Semiconductor device and method for manufacturing semiconductor device

By modifying the electrodes and insulating film surfaces with AlN-based and SiON-based layers through plasma nitriding, the semiconductor device addresses cracking issues and improves resistance to thermal stress, enhancing reliability and reducing processing complexity.

JP2024155630APending Publication Date: 2024-10-31MINEBEA POWER SEMICON DEVICE INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023070505
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

The silicon nitride passivation film used in semiconductor devices is prone to cracking due to thermal stress, leading to a decrease in high temperature and high humidity bias test resistance, and requires additional processing steps for removal in the active region.

Method used

A semiconductor device with a first semiconductor layer, a second semiconductor layer, an interlayer insulating film, and a field plate electrode, where the electrodes and insulating film surfaces are modified with an AlN-based and SiON-based modified layers formed through plasma nitriding, enhancing moisture resistance and reducing film stress.

Benefits of technology

The modified layers improve moisture resistance, prevent corrosion, and enhance high temperature and high humidity bias test resistance while reducing the number of processing steps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155630000001_ABST
    Figure 2024155630000001_ABST
Patent Text Reader

Abstract

To prevent cracking due to film stress and to improve resistance to high temperature and high humidity bias tests.SOLUTION: An IGBT chip 1 has an n-type semiconductor substrate 6, a p-type diffusion layer 8 partially formed on the surface portion of the n-type semiconductor substrate 6, an interlayer insulating film 9 in contact with the n-type semiconductor substrate 6 and the p-type diffusion layer 8, and a field plate electrode 12 in contact with the p-type diffusion layer 8 and the interlayer insulating film 9, the field plate electrode 12 has an AlN-based modified layer 21 on its surface, which is an inorganic film containing nitride, and the interlayer insulating film 9 has a SiON-based modified layer 22 on the surface, which is an inorganic film containing nitride.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. [Background technology]

[0002] One of the causes of the breakdown voltage degradation of power semiconductor chips is electric field concentration at the chip end. When a junction is formed on the surface of a power semiconductor chip, a depletion layer spreads in a fan shape at the end when a reverse bias is applied. The electric field lines of the charges in the fan-shaped region gather at the chip end, causing what is known as electric field concentration. As a result, avalanche breakdown (dielectric breakdown) occurs at a voltage significantly lower than the theoretical breakdown voltage. In order to alleviate electric field concentration at the chip termination, it is necessary to disperse the electric field lines from the charges in the depletion layer region that spread out like a fan when a reverse bias is applied from the chip termination to the entire termination structure (hereinafter also referred to as the termination region).

[0003] Power semiconductors are used in a variety of harsh environments, and therefore must satisfy multiple reliability requirements. One of the required reliability requirements is resistance to high temperature, high humidity bias testing (H3TRB), in which a constant voltage is continuously applied in a high temperature, high humidity environment. In power semiconductors with a field plate structure formed with Al electrodes, it is known that moisture in high-temperature, high-humidity environments can cause the Al electrodes to corrode, resulting in increased leakage current and a deterioration in voltage resistance.

[0004] Patent Document 1 describes a semiconductor device including a semiconductor portion, a termination insulating film, a first protective film, a second electrode, a termination electrode, a first insulating film, and a second protective film. It is also described that the semiconductor device described in Patent Document 1 has a passivation region formed of an inorganic film that prevents moisture from penetrating on the Al electrode. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent Publication No. 2022-047410 Summary of the Invention [Problem to be solved by the invention]

[0006] Silicon nitride films, which have excellent moisture resistance, are often used for the passivation film that forms the passivation region. However, silicon nitride films have a large stress, and depending on the film thickness, there is a risk of cracks occurring due to thermal stress caused by heat treatment in the process after the passivation film is formed or stress during mounting. If cracks occur, the moisture prevention function is lost, leading to a decrease in H3TRB resistance. Moreover, in the active region disposed on the main surface of the semiconductor substrate, the passivation film needs to be removed, which requires a processing step for removing the passivation film, resulting in an increase in the number of steps.

[0007] The present invention has been made in view of the above circumstances, and has an object to provide a semiconductor device that can prevent the occurrence of cracks due to film stress and improve resistance to a high-temperature, high-humidity bias test. [Means for solving the problem]

[0008] In order to solve the above problems, the semiconductor device of the present invention comprises a first semiconductor layer of a first conductivity type, a second semiconductor layer of a second conductivity type partially formed on a surface portion of the first semiconductor layer, an interlayer insulating film in contact with the first semiconductor layer and the second semiconductor layer, and a field plate electrode in contact with the second semiconductor layer and the interlayer insulating film, wherein the field plate electrode has a first modification layer on its surface made of an inorganic film containing a nitride, and the interlayer insulating film has a second modification layer on its surface made of an inorganic film containing the nitride. Effect of the Invention

[0009] According to the present invention, it is possible to prevent the occurrence of cracks due to film stress and to improve resistance to a high-temperature, high-humidity bias test. [Brief description of the drawings]

[0010] [Figure 1] 1 is a plan view showing an external appearance of a semiconductor device according to a first embodiment of the present invention. [Diagram 2] 2 is a cross-sectional view taken along the line AA' of FIG. [Figure 3A] 4A to 4C are cross-sectional views of a manufacturing process before forming a surface electrode of the semiconductor device according to the embodiment of the present invention. [Figure 3B] 3B is a cross-sectional view of a manufacturing process following FIG. 3A after forming a surface electrode. [Figure 3C] FIG. 3C is a cross-sectional view of the manufacturing process after plasma nitridation treatment subsequent to FIG. 3B. [Figure 3D] 3D is a cross-sectional view of a manufacturing process following FIG. 3C after forming an organic protective film. [Figure 3E] 3D is a cross-sectional view of the manufacturing process after removing the modified layer in the active area. [Figure 4] FIG. 11 is a plan view showing the appearance of a semiconductor device according to a second embodiment of the present invention. [Diagram 5] 5 is a cross-sectional view taken along the line BB' of FIG. [Figure 6A] 4A to 4C are cross-sectional views of a manufacturing process before forming a surface electrode of the semiconductor device according to the embodiment of the present invention. [Figure 6B] 6B is a cross-sectional view of a manufacturing process following FIG. 6A after forming a surface electrode. [Figure 6C] FIG. 6C is a cross-sectional view of the manufacturing process following FIG. 6B after plasma nitridation treatment. [Figure 6D] 6D is a cross-sectional view of a manufacturing process following FIG. 6C after forming an organic protective film. [Figure 6E] 6D is a cross-sectional view of the manufacturing process after removing the modified layer in the active region. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. In the drawings, the same components are designated by the same reference numerals, and detailed description of overlapping parts will be omitted. (First embodiment) 1 and 2 are diagrams showing a configuration of a semiconductor device according to a first embodiment of the present invention, in which Fig. 1 is a plan view showing the external appearance of the semiconductor device of the present embodiment, and Fig. 2 is a cross-sectional view taken along line A-A' in Fig. 1. In the following, an IGBT (Insulated Gate Bipolar Transistor) chip will be described as an example of a semiconductor device, but the subject matter of the present invention is not limited to this and can also be applied to diodes, thyristors, power MOSFETs, DMOSFETs (Double-Diffused MOSFETs), etc. An example of application to a diode will be described later.

[0012] 1, an IGBT chip 1 (semiconductor device) includes an active region 5 arranged on the main surface of a semiconductor substrate, and a termination region 4 arranged to surround the periphery of the active region 5. An emitter electrode 2 and a gate electrode pad 3 are formed on the active region 5. The termination region 4 is a termination structure that relieves electric field concentration at the chip termination portion of the IGBT chip 1, i.e., an electric field relief region.

[0013] 2, the termination region 4 includes, for example, a plurality of guard rings 7 (second semiconductor layer of second conductivity type) formed on the main surface of an n-type semiconductor substrate 6 (first semiconductor layer of first conductivity type), a p-type diffusion layer 8 (second semiconductor layer of second conductivity type), an interlayer insulating film 9 formed on the main surface of the semiconductor substrate 6, a gate wiring 10 formed in the interlayer insulating film 9, a gate electrode 11 formed on the interlayer insulating film 9 and connected to the gate wiring 10 through an opening formed in the interlayer insulating film 9, a field plate electrode 12 formed on the interlayer insulating film 9 and connected to the guard ring 7 through an opening formed in the interlayer insulating film 9, an emitter electrode 2 formed on the interlayer insulating film 9 and connected to the p-type diffusion layer 8 through an opening formed in the interlayer insulating film 9, and an organic protective film 13 formed to cover the interlayer insulating film 9 and the Al electrodes (emitter electrode 2, gate electrode 11, and field plate electrode 12). The gate electrode 11 is electrically connected to the gate electrode pad 3 shown in FIG.

[0014] The IGBT chip 1 has an active section 31 which is an active region that passes current, a gate finger section 32 which is a region having a gate wiring 10 and a gate electrode 11, and a termination section 33 which is a termination region that maintains a withstand voltage. The gate finger portion 32 has a well region (P-well) which is a diffusion layer and a gate electrode 11 electrically connected to the well region, and the termination region (termination portion 33) has a well region (P-well) which is a diffusion layer and a field plate electrode 12 electrically connected to the well region.

[0015] The n-type semiconductor substrate 6 is a Si substrate. The n-type semiconductor substrate 6 may be a SiC substrate, a GaN substrate, or the like. The guard ring 7 and the p-type diffusion layer 8 are p-type diffusion layers formed on the surface of the semiconductor substrate 6 by ion implantation. The interlayer insulating film 9 is made of a gate oxide film formed by pyrogenic oxidation or the like, which will be described later, and an interlayer film such as a TEOS (Tetra Ethoxy Silane) film or a BPSG (Boron-phospho silicate glass) film, all of which are silicon oxide films (SiO2).

[0016] The field plate electrode 12 is an electrode film made of a laminate film such as Ti / (in the following description, " / " indicates "or") TiN / Al, MoSi / Al, etc., and is formed in the same layer as the emitter electrode 2 and gate electrode pad 3 (FIG. 1) in the active region (active portion 31).

[0017] The emitter electrode 2, the gate wiring 10, the gate electrode 11, and the field plate electrode 12 are made of Al electrodes (Al-based electrodes).

[0018] The surfaces of the emitter electrode 2, gate electrode 11, and field plate electrode 12 in the inactive region are each formed by plasma nitriding the Al electrode itself (e.g., N2 plasma or NH3 plasma treatment) to form an AlN-based modified layer 21 (first modified layer). That is, the emitter electrode 2, gate electrode 11, and field plate electrode 12 in the inactive region have an AlN-based modified layer 21 formed on their surface portions by plasma nitriding. In this embodiment, plasma nitriding is used, but nitriding processes other than plasma, such as thermal nitriding, ion nitriding, or radical nitriding, may also be used.

[0019] The AlN-based modified layer 21 only modifies the surface of each electrode, so that the film thickness of each electrode remains the same as before the plasma nitriding process.

[0020] When the above-mentioned plasma nitridation process forms an AlN-based modified layer 21 on the surfaces of the emitter electrode 2, the gate electrode 11, and the field plate electrode 12, a SiON-based modified layer 22 (second modified layer) is simultaneously formed on the surface of the interlayer insulating film between each electrode.

[0021] That is, in one plasma nitridation process, an AlN-based modified layer 21 is formed on the surfaces of the emitter electrode 2, the gate electrode 11, and the field plate electrode 12, and a SiON-based modified layer 22 is formed on the surface of the interlayer insulating film 9 between each electrode.

[0022] The organic protective film 13 is, for example, a polyimide film. On the back surface of the semiconductor substrate 6, an n-type buffer layer 14, a p-type collector layer 15, and a collector electrode 16 are formed in this order from the substrate side.

[0023] The operation of the IGBT chip 1 configured as above will now be described. [IGBT chip 1 operation] When a voltage is applied between gate electrode 11 and emitter electrode 2 in the active region (active section 31), an n-channel inversion layer is formed directly below the gate oxide film of gate wiring 10, and the MOSFET portion turns ON. When a voltage is applied between collector electrode 16 and emitter electrode 2, an avalanche of holes occurs from collector electrode 16 toward emitter electrode 2, current flows between collector electrode 16 and emitter electrode 2, and the IGBT turns ON. When the voltage between gate electrode 11 and emitter electrode 2 is returned to 0 (zero), the inversion layer disappears, the n-channel of the MOSFET portion is cut off, and the IGBT turns OFF.

[0024] [Manufacturing method of IGBT chip 1] 3A to 3E are cross-sectional views showing the manufacturing process of the IGBT chip 1. Fig. 3A is a cross-sectional view of the manufacturing process before forming a surface electrode, Fig. 3B is a cross-sectional view of the manufacturing process after forming a surface electrode, Fig. 3C is a cross-sectional view of the manufacturing process after a plasma nitridation process, Fig. 3D is a cross-sectional view of the manufacturing process after forming an organic protective film, and Fig. 3E is a cross-sectional view of the manufacturing process after removing a modified layer in the active region. Each figure mainly shows a cross section of the termination region (termination portion 33) during the manufacturing process.

[0025] First, a gate oxide film (SiO2) (not shown) is formed on the main surface of an n-type semiconductor substrate 6 by selective oxidation using dry oxidation with dry oxygen (O2) or wet oxidation (pyrogenic oxidation) with water vapor generated by a combustion reaction of oxygen (O2) and hydrogen gas (H2). Then, a polysilicon film (Poly-Si) (not shown) is formed on the gate oxide film by a low-pressure CVD device or the like, and a gate electrode (11 in FIG. 2) is formed by patterning and etching using photolithography. Next, p-type impurities such as boron (B) are implanted into the main surface of the semiconductor substrate 6 by ion implantation to form p-type diffusion layers 7 and 8. This p-type diffusion layer 7 functions as a guard ring (7 in FIG. 2).

[0026] 3A, an interlayer insulating film (SiO2) 9 such as a TEOS film or a BPSG film is formed on the main surface of the semiconductor substrate 6 by using a plasma CVD apparatus, an atmospheric pressure CVD apparatus, or the like so as to cover the gate oxide film (not shown) and the gate wiring 10. Thereafter, an opening (contact hole) 17 is formed in the interlayer insulating film 9 by patterning and etching using photolithography, the opening (contact hole) 17 penetrating the p-type diffusion layer 8 and the guard ring 7. At this time, the opening (contact hole) 17 is also formed on the gate wiring 10.

[0027] 3B, an electrode film (not shown) made of, for example, Ti / TiN / Al, MoSi / Al, or the like is formed on the main surface of the semiconductor substrate 6 by a plasma CVD apparatus, a sputtering apparatus, or the like so as to cover the interlayer insulating film 9 and fill the opening (contact hole) 17 formed in the interlayer insulating film 9. Thereafter, the emitter electrode 2, the gate electrode 11, and the field plate electrode 12 (FIG. 2) are formed by patterning and etching using photolithography.

[0028] 3C, a plasma nitridation process using N2 plasma or NH3 plasma is performed to form modified layers (AlN-based modified layer 21 and SiON-based modified layer 22) on the surfaces of the Al electrodes (emitter electrode 2, gate electrode 11, and field plate electrode 12) and the interlayer insulating film 9. That is, by a single plasma nitridation process step, the AlN-based modified layer 21 is formed on the surfaces of the emitter electrode 2, gate electrode 11, and field plate electrode 12, and the SiON-based modified layer 22 is formed on the surface of the interlayer insulating film 9 between the electrodes.

[0029] The AlN-based modified layer 21 only modifies the surface of each electrode, so that the film thickness of each electrode remains the same as before the plasma nitriding process.

[0030] Next, as shown in FIG. 3D, an organic protective film (polyimide film) 13 is applied onto the main surface of the semiconductor substrate 6 by a coating device so as to cover the emitter electrode 2 having the AlN-based modified layer 21, the gate electrode 11, and the field plate electrode 12.

[0031] Next, as shown in FIG. 3E, the AlN-based modified layer 21 on the surface of the emitter electrode 2 in the active region is removed by patterning and etching using photolithography.

[0032] Finally, on the back surface of the semiconductor substrate 6, an n-type buffer layer 14, a p-type collector layer 15, and a collector electrode 16 are formed in this order from the substrate side in a back surface process. Through the manufacturing process described above, the termination structure shown in FIG. 2 is formed.

[0033] As described above, the IGBT chip 1 (semiconductor device) (FIGS. 1 and 2) of this embodiment includes an n-type semiconductor substrate 6 (first semiconductor layer of a first conductivity type), a p-type diffusion layer 8 (second semiconductor layer of a second conductivity type) partially formed on a surface portion of the n-type semiconductor substrate 6, an interlayer insulating film 9 in contact with the n-type semiconductor substrate 6 and the p-type diffusion layer 8, and a field plate electrode 12 in contact with the p-type diffusion layer 8 and the interlayer insulating film 9, where the field plate electrode 12 has, on its surface, an AlN-based modified layer 21 (first modified layer) made of an inorganic film formed by plasma nitridation treatment, and the interlayer insulating film 9 has, on its surface, a SiON-based modified layer 22 (second modified layer) made of an inorganic film formed by nitridation treatment (e.g., plasma nitridation treatment).

[0034] In addition, the manufacturing method of the IGBT chip 1 (Figures 3A to 3E) includes the steps of partially forming a p-type diffusion layer 8 (second semiconductor layer of second conductivity type) on a surface portion of an n-type semiconductor substrate 6 (first semiconductor layer of first conductivity type), forming an interlayer insulating film 9 in contact with the n-type semiconductor substrate 6 and the p-type diffusion layer 8, forming a field plate electrode 12 in contact with the p-type diffusion layer 8 and the interlayer insulating film 9, and nitriding (e.g., plasma nitriding) the field plate electrode 12 and the interlayer insulating film 9 to form a modified layer containing nitride on the surface (AlN-based modified layer 21, SiON-based modified layer 22).

[0035] After the field plate electrode 12 is formed in this manner, the Al electrodes (emitter electrode 2, gate electrode 11, and field plate electrode 12) themselves are subjected to plasma nitridation (e.g., N2 plasma, NH3 plasma, etc.). By the plasma nitridation, an AlN-based modified layer 21 is formed on the surfaces of the emitter electrode 2, gate electrode 11, and field plate electrode 12, and at the same time, a SiON-based modified layer 22 is also formed on the surface of the interlayer insulating film 9 between the electrodes.

[0036] The AlN-based modified layer 21 of the IGBT chip 1 (FIGS. 1 and 2) of this embodiment improves the moisture resistance of the surface of the Al electrode, thereby preventing corrosion of the Al electrode and improving H3TRB resistance. The AlN-based modified layer 21 only modifies the surface of each Al electrode, so the thickness of each electrode remains the same as before the plasma nitriding process, preventing the occurrence of cracks due to film stress.

[0037] Moreover, the SiO2 interlayer insulating film 9 is also nitrided at the same time, and the surface becomes a SiON layer, which makes it possible to prevent moisture from penetrating through the interlayer insulating film 9, and is expected to improve H3TRB resistance.

[0038] As described above, it is possible to reliably prevent the intrusion of moisture from the front surface side of the IGBT chip 1 while suppressing the occurrence of cracks due to film stress, and to improve resistance to a high-temperature, high-humidity bias test.

[0039] Furthermore, the process of removing the passivation film is no longer necessary in the active region disposed on the main surface of the semiconductor substrate, and the number of processes can be reduced.

[0040] The IGBT chip 1 (Figures 1 and 2) of this embodiment has an emitter electrode 2 in contact with a p-type diffusion layer 8 (second semiconductor layer) and an interlayer insulating film 9, and the emitter electrode 2 has an AlN-based modified layer 21 on its surface formed by plasma nitridation treatment.

[0041] In this way, the AlN-based modified layer 21 (first modified layer) of the IGBT chip 1 improves the moisture resistance of the surface of the emitter electrode 2, thereby preventing corrosion of the emitter electrode 2 and improving the H3TRB resistance. Also, the occurrence of cracks due to film stress in the emitter electrode 2 can be suppressed.

[0042] In the IGBT chip 1 (FIGS. 1 and 2) of this embodiment, the field plate electrode 12 is an aluminum-based electrode, and the AlN-based modified layer 21 is aluminum nitride obtained by modifying the aluminum-based electrode through plasma nitriding.

[0043] By doing so, the AlN-based modified layer 21 of the IGBT chip 1 improves the moisture resistance of the surface of the emitter electrode 2, thereby preventing corrosion of the emitter electrode 2 and improving the H3TRB resistance.

[0044] In the IGBT chip 1 (FIGS. 1 and 2) of this embodiment, the SiON-based modified layer 22 (second modified layer) is silicon oxynitride.

[0045] By doing so, the SiON-based modified layer 22 of the IGBT chip 1 can also prevent moisture from penetrating through the interlayer insulating film 9, and the H3TRB resistance can be improved.

[0046] The IGBT chip 1 (Figures 1 and 2) of this embodiment comprises an active region (active portion 31) arranged on the main surface of the semiconductor substrate, and a termination region (termination portion 33) arranged on the main surface so as to surround the active region, and the termination region comprises a field plate electrode 12 and an interlayer insulating film 9.

[0047] In this way, the IGBT chip 1 can realize a highly reliable semiconductor device that can improve the high-temperature, high-humidity bias resistance of the chip termination structure (termination region) in a relatively simple manner while suppressing the effects on device characteristics.

[0048] In the IGBT chip 1 (FIGS. 1 and 2) of this embodiment, the AlN-based modified layer 21 (first modified layer) of the emitter electrode 2 in the active region arranged on the main surface of the semiconductor substrate is removed.

[0049] In this manner, the IGBT chip 1 can be electrically connected to the emitter electrode 2 by removing the AlN-based modified layer 21 of the emitter electrode 2 in the active region.

[0050] Second embodiment Fig. 4 and Fig. 5 are diagrams showing the configuration of a semiconductor device according to a second embodiment of the present invention. Fig. 4 is a plan view showing the appearance of the semiconductor device of this embodiment, and Fig. 5 is a cross-sectional view taken along line B-B' in Fig. 4. This is an example in which the semiconductor device is applied to a diode.

[0051] 4, diode 50 (semiconductor device) includes active region 55 arranged on the main surface of a semiconductor substrate, and termination region 54 arranged to surround active region 55. Termination region 54 is a termination structure that relieves electric field concentration at the chip termination portion of diode 50, i.e., an electric field relief region.

[0052] As shown in FIG. 4, termination region 54 has, for example, a plurality of guard rings 57 formed on the main surface of n-type semiconductor substrate 56, a P layer 58, an interlayer insulating film 59 formed on the main surface of semiconductor substrate 56, a field plate electrode 61 formed on interlayer insulating film 59 and connected to guard ring 57 through an opening formed in interlayer insulating film 59, an anode electrode 60 formed on interlayer insulating film 59 and connected to P layer 58 through an opening formed in interlayer insulating film 59, and an organic protective film 63 formed to cover interlayer insulating film 59 and Al electrodes (anode electrode 60, field plate electrode 61).

[0053] Diode 50 has an active portion 81 which is an active region that passes current, and a termination portion 82 which is a termination region that maintains a withstand voltage. The active region (active portion 81) has a P layer 58 and an anode electrode 60. The termination region (termination portion 82) has a well region (P-well) which is a diffusion layer, and a field plate electrode 61 electrically connected to the well region.

[0054] The n-type semiconductor substrate 56 is a Si substrate. The n-type semiconductor substrate 56 may be a SiC substrate, a GaN substrate, or the like. The guard ring 57 is a p-type diffusion layer formed on the surface of the semiconductor substrate 56 by ion implantation. The P layer 58 is connected to an anode electrode 60 and serves as the anode of the diode 50 . The interlayer insulating film 59 is made of a gate oxide film formed by pyrogenic oxidation or the like, and an interlayer film such as a TEOS film or a BPSG film, both of which are silicon oxide films (SiO2).

[0055] The field plate electrode 61 is an electrode film made of a laminated film of, for example, Ti / TiN / Al, MoSi / Al, or the like, and is formed in the same layer as the anode electrode 60 in the active region (active portion 81).

[0056] The anode electrode 60 and the field plate electrode 61 are made of Al electrodes (Al-based electrodes).

[0057] The surfaces of the anode electrode 60 and the field plate electrode 61 in the inactive region are each subjected to plasma nitriding (e.g., N2 plasma or NH3 plasma treatment) of the Al electrode itself, forming an AlN-based modified layer 71. That is, the anode electrode 60 and the field plate electrode 61 in the inactive region have an AlN-based modified layer 71 formed on their surface portions by plasma nitriding.

[0058] Since the AlN-based modified layer 71 only modifies the surface of each electrode, the film thickness of each electrode remains the same as before the plasma nitriding process.

[0059] When the AlN-based modified layer 71 is formed on the surfaces of the anode electrode 60 and the field plate electrode 61 by the above-mentioned plasma nitridation process, a SiON-based modified layer 72 is also formed on the surface of the interlayer insulating film between the electrodes.

[0060] That is, in one plasma nitridation process, an AlN-based modified layer 71 is formed on the surfaces of the anode electrode 60 and the field plate electrode 61, and a SiON-based modified layer 72 is formed on the surface of the interlayer insulating film 59 between the electrodes.

[0061] The organic protective film 63 is, for example, a polyimide film. On the back surface of the semiconductor substrate 6, an n-type buffer layer 64, an N + On layer 65, a cathode electrode 66 is formed.

[0062] A method for manufacturing the diode 50 configured as above will now be described. 6A to 6E are cross-sectional views showing the manufacturing process of the diode 50. Fig. 6A is a cross-sectional view of the manufacturing process before forming a front surface electrode, Fig. 6B is a cross-sectional view of the manufacturing process after forming a front surface electrode, Fig. 6C is a cross-sectional view of the manufacturing process after a plasma nitridation process, Fig. 6D is a cross-sectional view of the manufacturing process after forming an organic protective film, and Fig. 6E is a cross-sectional view of the manufacturing process after removing a modified layer in the active region. Each figure mainly shows a cross section of the termination region (termination portion 82) during the manufacturing process.

[0063] First, a gate oxide film (SiO2) (not shown) is formed on the main surface of an n-type semiconductor substrate 56 by selective oxidation using dry oxidation with dry oxygen (O2) or wet oxidation (pyrogenic oxidation) with water vapor generated by a combustion reaction of oxygen (O2) and hydrogen gas (H2). Then, a polysilicon film (Poly-Si) (not shown) is formed on the gate oxide film by a low-pressure CVD device or the like, and a gate electrode (reference numeral 11 in FIG. 2) is formed by patterning and etching using photolithography. Next, a p-type impurity such as boron (B) is implanted into the main surface of the semiconductor substrate 56 by ion implantation to form a p-type diffusion layer 57 and a P layer 58. This p-type diffusion layer 57 functions as a guard ring (reference numeral 57 in FIG. 5). The P layer 58 becomes the anode of the diode 50.

[0064] 6A, an interlayer insulating film (SiO2) 59 such as a TEOS film or a BPSG film is formed on the main surface of the semiconductor substrate 56 using a plasma CVD device, an atmospheric pressure CVD device, or the like. After that, an opening (contact hole) 67 penetrating the interlayer insulating film 9 to the guard ring 57 is formed by patterning and etching using photolithography.

[0065] 6B, an electrode film (not shown) made of, for example, Ti / TiN / Al, MoSi / Al, or the like is formed on the main surface of semiconductor substrate 56 by a plasma CVD apparatus, a sputtering apparatus, or the like so as to cover interlayer insulating film 59 and fill openings (contact holes) 67 formed in interlayer insulating film 59. Thereafter, an anode electrode 60 and a field plate electrode 61 (FIG. 5) are formed by patterning and etching using photolithography.

[0066] 6C, a plasma nitridation process using N2 plasma or NH3 plasma is performed to form modified layers (AlN-based modified layer 71 and SiON-based modified layer 72) on the surfaces of the Al electrodes (anode electrode 60 and field plate electrode 61) and the interlayer insulating film 9. That is, by a single plasma nitridation process step, the AlN-based modified layer 71 is formed on the surfaces of the anode electrode 60 and the field plate electrode 61, and the SiON-based modified layer 72 is formed on the surface of the interlayer insulating film 59 between the electrodes.

[0067] Since the AlN-based modified layer 71 only modifies the surface of each electrode, the film thickness of each electrode remains the same as before the plasma nitriding process.

[0068] Next, as shown in FIG. 6D, an organic protective film (polyimide film) 63 is applied onto the main surface of the semiconductor substrate 56 by a coating device so as to cover the anode electrode 60 having the AlN-based modified layer 71 and the field plate electrode 61.

[0069] Next, as shown in FIG. 6E, the AlN-based modified layer 71 on the surface of the anode electrode 60 in the active region is removed by patterning and etching using photolithography.

[0070] Finally, in a back surface process, an n-type buffer layer 64, an N + Layer 65 forms the cathode electrode 66 . Through the manufacturing process described above, the termination structure shown in FIG. 5 is formed.

[0071] As described above, the diode 50 (semiconductor device) (FIGS. 4 and 5) of this embodiment includes an n-type semiconductor substrate 56 (first semiconductor layer of a first conductivity type), a p-type diffusion layer 57 (second semiconductor layer of a second conductivity type) partially formed on a surface portion of the n-type semiconductor substrate 56, an interlayer insulating film 59 in contact with the n-type semiconductor substrate 56 and the p-type diffusion layer 57, and a field plate electrode 61 in contact with the p-type diffusion layer 57 and the interlayer insulating film 59. The field plate electrode 61 has, on its surface, an AlN-based modified layer 71 (first modified layer) made of an inorganic film (containing nitride) formed by nitriding (e.g., plasma nitriding), and the interlayer insulating film 59 has, on its surface, a SiON-based modified layer 72 (second modified layer) made of an inorganic film (containing nitride) formed by nitriding (e.g., plasma nitriding).

[0072] Furthermore, the manufacturing method of diode 50 (FIGS. 6A to 6E) includes the steps of partially forming a p-type diffusion layer 57 (second semiconductor layer of second conductivity type) on a surface portion of an n-type semiconductor substrate 56 (first semiconductor layer of first conductivity type), forming an interlayer insulating film 59 in contact with the n-type semiconductor substrate 56 and the p-type diffusion layer 57, forming a field plate electrode 61 in contact with the p-type diffusion layer 57 and the interlayer insulating film 59, and nitriding (e.g., plasma nitriding) the field plate electrode 61 and the interlayer insulating film 59 to form modified layers (AlN-based modified layer 71, SiON-based modified layer 72) made of an inorganic film containing nitride on the surface.

[0073] By doing this, in the diode 50 of this embodiment (Figures 4 and 5), like the IGBT chip 1 of the first embodiment (Figures 1 and 2), the AlN-based modified layer 71 improves the moisture resistance of the surface of the Al electrode, thereby preventing corrosion of the Al electrode and improving H3TRB resistance.

[0074] The AlN-based modified layer 71 only modifies the surface of each Al electrode, so the thickness of each electrode remains the same as before the plasma nitriding process, preventing the occurrence of cracks due to film stress.

[0075] In addition, the SiO2 interlayer insulating film 59 is also nitrided at the same time, and the surface becomes a SiON layer, which makes it possible to prevent moisture from penetrating through the interlayer insulating film 59, and is expected to improve H3TRB resistance.

[0076] As described above, it is possible to reliably prevent moisture from entering from the front surface side of the diode 50 while suppressing the occurrence of cracks due to film stress, and to improve resistance to a high-temperature, high-humidity bias test.

[0077] Furthermore, the process of removing the passivation film is no longer necessary in the active region disposed on the main surface of the semiconductor substrate, and the number of processes can be reduced.

[0078] The diode 50 of this embodiment (Figures 4 and 5) includes an anode electrode 60 in contact with a p-type diffusion layer 57 (second semiconductor layer) and an interlayer insulating film 59, and the anode electrode 60 has an AlN-based modified layer 71 formed on its surface by plasma nitridation treatment.

[0079] In this way, in the diode 50, the AlN-based modified layer 71 (first modified layer) improves the moisture resistance of the surface of the emitter electrode 2, thereby preventing corrosion of the anode electrode 60 and improving the H3TRB resistance. Also, in the anode electrode 60, the occurrence of cracks due to film stress can be suppressed.

[0080] In the diode 50 of this embodiment (FIGS. 4 and 5), the AlN-based modified layer 71 (first modified layer) of the anode electrode 60 in the active region disposed on the main surface of the semiconductor substrate is removed.

[0081] In this manner, the diode 50 can be electrically connected to the anode electrode 60 by removing the AlN-based modified layer 71 of the anode electrode 60 in the active region.

[0082] The present invention is particularly effective for high-voltage products that often have a structure in which guard rings 7, 57 and field plate electrodes 12, 61 are provided in the termination region as described above, but is not necessarily limited to this. It can also be applied to semiconductor chips that employ other termination structures that do not use guard rings 7, 57 or field plate electrodes 12, 61, and to products with relatively low voltage resistance.

[0083] Furthermore, the present invention is not limited to the above-described embodiments, but includes various modified examples. For example, the above-described embodiments have been described in detail to aid in understanding the present invention, and the present invention is not necessarily limited to those having all of the configurations described. Furthermore, it is possible to replace a part of the configuration of one embodiment with the configuration of another embodiment, and it is also possible to add the configuration of another embodiment to the configuration of one embodiment. Furthermore, it is possible to add, delete, or replace a part of the configuration of each embodiment with another configuration. For example, IGBTs are used, but other types of elements can be applied. Depending on the device, the main terminals and sense terminals are called "drain" and "source" instead of the above-mentioned "collector" and "emitter". [Explanation of symbols]

[0084] 1. IGBT chip (semiconductor device) 2 Emitter electrode 3 Gate electrode pad 6, 56 Semiconductor substrate (first semiconductor layer of first conductivity type) 7,57 Guard Ring 8 p-type diffusion layer (second semiconductor layer of second conductivity type) 9,59 Interlayer insulating film 10 Gate wiring 11 Gate electrode 12,61 Field plate electrode 13,63 Organic protective film 14 n-type buffer layer 15 p-type collector layer 16 Collector electrode 21,71 AlN-based modified layer (first modified layer) 22,72 SiON-based modified layer (second modified layer) 31,81 Active part (active area) 32 Gate finger part 33,82 Termination section (termination area) 50 Diode (semiconductor device) 58 P layer 64 n-type buffer layer 65 N + layer 66 Cathode Electrode

Claims

1. a first semiconductor layer of a first conductivity type; a second semiconductor layer of a second conductivity type partially formed on a surface portion of the first semiconductor layer; an interlayer insulating film in contact with the first semiconductor layer and the second semiconductor layer; and a field plate electrode in contact with the second semiconductor layer and the interlayer insulating film; the field plate electrode has a first modified layer on a surface thereof, the first modified layer being made of an inorganic film containing a nitride; The interlayer insulating film has a second modified layer on a surface thereof, the second modified layer being an inorganic film containing the nitride. A semiconductor device comprising:

2. an emitter electrode in contact with the second semiconductor layer and the interlayer insulating film; The emitter electrode has the first modified layer containing the nitride on a surface thereof.

2. The semiconductor device according to claim 1,

3. an anode electrode in contact with the second semiconductor layer and the interlayer insulating film; The anode electrode has the first modified layer containing the nitride on a surface thereof.

2. The semiconductor device according to claim 1,

4. the field plate electrode is an aluminum-based electrode, The first modified layer is aluminum nitride obtained by modifying the aluminum-based electrode through the nitriding treatment.

2. The semiconductor device according to claim 1,

5. The second modified layer is silicon oxynitride.

2. The semiconductor device according to claim 1,

6. an active region disposed on a major surface of a semiconductor substrate; a termination region disposed on the main surface so as to surround the active region; The termination region includes the field plate electrode and the interlayer insulating film.

2. The semiconductor device according to claim 1,

7. The first modified layer of the emitter electrode in the active region disposed on the main surface of the semiconductor substrate is removed.

3. The semiconductor device according to claim 2.

8. The first modified layer of the anode electrode in the active region disposed on the main surface of the semiconductor substrate is removed.

4. The semiconductor device according to claim 3.

9. partially forming a second semiconductor layer of a second conductivity type on a surface portion of the first semiconductor layer; forming an interlayer insulating film in contact with the first semiconductor layer and the second semiconductor layer; forming a field plate electrode in contact with the second semiconductor layer and the interlayer insulating film; and a step of nitriding the field plate electrode and the interlayer insulating film to form a modified layer made of an inorganic film containing nitride on the surface.

4. A method for manufacturing a semiconductor device comprising the steps of:

Citation Information

Patent Citations

  • Semiconductor device

    JP2022047410A