [Hour] when stored in a The experimental results were as follows. In this experiment, the storage time was 0 hours, 10 hours, 50 hours, and 100 The sheet resistance at each time was measured, and the change from the sheet resistance at time 0 was The conversion rate was calculated using the same measuring device as that used in Figure 13.

[0068] From the results in Figure 14, the difference between ruthenium oxide that has not been heat-treated and that has been heat-treated at 100°C is It can be seen that the sheet resistance of the ruthenium oxide that was stored in the SiO2 film changed. The sheet resistance decreases over time, and after a certain time has elapsed, there is almost no change. On the other hand, in the case of ruthenium oxide that was heat-treated at 200°C or higher, It can be seen that the sheet resistance is almost constant regardless of the storage time.

[0069] From these results, it is believed that the heat treatment is performed at a higher temperature than the temperature environment in which ruthenium oxide is placed. Ruthenium oxide has a sheet resistance that remains almost constant even when exposed to that temperature environment for a long period of time. It can also be seen that the heat treatment was not performed or was performed at a lower temperature than that in the temperature environment. When heat-treated ruthenium oxide is left in a temperature environment for a long period of time, the sheet resistance changes. It is clear that this has been achieved.

[0070] Therefore, taking into consideration the environment in which the conductive film 813 of ruthenium oxide is used, The conductive film 813 that has been heat-treated at a temperature higher than the temperature at which it is used is thermally This results in a conductive film with excellent resistance change to the applied voltage.

[0071] Whether or not to perform heat treatment and at what temperature to perform heat treatment depend on the environment in which the conductive film 813 is used. The temperature range of the expected operating environment should be determined appropriately. It is sufficient to perform heat treatment on the conductive film 813 at a temperature exceeding the maximum temperature in the thermal treatment.

[0072] When the heat treatment is performed, the step of providing the conductive film 813 on the base material of the wavelength conversion member 81 is A process of forming a conductive film 813 on the base material of the member 81 and a process of subjecting the formed conductive film 813 to a heat treatment. In the step of forming the conductive film 813, for example, a sputtering process is used. In the step of performing heat treatment on the conductive film 813, for example, The heat treatment can be carried out using a annealing process.

[0073] In addition, in the process of forming the conductive film 813, for example, a film having a thickness of 100 nm or more and 400 nm or less is formed. In the step of subjecting the conductive film 813 to a heat treatment, for example, Considering the usage environment of the wavelength conversion member 81 in the illustrated light emitting device 1, the temperature is set to 100° C. or higher. It is possible to use ruthenium oxide that has been heat-treated at temperatures above 300°C. It is possible to adopt ruthenium oxide that has been heat-treated at a temperature below 1000° C.

[0074] As an example of a preferable conductive film 813, when it is moved from room temperature to an environment of 100° C. Conductive films with a sheet resistance change rate of less than 3% after storage for 50 or 100 hours In addition, another exemplary preferred conductive film 813 is a conductive film that can withstand 5000 ℃ at 100℃. Conductive films with a sheet resistance change rate of less than 2% when stored for 0 or 100 hours are listed. In addition, as another exemplary preferred conductive film 813, a conductive film that has been annealed for 50 hours in an environment of 200° C. The conductive film has a sheet resistance change rate of less than 3% when stored for 100 hours or for 100 hours. In addition, another exemplary preferred conductive film 813 is a film that has been annealed in an environment of 200° C. for up to 50 hours. or a conductive film whose sheet resistance changes by less than 2% when stored for 100 hours. .

[0075] FIG. 15 shows the thermal conductivity of ruthenium oxide and indium tin oxide in various environments from room temperature to high temperature and high humidity. The rate of change in wiring resistance [Ω] over storage time [Hours] when the device is moved to a lower temperature and stored in a cool, dark place. The high temperature and humidity environment was 85°C and 85% humidity. In addition, the wiring resistance at 0 hours storage time and the wiring resistance at 100 hours storage time were The resistance value was measured, and the rate of change from the wiring resistance at time 0 was calculated.

[0076] In addition, in this experiment, ruthenium oxide and indium oxide with uniform shapes (width, thickness, length) were used. Specifically, the width is 200 μm, the thickness is 100 μm, and the thickness is 10 μm. A linear conductive film 813 was used. Ruthenium oxide and indium tin oxide were used. Ten samples were prepared, and the average resistance change rate of the ten samples was measured and shown in Figure 15. .

[0077] In this experiment, ruthenium oxide was annealed at 300°C and 500°C. Annealed indium tin oxide was used. The annealing process gives the conductive film made of indium tin oxide a transparent property. This is the process for that purpose.

[0078] From the results in Figure 15, almost no resistance change was observed for ruthenium oxide, but In particular, the resistance change of ruthenium oxide was several percent. The resistance change rate of the 10 specimens was in the range of 0.2% to 0.5%, and the resistance change rate of the indium oxide The resistance change rate of the ten samples was in the range of 2.6% to 3.8%.

[0079] The measurements were continued even after 100 hours had passed. Even after 0 hours, the resistance continues to rise monotonically, and even now, more than 400 hours have passed. It continues to rise.

[0080] These results show that when the environment changes from room temperature to high temperature and humidity, indium tin oxide oxidizes. It can be said that this material is more susceptible to changes in wiring resistance than ruthenium. Conductive films with better resistance changes to temperature or humidity than indium tin conductive films are It can be seen that this can be achieved by using a conductive film of tungsten.

[0081] As an example of a preferable conductive film 813, a high temperature and high humidity environment having a temperature of 85° C. to a humidity of 85% is used. When stored in a cool, dark place for 100 hours, the change in wiring resistance is 2.5% or less. In addition, an exemplary more preferable conductive film 813 is a conductive film that can be formed at room temperature to a temperature Wiring resistance when stored for 100 hours in a high temperature and humidity environment of 85°C and 85% humidity A conductive film having a rate of change of 1.5% or less is also an example of a more preferable conductive film. As the film 813, the film was transferred from room temperature to a high-temperature and high-humidity environment of 85°C and 85% humidity for 10 minutes. The conductive film has a change rate of wiring resistance of 0.5% or less when stored for 0 hours.

[0082] In the wavelength conversion member 81, a plurality of metal films 814 are provided on the surface on which the conductive film 813 is provided. A plurality of metal films 814 are provided on the surrounding portion 812. 14 is provided on the outside of the wavelength converting portion 811. The conductive film 813 and the two metal films 814 connected to each other are included. 4 are not connected to each other.

[0083] In a plan view seen from the surface on which the conductive film 813 is provided, One end of the conductive film 813 overlaps with one of the two metal films 814. The metal film 814 is made of, for example, Ti / Pt / Au. It can be formed.

[0084] (Translucent member 82) The light-transmitting member 82 has a lower surface, an upper surface, and a side surface. Here, the term "transparent" refers to a light transmittance of 80% or more. The light-transmitting member 82 has a base material formed in a rectangular parallelepiped flat plate shape. The shape is not limited to a rectangular parallelepiped.

[0085] The base material of the light-transmitting member 82 can be formed by using sapphire as the main material. Ear is a material with relatively high transmittance and strength. Other than ear, for example, quartz, silicon carbide, or glass may also be used.

[0086] The light-transmitting member 82 has a plurality of metal films 821. The metal films 821 are provided on the upper surface side of the light-transmitting member 82. The two metal films 821 are disposed on the outer peripheral area of ​​the light-transmitting member 82. The two metal films 821 are not provided in the central region of the light-transmitting member 82.

[0087] The two metal films 821 have a junction region in part. It can be formed by providing Ti / Pt / Au. Also, in the junction region, for example, AuSn can be further provided thereon to form the layer.

[0088] (Light blocking member 90) The light blocking member 90 is made of a resin having light blocking properties. It has the property of blocking light, absorbing light, reflecting light, etc. For example, a filler such as a light diffusing material and / or a light absorbing material may be added to the resin. It can be formed by containing

[0089] The resin for forming the light blocking member 90 may be an epoxy resin, a silicone resin, or an acrylate. Resin, urethane resin, phenolic resin, BT resin, etc. Also, light absorbing fluorine The filler may be a dark color pigment such as carbon black.

[0090] (Light emitting device 1) Next, the light emitting device 1 manufactured using these components will be described. First, two light reflecting members 40 are disposed on the bottom surface 12 of the base 10. 0 are disposed on different metal films, and their lower surfaces are bonded to the bottom surface 12 of the base 10. Moreover, the two light reflecting members 40 are disposed symmetrically with respect to the point SP (see FIG. 7). In addition, the two light reflecting members 40 are arranged such that the upper ends of the light reflecting surfaces 41 are in contact with the inner surface 1 of the base 10 when viewed from above. 4 or parallel or perpendicular to the outer surface 15.

[0091] Next, the protection element 50 and the temperature measuring element 60 are disposed on the bottom surface 12 of the base 10. The element 50 is disposed on the metal film on which one of the two light reflecting members 40 is disposed, and is connected to the metal film. The temperature measuring element 60 is made of a metal different from the metal film on which the two light reflecting members 40 are arranged. The membrane is placed on top of and bonded to the metal membrane.

[0092] Next, two submounts 30 are placed on the bottom surface 12 of the base 10. The electrodes 30 are disposed on different metal films, and their lower surfaces are bonded to the bottom surface 12 of the base 10. In addition, each of the two submounts 30 has a gold substrate on which a light reflecting member 40 is disposed. The submount 30 and the light reflecting member 40 are disposed on different metal films. It may be possible.

[0093] Next, the light emitting element 20 is placed on the submount 30. In the illustrated example of the light emitting device 1, The semiconductor laser element 20 is disposed on a submount 30. In addition, the two semiconductor laser elements The submounts 20 are disposed on the upper surfaces of different submounts 30, and their lower surfaces are bonded to each other. The two semiconductor laser elements 20 are arranged symmetrically with respect to the point SP. A point where the two semiconductor laser elements 20 are symmetrical, a point where the two light reflecting members 40 are symmetrical, is in the same position. In the following explanation, this point SP will be called the symmetric point.

[0094] The two semiconductor laser elements 20 have their emission end faces aligned with the inner surface 14 of the base 10 or The outer surface 15 is not parallel or perpendicular to the outer surface 15. Therefore, the upper end of the light reflecting surface 41 is not parallel or perpendicular to the outer surface 15. That is, the semiconductor laser element 20 is not perpendicular to the inner surface 14 of the base 10 and the The light emitting end surface is arranged so as to be inclined with respect to the outer surface 15 or the upper end of the light reflecting surface 41. can be.

[0095] Instead of disposing the semiconductor laser element 20 at an angle, the light reflecting member 40 is disposed at an angle. That is, the semiconductor laser element 20 may be provided on the inner surface 14 of the base 10 or The light reflecting member 40 is arranged parallel or perpendicular to the outer surface 15 so as not to be parallel or perpendicular to the outer surface 15. may be placed in

[0096] The light emitted from the output end face of each of the two semiconductor laser elements 20 is divided into corresponding light The light is irradiated onto the reflecting member 40. The corresponding light reflecting member 40 is disposed on the same metal film. The light reflecting member 40 is a semi-transparent member having a semi-transparent surface 41. The semiconductor laser element 20 is disposed.

[0097] In addition, between the corresponding semiconductor laser element 20 and the light reflecting member 40, The semiconductor laser element 20 is located farther from the symmetrical point than the semiconductor laser element 20. The light emitted from the light emitting element 20 advances in a direction approaching the symmetric point. At least one of them is disposed in a position close to the temperature measuring element 60. The temperature can be measured well.

[0098] The submount 30 on which the light emitting element 20 is disposed is a light emitting device 1. The submount 30 serves as a heat dissipation member that dissipates the generated heat. In order to make it function as a heat sink, it is necessary to form it from a material having a higher thermal conductivity than the light emitting element 20. If the base is made of a material with a higher thermal conductivity than the bottom surface of the base, a higher heat dissipation effect can be obtained. Cut.

[0099] In addition, the submount 30 is disposed at the light emitting position of the semiconductor laser element 20 in the light emitting device 1. For example, the light passing through the optical axis can be adjusted so that it is parallel to the bottom surface 12. In addition, when it is desired to irradiate a specific position on the light reflecting surface 41, the submount can be adjusted. Used as a component.

[0100] Next, in order to electrically connect the light emitting element 20, the protective element 50, and the temperature measuring element 60, The plurality of wirings 70 (first wirings 71) are joined to the bottom surface 1 of the base 10. 2. This allows the metal film on the upper surface 11 of the base 10 to be These elements can be electrically connected to an external power source.

[0101] Next, the optical member 80 is placed. In the illustrated example of the light emitting device 1, the optical member 80 is Thus, an optical member 80 in which a wavelength conversion member 81 and a light-transmitting member 82 are joined together is prepared. In addition, the metal film 814 of the wavelength conversion member 81 and the metal film 821 of the light-transmitting member 82 are electrically The wavelength conversion member 81 and the light-transmitting member 82 are joined together to form a The optical member 80 is then formed.

[0102] The optical member 80 is disposed on the upper surface of the base 10. In addition, the lower surface of the optical member 80 is The optical member 80 is bonded to the upper surface of the step portion 16 of the base portion 10. The member 80 is bonded to the upper surface of the first step portion 161. Material 82 joins with base 10 .

[0103] The optical member 80 is bonded to the base 10 to form a closed space in which the semiconductor laser element 20 is disposed. In this way, in the light emitting device 1, the optical member 80 serves as a lid member. In addition, the closed space is formed in an airtight sealed state. This makes it possible to prevent organic matter and the like from collecting on the light emitting end face of the semiconductor laser element 20.

[0104] A major portion of the light emitted by the light emitting element 20 is incident on the optical member 80. The light is incident on the wavelength conversion member 81 of the optical member 80. The light is incident on the light source 80. The light is also transmitted through the light-transmitting member 82 of the optical member 80. After being transmitted, the light enters the wavelength conversion section 811 .

[0105] The wavelength conversion member 81 has a light entrance area on its lower surface where the main part of the light is incident, and The surface of the wavelength conversion member 81 that includes the light incidence region is a surface of the light emitting element 2. It can be said to be the incident surface where light from 0 enters.

[0106] In the wavelength conversion member 81, the wavelength conversion portion 811 forms a light entrance region, and the surrounding portion 8 The peripheral region is not limited to the embodiment in which the peripheral region is formed by the surrounding portion 812. For example, the size of the wavelength converting portion 811 may be increased, and the lower surface of the wavelength converting portion 811 may be For example, the side surface of the wavelength conversion unit 811 may include a light entrance area and a peripheral area. In the wavelength conversion member that does not have the surrounding portion 812, the lower surface of the wavelength conversion portion 811 is provided with a light entrance region. The surrounding area is included.

[0107] A part or all of the light incident on the wavelength conversion section 811 is converted into a different wavelength by the wavelength conversion section 811. The light from the light emitting element 20 or the wavelength-converted light is converted into light of a wavelength corresponding to the wavelength of the light. The light is emitted to the outside of the light emitting device 1 from the upper surface of the wavelength conversion section 811. This serves as the light extraction surface of the light emitting device 1 .

[0108] In addition, if the heat generated by the wavelength conversion is concentrated at a specific location, the light from the wavelength conversion unit 811 may be reduced. Since the conversion efficiency is likely to decrease, it is better for the distribution of light incident on the wavelength conversion section 811 to be diffused. For example, the light intensity of the laser light emitted from each of the two semiconductor laser elements 20 is For example, the light reflecting surface 41 of the light reflecting member 40 is adjusted so that the light reflecting surface 41 does not overlap with the light reflecting surface 41. Such control is possible by adjusting the

[0109] In the optical member 80, the light-transmitting member 82 and the wavelength conversion member 81 are joined together. In addition, the wavelength conversion member 81 is bonded to the upper surface of the light-transmitting member 82. The surrounding portion 812 and the light-transmitting member 82 are joined together. 4 and the metal film 821 of the light-transmitting member 82 are joined. The bonding area of ​​the metal film 821 of the light-transmitting member 82 is bonded to 814 .

[0110] The conductive film 813 is a thin linear film that surrounds the wavelength conversion section 811 in the vicinity thereof. Therefore, if an abnormality such as a crack occurs in the wavelength conversion portion 811, the conductive layer 814 will respond to the shock. The electrical connection state is changed by cracking the conductive film 813. By detecting the rise, an abnormality in the wavelength conversion unit 811 can be detected.

[0111] For this reason, the conductive film 813 serves as a sensor for detecting an abnormality in the wavelength conversion unit 811. The wavelength conversion unit 811 can be said to be a detection element. Also, the wavelength conversion unit 811 detects an abnormality by the abnormality detection element. Similarly, the light incidence area can be called the detection target area. .

[0112] The conductive film 813 is made of oxide, which is brittle and easily broken compared to metal materials. This can improve the accuracy of detecting damage to the wavelength conversion unit.

[0113] The conductive film 813 is disposed on the incident surface of the wavelength conversion member 81 on which the light from the light emitting element 20 is incident. The conductive film 813 is provided on the side of the wavelength conversion member 81 facing the light-transmitting member 82. Therefore, the light-transmitting member 82 is provided on the side where the conductive film 813 is provided. 3 or in contact with the conductive film 813.

[0114] When the temperature of the wavelength conversion portion 811 rises, the temperature of the conductive film 813 also rises. When high-power light is incident on the portion 811, the resistance of the conductive film 813 increases, and the measured resistance If the resistance change due to heat is large, the abnormality detection may malfunction. As shown by the experimental results in Figs. 13 to 15, the conductive film 8 formed of ruthenium oxide 13 can suppress such malfunctions.

[0115] The conductive film 813 is a narrow film sandwiched between the base material of the wavelength conversion member 81 and the light-transmitting member 82. Since the conductive film 813 is disposed in space, the temperature of the conductive film 813 follows the temperature of the wavelength converting portion 811. Considering the environment in which the conductive film 813 is used, the wavelength conversion The member 81 is preferably provided with a conductive film 813 that has been subjected to a heat treatment.

[0116] In addition, for conductive films of the same size and shape, the lower the sheet resistance of the conductive film, the higher the wiring resistance. When used for abnormality detection, if the wiring resistance is too low, the change in resistance will be small and the detection Taking this into consideration, the light emitting device 1 shown in the figure is heated to, for example, 100° C. or higher. It is preferable to use a conductive film 813 of ruthenium oxide that has been annealed at a temperature of 300° C. or less. For example, ruthenium oxide annealed at a temperature of 150° C. to 300° C. It is more preferable to use a conductive film 813 made of a fluorine-based material.

[0117] The conductive film 813 is not provided directly under the light incidence region. 21 is not provided directly under the light incidence area. This allows the light to enter the wavelength converting section 811 without being blocked by the light emitting section 3 .

[0118] In addition, the bonding area of ​​the metal film 821 of the light-transmitting member 82 is the same as that of the metal film 814 of the wavelength conversion member 81. The metal film 821 of the light-transmitting member 82 is located in a region where the conductive film 813 is provided. Therefore, by providing the conductive film 813 having a light-shielding property, the wavelength conversion The conductive film 813 can block light incident on the outside of the switching portion 811. The transmittance of the light emitted from the

[0119] The upper surface of the light-transmitting member 82 is larger than the lower surface of the wavelength conversion member 81. In plan view, the upper surface of the light-transmitting member 82 surrounds the lower surface of the wavelength conversion member 81. The light-transmitting member 82 is surrounded by two metal films 821 on the upper surface of the light-transmitting member 82. The length changing member 81 is provided from an area overlapping with the lower surface of the length changing member 81 to an area where the length changing member 81 does not overlap with the lower surface of the length changing member 81 .

[0120] Next, the wiring 70 (second wiring 72) for electrically connecting the anomaly detection element is joined. For electrical connection, a metal film provided on the second step portion 162 of the base portion 10 and the optical member 80 are provided. The second wiring 72 has one end connected to the metal film on the upper surface of the light-transmitting member 82. The other end is joined to the metal film on the upper surface of the second step portion 162. The anomaly detection element can be electrically connected to an external power source via the metal film on the upper surface 11 of the semiconductor device. Cut.

[0121] Next, the light-shielding member 90 is formed inside the frame formed by the upper surface 11 of the base 10. The light blocking member 90 is formed so as to fill the gap between the base 10 and the wavelength conversion member 81. The insulating layer 0 can be formed, for example, by pouring in a thermosetting resin and curing it with heat. By providing the optical member 90, leakage of light from other than the light extraction surface is suppressed.

[0122] The light blocking member 90 is disposed on the inner surface 14 intersecting with the upper surface 11 of the base 10 and on the step portion 16 of the base 10. the surface of the light-transmitting member 82, the side surface of the light-transmitting member 82, the upper surface of the light-transmitting member 82, and the side surface of the wavelength conversion member 81. Also, it does not reach the upper surface of the wavelength conversion member 81. Even if it does reach the upper surface of the wavelength conversion portion 811, it does not reach the upper surface of the wavelength conversion portion 811. The light blocking member 90 can be provided so as to fill the gap while avoiding the length changing portion 811. .

[0123] In addition, in forming the light blocking member 90, the resin is used to form the light transmitting member 82 and the wavelength converting member 81. The light may enter the gap, but does not reach the bottom surface of the wavelength conversion unit 811. 2, the second wiring 72 is enclosed therein. That is, when the light blocking member 90 is formed, Therefore, the second wiring 72 is not exposed. This protects the second wiring 72 from adhesion of water droplets, etc. However, it does not necessarily have to be contained within.

[0124] The light shielding member 90 is a metal area exposed inside the frame formed by the upper surface 11 of the base 10 when viewed from above. In the light emitting device 1, the light blocking member 90 is made of an insulating material. It serves as an insulating material. This allows the abnormality detection mechanism to function properly. In addition, a conductive area for supplying power to the light emitting device 1 from an external power source can be provided on the base 1. It can be limited to the outside of a concave depression of 0.

[0125] As explained above, the present invention having the technical features disclosed in the specification is For example, the present invention is not limited to the structure described in the embodiment. The present invention can also be applied to a light emitting device having elements, and the disclosed structure is different. The existence of such a problem does not constitute a reason for not being able to apply the present invention.

[0126] This means that all the components of the light emitting device disclosed in the embodiment are necessary and sufficient. This shows that the present invention can be applied even if the above is not essential. For example, Some components of the light emitting device disclosed in the embodiments are described in the claims. If not, the component may be replaced, without being limited to those disclosed in this embodiment. Allowing freedom of design by those skilled in the art, such as omissions, deformation of shapes, and changes in materials, It is claimed that the invention described in the claims applies. [Industrial Applicability]

[0127] The optical member or the light emitting device according to the embodiment is used in an in-vehicle headlight, a lighting device, a projector, etc. Used as a light source for backlights in displays, head mounted displays, and other displays. This can be used in optical systems in which [Explanation of symbols]

[0128] 1 Light emitting device 10 base 11 Top side 12 Bottom 13 Bottom side 14 Inner surface 15 External surface 16 Step 161 First step 162 Second step 20 Light emitting element 30 Submount 40 Light reflecting member 41 Light reflective surface 411 1st reflective surface 412 Second reflective surface 50 Protection element 60 Temperature measuring element 70 Wiring 71 1st wiring 72 2nd wiring 80 Optical Components 81 Wavelength conversion material 811 Wavelength conversion unit 812 Encirclement 813 Conductive film 814 Metal Film 82 Translucent material 821 Metal Film 90 Light-shielding material

Claims

1. A light-emitting element; a wavelength conversion member including: a wavelength conversion unit that converts light emitted from the light emitting element into light of a different wavelength and emits the light to the outside; an enclosure that surrounds the wavelength conversion unit; and a conductive film that is provided on the enclosure and surrounds the wavelength conversion unit; having The conductive film is formed using ruthenium oxide that has been annealed at a predetermined temperature.

2. A light-emitting element; a wavelength conversion member including: a wavelength conversion unit that converts light emitted from the light emitting element into light of a different wavelength and emits the light to the outside; an enclosure that surrounds the wavelength conversion unit; and a conductive film that is provided on the enclosure and surrounds the wavelength conversion unit; having The conductive film is annealed at a predetermined temperature, is an oxide, and has a change in wiring resistance of 2.5% or less when stored for 100 hours in a high-temperature, high-humidity environment of 85°C and 85% humidity from room temperature.

3. A light-emitting element; A wavelength conversion unit that converts the light emitted from the light emitting element into light of a different wavelength and emits the light to the outside. a wavelength converting member including: an enclosure portion that surrounds a side surface of the wavelength converting portion; and a conductive film that is disposed in the enclosure portion and surrounds the wavelength converting portion; having The conductive film is annealed at a predetermined temperature, and has a transmittance of 60% or less for the light emitted from the light-emitting element. Furthermore, the light-emitting device has a change in wiring resistance of 2.5% or less when stored for 100 hours in a high-temperature, high-humidity environment at a temperature of 85°C and a humidity of 85% from room temperature.

4. 4 . The light emitting device according to claim 1 , wherein the enclosure is unable to convert light emitted from the light emitting element into light having a different wavelength and emit the converted light to the outside.

5. A light-emitting element; a wavelength conversion member including a wavelength conversion portion on which a main portion of light from the light emitting element is incident, and a conductive film surrounding the area on the outside of the area on which the main portion of light from the light emitting element is incident; having The conductive film is annealed at a predetermined temperature, and has a transmittance of 60% or less for the light emitted from the light-emitting element. Furthermore, the light-emitting device has a change in wiring resistance of 2.5% or less when stored for 100 hours in a high-temperature, high-humidity environment at a temperature of 85°C and a humidity of 85% from room temperature.

6. A light-emitting element; a wavelength conversion member including: a wavelength conversion unit that converts light emitted from the light emitting element into light of a different wavelength and emits the light to the outside; an enclosure that surrounds the wavelength conversion unit; and a conductive film that is provided on the enclosure and surrounds the wavelength conversion unit; having The light emitting device, wherein the conductive film has a substantially constant rate of change in sheet resistance when stored in an environment of 160° C. for a storage time of 10 hours or more.

7. 7. The light emitting device according to claim 1, wherein the conductive film is an abnormality detection element that detects whether or not an abnormality such as a breakage has occurred in the wavelength conversion portion.

8. the wavelength conversion unit has an incident surface onto which light from the light emitting element is incident, The light emitting device according to claim 1 , wherein the conductive film is provided on the light incident surface side.

9. The light emitting device according to claim 1 , wherein the wavelength converting member further comprises a metal film disposed outside the wavelength converting portion and electrically connected to the conductive film.

10. Further comprising a light-transmitting member connected to the wavelength conversion member, The light emitting device according to claim 1 , wherein the conductive film is provided on a side of the wavelength conversion member facing the light transmissive member.

11. The light emitting device according to claim 10 , wherein the conductive film is not in contact with the light-transmitting member.

12. The light emitting device according to claim 1 , wherein the predetermined temperature is 150° C. or higher.

13. 6. The light emitting device according to claim 1, wherein the predetermined temperature is a temperature that exceeds a maximum temperature in a temperature range of an assumed environment in which the conductive film is used.

14. A base material having a wavelength converting portion that outputs light having a wavelength different from that of incident light and an enclosure portion that surrounds a side surface of the wavelength converting portion; a conductive film disposed on an upper surface or a lower surface of the surrounding portion and surrounding the wavelength converting portion; The conductive film is an optical component formed using ruthenium oxide that has been annealed at a predetermined temperature.

15. A base material having a wavelength converting portion that outputs light having a wavelength different from that of incident light and an enclosure portion that surrounds a side surface of the wavelength converting portion; a conductive film disposed on an upper surface or a lower surface of the surrounding portion and surrounding the wavelength converting portion; The conductive film is annealed at a predetermined temperature, is an oxide, and has a sheet resistance change rate of less than 3% when moved from room temperature to an environment of 100°C and stored for 50 hours or 100 hours.

16. A base material having a wavelength conversion portion that emits light having a wavelength different from that of incident light; a conductive film surrounding a predetermined region of the base material; The conductive film is an optical component that has been annealed at a predetermined temperature, has a visible light transmittance of 60% or less, and has a sheet resistance change rate of less than 3% when stored in an environment of 100°C from room temperature for 50 hours or 100 hours.

17. 17. The light emitting device according to claim 14, wherein the predetermined temperature is 150[deg.] C. or higher.

18. 17. The light emitting device according to claim 14, wherein the predetermined temperature is a temperature that exceeds a maximum temperature in a temperature range of an assumed environment in which the conductive film is used.

19. A base material having a wavelength converting portion that outputs light having a wavelength different from that of incident light and an enclosure portion that surrounds a side surface of the wavelength converting portion; a conductive film disposed on an upper surface or a lower surface of the surrounding portion and surrounding the wavelength converting portion; The conductive film has a substantially constant rate of change in sheet resistance when stored in an environment of 160° C. for a storage time of 10 hours or more.

Citation Information

Patent Citations

  • Semiconductor laser drive circuit

    JP1999214777A

  • Light-emitting device

    JP2019175903A

  • Optical member and light emitting device

    JP2019117827A