Buckling restraint brace and method of manufacturing the same
By employing a mixture of lubricant and synthetic resin as unbonded materials on both sides of the core material and incorporating slits, the buckling restraint brace addresses the challenge of non-uniform buckling and manufacturing complexity, achieving efficient energy absorption and deformation distribution.
Patent Information
- Application Number
- JP2023065016
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-12
- Publication Date
- 2024-10-25
AI Technical Summary
Existing buckling restraint braces face challenges in efficiently managing buckling in both the weak and strong axis directions of the core material, requiring time-consuming and difficult manufacturing processes for unbonded materials like butyl rubber, especially on the narrow side, which complicates the application of unbonded materials to non-uniform core shapes.
The use of a mixture of lubricant and synthetic resin as unbonded materials applied to both the wide and narrow surfaces of the core material, along with slits on the wide surface to adjust yield strength, facilitates easier manufacturing and adaptability to various core dimensions and shapes, allowing for uniform buckling in both axis directions.
This approach enhances manufacturability and adaptability, enabling efficient buckling restraint braces with improved energy absorption performance during earthquakes by uniformly distributing plastic deformation across the core material, reducing frictional forces and simplifying the manufacturing process.
Smart Images

Figure 2024151565000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a buckling restrained brace and a method for making the same. [Background technology]
[0002] Buckling-restrained braces with buckling prevention measures have been used as braces that form building frames (column-beam frames, roof frames, etc.). Buckling-restrained braces come in a variety of stiffening forms, including a form in which the periphery of a steel core is stiffened only with steel plates, a form in which the periphery of a steel core is stiffened with RC (Reinforced Concrete), and a form in which the periphery of a steel core is covered with steel and mortar.
[0003] Here, Patent Document 1 proposes a buckling-restrained brace in which a core member is restrained by restraining members formed of a pair of square steel pipes, and which does not cause local destruction in the restraining members that receive a pressing force from the core member. Specifically, the buckling-restrained brace includes a core member that has joints at both ends of the plate-like portion for joining to other members, and restraining members arranged opposite each face perpendicular to the weak axis direction of the plate-like portion.
[0004] In this buckling restraint brace, an insert plate that comes into contact with the restraint member is provided between the plate-like portion and the restraint member, and the restraint member, which is made of a square steel pipe, has corners with curved areas at the intersections of its surfaces. A weld is provided between the surface of the insert plate that comes into contact with the restraint member and the corner of the restraint member to secure the restraint member to the insert plate. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent No. 6445862 Summary of the Invention [Problem to be solved by the invention]
[0006] The buckling restraint brace described in Patent Document 1 makes it easy to use components such as prefabricated square steel pipes as restraint materials, making it possible to suppress localized failure of the restraint material when subjected to compressive force from the core material, without incurring high costs.
[0007] The buckling restrained brace is assembled into the building frame by bolting both ends to connecting fixtures such as brackets and gusset plates provided at the corners of the building frame. When the building frame is deformed during an earthquake, an external force such as a horizontal force during an earthquake enters the end of the buckling restrained brace through the bracket, etc., and the external force is transmitted from the end of the core material to the entire area as a compressive force, etc., causing the entire core material to plastically deform, thereby demonstrating the energy absorption performance during an earthquake. More specifically, when a compressive force acts on the core material, a higher-order mode buckling (wave-like deformation) occurs in the weak axis direction throughout the entire area, and the entire core material is buckled as evenly as possible, thereby enabling the entire buckling restrained brace to demonstrate its plastic deformation performance.
[0008] In the buckling restrained brace described in Patent Document 1, in order to cause the above-mentioned higher-order mode buckling to occur on the wide surface of the core material, an unbonded material having deformability such as butyl rubber is interposed between the wide surface of the core material and the restraining material, and the thickness of the unbonded material is used as a clearance, and when the core material is subjected to a compressive force, a higher-order mode buckling in the weak axis direction of the core material occurs within this clearance. However, when a compressive force acts on the core material, buckling can occur not only in the weak axis direction of the wide surface, but also in the strong axis direction of the narrow surface, but the buckling restrained brace described in Patent Document 1 does not mention the unbonded material that corresponds to this buckling in the strong axis direction.
[0009] If an unbonded material made of butyl rubber or the like were to be applied to the narrow surface (strong axis direction) of the core material in the same way as the wide surface (weak axis direction), a series of manufacturing steps would be required, such as cutting a commercially available, fixed-shape butyl rubber to fit the narrow surface of the core material, adjusting the dimensions, and then attaching the cut butyl rubber to the narrow surface. However, this cutting and attachment process requires a lot of time and effort, and it is extremely difficult to carry out this series of manufacturing steps with precision.
[0010] The present invention has been made in consideration of the above-mentioned problems, and aims to provide a buckling restraint brace that is easy to manufacture and has an unbonded material that is well adaptable to the shapes and dimensions of both the wide and narrow faces of the core material that makes up the buckling restraint brace, and a method for manufacturing the same. [Means for solving the problem]
[0011] In order to achieve the above object, one aspect of the buckling restraint brace according to the present invention is as follows: A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; A pair of plate-shaped stiffeners made of steel that face the pair of narrow surfaces of the core material and connect side surfaces of the pair of restraint materials; a first unbond material included in an unbond material attached to at least one of the wide surface of the core material and the opposing surface of the restraint material; a second unbond material included in an unbond material attached to at least one of the narrow surface of the core material and the opposing surface of the stiffener material; The first unbonded material and the second unbonded material are both formed from a mixture of a lubricant and a synthetic resin.
[0012] According to the present embodiment, the first unbonded material attached to at least one of the wide surface of the core material and the opposing surface of the restraining material, and the second unbonded material attached to at least one of the narrow surface of the core material and the opposing surface of the stiffening material are both formed from a mixture of lubricant and synthetic resin. For example, the unbonded material is formed by applying it to the wide surface (weak axis direction) and narrow surface (strong axis direction) of the core material by painting or spraying, etc., which makes the unbonded material easy to manufacture and results in a buckling restraint brace with an unbonded material that has good adaptability to the shape and dimensions of the core material.
[0013] Here, "at least one of the wide surface of the core material and the opposing surface of the restraining material" means both the wide surface of the core material and the opposing surface of the restraining material, and either one of the wide surface of the core material and the opposing surface of the restraining plate. Similarly, "at least one of the narrow surface of the core material and the opposing surface of the stiffening material" means both the narrow surface of the core material and the opposing surface of the stiffening material, and either one of the wide surface of the core material and the opposing surface of the stiffening material.
[0014] Conventional unbonded materials made of butyl rubber or the like use their thickness as a clearance, allowing higher-order mode buckling to occur within this clearance when the core material is subjected to a compressive force. In contrast, in this embodiment, in which a first unbonded material and a second unbonded material are formed by coating on at least one of the wide surface of the core material and the opposing surface of the restraining material, and at least one of the narrow surface of the core material and the opposing surface of the stiffening material, a clearance is provided in the first unbonded material for causing higher-order mode buckling in the weak axis direction of the core material, and a clearance is provided in the second unbonded material for causing higher-order mode buckling in the strong axis direction of the core material.
[0015] In addition, for example, a steel insert plate may be interposed between the first unbonded material attached to the wide surface of the core material and the restraint material. This insert plate makes it possible to effectively prevent the restraint material from being locally damaged by the pressing force caused by the buckling of the higher order mode in the weak axis direction of the core material acting directly on the restraint material.
[0016] Another aspect of the buckling restraint brace according to the present invention is A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; A pair of plate-shaped stiffeners made of steel that face the pair of narrow surfaces of the core material and connect side surfaces of the pair of restraint materials; a first unbond material included in an unbond material attached to at least one of the wide surface of the core material and the opposing surface of the restraint material; a second unbond material included in an unbond material attached to at least one of the narrow surface of the core material and the opposing surface of the stiffener material; The first unbonded material is formed of a fixed unbonded material, The second unbonded material is characterized in that it is made of a mixture of a lubricant and a synthetic resin.
[0017] According to this embodiment, a standard unbonded material is applied to the first unbonded material corresponding to the wide surface of the core material, and a mixture of lubricant and synthetic resin is applied to the second unbonded material corresponding to the narrow surface of the core material. This improves the manufacturability of the second unbonded material, which corresponds to the narrow surface of the core material, which is particularly difficult to cut and install, and results in a buckling restraint brace with an unbonded material that is well adaptable to the shape and dimensions of the core material.
[0018] In another aspect of the buckling restrained brace according to the present invention, The unbonded material is characterized in that a gap for buckling deformation of the core material is provided on the side opposite to the attachment surface to the core material, the restraining material, or the stiffening material.
[0019] According to the present embodiment, gaps for buckling deformation in the weak axis and strong axis directions of the core material are provided on the side of the first unbonded material and the second unbonded material opposite the attachment surface to the core material, the restraint material, or the stiffener material, so that these gaps can absorb higher-order mode buckling in both the weak axis and strong axis directions of the core material.
[0020] In another aspect of the buckling restrained brace according to the present invention, The broad surface of the core material is provided with slits extending in the longitudinal direction of the core material to adjust the strength of the core material.
[0021] According to the present embodiment, slits are provided on the wide surface of the core material to adjust the strength of the core material. For example, when the cross-sectional area of the entire cross-section of the core material is too large and the strength becomes too high, the cross-sectional area of the core material can be adjusted by the slits.
[0022] In another aspect of the buckling restrained brace according to the present invention, A third unbond material included in the unbond material is disposed in the slit; The third unbonded material is characterized in that it is made of a mixture of a lubricant and a synthetic resin.
[0023] According to this embodiment, when a slit is provided on the wide surface of the core material, the unbonded material formed of a mixture of a lubricant and a synthetic resin is disposed in the slit, so that, for example, when a hard spacer is inserted into the slit, the core material is deformed by buckling, and there is no problem that frictional force is generated between the spacer and the wall surface of the slit. This spacer is a means for suppressing the core material from deforming inward by providing a slit in the core material. In addition, since the slit is generally an elongated groove, it is practically impossible to cut a standard butyl rubber or the like and fit it into the slit, but in this embodiment, the slit is coated with a mixture of a lubricant and a synthetic resin, so that the third unbonded material can be easily disposed in the slit.
[0024] In addition, one aspect of a method for manufacturing a buckling restrained brace according to the present invention includes the steps of: 1. A method of fabricating a buckling restrained brace, comprising the steps of: A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; a preparation process for preparing a pair of steel plate-shaped stiffeners that face the pair of narrow surfaces of the core material and connect side surfaces of the pair of restraint materials; A mixture of a lubricant and a synthetic resin is applied or sprayed onto at least one of the wide surface of the core material and the opposing surface of the restraint material to form a first unbonded material; an unbonded material forming step of forming a second unbonded material by applying or spraying a mixture of a lubricant and a synthetic resin to at least one of the narrow surface of the core material and the opposing surface of the stiffener; and an assembly process in which each component is assembled to produce a buckling restraint brace.
[0025] According to the present embodiment, a first unbonded material is formed by applying or spraying a mixture of lubricant and synthetic resin to at least one of the wide surface of the core material and the opposing surface of the restraint material, and a second unbonded material is formed by similarly applying or spraying the mixture to at least one of the narrow surface of the core material and the opposing surface of the stiffener material. This improves the manufacturability of both the first and second unbonded materials, and allows the production of a buckling restraint brace with an unbonded material that is easily adaptable to the shape and dimensions of the core material.
[0026] Another aspect of the method for manufacturing a buckling restrained brace according to the present invention is to When a slit is provided on the wide surface of the core material extending in the longitudinal direction of the core material to adjust the strength of the core material, the unbonded material forming process is further characterized in that a mixture of lubricant and synthetic resin is applied or sprayed onto the slit to form a third unbonded material.
[0027] According to the present embodiment, by applying a mixture of lubricant and synthetic resin to the slit provided on the wide surface of the core material, it becomes possible to easily arrange a third unbonded material in the slit, whereas it is virtually impossible to manufacture the slit, which is a long, narrow groove, by cutting and fitting a standard piece of butyl rubber or the like into it. Effect of the Invention
[0028] As can be understood from the above explanation, the buckling restrained brace and its manufacturing method of the present invention make it possible to provide a buckling restrained brace that is easy to manufacture and has unbonded material that is well adaptable to the shapes and dimensions of both the wide and narrow faces of the core material that makes up the buckling restrained brace. [Brief description of the drawings]
[0029] [Figure 1] FIG. 1 is an exploded perspective view of an example buckling restrained brace according to embodiments. [Figure 2A] FIG. 1 is a longitudinal cross-sectional view of an example of a buckling restraint brace according to an embodiment in a pre-assembly state taken in a direction perpendicular to the axis. [Figure 2B] FIG. 11 is a longitudinal cross-sectional view in a direction perpendicular to the axis of another example of a buckling restraint brace according to an embodiment in a pre-assembled state. [Diagram 3] FIG. 1 is a perspective view of an example of a buckling restrained brace according to embodiments. [Figure 4] FIG. 1 is a longitudinal cross-sectional view of an example of an assembled state of a buckling restraint brace according to an embodiment of the present invention, taken in a direction perpendicular to the axis. [Figure 5A] FIG. 13 is a schematic diagram of a longitudinal section of a buckling restrained brace in a direction perpendicular to the axis, illustrating the state in which stiffening forces act from the core material to the restraining material and stiffening material during higher-order mode buckling. [Figure 5B] FIG. 13 is a schematic diagram of an axial cross section of a buckling restrained brace, illustrating the state in which a stiffening force acts from the core material to the restraining material during higher-order mode buckling. [Figure 5C] FIG. 13 is a schematic diagram of a vertical cross section in the axial direction of a buckling restrained brace, illustrating the state in which a stiffening force acts from the core material to the stiffening material during higher-order mode buckling. [Figure 6] 1 is a diagram illustrating the geometric moment of inertia of a core material depending on whether or not there is a slit in the wide surface of the core material. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0030] Hereinafter, a buckling restraint brace according to an embodiment and a method for manufacturing the same will be described with reference to the accompanying drawings. In this specification and the drawings, substantially identical components are designated by the same reference numerals to avoid redundant description.
[0031] [Buckling restraint brace according to embodiment and its manufacturing method] An example of a buckling restrained brace according to an embodiment and a method for manufacturing the same will be described with reference to Figures 1 to 6. Here, Figure 1 is an exploded perspective view of an example of a buckling restrained brace according to an embodiment, and Figures 2A and 2B are both vertical cross-sectional views in a direction perpendicular to the axis of the buckling restrained brace according to an embodiment in a pre-assembled state. Also, Figure 3 is a perspective view of an example of a buckling restrained brace according to an embodiment, and Figure 4 is a vertical cross-sectional view in a direction perpendicular to the axis of an example of a buckling restrained brace according to an embodiment in an assembled state.
[0032] The buckling restrained brace 100 has a core material 10, a pair of restraining members 30 arranged to face a pair of wide surfaces 10a of the core material 10, a pair of stiffening members 50 arranged to face a pair of narrow surfaces 10b of the core material 10, a first unbonded member 20A interposed between the core material 10 and the restraining members 30, and a second unbonded member 20B interposed between the core material 10 and the stiffening members 50. Here, in addition to the illustrated example, a form in which a steel insert plate is interposed between the first unbonded member 20 and the restraining member 30 may also be used.
[0033] It is preferable that the core material 10 be formed from a steel material with a low yield point, such as SN material (rolled steel material for architectural structures) or LYP material (very low yield point steel material). By using a core material 10 made from these materials, the yielding of the core material 10 results in good earthquake energy absorption.
[0034] The core material 10 is formed from a long, thin steel plate and has a narrow width portion 11 at the center of its longitudinal direction where the width of the wide surface 10a is relatively narrow, and a wide width portion 12 at the end of its longitudinal direction where the width of the wide surface 10a is relatively wide.
[0035] Since the core material 10 has a narrow width portion 11 at the center of its longitudinal direction and a wide width portion 12 at each end of the longitudinal direction, the narrow width portion 11 at the center can be made into a region that is easily plasticized, and further, the plasticization region can be limited to the narrow width portion 11 at the center.
[0036] A cylindrical steel protrusion 15 protrudes from the two wide surfaces 10a of the narrow portion 11 at the center of the narrow portion 11 of the core material 10. The protrusion 15 is joined to the wide surfaces 10a of the narrow portion 11 by welding or the like.
[0037] The restraining material 30 is formed of a square steel pipe having a rectangular cross section. In the restraining material 30, a projection hole 30b into which the projection 15 of the core material 10 fits is provided on an opposing surface 30a on which the first unbonded material 20A is formed.
[0038] On the sides of the core material 10, both sides (sides corresponding to the short sides of the rectangle) of the pair of restraint materials 30 are connected by welding or the like to a pair of stiffening materials 50 made of steel plates, and the core material 10 is surrounded by the pair of restraint materials 30 and the pair of stiffening materials 50.
[0039] Slits 14, which are fine holes for adjusting the strength of the core material 10, are provided on both sides of the protrusion 15 of the narrow portion 11 of the core material 10. In Figure 1, the third unbonded material 20C is shown as being typically attached to the slits 14 in the X1 direction, but in reality, the third unbonded material 20C is not a standard component, and the third unbonded material 20C is formed inside the slit 14 by applying or spraying a mixture of lubricant and synthetic resin into the slit 14.
[0040] Here, lubricants include solid lubricants and liquid lubricants. Solid lubricants include molybdenum disulfide (MoS2), graphite, and fluororesin (PTFE: polytetrafluoroethylene). A solid lubricant film is formed on the friction surface, which can suppress direct contact of the friction surface materials and suppress the occurrence of galling. On the other hand, liquid lubricants include lubricating oil. Synthetic resins (paints) include epoxy resins, silicon resins, acrylic resins, acrylic silicon resins, chlorinated rubber resins, silicon resins, phenolic resins, phthalic acid resins, unsaturated polyester resins, and polyurethane resins.
[0041] A pair of joining plates 13 made of steel plates are joined by welding or the like to the wide portions 12 at both ends of the core material 10 so as to be joined to other members perpendicular to the wide surfaces 10a.
[0042] The wide portion 12 and the connecting plate 13 are provided with bolt holes 12a, 13a, respectively, which are aligned with the bolt holes of connecting fixtures (other components) such as brackets and gusset plates that protrude into the structural surface from corners, etc. of the building frame (not shown), and are bolted together.
[0043] A reinforcing plate 18 made of a steel plate is joined to the pair of joining plates 13 by welding or the like, and the end of the restraint material 30 is accommodated in the space formed by the wide portion 12 of the core material 10, the pair of joining plates 13, and the reinforcing plate 18.
[0044] The first unbonded material 20A and the second unbonded material 20B are formed of a mixture of a lubricant and a synthetic resin, similar to the third unbonded material 20C.
[0045] In Fig. 1, the first unbond material 20A is shown to be attached in the X2 direction to the opposing surface 30a of the restraining material 30 that faces the wide surface 10a of the core material 10, but in reality, as shown in Fig. 2A, the first unbond material 20A is formed to be thin and have a protruding hole 20a in the center by applying or scattering a mixture of lubricant and synthetic resin with a brush or the like to the opposing surface 30a of the restraining material 30. Similarly, in Fig. 1, the second unbond material 20B is shown to be attached in the X3 direction to the opposing surface 50a of the stiffening material 50 that faces the narrow surface 10b of the core material 10, but in reality, as shown in Fig. 2A, the second unbond material 20B is formed to be thin and have a protruding hole 20a in the center by applying or scattering a mixture of lubricant and synthetic resin with a brush or the like to the opposing surface 50a of the stiffening material 50.
[0046] Here, instead of forming the unbond material 20 on the opposing surface 30a of the restraining member 30 and the opposing surface 50a of the stiffening member 50, as shown in Fig. 2B, a first unbond material 20A may be formed on the wide surface 10a of the core material 10, and a second unbond material 20B may be formed on the narrow surface 10b of the core material 10. Furthermore, although not shown, the first unbond material 20A may be formed on both the opposing surface 30a of the restraining member 30 and the wide surface 10a of the core material 10, and the second unbond material 20B may be formed on both the opposing surface 50a of the stiffening member 50 and the narrow surface 10b of the core material 10.
[0047] In addition, although not shown in the figures, in a configuration in which an insert plate is interposed between the restraint material 30 and the wide surface 10a of the core material 10, the first unbonded material may be formed on the opposing surface of the insert plate that faces the wide surface 10a of the core material 10, or the first unbonded material may be formed on both the opposing surface of the insert plate and the wide surface 10a of the core material 10.
[0048] Compared with conventional unbonded materials made of butyl rubber or the like, the unbonded material 20 formed from a mixture of lubricant and synthetic resin can achieve low friction with a friction coefficient of μ=0.04 and can withstand a heat temperature of about 300°C.
[0049] In addition, since the unbonded material 20 is formed by applying a mixture of lubricant and synthetic resin to the opposing surface 30a of the restraining material 30, the wide surface 10a of the core material 10, etc., it has good adaptability to restraining materials 30, core materials 10, and stiffening materials 50 of various shapes and sizes, and eliminates the need to cut and process commercially available products to fit the shape and dimensions of the restraining material 30, etc., as is the case with conventional unbonded materials made of butyl rubber, etc.
[0050] In particular, since it is not easy to manufacture the narrow second unbonded material 20B corresponding to the narrow surface 10b of the core material 10 and attach it to the stiffener 50, etc., the manufacturability of attaching the second unbonded material 20B to the stiffener 50, etc. is significantly improved.
[0051] Furthermore, since the core material 10 has a long and narrow slit 14 with a width of approximately 0.5 mm to 1 mm, it is virtually impossible to manufacture the core material 10 by cutting a standard butyl rubber and fitting it into the slit 14. However, the third unbonded material 20C can be easily disposed within the slit 14 by applying a mixture of lubricant and synthetic resin to the slit 14.
[0052] Although not shown in the figures, the first unbonded material 20A, which has larger dimensions and relatively better manufacturability compared to the second unbonded material 20B and the third unbonded material 20C, is cut and processed from a standard butyl rubber or the like and attached to the opposing surface 30a of the restraining material 30 or the opposing surface 50a of the stiffening material 50, etc., and the second unbonded material 20B and the third unbonded material 20C may be buckling restraint braces formed by coating a mixed material as in the illustrated example.
[0053] 4, a gap 25 of, for example, about 1 mm is formed between the first unbonded material 20A formed on the opposing surface 30a of the restraining material 30 and the wide surface 10a of the core material 10. Meanwhile, a gap 26 of, for example, about 1 mm is also formed between the second unbonded material 20B formed on the opposing surface 50a of the stiffening material 50 and the narrow surface 10b of the core material 10.
[0054] Within these gaps 25, 26, compressive forces act on the core material 10 when the building frame in which the buckling restraint brace 100 is incorporated is deformed, causing higher-order mode buckling (wavy deformation) in the out-of-plane direction (weak axis direction) and the in-plane direction (strong axis direction) at the wide surface 10a and narrow surface 10b of the narrow portion 11, respectively.
[0055] Here, we will outline a method for manufacturing the buckling restraint brace 100. First, prepare a steel plate-shaped core material 10, a pair of restraint materials 30 made of square steel pipes, and a pair of steel plate-shaped stiffeners 50 that face a pair of narrow faces 10b of the core material 10 and connect the side faces of the pair of restraint materials 30 (this is the preparation process).
[0056] Next, a mixture of lubricant and synthetic resin is applied or sprayed onto at least one of the wide surface 10a of the core material 10 and the opposing surface 30a of the restraining member 30 to form a first unbonded material 20A. A mixture of lubricant and synthetic resin is applied or sprayed onto at least one of the narrow surface 10b of the core material 10 and the opposing surface 50a of the stiffening member 50 to form a second unbonded material 20B. A mixture of lubricant and synthetic resin is applied or sprayed onto the slits 14 provided on the wide surface 10a of the core material 10 to form a third unbonded material 20C (the above is the unbonded material forming process).
[0057] Next, the individual members are joined together by welding, bolting, or the like to produce the buckling restrained brace 100 shown in FIG. 3 (assembly process).
[0058] Next, with reference to Figs. 5 and 6, the friction force reduction effect of the unbonded material on the high-order mode buckling occurring in the weak axis direction and the strong axis direction of the core material 10, and the friction force between the core material and the restraining material and between the core material and the stiffening material that may be generated by the stiffening force at the time of buckling will be described. Here, Fig. 5A is a schematic diagram of a vertical section in the axial direction of the buckling restrained brace, explaining a state in which a stiffening force at the time of buckling in a high-order mode is acting from the core material to the restraining material and the stiffening material. Also, Fig. 5B is a schematic diagram of a vertical section in the axial direction of the buckling restrained brace, explaining a state in which a stiffening force at the time of buckling in a high-order mode is acting from the core material to the restraining material. Also, Fig. 5C is a schematic diagram of a vertical section in the axial direction of the buckling restrained brace, explaining a state in which a stiffening force at the time of buckling in a high-order mode is acting from the core material to the stiffening material. Furthermore, Fig. 6 is a diagram explaining the second moment of area of the core material depending on the presence or absence of a slit in the wide surface of the core material.
[0059] The buckling restrained brace 100 is incorporated into a building frame by bolting its both ends to connecting jigs provided at the corners of the building frame, etc. When the building frame deforms during an earthquake, external forces such as horizontal forces during an earthquake enter the ends of the buckling restrained brace 100 through the connecting jigs, and as shown in Figures 5B and 5C, the external force is transmitted as compressive force N from the ends of the core material 10 to its entire area, causing plastic deformation of the entire area of the core material 10, thereby demonstrating its energy absorption performance during an earthquake.
[0060] In other words, when a compressive force N is applied to the core material 10, as shown in Figures 5A to 5C, higher-mode buckling (wavy deformation) occurs throughout the entire core material 10 in its weak axis and strong axis directions, thereby causing the entire core material 10 to buckle as evenly as possible, thereby enabling the overall plastic deformation performance of the buckling-constrained brace 100 to be exhibited.
[0061] As shown in Figures 5A and 5B, when the core material 10 buckles in the weak axis direction, a stiffening force Q1 acts on the restraining material 30 from the peaks and valleys of the buckling deformation via the first unbonded material 20A. On the other hand, as shown in Figures 5A and 5C, when the core material 10 buckles in the strong axis direction, a stiffening force Q2 acts on the stiffening material 50 from the peaks and valleys of the buckling deformation via the second unbonded material 20B.
[0062] Here, slits 14 are provided on the wide surface 10a of core material 10 to adjust the yield strength of core material 10, and the cross-sectional area of core material 10 is adjusted by slits 14 when, for example, the entire cross section of core material 10 would result in too large a cross-sectional area and too high a yield strength. By providing slits 14 in core material 10, the second moment of area of core material 10 becomes smaller. Specifically, as shown in Figure 6, when core material 10 has a thickness b and a width h1, the second moment of area I1 of core material 10 without slits 14 is expressed as follows: I1 = 1 / 12 × bh1 3 The second moment of area I2 of the core material 10 when the slit 14 is present is I2 = 1 / 12 × bh2 3 (×2), and the second moment of area is proportional to the cube of the width h of the core material 10.
[0063] The buckling load of the core material 10 is d N max , the wavelength of the higher-order buckling mode of the core material 10 is l n , the second moment of area of the core material is I s When we do this, l n 2 =4π 2 E t I s / d N max Based on the known relational expression, the wavelength l of the higher-order buckling mode of the core material 10 is n is the second moment of area of the core material 10, I s The stiffening forces Q1, Q2 (4 d N max S / L n ) is the wavelength l nIn other words, the smaller the second moment of area of core material 10, the smaller the wavelength at the time of buckling, and the greater the stiffening forces Q1 and Q2. By providing slits 14 in wide surface 10a of core material 10, the second moment of area, particularly in the strong axis direction, becomes smaller, and the sum of stiffening forces Q1 and Q2 becomes greater.
[0064] When a compressive force N is applied to the buckling restrained brace 100, the increased load is transmitted as frictional forces F1, F2 to the restraining members 30 and stiffening members 50 from the stiffening forces Q1, Q2 at the time of buckling of the core material 10, and these frictional forces F1, F2 are expressed as the product of the stiffening forces Q1, Q2 and the friction coefficients μ1, μ2 between the core material 10 and the restraining members 30 and stiffening members 50. The frictional forces F1, F2 between the core material 10 and the restraining members 30 and stiffening members 50 can cause damage to the restraining members 30 and stiffening members 50 and inhibit deformation of the core material 10, so it is preferable to reduce them.
[0065] As described above, the second moment of area of the core material 10 with the slits 14 is a specified value, so in order to reduce the friction forces F1 and F2, it is necessary to reduce the friction coefficients μ1 and μ2. However, the first unbonded material 20A and the second unbonded material 20B corresponding to the wide surface 10a and the narrow surface 10b of the core material 10 make it possible to reduce both the friction coefficient μ1 between the core material 10 and the restraining material 30 and the friction coefficient μ2 between the core material 10 and the stiffening material 50, thereby effectively reducing the friction forces F1 and F2.
[0066] In addition, the present invention is not limited to the configuration shown here, and may be implemented in other embodiments in which other components are combined with the configurations and the like of the above-mentioned embodiment. In this regard, the present invention may be modified within the scope of the gist of the present invention, and may be appropriately determined according to the application form. [Explanation of symbols]
[0067] 10: Core material 10a: Wide surface 10b:Narrow side 11: Narrow section 12: Wide section 12a: Bolt hole 13: Joint plate 13a: Bolt hole 14: Slit 15: Protrusion 18: Reinforcement plate 20: Unbonded material 20A: First unbonded material (unbonded material) 20B: Second unbonded material (unbonded material) 20C: 3rd unbonded material (unbonded material) 20a:Protrusion hole 25,26:Gap 30: Restraint material (square steel pipe) 30a: Opposite surface 30b:Protrusion hole 50: Stiffener 50a: Opposing surface 100: Buckling restraint brace N: Axial force (compressive force) Q1,Q2: Stiffening force (pressing force) F1,F2: Friction force
Claims
1. A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; A pair of plate-shaped stiffeners made of steel that face the pair of narrow surfaces of the core material and connect side surfaces of the pair of restraint materials; a first unbond material included in an unbond material attached to at least one of the wide surface of the core material and the opposing surface of the restraint material; a second unbond material included in an unbond material attached to at least one of the narrow surface of the core material and the opposing surface of the stiffener material; A buckling restraint brace, characterized in that both the first unbonded material and the second unbonded material are formed from a mixture of a lubricant and a synthetic resin.
2. A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; A pair of plate-shaped stiffeners made of steel that face the pair of narrow surfaces of the core material and connect side surfaces of the pair of restraint materials; a first unbond material included in an unbond material attached to at least one of the wide surface of the core material and the opposing surface of the restraint material; a second unbond material included in an unbond material attached to at least one of the narrow surface of the core material and the opposing surface of the stiffener material; The first unbond material is formed of a fixed unbond material, A buckling restraint brace, characterized in that the second unbonded material is formed from a mixture of a lubricant and a synthetic resin.
3. The buckling restraint brace according to claim 1 or 2, characterized in that a gap is provided on the unbonded material opposite the attachment surface to the core material, the restraint material, or the stiffener, for buckling deformation of the core material.
4. 3. A buckling restraint brace as described in claim 1 or 2, characterized in that a slit is provided on the wide surface of the core material extending in the longitudinal direction of the core material to adjust the strength of the core material.
5. A third unbond material included in the unbond material is disposed in the slit; The buckling restraint brace of claim 4, wherein the third unbonded material is formed of a mixture of a lubricant and a synthetic resin.
6. 1. A method of fabricating a buckling restrained brace, comprising the steps of: A steel plate-shaped core material having a pair of wide surfaces and a pair of narrow surfaces; A pair of restraining members made of square steel pipes arranged to face the pair of wide surfaces of the core material; a preparation process for preparing a pair of plate-shaped stiffeners made of steel, the pair of stiffeners facing the pair of narrow surfaces of the core material and connecting side surfaces of the pair of restraint materials; A mixture of a lubricant and a synthetic resin is applied or sprayed onto at least one of the wide surface of the core material and the opposing surface of the restraint material to form a first unbonded material; an unbonded material forming step of forming a second unbonded material by applying or spraying a mixture of a lubricant and a synthetic resin to at least one of the narrow surface of the core material and the opposing surface of the stiffener; and an assembly process for assembling each component to produce a buckling restrained brace.
7. The method for manufacturing a buckling restraint brace described in claim 6, characterized in that when a slit is provided on the wide surface of the core material extending in the longitudinal direction of the core material to adjust the strength of the core material, the unbonded material forming process further comprises applying or spraying a mixture of lubricant and synthetic resin to the slit to form a third unbonded material.
Citation Information
Patent Citations
Method and apparatus for continuous liquid impregnation treatment of long material
JP1989045862A