Semiconductor element and manufacturing method for the same
The semiconductor device improves reliability and electrical performance by using silicide layers with sloped extensions to increase contact area and reduce resistance in shrinking semiconductor devices.
Patent Information
- Application Number
- JP2024008205
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-27
- Filing Date
- 2024-01-23
- Publication Date
- 2024-11-08
AI Technical Summary
As semiconductor devices shrink in size, their operating characteristics deteriorate, leading to reliability and electrical performance issues.
A semiconductor device design featuring a substrate with active regions, source/drain patterns, and active contacts that include silicide layers, with specific sloped extensions covering the source/drain patterns to increase contact area and reduce resistance.
The design enhances reliability and electrical characteristics by increasing the contact area between active contacts and source/drain patterns, thereby reducing contact resistance.
Smart Images

Figure 2024159473000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and a method for manufacturing the same, and more particularly to a semiconductor device including a field effect transistor and a method for manufacturing the same. [Background technology]
[0002] Semiconductor devices include integrated circuits composed of MOS field effect transistors (MOS (Metal Oxide Semiconductor) FETs). As the size and design rules of semiconductor devices are gradually reduced, the scale down of MOS field effect transistors is also accelerating. As the size of MOS field effect transistors is reduced, the operating characteristics of semiconductor devices may be degraded. Therefore, various methods are being researched to form semiconductor devices with better performance while overcoming the limitations caused by the high integration of semiconductor devices. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] US Patent No. 11,362,194 B2 Summary of the Invention [Problem to be solved by the invention]
[0004] SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide a semiconductor device having improved reliability and electrical characteristics.
[0005] Another object of the present invention is to provide a method for manufacturing a semiconductor device having improved reliability and electrical characteristics. [Means for solving the problem]
[0006] A semiconductor device according to the concept of the present invention includes a substrate including an active region, an active pattern on the active region, a source / drain pattern on the active pattern, an active contact extending from an upper surface of the source / drain pattern to a sidewall, the active contact including a first portion covering the sidewall of the source / drain pattern and a second portion covering the upper surface of the source / drain pattern, a first layer provided between the source / drain pattern and the first portion, and a second layer separated from the first layer via the first portion, each of the first layer and the second layer including a silicide layer.
[0007] According to another aspect of the present invention, a semiconductor device includes a substrate including an active region, an active pattern on the active region, a source / drain pattern on the active pattern, and an active contact electrically connected to the source / drain pattern, wherein a sidewall of the source / drain pattern includes a first surface and a second surface, the first surface and the second surface meet each other to define an apex of the source / drain pattern, the active contact includes a first extension covering the first surface and a second extension covering the second surface, the first extension having a first slope and extending along the first surface, and the second extension having a second slope and extending along the second surface, wherein one of the first slope and the second slope may be a positive slope and the other may be a negative slope.
[0008] According to another aspect of the present invention, a method for manufacturing a semiconductor device may include forming an active pattern on a substrate, forming a source / drain pattern on the active pattern, forming a first silicon layer extending from an upper surface to a sidewall of the source / drain pattern, a sacrificial layer on the first silicon layer, a second silicon layer on the sacrificial layer, forming a stop layer on the second silicon layer, forming a first interlayer insulating layer on the active pattern and a second interlayer insulating layer on the first interlayer insulating layer, etching the first and second interlayer insulating layers to form recess holes, etching and removing a portion of the stop layer and a portion of the second silicon layer exposed by the recess holes, removing the sacrificial layer exposed by the recess holes, doping the first and second silicon layers exposed by the recess holes with impurities, depositing a metal material on the first and second silicon layers exposed by the recess holes to form a silicide layer, and forming an active contact inside the recess hole. Effect of the Invention
[0009] In the semiconductor device according to the present invention, the active contact may cover the top surface and both side walls of the source / drain pattern. In this case, a first layer may be formed between the source / drain pattern and the active contact, and a second layer may be formed separated from the source / drain pattern via the active contact. Each of the first layer and the second layer may include a silicide layer and a silicon layer. As a result, the contact area between the active contact and the source / drain pattern may be increased, thereby reducing the contact resistance between the active contact and the source / drain pattern. In addition, the contact resistance may be reduced by doping impurities into the contact surface between the first layer and the active contact. As a result, the semiconductor device to which the present invention is applied may have improved reliability and electrical characteristics. [Brief description of the drawings]
[0010] [Figure 1]1 is a conceptual diagram illustrating a logic cell of a semiconductor device according to an embodiment of the present invention; [Diagram 2] 1 is a conceptual diagram illustrating a logic cell of a semiconductor device according to an embodiment of the present invention; [Diagram 3] 1 is a conceptual diagram illustrating a logic cell of a semiconductor device according to an embodiment of the present invention; [Figure 4] 1 is a plan view illustrating a semiconductor device according to an embodiment of the present invention; [Figure 5A] 5 is a cross-sectional view taken along line AA' in FIG. 4. [Figure 5B] FIG. 5 is a cross-sectional view taken along line BB' in FIG. [Figure 5C] 5 is a cross-sectional view taken along line CC' in FIG. 4. [Figure 5D] FIG. 5 is a cross-sectional view taken along line DD' in FIG. [Figure 6] FIG. 5B is an enlarged view of an embodiment of region M of FIG. 5A. [Figure 7] FIG. 5C is an enlarged view of an embodiment of region N of FIG. 5B. [Figure 8] FIG. 5D is an enlarged view of an embodiment of region A of FIG. 5C. [Figure 9A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 9B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 10A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 10B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 11A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 11B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 11C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 12A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 12B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 12C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 12D] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 12E] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 13A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 13B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 13C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 13D] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 14A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 14B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 14C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 14D] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 15A] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 15B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 15C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 16A]1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 16B] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 16C] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 16D] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 17] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 18] 1A to 1C are cross-sectional views illustrating a method of manufacturing a semiconductor device according to an embodiment of the present invention. [Figure 19] FIG. 5D is an enlarged view of area A of FIG. 5C according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] 1 to 3 are conceptual diagrams illustrating a logic cell of a semiconductor device according to an embodiment of the present invention.
[0012] 1, a single height cell (SHC) may be provided. Specifically, a first power wiring M1_R1 and a second power wiring M1_R2 may be provided on a substrate 100. The first power wiring M1_R1 may be a path through which a source voltage VSS, for example, a ground voltage, is provided. The second power wiring M1_R2 may be a path through which a drain voltage VDD, for example, a power voltage, is provided.
[0013] A single height cell SHC may be defined between the first power wiring M1_R1 and the second power wiring M1_R2. The single height cell SHC may include one first active area AR1 and one second active area AR2. One of the first and second active areas AR1, AR2 may be a PMOSFET area, and the other of the first and second active areas AR1, AR2 may be an NMOSFET area. In other words, the single height cell SHC may have a CMOS structure provided between the first power wiring M1_R1 and the second power wiring M1_R2.
[0014] Each of the PMOSFET region PR and the NMOSFET region NR may have a first width W1 in the first direction D1. The length of the single height cell SHC in the first direction D1 may be defined as a first height HE1. The first height HE1 may be substantially equal to the distance (e.g., pitch) between the first power wiring M1_R1 and the second power wiring M1_R2.
[0015] The single height cell SHC may constitute one logic cell. In this specification, a logic cell may refer to a logic element (e.g., AND, OR, XOR, XNOR, inverter, etc.) that performs a specific function. That is, a logic cell may include transistors for forming a logic element and wiring that connects the transistors to each other.
[0016] 2, a double height cell (DHC) may be provided. Specifically, a first power wiring M1_R1, a second power wiring M1_R2, and a third power wiring M1_R3 may be provided on a substrate 100. The first power wiring M1_R1 may be disposed between the second power wiring M1_R2 and the third power wiring M1_R3. The third power wiring M1_R3 may be a path through which a source voltage VSS is provided.
[0017] A double-height cell DHC may be defined between the second power wiring M1_R2 and the third power wiring M1_R3. The double-height cell DHC may include a first PMOSFET region PR1, a second PMOSFET region PR2, a first NMOSFET region NR1, and a second NMOSFET region NR2.
[0018] The first NMOSFET region NR1 may be adjacent to the second power wiring M1_R2. The second NMOSFET region NR2 may be adjacent to the third power wiring M1_R3. The first and second PMOSFET regions PR1, PR2 may be adjacent to the first power wiring M1_R1. In a plan view, the first power wiring M1_R1 may be disposed between the first and second PMOSFET regions PR1, PR2.
[0019] The length of the double height cell DHC in the first direction D1 may be defined as a second height HE2. The second height HE2 may be approximately twice the first height HE1 of FIG. 1. The first and second PMOSFET regions PR1 and PR2 of the double height cell DHC may be connected to operate as one PMOSFET region. Therefore, the channel size of the PMOS transistor of the double height cell DHC may be larger than the channel size of the PMOS transistor of the single height cell SHC of FIG. 1.
[0020] In the present invention, the double height cell DHC shown in Figure 2 can be defined as a multi-height cell. Although not shown, the multi-height cell can include a triple height cell whose cell height is about three times that of the single height cell SHC.
[0021] 3, a first single height cell SHC1, a second single height cell SHC2, and a double height cell DHC may be two-dimensionally arranged on a substrate 100. The first single height cell SHC1 may be arranged between first and second power wirings M1_R1, M1_R2. The second single height cell SHC2 may be arranged between first and third power wirings M1_R1, M1_R3. The second single height cell SHC2 may be adjacent to the first single height cell SHC1 in a first direction D1.
[0022] The double height cell DHC may be disposed between the second and third power wirings M1_R2 and M1_R3. The double height cell DHC may be adjacent to the first and second single height cells SHC1 and SHC2 in the second direction D2.
[0023] An isolation structure DB may be provided between the first single height cell SHC1 and the double height cell DHC, and between the second single height cell SHC2 and the double height cell DHC, such that the active area of the double height cell DHC may be electrically isolated from the active areas of the first and second single height cells SHC1 and SHC2.
[0024] Fig. 4 is a plan view illustrating a semiconductor device according to an embodiment of the present invention. Figs. 5A to 5D are cross-sectional views taken along lines A-A', B-B', C-C', and D-D' in Fig. 4, respectively. The semiconductor device illustrated in Figs. 4 and 5A to 5D is a more detailed example of the single height cell SHC of Fig. 1.
[0025] 4 and 5A to 5D, a single height cell SHC may be provided on a substrate 100. A logic transistor constituting a logic circuit may be disposed on the single height cell SHC. The substrate 100 may be a semiconductor substrate including silicon, germanium, silicon-germanium, etc., or a compound semiconductor substrate. As an example, the substrate 100 may be a silicon substrate.
[0026] The substrate 100 may include a first PMOSFET region PR and a first NMOSFET region NR. Each of the first PMOSFET region PR and the first NMOSFET region NR may extend in a second direction D2.
[0027] A first active pattern AP1 and a second active pattern AP2 may be defined by a trench TR formed in the upper portion of the substrate 100. The first active pattern AP1 may be provided on a PMOSFET region PR, and the second active pattern AP2 may be provided on an NMOSFET region. The first and second active patterns AP1 and AP2 may extend in a second direction D2. The first and second active patterns AP1 and AP2 may be vertically protruding portions of the substrate 100.
[0028] An isolation layer ST may be provided on the substrate 100. The isolation layer ST may fill the trench TR. The isolation layer ST may include a silicon oxide layer. The isolation layer ST may not cover first and second channel patterns CH1 and CH2, which will be described later.
[0029] A liner film FL may be interposed between the first and second active patterns AP1, AP2 and the isolation film ST. The liner film FL may directly cover each sidewall of the first and second active patterns AP1, AP2. In other words, the liner film FL may directly cover the sidewall of the trench TR. The liner film FL may directly cover the bottom surface of the trench TR. For example, the liner film FL may include a silicon oxide film, a silicon nitride film, or a combination thereof.
[0030] A first channel pattern CH1 may be provided on the first active pattern AP1. A second channel pattern CH2 may be provided on the second active pattern AP2. Each of the first channel pattern CH1 and the second channel pattern CH2 may include a first semiconductor pattern SP1, a second semiconductor pattern SP2, and a third semiconductor pattern SP3, which are sequentially stacked. The first to third semiconductor patterns SP1, SP2, and SP3 may be spaced apart from each other in a vertical direction (i.e., a third direction D3). The first semiconductor pattern SP1 may be formed at a lowermost portion of the semiconductor pattern, and the third semiconductor pattern SP3 may be formed at an uppermost portion of the semiconductor pattern.
[0031] Each of the first to third semiconductor patterns SP1, SP2, and SP3 may include silicon (Si), germanium (Ge), or silicon-germanium (SiGe). For example, each of the first to third semiconductor patterns SP1, SP2, and SP3 may include crystalline silicon, more specifically, single crystal silicon. In one embodiment of the present invention, the first to third semiconductor patterns SP1, SP2, and SP3 may be stacked nanosheets.
[0032] A plurality of first source / drain patterns SD1 may be provided on the first active pattern AP1. A plurality of first recesses RS1 may be formed on the first active pattern AP1. A first source / drain pattern SD1 may be provided in each of the first recesses RS1. The first source / drain pattern SD1 may be an impurity region of a first conductivity type (e.g., p-type). A first channel pattern CH1 may be interposed between the pair of first source / drain patterns SD1. In other words, the stacked first to third semiconductor patterns SP1, SP2, and SP3 may connect the pair of first source / drain patterns SD1 to each other.
[0033] A plurality of second source / drain patterns SD2 may be provided on the second active pattern AP2. A plurality of second recesses RS2 may be formed on the second active pattern AP2. The second source / drain patterns SD2 may be provided in the second recesses RS2, respectively. The second source / drain patterns SD2 may be impurity regions of a second conductivity type (e.g., n-type). A second channel pattern CH2 may be interposed between the pair of second source / drain patterns SD2. In other words, the stacked first to third semiconductor patterns SP1, SP2, and SP3 may connect the pair of second source / drain patterns SD2 to each other.
[0034] The first and second source / drain patterns SD1 and SD2 may be epitaxial patterns formed by a selective epitaxial growth (SEG) process. As an example, a top surface of each of the first and second source / drain patterns SD1 and SD2 may be higher than a top surface of the third semiconductor pattern SP3. As another example, a top surface of at least one of the first and second source / drain patterns SD1 and SD2 may be located at substantially the same level as a top surface of the third semiconductor pattern SP3.
[0035] In one embodiment of the present invention, the first source / drain pattern SD1 may include a semiconductor element having a lattice constant larger than that of the semiconductor element of the substrate 100. For example, the first source / drain pattern SD1 may include at least one of silicon (Si) and silicon-germanium (SiGe). Thus, the pair of first source / drain patterns SD1 may provide a compressive stress to the first channel pattern CH1 therebetween. The second source / drain pattern SD2 may include the same semiconductor element as the substrate 100. For example, the second source / drain pattern SD2 may include at least one of silicon-arsenide (SiAs) and silicon-phosphorus (SiP).
[0036] In one embodiment of the present invention, the sidewall of the first source / drain pattern SD1 may have an uneven embossing shape. In other words, the sidewall of the first source / drain pattern SD1 may have a wave-patterned profile. The sidewall of the first source / drain pattern SD1 may protrude toward first to third portions PO1, PO2, and PO3 of the gate electrode GE, which will be described later.
[0037] A gate electrode GE may be provided on the first and second channel patterns CH1, CH2. Each gate electrode GE may extend in a first direction D1 across the first and second channel patterns CH1, CH2. Each gate electrode GE may be vertically overlapped with the first and second channel patterns CH1, CH2. The gate electrodes GE may be arranged in a second direction D2 according to a first pitch.
[0038] The gate electrode GE may include a first portion PO1 interposed between the active pattern AP1 or AP2 and the first semiconductor pattern SP1, a second portion PO2 interposed between the first semiconductor pattern SP1 and the second semiconductor pattern SP2, a third portion PO3 interposed between the second semiconductor pattern SP2 and the third semiconductor pattern SP3, and a fourth portion PO4 on the third semiconductor pattern SP3.
[0039] 5D, the gate electrode GE may be provided on the top surface TS, bottom surface BS, and side walls SW of each of the first to third semiconductor patterns SP1, SP2, and SP3. In other words, the transistor according to this embodiment may be a three-dimensional field effect transistor (e.g., MBCFET or GAAFET) in which the gate electrode GE three-dimensionally surrounds the channel.
[0040] An inner spacer ISP may be interposed between the first to third portions PO1, PO2, and PO3 of the gate electrode GE and the second source / drain pattern SD2 on the NMOSFET region. Each of the first to third portions PO1, PO2, and PO3 of the gate electrode GE may be spaced apart from the second source / drain pattern SD2 via the inner spacer ISP. The inner spacer ISP may prevent leakage current from the gate electrode GE.
[0041] 4 and 5A to 5D again, a pair of gate spacers GS may be disposed on both side walls of the fourth portion PO4 of the gate electrode GE. The gate spacer GS may extend in a first direction D1 along the gate electrode GE. An upper surface of the gate spacer GS may be higher than an upper surface of the gate electrode GE. An upper surface of the gate spacer GS may be coplanar with an upper surface of a first interlayer insulating film 110 described below. In one embodiment, the gate spacer GS may include at least one of SiCN, SiCON, and SiN. In another embodiment, the gate spacer GS may include a multi-layer made of at least two of SiCN, SiCON, and SiN.
[0042] A gate capping pattern GP may be provided on the gate electrode GE. The gate capping pattern GP may extend in a first direction D1 along the gate electrode GE. The gate capping pattern GP may include a material having an etch selectivity with respect to the first and second interlayer insulating films 110 and 120 described below. Specifically, the gate capping pattern GP may include at least one of SiON, SiCN, SiCON, and SiN.
[0043] A gate insulating film GI may be interposed between the gate electrode GE and the first channel pattern CH1 and between the gate electrode GE and the second channel pattern CH2. The gate insulating film GI may cover a top surface TS, a bottom surface BS, and both side walls SW of each of the first to third semiconductor patterns SP1, SP2, and SP3. The gate insulating film GI may cover an upper surface of the device isolation film ST below the gate electrode GE.
[0044] In one embodiment of the present invention, the gate insulating film GI may include a silicon oxide film, a silicon oxynitride film, and / or a high dielectric film. The high dielectric film may include a high dielectric constant material having a higher dielectric constant than a silicon oxide film. As an example, the high dielectric constant material may include at least one of hafnium oxide, hafnium silicon oxide, hafnium zirconium oxide, hafnium tantalum oxide, lanthanum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, lithium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.
[0045] The gate electrode GE may include a first electrode pattern and a second electrode pattern on the first electrode pattern. The first electrode pattern may be provided on the gate insulating film GI and may be adjacent to the first to third semiconductor patterns SP1, SP2, and SP3. The first electrode pattern may include a work function metal for adjusting a threshold voltage of a transistor. A desired threshold voltage of the transistor may be achieved by adjusting a thickness and a composition of the first electrode pattern. For example, the first to third inner electrodes PO1, PO2, and PO3 of the gate electrode GE may be formed of the first electrode pattern which is a work function metal.
[0046] The first electrode pattern may include a metal nitride film. For example, the first electrode pattern may include at least one metal selected from the group consisting of titanium (Ti), tantalum (Ta), aluminum (Al), tungsten (W), and molybdenum (Mo) and nitrogen (N). Furthermore, the first electrode pattern may further include carbon (C). The first electrode pattern may include a plurality of stacked work function metal films.
[0047] The second electrode pattern may include a metal having a lower resistance than the first electrode pattern. For example, the second electrode pattern may include at least one metal selected from the group consisting of tungsten (W), aluminum (Al), titanium (Ti), and tantalum (Ta). For example, the outer electrode PO4 of the gate electrode GE may include a first electrode pattern and a second electrode pattern on the first electrode pattern.
[0048] A first interlayer insulating film 110 may be provided on the substrate 100. The first interlayer insulating film 110 may cover the gate spacer GS and the first and second source / drain patterns SD1 and SD2. An upper surface of the first interlayer insulating film 110 may be substantially coplanar with an upper surface of the gate capping pattern GP and an upper surface of the gate spacer GS. A second interlayer insulating film 120 covering the gate capping pattern GP may be provided on the first interlayer insulating film 110. A third interlayer insulating film 130 may be provided on the second interlayer insulating film 120. A fourth interlayer insulating film 140 may be provided on the third interlayer insulating film 130. As an example, the first to fourth interlayer insulating films 110-140 may include silicon oxide films.
[0049] The single height cell SHC may have a first boundary BD1 and a second boundary BD2 facing each other in a second direction D2. The first and second boundaries BD1, BD2 may extend in the first direction D1. The single height cell SHC may have a third boundary BD3 and a fourth boundary BD4 facing each other in the first direction D1. The third and fourth boundaries BD3, BD4 may extend in the second direction D2.
[0050] A pair of isolation structures DB facing each other in the second direction D2 may be provided on both sides of the single height cell SHC. For example, the pair of isolation structures DB may be provided on first and second boundaries BD1 and BD2 of the single height cell SHC, respectively. The isolation structures DB may extend parallel to the gate electrodes GE in the first direction D1. A pitch between the isolation structures DB and the gate electrodes GE adjacent thereto may be equal to the first pitch.
[0051] The isolation structure DB may extend into the first and second active patterns AP1 and AP2 through the first and second interlayer insulating films 110 and 120. The isolation structure DB may penetrate the upper portions of the first and second active patterns AP1 and AP2. The isolation structure DB may electrically isolate the active region of the single height cell SHC from the active regions of other adjacent cells.
[0052] An active contact AC may be provided to penetrate the first and second interlayer insulating films 110 and 120 and be electrically connected to the first and second source / drain patterns SD1 and SD2, respectively. A pair of active contacts AC may be provided on both sides of the gate electrode GE, respectively. In a plan view, the active contacts AC may have a bar shape extending in a first direction D1.
[0053] The active contact AC may be a self-aligned contact. In other words, the active contact AC may be formed in a self-aligned manner using the gate capping pattern GP and the gate spacer GS. For example, the active contact AC may cover at least a portion of a sidewall of the gate spacer GS. Although not shown, the active contact AC may cover a portion of an upper surface of the gate capping pattern GP.
[0054] A gate contact GC may be provided through the second interlayer insulating film 120 and the gate capping pattern GP to be electrically connected to the gate electrode GE. In a plan view, the gate contact GC may be disposed to overlap the first active region AR1 and the second active region AR2. For example, the gate contact GC may be provided on the second active pattern AP2.
[0055] The gate contact GC may include a conductive pattern FM and a barrier pattern BM surrounding the conductive pattern FM. For example, the conductive pattern FM may include at least one metal selected from aluminum, copper, tungsten, molybdenum, and cobalt. The barrier pattern BM may cover the sidewall and bottom surface of the conductive pattern FM. The barrier pattern BM may include a metal film / metal nitride film. The metal film may include at least one of titanium, tantalum, tungsten, nickel, cobalt, and platinum. The metal nitride film may include at least one of a titanium nitride film (TiN), a tantalum nitride film (TaN), a tungsten nitride film (WN), a nickel nitride film (NiN), a cobalt nitride film (CoN), and a platinum nitride film (PtN).
[0056] A first metal layer M1 may be provided in the third interlayer insulating film 130. For example, the first metal layer M1 may include a first power wiring M1_R1, a second power wiring M1_R2, and a first wiring M1_I. Each of the wirings M1_R1, M1_R2, and M1_I of the first metal layer M1 may extend parallel to each other in the second direction D2.
[0057] Specifically, the first and second power wirings M1_R1 and M1_R2 may be provided on third and fourth boundaries BD3 and BD4, respectively, of the single height cell SHC. The first power wiring M1_R1 may extend in the second direction D2 along the third boundary BD3. The second power wiring M1_R2 may extend in the second direction D2 along the fourth boundary BD4.
[0058] The first wirings M1_I of the first metal layer M1 may be disposed between the first and second power wirings M1_R1, M1_R2. The first wirings M1_I of the first metal layer M1 may be arranged along the first direction D1 at a second pitch. The second pitch may be smaller than the first pitch. The line width of each of the first wirings M1_I may be smaller than the line width of each of the first and second power wirings M1_R1, M1_R2.
[0059] The first metal layer M1 may further include a first via VI1. The first via VI1 may be provided under each of the lines M1_R1, M1_R2, and M1_I of the first metal layer M1. The active contact AC and the lines of the first metal layer M1 may be electrically connected to each other through the first via VI1. The gate contact GC and the lines of the first metal layer M1 may be electrically connected to each other through the first via VI1.
[0060] The wiring of the first metal layer M1 and the first via VI1 thereunder may be formed in separate processes. In other words, the wiring of the first metal layer M1 and the first via VI1 may be formed in a single damascene process. The semiconductor device according to this embodiment may be formed using a process of less than 20 nm.
[0061] A second metal layer M2 may be provided in the fourth interlayer insulating film 140. The second metal layer M2 may include a plurality of second wirings M2_I. Each of the second wirings M2_I of the second metal layer M2 may have a line shape or a bar shape extending in the first direction D1. In other words, the second wirings M2_I may extend parallel to each other in the first direction D1.
[0062] The second metal layer M2 may further include a second via VI2 provided under each of the second wirings M2_I. The wiring of the first metal layer M1 and the wiring of the second metal layer M2 may be electrically connected to each other through the second via VI2. For example, the wiring of the second metal layer M2 and the second via VI2 thereunder may be formed together by a dual damascene process.
[0063] The wiring of the first metal layer M1 and the wiring of the second metal layer M2 may include the same or different conductive materials. For example, the wiring of the first metal layer M1 and the wiring of the second metal layer M2 may include at least one metal material selected from aluminum, copper, tungsten, molybdenum, ruthenium, and cobalt. Although not shown, metal layers (e.g., M3, M4, M5...) stacked on the fourth interlayer insulating film 140 may be additionally disposed. Each of the stacked metal layers may include wiring for routing between cells.
[0064] The active contact AC and the first and second source / drain patterns SD1, SD2 will be described in more detail with reference to Figures 6, 7, and 8. Figure 6 is an enlarged view of an embodiment of region M of Figure 5A. Figure 7 is an enlarged view of an embodiment of region N of Figure 5B. Figure 8 is an enlarged view of an embodiment of region A of Figure 5C.
[0065] 6, the first source / drain pattern SD1 may include a buffer layer BFL and a main layer MAL on the buffer layer BFL. The buffer layer BFL may cover an inner wall of the first recess RS1. The buffer layer BFL may have a U-shape along the profile of the first recess RS1.
[0066] The buffer layer BFL may include a semiconductor element (e.g., SiGe) having a lattice constant larger than that of the semiconductor element of the substrate 100. The buffer layer BFL may include a relatively low concentration of germanium (Ge). In another embodiment of the present invention, the buffer layer BFL may include only silicon (Si) without germanium (Ge). For example, the concentration of germanium (Ge) in the buffer layer BFL may be 0 at% to 30 at%. The main layer MAL may include a relatively high concentration of germanium (Ge). The concentration of germanium (Ge) in the main layer MAL may be higher than the concentration of germanium (Ge) in the buffer layer BFL. For example, the concentration of germanium (Ge) in the main layer MAL may be 30 at% to 70 at%.
[0067] An active contact AC may be formed on the first source / drain pattern SD1. A lower surface of the active contact AC may be lower than an upper surface of the top semiconductor pattern SP3. A lower portion of the active contact AC may be provided in a first recess RS1. A first silicon layer SL1 and a first silicide layer SC1 may be provided between the first source / drain pattern SD1 and the active contact AC. Specifically, the first silicon layer SL1 may be provided on the buffer layer BFL and the main layer MAL. A first silicide layer SC1 may be provided between the first silicon layer SL1 and the active contact AC.
[0068] The active contact AC may be electrically connected to the source / drain patterns SD1, SD2 through the first silicide layer SC1. For example, the first silicide layer SC1 may include at least one of titanium silicide, tantalum silicide, tungsten silicide, nickel silicide, and cobalt silicide. The first silicide layer SC1 may be doped with impurities. The first silicide layer SC1 may have a higher impurity concentration in a portion adjacent to the active contact AC. The first silicon layer SL1 and the first source / drain pattern SD1 may also be doped with impurities, and the first silicide layer SC1 may have a higher impurity concentration in a portion adjacent to the first silicide layer SC1. The impurities may include at least one of B (boron), Ga (gallium), and In (indium).
[0069] 8, the active contact AC may extend from an upper surface to both side walls of the first source / drain pattern SD1 and may have a wrap-around structure covering the upper surface and both side walls of the first source / drain pattern SD1.
[0070] A sidewall of the first source / drain pattern SD1 may include a first surface SPW1 and a second surface SPW2. The first surface SPW1 and the second surface SPW2 may meet to define an apex of the first source / drain pattern SD1. One of the slopes of the first surface SPW1 and the second surface SPW2 may be a positive slope, and the other may be a negative slope.
[0071] The active contact AC may include a first extension AC1a covering the first surface SPW1 and a second extension AC1b covering the second surface SPW2. The first extension AC1a may have a first gradient and extend along the first surface SPW1, and the second extension AC1b may have a second gradient and extend along the second surface SPW2. One of the first gradient and the second gradient may be a positive gradient, and the other may be a negative gradient. Thus, the active contact AC may extend along both side walls of the first source / drain pattern SD1. The first layer L1, the second layer L2, and the stop film STL described below may also extend along both side walls of the first source / drain pattern SD1 like the first and second extensions AC1a and AC1b of the active contact.
[0072] The active contact AC may include a first portion AC1 covering both sidewalls of the first source / drain pattern SD1 and a second portion AC2 covering an upper surface of the first source / drain pattern SD1. A first layer L1 may be provided between the first source / drain pattern SD1 and the active contact AC. The first layer L1 may include a first silicon layer SL1 and a first silicide layer SC1 on the first silicon layer SL1. The first silicon layer SL1 may cover an upper surface and both sidewalls of the first source / drain pattern SD1. The first silicide layer SC1 may cover an upper surface and both sidewalls of the first silicon layer SL1.
[0073] A second layer L2 may be provided that is separated from the first layer L1 via a first portion AC1. The second layer L2 may include a second silicide layer SC2 and a second silicon layer SL2 on the second silicide layer SC2. The second silicide layer SC2 may cover an outer wall of the first portion AC1. The outer wall of the first portion AC1 may be an opposite side to a surface where the first portion AC1 contacts the first layer L1. The second silicon layer SL2 may cover an outer wall of the second silicide layer SC2. The outer wall of the second silicide layer SC2 may be an opposite side to a surface where the second silicide layer SC2 contacts the first portion AC.
[0074] A stop layer STL may be provided on an outer wall of the second layer L2. The outer wall of the second layer L2 may be the side wall opposite to the side wall where the second layer L2 contacts the active contact AC. The stop layer STL may include a silicon nitride (SiN) layer.
[0075] The active contact AC may include a conductive pattern FM and a barrier pattern BM surrounding the conductive pattern FM. The barrier pattern BM may be provided between the conductive pattern FM and the first layer L1 and between the conductive pattern FM and the second layer L2. The barrier pattern BM may cover an upper surface and both side walls of the first silicide layer SC1.
[0076] For example, the conductive pattern FM may include at least one metal selected from aluminum, copper, tungsten, molybdenum, and cobalt. The barrier pattern BM may cover the sidewall and bottom surface of the conductive pattern FM. The barrier pattern BM may include a metal film / metal nitride film. The metal film may include at least one of titanium, tantalum, tungsten, nickel, cobalt, and platinum. The metal nitride film may include at least one of titanium nitride film (TiN), tantalum nitride film (TaN), tungsten nitride film (WN), nickel nitride film (NiN), cobalt nitride film (CoN), and platinum nitride film (PtN).
[0077] 7, the active contact AC on the second source / drain pattern SD2 may include the same technical features as the active contact AC on the first source / drain pattern SD1, except that the impurity of the first silicide layer SC1 on the second source / drain pattern SD2 may include at least one of As (arsenic), P (phosphorus), and Sb (antimony).
[0078] According to the present invention, the active contact AC may cover the top surface and both side walls of the first and second source / drain patterns SD1, SD2. Therefore, the contact area between the active contact AC and the first and second source / drain patterns SD1, SD2 may be increased, and the contact resistance between the active contact AC and the first and second source / drain patterns SD1, SD2 may be reduced. A first layer L1 may be formed between the first and second source / drain patterns SD1, SD2 and the active contact AC, and a second layer L2 may be formed separated from the first and second source / drain patterns SD1, SD2 via the active contact AC. Each of the first and second silicide layers SC1, SC2 may be doped with impurities, thereby further reducing the contact resistance between the active contact AC and the first and second source / drain patterns SD1, SD2. As a result, the semiconductor device to which the present invention is applied may have improved reliability and electrical characteristics.
[0079] 9A to 18 are cross-sectional views for explaining a method for manufacturing a semiconductor device according to an embodiment of the present invention. FIGS. 9A, 10A, 11A, 12A, 13A, and 14A are cross-sectional views taken along line A-A' in FIG. 4. FIGS. 11B, 12B, 13B, and 14B are cross-sectional views taken along line B-B' in FIG. 4. FIGS. 11C, 12C, 13C, 14C, 15A, 16A, and 18 are cross-sectional views taken along line C-C' in FIG. 4. FIGS. 9B, 10B, 13D, and 14D are cross-sectional views taken along line D-D' in FIG. 4.
[0080] Figures 12D and 12E are enlarged views showing region M of Figure 12A and region N of Figure 12B, respectively. Figures 15B and 15C are views for explaining a manufacturing method for forming the first source / drain pattern SD1 shown in Figure 6. Figures 16B and 16C are views for explaining a manufacturing method for forming the second source / drain pattern SD2 shown in Figure 7. Figures 16D and 17 are views for explaining a manufacturing method for forming the first source / drain pattern SD1 shown in Figure 8.
[0081] 9A and 9B, a substrate 100 including a PMOSFET region PR and an NMOSFET region NR may be provided. An active layer ACL and a sacrificial layer SAL may be formed on the substrate 100, which are alternately stacked. The active layer ACL may include one of silicon (Si), germanium (Ge), and silicon-germanium (SiGe), and the sacrificial layer SAL may include another of silicon (Si), germanium (Ge), and silicon-germanium (SiGe).
[0082] The sacrificial layer SAL may include a material having an etching selectivity with respect to the active layer ACL. For example, the active layer ACL may include silicon (Si), and the sacrificial layer SAL may include silicon-germanium (SiGe). The concentration of germanium (Ge) in each of the sacrificial layers SAL may be 10 at% to 50 at%.
[0083] Mask patterns may be formed on the PMOSFET region PR and the NMOSFET region NR of the substrate 100. The mask patterns may have a line shape or a bar shape extending in the second direction D2.
[0084] A patterning process may be performed using the mask pattern as an etching mask to form trenches TR defining first and second active patterns AP1 and AP2. The first and second active patterns AP1 and AP2 may be formed on the PMOSFET region PR and the NMOSFET region NR, respectively.
[0085] A stack pattern STP may be formed on each of the first and second active patterns AP1 and AP2. The stack pattern STP may include active layers ACL and sacrificial layers SAL alternately stacked with each other. The stack pattern STP may be formed together with the first and second active patterns AP1 and AP2 during the patterning process.
[0086] An isolation layer ST may be formed to fill the trench TR. An isolation layer ST may be formed on the liner layer FL. In particular, an insulating layer may be formed on the entire surface of the substrate 100 to cover the first and second active patterns AP1 and AP2 and the stack pattern STP. The insulating layer may be recessed until the stack pattern STP is exposed, and then the isolation layer ST may be formed.
[0087] The isolation layer ST may include an insulating material such as a silicon oxide layer. The stack pattern STP may be exposed on the isolation layer ST. In other words, the stack pattern STP may protrude vertically onto the isolation layer ST.
[0088] 10A and 10B, sacrificial patterns PP may be formed across stack patterns STP on a substrate 100. Each sacrificial pattern PP may be formed in a line shape or a bar shape extending in a first direction D1. The sacrificial patterns PP may be arranged along a second direction D2 at a first pitch.
[0089] Specifically, forming the sacrificial pattern PP may include forming a sacrificial layer on the entire surface of the substrate 100, forming a hard mask pattern MP on the sacrificial layer, and patterning the sacrificial layer using the hard mask pattern MP as an etching mask. The sacrificial layer may include polysilicon.
[0090] A pair of gate spacers GS may be formed on both sidewalls of each of the sacrificial patterns PP. Forming the gate spacers GS may include conformally forming a gate spacer film on the entire surface of the substrate 100 and anisotropically etching the gate spacer film. The gate spacer film may include at least one of SiCN, SiCON, and SiN. As another example, the gate spacer film may be a multi-layer including at least two of SiCN, SiCON, and SiN.
[0091] 11A to 11C, a first recess RS1 may be formed in a stack pattern STP on a first active pattern AP1. A second recess RS2 may be formed in a stack pattern STP on a second active pattern AP2. During the formation of the first and second recesses RS1 and RS2, the device isolation layers ST on both sides of each of the first and second active patterns AP1 and AP2 may be further recessed (see FIG. 11C).
[0092] Specifically, the stack pattern STP on the first active pattern AP1 may be etched using the hard mask pattern MP and the gate spacer GS as an etching mask to form the first recess RS1. The first recess RS1 may be formed between a pair of sacrificial patterns PP. Forming the first recess RS1 may include additionally performing a selective etching process on the exposed sacrificial layer SAL. Thus, the first recess RS1 may have a corrugated inner wall.
[0093] The second recess RS2 in the stack pattern STP on the second active pattern AP2 may be formed in the same manner as forming the first recess RS1, except that forming the second recess RS2 may further include forming an inner spacer ISP in the region where the sacrificial layer SAL is recessed. As a result, the inner sidewall of the second recess RS2 may not have a wavy pattern like the inner sidewall of the first recess RS1.
[0094] First to third semiconductor patterns SP1, SP2, SP3 may be formed between adjacent first recesses RS1 from the active layer ACL. First to third semiconductor patterns SP1, SP2, SP3 may be formed between adjacent second recesses RS2 from the active layer ACL. Thus, the first semiconductor pattern SP1 may be formed at the bottom of the semiconductor pattern, and the third semiconductor pattern SP3 may be formed at the top of the semiconductor pattern. The first to third semiconductor patterns SP1, SP2, SP3 between adjacent first recesses RS1 may form a first channel pattern CH1. The first to third semiconductor patterns SP1, SP2, SP3 between adjacent second recesses RS2 may form a second channel pattern CH2.
[0095] 12A to 12E, a first source / drain pattern SD1 may be formed in each of the first recesses RS1, and FIGS. 12D and 12E are enlarged views of an M region of FIG. 12A and an N region of FIG. 12B, respectively.
[0096] 12A and 12D, a buffer layer BFL may be formed by performing a SEG process using the inner wall of the first recess RS1 as a seed layer. The buffer layer BFL may be grown using the first to third semiconductor patterns SP1, SP2, and SP3 exposed by the first recess RS1 and the substrate 100 as seeds. For example, the SEG process may include a Chemical Vapor Deposition (CVD) process or a Molecular Beam Epitaxy (MBE) process.
[0097] The buffer layer BFL may include a semiconductor element (e.g., SiGe) having a lattice constant larger than that of the semiconductor element of the substrate 100. The buffer layer BFL may include a relatively low concentration of germanium (Ge). In another embodiment of the present invention, the buffer layer BFL may include only silicon (Si) without germanium (Ge). The concentration of germanium (Ge) in the buffer layer BFL may be 0 at% to 30 at%.
[0098] The main layer MAL may be formed by performing a SEG process on the buffer layer BFL. The main layer MAL may be formed to completely fill the first recess RS1. The main layer MAL may contain a relatively high concentration of germanium (Ge). For example, the concentration of germanium (Ge) in the main layer MAL may be 30 at % to 70 at %.
[0099] During the formation of the buffer layer BFL and the main layer MAL, impurities (e.g., boron, gallium, or indium) that cause the first source / drain pattern SD1 to have a p-type may be implanted in-situ. As another example, impurities may be implanted into the first source / drain pattern SD1 after the first source / drain pattern SD1 is formed.
[0100] A second source / drain pattern SD2 may be formed in each of the second recesses RS2. Specifically, the second source / drain pattern SD2 may be formed by performing a SEG process using an inner wall of the second recess RS2 as a seed layer. For example, the second source / drain pattern SD2 may include the same semiconductor element (e.g., Si) as the substrate 100.
[0101] While the second source / drain pattern SD2 is formed, impurities (e.g., phosphorus, arsenic, or antimony) that cause the second source / drain pattern SD2 to have n-type may be implanted in-situ. As another example, impurities may be implanted into the second source / drain pattern SD2 after the second source / drain pattern SD2 is formed.
[0102] 12C to 12D, a first silicon layer SL1 may be formed on the buffer layer BFL and the main layer MAL. The first silicon layer SL1 may cover an upper surface and both side walls of the first source / drain pattern SD1. An etching pattern SF may be formed on the first silicon layer SL1, and a second silicon layer SL2 may be formed on the etching pattern SF. The etching pattern SF may extend from an upper surface of the first silicon layer SL1 to both side walls. The second silicon layer SL2 may extend from an upper surface of the etching pattern SF to both side walls. The etching pattern SF may be formed between the first silicon layer SL1 and the second silicon layer SL2. The average thickness of the etching pattern SF may be greater than the average thicknesses of the first and second silicon layers SL1 and SL2.
[0103] The etching pattern SF may include silicon-germanium (SiGe). The concentration of germanium (Ge) in the etching pattern SF may be higher than that of the first and second silicon layers SL1 and SL2. The etching pattern SF may include a material having etching selectivity with respect to the first and second silicon layers SL1 and SL2. The first and second silicon layers SL1 and SL2 may not include germanium (Ge). The first silicon layer SL1 and the second silicon layer SL2 may include substantially the same material.
[0104] A stop layer STL may be formed on the second silicon layer SL2. The stop layer STL may extend from an upper surface of the second silicon layer SL2 to both side walls. The stop layer STL may include a material having an etch selectivity with respect to the first interlayer insulating film 110 described below. For example, the stop layer STL may include a silicon nitride (SiN) layer.
[0105] 13A to 13D, a first interlayer insulating film 110 may be formed to cover the first and second source / drain patterns SD1 and SD2, the hard mask pattern MP, and the gate spacer GS. As an example, the first interlayer insulating film 110 may include a silicon oxide film.
[0106] The first interlayer insulating film 110 may be planarized until the top surface of the sacrificial pattern PP is exposed. The planarization of the first interlayer insulating film 110 may be performed using an etch back or chemical mechanical polishing (CMP) process. During the planarization process, the hard mask pattern MP may be entirely removed. As a result, the top surface of the first interlayer insulating film 110 may be coplanar with the top surface of the sacrificial pattern PP and the top surface of the gate spacer GS.
[0107] The exposed sacrificial pattern PP may be selectively removed. By removing the sacrificial pattern PP, an outer region ORG exposing the first and second channel patterns CH1 and CH2 may be formed (see FIG. 13D). The removal of the sacrificial pattern PP may include wet etching using an etchant that selectively etches polysilicon.
[0108] The sacrificial layer SAL exposed through the outer region ORG may be selectively removed to form the inner region IRG (see FIG. 13D). In particular, an etching process for selectively etching the sacrificial layer SAL may be performed to remove only the sacrificial layer SAL while leaving the first to third semiconductor patterns SP1, SP2, and SP3 as they are. The etching process may have a high etching rate for silicon-germanium having a relatively high germanium concentration. For example, the etching process may have a high etching rate for silicon-germanium having a germanium concentration of more than 10 at%.
[0109] During the etching process, the sacrificial layer SAL on the PMOSFET region PR and the NMOSFET region NR may be removed. The etching process may be a wet etching process. An etching material used in the etching process may quickly remove the sacrificial layer SAL having a relatively high germanium concentration.
[0110] 13D, the sacrificial layer SAL is selectively removed, so that only the first to third semiconductor patterns SP1, SP2, and SP3 stacked on the first and second active patterns AP1 and AP2 are left. First to third inner regions IRG1, IRG2, and IRG3 may be formed through the regions from which the sacrificial layer SAL is removed.
[0111] Specifically, a first inner region IRG1 may be formed between the active pattern AP1 or AP2 and the first semiconductor pattern SP1, a second inner region IRG2 may be formed between the first semiconductor pattern SP1 and the second semiconductor pattern SP2, and a third inner region IRG3 may be formed between the second semiconductor pattern SP2 and the third semiconductor pattern SP3.
[0112] 13A to 13D, a gate insulating layer GI may be formed on the exposed first to third semiconductor patterns SP1, SP2, and SP3. The gate insulating layer GI may be formed to surround each of the first to third semiconductor patterns SP1, SP2, and SP3. The gate insulating layer GI may be formed in each of the first to third inner regions IRG1, IRG2, and IRG3. The gate insulating layer GI may be formed in the outer region ORG.
[0113] 14A to 14D, a gate electrode GE may be formed on the gate insulating film GI. The gate electrode GE may be formed to fill first to third inner regions IRG1, IRG2, and IRG3 and an outer region ORG. The gate electrode GE may include a first portion PO1, a second portion PO2, and a third portion PO3 that fill the first to third inner regions IRG1, IRG2, and IRG3, respectively. The gate electrode GE may include a fourth portion PO4 that fills the outer region ORG. A gate capping pattern GP may be formed on the gate electrode GE.
[0114] 14A to 14D, a second interlayer insulating layer 120 may be formed on the first interlayer insulating layer 110. The second interlayer insulating layer 120 may include a silicon oxide layer.
[0115] A method for forming an active contact AC will be described in more detail with reference to Figures 15A to 18. Figures 15B and 15C are views for explaining a manufacturing method for forming the first source / drain pattern SD1 shown in Figure 6.
[0116] 15A to 15C, the first and second interlayer insulating films 110 and 120 may be etched to form first and second recess holes RSH1 and RSH2 exposing the stop layer STL. The first recess hole RSH1 may be formed on the PMOSFET region PR, and the second recess hole RSH2 may be formed on the NMOSFET region NR. The level of the bottom surface of each of the first and second recess holes RSH1 and RSH2 may be lower than the level of the top surface of the stop layer STL and the level of the top surface of the etching pattern SF. The stop layer STL may not be removed by the etching process.
[0117] After the first and second recess holes RSH1 and RSH2 are formed, a part of the stopping film STL and a part of the second silicon layer SL2 may be removed. Specifically, only the upper part of the stopping film STL and the upper part of the second silicon layer SL2 exposed by the first and second recess holes RSH1 and RSH2 may be removed. Therefore, the stopping film STL and the second silicon layer SL2 located below the level of the lowest surface of each of the first and second recess holes RSH1 and RSH2 may remain without being removed. As the upper part of the stopping film STL and the upper part of the second silicon layer SL2 are removed, the etching pattern SF may be exposed by the first and second recess holes RSH1 and RSH2.
[0118] 16B and 16C are views for explaining a manufacturing method for forming the second source / drain pattern SD2 shown in Fig. 7. Figs. 16D and 17 are views for explaining a manufacturing method for forming the first source / drain pattern SD1 shown in Fig. 8.
[0119] 16A to 16D, the etching pattern SF exposed by the first and second recess holes RSH1 and RSH2 may be removed by a first etching process. More specifically, the first etching process may be a wet etch or a dry etch. The dry etch may be performed using a fluorine (F 2 ), Chlorine (Cl 2), and hydrogen chloride (HCl) may be used, and the wet etching may be performed using hydrogen peroxide (H 2 O 2 ), acetic acid (CH 3 A solution containing at least one of hydrogen peroxide (COOH), hydrogen fluoride (HF), and fluorine (HF) can be used.
[0120] Therefore, the first and second silicon layers SL1 and SL2 may be exposed by the first and second recess holes RSH1 and RSH2. Impurities may be implanted and doped on the exposed outer wall OW of the first silicon layer SL1 and the exposed outer wall IW of the second silicon layer SL2. The impurities may be implanted on the outer walls OW and IW by a plasma doping (PLAD) method. More specifically, impurity ions in a plasma state may be directly implanted on the outer walls OW and IW of the first and second silicon layers SL1 and SL2. The impurities on the PMOSFET region PR may include at least one of B (boron), Ga (gallium) and In (indium). The impurities on the NMOSFET region NR may include at least one of As (arsenic), P (phosphorus) and Sb (antimony).
[0121] 16D, the first and second silicon layers SL1 and SL2 may have a higher impurity concentration in the portions adjacent to the outer walls OW and IW, respectively. By implanting the impurities, the contact resistance between the active contact AC and the first and second source / drain patterns SD1 and SD2, which will be described later, may be reduced.
[0122] 17, a first silicide layer SC1 may be formed on an exposed outer wall OW of the first silicon layer SL1. A second silicide layer SC2 may be formed on an exposed outer wall IW of the second silicon layer SL2. In particular, a metal material may be deposited on the outer wall OW of the first silicon layer SL1 to form the first silicide layer SC1. A metal material may be deposited on the outer wall IW of the second silicon layer SL2 to form the second silicide layer SC2. The metal material may include at least one of titanium, tantalum, tungsten, nickel, and cobalt. Depositing the metal material may include a chemical vapor deposition (CVD) process.
[0123] Referring again to FIG. 18 and FIG. 8, an active contact AC may be formed in each of the first and second recess holes RSH1 and RSH2. Forming the active contact AC may include forming a barrier pattern BM and forming a conductive pattern FM on the barrier pattern BM. The barrier pattern BM may be conformally formed and may include a metal film / metal nitride film. The metal film may include at least one of titanium, tantalum, tungsten, nickel, cobalt, and platinum. The metal nitride film may include at least one of a titanium nitride film (TiN), a tantalum nitride film (TaN), a tungsten nitride film (WN), a nickel nitride film (NiN), a cobalt nitride film (CoN), and a platinum nitride film (PtN). The conductive pattern FM may include a low resistance metal. For example, the conductive pattern FM may include at least one of aluminum, copper, tungsten, molybdenum, and cobalt.
[0124] A gate contact GC may be formed through the second interlayer insulating film 120 and the gate capping pattern GP to be electrically connected to the gate electrode GE. The formation of the gate contact GC may be the same as the formation of the active contact AC.
[0125] An isolation structure DB may be formed at a first boundary BD1 and a second boundary BD2 of the single height cell SHC. The isolation structure DB may extend from the second interlayer insulating film 120 through the gate electrode GE into the active pattern AP1 or AP2. The isolation structure DB may include an insulating material such as a silicon oxide layer or a silicon nitride layer.
[0126] A third interlayer insulating film 130 may be formed on the active contacts AC and the gate contacts GC. A first metal layer M1 may be formed in the third interlayer insulating film 130. A fourth interlayer insulating film 140 may be formed on the third interlayer insulating film 130. A second metal layer M2 may be formed in the fourth interlayer insulating film 140.
[0127] 19 is an enlarged view of region A of FIG. 5C according to another embodiment of the present invention. Referring to FIG. 19, the fence portion FEP on the sidewalls of the first and second active patterns AP1 and AP2 may protrude above the isolation layer ST. The fence portion FEP may be a part of the gate spacer GS remaining on the upper sidewalls of each of the first and second active patterns AP1 and AP2. In other words, the fence portion FEP according to this embodiment may include the same insulating material as the gate spacer GS.
[0128] The fence part FEP may cover the lower sidewalls of the first and second source / drain patterns SD1 and SD2. An upper surface of the fence part FEP may be higher than the bottom of the first recess RS1. In this case, a sidewall of the first layer L1 may be in direct contact with the fence part FEP. At least a portion of the second layer L2 may be in contact with the fence part FEP.
[0129] The fence part FEP may be in direct contact with the lower surface of each of the first and second silicide layers SC1 and SC2. The fence part FEP may be in direct contact with the lower surface of each of the first and second silicon layers SL1 and SL2. The fence part FEP may also be in direct contact with the lower surface of the barrier pattern BM and the lower surface of the conductive pattern FM.
[0130] Although the embodiments of the present invention have been described above with reference to the attached drawings, the present invention may be embodied in other specific forms without modifying the technical concept or essential features thereof. Therefore, it should be understood that the embodiments described above are illustrative in all respects and are not limiting. [Explanation of symbols]
[0131] 100 Substrates 110, 120, 130, 140 Interlayer insulating film AC Active Contact AP1, AP2 activity patterns AR1, AR2 active region BM Barrier Pattern FM Conductive Pattern GC Gate Contact GP Gate Capping Pattern GS Gate Spacer SC1, SC2 silicide layer SD1, SD2 source / drain patterns
Claims
1. a substrate including an active region; an active pattern on the active area; a source / drain pattern on the active pattern; an active contact extending from an upper surface to a sidewall of the source / drain pattern, the active contact including a first portion covering the sidewall of the source / drain pattern and a second portion covering the upper surface of the source / drain pattern; a first layer provided between the source / drain pattern and the first portion; a second layer separated from the first layer via the first portion, The semiconductor device, wherein the first layer and the second layer each include a silicide layer.
2. 2. The semiconductor device of claim 1, wherein the first layer comprises a first silicon layer covering an upper surface and both sidewalls of the source / drain pattern and a first silicide layer on the first silicon layer.
3. 2. The semiconductor device of claim 1, wherein the second layer includes a second silicide layer overlying an outer wall of the first portion and a second silicon layer overlying the second silicide layer.
4. 2. The semiconductor device of claim 1, wherein the silicide layer comprises at least one of titanium silicide, tantalum silicide, tungsten silicide, nickel silicide, and cobalt silicide.
5. the active contact includes a conductive pattern and a barrier pattern surrounding the conductive pattern; The semiconductor device of claim 1 , wherein the barrier pattern is provided between the conductive pattern and the first layer and between the conductive pattern and the second layer.
6. The semiconductor device of claim 5 , wherein the barrier pattern covers an upper surface and both sidewalls of the silicide layer.
7. a stop film on a sidewall of the second layer; The semiconductor device of claim 1 , wherein the stop film comprises SiN.
8. 2. The semiconductor device of claim 1, wherein the silicide layer has a higher impurity concentration in a region closer to the active contact.
9. The semiconductor device according to claim 2 , wherein the first silicon layer has a higher impurity concentration as it is closer to the silicide layer.
10. a substrate including an active region; an active pattern on the active area; a source / drain pattern on the active pattern; an active contact electrically connected to the source / drain pattern; a sidewall of the source / drain pattern includes a first surface and a second surface; the first surface and the second surface meet to define a vertex of the source / drain pattern; the active contact includes a first extension over the first surface and a second extension over the second surface; the first extension has a first slope and extends along the first surface; the second extension has a second slope and extends along the second surface; A semiconductor device, wherein one of the first gradient and the second gradient is a positive gradient and the other is a negative gradient.