Weld structure

The welded structure addresses insufficient joint strength in aluminum-nickel welds by forming a nickel-rich and aluminum-rich layer configuration with controlled protrusions, achieving stable bonding through minimized blowholes and heat transfer.

JP2024154530AActive Publication Date: 2024-10-31PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023068375
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-19
Publication Date
2024-10-31
Estimated Expiration
2043-04-19

AI Technical Summary

Technical Problem

Welding members composed of aluminum and nickel often results in insufficient joint strength.

Method used

A welded structure is formed by welding a member mainly composed of aluminum and a member mainly composed of nickel, with a nickel-rich layer and an aluminum-rich layer formed on protruding portions, where the aluminum-rich layer is thinner than the nickel-rich layer, and the protruding portions are arranged to minimize heat transfer and blowhole formation.

Benefits of technology

Stable and sufficient joint strength is achieved by minimizing blowhole formation and heat transfer, ensuring robust bonding between the aluminum and nickel members.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154530000001_ABST
    Figure 2024154530000001_ABST
Patent Text Reader

Abstract

To stably obtain sufficient joining strength in a welded structure formed by welding a member containing aluminum as a main component and a member containing nickel as a main component.SOLUTION: A welded structure (1) has an interface (L) in which a first member (10) containing aluminium as a main component and a second member (20) containing nickel as a main component and a welded portion (30) formed by melting a part of the interface (L). A nickel-rich layer (40) in which a ratio of a nickel component is more than the aluminum component and an aluminum-rich layer (50) in which a ratio of the aluminum component is more than the nickel component are formed in each of a plurality of projected portions (61-64). In each of welded cross sections of each of the plurality of projected portions (61-64) projecting to the side of the first member (10) more than the interface (L), an area (50) occupied by an aluminum rich layer is fewer than an area (40) occupied by the nickel-rich layer.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a welded structure formed by welding a member mainly composed of aluminum (a member made of aluminum or an aluminum alloy) and a member mainly composed of nickel (a member made of nickel or a nickel alloy). [Background technology]

[0002] For example, Japanese Patent Laid-Open Publication No. 11-73940 (Patent Document 1) discloses a technique for laser welding a member whose main component is aluminum and a member whose main component is nickel. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 11-73940 Summary of the Invention [Problem to be solved by the invention]

[0004] When a member containing aluminum as a main component and a member containing nickel as a main component are welded together, sufficient joint strength may not be obtained.

[0005] The present disclosure has been made to solve the above-mentioned problems, and a purpose of the present disclosure is to stably obtain sufficient joint strength in a welded structure formed by welding a member mainly composed of aluminum and a member mainly composed of nickel. [Means for solving the problem]

[0006] (Item 1) A welded structure according to the present disclosure is a welded structure formed by welding a first member mainly made of aluminum and a second member mainly made of nickel, and includes an interface where the first member and the second member come into contact, and a welded portion formed by melting a part of the interface. The welded portion includes a plurality of protruding portions each protruding toward the first member from the interface. Each of the plurality of protruding portions is formed with a nickel-rich layer having a higher ratio of nickel than the aluminum component, and an aluminum-rich layer having a higher ratio of aluminum than the nickel component. In the welded cross section of each of the plurality of protruding portions, the area occupied by the aluminum-rich layer is smaller than the area occupied by the nickel-rich layer.

[0007] (2) In the welded structure according to the first aspect, the multiple protruding portions are spaced apart from one another.

[0008] (Item 3) In the welded structure according to item 1, the roots of the plurality of protruding portions overlap each other.

[0009] (4) In the welded structure according to the first aspect, the welded portion has a plurality of bead portions each extending in a first direction and adjacent to each other in a direction intersecting the first direction. The plurality of protruding portions are formed at positions corresponding to the plurality of bead portions, respectively. Effect of the Invention

[0010] According to the present disclosure, in a welded structure formed by welding a member mainly made of aluminum and a member mainly made of nickel, sufficient joint strength can be stably obtained. [Brief description of the drawings]

[0011] [Figure 1] FIG. 1 is a diagram illustrating an example of a welded structure. [Diagram 2] FIG. 1 is a diagram showing a weld cross section of a welded structure. [Diagram 3] FIG. 13 is a view showing a welded cross section of a comparative example. [Figure 4]This is a diagram (part 1) of an example of a welded structure viewed from the Z direction. [Diagram 5] FIG. 2 is a diagram showing the weld cross section of a welded structure (part 2). [Figure 6] This is a diagram (part 2) of an example of a welded structure viewed from the Z direction. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. In the drawings, the same or corresponding parts are designated by the same reference characters and their description will not be repeated.

[0013] FIG. 1 is a diagram that shows a schematic diagram of an example of a welded structure 1 according to the present embodiment. The welded structure 1 is formed by welding a plate-shaped first member 10 mainly made of aluminum to a plate-shaped second member 20 mainly made of nickel and aluminum. The welded structure 1 is welded by irradiating a laser beam toward an outer surface of the second member 20 in a state where the first member 10 and the second member 20 are overlapped. In the figure, the Z direction indicates the overlapping direction of the first member 10 and the second member 20, the X direction indicates the longitudinal direction of the second member 20, and the Y direction indicates the direction perpendicular to the X direction and the Z direction.

[0014] Generally, the weld strength is low when aluminum and nickel are welded together, so it is desirable to ensure the weld strength by increasing the weld area. In the example shown in Fig. 1, a plurality of weld beads 31-34, each extending linearly along the X direction, are formed close to each other in the Y direction. Each weld bead 31-34 is formed by moving a laser beam in the welding advance direction (X direction). In this way, by forming a plurality of weld beads 31-34, the weld area between the first member 10 and the second member 20 is increased, and the joining strength between the two is ensured.

[0015] 2 is a diagram showing a welded cross section of the welded structure 1 according to the present embodiment. The welded structure 1 includes a welded portion 30. The welded portion 30 is formed by melting the periphery of an interface L where the first member 10 and the second member 20 are in contact with each other by irradiation with a laser beam.

[0016] Welded portion 30 includes a plurality of protruding portions 61-64 that protrude toward first member 10 relative to interface L. The plurality of protruding portions 61-64 are formed at positions corresponding to the plurality of weld beads 31-34, respectively. The plurality of protruding portions 61-64 are formed by melting first member 10 and second member 20 up to the first member 10 side relative to interface L when weld beads 31-34 are formed. Note that FIG. 2 shows an example in which one welded portion 30 is formed by overlapping the roots of protruding portions 61-64 with each other.

[0017] The welded portion 30 includes a nickel-rich layer 40 and an aluminum-rich layer 50. The nickel-rich layer 40 and the aluminum-rich layer 50 are formed by mixing the nickel component of the second member 20 and the aluminum component of the first member 10 due to melting during welding. The nickel-rich layer 40 is a layer in which the proportion of the nickel component is higher than the aluminum component. The aluminum-rich layer 50 is a layer in which the proportion of the aluminum component is higher than the nickel component. The nickel-rich layer 40 and the aluminum-rich layer 50 are formed on each of the protruding portions 61-64.

[0018] The nickel-rich layer 40 is formed from the outer surface 20a of the second member 20 to a region closer to the first member 10 than the interface L. The aluminum-rich layer 50 is formed adjacent to the nickel-rich layer 40 so as to cover the surface of the nickel-rich layer 40 on the first member 10 side.

[0019] Of the second member 20, the nickel-rich layer 40, the aluminum-rich layer 50, and the first member 10, the second member 20 has the greatest strength, the nickel-rich layer 40 has the next greatest strength after the second member 20, the first member 10 has the next greatest strength after the nickel-rich layer 40, and the aluminum-rich layer 50 has the lowest strength.

[0020] In the welded structure 1 according to the present embodiment, as shown in Fig. 2, the area of ​​the aluminum-rich layer 50 of each of the protruding portions 61-64 is smaller than the area of ​​the nickel-rich layer 40 of each of the protruding portions 61-64 (the area of ​​the nickel-rich layer 40 on the first member 10 side relative to the interface L). Furthermore, in the welded structure 1, as shown in Fig. 2, the thickness (Z direction dimension) of the aluminum-rich layer 50 of each of the protruding portions 61-64 is smaller than the thickness of the nickel-rich layer 40 of each of the protruding portions 61-64 (the Z direction distance from the interface L of the nickel-rich layer 40 to each tip). The thickness of the aluminum-rich layer 50 is, for example, 100 µm or less.

[0021] The welding conditions (intensity of the welding laser light, welding speed, environmental temperature, etc.) that result in the relationship between the nickel-rich layer 40 and the aluminum-rich layer 50 as shown in FIG. 2 are determined in advance by experiment or the like, and the first member 10 and the second member 20 are welded together under these welding conditions, thereby obtaining the welded structure 1 according to this embodiment.

[0022] The aluminum-rich layer 50 has a characteristic that blowholes (air shots) are more likely to occur than the nickel-rich layer 40. If a plurality of blowholes are connected in the aluminum-rich layer 50, this leads to a decrease in joint strength. In the welded structure 1 according to this embodiment, as described above, the aluminum-rich layer 50 is thin, so that blowholes are less likely to be connected in the Z direction in the aluminum-rich layer 50. Therefore, in the welded structure 1 according to this embodiment, it is possible to suppress a decrease in joint strength.

[0023] FIG. 3 is a diagram showing a welded cross section of a welded structure according to a comparative example. In the comparative example shown in FIG. 3, the area of ​​each aluminum-rich layer 50 of the protruding parts 61-64 is larger than the area of ​​each nickel-rich layer 40 of the protruding parts 61-64 (the area of ​​the nickel-rich layer 40 on the first member 10 side from the interface L). Furthermore, in the comparative example shown in FIG. 3, the thickness of each aluminum-rich layer 50 of the protruding parts 61-64 is thicker than the thickness of the nickel-rich layer 40 of the protruding parts 61-64 (the Z-direction distance from the interface L of the nickel-rich layer 40 to each tip). Thus, in the comparative example shown in FIG. 3, since the aluminum-rich layer 50 is thick, blowholes are likely to be connected in the Z direction in the aluminum-rich layer 50, and there is a concern that the joint strength will decrease. In contrast, in the welded structure 1 according to the present embodiment, as described above, the aluminum-rich layer 50 is thin and blowholes are unlikely to be connected in the Z direction, so sufficient joint strength can be stably obtained.

[0024] As described above, the welded structure 1 according to the present embodiment includes an interface L where a first member 10 mainly made of aluminum and a second member 20 mainly made of nickel come into contact with each other, and a welded portion 30 formed by melting the periphery of the interface L. The welded portion 30 includes a plurality of protruding portions 61-64 each disposed along the interface L and protruding toward the first member 10 side beyond the interface L. Each of the plurality of protruding portions 61-64 includes a nickel-rich layer 40 having a higher ratio of nickel than aluminum, and an aluminum-rich layer 50 having a higher ratio of aluminum than nickel. In the welded cross section of each of the plurality of protruding portions 61-64, the area occupied by the aluminum-rich layer 50 is smaller than the area occupied by the nickel-rich layer 40.

[0025] In the welded structure 1 according to this embodiment, the aluminum-rich layer 50 in which blowholes are likely to occur is thin, which makes it difficult for blowholes to be connected three-dimensionally in the aluminum-rich layer 50. As a result, in the welded structure 1 formed by welding the first member 10 mainly made of aluminum and the second member 20 mainly made of nickel, sufficient joint strength can be stably obtained.

[0026] In the welded structure 1 according to the present embodiment, the roots of the multiple protruding portions 61-64 overlap each other. In such a structure, the distance between the multiple weld beads 31-34 is short, and in the process of sequentially forming the multiple weld beads 31-34, heat is likely to be transferred to the already formed weld beads, which may cause the aluminum-rich layer 50 to thicken and reduce the joint strength. However, in the welded structure 1 according to the present embodiment, even in the structure in which the roots of the multiple protruding portions 61-64 overlap each other, welding conditions that keep the area (thickness) of the aluminum-rich layer 50 thin as described above are determined in advance by experiments or the like, and the first member 10 and the second member 20 are welded under these welding conditions, so that the decrease in the joint strength can be stably suppressed.

[0027] [Variation 1] In the welded structure 1 according to the above-described embodiment, the roots of the plurality of projecting portions 61 to 64 overlap one another, but the plurality of projecting portions 61 to 64 may be spaced apart from one another.

[0028] Fig. 4 is a view of an example of a welded structure 1A according to Modification 1 as viewed from the Z direction. In welded structure 1A according to Modification 1, as shown in Fig. 4, a plurality of weld beads 31a to 34a are formed at predetermined distances in the Y direction.

[0029] 5 is a diagram showing a welded cross section of a welded structure 1A according to Modification 1. In the welded structure 1A according to Modification 1, a plurality of protruding portions 61a to 64a protruding toward the first member 10 side relative to the interface L are spaced apart from one another.

[0030] In welded structure 1A according to modification 1, multiple protruding portions 61a-64a are separated from one another, and the amount of heat transferred to already formed weld beads in the process of sequentially forming multiple weld beads 31a-34a can be reduced. This prevents aluminum-rich layer 50 from becoming thicker, making it more difficult for blowholes to form continuous connections. As a result, it is easier to prevent a decrease in the strength of the welded portion.

[0031] [Variation 2] In the above embodiment and modification 1, an example has been described in which linear weld beads 31-34 each extending in the X direction are aligned in the Y direction. However, the shape of the weld beads is not necessarily limited to being linear.

[0032] FIG. 6 is a view of an example of a welded structure 1B according to the present modified example 2, as viewed from the Z direction. In the welded structure 1B according to the present modified example 1, as shown in FIG. 6, one weld bead 31b is formed in a curved shape. Although there are some intersections in the weld beads 31b, most of the other portions are spaced apart from each other by a predetermined distance without overlapping. By preventing the weld beads 31b from overlapping in this manner, the amount of heat transferred to the already formed portion during the process of forming a new portion of the weld bead 31b can be reduced. As a result, as in the modified example 1, the aluminum-rich layer 50 is prevented from becoming thick, and blowholes are less likely to be connected, making it easier to prevent a decrease in the strength of the welded portion.

[0033] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present disclosure is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0034] 1, 1A, 1B welded structure, 10 first member, 20 second member, 20a outer surface, 30 welded portion, 31-34, 31a-34a, 31b weld bead, 40 nickel-rich layer, 50 aluminum-rich layer, 61-64, 61a-64a protruding portion, L interface.

Claims

1. A welded structure formed by welding a first member mainly made of aluminum and a second member mainly made of nickel, an interface where the first member and the second member contact each other; a weld formed by melting a portion of the interface, the welded portion includes a plurality of protruding portions each protruding toward the first member side relative to the interface, a nickel-rich layer having a higher ratio of nickel than aluminum, and an aluminum-rich layer having a higher ratio of aluminum than nickel, a welded structure, wherein an area of ​​the aluminum-rich layer is smaller than an area of ​​the nickel-rich layer in a weld cross section of each of the plurality of protruding portions.

2. The welded structure of claim 1 , wherein the plurality of protruding portions are spaced apart from one another.

3. The welded structure according to claim 1 , wherein the plurality of protruding portions overlap each other at their roots.

4. The weld portion has a plurality of bead portions each extending in a first direction and adjacent to each other in a direction intersecting the first direction, The welded structure according to claim 1 , wherein the plurality of protruding portions are formed at positions corresponding to the plurality of bead portions, respectively.

Citation Information

Patent Citations

  • Laser welding joint

    JP2017094382A

  • Production method for different material joined structure, and the structure

    JP2021030308A

  • Method for manufacturing joint structure of dissimilar materials

    JP2023008279A

  • Connecting structure of sealed battery and its manufacture

    JP1999073940A