Gallium-nitride high-electron-mobility transistor having p-type layer deeply injected into silicon carbide substrate
By employing a SiC substrate with a high purity GaN buffer layer and controlled p-type material layer formation, the drain lag effect in GaN HEMTs is mitigated, achieving high voltage capability and efficient switching for power and RF applications.
Patent Information
- Application Number
- JP2024146206
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2017-02-03
- Filing Date
- 2024-08-28
- Publication Date
- 2024-10-31
AI Technical Summary
Gallium nitride (GaN)-based high electron mobility transistors (HEMTs) face issues with drain lag effect due to iron (Fe) or carbon (C) implantation, leading to reduced switching current and efficiency, and leakage current through the buffer layer, which are undesirable for high-power and radio frequency applications.
The use of a silicon carbide (SiC) substrate with a high purity GaN buffer layer and a p-type material layer formed through controlled ion implantation and annealing, eliminating Fe and C, and optimizing breakdown voltage without drain lag.
This approach enables GaN HEMTs with high voltage capability, minimizing drain lag effects, reducing leakage current, and enhancing switching efficiency, suitable for power switching and high-power RF devices.
Smart Images

Figure 2024156010000001_ABST
Abstract
Description
[Technical field]
[0001] [CROSS REFERENCE TO RELATED APPLICATIONS] This application is a continuation-in-part of U.S. patent application Ser. No. 15 / 192,545, filed Aug. 15, 2016, the entirety of which is incorporated herein by reference.
[0002] Field of the Disclosure The present disclosure relates to microelectronic devices, and more particularly to gallium nitride high electron mobility transistors having p-type layers. The present disclosure further relates to methods of manufacturing microelectronic devices, and more particularly to methods of manufacturing gallium nitride high electron mobility transistors having p-type layers. [Background technology]
[0003] Gallium nitride (GaN) based high electron mobility transistors (HEMTs) are very promising candidates for high power radio frequency (RF) applications as well as low frequency high power switching applications due to the high voltage and high current that can be achieved due to the material properties of GaN. However, a significant problem in these devices is the design of the buffer layer to achieve high voltage functionality. Currently, many designs use deep level implants of iron (Fe) or carbon (C) to minimize the current through the buffer layer under high drain voltage conditions. However, both Fe and C cause the drain lag effect, i.e., the delayed recovery of the drain current when the drain voltage changes from a high value to a low value. This is highly undesirable for both power and RF applications as it causes switching current degradation, efficiency loss, and other problems. The drain lag effect can be eliminated by using a high purity buffer layer that does not contain Fe or C. However, these devices still have leakage current through the buffer layer, which is also unacceptable.
[0004] Therefore, an alternative solution is needed to address the lag effect in GaN HEMTs. Summary of the Invention
[0005] According to an aspect of the disclosure, there is provided a high electron mobility transistor comprising: a SiC substrate layer; a GaN buffer layer disposed on the SiC substrate layer; and a p-type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is disposed, the p-type material layer being disposed on one of the SiC substrate layer and a first layer disposed on the SiC substrate layer.
[0006] According to another aspect of the disclosure, there is provided a method for manufacturing a high electron mobility transistor, comprising: providing a SiC substrate layer; providing a GaN buffer layer on the SiC substrate layer; and providing a p-type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is provided, and further comprising providing the p-type material layer in one of the SiC substrate and a first layer disposed on the SiC substrate layer.
[0007] Further features, advantages, and aspects of the present disclosure will be set forth or become apparent upon consideration of the following detailed description, drawings, and claims. Moreover, it should be understood that both the foregoing summary of the disclosure and the following detailed description are exemplary and are intended to provide further explanation without limiting the scope of the present disclosure as set forth in the claims. The accompanying drawings, which are included to provide a further understanding of the present disclosure, are incorporated in and constitute a part of this specification, illustrate aspects of the disclosure, and together with the detailed description, serve to explain the principles of the disclosure. No attempt is made to show details of the disclosed structure in more detail than is necessary for a fundamental understanding of the disclosure and the various ways in which it may be practiced. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 shows a cross-sectional view of one embodiment of a transistor according to the present disclosure. [Diagram 2]FIG. 2 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Diagram 3] FIG. 3 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Figure 4] FIG. 4 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Diagram 5] FIG. 5 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Figure 6] FIG. 6 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Figure 7] FIG. 7 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. [Figure 8] FIG. 8 illustrates a method for fabricating a transistor according to the present disclosure. [Figure 9] FIG. 9 shows the distribution of Al implanted under channeling conditions according to an embodiment of the present disclosure compared to a simulation under conventional implant conditions. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The embodiments of the present disclosure and various features and advantageous details thereof will be more fully described with reference to the non-limiting embodiments and examples described and / or shown in the accompanying drawings and described in detail in the following specification. Those skilled in the art will recognize that the features shown in the drawings are not necessarily drawn to scale, and it should be noted that features of one embodiment may be used in another embodiment, even if not explicitly stated in the specification. Descriptions of well-known elements and processing techniques may be omitted so as not to unnecessarily obscure the embodiments of the present disclosure. The examples used in the specification are merely intended to aid in the understanding of the methods used in the present disclosure and further enable those skilled in the art to practice the embodiments of the present disclosure. Thus, the embodiments and examples in the specification should not be construed as limiting the scope of the present disclosure, which is defined only by the appended claims and applicable law. Furthermore, it should be noted that like reference numerals represent like parts throughout the representations of the several figures.
[0010] Terms such as first, second, etc. are used to describe various elements used herein, but it should be understood that these elements should not be limited by these terms. These terms are used only to distinguish one element from another element. For example, a first element can be referred to as a second element, and similarly, a second element can be referred to as a first element, without departing from the scope of the present disclosure. As used herein, the term "and / or" includes any or all combinations of one or more of the listed items.
[0011] When an element, such as a layer, region, or substrate, is referred to as being "on" or extending "onto" another element, it is understood that it can be directly on or extend directly onto the other element, or intervening elements may be present. In contrast, when an element is referred to as being "directly on" or extending "directly onto" another element, there are no intervening elements. Similarly, when an element, such as a layer, region, or substrate, is referred to as being "over" or extending "over" another element, it is understood that it can be directly on or extend directly onto the other element, or intervening elements may be present. In contrast, when an element is referred to as being "directly over" or extending "directly over" another element, there are no intervening elements. When an element is referred to as being "connected" or "coupled" to another element, it should be understood that the element can be directly connected or coupled to the other element, or intervening elements may be present. In contrast, when an element is referred to as being "directly connected" or "directly coupled" to another element, there are no intervening elements present.
[0012] Relative terms such as "below" or "above" or "upper" or "lower" or "horizontal" or "vertical" may be used herein to describe the relationship of one element, layer, or region to another element, layer, or region shown in the figures. It is understood that these terms and their above-discussed aspects are intended to encompass different orientations of the device in addition to the orientation depicted in the figures.
[0013] The terms used in the specification are intended to describe only certain embodiments and are not intended to limit the disclosure. As used in the specification, the singular forms "a", "an" and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It is further understood that the terms "comprises", "comprising", "includes" and / or "including" as used in the specification specify the presence of stated features, integers, steps, operations, elements and / or components, and do not exclude the presence of one or more other features, integers, steps, operations, elements, components and / or groups thereof.
[0014] Unless otherwise defined, all terms (including technical and scientific terms) used in the specification have the same meaning as commonly understood by those skilled in the art to which this disclosure belongs. It should be understood that terms used in the specification should be interpreted to have a meaning that is not inconsistent with the meaning in the context of this specification and the related art, and should not be interpreted in an idealized or overly formal sense unless expressly defined in the specification.
[0015] In addition to the type of structure, the properties of the semiconductor material from which a transistor is formed can also affect the operating parameters. The properties that affect the operating parameters of a transistor, such as electron mobility, saturated electron drift velocity, dielectric breakdown field, and thermal conductivity, can affect the high frequency and high power characteristics of the transistor.
[0016] Electron mobility is a measure of how quickly electrons accelerate to their saturation velocity in the presence of an electric field. Traditionally, semiconductor materials with high electron mobility have been preferred because they can generate more current with less electric field and have a faster response time when an electric field is applied. Saturation electron drift velocity is the maximum speed at which electrons can be captured inside the semiconductor material. Materials with higher saturation electron drift velocity are preferred for high frequency applications because they can move from source to drain in a short time due to their higher speed.
[0017] The breakdown field is the electric field strength at which a Schottky junction breaks down, causing a sudden increase in the current passing through the gate of the device. High breakdown field materials are preferred for high power, high frequency transistors because a larger electric field can generally be supported by a given material size. Electrons are accelerated faster by a larger electric field than by a smaller field, so a larger electric field allows for faster movement.
[0018] Thermal conductivity is the ability of a semiconductor material to dissipate heat. In typical operation, all transistors generate heat. Similarly, high power and high frequency transistors usually generate a greater amount of heat than small signal transistors. As the temperature of a semiconductor material increases, the junction leakage current generally increases and the current passing through a field effect transistor generally decreases due to the decrease in carrier mobility with increasing temperature. Thus, if heat can be dissipated from the semiconductor, the material can maintain a lower temperature and also carry a larger current with less leakage current.
[0019] The present disclosure includes both extrinsic and intrinsic semiconductors. Intrinsic semiconductors are undoped (pure). Extrinsic semiconductors are doped, meaning that a substance is introduced to modify the electron and hole carrier density of the semiconductor at thermal equilibrium. Both p-type and n-type semiconductors are disclosed, with p-type having a hole density greater than the electron density and n-type having a electron density greater than the hole density.
[0020] Silicon carbide (SiC) has excellent physical and electronic properties that theoretically allow the fabrication of electronic devices that can operate at higher temperatures, higher power, and higher frequencies than devices fabricated from silicon (Si) or gallium arsenide (GaAs). A high dielectric breakdown field of about 4×E6V / cm, a high saturated electron drift velocity of about 2.0×E7cm / sec, and a high thermal conductivity of about 4.9W / cm-°K make SiC well suited for high frequency and high power applications.
[0021] Drain lug in the disclosed GaN HEMTs is addressed in some embodiments by adding structures. In these structures, a p-type layer is used to simultaneously achieve high breakdown voltage and no drain lug. The p-type layer helps optimize the breakdown voltage and can be easily charged and discharged, thereby ensuring no drain lug. In one embodiment, the p-type layer is formed on a SiC substrate.
[0022] This approach overcomes two problems: 1. It is difficult to form a p-type layer in GaN using ion implantation. Selective ion implantation allows for optimization of device structures by obtaining different densities in different regions, which is made more difficult with epitaxial growth. 2. The p-type doping of GaN with magnesium (Mg) also exhibits a memory effect that prevents the growth of an abrupt interface.
[0023] The disclosed methods and structures may enable the development of GaN HEMTs with high breakdown voltage capability suitable for power switching without adverse lag effects. The disclosed methods and structures may also lead to lower cost and more compact device structures. Furthermore, with proper design, the disclosed structures may be applicable to high power RF devices for communications and other applications. An important advantage is minimizing the memory effect of the device, which is a serious challenge in communications applications.
[0024] FIG. 1 illustrates a cross-sectional view of one embodiment of a transistor according to the present disclosure, and FIG. 2 illustrates a cross-sectional view of another embodiment of a transistor according to the present disclosure. In particular, FIG. 1 illustrates a cross-sectional view of a transistor 100. The transistor 100 may include a substrate layer 102. The substrate layer 102 may be comprised of silicon carbide (SiC). In some embodiments, the substrate layer 102 may be a semi-insulating SiC substrate, a p-type substrate, an n-type substrate, or the like. In some embodiments, the substrate layer 102 may be very lightly doped. In one embodiment, the background impurity level may be low. In one embodiment, the background impurity level may be 1E15 / cm3 or less. The substrate layer 102 may be formed of SiC selected from the group of 6H, 4H, 15R 3C SiC, or the like.
[0025] In alternative embodiments, the substrate layer 102 may be GaAs, GaN, or other materials suitable for the applications described herein. In alternative embodiments, the substrate layer 102 may be sapphire, spinel, ZnO, silicon, or any other material capable of supporting the growth of group-III nitride materials.
[0026] The substrate layer 102 may include a p-type material layer 120. The p-type material layer 120 may be formed by ion implantation of aluminum (Al) and annealing. In other embodiments, the p-type material layer 120 may be formed by ion implantation of boron, gallium, or any other material capable of forming a p-type layer. In one embodiment, the p-type material layer 120 may be formed by implantation of Al and annealing prior to the growth of any GaN layer. In one embodiment, the ion implantation may use channeling implantation. In one embodiment, the channeling implantation may include aligning an ion beam to the substrate layer 102. Aligning the ion beam may increase the efficiency of the implantation.
[0027] Aspects of the present disclosure are based on the recognition that implant channeling can be used to controllably create implanted regions in silicon carbide that are highly uniform in depth using low energy implants that reduce lattice damage. Channeling is experienced when ions are implanted along the crystallographic axes of the semiconductor. If the implant direction is close to the major axes of the crystal lattice, the atoms in the crystal lattice appear to "line up" with respect to the implant direction, and the implanted ions appear to move down channels created by the crystal structure. This reduces the likelihood of collisions between the implanted ions and the atoms in the crystal lattice, especially near the surface of the semiconductor layer. The depth of implantation is significantly increased.
[0028] Generally, channeling occurs in silicon carbide when the implant direction is within about 2° of the crystallographic axes of the silicon carbide crystal. When the implant direction is greater than about 2° of the crystallographic axes of the silicon carbide crystal, the atoms in the lattice appear to be randomly distributed with respect to the implant direction, and the channeling effect is reduced. As used herein, the term "implant angle" refers to the angle between the implant direction and the c-axis or <0001> The c-axis of the silicon carbide layer is the angle between the crystal axis of the semiconductor layer into which the ions are implanted, such as the c-axis. Thus, implant angles of less than about 2° with respect to the c-axis of the silicon carbide layer are believed to lead to channeling, however, other implant angles may be used as well.
[0029] In one embodiment, p-type material layer 120 may be formed by ion implantation of 27Al in 4H—SiC implanted with channeling conditions of implant energy of E1=100 keV, dose of 1E13 cm2 at 25° C. In one embodiment, p-type material layer 120 may be formed by ion implantation of 27Al in 4H—SiC implanted with channeling conditions of implant energy of E2=300 keV, dose of 1E13 cm2 at 25° C. However, other implantation conditions and doses are contemplated as well. For example, in some embodiments, the implant energy is between 20 keV and 80 keV, 80 keV and 120 keV, 120 keV and 160 keV, 160 keV and 200 keV, 200 keV and 240 keV, 240 keV and 280 keV, 280 keV and 340 keV, 340 keV and 400 keV, 20 keV and 400 keV, and / or 80 keV. eV to 340 keV, and in some embodiments, the implantation dose may be 0.6E13 cm2 to 0.8E13 cm2, 0.8E13 cm2 to 1.2E13 cm2, 1.2E13 cm2 to 1.6E13 cm2, 1.6E13 cm2 to 2E13 cm2, 0.6E13 cm2 to 2E13 cm2, and / or 0.8E13 cm2 to 1.2E13 cm2. Furthermore, it should be noted that the p-type material layer 120 may be formed by implantation of boron (B), gallium (Ga), etc., followed by a high temperature anneal.
[0030] In one embodiment, the p-type material layer 120 may be deep-layered by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 1 μm or less by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.7 μm or less by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.5 μm or less by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.3 μm to 0.5 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.2 μm to 0.6 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.4 μm to 0.6 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.6 μm to 0.8 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.6 μm to 1.6 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 0.6 μm to 2.1 μm by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 1 μm to 5 μm by ion implantation. In one embodiment, the implantation and / or doping of the p-type material layer 120 may extend to a depth of up to 5 μm in the range of 5E15 to 5E17 per cm3. In one embodiment, the p-type material layer 120 may have a thickness of 10% to 20% of the thickness of the substrate 102 by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 20% to 30% of the thickness of the substrate 102 by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 30% to 40% of the thickness of the substrate 102 by ion implantation. In one embodiment, p-type material layer 120 may be implanted with ions to have a thickness that is between 40% and 50% of the thickness of substrate 102. In one embodiment, p-type material layer 120 may be implanted with ions to have a thickness that is between 50% and 60% of the thickness of substrate 102. In one embodiment, p-type material layer 120 may be implanted with ions to have a thickness that is between 60% and 70% of the thickness of substrate 102. In one embodiment, p-type material layer 120 may be implanted with ions to have a thickness that is between 70% and 80% of the thickness of substrate 102.In one embodiment, the p-type material layer 120 may have a thickness of 80% to 90% of the thickness of the substrate 102 by ion implantation.
[0031] The p-type material layer 120 is implanted into the substrate layer 102 followed by annealing. The annealing may activate the implant. In one embodiment, a masking layer material may be used during the implantation. In some embodiments, a capping layer material may be used to cover the wafer surface to prevent the substrate from separating at high temperatures during the annealing of the p-type material layer 120. Once the p-type material layer 120 is formed, the masking layer material may be removed. The annealing may be performed at a temperature range of 1500-1850° C. for 5 minutes-30 minutes. Other annealing temperatures and time profiles are contemplated as well.
[0032] In some embodiments, the substrate layer 102 may comprise a p-type material SiC substrate. In this embodiment, the formation of the p-type material layer 120 by implantation may not be necessary. Further, in this embodiment, the substrate layer 102 being a p-type material SiC substrate may be subsequently subjected to the methods described herein, including the implantation of the p+ layer 106.
[0033] FIG 3 illustrates a cross-sectional view of another embodiment of a transistor according to the present disclosure, and FIG 4 illustrates a cross-sectional view of another embodiment of a transistor according to the present disclosure. As shown in FIG 3 and FIG 4, an epitaxial layer 202 may be formed on a substrate layer 102. In the embodiment of FIG 3 and FIG 4, a p-type material layer 120 may be present in the epitaxial layer 202. In some embodiments, the p-type material layer 120 may be present in the epitaxial layer 202 in some embodiments where the substrate layer 102 comprises GaAs, GaN, etc. In one embodiment, the epitaxial layer 202 is formed of SiC.
[0034] In one embodiment, the epitaxial layer 202 may be disposed on the top surface of the substrate layer 102. In one embodiment, the epitaxial layer 202 may be disposed directly on the top surface of the substrate layer 102. The p-type material layer 120 may then be implanted into the epitaxial layer 202, followed by annealing as described herein. Further to this embodiment, the epitaxial layer 202 may be subjected to the methods described herein, including implantation of the p+ layer 106. In one embodiment, the p-type material layer 120 may have a thickness of 10% to 20% of the thickness of the epitaxial layer 202 by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 20% to 30% of the thickness of the epitaxial layer 202 by ion implantation. In one embodiment, the p-type material layer 120 may have a thickness of 30% to 40% of the thickness of the epitaxial layer 202 by ion implantation. In one embodiment, the p-type material layer 120 may be implanted with ions to have a thickness that is 40% to 50% of the thickness of the epitaxial layer 202. In one embodiment, the p-type material layer 120 may be implanted with ions to have a thickness that is 50% to 60% of the thickness of the epitaxial layer 202. In one embodiment, the p-type material layer 120 may be implanted with ions to have a thickness that is 60% to 70% of the thickness of the epitaxial layer 202. In one embodiment, the p-type material layer 120 may be implanted with ions to have a thickness that is 70% to 80% of the thickness of the epitaxial layer 202. In one embodiment, the p-type material layer 120 may be implanted with ions to have a thickness that is 80% to 90% of the thickness of the epitaxial layer 202.
[0035] In another embodiment, the epitaxial layer 202 may use a p-type material and the epitaxial layer 202 may be disposed on the top surface of the substrate layer 102. In another embodiment, the epitaxial layer 202 may use a p-type material and the epitaxial layer 202 may be disposed directly on the top surface of the substrate layer 102. In this regard, in some embodiments, the p-type material epitaxial layer 202 may be grown such that the epitaxial layer 202 has a p-type material layer 120 and may not require implantation as described herein to form the p-type material layer 120. The epitaxial layer 202 may then be subjected to methods including implantation of the p+ layer 106, which are described in more detail below. In some embodiments, the epitaxial layer 202 may be formed by epitaxial growth using an off-axis oriented wafer.
[0036] Figure 5 illustrates another embodiment of a transistor according to the present disclosure. In the embodiment of Figure 5, epitaxial layer 202 may be formed using p-type material, and epitaxial layer 202 may be disposed directly on top of substrate layer 102. In this embodiment, the entire epitaxial layer 202 may form p-type material layer 120. Epitaxial layer 202 may then be subjected to a method including implantation of p+ layer 106, which is described in more detail below.
[0037] In some embodiments, p-type material layer 120 may also be configured to have a doping and / or implantation profile that varies perpendicular to the surface. In some embodiments, p-type material layer 120 may also be configured to have a profile that varies perpendicular to the surface extending in the cross-sectional views of FIGS. 1-7.
[0038] In one embodiment, the p-type material layer 120 may be uniformly present beneath the application specific transistor 100 as shown in Figures 1 and 3. In one embodiment, the p-type material layer 120 may be uniformly present beneath the power switching application transistor 100 as shown in Figures 1 and 3.
[0039] In another embodiment for a particular application, such as an RF application, the p-type material layer 120 may be located in a limited area, such as a portion of the gate-source region of transistor 100, as shown in FIGS. 2 and 4 and described in further detail below.
[0040] In some embodiments, a portion of the voltage from the drain 112 to the source 110 may be dropped in the p-type material layer 120 region. This may deplete the lateral channel. The lateral depletion may reduce the lateral electric field and also increase the breakdown voltage. Alternatively, a more compact structure may be obtained for a required breakdown voltage. The p-type material layer 120 may eliminate the need for C or Fe doping of the buffer required to maintain the applied drain voltage. Eliminating the C and Fe deep levels results in less current reduction under (non-trapping) operating conditions. Additionally, in some embodiments, the p-type material layer 120 supports the electric field.
[0041] In some embodiments, the substrate layer 102 may comprise a p+ layer 106 as shown in Figures 1 and 2. In some embodiments, the epitaxial layer 202 may comprise a p+ layer 106 as shown in Figures 3 and 4. The p+ layer 106 may be used to reduce the charging time constant and to facilitate contact formation. In some embodiments, the p+ layer 106 may also be formed by ion implantation and annealing. The p+ layer 106 may be doped as highly as possible with the lowest sheet resistance achievable. In some embodiments, the p+ layer 106 may be present in the gate-source region. In some embodiments, the p+ layer 106 may also be present in the gate-source region and partially under the gate. In some embodiments, the p+ layer 106 may be present in a limited region as described in more detail below. In some embodiments, the p+ layer 106 may be less than 0.3 μm thick. In some embodiments, the p+ layer 106 may be less than 0.2 μm thick. In some embodiments, the p+ layer 106 may be between 0.1 μm and 0.3 μm thick. In some embodiments, the p+ layer 106 may be between 0.05 μm and 0.25 μm thick. In some embodiments, the p+ layer 106 may be between 0.15 μm and 0.25 μm thick.
[0042] A buffer layer 104, or a nucleation layer, may be formed on the substrate layer 102. In one embodiment, the buffer layer 104 is formed directly on the substrate layer 102. In one embodiment, the epitaxial layer 202 may be disposed on the top surface of the substrate layer 102 and the buffer layer 104 may be formed on the epitaxial layer 202. In one embodiment, the epitaxial layer 202 may be disposed on the top surface of the substrate layer 102 and the buffer layer 104 may be formed directly on the epitaxial layer 202. The buffer layer 104 may be GaN, aluminum gallium nitride (AlGaN), aluminum nitride (AlN), or other suitable material and may include a nucleation layer of AlN. In one embodiment, the buffer layer 104 is formed from AlGaN. The buffer layer 104 may be a p-type material or alternatively may be undoped. The AlN nucleation layer may be used to adhere the substrate layer 102 and to facilitate the growth of the buffer layer 104. The buffer layer 104 may be constrained to the substrate layer 102 .
[0043] In one embodiment, the buffer layer 104 may be high purity GaN. In one embodiment, the buffer layer 104 may be high purity GaN that may be lightly doped n-type. In one embodiment, the buffer layer 104 may use an AlGaN back barrier to provide good electron confinement.
[0044] 6 shows a cross-sectional view of another embodiment of a transistor according to the present disclosure. In particular, the embodiment of FIG. 6 shows that the buffer layer 104 may include an upper portion 602 of high purity GaN, and the buffer layer 104 may include a lower portion 604 that may form an AlGaN back barrier to achieve good electron confinement. In one embodiment, the lower portion 604 that forms the back barrier may be n-type AlGaN. The back barrier structure may be implemented in any embodiment of the present disclosure.
[0045] In one embodiment, the buffer layer 104 may be designed as a high purity type with the Fermi level in the upper half of the bandgap, minimizing the slow trapping effect typically observed in GaN HEMTs, where traps below the Fermi level are always filled, thus preventing slow transients. In some embodiments, the buffer layer 104 may be as thin as possible consistent with achieving good crystal quality; a candidate 0.4 μm layer has already demonstrated good quality.
[0046] In some embodiments, an AlZGa1-ZN (0<=Z<=1) nucleation or buffer layer 104 may be grown on the substrate layer 102 by epitaxial crystal growth techniques such as MOCVD (metal organic chemical vapor deposition), HVPE (hydride vapor phase epitaxy) or MBE (molecular beam epitaxy). The composition of the nucleation layer depends on the material of the substrate layer 102.
[0047] In another embodiment, the buffer layer 104 may be formed by a lateral epitaxial overgrowth (LEO) process. The LEO process can improve, for example, the crystal quality of the GaN layer. When the semiconductor layers of the HEMTs are epitaxial, the layer on which each epitaxial layer is grown can affect the device characteristics. For example, the LEO process can reduce the dislocation density in the epitaxial GaN layer.
[0048] A barrier layer 108 may be formed on the buffer layer 104. In one embodiment, the barrier layer 108 may be formed directly on the buffer layer 104. The barrier layer 108 may be further layers between the buffer layer 104 and the source 110, drain 112, and gate 114. The barrier layer 108 may be AlGaN, AlN, or other suitable material. In one embodiment, the barrier layer 108 is AlGaN. In one embodiment, the barrier layer 108 may be undoped. In one embodiment, the barrier layer 108 may be an n-type material. In some embodiments, the barrier layer 108 may have a stack of n-type materials with different carrier densities. In one embodiment, the barrier layer 108 may be a group III nitride or a combination thereof.
[0049] A protective layer 116 may be disposed on the barrier layer 108 adjacent to the gate 114 and the drain 112, opposite the buffer layer 104, to protect and isolate the gate 114 and the drain 112. The protective layer 116 may be an inert layer made of SiN, AlO, SiO, SiO2, AlN, or the like, or a combination thereof, including stacks thereof. In one embodiment, the protective layer 116 is an inert layer made of SiN. In one embodiment, the protective layer 116 may be deposited using MOCVD, plasma enhanced chemical vapor deposition (CVD), hot filament CVD, or sputtering. In one embodiment, the protective layer 116 may comprise a deposit of Si3N4. In one embodiment, the protective layer 116 forms an insulating layer. In one embodiment, the protective layer 116 forms an insulator.
[0050] The source 110 may have a p-type material contact 118 on the p+ layer 106. The p-type material contact 118 may be formed on the p+ layer 106 in a recess in the buffer layer 104 and the barrier layer 108. The p-type material contact 118 may be electrically coupled to the p+ layer 106. The recess may extend to the p+ layer 106 so that the p-type material contact 118 may be formed therein. The recess may be formed by etching or may use a material to define the recess. The material may be removed after the recess is formed.
[0051] In some embodiments, the implant of p-type material layer 120 may extend the entire length of transistor 100, as shown in Figures 1 and 3. In some embodiments, the implant of p-type material layer 120 may extend a portion of the length of transistor 100, as shown in Figures 2 and 4.
[0052] In some embodiments, the p-type material layer 120 may be neutralized to limit the length of the p-type material layer 120. In one embodiment, neutralizing may include implanting an impurity. In one embodiment, neutralizing the p-type material layer 120 may include absorbing the charge of the p-type material layer 120 with a material of opposite polarity. Another method for limiting the length of the p-type material layer 120 may be etching the p-type material layer 120. Another method for limiting the length of the p-type material layer 120 may be using a masking material to limit the implanted area.
[0053] In another embodiment, p-type material layer 120 may be formed by growing a layer of p-type material 120. For example, the growth may be epitaxial. To limit the length of p-type material layer 120, p-type material layer 120 may be etched or otherwise neutralized.
[0054] The p-type material layer 120 can help avoid problems with dielectric breakdown and material impurities. For example, without the p-type material layer 120, the transistor 100 may require well-discharged impurities. The p-type material layer 120 may be formed below the source 110 and may extend toward the gate 114 of the device.
[0055] In one embodiment, the layer of p-type material 120 may extend and remain the entire length, as shown in Figures 1 and 3. In one embodiment, the layer of p-type material 120 may extend and remain generally the entire length, as shown in Figures 1 and 3. In one embodiment, the layer of p-type material 120 may extend and remain substantially the entire length, as shown in Figures 1 and 3.
[0056] In another aspect of the disclosure, the p-type material layer 120 may not extend across the entire area of the transistor 100, as indicated by the arrow LENGTH P 120 as shown in Figures 2 and 4. In this regard, the p-type material layer 120 may be selectively disposed as described in more detail below, the p-type material layer 120 may be disposed across its entire length and selectively removed as described in more detail below, the p-type material layer 120 may be disposed across its entire length and selectively electrically neutralized, etc. As such, the specific structures of the p-type material layer 120 described below encompass any of these methods that result in the p-type material layer 120 having an operative structure and configuration as described below. In other words, the length and / or size of the p-type material layer 120 does not include portions that are partially electrically neutralized, partially etched, etc. The length and / or size of the p-type material layer 120 may depend on the application of the transistor 100, the requirements for the transistor 100, etc. By limiting the p-type material layer 120 so that it does not extend beyond the gate 114, adverse effects on RF performance for a particular transistor application may be avoided.
[0057] With reference to embodiments described in more detail below, the layer of p-type material 120 may extend horizontally, parallel to arrow LENGTH P 120. Additionally, the layer of p-type material 120 may extend horizontally, parallel to arrow LENGTH P 120, to a point determined by a line perpendicular to arrow LENGTH P 120 and extending through the elements of transistor 100, as indicated by line 150.
[0058] In one embodiment of the disclosure, the layer of p-type material 120 may extend laterally from at least below the source 110 towards a first end 124 of the gate 114. In one embodiment of the disclosure, the layer of p-type material 120 may extend laterally from at least below the source 110 to a location below the first end 124 of the gate 114.
[0059] In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about 0 μm to about 0.7 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about μm to about 0.5 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about 0 μm to about 0.3 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally from at least below the source 110 to a position below the second end 122 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about 0 μm to about 0.7 μm of the second end 122 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about 0 μm to about 0.5 μm of the second end 122 of the gate 114. In some embodiments of the present disclosure, the p-type material layer 120 may extend horizontally to a point in the range of about 0 μm to about 0.3 μm of the second end 122 of the gate 114.
[0060] In other aspects, the length LENGTH P 120 of the p-type material layer 120 can be viewed in relation to the location and / or size of other elements. The length SD can be the length between the inner edge 142 of the source 110 and the inner edge 144 of the drain 112, as shown in FIG.
[0061] In one embodiment, the length of the p-type material layer 120 may extend from 10% to 20% of the length of the SD, meaning that the p-type material layer 120 may extend from 10% to 20% past the inner end 142 of the source 110 towards the drain 112. In one embodiment, the length of the p-type material layer 120 may extend from 20% to 30% of the length of the SD, meaning that the p-type material layer 120 may extend from 20% to 30% of the length of the SD, meaning that the p-type material layer 120 may extend from 20% to 30% of the length of the SD, meaning that the p-type material layer 120 may extend from 30% to 40% of the length of the SD, meaning that the p-type material layer 120 may extend from 30% to 40% of the length of the SD, meaning that the p-type material layer 120 may extend from 30% to 40% of the length of the SD, meaning that the p-type material layer 120 may extend from 30% to 40% of the length of the SD. In one embodiment, the length of the p-type material layer 120 may extend from 40% to 50% of the length of the SD, meaning that the p-type material layer 120 may extend from 40% to 50% past the inner end 142 of the source 110 towards the drain 112. In one embodiment, the length of the p-type material layer 120 may extend from 50% to 60% of the length of the SD, meaning that the p-type material layer 120 may extend from 50% to 60% past the inner end 142 of the source 110 towards the drain 112.
[0062] In one embodiment of the present disclosure, the p+ layer 106 may not extend across the entire area of the substrate layer 102, as indicated by the arrow LENGTH P+ 106 shown in FIGS. 1-7. In this regard, the p+ layer 106 may be selectively disposed as described in more detail below, the p+ layer 106 may be disposed across its entire length and selectively removed as described in more detail below, the p+ layer 106 may be disposed across its entire length and selectively electrically neutralized, etc., as described in more detail below. Thus, the specific structures of the p+ layer 106 described below encompass any of these methods that result in the p+ layer 106 having an operating structure and configuration as described below. In other words, the length and / or size of the p+ layer 106 does not include portions that are partially electrically neutralized, partially etched, etc. It does not include portions that are partially electrically neutralized, partially etched, etc. The length and / or size of the p+ layer 106 may depend on the application of the transistor 100, the requirements for the transistor 100, etc.
[0063] With reference to embodiments described further below, the p+ layer 106 may extend horizontally, parallel to the arrow LENGTH P+ 106. Additionally, the p+ layer 106 may extend horizontally, parallel to the arrow LENGTH P+ 106, to a point determined by a line extending perpendicular to the arrow LENGTH P+ 106 and through the elements of the transistor 100 as indicated by line 150.
[0064] In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.7 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.5 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.3 μm of the first end 124 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend laterally from at least below the source 110 to a position below the second end 122 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.7 μm of the second end 122 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.5 μm of the second end 122 of the gate 114. In some embodiments of the present disclosure, the p+ layer 106 may extend to a point in the range of about 0 μm to about 0.3 μm of the second end 122 of the gate 114.
[0065] In other embodiments, the length LENGTH P+ 106 of the p+ layer 106 may be viewed in relation to the position and / or length of other elements based on the length SD, which may be the length from the inner end 142 of the source 110 toward the inner end 144 of the drain 112, as shown in FIG.
[0066] In one embodiment, the length of the p+ layer 106 may extend from 10% to 20% of the length of the SD, meaning that the p+ layer 106 may extend from 10% to 20% past the inner edge of the source 110 towards the drain 112. In one embodiment, the length of the p+ layer 106 may extend from 20% to 30% of the length of the SD, meaning that the p+ layer 106 may extend from 20% to 30% of the length of the SD, meaning that the p+ layer 106 may extend from 20% to 30% of the length of the SD, meaning that the p+ layer 106 may extend from 30% to 40% of the length of the SD, meaning that the p+ layer 106 may extend from 30% to 40% of the length of the SD, meaning that the p+ layer 106 may extend from 30% to 40% of the length of the SD. In one embodiment, the length of the p+ layer 106 may extend from 40% to 50% of the length of the SD, meaning that the p+ layer 106 may extend from 40% to 50% past the inner edge of the source 110 toward the drain 112. In one embodiment, the length of the p+ layer 106 may extend from 50% to 60% of the length of the SD, meaning that the p+ layer 106 may extend from 50% to 60% of the length of the SD, meaning that the p+ layer 106 may extend from 50% to 60% of the length of the SD, meaning that the p+ layer 106 may extend from 60% to 70% of the length of the SD, meaning that the p+ layer 106 may extend from 60% to 70% of the length of the SD, meaning that the p+ layer 106 may extend from 60% to 70% of the length of the SD. In one embodiment, the length of the p+ layer 106 may extend 70% to 80% of the length of the SD, meaning that the p+ layer 106 may extend 70% to 80% past the inner end of the source 110 toward the drain 112.
[0067] A gate contact may be provided to the gate 114 between the source 110 and the drain 112. Additionally, in some aspects of the present disclosure, the gate contact may be disposed on the barrier layer 108.
[0068] The gate 114 may be formed of platinum (Pt), nickel (Ni), and / or gold (Au), although other metals known to those skilled in the art capable of achieving the Schottky effect may be used. In one embodiment, the gate 114 may include a Schottky gate contact having a three-layer structure. Such a structure may be advantageous due to its high adhesion to some materials. In one embodiment, the gate 114 may further include an overlying layer of a highly conductive metal. The field plate 132 may be disposed on top of another protective layer and may be separate from the gate 114. The field plate 132 may be electrically connected to the source 110 and may be referred to as a source-connected field plate.
[0069] In another embodiment, a metal cladding layer may be provided over one or more of the source 110 and p-type material contact 118, the drain 112, and the gate 114. The cladding layer may be Au, silver (Ag), Al, Pt, and / or copper (Cu). Other suitable highly conductive metals may be used for the cladding layer. Additionally, the metal cladding layer may be electrically coupled to the p-type material contact 118.
[0070] FIG. 7 illustrates a cross-sectional view of another embodiment of a transistor according to the present disclosure. In the embodiment of FIG. 7, a p-type material layer 120 may be formed in or on the substrate layer 102, and the transistor 100 may include a second buffer layer 106. Although FIG. 7 illustrates the transistor 100 with a first buffer layer 104 and a second buffer layer 106, the transistor 100 may use only one buffer layer 104. In one embodiment, Al may be implanted into the substrate layer 102 and annealed to form the p-type material layer 120 in the substrate layer 102. In one embodiment, the substrate layer 102 may be doped with the p-type material layer 120. In one embodiment, the substrate layer 102 may be doped with boron to form the p-type material layer 120. Other materials, including Ga, are also contemplated. The length of the p-type material layer 120 near the surface of the p-type material layer 120 may be limited using techniques described in other embodiments above.
[0071] The second buffer layer 106 may be deposited or grown on the first buffer layer 104 on the side of the first buffer layer 104 opposite the substrate layer 102. In one embodiment, the second buffer layer 106 is formed directly on the first buffer layer 104. The second buffer layer 106 may be a high purity material such as gallium nitride (GaN), AlN, or the like. In one embodiment, the second buffer layer 106 may be high purity GaN. In one embodiment, the second buffer layer 106 may be high purity AlN. The second buffer layer 106 may be a p-type material or an n-type material. In another embodiment, the second buffer layer 106 may be undoped.
[0072] Figure 8 illustrates a method 500 for fabricating a transistor according to the present disclosure. In particular, Figure 8 illustrates an example method 500 for fabricating the transistor 100 of Figures 1-7. It should be noted that method 500 is merely exemplary and that modifications may be made thereto consistent with various aspects disclosed herein.
[0073] The method 500 may begin with step 502, which is the formation of a substrate layer 102. The substrate layer 102 may be formed from silicon carbide (SiC). In some embodiments, the substrate layer 102 may be a semi-insulating SiC substrate, a p-type substrate, an n-type substrate, or the like. In some embodiments, the substrate layer 102 may be very lightly doped. In one embodiment, the background impurity level may be low. In one embodiment, the background impurity level may be 1E15 / cm3 or lower. The substrate layer 102 may be formed from SiC selected from the group, such as 6H, 4H, 15R 3C SiC. In another embodiment, the substrate layer 102 may be GaAs, GaN, or other materials suitable for the applications described herein. In another embodiment, the substrate layer 102 may include sapphire, spinel, ZnO, silicon, or any other material capable of supporting the growth of group III nitride materials.
[0074] In some embodiments, the substrate layer 102 may be formed from a p-type material SiC substrate. In this embodiment, the formation of the p-type material layer 120 by implantation in step 504 may not be required. Further, in this embodiment, the substrate layer 102 being a p-type material SiC substrate may be subjected to a method including implanting the p+ layer 106 substantially as described herein.
[0075] In a first embodiment directed to the transistor 100 of FIG. 1 and FIG. 2, the method 500 may include a step 504 of implanting Al into the substrate layer 102 to form a p-type material layer 120 in the substrate layer 102 as shown in FIG. 1 and FIG. 2. The p-type material layer 120 may be formed by ion implantation of Al and annealing. In one embodiment, the p-type material layer 120 may be formed by implantation of Al and annealing prior to the growth of any GaN layer. In one embodiment, the implantation of ions may use a channeling implantation. In one embodiment, the channeling implantation may include aligning an ion beam to the substrate layer 102. The alignment of the ion beam may improve the efficiency of the implantation. The method 500 may further include implanting Al into the substrate layer 102 to form a p+ layer 106 in the substrate layer 102 as shown in FIG. 1 and FIG. 2. The substrate layer 102 may then be annealed as defined herein. In one embodiment, p-type material layer 120 may be formed by ion implantation of 27Al in 4H—SiC implanted with channeling conditions of implant energy of E1=100 keV and dose of 1E13 cm2 at 25° C. In one embodiment, p-type material layer 120 may be formed by ion implantation of 27Al in 4H—SiC implanted with channeling conditions of implant energy of E2=300 keV and dose of 1E13 cm2 at 25° C. However, other implant energies and doses are contemplated as well.
[0076] 1 and 2, a buffer layer 104 may be formed on the substrate layer 102 in step 506. The buffer layer 104 may be grown or deposited on the substrate layer 102. In one embodiment, the buffer layer 104 may be GaN. In another embodiment, the buffer layer 104 may be formed by a LEO process.
[0077] In a second embodiment directed to the transistor 100 of Figures 3 and 4, the method 500 may include a step 504 of forming an epitaxial layer 202 on the substrate layer 102. Thereafter, implanting Al into the epitaxial layer 202 to form a p-type material layer 120 in the epitaxial layer 202 as shown in Figures 3 and 4. The method 500 may further include implanting Al into the epitaxial layer 202 to form a p+ layer 106 in the epitaxial layer 202 as shown in Figures 3 and 4. The epitaxial layer 202 may then be annealed as defined herein.
[0078] 3 and 4, a buffer layer 104 may be formed on the epitaxial layer 202 in step 506. The buffer layer 104 may be grown or deposited on the epitaxial layer 202. In one embodiment, the buffer layer 104 may be GaN. In another embodiment, the buffer layer 104 may be formed by a LEO process.
[0079] In step 508, a barrier layer 108 may be formed on the buffer layer 104. The barrier layer 108 may be an n-type conductivity layer or may be undoped. In one embodiment, the barrier layer 108 may be AlGaN.
[0080] In step 510, a protective layer 116 may be formed. The protective layer 116 may be an inert layer such as SiN, AlO, SiO, SiO2, AlN, etc., or a combination including stacks thereof, which may be deposited over the exposed surface of the barrier layer 108. In another aspect of the disclosure, a recess may be formed by removing at least a portion of the barrier layer 108 and at least a portion of the buffer layer 104 to form a location for contacting the p+ layer 106. The recess may remove any material on the p+ layer 106 within a portion of the region associated with the source 110 by exposing the p+ layer 106 opposite the substrate layer 102.
[0081] Further during the method 500, a source 110 may be disposed on the barrier layer 108. The source 110 may be an ohmic contact of a suitable material that may be annealed. For example, the source 110 may be annealed at a temperature of about 500° C. to about 800° C. for about 2 minutes. However, other times and temperatures may also be used. For example, times of about 30 seconds to about 10 minutes are possible.
[0082] Further during method 500, drain 112 may be disposed on barrier layer 108. Like source 110, drain 112 may be an ohmic contact of Ni or other suitable material and may be annealed in a similar manner. In one embodiment, an n+ implant is used through barrier layer 108 and the contact is formed by implantation.
[0083] Further during the method 500, a gate 114 may be disposed on the barrier layer 108 between the source 110 and the drain 112. A layer of Ni, Pt, Au, etc. may be formed on the gate 114 by evaporation or other techniques. The gate structure may be completed by further deposition of Pt and Au, or other suitable materials.
[0084] Further during the method 500, the p-type material contact 118 may be formed. Once the p+ layer 106 is exposed, nickel or other suitable material may be evaporated to deposit on the p-type material contact 118. The nickel or other suitable material may be annealed, for example, to form an ohmic contact. Such deposition and annealing methods may be performed by using conventional techniques known to those skilled in the art. For example, the ohmic contact to the p-type material contact 118 may be annealed at a temperature of about 600° C. to about 1050° C. Once the p-type material contact 118 is formed on the p+ layer 106, a metallization layer may electrically couple the p-type material contact 118 of the p+ layer 106 to the source 110. In this way, the electrical conductivity of the p+ layer 106 and the source 110 may be maintained at the same potential.
[0085] The source 110 and drain 112 electrodes may be formed by ohmic contact such that current flows between the source 110 and drain 112 using a two-dimensional electron gas (2DEG) that is generated at the heterointerface between the buffer layer 104 and the barrier layer 108 when the gate 114 is biased at an appropriate level.
[0086] The gate 114 may extend over the top surface of the spacer or protective layer 116. The protective layer 116 may be etched and the gate 114 deposited such that the bottom surface of the gate 114 contacts the surface of the barrier layer 108. The metal forming the gate 114 may be patterned to extend across the protective layer 116 to form a top surface field plate structure 132 of the gate 114. In one embodiment, the field plate structure 132 extends toward the end of the gate 114 facing the drain 112. In one embodiment, the field plate structure 132 extends toward the source 110. In one embodiment, the field plate structure 132 extends toward the drain 112 and toward the source 110. In another embodiment, the field plate structure 132 does not extend toward the end of the gate 114. Finally, the structure may be covered with an insulating passivation layer 134, such as silicon nitride. The insulating passivation layer 134 may also be implanted in the same manner as the protective layer 116. Additionally, it should be noted that the cross-sectional shapes of gate 114 shown in Figures 1-6 are exemplary. For example, the cross-sectional shape of gate 114 in some embodiments may not include a T-shaped extension. Other configurations of gate 114 may be used, such as the configuration of gate 114 shown in Figure 7.
[0087] It should be noted that the steps of method 500 may be performed in a different order consistent with the aspects described above. Additionally, method 500 may be modified in a manner consistent with various aspects disclosed herein.
[0088] FIG. 9 shows the distribution of Al implanted under channeling conditions according to an embodiment of the present disclosure compared to a simulation under conventional implant conditions.
[0089] In particular, FIG. 9 shows the distribution (secondary ion mass spectrometry (SIMS) data) of 27Al in 4H-SiC implanted under channeling conditions along the C-axis compared to simulations under conventional implant conditions off-axis (TRIM). The implant energies used are E1=100 keV and E2=300 keV with a dose of 1E13 cm-2 at 25°C. In this regard, the p-type material layer 120 may be implanted consistent with this implant energy and dose. However, other implant energies and doses are also contemplated, not just those described herein.
[0090] In one embodiment, p-type material layer 120 may have a doping concentration that is less than p+ layer 106. In one embodiment, p+ layer 106 may be doped as highly as possible with the minimum sheet resistance achievable. In one embodiment, p-type material layer 120 may have a doping concentration that is less than p+ layer 106. In one embodiment, p+ layer 106 may be doped as highly as possible with the minimum sheet resistance achievable.
[0091] In one embodiment, the doping of p-type material layer 120 may be less than 1E17 cm3. In one embodiment, the doping of p-type material layer 120 may be less than 2E17 cm3. In one embodiment, the doping of p-type material layer 120 may be less than 6E17 cm3. In one embodiment, the doping of p-type material layer 120 may be less than 2E18 cm3. In one embodiment, the doping of p-type material layer 120 may be in the range of 5E15 to 5E17 per cm3. In these embodiments, the doping concentration of p+ layer 106 may be higher than the doping concentration of p-type material layer 120.
[0092] Thus, the present disclosure has revealed a simpler alternative for forming p-type layers in HEMTs. The disclosed structures can be easily manufactured with currently available technology. Furthermore, the use of the disclosed high purity materials minimizes the drain lag effect. Furthermore, the disclosed p-type material layers provide a field blocking for good electron confinement with low leakage. Additionally, aspects of this disclosure have detailed transistors having p-type layers and variations in the way those p-type layers are formed. The disclosed transistors maximize RF power, allow efficient discharge, and maximize dielectric breakdown.
[0093] While the present disclosure has been described in terms of exemplary embodiments, those skilled in the art will recognize that the disclosure can be practiced with modification within the spirit and scope of the appended claims. The examples given above are merely illustrative and are not intended to be an exhaustive list of all possible designs, embodiments, applications or modifications of the present disclosure.
Claims
1. 1. A high electron mobility transistor, comprising: a SiC substrate layer; a GaN buffer layer disposed on the SiC substrate layer; a p-type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is provided; Equipped with The p-type material layer is provided on one of the SiC substrate layer and a first layer disposed on the SiC substrate layer. Transistor.
2. a p+ type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is provided, the length of the p+ type material layer being shorter than a total length of the SiC substrate layer; The p-type material layer and the p+ type material layer are provided on one of the SiC substrate layer and the first layer disposed on the SiC substrate layer. The transistor of claim 1 .
3. 3. The transistor of claim 2, wherein the length of the p+ type material layer parallel to the surface of the SiC substrate layer extends from at least the source to at least an end of the gate adjacent the drain.
4. The transistor of claim 1 , wherein the length of the layer of p-type material is less than the overall length of the SiC substrate layer.
5. The transistor of claim 4 , wherein the p-type material layer has a length parallel to a surface of the SiC substrate layer extending at least from the source toward an end of the gate adjacent the drain.
6. 2. The transistor of claim 1, wherein the layer of p-type material is disposed on the SiC substrate layer, and the layer of p-type material comprises aluminum implanted in the SiC substrate layer.
7. 3. The transistor of claim 2, wherein the p+ type material layer is disposed on the SiC substrate layer, and the p+ type material layer comprises aluminum implanted in the SiC substrate layer.
8. 2. The transistor of claim 1 , wherein the layer of p-type material is provided in the first layer disposed on the SiC substrate layer, the first layer being SiC and comprising an epitaxial layer, the layer of p-type material comprising aluminum in the epitaxial layer.
9. 2. The transistor of claim 1, wherein the layer of p-type material is disposed on the SiC substrate layer, and wherein the layer of p-type material is configured to have a depth greater than 0.5 μm.
10. 2. The transistor of claim 1, wherein the layer of p-type material extends the entire length of one of the SiC substrate layer and the first layer disposed on the SiC substrate layer.
11. A method for manufacturing a high electron mobility transistor, comprising the steps of: providing a SiC substrate layer; providing a GaN buffer layer on the SiC substrate layer; providing a p-type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is provided; providing the p-type material layer on one of the SiC substrate layer and a first layer disposed on the SiC substrate layer; A method comprising:
12. providing a p+ type material layer having a length parallel to a surface of the SiC substrate layer on which the GaN buffer layer is provided, the length of the p+ type material layer being shorter than a total length of the SiC substrate layer; providing the p-type material layer and the p+ type material layer on one of the SiC substrate layer and the first layer disposed on the SiC substrate layer; Further comprising: providing the p-type material layer having a length parallel to a surface of the SiC substrate layer having the GaN buffer layer thereon further comprises implanting the p-type material utilizing a channeling condition. The method of claim 11.
13. 13. The method of claim 12, wherein the length of the p+ type material layer parallel to the surface of the SiC substrate layer extends from at least a source to at least an edge of a gate adjacent a drain.
14. The method of claim 11 , wherein the length of the layer of p-type material is less than the entire length of the SiC substrate layer.
15. The method of claim 14, wherein the length of the p-type material layer parallel to the surface of the SiC substrate layer extends at least from the source toward an end of the gate adjacent the drain.
16. 12. The method of claim 11, wherein the p-type material layer is disposed on the SiC substrate layer, the p-type material layer comprising aluminum implanted into the SiC substrate layer, and the p+ type material layer is disposed on the SiC substrate layer, the p+ type material layer comprising aluminum implanted into the SiC substrate layer.
17. The method of claim 12 , wherein the layer of p-type material is provided on the SiC substrate layer, the layer of p-type material being configured to have a depth of greater than 0.5 μm.
18. 1. A high electron mobility transistor, comprising: A substrate layer; a buffer layer disposed on the substrate layer; a p-type material having a length parallel to a surface of the substrate layer on which the buffer layer is disposed; a p+ type material having a length parallel to a surface of the substrate layer on which the buffer layer is disposed, the length of the p+ type material being less than an overall length of the substrate layer; Equipped with the p-type material layer and the p+ type material layer are provided on one of the substrate layer and a first layer disposed on the substrate layer; Transistor.
19. 20. The transistor of claim 18, wherein a length of the p+ type material parallel to the surface of the substrate layer extends from at least the source to at least an edge of the gate adjacent the drain, and the p- type material is configured to be deeper than a depth of the p+ type material.
20. 20. The transistor of claim 18, wherein the layer of p-type material is disposed on the substrate layer, the p-type material comprising aluminum implanted in the substrate layer, and the layer of p+ type material is disposed on the substrate layer, the p+ type material comprising aluminum implanted in the substrate layer.
Citation Information
Patent Citations
Field effect transistor
JP1998270462A
Iii-v nitride compound semiconductor device
JP2002076024A
A transistor with a p-type buried layer under the source region and its fabrication method.
JP2006507683A
Nitride-based transistor for millimetric wave operation
JP2007227885A
hfet
JP2011238701A