Manufacturing method of high pressure tank

By varying the winding angle switching points for each layer in the manufacturing process, the method addresses the issue of low strength at fiber tow transitions, resulting in improved structural integrity of high-pressure tanks.

JP2024158075AActive Publication Date: 2024-11-08TOYOTA JIDOSHA KK
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023072936
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-11-08
Estimated Expiration
2043-04-27

AI Technical Summary

Technical Problem

The existing methods for manufacturing high-pressure tanks with multilayer structures face issues of low strength at switching points where the winding angle of fiber tows changes, leading to potential slippage and reduced strength due to uneven distribution of fiber tow thickness.

Method used

A manufacturing method that varies the winding angle switching points for each layer of low helical fiber reinforced plastic layers, dispersing these points to prevent localized thinning and enhance structural integrity.

Benefits of technology

This method effectively suppresses the formation of low-strength regions by ensuring consistent fiber tow distribution across layers, enhancing the overall strength and structural integrity of the high-pressure tank.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158075000001_ABST
    Figure 2024158075000001_ABST
Patent Text Reader

Abstract

To make it possible to suppress an occurrence of a low strength part when laminating low helical layers having different winding angles for each layer.SOLUTION: A fiber reinforced plastic layer is formed by winding fiber tows 30 impregnated with a binder resin around a liner 20. The fiber reinforced plastic layer includes a low helical layer. In this manufacturing method, when forming a plurality of low helical layers, a winding angle θ of the fiber tows 30 is made different for each layer. Furthermore, in this manufacturing method, a switching point position of the winding angle on the liner 20, which is a winding end point {L(s),Pe(k-1)} of a given low helical layer and a winding start point {L(s+1),Ps(1)} of a next low helical layer, is made different for each low helical layer.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Disclosed herein is a method for manufacturing a high pressure tank. [Background technology]

[0002] The high-pressure tank has a multi-layer structure. For example, as disclosed in Patent Documents 1 to 3, the high-pressure tank includes a liner and a fiber-reinforced plastic layer.

[0003] The liner is the innermost part of the high-pressure tank. The liner has a cylindrical part as the central part and a pair of dome parts connected to both ends of the cylindrical part in the central axial direction. A fluid such as hydrogen gas is sealed inside the liner.

[0004] A fiber-reinforced plastic layer is laminated on the liner. The fiber-reinforced plastic layer is formed by winding fiber tows, which are fiber bundles, around the liner.

[0005] The fiber tow is wound around the liner by a so-called low-angle helical winding. In the low-angle helical winding, the winding angle of the fiber tow is set to an angle close to parallel to the central axis of the liner. The layer of fiber-reinforced plastic wound by the low-angle helical winding is also called a low-helical layer. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2020-122543 A [Patent Document 2] JP 2019-195955 A [Patent Document 3] JP 2012-149739 A Summary of the Invention [Problem to be solved by the invention]

[0007] Incidentally, there are cases where the low helical layer is formed over a plurality of layers. In such cases, the low helical layer of the multi-layer structure is set so that the winding angle of the fiber tow differs in each layer.

[0008] 5, in a given layer of the low helical layers, the fiber tow 102 is wound around the liner 100 at a winding angle θ101. In a layer above that, the fiber tow 102 is wound around the liner 100 at a winding angle θ102 (≠θ101). In a layer above that, the fiber tow 102 is wound around the liner 100 at a winding angle θ103 (≠θ102).

[0009] When the winding angle is changed from θ101 to θ102, the fiber tow 102 slides upward at the switching point P100 in the upper part of Fig. 5. In other words, the fiber tow 102 near the switching point P100 deviates from the intended winding position. Similarly, as shown in the middle and lower parts of Fig. 5, slippage (displacement) of the fiber tow 102 occurs at the switching point P100 in other layers as well. If slippage of the fiber tow 102 occurs at the switching point P100 across other layers, the strength of the switching point P10 may be lower than other portions.

[0010] Therefore, this specification discloses a method for manufacturing a high-pressure tank that can suppress the occurrence of low strength portions when stacking low helical layers with different winding angles for each layer. [Means for solving the problem]

[0011] This specification discloses a method for manufacturing a high-pressure tank. The manufacturing method includes a step of forming a liner and a lamination step. The liner includes a cylindrical portion and a pair of dome portions provided at both ends of the cylindrical portion in the central axis direction. In the lamination step, a fiber reinforced plastic layer is formed on the liner. In the lamination step, a fiber tow impregnated with a binder resin is wound around the liner to form a fiber reinforced plastic layer. The fiber reinforced plastic layer includes a low helical layer. The low helical layer is formed by winding the fiber tow around the liner multiple times using low-angle helical winding in which the winding angle with respect to the central axis of the liner is an acute angle. In the fiber reinforced plastic layer, the low helical layer is formed over multiple layers. In this manufacturing method, when forming the low helical layer over multiple layers, the winding angle of the fiber tow is made different for each layer. Furthermore, in this manufacturing method, the switching point position of the winding angle on the liner, which is the winding end point of the low helical layer of a predetermined layer and the winding start point of the low helical layer of the next layer, is made different for each layer of the low helical layer.

[0012] According to the above-mentioned configuration, the switching point positions of the winding angle of the fiber tow are different for each low helical layer. By dispersing the switching point positions on the liner, it is possible to suppress the occurrence of low-strength regions in which the fiber tows are excessively thin compared to the surrounding areas. Effect of the Invention

[0013] According to the method for manufacturing a high-pressure tank disclosed in this specification, it is possible to suppress the occurrence of low-strength portions when stacking low helical layers having different winding angles for each layer. [Brief description of the drawings]

[0014] [Figure 1] 1 is a front view illustrating a configuration of a high-pressure tank manufactured by a manufacturing method according to an embodiment of the present invention. FIG. [Diagram 2] FIG. 2 is a diagram illustrating a filament winding process in the manufacturing process of a high-pressure tank. [Diagram 3] FIG. 11 is a perspective view for explaining the definition of a circuit in low-angle helical winding. [Figure 4] 1A to 1C are diagrams illustrating a process of stacking a plurality of low helical layers according to a manufacturing method according to the present embodiment. [Diagram 5] 1A to 1C are diagrams illustrating a process of stacking a plurality of low helical layers according to a manufacturing method of the prior art. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] A method for manufacturing a high-pressure tank according to an embodiment will be described below with reference to the drawings. The shapes, materials, quantities, and values ​​described below are examples for the purpose of explanation and can be changed as appropriate according to the specifications of the high-pressure tank. In addition, the same reference numerals are used for equivalent elements in all drawings below.

[0016] 1 illustrates a high-pressure tank 10 that is a target of the manufacturing method according to this embodiment. For example, the high-pressure tank 10 is a hydrogen tank filled with hydrogen gas. For example, the high-pressure tank 10 is mounted on a fuel cell vehicle (FCEV, Fuel Cell Electric Vehicle).

[0017] The manufacturing method for the high-pressure tank 10 according to this embodiment includes a liner forming process, a filament winding process, and an inspection process. In the liner forming process, the liner 20 is formed from a plurality of parts. In the filament winding process, fiber reinforced plastic is laminated on the liner 20. The filament winding process is also called a lamination process. Furthermore, in the inspection process, the high-pressure tank 10 is subjected to a water pressure inspection and an airtight inspection.

[0018] The high pressure tank 10 has a layered structure, for example, the high pressure tank 10 has a liner 20 and a fiber reinforced plastic layer.

[0019] The liner 20 is a hollow body in which hydrogen gas is sealed. The liner 20 includes a cylindrical portion 22 and dome portions 24, 26. The pair of dome portions 24, 26 are disposed on both ends of the cylindrical portion 22 in the direction of the central axis C1. For example, in a liner forming process, the dome portions 24, 26 and the cylindrical portion 22 are welded together.

[0020] The liner 20 is required to have gas barrier properties. For this reason, the liner 20 is made of a resin material such as a nylon resin. Furthermore, caps 25 and 27 are attached to both ends of the dome portions 24 and 26 along the central axis C1.

[0021] The fiber reinforced plastic layer is laminated on the liner 20. The fiber reinforced plastic layer is formed by winding a so-called towpreg (also called a tow prepreg), which is a fiber tow, which is a bundle of fibers, impregnated with a binder resin.

[0022] The fibers of the towpreg are made of fiber-reinforced plastic (FRP). For example, carbon fiber reinforced plastic (CFRP) and glass fiber reinforced plastic (GFRP) are used as the fibers of the towpreg.

[0023] The fiber reinforced plastic layer has a laminate structure including a plurality of low helical layers formed by winding the fiber tows 30 on the liner 20 with a low angle helical winding.

[0024] The low-angle helical winding refers to a winding mode in which the winding angle θ is an acute angle with respect to the central axis C1 of the liner 20. For example, in the low-angle helical winding, the winding angle θ is set to be 10° or more and 80° or less.

[0025] 2 illustrates a filament winding process. In this process, a fiber tow 30 is wound around a liner 20. The liner 20 is coupled to a motor 50 via a nozzle 25. The motor 50 rotates the liner 20 around a central axis C1.

[0026] Further, a guide 52 is disposed radially away from the central axis C1 of the liner 20. The guide 52 has a function of a creel (warping tool) for the fiber tow 30. That is, the fiber tow 30 impregnated with the binder resin is supplied from the guide 52 and wound around the liner 20.

[0027] For example, the guide 52 is movable in an X-axis direction parallel to the central axis C1, a Y-axis direction parallel to the radial direction of the liner 20, and a Z-axis direction which is the height direction. For example, the guide 52 is equipped with an XYZ stage mechanism. Furthermore, the guide 52 is capable of twisting the fiber tows 30 to be supplied. For example, a servo motor is provided in a feeder (not shown) of the guide 52, capable of rotating the feeder around the feed axis of the fiber tows 30.

[0028] Here, the low-angle helical winding is controlled using a total of five parameters: the twist angle φ when the fiber tow 30 is fed, the movement axes X, Y, and Z of the guide 52, and the rotation angle α of the liner 20. For example, a winding control unit (not shown) of the filament winding device controls the rotation speed of the liner 20 and the movement speed of the guide 52 in the X-axis direction to wind the fiber tow 30 around the liner 20 while keeping the winding angle θ constant.

[0029] In the low-angle helical winding, the fiber tow 30 is wound around the liner 20 a plurality of times to form one low-angle helical layer. The "number of circuit turns" is used as a parameter indicating the number of turns in the low-angle helical winding.

[0030] Referring to FIG. 3, in the low-angle helical winding, for example, when an arbitrary point on the cylindrical portion 22 is set as the winding starting point, a winding route is adopted in which the fiber tow 30 is wound around one of the die 27, and then the fiber tow 30 is wound around the other die 25 by moving again on the cylindrical portion 22.

[0031] Taking into consideration the periodicity of the winding, the number of circuit turns is determined as follows: In Fig. 3, the winding start point Ps(k) of the kth turn of the circuit of the sth low helical layer L(s), i.e., the winding start point {L(s),Ps(k)}, is positioned on the liner 20.

[0032] The fiber tow 30 is wound around the cylindrical portion 22 from the winding starting point {L(s), Ps(k)}. The fiber tow 30 is further wound so as to surround the die 27. The fiber tow 30 is wound again around the cylindrical portion 22, with the die 27 as a turning back point. The fiber tow 30 is further wound so as to surround the other die 25. The fiber tow 30 is then wound around the cylindrical portion 22.

[0033] In this winding process, the guide 52 (see FIG. 2) moves in the direction of the central axis C1 and turns back when its axial position coincides with the nozzle 27. The guide 52 further moves in the direction of the central axis C1 and turns back again when its axial position coincides with the nozzle 25. The axial position of the guide 52 further coincides with the winding start point {L(s),Ps(k)}. The position of the fiber tow 30 at this time becomes the winding end point {L(s),Pe(k)} of the kth circuit.

[0034] In Fig. 3, a control line CL indicating the positions of the winding start point and the winding end point is shown by a dashed line. The control line CL is illustrated on the liner 20 along the circumference of the cylindrical portion 22, passing through the winding start point {L(s),Ps(k)}. The intersection of the fiber tow 30 returning from the die 25 to the cylindrical portion 22 and the control line CL is the winding end point {L(s),Pe(k)} of the kth circuit. This winding end point {L(s),Pe(k)} of the kth circuit is also the winding start point {L(s),Ps(k+1)} of the next k+1th circuit.

[0035] In the high-pressure tank 10 according to this embodiment, a plurality of low helical layers are formed as the fiber reinforced plastic layers. Furthermore, the plurality of low helical layers are set so that the winding angle θ of the fiber tow 30 differs for each layer.

[0036] As described above, if the switching point position of the winding angle θ is fixed for every layer, the switching point position may become a low-strength portion where the layer of the fiber tow 30 is thinner than the surrounding area. Therefore, in the manufacturing method of the high-pressure tank according to this embodiment, winding is performed such that the switching point position of the winding angle θ on the liner 20 is different for each layer.

[0037] <Low helical layer formation process> 4 illustrates a filament winding process among the manufacturing processes for the high-pressure tank 10 according to this embodiment. This process is also called a lamination process because it is a process for forming a fiber-reinforced plastic layer on the liner 20.

[0038] For example, a computer (not shown) of the filament winding machine includes a winding setting unit. The winding setting unit sets the winding path of the fiber tow 30 in each layer of the low helical layer. When setting the winding path, the so-called liner phase is intentionally shifted, as described below.

[0039] 4 illustrates a process for forming a low helical layer of the first layer L(1) on the liner 20. First, a winding start point {L(1), Ps(1)} (not shown) of the first layer and the first turn of the circuit is set at an arbitrary position on the cylindrical portion 22.

[0040] The winding setting unit sets the number of circuit turns in each layer of the low helical layers across multiple layers. The winding setting unit calculates the pitch between the circuits based on the number of circuit turns and the winding angle θ1 in the first layer.

[0041] The pitch between the circuits refers to the distance on the control line CL between the winding start points Ps(k) for each circuit turn. That is, for each circuit turn, the fiber tows 30 are wound around the liner 20 along the central axis C1 with a one pitch offset.

[0042] In determining the pitch between the circuits, the winding setting unit determines a tentative winding end point of the circuit. For example, if the number of circuit revolutions set is n, the tentative winding end point {L(1), Pe(n)} is the same as the winding start point {L(1), Ps(1)} on the control line CL.

[0043] Next, the winding setting unit sets the winding end point {L(1), Pe(n-1)} one turn before the tentative winding end point {L(1), Pe(n)} as the true winding end point. That is, in the first low helical layer, the winding end point of the fiber tow 30 is set to a position shifted by one pitch from the winding start point {L(1), Ps(1)} of the first turn of the circuit.

[0044] The winding end point {L(1), Pe(n-1)} of the final turn of the circuit of the first low helical layer is the winding start point {L(2), Ps(1)} of the first turn of the circuit of the second low helical layer. As illustrated in the upper and middle parts of Figure 4, the winding angle θ2 of the second low helical layer is different from the winding angle θ1 of the first low helical layer.

[0045] In forming the second low helical layer, the winding setting unit sets the winding end point {L(2), Pe(n-1)} one turn before the tentative winding end point {L(2), Pe(n)} as the true winding end point, in the same manner as in the first layer. That is, in the second low helical layer, the winding end point of the fiber tow 30 is set at a position shifted by one pitch in the direction from the winding start point {L(2), Ps(1)} of the second turn of the circuit.

[0046] The winding end point {L(2), Pe(n-1)} of the final turn of the circuit of the second low helical layer is the winding start point {L(3), Ps(1)} of the first turn of the circuit of the third low helical layer. As illustrated in the middle and lower parts of Figure 4, the winding angle θ3 of the third low helical layer is different from the winding angle θ2 of the second low helical layer.

[0047] In forming the third low helical layer, similarly to the first and second layers, the winding setting unit sets the winding end point {L(3),Pe(n-1)} one turn before the tentative winding end point {L(3),Pe(n)} as the true winding end point. That is, in the third low helical layer, the winding end point of the fiber tow 30 is set at a position shifted by one pitch from the winding start point {L(3),Ps(1)} of the third turn of the circuit.

[0048] In this manner, in a low helical layer of a predetermined layer (e.g., the kth layer), the winding of the fiber tow 30 is performed such that the winding start point {L(k),Ps(1)} of the first turn of the circuit and the winding end point (L(k),Pe(n-1)) of the final turn of the circuit are positioned differently on the liner 20. This allows the switching point position of the winding angle θ to be different across each layer. By varying the switching point position of the winding angle θ on the liner 20, the occurrence of low strength portions where the fiber tow 30 is locally thin is suppressed. [Explanation of symbols]

[0049] 10 high pressure tank, 20 liner, 22 cylindrical section, 24, 26 dome section, 30 fiber tow.

Claims

[Claim 1] forming a liner including a cylindrical portion and a pair of dome portions provided at both ends of the cylindrical portion in a central axis direction; forming a fiber-reinforced plastic layer on the liner; Including, In the lamination step, the fiber tows impregnated with a binder resin are wound around the liner to form the fiber reinforced plastic layer; The fiber reinforced plastic layer includes a low helical layer formed by winding the fiber tow around the liner a plurality of times in a low angle helical winding manner in which the winding angle with respect to the central axis of the liner is an acute angle, The low helical layer is formed over a plurality of layers in the fiber reinforced plastic layer, When forming the low helical layer over a plurality of layers, the winding angle of the fiber tow is made different for each layer, a switching point position of the winding angle on the liner, which is a winding end point of the low helical layer of a given layer and a winding start point of the low helical layer of the next layer, is made different for each of the low helical layers; A method for manufacturing high-pressure tanks.

Citation Information

Patent Citations

  • High pressure tank, high pressure tank mounting device, and pressure tank manufacturing method

    JP2019219025A

  • High-pressure tank and its manufacturing method

    JP2020122543A

  • Tank and method for manufacturing the same

    WO2010116527A1

  • Method for manufacturing high-pressure tank, and high-pressure tank

    JP2012149739A

  • Filament winding apparatus, method for designing filament winding, and method for manufacturing tank