Painting structure

The coating structure addresses inefficiencies in masking by using varying surface irregularities to create distinct designs with a single paint layer, enhancing flexibility and reducing costs.

JP2024157449APending Publication Date: 2024-11-07KK TOKAI RIKA DENKI SEISAKUSHO
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023071830
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-25
Publication Date
2024-11-07

AI Technical Summary

Technical Problem

Existing coating structures require masking to change the design of painted and non-painted parts, which is inefficient and costly.

Method used

A coating structure with a base surface featuring varying depths and intervals of surface irregularities, allowing a single paint layer to create distinct designs without masking by adjusting the depth and presence of surface irregularities in different regions.

Benefits of technology

Enables design flexibility without masking, reducing costs and improving separation appearance, while maintaining design differences through a matte paint layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024157449000001_ABST
    Figure 2024157449000001_ABST
Patent Text Reader

Abstract

To change a design of a paint layer surface even without masking.SOLUTION: There is provided a paint structure 10 that is configured in that a base surface 16 of a base material 14 is provided with a grain 18, and a paint layer 20 covers the base surface 16. A depth of the grain 18 in a one-side region 12A is made larger than a depth of the grain 18 in a middle region 12B. On a surface of the paint layer 20, a depth of a one-side unevenness 22A in the one-side region 12A is made larger than a depth of a middle unevenness 22B in the middle region 12B. Therefore, a surface of the one-side region 12A and a surface of the middle region 12B of the paint layer 20 can have different designs.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coating structure in which a substrate is coated with a paint layer. [Background technology]

[0002] In the front bumper described in Patent Document 1 below, a non-painted portion and a painted portion are provided on the surface of a resin member.

[0003] Here, in this front bumper, the non-painted portions are masked with tape and the painted portions are painted. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 5-253533 Summary of the Invention [Problem to be solved by the invention]

[0005] In consideration of the above, an object of the present invention is to provide a coating structure that allows the design of the paint layer surface to be changed without the need for masking. [Means for solving the problem]

[0006] The paint structure of a first aspect of the present invention comprises a substrate having a base surface on which base surface irregularities are provided, and a first region on the base surface in which the depth of the base surface irregularities is increased and a second region in which the depth of the base surface irregularities is decreased, the first region being adjacent to the base surface, and a paint layer formed from a single paint, covering the base surface, and in which the depth of the first irregularities corresponding to the base surface irregularities is increased on a surface corresponding to the first region, and the depth of the second irregularities corresponding to the base surface irregularities is decreased on a surface corresponding to the second region.

[0007] The coating structure of the second aspect of the present invention is the coating structure of the first aspect of the present invention, in which a third region is provided on the base surface in which the depth of the base surface irregularities is smaller than that of the first region and larger than that of the second region, and the depth of the third irregularities corresponding to the base surface irregularities on the surface of the paint layer corresponding to the third region is intermediate between the first irregularities and the second irregularities.

[0008] A third aspect of the paint structure of the present invention comprises a substrate having a base surface on which base surface irregularities are provided, and a first region on the base surface in which the depth of the base surface irregularities is increased and a second region in which the depth of the base surface irregularities is decreased, the first region being adjacent to the depth of the base surface irregularities, and a paint layer formed from a single paint, covering the base surface, the surface corresponding to the first region being provided with surface irregularities corresponding to the base surface irregularities, and the surface corresponding to the second region not being provided with the surface irregularities corresponding to the base surface irregularities.

[0009] A fourth aspect of the paint structure of the present invention comprises a substrate having a base surface on which base surface irregularities are provided, and a first region on the base surface in which the spacing between the base surface irregularities is increased and a second region in which the spacing between the base surface irregularities is decreased, the first region being adjacent to the base surface, and a paint layer formed from a single paint, covering the base surface, and in which the depth of the first irregularities corresponding to the base surface irregularities is increased on the surface corresponding to the first region, and the depth of the second irregularities corresponding to the base surface irregularities is decreased on the surface corresponding to the second region.

[0010] The coating structure of the fifth aspect of the present invention is the coating structure of the fourth aspect of the present invention, in which a third region is provided on the base surface in which the spacing between the base surface irregularities is smaller than that in the first region and larger than that in the second region, and the depth of the third irregularities corresponding to the base surface irregularities on the surface of the paint layer corresponding to the third region is intermediate between the first irregularities and the second irregularities.

[0011] A sixth aspect of the paint structure of the present invention comprises a substrate having a base surface on which base surface irregularities are provided, and a first region on the base surface in which the spacing between the base surface irregularities is increased and a second region in which the spacing between the base surface irregularities is decreased, the first region being adjacent to the base surface, and a paint layer formed from a single paint, covering the base surface, the surface corresponding to the first region being provided with surface irregularities corresponding to the base surface irregularities, and the surface corresponding to the second region not being provided with the surface irregularities corresponding to the base surface irregularities.

[0012] A coating structure according to a seventh aspect of the present invention is the coating structure according to any one of the first to sixth aspects of the present invention, wherein the coating layer is formed by a matte paint. Effect of the Invention

[0013] In the coating structure of the first aspect of the present invention, base surface irregularities are provided on the base surface of the substrate, and the coating layer is formed of a single coating material to cover the base surface.

[0014] Here, the first and second regions of the base surface are adjacent to each other, the depth of the base surface unevenness is made large in the first region of the base surface and small in the second region of the base surface, and in the paint layer, the depth of the first unevenness corresponding to the base surface unevenness is made large in the surface corresponding to the first region and the depth of the second unevenness corresponding to the base surface unevenness is made small in the surface corresponding to the second region. Therefore, the design of the surface corresponding to the first region and the surface corresponding to the second region in the paint layer can be made different, and the design of the paint layer surface can be changed without masking.

[0015] In the coating structure of the second aspect of the present invention, the depth of the base surface unevenness in the third region of the base surface is made smaller than that in the first region and larger than that in the second region, and the depth of the third unevenness corresponding to the base surface unevenness in the surface corresponding to the third region of the paint layer is intermediate between the first unevenness and the second unevenness. This makes it possible to differentiate the designs of the surface corresponding to the first region, the surface corresponding to the second region, and the surface corresponding to the third region of the paint layer.

[0016] In the coating structure of the third aspect of the present invention, base surface irregularities are provided on the base surface of the substrate, and the coating layer is formed of a single coating material to cover the base surface.

[0017] Here, the first and second regions of the base surface are adjacent to each other, the depth of the base surface unevenness is made large in the first region of the base surface and small in the second region of the base surface, and in the paint layer, the surface corresponding to the first region has surface unevenness corresponding to the base surface unevenness, while the surface corresponding to the second region does not have surface unevenness corresponding to the base surface unevenness. Therefore, the design of the surface corresponding to the first region and the surface corresponding to the second region in the paint layer can be made different, and the design of the paint layer surface can be changed without masking.

[0018] In the coating structure of the fourth aspect of the present invention, base surface irregularities are provided on the base surface of the substrate, and the coating layer is formed of a single coating material to cover the base surface.

[0019] Here, the first and second regions of the base surface are adjacent to each other, the intervals between the base surface irregularities are increased in the first region of the base surface and decreased in the second region of the base surface, and in the paint layer, the depth of the first irregularities corresponding to the base surface irregularities is increased in the surface corresponding to the first region and the depth of the second irregularities corresponding to the base surface irregularities is decreased in the surface corresponding to the second region. This makes it possible to make the designs of the surface corresponding to the first region and the surface corresponding to the second region in the paint layer different, and the design of the paint layer surface can be changed without masking.

[0020] In the coating structure of the fifth aspect of the present invention, the interval between the base surface irregularities in the third region of the base surface is made smaller than in the first region and larger than in the second region, and the depth of the third irregularities corresponding to the base surface irregularities in the surface corresponding to the third region of the paint layer is intermediate between the first irregularities and the second irregularities. This makes it possible to differentiate the designs of the surface corresponding to the first region, the surface corresponding to the second region, and the surface corresponding to the third region of the paint layer.

[0021] In the coating structure of the sixth aspect of the present invention, base surface irregularities are provided on the base surface of the substrate, and the coating layer is formed by a single coating material to cover the base surface.

[0022] Here, the first and second regions of the base surface are adjacent to each other, the interval between the base surface irregularities is increased in the first region of the base surface while the interval between the base surface irregularities is decreased in the second region of the base surface, and in the paint layer, the surface corresponding to the first region has surface irregularities corresponding to the base surface irregularities while the surface corresponding to the second region does not have surface irregularities corresponding to the base surface irregularities. This makes it possible to make the designs of the surface corresponding to the first region and the surface corresponding to the second region of the paint layer different, and allows the design of the paint layer surface to be changed without masking.

[0023] In the coating structure of the seventh aspect of the present invention, the paint layer is formed with a matte paint, which allows for greater differences in the design of the paint layer surface due to differences in the depth of the surface irregularities of the paint layer. [Brief description of the drawings]

[0024] [Figure 1] 1A and 1B are diagrams showing a coating structure according to a first embodiment of the present invention, where 1A is a plan view and 1B is a cross-sectional view (cross-sectional view taken along line 1B-1B in 1A). [Diagram 2] 2A and 2B are diagrams showing a coating structure according to a second embodiment of the present invention, where 2A is a plan view and 2B is a cross-sectional view (cross-sectional view taken along line 2B-2B in 2A). [Diagram 3] 3 is a graph showing the relationship between the depth or spacing of the grains and the gloss of the paint layer surface in the coating structure according to the first or second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0025] [First embodiment] FIG. 1(A) shows a plan view of a coating structure 10 according to a first embodiment of the present invention, and FIG. 1(B) shows a cross-sectional view of the coating structure 10 (cross-sectional view taken along line 1B-1B in FIG. 1(A)).

[0026] The paint structure 10 according to this embodiment is applied to, for example, a decorative component of a vehicle.

[0027] As shown in Figures 1(A) and (B), the coating structure 10 has one side region 12A, a middle region 12B, an other side region 12C and an additional region 12D, where the one side region 12A and the middle region 12B are adjacent to each other, the middle region 12B and the other side region 12C are adjacent to each other, and the other side region 12C and the additional region 12D are adjacent to each other.

[0028] The coating structure 10 is provided with a substrate 14, which is made of, for example, resin. The surface of the substrate 14 is a base surface 16, and the base surface 16 is formed with grains 18 as base surface irregularities.

[0029] In the one side region 12A, the base surface 16 is made into a one side base surface region 16A as a first region, and in the one side base surface region 16A, the same grain 18 is uniformly formed, the depth of the grain 18 (the height direction dimension from the minimum height position of the recess to the maximum height position of the protrusion) is α1 (e.g., 50 μm), and the spacing of the grain 18 (the distance between the maximum height positions of the protrusions or the minimum height positions of the recesses) is β.

[0030] In the intermediate region 12B, the base surface 16 is made into an intermediate base surface region 16B as a first region, a second region or a third region, and in the intermediate base surface region 16B, the same grains 18 are uniformly formed, the depth of the grains 18 is set to α2 (e.g., 30 μm) which is smaller than α1, and the spacing between the grains 18 is set to β.

[0031] In the other side region 12C, the base surface 16 is made into an other side base surface region 16C as a second region, and in the other side base surface region 16C, the same grains 18 are uniformly formed, the depth of the grains 18 is α3 (e.g., 10 μm) which is smaller than α2, and the spacing between the grains 18 is β.

[0032] The base surface 16 is divided into additional base surface regions 16D in the additional region 12D, and the grain 18 is not formed in the additional base surface regions 16D.

[0033] As a result, the depth of the grain 18 is greater in the one-side base surface region 16A than in the intermediate base surface region 16B, and is greater in the intermediate base surface region 16B than in the other-side base surface region 16C. Furthermore, the spacing between the grains 18 is the same in the one-side base surface region 16A, the intermediate base surface region 16B, and the other-side base surface region 16C. Moreover, the maximum height positions of the grains 18 are the same or approximately the same in the one-side base surface region 16A, the intermediate base surface region 16B, and the other-side base surface region 16C.

[0034] The front side of the base surface 16 of the substrate 14 is painted with a single (same) paint, and the front side of the base surface 16 is covered with a paint layer 20. The paint of the paint layer 20 is, for example, an opaque matte paint, and surface irregularities 22 are formed on the surface of the paint layer 20.

[0035] On the surface of the paint layer 20, in the one side region 12A, the same one side irregularities 22A which are surface irregularities 22 (first irregularities, front irregularities) are uniformly formed, and the one side irregularities 22A are formed due to the grain 18 in the one side base surface region 16A on the base surface 16 of the substrate 14, and have a shape corresponding to the grain 18 (a shape roughly following the grain 18).

[0036] On the surface of the paint layer 20, identical intermediate irregularities 22B which are surface irregularities 22 (first irregularity, second irregularity, third irregularity, front irregularity) are uniformly formed in the intermediate region 12B, and the intermediate irregularities 22B are formed due to the grain 18 of the intermediate base surface region 16B on the base surface 16 of the substrate 14, and have a shape corresponding to the grain 18 (a shape roughly following the grain 18).

[0037] In the other side region 12C on the surface of the paint layer 20, a substantially identical other side irregularity 22C which is a surface irregularity 22 is uniformly formed, and the other side irregularity 22C is not caused by the grain 18 of the other side base surface region 16C on the base surface 16 of the substrate 14, but is formed by paint particles and has a shape which does not correspond to the grain 18 (a shape which does not follow the grain 18).

[0038] On the surface of the paint layer 20, in the additional region 12D, a substantially identical additional irregularity 22D which is a surface irregularity 22 is uniformly formed, and the additional irregularity 22D is formed by paint particles and has the same shape as the other side irregularity 22C because the grain 18 is not formed in the additional base surface region 16D on the base surface 16 of the substrate 14.

[0039] The one-side irregularities 22A and the intermediate irregularities 22B are provided with irregularities formed by paint particles, similar to the other-side irregularities 22C and the additional irregularities 22D.

[0040] As a result, the depth of one-side unevenness 22A is greater than that of intermediate unevenness 22B, which in turn is greater than those of other-side unevenness 22C and additional unevenness 22D, and as the depth of surface unevenness 22 is increased, the visibility of surface unevenness 22 is increased and the gloss of the surface of paint layer 20 is decreased. Also, the maximum height positions of one-side unevenness 22A, intermediate unevenness 22B, other-side unevenness 22C and additional unevenness 22D are set to be the same or approximately the same.

[0041] 3, when the depth of the grain 18 on the base surface 16 of the substrate 14 is less than a predetermined value (in the case of the other side region 12C and the additional region 12D), the surface unevenness 22 caused by the grain 18 is not formed on the surface of the paint layer 20, and the gloss of the surface of the paint layer 20 is increased. On the other hand, when the depth of the grain 18 is equal to or greater than a predetermined value (in the case of the one side region 12A and the middle region 12B), the surface unevenness 22 caused by the grain 18 is formed on the surface of the paint layer 20, and as the depth of the grain 18 is increased, the depth of the surface unevenness 22 is increased, and the gloss of the surface of the paint layer 20 is reduced. Also, as the particle size of the paint in the paint layer 20 becomes smaller, the predetermined value is decreased, and the surface unevenness 22 caused by the grain 18 is more likely to be formed on the surface of the paint layer 20. Furthermore, as the particle size of the paint in the paint layer 20 increases, the gaps between the paint particles become larger, making it easier for the grain 18 to fill in the gaps, and making it more difficult for surface irregularities 22 caused by the grain 18 to form on the surface of the paint layer 20.

[0042] Next, the operation of this embodiment will be described.

[0043] In the coating structure 10 configured as described above, the base surface 16 of the substrate 14 is provided with a grain 18, and the coating layer 20 is formed of a single coating material and covers the base surface 16.

[0044] Here, the depth of the grain 18 in the one side region 12A (one side base surface region 16A) is made larger than the depth of the grain 18 in the middle region 12B (middle base surface region 16B), and on the surface of the paint layer 20, the depth of the one side irregularity 22A corresponding to the grain 18 in the one side region 12A is made larger than the depth of the middle irregularity 22B corresponding to the grain 18 in the middle region 12B. Therefore, the visibility of the one side irregularity 22A in the one side region 12A is made larger than the visibility of the middle irregularity 22B in the middle region 12B, so that the design of the surface of the one side region 12A and the surface of the middle region 12B in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0045] Furthermore, the one-side base surface region 16A and the middle base surface region 16B in the base surface 16 of the substrate 14 are adjacent to each other, and the one-side irregularities 22A and the middle irregularities 22B in the surface of the paint layer 20 are adjacent to each other. This makes it possible to provide a parting (boundary) between the surface of the one-side region 12A and the surface of the middle region 12B in the paint layer 20. Moreover, since a parting without using masking can be provided, it is possible to eliminate the need to provide a recess along the outer periphery of the masking in the base surface 16, and the parting can be made sharp and the appearance of the parting can be improved.

[0046] Further, the depth of the grain 18 in the middle region 12B (middle base surface region 16B) is made larger than the depth of the grain 18 in the other side region 12C (other side base surface region 16C), and on the surface of the paint layer 20, the depth of the middle asperities 22B corresponding to the grain 18 in the middle region 12B is made larger than the depth of the other side asperities 22C not corresponding to the grain 18 in the other side region 12C. Therefore, by making the visibility of the middle asperities 22B in the middle region 12B larger than the visibility of the other side asperities 22C in the other side region 12C, the design of the surface of the middle region 12B and the surface of the other side region 12C in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0047] Furthermore, the middle base surface region 16B and the other side base surface region 16C in the base surface 16 of the substrate 14 are adjacent to each other, and the middle irregularities 22B and the other side irregularities 22C in the surface of the paint layer 20 are adjacent to each other. This makes it possible to provide a parting (boundary) between the surface of the middle region 12B and the surface of the other side region 12C in the paint layer 20. Moreover, since a parting without using masking can be provided, it is not necessary to provide a recess along the outer periphery of the masking in the base surface 16, and the parting can be made sharp and the appearance of the parting can be improved.

[0048] Further, the depth of the grain 18 in the one side region 12A (one side base surface region 16A) is made larger than the depth of the grain 18 in the other side region 12C (other side base surface region 16C), and on the surface of the paint layer 20, the depth of the one side irregularities 22A corresponding to the grain 18 in the one side region 12A is made larger than the depth of the other side irregularities 22C not corresponding to the grain 18 in the other side region 12C. Therefore, the visibility of the one side irregularities 22A in the one side region 12A is made larger than the visibility of the other side irregularities 22C in the other side region 12C, so that the design of the surface of the one side region 12A and the surface of the other side region 12C in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0049] Furthermore, the paint layer 20 is formed of a matte paint. Therefore, the difference in the design of the surface of the paint layer 20 can be greatly increased by the difference in the depth of the surface irregularities 22 of the paint layer 20. Moreover, even if the paint layer 20 peels off due to wear or the like, the grain 18 of the base surface 16 of the substrate 14 can prevent the surface of the coating structure 10 from becoming glossy.

[0050] [Second embodiment] FIG. 2(A) shows a plan view of a coating structure 50 according to a second embodiment of the present invention, and FIG. 2(B) shows a cross-sectional view of the coating structure 50 (cross-sectional view taken along line 2B-2B in FIG. 2(A)).

[0051] The coating structure 50 according to this embodiment has a configuration substantially similar to that of the first embodiment, but differs in the following respects.

[0052] As shown in (A) and (B) of Figures 2, in the coating structure 50 of this embodiment, in one side base surface region 16A of the base surface 16 of the substrate 14, the depth of the grain 18 is α (e.g., 30 μm) and the spacing between the grains 18 is β.

[0053] In the intermediate base surface region 16B of the base surface 16 of the substrate 14, the depth of the grain 18 is set to α, and the interval between the grains 18 is set to β / 2.

[0054] In the other side region 12C of the base surface 16 of the substrate 14, the depth of the grain 18 is set to α, and the interval between the grains 18 is set to β / 4.

[0055] As a result, the depth of the grain 18 is the same in the one-side base surface region 16A, the intermediate base surface region 16B, and the other-side base surface region 16C. Furthermore, the spacing between the grains 18 is greater in the one-side base surface region 16A than in the intermediate base surface region 16B, and is greater in the intermediate base surface region 16B than in the other-side base surface region 16C. Furthermore, the maximum height position and the minimum height position of the grain 18 are the same or approximately the same in the one-side base surface region 16A, the intermediate base surface region 16B, and the other-side base surface region 16C.

[0056] On the surface of the paint layer 20, in the one side region 12A, the same one side irregularity 22A which is the surface irregularity 22 is uniformly formed, and the one side irregularity 22A is formed due to the grain 18 in the one side base surface region 16A of the base surface 16 of the substrate 14, and has a shape corresponding to the grain 18 (a shape roughly following the grain 18).

[0057] On the surface of the paint layer 20, in the intermediate region 12B, the same intermediate irregularities 22B, which are surface irregularities 22, are uniformly formed, and the intermediate irregularities 22B are formed due to the grain 18 of the intermediate base surface region 16B on the base surface 16 of the substrate 14, and have a shape corresponding to the grain 18 (a shape that roughly follows the grain 18).

[0058] In the other side region 12C on the surface of the paint layer 20, a substantially identical other side irregularity 22C which is a surface irregularity 22 is uniformly formed, and the other side irregularity 22C is not caused by the grain 18 of the other side base surface region 16C on the base surface 16 of the substrate 14, but is formed by paint particles and has a shape which does not correspond to the grain 18 (a shape which does not follow the grain 18).

[0059] The depth of the one-side unevenness 22A is greater than the depth of the intermediate unevenness 22B, and the depth of the intermediate unevenness 22B is greater than the depths of the other-side unevenness 22C and the additional unevenness 22D. In addition, the maximum height positions of the one-side unevenness 22A, the intermediate unevenness 22B, the other-side unevenness 22C, and the additional unevenness 22D are the same or approximately the same.

[0060] 3, when the interval between the grains 18 on the base surface 16 of the substrate 14 is less than a predetermined value (in the case of the other side region 12C and the additional region 12D), the surface unevenness 22 caused by the grains 18 is not formed on the surface of the paint layer 20, and the gloss of the surface of the paint layer 20 is increased. On the other hand, when the interval between the grains 18 is equal to or more than a predetermined value (in the case of the one side region 12A and the middle region 12B), the surface unevenness 22 caused by the grains 18 is formed on the surface of the paint layer 20, and as the interval between the grains 18 is increased, the depth of the surface unevenness 22 is increased, and the gloss of the surface of the paint layer 20 is reduced. Also, as the particle size of the paint in the paint layer 20 becomes smaller, the predetermined value is decreased, and the surface unevenness 22 caused by the grains 18 is more likely to be formed on the surface of the paint layer 20.

[0061] Next, the operation of this embodiment will be described.

[0062] In the coating structure 50 configured as above, the base surface 16 of the substrate 14 is provided with the grain 18, and the coating layer 20 is formed from a single (same) coating material and covers the base surface 16.

[0063] Here, the intervals of the embossments 18 in the one side region 12A (one side base surface region 16A) are made larger than the intervals of the embossments 18 in the middle region 12B (middle base surface region 16B), and on the surface of the paint layer 20, the depth of the one side unevenness 22A corresponding to the embossments 18 in the one side region 12A is made larger than the depth of the middle unevenness 22B corresponding to the embossments 18 in the middle region 12B. Therefore, the visibility of the one side unevenness 22A in the one side region 12A is made larger than the visibility of the middle unevenness 22B in the middle region 12B, so that the design of the surface of the one side region 12A and the surface of the middle region 12B in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0064] Furthermore, the one-side base surface region 16A and the middle base surface region 16B in the base surface 16 of the substrate 14 are adjacent to each other, and the one-side irregularities 22A and the middle irregularities 22B in the surface of the paint layer 20 are adjacent to each other. This makes it possible to provide a parting (boundary) between the surface of the one-side region 12A and the surface of the middle region 12B in the paint layer 20. Moreover, since a parting without using masking can be provided, it is possible to eliminate the need to provide a recess along the outer periphery of the masking in the base surface 16, and the parting can be made sharp and the appearance of the parting can be improved.

[0065] In addition, the intervals between the embossments 18 in the middle region 12B (middle base surface region 16B) are greater than the intervals between the embossments 18 in the other side region 12C (other side base surface region 16C), and on the surface of the paint layer 20, the depth of the middle asperities 22B corresponding to the embossments 18 in the middle region 12B is greater than the depth of the other side asperities 22C not corresponding to the embossments 18 in the other side region 12C. Therefore, the visibility of the middle asperities 22B in the middle region 12B is greater than the visibility of the other side asperities 22C in the other side region 12C, so that the design of the surface of the middle region 12B and the surface of the other side region 12C in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0066] Furthermore, the middle base surface region 16B and the other side base surface region 16C in the base surface 16 of the substrate 14 are adjacent to each other, and the middle irregularities 22B and the other side irregularities 22C in the surface of the paint layer 20 are adjacent to each other. This makes it possible to provide a parting (boundary) between the surface of the middle region 12B and the surface of the other side region 12C in the paint layer 20. Moreover, since a parting without using masking can be provided, it is not necessary to provide a recess along the outer periphery of the masking in the base surface 16, and the parting can be made sharp and the appearance of the parting can be improved.

[0067] In addition, the intervals between the embossments 18 in the one-side region 12A (one-side base surface region 16A) are made larger than the intervals between the embossments 18 in the other-side region 12C (other-side base surface region 16C), and on the surface of the paint layer 20, the depth of the one-side irregularities 22A corresponding to the embossments 18 in the one-side region 12A is made larger than the depth of the other-side irregularities 22C not corresponding to the embossments 18 in the other-side region 12C. Therefore, the visibility of the one-side irregularities 22A in the one-side region 12A is made larger than the visibility of the other-side irregularities 22C in the other-side region 12C, so that the design of the surface of the one-side region 12A and the surface of the other-side region 12C in the paint layer 20 can be made different, and the design of the surface of the paint layer 20 can be changed without masking, and the design of the surface of the paint layer 20 can be changed without using multiple types of paint, thereby reducing costs.

[0068] Furthermore, the paint layer 20 is formed of a matte paint. Therefore, the difference in the design of the surface of the paint layer 20 can be increased by the difference in the depth of the surface irregularities 22 of the paint layer 20. Moreover, even if the paint layer 20 peels off due to wear or the like, the grain 18 of the base surface 16 of the substrate 14 can prevent the surface of the coating structure 50 from becoming glossy.

[0069] In the first and second embodiments, the other-side irregularities 22C may be formed on the surface of the paint layer 20 in the other-side region 12C due to the grains 18 in the other-side base surface region 16C in the base surface 16 of the substrate 14, and may be formed into a shape corresponding to the grains 18 (a shape substantially following the grains 18). Therefore, on the surface of the paint layer 20, not only is the depth of the intermediate irregularities 22B corresponding to the grains 18 in the intermediate region 12B greater than the depth of the other-side irregularities 22C corresponding to the grains 18 in the other-side region 12C, but the depth of the other-side irregularities 22C corresponding to the grains 18 in the other-side region 12C is greater than the depth of the additional irregularities 22D not corresponding to the grains 18 in the additional region 12D. This not only makes it possible to differentiate the design of the surface of the intermediate region 12B in the paint layer 20 from the surface of the other side region 12C, but also makes it possible to differentiate the design of the surface of the other side region 12C in the paint layer 20 from the surface of the additional region 12D.

[0070] Furthermore, in the first embodiment, the depth of the grain 18 is different between the one side base surface region 16A, the intermediate base surface region 16B, and the other side base surface region 16C on the base surface 16 of the substrate 14. Furthermore, in the second embodiment, the intervals of the grain 18 are different between the one side base surface region 16A, the intermediate base surface region 16B, and the other side base surface region 16C on the base surface 16 of the substrate 14. However, the depth and intervals of the grain 18 may be different between the one side base surface region 16A, the intermediate base surface region 16B, and the other side base surface region 16C on the base surface 16 of the substrate 14.

[0071] In the first and second embodiments, the grain 18 may not be provided in a portion of the region from the one-side base surface region 16A through the intermediate base surface region 16B to the other-side base surface region 16C in the base surface 16 of the substrate 14. This allows the surface of the paint layer 20 to have a portion where the surface irregularities 22 caused by the grain 18 are not formed, thereby increasing the variety of designs on the surface of the paint layer 20.

[0072] Furthermore, in the above first and second embodiments, the one side region 12A and the middle region 12B are adjacent to each other, the middle region 12B and the other side region 12C are adjacent to each other, and the other side region 12C and the additional region 12D are adjacent to each other. However, the one side region 12A and the other side region 12C may be adjacent to each other, the one side region 12A and the additional region 12D may be adjacent to each other, or the middle region 12B and the additional region 12D may be adjacent to each other.

[0073] In the first and second embodiments, at least one of the tops of the protrusions and the bottoms of the recesses in the grain 18 on the base surface 16 of the substrate 14 may be made flat.

[0074] Furthermore, in the first and second embodiments, the paint of the paint layer 20 is made opaque. However, the paint of the paint layer 20 may be made transparent.

[0075] Furthermore, in the matte paint of the paint layer 20, if the particle size is smaller than a certain value smaller than that of the first or second embodiment described above, the smaller the depth or spacing of the grain 18, the more the particles will penetrate into the recesses of the grain 18, causing the surface of the paint layer 20 to diffusely reflect light and reduce the glossiness, while the larger the depth or spacing of the grain 18, the more the paint will conform to the grain 18, making the surface of the paint layer 20 less susceptible to the effect of diffuse reflection of light and increasing the glossiness. [Explanation of symbols]

[0076] 10... Paint structure, 14... Base material, 16... Base surface, 16A... One side base area (first area), 16B... Intermediate base area (first area, second area, third area), 16C... Other side base area (first area). 2 areas), 18... Grain (base surface unevenness), 20... Paint layer, 22A... One side unevenness (first unevenness, surface unevenness), 22B... Intermediate unevenness (first unevenness, second unevenness, third unevenness, surface unevenness), 50... Paint structure

Claims

1. A base material having a base surface on which base surface irregularities are provided, and a first region in which the depth of the base surface irregularities is increased and a second region in which the depth of the base surface irregularities is decreased are provided adjacent to each other on the base surface; a paint layer formed of a single paint, covering the base surface, in which a depth of a first unevenness corresponding to the base surface unevenness is increased on a surface corresponding to the first region, and a depth of a second unevenness corresponding to the base surface unevenness is decreased on a surface corresponding to the second region; A coating structure comprising:

2. A coating structure as described in claim 1, wherein a third region is provided on the base surface in which the depth of the base surface asperity is smaller than that of the first region and larger than that of the second region, and the depth of the third asperity corresponding to the base surface asperity on the surface of the paint layer corresponding to the third region is intermediate between the first asperity and the second asperity.

3. A base material having a base surface on which base surface irregularities are provided, and a first region in which the depth of the base surface irregularities is increased and a second region in which the depth of the base surface irregularities is decreased are provided adjacent to each other on the base surface; a paint layer formed of a single paint, covering the base surface, the paint layer having a surface irregularity corresponding to the base surface irregularity on a surface corresponding to the first region, and the paint layer having no surface irregularity corresponding to the base surface irregularity on a surface corresponding to the second region; A coating structure comprising:

4. A base material having a base surface on which base surface irregularities are provided, and a first region in which the intervals between the base surface irregularities are increased and a second region in which the intervals between the base surface irregularities are decreased are provided adjacent to each other on the base surface; a paint layer formed of a single paint, covering the base surface, in which a depth of a first unevenness corresponding to the base surface unevenness is increased on a surface corresponding to the first region, and a depth of a second unevenness corresponding to the base surface unevenness is decreased on a surface corresponding to the second region; A coating structure comprising:

5. A coating structure as described in claim 4, wherein a third region is provided on the base surface in which the spacing between the base surface irregularities is smaller than that in the first region and larger than that in the second region, and the depth of the third irregularities corresponding to the base surface irregularities on the surface of the paint layer corresponding to the third region is intermediate between the first irregularities and the second irregularities.

6. A base material having a base surface on which base surface irregularities are provided, and a first region in which the intervals between the base surface irregularities are increased and a second region in which the intervals between the base surface irregularities are decreased are provided adjacent to each other on the base surface; a paint layer formed of a single paint, covering the base surface, the paint layer having a surface irregularity corresponding to the base surface irregularity on a surface corresponding to the first region, and the paint layer having no surface irregularity corresponding to the base surface irregularity on a surface corresponding to the second region; A coating structure comprising:

7. The coating structure according to any one of claims 1, 3, 4 and 6, wherein the coating layer is formed by a matte coating.

Citation Information

Patent Citations

  • Metallic mold and resin molded article

    JP2009006654A

  • Method for forming patterned surface

    JP2010149110A

  • Construction material, decorative member, and method for manufacturing decorative member

    WO2021153767A1

  • Boundary line structure for coating bamper

    JP1993253533A