Pellicle frame, pellicle, exposure original plate with pellicle, exposure method, and method for manufacturing semiconductor
A ductile metal pellicle frame with cutouts and ventilation holes addresses the challenge of EUV pellicle durability under pressure changes and peeling, improving the manufacturing process for semiconductors and liquid crystal display panels.
Patent Information
- Application Number
- JP2024127953
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-06-08
- Filing Date
- 2024-08-02
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2041-05-27
AI Technical Summary
EUV pellicles face challenges in withstanding pressure changes from atmospheric pressure to vacuum without being damaged, and are prone to damage during peeling due to lack of ductility in ceramic materials, making them difficult to process without increasing thickness.
A pellicle frame made of ductile metal with cutouts and ventilation holes to manage pressure changes and reduce damage during peeling, featuring a total ventilation area of 1 mm³ per 0.001mm², with notches and through holes for enhanced durability.
The pellicle frame minimizes damage during pressure changes and peeling, ensuring high workability and suitability for EUV exposure, enhancing the manufacturing process of semiconductors and liquid crystal display panels.
Smart Images

Figure 2024150755000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a pellicle frame that is attached to a lithography photomask to protect against foreign matter, a pellicle, an exposure master plate with a pellicle, an exposure method, a semiconductor manufacturing method, and a liquid crystal display panel manufacturing method. [Background technology]
[0002] In recent years, LSI design rules have been miniaturized to the sub-quarter micron level, and as a result, the wavelength of exposure light sources has been shortened. That is, exposure light sources have shifted from g-line (436 nm) and i-line (365 nm) from mercury lamps to KrF excimer lasers (248 nm) and ArF excimer lasers (193 nm), and furthermore, EUV exposure using EUV (Extreme Ultra Violet) light with a dominant wavelength of 13.5 nm is being considered.
[0003] In the manufacture of semiconductors such as LSIs and VLSIs, or liquid crystal display panels, patterns are created by irradiating light onto semiconductor wafers or liquid crystal originals. However, if foreign matter is attached to the lithography photomasks and reticles (collectively referred to below as "exposure originals") used in this case, the foreign matter can absorb or bend the light, causing deformation of the transferred pattern, rough edges, and black staining of the base, impairing the dimensions, quality, appearance, etc.
[0004] These operations are usually carried out in a clean room, but it is still difficult to keep the exposure master clean at all times. Therefore, a method is generally adopted in which a pellicle is attached to the surface of the exposure master to prevent foreign matter before exposure. In this case, foreign matter does not adhere directly to the surface of the exposure master, but adheres to the pellicle, so if the focus is set on the pattern of the exposure master during lithography, the foreign matter on the pellicle will not be involved in the transfer.
[0005] The basic structure of this pellicle is that a pellicle film with high transmittance to the light used for exposure is stretched on the upper end surface of a pellicle frame made of aluminum, titanium, etc., and an airtight gasket is formed on the lower end surface. The airtight gasket generally uses an adhesive layer, and a protective sheet is attached to protect this adhesive layer. The pellicle film is made of nitrocellulose, cellulose acetate, fluorine-based polymer, etc., which have high transmittance to the light used for exposure (g-line (436 nm) from a mercury lamp, i-line (365 nm), KrF excimer laser (248 nm), ArF excimer laser (193 nm), etc.), but for EUV exposure, ultrathin silicon film and carbon film are being considered as pellicle films.
[0006] In addition, since EUV exposure is performed in a vacuum, the EUV pellicle must be able to withstand the pressure change from atmospheric pressure to vacuum, and the EUV pellicle is required to have a large ventilation area.
[0007] Therefore, Patent Document 1 proposes a pellicle having a pellicle frame in which two opposing side surfaces of the pellicle frame are each provided with vent holes with an open area ratio of 50 to 90% relative to the other side surface. However, what affects the pressure change inside and outside the pellicle is the ventilation area relative to the internal space volume of the pellicle, and it is insufficient to discuss this only in terms of the open area ratio of the pellicle frame.
[0008] In addition, in Patent Document 2, the total flow area of the through holes provided in the ceramic frame is less than 1 cm of the volume of the internal space of the pellicle. 3 0.005cm per 2 We have proposed a pellicle frame as described above. However, in the case of ceramic, since the material is not ductile, it has been found that if a strong force is applied locally to the pellicle frame, such as when peeling off the pellicle, the pellicle frame may break and generate foreign matter. In order to give the pellicle frame strength, it is generally sufficient to make the pellicle frame thicker, but since the maximum height of EUV pellicles is limited to 2.5 mm, it is difficult to prevent breakage by making the pellicle frame thicker. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] JP 2004-294786 A [Patent Document 2] JP 2018-200380 A Summary of the Invention [Problem to be solved by the invention]
[0010] The present invention has been made in consideration of the above circumstances, and has an object to provide a pellicle that can withstand the pressure change from atmospheric pressure to vacuum when EUV exposure is performed in a vacuum, is less likely to cause damage to the pellicle film, has good processability for the pellicle frame, and uses a pellicle frame that is less likely to be damaged when the pellicle is peeled off. [Means for solving the problem]
[0011] The present inventors have developed a frame-shaped pellicle frame having an upper end surface on which a pellicle membrane is provided and a lower end surface facing a photomask, and provided a cutout portion from the outer surface to the inner surface of the end surface of the pellicle frame, and set the ventilation area at any of the inner surface, the outer surface, the pellicle internal space side, and the pellicle external space side to 1 mm2 of the volume of the pellicle internal space. 3 0.001mm per 2 It was found that by setting the above, damage to the pellicle membrane during pressure changes can be suppressed. Furthermore, while fine processing is required for the pellicle frame to provide a large number of vents, it was found that using a ductile metal as the material reduces losses due to damage to the pellicle frame during processing, and also reduces the risk of the pellicle frame being damaged when the pellicle is peeled off from the photomask, which led to the present invention.
[0012] Accordingly, the present invention provides the following pellicle frame, pellicle, exposure master plate with pellicle, exposure method, semiconductor manufacturing method, and liquid crystal display panel manufacturing method. 1. A frame-shaped pellicle frame having an upper end surface on which a pellicle film is provided and a lower end surface facing a photomask, the pellicle frame being made of metal, and a cutout portion with an open upper end surface or lower end surface is provided from the outer surface toward the inner surface, and the total ventilation area on the inner surface is within 1 mm of the volume of the internal space of the pellicle. 3 0.001mm per 2 A pellicle frame characterized by the above. 2. A frame-shaped pellicle frame having an upper end surface on which a pellicle film is provided and a lower end surface facing a photomask, the pellicle frame being made of metal, and a cutout portion with an open upper end surface or lower end surface is provided from the outer surface to the inner surface, and the total ventilation area on the inner space side of the pellicle is within 1 mm of the volume of the inner space of the pellicle. 3 0.001mm per 2 A pellicle frame characterized by the above. 3. A frame-shaped pellicle frame having an upper end surface on which a pellicle film is provided and a lower end surface facing a photomask, the pellicle frame being made of metal, and a cutout portion with an open upper end surface or lower end surface is provided from the outer surface to the inner surface, and the total ventilation area on the outer surface is within 1 mm of the volume of the internal space of the pellicle. 3 0.001mm per 2 A pellicle frame characterized by the above. 4. A frame-shaped pellicle frame having an upper end surface on which a pellicle film is provided and a lower end surface facing a photomask, the pellicle frame being made of metal, and a cutout portion with an open upper end surface or lower end surface is provided from the outer surface to the inner surface, and the total ventilation area on the outer space side of the pellicle is within 1 mm of the volume of the inner space of the pellicle. 3 0.001mm per 2 A pellicle frame characterized by the above. 5. The pellicle frame according to any one of 1 to 4 above, wherein a through hole having an opening on at least the inner surface is provided. 6. The pellicle frame according to any one of 1 to 4 above, wherein the metal material of the pellicle frame is selected from the group consisting of titanium, titanium alloys, aluminum and aluminum alloys. 7. The total of the above ventilation areas is the internal volume of the pellicle (1 mm2). 3 0.02mm per 2 5. A pellicle frame according to any one of the above items 1 to 4. 8. A pellicle frame according to any one of 1 to 4 above, wherein the height of the cutout portion is 50% or less of the thickness of the pellicle frame. 9. The pellicle frame according to any one of 1 to 4 above, wherein the thickness of the pellicle frame is 2.5 mm or less. 10. A pellicle comprising a pellicle frame according to any one of 1 to 9 above, and a pellicle membrane provided on the upper end surface of the pellicle frame via a pressure-sensitive adhesive or adhesive. 11. The pellicle according to claim 10, which is used for exposure under vacuum or reduced pressure. 12. A pellicle according to claim 10 or 11, which is used for EUV exposure. 13. A pellicle as described in 10 or 11 above, wherein the height of the pellicle is 2.5 mm or less. 14. A pellicle according to claim 10 or 11, wherein the pellicle membrane is supported by a frame. 15. An exposure master with a pellicle, comprising the pellicle according to 10 above attached to the exposure master. 16. The exposure master with a pellicle according to the above item 15, wherein the exposure master is an exposure master for EUV. 17. An exposure master with a pellicle according to claim 15, which is an exposure master with a pellicle used in EUV lithography. 18. An exposure method comprising exposing using the exposure master with a pellicle according to 15 above. 19. A method for manufacturing a semiconductor, comprising the step of exposing a substrate under vacuum or reduced pressure using the pellicle-attached exposure master described in 15 above. 20. A method for producing a liquid crystal display panel, comprising the step of exposing a substrate under vacuum or reduced pressure using the exposure master with a pellicle as described in 15 above. 21. A method for manufacturing a semiconductor, comprising the step of exposing a substrate to EUV light using the pellicle-attached exposure master described in 15 above. 22. A method for producing a liquid crystal display panel, comprising the step of exposing a substrate to EUV light using the pellicle-attached exposure master described in 15 above. Effect of the Invention
[0013] According to the pellicle frame and pellicle of the present invention, it is possible to provide a pellicle frame and pellicle in which the pellicle film is less likely to be damaged when the pressure changes from atmospheric pressure to vacuum, and which is less likely to be damaged when the pellicle frame is processed or when the pellicle is peeled off. The present invention is particularly useful for pellicles for EUV exposure, and by using the above pellicle, it is extremely useful in a method for manufacturing a semiconductor or liquid crystal display panel which includes a step of exposing a substrate using an exposure master with a pellicle attached. [Brief description of the drawings]
[0014] [Figure 1] 1A and 1B are schematic diagrams showing one embodiment of a pellicle frame of the present invention, in which (A) is a view from the top end surface side, (B) is a view from the long side outer surface side, and (C) is a view from the short side outer surface side. [Diagram 2] 1 is a schematic diagram showing the appearance of the pellicle of the present invention attached to a photomask. [Diagram 3] Schematic diagrams showing another embodiment of the pellicle frame of the present invention, where (A) is a view from the top end surface side, (B) is a view from the long side outer surface side, and (C) is a view from the short side outer surface side. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The present invention will now be described in further detail. 1(A) to (C) show an example of a pellicle frame 1 of the present invention, where reference numeral 11 denotes the inner surface of the pellicle frame, reference numeral 12 denotes the outer surface of the pellicle frame, reference numeral 13 denotes the upper end surface of the pellicle frame, and reference numeral 14 denotes the lower end surface of the pellicle frame. A cutout portion 20 is provided in the upper end surface of the pellicle frame 1, reference numeral 21 denotes the width of the cutout portion, reference numeral 22 denotes the depth of the cutout portion, and reference numeral 23 denotes the height of the cutout portion. Furthermore, the pellicle frame 1 is provided with a plurality of through holes 30. Note that a tool hole used to peel the pellicle from the photomask is usually provided on the long side of the pellicle frame, but is not shown in FIG. 1.
[0016] 2 shows a photomask 10 with a pellicle attached to a photomask, in which a pellicle film 2 is attached or adhered to and stretched over the upper end surface of a pellicle frame 1 with a pressure sensitive adhesive or bonding agent 4. In addition, a photomask 3 is removably adhered or adhered to the lower end surface of the pellicle frame 1 with a pressure sensitive adhesive or bonding agent 5, thereby protecting the pattern surface on the photomask 3.
[0017] As shown in FIG. 1, the pellicle frame of the present invention is a frame-shaped pellicle frame having an upper end surface on which a pellicle membrane is provided and a lower end surface facing a photomask.
[0018] If the pellicle frame is frame-shaped, its shape corresponds to the shape of the photomask to which the pellicle is attached. In general, it is a quadrilateral (rectangular or square) frame. The shape of the corners (edges) of the pellicle frame may be angular (pointed) as it is, or may be chamfered with R-chamfering or C-chamfering to form a curved shape or other shape.
[0019] The pellicle frame also has a surface for providing a pellicle membrane (here, the upper end surface) and a surface that faces the photomask when the photomask is attached (here, the lower end surface).
[0020] As shown in FIG. 2, a pellicle film is attached to the upper end surface of the pellicle frame via an adhesive or the like, and a pressure sensitive adhesive or the like is provided on the lower end surface for attaching the pellicle to a photomask, but this is not limited to the above.
[0021] The material of the pellicle frame is preferably a ductile metal. Furthermore, since EUV exposure requires higher precision than ArF exposure, the flatness requirements for the photomask are stricter. It is known that the flatness of the photomask is affected by the pellicle. In order to minimize the effect of the pellicle on the photomask, it is preferable to use lightweight titanium, titanium alloys, aluminum, or aluminum alloys.
[0022] The dimensions of the pellicle frame are not particularly limited, but when the height of the EUV pellicle is limited to 2.5 mm or less, the thickness of the EUV pellicle frame is smaller than that, and is preferably 2.5 mm or less. In particular, the thickness of the EUV pellicle frame is preferably 1.5 mm or less, taking into account the thickness of the pellicle film, photomask adhesive, etc. Also, the lower limit of the thickness of the pellicle frame is preferably 1.0 mm or more.
[0023] In the pellicle frame of the present invention, a cutout portion with an open upper end surface or lower end surface is provided from the outer surface toward the inner surface. That is, the cutout portion means a recess (concave portion) provided on the upper end surface or lower end surface of the pellicle frame and connected from the outer surface to the inner surface. For example, as shown in Figs. 1(B) and (C), the cutout portion 20 has a substantially U-shaped recess when viewed from the outer surface of the pellicle frame. The substantially U-shaped recess includes a shape in which the corners are sharpened and cut into a square shape, as well as a shape in which the corners are rounded. Also, as shown in Fig. 1(A), the cutout portion 20 has a recess formed with the same width from the outer surface toward the inner surface when viewed from the top, but is not limited to this, and may have a tapered shape that gradually narrows or widens from the outer surface toward the inner surface. Furthermore, the height of the cutout portion in the height direction (see reference numeral 23 in FIG. 1) is not limited to being uniform from the outer surface to the inner surface, but may be tapered so as to gradually expand or contract. There is no particular limitation on the location or number of the cutout portions.
[0024] In addition, the cutout portion is not particularly limited in terms of its shape or dimensions, but if the height of the cutout portion (reference numeral 23 in FIG. 1) is increased, the thickness of the pellicle frame below the cutout portion is accordingly reduced, and when the pellicle is peeled off, the pellicle frame is bent from the thinnest portion as a starting point, and the impact may damage the pellicle film. Damage to the pellicle film when the pellicle is peeled off is a problem because it takes time to regenerate the photomask. Therefore, the height of the cutout portion is preferably 50% or less of the thickness of the pellicle frame, more preferably 30% or less, and even more preferably 15% or less. On the other hand, from the viewpoint of ease of processing, the height of the cutout portion is preferably 5% or more of the thickness of the pellicle frame.
[0025] In Figure 1, a cutout portion 20 is provided on the upper end surface of the pellicle frame 1, but as another embodiment of the pellicle frame, a pellicle frame having a cutout portion 20 provided on the lower end surface of the pellicle frame 1 is shown in Figures 3(A) to (C).
[0026] In the present invention, in order to prevent damage to the pellicle membrane when the pressure changes from atmospheric pressure to vacuum, the total ventilation area of any of the inner surface, outer surface, inner space side of the pellicle, and outer space side of the pellicle is set to 1 mm2 of the volume of the inner space of the pellicle. 3 0.001mm per 2 The total ventilation area should be set to 1 mm or more. In order to reduce the risk of damage to the pellicle membrane, the larger the ventilation area, the better. The total ventilation area should be set to 1 mm or less per 1 mm of the volume of the space inside the pellicle. 3 0.0013mm per 2 More preferably, the value is 0.0015 mm. 2 The upper limit is preferably 0.02 mm from the viewpoint of preventing damage to the pellicle frame and maintaining its strength. 2 Less than or equal to 0.015 mm, more preferably 2 The following is the result.
[0027] In addition, it is preferable that the pellicle frame of the present invention is provided with a through hole having an opening at least on the inner surface. That is, one of the openings of the through hole can be provided on the inner surface, and the other opening of the through hole can be formed on the outer surface of the pellicle frame or on the upper end surface where the pellicle membrane is located. When the other opening of the through hole is formed on the upper end surface of the pellicle frame, a filter can be provided on the upper end surface, which is particularly advantageous for EUV where the frame thickness is thin.
[0028] The shape and dimensions of the through hole (vent hole) are not particularly limited, but it is preferable to adopt a circular or elliptical shape, and the opening area of the through hole (vent hole) is 0.03 mm 2 For ease of processing, it is preferable that the thinnest part between the pellicle end face and the air hole is 0.2 mm or more.
[0029] In the pellicle frame of Fig. 1, both a cutout portion and a through hole (vent hole) are formed, but the present invention is not limited to this and only a cutout portion may be used. However, as described below, in order to ensure a certain area as a vent, to fully exert the desired effects of the present invention, and to ensure sufficient strength of the pellicle frame, it is desirable to use both a cutout portion and a through hole. In this case, the area of the cutout portion on each of the long and short sides of the pellicle frame is 0.05 to 400 mm 2 The number of holes ranges from 1 to 50, while the area of the through holes ranges from 0.03 to 130 mm 2 The number of the electrodes can be within the range of 1 to 250.
[0030] In the pellicle frame of the present invention, the ventilation area is calculated as the ventilation area at any one of the inner surface, outer surface, pellicle inner space side, and pellicle outer space side when the pellicle is completed. For example, if there are 40 ventilation holes with a diameter of 0.8 mm, 40 cutouts with a width of 10 mm (see reference number 21 in FIG. 1) and a height of 0.2 mm (see reference number 23 in FIG. 1) on the end surface on the pellicle membrane side, and the thickness of the pellicle membrane adhesive formed on the upper end surface other than the cutouts is 0.1 mm, the total ventilation area present in this pellicle is 140 mm. 2 In other words, the thickness of the adhesive is also calculated as the ventilation area. [Area of vent hole: Formula 1] 0.4 x 0.4 x 3.14 x 40 (number) = 20.096 (mm 2 ) [Opening area of the notch: Formula 2] 10 x (0.2 + 0.1) x 40 (number) = 120 (mm 2 )
[0031] In other words, when a cutout is provided in the pellicle frame, the cutout is easier to fabricate than an air hole, and as described above, the thickness of the laminated adhesive layer is also added to the ventilation space other than the cutout, so there is a great advantage in the present invention in requiring the cutout as a ventilation portion.
[0032] In the present invention, the internal space volume of a pellicle means the true internal space volume including the thickness of the adhesive when the pellicle is completed. For example, in the case where the inner dimensions of the pellicle frame are 143 mm long x 110 mm wide x 1.5 mm high, the thickness of the adhesive for the pellicle film and the adhesive for the photomask is 0.1 mm, and the pellicle film is an extremely thin single crystal silicon film supported by a Si frame with a height of 0.725 mm, the extremely thin silicon film is sufficiently thin that it can be ignored when calculating the volume, and therefore the internal space volume of the pellicle is 38145 mm. 3 It becomes. [Internal space volume of pellicle: Equation 3] 143×110×(1.5+0.1+0.1+0.725)=38145.25(mm 3 ) The total ventilation area at this time is 20.096 (mm 2 )+120(mm 2 )〕 / 38145mm 3 ≒0.0037. The volume of the space inside the pellicle is 1 mm 3 Approximately 0.0037 mm per 2 This can be calculated as follows.
[0033] The ventilation section may be provided with a filter as necessary.
[0034] In the pellicle of the present invention, a pellicle membrane is provided on the upper end surface of the pellicle frame as described above via a pressure-sensitive adhesive or adhesive for the pellicle membrane. There are no particular limitations on the pressure-sensitive adhesive or adhesive for the pellicle membrane, and any known pressure-sensitive adhesive or adhesive can be used. In general, the pressure-sensitive adhesive or adhesive is formed over the entire circumferential direction of one end surface of the pellicle frame, with a width equal to or smaller than the width of the pellicle frame. If there is a cutout portion on one end surface of the pellicle frame, it is preferable that the pressure-sensitive adhesive or adhesive is formed on the end surface other than the cutout portion.
[0035] The material of the pellicle film is not particularly limited, but it is preferable that the material has high transmittance at the wavelength of the exposure light source and high light resistance. For example, an ultrathin silicon film, Si film, carbon film, etc. are used for EUV exposure. Examples of these carbon films include films of graphene, diamond-like carbon, carbon nanotubes, etc. In addition, if it is difficult to handle the pellicle film alone, a pellicle film supported by a frame such as silicon can be used. In that case, the pellicle can be easily manufactured by bonding the frame area to the pellicle frame.
[0036] Furthermore, a pressure sensitive adhesive or glue is applied to the lower end surface of the pellicle frame for mounting the pellicle frame to a photomask. In general, the pressure sensitive adhesive or glue is applied to the entire circumferential circumference of one end surface of the pellicle frame, with a width equal to or less than the width of the pellicle frame. If the one end surface of the pellicle frame has a notch, the pressure sensitive adhesive or glue is applied to the end surface other than the notch.
[0037] The photomask adhesive may be a known adhesive, and an acrylic adhesive, a silicone adhesive, a rubber adhesive, etc. may be suitably used, and a silicone adhesive is particularly preferred from the viewpoint of heat resistance. The adhesive may be processed into any shape as necessary.
[0038] A release layer (separator) for protecting the adhesive may be attached to the lower end surface of the photomask adhesive. The material of the release layer is not particularly limited, but for example, polyethylene terephthalate (PET), polytetrafluoroethylene (PTFE), tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA), polyethylene (PE), polycarbonate (PC), polyvinyl chloride (PVC), polypropylene (PP), etc. may be used. In addition, a release agent such as a silicone-based release agent or a fluorine-based release agent may be applied to the surface of the release layer as necessary.
[0039] The pellicle frame of the present invention may be provided with protrusions facing outward or inward. By using such protrusions, a filter can be formed. In addition, by providing the protrusions facing outward with a connection mechanism (screws, adhesive, etc.) with an exposure master plate, the adhesive for the photomask can be omitted.
[0040] The pellicle of the present invention may be used not only as a protective member for preventing foreign matter from adhering to an exposed original plate in an EUV exposure device, but also as a protective member for protecting the exposed original plate during storage or transportation of the exposed original plate. Methods for attaching a pellicle to an exposed original plate such as a photomask to manufacture an exposed original plate with a pellicle include the above-mentioned method of attaching the pellicle with an adhesive for photomasks, as well as electrostatic adsorption and mechanical fixing methods.
[0041] The method for manufacturing a semiconductor or liquid crystal display panel according to the embodiment of the present invention includes a step of exposing a substrate (semiconductor wafer or liquid crystal original plate) using the above-mentioned exposure original plate with pellicle. For example, in a lithography process, which is one of the manufacturing processes for a semiconductor or liquid crystal display panel, the above-mentioned exposure original plate with pellicle is placed on a stepper and exposed to form a photoresist pattern corresponding to an integrated circuit or the like on the substrate. Generally, in EUV exposure, a projection optical system is used in which EUV light is reflected by the exposure original plate and guided to the substrate, and these are performed under reduced pressure or vacuum. As a result, even if foreign matter adheres to the pellicle in the lithography process, the foreign matter is not imaged on the wafer coated with photoresist, so that short circuits, breaks, etc. of integrated circuits due to the image of the foreign matter can be prevented. Therefore, the use of the exposure original plate with pellicle can improve the yield in the lithography process. EXAMPLES
[0042] The present invention will be specifically described below with reference to examples and comparative examples, but the present invention is not limited to the following examples.
[0043] [Example 1] A titanium pellicle frame (inner dimensions 143 mm × 110 mm × height 1.5 mm, frame width 4 mm) was fabricated. A cutout portion measuring 30 mm in width × 0.1 mm in height × 4 mm in depth was provided on the upper end surface at the center of each side of the pellicle frame. In addition, 12 through holes with a diameter of 0.8 mm were provided on each side. The pellicle frame was washed, and 100 parts by mass of silicone adhesive ("X-40-3264" manufactured by Shin-Etsu Chemical Co., Ltd.) was mixed with 1 part by mass of hardener ("PT-56" manufactured by Shin-Etsu Chemical Co., Ltd.) and agitated at the notch-free portion of the upper end surface of the pellicle frame to a width of 1 mm and a thickness of 0.1 mm. In addition, 100 parts by mass of acrylic adhesive ("SK Dyne 1499M" manufactured by Soken Chemical Co., Ltd.) was mixed with 0.1 parts by mass of hardener ("L-45" manufactured by Soken Chemical Co., Ltd.) and agitated as a photomask adhesive to a width of 1 mm and a thickness of 0.1 mm on the entire circumference of the lower end surface of the pellicle frame. After that, the pellicle frame was heated at 100°C for 12 hours to harden the adhesive on the upper and lower end surfaces. Next, a 50 nm-thick ultrathin silicon film supported by a 0.725 mm-thick Si frame was attached to the top surface of the pellicle frame with pressure, completing the pellicle.
[0044] [Example 2] An aluminum pellicle frame (inner dimensions: 143 mm x 110 mm x height: 1.5 mm, frame width: 4 mm) was prepared. 48 through holes with a diameter of 0.8 mm were provided on each side of the pellicle frame. Other than the shape of the frame, the structure was the same as in Example 1.
[0045] [Comparative Example 1] A titanium pellicle frame (inner dimensions 143 mm × 110 mm × 1.5 mm, frame width 4 mm) was fabricated. A cutout portion measuring 30 mm in width × 0.1 mm in height × 4 mm in depth was provided on the upper end surface at the center of each side of the pellicle frame. Other than the shape of this pellicle frame, it was the same as in Example 1.
[0046] [Comparative Example 2] An attempt was made to fabricate the pellicle frame of Example 1 using alumina, which is a ceramic, but it broke during production.
[0047] [Vacuum test] The pellicles produced in Examples 1 and 2 and Comparative Example 1 were attached to a 6-inch square quartz mask, and a vacuum test was carried out. In this vacuum test, the above-mentioned masked pellicle was placed in a vacuum chamber, the pressure was reduced from atmospheric pressure to 1 Pa in 170 seconds, and then the pressure was returned from 1 Pa to atmospheric pressure in 250 seconds, and it was confirmed whether the pellicle film was damaged. The results are shown in Table 1 below.
[0048] [Table 1]
[0049] From the results in Table 1 above, in Examples 1 and 2, no damage to the pellicle membrane was confirmed and the results were good, but in Comparative Example 1, damage to the pellicle membrane was confirmed. [Explanation of symbols]
[0050] 1 Pellicle frame 11 Inner surface of pellicle frame 12 Outer surface of pellicle frame 13 Upper end surface of pellicle frame 14 Bottom surface of pellicle frame 20 Cutout 21 Width of cutout 22 Depth of cutout 23 Height of cutout 30 Through holes (ventilation holes) 2. Pellicle membrane 3. Photomask 4. Pellicle membrane adhesive or glue 5. Photomask adhesives or glues 10 Photomask with pellicle
Claims
1. A pellicle comprising a frame-shaped metal pellicle frame having two end faces, A pellicle characterized in that at least one end face of the pellicle frame has a recess extending from the outer surface to the inner surface, and the pellicle frame has 28 to 250 through holes having openings on at least the inner surface.
2. The total ventilation area on the inner surface of the pellicle frame is equal to or less than 1 mm of the volume of the inner space of the pellicle. 3 0.001mm per 2 The pellicle according to claim 1.
3. The total ventilation area on the inner space side of the pellicle is 1 mm 3 0.001mm per 2 The pellicle according to claim 1.
4. The total ventilation area on the outer surface of the pellicle frame is equal to or less than 1 mm of the volume of the inner space of the pellicle. 3 0.001mm per 2 The pellicle according to claim 1.
5. The total ventilation area on the outer space side of the pellicle is 1 mm2 of the inner space volume of the pellicle. 3 0.001mm per 2 The pellicle according to claim 1.
6. The pellicle according to any one of claims 1 to 5, wherein the thinnest part between the through hole and the end face of the pellicle frame is 0.2 mm or more.
7. The total ventilation area is equal to the volume of the internal space of the pellicle. 3 0.02mm per 2 The pellicle according to any one of claims 2 to 6, wherein:
8. 8. The pellicle according to claim 1, wherein the height of the recess is 50% or less of the thickness of the pellicle frame.
9. The pellicle according to any one of claims 1 to 8, wherein the thickness of the pellicle frame is 2.5 mm or less.
10. 10. The pellicle according to claim 1, wherein the end face of the pellicle frame having the recess has a pellicle membrane via an adhesive or a adhesive.
11. The pellicle according to any one of claims 1 to 10, which is used for exposure under vacuum or reduced pressure.
12. The pellicle according to any one of claims 1 to 10, which is used for EUV exposure.
13. 13. An exposure master with a pellicle, comprising: an exposure master with a pellicle according to any one of claims 1 to 12 attached thereto.
14. An exposure method comprising exposing using the exposure master with a pellicle according to claim 13.
15. A method for manufacturing a semiconductor device, comprising the step of exposing a substrate using the pellicle-attached exposure master according to claim 13.
Citation Information
Patent Citations
Pellicle frame and pellicle
JP2019070745A
Pellicle frame and pellicle
JP2020042105A
Pellicle frame and pellicle
JP2020126095A
Vent for an optical pellicle system
US20040043302A1
Pellicle having buffer zone and photomask structure having pellicle
US20130089814A1
Cited By
Pellicle frame, pellicle, exposure original plate with pellicle, exposure method, and method for manufacturing semiconductor
WO2026100332A1
Pellicle frame, pellicle, and method for releasing pellicle
WO2026150798A1