Foreign substance removal method, foreign substance removal device, and method for manufacturing article
The described method uses a curable composition to adhere, cure, and separate foreign matter from substrates, addressing the risks of damage and incomplete removal in imprint technology, ensuring efficient and precise pattern formation.
Patent Information
- Application Number
- JP2024143986
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-12
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-13
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing foreign matter removal methods in imprint technology risk damaging the mold and substrate due to the crushing of foreign objects and incomplete removal of foreign matter with adhesive methods.
A method involving a curable composition that is supplied, contacted with the substrate, cured, and then separated with the mold to remove foreign matter, utilizing a layer that enhances adhesion to ensure complete removal without substrate or mold damage.
Effectively removes foreign matter from substrates without damaging the mold or substrate, ensuring precise pattern formation and preventing defects in imprint processes.
Smart Images

Figure 2024160394000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a foreign matter removal method, a foreign matter removal device, and a method for manufacturing an article. [Background technology]
[0002] As the demand for miniaturization of semiconductor devices and MEMS increases, imprinting technology, which can form fine patterns (structures) on the order of a few nanometers on a substrate, is attracting attention in addition to conventional photolithography technology. Imprinting technology is a microfabrication technology in which an uncured imprinting material is supplied (applied) onto a substrate, and the imprinting material is brought into contact with a mold to form a pattern of the imprinting material on the substrate that corresponds to the fine uneven pattern formed on the mold.
[0003] In imprint technology, a photo-curing method is one of the methods for curing an imprint material. In the photo-curing method, the imprint material is supplied to a shot area on a substrate, and is brought into contact with a mold, and then irradiated with light to cure the imprint material. The mold is then separated from the cured imprint material, forming a pattern of the imprint material on the substrate.
[0004] In such imprinting techniques, if the mold and the imprinting material on the substrate are brought into contact with each other while foreign matter is adhering to the substrate, not only will it be impossible to form a structure of the desired shape, but the mold and the substrate may even be damaged. Therefore, it is necessary to remove any foreign matter adhering to the substrate before carrying out the imprinting process.
[0005] Patent Document 1 describes a method in which, before a pattern is formed on a wafer, the position of a foreign object on the wafer is identified, the foreign object is crushed, and then a mold for removing foreign objects with an adhesive film attached thereto is brought into contact with the crushed foreign object to remove the foreign object. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP2012-243805A Summary of the Invention [Problem to be solved by the invention]
[0007] However, in the foreign matter removal method described in Patent Document 1, there is a possibility that components such as the pattern and the underlayer may be damaged when crushing the foreign matter. In addition, when removing the foreign matter using an adhesive, there is a concern that it may not be possible to remove all of the foreign matter.
[0008] The present invention has been made in view of the above-mentioned problems, and has an object to provide a configuration capable of removing foreign matter on a substrate. [Means for solving the problem]
[0009] In order to achieve the above object, the present invention provides a foreign matter removal method for removing foreign matter on a substrate, the method comprising: a supplying step of supplying a curable composition onto the substrate; a contacting step of bringing a member into contact with the curable composition on the substrate; a curing step of curing the curable composition in a state where the curable composition is in contact with the member; and a removal step of removing the curable composition containing the foreign matter and the foreign matter from the substrate by separating the member from the substrate, wherein a foreign matter processing step including the supplying step, the contacting step, the curing step, and the removing step are performed multiple times using the same member so that the cured curable composition is laminated on the member, and in the contacting step, the curable composition and the member come into contact with each other via a layer that improves adhesion between the curable composition and the member, and in the removing step, the member is separated from the substrate while the curable composition containing the foreign matter is in close contact with the member, thereby removing the foreign matter from the substrate. Effect of the Invention
[0010] According to the present invention, it is possible to provide a configuration that is advantageous for removing foreign matter on a substrate. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a schematic diagram illustrating a configuration of an imprint apparatus. [Diagram 2] 11 is a flowchart illustrating a flow of a foreign matter removal process. [Diagram 3] 3 is a flowchart illustrating the imprint process of FIG. 2. [Figure 4] 5A to 5C are diagrams illustrating a flow of a foreign matter removal process according to the first embodiment. [Diagram 5] 11A and 11B are diagrams illustrating examples of failures in the foreign matter removal process. [Figure 6] 13 is a diagram showing an example of an arrangement of droplets ejected during a foreign matter removal process. [Figure 7] 13A and 13B are diagrams showing the positional relationship between droplets discharged during a foreign matter removal process and a mesa end portion. [Figure 8] FIG. 11 is an explanatory diagram according to a second embodiment. [Figure 9] FIG. 11 is an explanatory diagram according to a third embodiment. [Figure 10] 1A to 1C are diagrams for explaining a method for manufacturing an article. [Figure 11] FIG. 13 is an explanatory diagram relating to a fourth embodiment. [Figure 12] FIG. 13 is an explanatory diagram relating to a fourth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, preferred embodiments of the present invention will be described with reference to the accompanying drawings. In each drawing, the same reference numerals are used to refer to the same components, and duplicated explanations will be omitted.
[0013] (First embodiment) The imprinting apparatus is an apparatus that brings a curable composition (imprinting material) supplied onto a substrate into contact with a mold, and applies energy for curing to the curable composition to form a pattern of a cured product to which a concave-convex pattern of the mold is transferred. For example, the imprinting apparatus supplies a curable composition onto a substrate, and hardens the curable composition while the mold on which the concave-convex pattern is formed is brought into contact with the curable composition on the substrate. Then, the mold pattern can be transferred to the curable composition on the substrate by widening the gap between the mold and the substrate and peeling (demolding) the mold from the cured curable composition. Such a series of processes is called an imprinting process, and is performed for each of a plurality of shot regions on a substrate. In other words, when performing an imprinting process on each of a plurality of shot regions on a substrate, the imprinting process is repeated as many times as the number of shot regions on the substrate.
[0014] FIG. 1 is a diagram showing the configuration of an imprinting apparatus 1. The configuration of the imprinting apparatus 1 will be described with reference to FIG. 1. Here, the surface on which a substrate 10 is placed is defined as the XY plane, and the direction perpendicular thereto is defined as the Z direction, and the respective axes are determined as shown in FIG. 1. The imprinting apparatus 1 is an apparatus that brings a curable composition supplied onto a substrate into contact with a mold 8 and applies energy for curing to the curable composition, thereby forming a pattern of a cured product in which the concave-convex pattern of the mold is transferred. The mold 8 may also be called a mold, template, or original plate. The imprinting apparatus 1 in FIG. 1 is used for manufacturing devices such as semiconductor devices as articles. Here, the imprinting apparatus 1 employing a photocuring method will be described.
[0015] The imprint apparatus 1 includes a mold holding section 3 (also referred to as an imprint head or member holding section) that holds and moves a mold 8, a substrate holding section 4 (stage) that holds and moves a substrate 10, and a discharge mechanism 5 (curable composition supply section) that places the curable composition on the substrate. The imprint apparatus 1 also includes a light irradiation system 2 (curing section) that irradiates light 9 to cure the curable composition, an imaging section 6 that irradiates light 35 and images the contact state between the mold and the curable composition, and a control section 7 that controls the operation of the imprint apparatus 1. The imprint apparatus 1 also includes a detector 12 that detects marks formed on the mold and the substrate.
[0016] The substrate holding unit 4 includes a substrate chuck 16 that holds the substrate 10, and a substrate driving mechanism 17 that controls the position of the substrate 10 with respect to at least two axes, the X-axis direction and the Y-axis direction, in the XYZ coordinate system. The substrate holding unit 4 also includes a plurality of reference mirrors 18 on its side corresponding to the X, Y, Z, ωx, ωy, and ωz directions. In contrast, the imprint apparatus 1 includes a plurality of laser interferometers 19 (length measuring devices) that measure the position of the substrate holding unit 4 by irradiating beams onto each of these reference mirrors 18. The laser interferometer 19 measures the position of the substrate holding unit 4, and the control unit 7 executes positioning control of the substrate 10 (substrate holding unit 4) based on the measured value at this time. The imprint apparatus 1 may measure the position of the substrate holding unit 4 using an encoder instead of the reference mirror 18 and the laser interferometer 19.
[0017] The mold holding part 3 is moved in the vertical direction (Z-axis direction) by a mold driving mechanism 38 (actuator) provided on the mold holding part while holding the mold 8 by the mold chuck 11. The mold holding part 3 is moved downward (-Z direction) by the mold driving mechanism 38, so that the pattern area 8a of the mold 8 comes into contact with (imprints) the curable composition 14. The pattern area 8a of the mold 8 used in the imprinting device 1 is formed with a reverse pattern of the concave-convex pattern to be formed on the substrate. In the following description, the mesa part of the mold is the pattern area 8a, but it may be a flat part where no pattern is formed. After the curable composition is cured, the mold holding part 3 is moved upward (+Z direction) by the mold driving mechanism 38, so that the pattern area 8a of the mold 8 is separated from the cured curable composition (mold release). For imprinting and mold release, the substrate holding part 4 may move in the Z-axis direction instead of the mold holding part 3, or the mold holding part 3 and the substrate holding part 4 may move relatively.
[0018] Furthermore, the mold holding part 3 may be provided with a space 13 separated by a light transmitting member 41 (e.g., a quartz plate) and the mold 8, and the mold 8 can be deformed during imprinting or demolding by adjusting the pressure in the space 13. For example, by increasing the pressure in the space 13 during imprinting, the mold 8 can be deformed into a convex shape relative to the substrate 10, and the pattern region 8a can be brought into contact with the curable composition 14.
[0019] The detector 12 can detect the mark formed on the mold 8 and the mark formed on the substrate 10. The imprint apparatus 1 can determine the relative positions of the mold 8 and the substrate 10 based on the detection results of the detector 12, and can align the mold 8 and the substrate 10 by moving at least one of the mold 8 and the substrate 10.
[0020] The imaging unit 6 is configured (arranged) so as to include in its field of view the pattern region 8a of the mold 8 held by the mold holding unit 3, and captures an image of at least one of the mold 8 and the substrate 10. The imaging unit 6 is a camera (spread camera) capable of observing the contact state between the mold 8 and the curable composition on the substrate 10, and of confirming the state on the substrate 10.
[0021] The control unit 7 includes a CPU, a memory, etc., and controls the operation of each mechanism of the imprint apparatus 1 to form patterns in multiple shot areas formed on the substrate 10. The control unit 7 can also be configured to control the mold holding unit 3, the substrate holding unit 4, the discharge mechanism 5, the light irradiation system 2 (curing unit), the imaging unit 6, and the detector 12. The control unit 7 may be provided within the imprint apparatus 1, or may be provided in a location separate from the imprint apparatus 1 and controlled remotely.
[0022] The curable composition is a curable composition (sometimes called an uncured resin) that is cured by applying energy for curing. As the energy for curing, electromagnetic waves or the like are used. As the electromagnetic waves, for example, infrared rays, visible rays, ultraviolet rays, or other light having a wavelength selected from the range of 10 nm or more and 1 mm or less are used.
[0023] The curable composition is a composition that is cured by irradiation with light or by heating. Among them, the photocurable composition that is cured by light contains at least a polymerizable compound and a photopolymerization initiator, and may contain a non-polymerizable compound or a solvent as necessary. The non-polymerizable compound is at least one selected from the group consisting of a sensitizer, a hydrogen donor, an internal mold release agent, a surfactant, an antioxidant, a polymer component, and the like.
[0024] The curable composition is applied onto the substrate in the form of droplets, or in the form of islands or a film formed by a plurality of droplets connected together, by an inkjet liquid ejection head or the like of the ejection mechanism 5. The viscosity of the curable composition (viscosity at 25° C.) is, for example, 1 mPa s or more and 100 mPa s or less.
[0025] The substrate may be made of glass, ceramics, metal, semiconductor, resin, etc., and may have a member made of a material different from that of the substrate formed on its surface as required. Specific examples of the substrate include silicon wafers, compound semiconductor wafers, and quartz glass.
[0026] In such an imprint apparatus 1, if a foreign object is present on the substrate during the imprint process, the pattern structure provided in the pattern area 8a of the mold may be destroyed. Therefore, it is necessary to remove the foreign object from the substrate before the imprint process is performed by the imprint apparatus 1.
[0027] A method for removing foreign matter on a substrate will be described below with reference to Figures 2 and 3. Note that in the following description, a foreign matter removal process performed in the imprint apparatus 1 shown in Figure 1 will be described, but the process may be performed in a foreign matter removal apparatus separate from the imprint apparatus 1 before an imprint process for forming a pattern.
[0028] After a pattern is formed on a substrate in a semiconductor process, foreign matter 53 may adhere to the surface of the substrate 10. It is known that as patterns become finer and have higher aspect ratios, it becomes difficult to remove these foreign matters by conventional wet cleaning methods, and the foreign matter removal method described below in which the foreign matters are removed by encapsulating them in a curable composition is effective.
[0029] 2 and 3 are flowcharts explaining a method for foreign matter removal processing. Each step in this flowchart is executed by a control unit that comprehensively controls each mechanism of the imprint apparatus (foreign matter removal apparatus). In the imprint apparatus 1 of FIG. 1, each part is controlled by the control unit 7 to execute the steps.
[0030] In S201, the substrate 10 is received from an external transport means or the like and held by the substrate holder 4. Then, in S201, the surface of the substrate 10 that has been brought in is inspected for the presence of foreign matter. If foreign matter is present, the number of foreign matter particles and the coordinate position and size (size in the XY direction and height in the Z direction) of each foreign matter are acquired. Any method can be used to detect foreign matter as long as the measurement method can determine the size, height, and coordinate on the substrate of the foreign matter, and for example, a measurement method using scattered laser light as shown in FIG. 4(a) can be used. FIG. 4(e) is a view of a foreign matter 53 on the shot region 10b (imprint region) of the substrate in FIG. 4(a) as viewed from above the substrate.
[0031] When the light irradiation unit 60 irradiates the substrate 10 with a laser beam 62, the laser beam 62 is reflected by the substrate surface and enters the photodetector 61. If there is a foreign object 53 on the substrate, the reflection state of the laser changes, and the amount of light detected by the photodetector 61 fluctuates. From this fluctuation, the position (coordinate position) and size of the foreign object can be measured. Also, by scattering microparticles of known size on the substrate in advance, for example, silica particles of different sizes, on the substrate and measuring them with a laser, the correlation between the reflection intensity of light and the size of the silica particles can be obtained. By drawing a calibration curve from this correlation, the size of the foreign object can be known. Since the reflected light depends on the surface state of the substrate, it is necessary to know the surface state of the substrate to be measured in advance. The coordinates of the foreign object on the substrate can be known from the position where the reflection state changes. By such a measurement method, the coordinates and size of the foreign object on the substrate can be known. In addition to the measurement method using scattered laser light, the imaging unit 6 may be used as an acquisition unit to acquire the coordinate position and size. Furthermore, instead of performing the inspection within the imprint apparatus 1, the inspection results may be obtained from an external inspection device.
[0032] Thereafter, the processes of S203 to S208 are repeated the same number of times as the number of foreign objects found in the foreign object inspection of S202.
[0033] In S203, it is determined whether or not to remove foreign matter. For example, if the size of the foreign matter does not affect the imprinting process, it may be determined not to remove the foreign matter. Since foreign matter larger than the film thickness of the curable composition supplied in the imprinting process is not embedded in the curable composition and is likely to damage the mold, it is preferable to determine that the foreign matter is removed. In addition, if the size of the foreign matter is too large to be removed, an error may be generated and the process may be terminated so that the subsequent imprinting process itself is not performed. Note that even if the foreign matter removal determination process such as S203 is not performed, the foreign matter may be counted during the foreign matter inspection in S202 and separated by size without being counted.
[0034] In S204, the application position (droplet drop position) and application amount (drop amount) of the curable composition to be applied to the substrate for removing foreign matter are determined. Specifically, the droplets are determined to be in an amount that can sufficiently enclose the foreign matter, which is determined based on the size of the foreign matter inspected and obtained in S202, and does not protrude from the edge of the mold 8 (member) for removing foreign matter, so that the droplets do not protrude from the edge of the mold 8.
[0035] In S205, the curable composition for removing foreign matter is discharged by the discharge mechanism 5 onto the substrate in the position and amount determined in S204, and the curable composition is applied onto the substrate. As a result, droplets of the curable composition 14 are disposed by the discharge mechanism 5 as shown in Fig. 4(b). Fig. 4(f) is a view of the shot region 10b of the substrate in Fig. 4(b) viewed from above the substrate.
[0036] Various patterns can be used for arranging the droplets of the curable composition 14. For example, a square pattern 71 in which the droplets are arranged at a certain pitch in a square lattice pattern as shown in Fig. 6(a), a diamond pattern 72 in which the droplets are arranged at a certain pitch in a triangular pattern as shown in Fig. 6(b), and a random pattern in which the droplets are arranged so as to be uniform over a predetermined area as shown in Fig. 6(c) can be used. As long as the desired thickness of the curable composition is obtained, the arrangement pattern is not limited and any one can be selected. Moreover, a plurality of types of patterns may be combined.
[0037] In S206, the mold 8 is brought into contact with the multiple droplets applied on the substrate to imprint the mold. The contact conditions, such as the pressure and height of the mold 8 when it is brought into contact, are preferably determined based on the information, such as the size of the foreign matter, acquired in S202. The mold 8 used for removing foreign matter is preferably provided with an adhesion layer 20 on its surface to improve adhesion with the curable composition 14, unlike the mold used in the imprint process. If the adhesion between the mold 8 and the curable composition after curing is greater than the adhesion between the substrate and the cured curable composition, it is acceptable to only perform a surface treatment to improve adhesion without providing the adhesion layer 20. For example, in order to improve adhesion, fine irregularities (surface treatment layer) may be provided on the surface of the mold 8 to improve adhesion, thereby improving adhesion with the curable composition by the anchor effect. In addition, since the mold 8 is used for removing foreign matter, the surface of the mold 8 is preferably a flat surface without a pattern structure.
[0038] The method of providing the adhesion layer 20 on the surface of the mold 8 may be by coating with a coating device outside the imprinting device or by coating within the device, and the coating means is not particularly limited. For example, the coating may be by a spin coating method or a dip method. In the case of the spin coating method, the curable composition can be uniformly coated over the entire substrate using a general spin coating device.
[0039] After application, a baking treatment may be performed to harden the adhesive material. The adhesive material is made of a material having a carboxyl group that bonds with the mold and an acrylic group that reacts with the curable composition, and has the function of adhering the mold and the curable composition to each other.
[0040] The droplet is brought into contact with the mold 8 to imprint, and after waiting for a sufficient time until the curable composition fills the contact area of the mold, the process proceeds to S207, where light 9 for curing the curable composition is irradiated from the light irradiation system 2 to the curable composition 14 on the substrate through the mold 8 and the adhesive layer 20 to cure the composition. At this time, it is preferable that the curing conditions such as the amount of irradiation light are set according to the application amount (film thickness) of the curable composition determined in S204. Generally, the wavelength of the light 9 can be mainly in the ultraviolet region. FIG. 4(c) is a diagram showing a state in which the mold 8 provided with the adhesive layer 20 is brought into contact with the curable composition 14 that encases the foreign matter 53, and the curing light 9 is irradiated.
[0041] In S208, the mold 8 is separated from the cured curable composition on the substrate. At this time, by using the mold 8 provided with the adhesive layer 20 having high adhesiveness to the curable composition 14, the curable composition that has encapsulated and fixed the foreign matter adheres to the mold 8 side, not to the substrate, and is separated. FIG. 4(d) shows the state in which the mold 8 has been separated from the cured curable composition.
[0042] After the curable composition enveloping the foreign matter 53 is separated from the substrate 10, the mold 8 must have the curable composition removed. For example, a method using ozone ashing or a method using a mixed solution of sulfuric acid and hydrogen peroxide solution to remove the curable composition can be used. The mold 8 may be removed from the imprinting apparatus and washed with a washing device, or may be washed inside the apparatus. However, it is not essential to remove the curable composition from the mold 8 after each foreign matter removal process, and the foreign matter removal process may be repeated several times and then the curable composition may be removed all at once. In this case, if an adhesive is applied to the surface of the curable composition attached to the mold 8 to provide an adhesive layer 20, the mold 8 can be used in the next foreign matter removal process. In this case, the mold 8 that has been repeatedly used in the foreign matter removal process without being washed will have a state in which the cured curable composition and the adhesive layer are alternately laminated.
[0043] Instead of providing the adhesion layer 20 on the surface of the mold 8, the adhesion layer 20 may be applied to the surface of the curable composition supplied onto the substrate 10. That is, the mold 8 may come into contact with the curable composition on the substrate via an adhesion layer (surface treatment layer) that improves adhesion to the curable composition. After the separation process in S208, the process returns to S203, and the process is repeated for the number of foreign matter detected in the foreign matter inspection process. If the foreign matter removal process has been performed on all foreign matter, the foreign matter processing process ends, and the process proceeds to the imprint process in S209 (details will be described later with reference to FIG. 3). After the imprint process ends, the substrate is removed from the imprint apparatus 1, and the series of processes ends.
[0044] Next, an example in which the application amount of the curable composition determined in S204 is not optimal will be shown with reference to Fig. 5. Fig. 5(a) shows a time series of a case in which the application amount of the curable composition is too small for the foreign matter and the foreign matter is not sufficiently enclosed, and Fig. 5(b) shows a time series of a case in which the application amount of the curable composition is too large for the foreign matter and the foreign matter overflows from the mold 8.
[0045] In the example of Fig. 5(a), when the mold 8 is brought into contact with the curable composition 14, a gap is formed between the mold 8 and the curable composition 14, as shown in Fig. 5(a-1). If such a gap is formed, when the mold is released as shown in Fig. 5(a-2), the adhesion layer 20 of the mold 8 and the part 14-2 of the curable composition are not sufficiently adhered to each other, and the part 14-2 of the curable composition cannot be separated from the substrate, and may remain on the substrate.
[0046] On the other hand, if the amount of curable composition is too large to fully enclose the foreign matter in FIG. 5(b), the curable composition may overflow from the edge of the mold 8 when the mold is imprinted, as shown in FIG. 5(b-3). The curable composition 14b that overflows from the mold is not sufficiently irradiated with the curing light 9 that cures the curable composition, and is not cured sufficiently. If the curing is insufficient, it will be torn off and remain on the substrate when the mold 8 is separated from the substrate 10. If the curable composition for removing foreign matter remains on the substrate, it will become a foreign matter, and there is a concern that it will cause pattern defects during the imprint process.
[0047] Therefore, the optimal application amount is an amount that sufficiently envelops the foreign matter, and it is necessary that the thickness of the curable composition is sufficient for the size (height) of the foreign matter. That is, in S204, it is necessary to calculate the amount of the curable composition based on the size (height) of the foreign matter obtained in S202. For example, consider a case where the size (height) of a foreign matter is about 50 nm. If the size of the mold 8 is 26 mm x 33 mm and the amount of the curable composition dropped is 1.0 pL per particle, in order to fill the foreign matter, in the case of an arrangement pattern in which the curable composition is arranged in a square with a pitch of 30 μm, about 43,000 particles must be arranged on the entire surface.
[0048] Furthermore, by disposing a droplet of the curable composition so that the position of the foreign matter is near the center of the mold 8 when imprinting and imprinting at that position, it is possible to make it difficult for the curable composition to spill out from the edge of the mold 8. Also, the arrangement interval of the curable composition in the peripheral part of the mold can be widened to prevent spilling out. Widening the arrangement interval means making the interval in the peripheral part of the mold larger than the interval in the central part. The arrangement interval of the curable composition can also be appropriately adjusted by the pressure with which the mold is imprinted, etc.
[0049] Specifically, as shown in FIG. 7(a), the density can be reduced by increasing the interval of the arrangement pitch of the droplets of the curable composition 14 in the shot region 10b located at the end of the mold 8. It is preferable to gradually change the arrangement pitch in the middle of the arrangement area of the curable composition. Also, as shown in FIG. 7(b), the droplets may be arranged so that the amount of the curable composition applied is reduced only in the shot region 10b. Also, as shown in FIG. 7(c), the arrangement pattern of the droplets of the curable composition 14 in the shot region 10b may be changed from a square lattice pattern to a diamond pattern. By considering the arrangement of the droplets in this way, it is also possible to reduce overflow from the end of the mold 8.
[0050] Next, the imprint process in S209 will be described in detail with reference to Fig. 3. When the foreign matter removal step is performed in advance in a foreign matter removal device separate from the imprint apparatus 1, a substrate from which foreign matters have been removed in the foreign matter removal device is prepared, and the substrate is then loaded into the imprint apparatus 1 for the imprint process.
[0051] The mold 8 used in the imprint process has a desired pattern structure and is not provided with an adhesive layer 20 as used in the foreign matter removal process.
[0052] In S301, the control unit 7 controls the discharge mechanism 5 to discharge an amount of droplets suitable for the imprint process, so that the curable composition is applied onto the substrate. In S302, the mold and the curable composition are brought into contact with each other. At this time, it is preferable to press the mold 8 while adjusting the pressure so that the concave-convex pattern structure of the mold 8 is filled with the curable composition.
[0053] In S303, based on the positional deviation between the substrate and the mold detected by the detector 12, at least one of the mold 8 and the substrate 10 is moved to align the mold 8 and the substrate 10.
[0054] In S304, light 9 for curing the curable composition is irradiated from the light irradiation system 2 to the curable composition 14 on the substrate through the mold 8 to cure the composition. The amount of irradiation light is preferably set according to the amount of the curable composition applied in S301. As with the foreign matter removal step, the wavelength of the light 9 can generally be in the ultraviolet region.
[0055] In S305, the mold 8 is released from the cured curable composition on the substrate. At this time, since the mold 8 used does not have an adhesive layer 20 on its surface, the curable composition remains on the substrate and a pattern structure is formed.
[0056] In S306, it is determined whether there are any unprocessed shot areas, and if there are, the process returns to S301 and continues, and if imprint processing has been completed for all shot areas, the imprint processing ends and the process proceeds to S210.
[0057] As described above, the foreign matter can be removed from the substrate surface by separating the curable composition containing the foreign matter so that the curable composition is in close contact with the mold 8 side in the foreign matter removal step performed before the imprinting process. Then, the mold 8 can be prevented from being damaged by the influence of the foreign matter by performing the imprinting process after removing the foreign matter.
[0058] In this embodiment, the mold 8 in the foreign matter removal step has been described as being the same size as the mold 8 used in the imprinting process. However, the mold 8 in the foreign matter removal step may be a member smaller in size than the mold 8 used in the imprinting process, as long as it is subjected to a surface treatment (adhesion layer) that improves adhesion to the curable composition as described above. In this case, a member of an optimal size may be determined based on information such as the size of the foreign matter obtained in S202 (member determination step), and the foreign matter removal process may be performed using the member. The mold 8 used in the foreign matter removal step may be not only rectangular, but also circular or elliptical.
[0059] Furthermore, the curable composition used in the foreign matter removal treatment and the curable composition used in the imprint treatment may be the same type of material, but they do not have to be the same type as long as they are curable compositions that are cured by curing energy, and a curable composition for the foreign matter removal treatment may be used.
[0060] If a curable composition for foreign matter removal treatment can be made, unlike a curable composition for imprint treatment, there is no need to consider the effects of subsequent processes, and therefore any material that does not have a function required for patterning, such as etching resistance, can be freely used. In other words, it becomes possible to use a material that can be easily arranged in an amount according to the size of the foreign matter by changing the viscosity as desired.
[0061] In the present embodiment, the foreign matter removal process is performed for each foreign matter, but if the foreign matters are close to each other, the foreign matter removal process may be performed for multiple foreign matters at once. In this case, it is preferable to perform the foreign matter removal process well by determining the position and amount of the curable composition according to information on the largest foreign matter among the multiple foreign matters to be subjected to the foreign matter removal process at once.
[0062] Second embodiment In the first embodiment, an example has been described in which a foreign matter removal process is performed before an imprint process is performed by the imprint apparatus 1. In the present embodiment, an example will be described in which a foreign matter removal process is performed before a planarization process is performed by a planarization process apparatus that planarizes unevenness on a substrate. In the present embodiment, a description of the same parts as in the first embodiment will be omitted, and the description will focus on the differences.
[0063] The planarization processing device is a device that performs a process of planarizing unevenness generated on a substrate by a process prior to forming a wiring layer or an insulating layer, using a planarization substrate having a flat contact surface. Specifically, a curable composition is applied to the entire surface of a substrate having a plurality of shot regions at once, and a planarization substrate having approximately the same size as the substrate or slightly larger than the substrate is used as a mold and brought into contact with the curable composition to perform planarization. Then, the curable composition is cured while the planarization substrate is in contact with the substrate, and the planarization substrate is then separated from the curable composition on the substrate to form a planarization layer made of the cured curable composition on the substrate. As described above, since the curing process of the curable composition needs to be performed while the planarization substrate is in contact with the substrate, the planarization substrate needs to be made of a material that transmits curing light such as ultraviolet light. Specifically, a mold made of a material such as quartz or glass can be used. FIG. 8(a) is a diagram showing a state in which the mold 8 of the planarization substrate and the substrate 10 are in contact with each other.
[0064] Even in such a planarizing apparatus, if there is a foreign object on the substrate as described in the first embodiment, the planarizing substrate may be damaged and good planarization may not be performed. Therefore, it is preferable to inspect the substrate for foreign objects before performing the planarizing process, and to use the planarizing apparatus as a foreign object removal device to perform the foreign object removal process. As a foreign object removal method, a rectangular mold 8 equivalent to the shot area described in the first embodiment or a mold 8 determined according to the size of the foreign object can be used. In addition, the planarizing substrate used in the planarizing process can be used to perform the foreign object removal process all at once on the entire substrate surface. By performing the foreign object removal using a mold 8 of a planarizing substrate having a size approximately equal to that of the substrate 10 as shown in FIG. 8(a), foreign objects in the entire substrate can be removed at once in a single foreign object removal process. Note that the contact surface of the mold 8 of the planarizing substrate used in the foreign object removal process must also be treated to improve adhesion with the curable composition such as the adhesion layer 20. Note that, in this embodiment, the adhesion layer 20 may also be applied to the surface of the curable composition supplied onto the substrate 10 instead of being provided on the surface of the mold 8. That is, the mold 8 may be brought into contact with the curable composition on the substrate via an adhesive layer (surface treatment layer) that improves adhesion to the curable composition.
[0065] When removing the entire area of the substrate at once, it is preferable to adjust the position and amount of the curable composition according to the largest foreign matter detected by the foreign matter detection. In addition, by using a flattened substrate mold 8 having approximately the same size as the substrate 10, foreign matter attached to the edge near the outer periphery of the substrate can also be removed.
[0066] In addition, the coating process of the curable composition for removing foreign matter (or for planarization) in this embodiment may be performed not only by discharging the composition as droplets from the discharge mechanism 5 as in the first embodiment, but also by applying the curable composition to the entire substrate by a spin coating method or the like. When performing the foreign matter removal process using a planarized substrate, it is necessary to apply the curable composition to the entire substrate with which the planarized substrate comes into contact. This is because if the curable composition is applied only around the foreign matter to remove the foreign matter, the substrate 10 and the mold 8 may come into contact in the region where the curable composition is not applied, causing scratches on the substrate 10 or the mold 8, which may result in defects in the subsequent process.
[0067] In addition, when applying the curable composition to remove foreign matter from the entire surface of the substrate at once, it is necessary to apply the curable composition so that it does not spill out from the outer periphery of the substrate. Figures 8(c-1) and 8(c-2) are examples of the curable composition 14 spilling out from the outer periphery of the substrate 10. If the curable composition 14 is applied to the vicinity of the outer periphery of the substrate 10 as shown in Figure 8(c-1), the curable composition 14 may spill out from the outer periphery of the substrate when the mold 8 is brought into contact with the substrate, as shown in Figure 8(c-2), and may wrap around from the edge of the substrate 10 to the rear surface of the substrate. If the curable composition 14 wraps around the rear surface of the substrate, it will contaminate the chuck portion and the substrate holding portion around the substrate, and the curable composition 14 will adhere to the rear surface of the subsequent substrate. If the curable composition 14 adheres to the rear surface of the substrate, the flatness of the substrate surface when held by the substrate holding portion will deteriorate, and there is a concern that alignment defects such as distortion will occur during pattern formation such as imprint processing.
[0068] Therefore, in order to prevent the wraparound of the curable composition 14, it is necessary to adjust the film thickness to an arbitrary value by adjusting the rotation speed during spin coating or the amount of droplets dropped onto the substrate during inkjet coating. In this case, it is known that changing the viscosity of the curable composition makes it easier to adjust the film thickness.
[0069] In the spin coating method, after applying the imprint material, a method (edge rinse) of removing the curable composition 14 from the outer periphery 81 of the substrate may be performed as shown in FIG. 8(b-1). After performing edge rinse, the substrate is brought into contact with a flattened substrate mold 8 (FIG. 8(b-2)) to perform a foreign matter removal process, thereby preventing the curable composition 14 from spilling out during the foreign matter removal process. The region from the substrate edge where edge rinse is performed is preferably adjusted as appropriate depending on the thickness of the curable composition 14 applied on the substrate 10.
[0070] In addition, in the method of applying the curable composition using the spin coating method, the number of applications is not limited to one, and in some cases, multiple applications may be performed. If the foreign matter detected on the substrate is large and the thickness of the curable composition is insufficient in one spin coating process, the spin coating process can be repeated multiple times to place an amount of the curable composition on the substrate that sufficiently covers the foreign matter.
[0071] Alternatively, the curable composition may be applied in advance to the entire surface of the substrate by spin coating, and then the curable composition 14 may be appropriately added by an inkjet method from the discharge mechanism 5. This makes it possible to locally increase the amount of the curable composition only around the foreign matter, and ensures that the foreign matter is wrapped in the curable composition.
[0072] (Third embodiment) In this embodiment, a method for adjusting the position of the curable composition so that droplets of the curable composition are dropped onto a foreign object when determining the position of the curable composition in S204 of Fig. 2 will be described. The following description will focus on the differences from the first and second embodiments, and will omit a description of the same parts.
[0073] In the method shown in the first embodiment, the position of the foreign object and the arrangement of the droplets of the curable composition do not necessarily coincide with each other, so when the droplets are arranged on the foreign object 53 in the shot region 10b shown in FIG. 9(a), the droplets and the foreign object 53 may be located apart as shown in FIG. 9(b). If the droplets of the curable composition 14 and the foreign object 53 are separated in this way, there is a concern that the curable composition 14 may be pushed out in an unintended direction when the mold 8 is brought into contact with the foreign object 53, and the foreign object 53 may not be well wrapped around. For example, if the foreign object has an irregular shape, it is considered that the curable composition 14 coming from the periphery may not be able to go around the foreign object well, and a gap may be generated between the foreign object and the curable composition 14. In a state where such a gap is generated, the foreign object cannot be sufficiently fixed by the curable composition, and the foreign object cannot be separated together with the mold 8 when it is separated from the substrate, and the foreign object may remain on the substrate.
[0074] 9(d), by performing a coating process in which droplets of the curable composition are dropped directly onto the foreign object 53, the foreign object can be completely surrounded by the curable composition, and the foreign object can be sufficiently fixed inside the curable composition by curing. In this state, the mold 8 can be separated from the substrate to remove the foreign object from the substrate.
[0075] Specifically, an arrangement pattern is determined in S204 so that droplets are arranged at the coordinate positions of the foreign objects acquired in S202 in Fig. 2, and droplets of the curable composition are arranged at those positions in S205. At this time, the arrangement positions may be adjusted so that the coordinates of some droplets 14c in the arrangement pattern are shifted as shown in Fig. 9(c), or droplets 14d for foreign objects may be added to the arrangement pattern as shown in Fig. 9(d). When droplets 14d for foreign objects are added, it is necessary to add them while taking into consideration that the curable composition does not protrude from the mold 8 when the mold 8 is brought into contact with the foreign object.
[0076] (Fourth embodiment) In this embodiment, a foreign matter removal method different from the foreign matter removal methods described in the first to third embodiments will be described. In this embodiment, the description of the same parts as in the other embodiments will be omitted, and the description will focus on the different parts. In the first to third embodiments, an example was given in which a curable composition was supplied in accordance with information such as the size of a foreign matter, but in this embodiment, an example will be described in which it is not necessary to obtain the size of a foreign matter in advance.
[0077] When removing foreign matter, the presence or absence of foreign matter on the substrate may be inspected as in the first and second embodiments to obtain information on the foreign matter on the substrate, but obtaining the foreign matter information may be omitted in order to improve throughput. In that case, regardless of whether the foreign matter 53 is attached to the substrate 10, it is preferable to apply a curable composition to all substrates in an amount (thickness) that is assumed to be capable of removing most of the foreign matter that may be attached to the substrate, and perform the foreign matter removal process. In that case, it is preferable to perform the foreign matter removal process all over the substrate at once using a planarizing member for a planarized substrate, and in the following embodiment, an example in which a planarizing device is used as a foreign matter removal device will be described. The substrate 10 from which foreign matter is to be removed may be a substrate for imprint processing for forming a concave-convex pattern as in the first embodiment, or a substrate used for planarization processing as in the second embodiment.
[0078] The foreign matter removal method according to this embodiment will be described with reference to FIG. 11. For a substrate 10 to which a foreign matter 53 shown in FIG. 11(a) may be attached, a curable composition 14-1 is applied to the entire surface of the substrate 10 as shown in FIG. 11(b). The application method can be an inkjet method or a spin coat method in which the composition is discharged as droplets from a discharge mechanism 5. In the case of the inkjet method, a uniform film of the curable composition can be formed by using the spreading of the droplets by increasing the number density per unit area of the droplets. In the case of the spin coat method, the curable composition can be uniformly applied to the entire substrate using a general spin coater. Furthermore, a material that increases the adhesion to the surface of the mold 8 for the planarization substrate is applied on the layer of the applied curable composition 14 using an inkjet method, a spin coat method, or the like, using a discharge mechanism (not shown), to provide an adhesion layer 20.
[0079] Furthermore, as shown in Fig. 11(c), the curable composition 14-1 and the mold 8 are imprinted so as to come into contact with each other via the adhesive layer 20. Then, light 9 for curing the curable composition is irradiated from the light irradiation system 2 to the curable composition 14-1 on the substrate 10 via the mold 8 and the adhesive layer 20 to cure the curable composition 14-1. As a result, the cured layer of the curable composition is cured in a state in which it encases the foreign matter 53. As a result, the cured curable composition 14-1 is well bonded to the mold 8 via the adhesive layer 20.
[0080] Thereafter, when a force is applied in a direction to separate the mold 8 from the substrate 10 as shown in FIG. 11(d), the cured curable composition 14-1 peels off from the surface of the substrate 10, and the foreign matter 53 is removed from the surface of the substrate 10.
[0081] When the removal of the foreign matter from the first substrate is completed, the operation proceeds to the removal of the foreign matter from the second substrate. As shown in FIG. 12(a), another substrate 10 with a foreign matter 53 attached thereto is carried into the device. At this time, the mold 8 has a hardened layer of the hardenable composition 14-1 already formed by the removal of the first foreign matter bonded to its surface. Next, as shown in FIG. 12(b), the hardenable composition 14-2 is applied to the entire surface of the substrate 10 in the same manner as in FIG. 11(b), and then a material that enhances the adhesion to the surface of the mold 8 is applied onto the hardenable composition 14-2 using a discharge mechanism (not shown) to provide an adhesion layer 20.
[0082] Further, as shown in FIG. 12(c), the curable composition 14-2 is pressed so as to come into contact with the mold 8 via the adhesive layer 20. Then, the light 9 for curing the curable composition 14-2 is irradiated from the light irradiation system 2 to the curable composition 14-2 on the substrate 10 via the mold 8 and the adhesive layer 20 to cure the curable composition 14-2. As a result, the cured layer (second layer) of the second sheet of curable composition 14-2 is also cured in a state in which the foreign matter 53 is wrapped around it. The light 9 for curing the second sheet of curable composition 14-2 must have an energy density that reaches the layer of the curable composition 14-2 applied in the second sheet of foreign matter removal treatment. By the above-mentioned curing treatment, the layer of the cured curable composition 14-2 is well bonded to the cured curable composition 14-1 on the surface of the mold 8 via the adhesive layer 20.
[0083] Thereafter, when a force is applied in a direction to separate the mold 8 from the substrate 10 as shown in FIG. 12(d), the cured curable composition 14-2 peels off from the surface of the substrate 10, and the foreign matter 53 is removed from the surface of the substrate 10.
[0084] As described above, the same mold 8 is used for the first and second substrates so that the cured curable composition is laminated without removing the previous cured curable composition, and the foreign matter removal operation of the present invention can be performed continuously without replacing the mold 8. As a result, a layer of the curable composition 14 containing foreign matter is laminated on the mold 8. However, if the layers of the curable composition are repeatedly laminated, the irradiation light for curing the curable composition will not reach the curable composition, so it is necessary to replace the mold 8 at an appropriate timing. As for the frequency of replacement, a method of replacing the mold 8 before the energy for curing does not reach the curable composition, or after a predetermined number of sheets, such as every 10 sheets, can be considered. That is, a control unit or the like that controls the device in an integrated manner can be provided to notify the user to replace the member when the same member has been used in the foreign matter removal process the maximum number of times that the curable composition can be cured.
[0085] After the curable composition encasing the foreign matter 53 has been separated from the substrate 10, the mold 8 must have the curable composition removed. For example, a method using ozone ashing or a method of peeling and removing the composition using a mixed solution of sulfuric acid and hydrogen peroxide can be used. The mold 8 may be taken out of the imprinting apparatus and washed with a washing device, or may be washed within the apparatus. Alternatively, the mold 8 may be disposed of without removing the curable composition.
[0086] As described above, the foreign matter can be removed from the substrate surface by separating the curable composition containing the foreign matter so that the curable composition is in close contact with the mold 8 side. Then, by performing an imprint process or a planarization process after removing the foreign matter, damage to the mold 8 due to the influence of the foreign matter can be prevented. Furthermore, in this embodiment, it is not necessary to clean the mold 8 every time a foreign matter removal operation is performed, so throughput is improved. In addition, the number of molds 8 used can be reduced, which is also advantageous in terms of cost.
[0087] In this embodiment, the adhesive layer 20 is applied to the surface of the curable composition, but as in the first and second embodiments, the adhesive layer 20 may be applied to the surface of the mold 8 that comes into contact with the curable composition 14. That is, in the case of removing the second sheet, the adhesive layer 20 may be applied to the surface of the curable composition 14-1 so that it can come into contact with the curable composition 14-2.
[0088] Furthermore, in the present embodiment, an example in which the adhesive layer 20 is provided has been described, but if the adhesive strength between the mold and the cured composition can be sufficiently ensured by the curing treatment, then the adhesive layer need not be provided.
[0089] (Regarding the manufacture of goods) The substrate manufactured by carrying out various patterning, flattening, and other substrate processing on the substrate from which foreign matter has been removed using the foreign matter removal method described in the first to fourth embodiments is used permanently as at least a part of various articles, or temporarily when manufacturing various articles. The articles include electric circuit elements, optical elements, MEMS, recording elements, sensors, and molds. Examples of the electric circuit elements include volatile or non-volatile semiconductor memories such as DRAM, SRAM, flash memory, and MRAM, and semiconductor elements such as LSI, CCD, image sensors, and FPGA. Examples of the molds include molds for imprinting.
[0090] The pattern of the cured product is used as it is as at least a part of a component of the article, or is used temporarily as a resist mask, which is removed after etching or ion implantation in a substrate processing step.
[0091] Next, a method for manufacturing an article will be described with reference to Fig. 10, in which a pattern is formed on a substrate from which foreign matter has been removed by an imprinting device, the substrate on which the pattern has been formed is processed, and an article is manufactured from the processed substrate. First, as shown in Fig. 10(a), a substrate 1z such as a silicon wafer having a workpiece 2z such as an insulator formed on its surface is prepared, and then an imprinting material 3z is applied to the surface of the workpiece 2z by an inkjet method or the like. Here, a state in which the imprinting material 3z in the form of multiple droplets has been applied onto the substrate is shown.
[0092] As shown in Fig. 10(b), the imprinting mold 4z is placed so that the side on which the concave-convex pattern is formed faces the imprinting material 3z on the substrate. As shown in Fig. 10(c), the substrate 1z to which the imprinting material 3z has been applied is brought into contact with the mold 4z, and pressure is applied. The imprinting material 3z fills the gap between the mold 4z and the workpiece 2z. When light is irradiated through the mold 4z in this state as energy for hardening, the imprinting material 3z hardens.
[0093] 10(d), after the imprint material 3z is cured, the mold 4z and the substrate 1z are separated, and a pattern of the cured product of the imprint material 3z is formed on the substrate 1z. In this cured product pattern, the recesses of the mold correspond to the protrusions of the cured product, and the protrusions of the mold correspond to the recesses of the cured product, i.e., the recessed and protruding pattern of the mold 4z is transferred to the imprint material 3z.
[0094] As shown in Fig. 10(e), when etching is performed using the pattern of the cured material as an etching-resistant mask, the portion of the surface of the workpiece 2z where there is no cured material or where only a thin layer remains is removed, forming a groove 5z. As shown in Fig. 10(f), when the pattern of the cured material is removed, an article having grooves 5z formed on the surface of the workpiece 2z can be obtained. Here, the pattern of the cured material is removed, but it may be used as an interlayer insulating film included in a semiconductor element or the like, that is, a component of an article, without being removed after processing.
[0095] The method for manufacturing an article also includes a step of forming a pattern on an imprint material supplied (applied) to a substrate using the above-mentioned imprint apparatus (imprint method), and a step of processing the substrate on which the pattern has been formed in the above step. Furthermore, the manufacturing method includes other well-known steps (oxidation, film formation, deposition, doping, planarization, etching, resist stripping, dicing, bonding, packaging, etc.). It can be said that the method for manufacturing an article of this embodiment is more advantageous than conventional methods in at least one of the performance, quality, productivity, and production cost of the article.
[0096] Although the preferred embodiments of the present invention have been described above, it goes without saying that the present invention is not limited to these embodiments, and various modifications and changes are possible within the scope of the gist of the present invention. [Explanation of symbols]
[0097] 1 Imprinting device 5 Supply section 7 Control section Type 8 9 Hardened part 10 Substrate 14 Curable composition 53 Foreign matter
Claims
1. A method for removing foreign matter on a substrate, comprising the steps of: a step of providing a curable composition on the substrate; a contacting step of contacting a member with the curable composition on the substrate; a curing step of curing the curable composition in a state where the curable composition is in contact with the member; a removing step of removing the curable composition including the foreign matter from the substrate by separating the member from the substrate; having A foreign matter removal method, characterized in that in the removal step, the foreign matter is removed from the substrate by separating the member from the substrate while the curable composition containing the foreign matter adheres to the member.
2. 2. The method for removing foreign matter according to claim 1, wherein a contact portion of the member that comes into contact with the curable composition in the contacting step is a flat surface on which no pattern is formed.
3. The method for removing foreign matter according to claim 1, characterized in that a layer is formed on at least one of the member and the curable composition, which improves adhesion between the curable composition and the member in the contacting step.
4. acquiring a position and a size of a foreign object on the substrate; and determining an amount of the curable composition to be supplied onto the substrate based on the information acquired in the acquiring step, 2. The method for removing foreign matter according to claim 1, wherein the supplying step supplies the curable composition onto the substrate in the amount determined in the determining step.
5. 4. The foreign matter removal method according to claim 3, wherein the layer is a surface treatment layer formed by performing a surface treatment on the member.
6. 4. The method for removing foreign matter according to claim 3, wherein the layer is an adhesive layer provided on the member.
7. The method for removing foreign matter according to claim 3 , wherein the layer is an adhesion layer provided on the curable composition.
8. 5. The foreign matter removal method according to claim 4, further comprising a member determining step of determining the member to be used in the contacting step based on the information acquired in the acquiring step.
9. 5. The method for removing foreign matter according to claim 4, wherein a curing condition for the curable composition in the curing step is determined according to an amount of the curable composition.
10. 5. The method for removing foreign matter according to claim 4, wherein the supplying step is performed by depositing a plurality of droplets of the curable composition on the substrate.
11. 11. The method for removing foreign matter according to claim 10, wherein in the supplying step, the curable composition is supplied onto the substrate based on an arrangement of the plurality of droplets that is determined according to a position of the foreign matter.
12. 5. The method for removing foreign matter according to claim 4, wherein the contact step determines contact conditions for the members based on the information acquired in the acquisition step, and causes the members to come into contact with each other.
13. The foreign matter removal method according to claim 1, characterized in that the foreign matter treatment process, including the supplying process, the contacting process, the curing process, and the removing process, is performed multiple times using the same member, thereby causing the cured curable composition to be laminated on the member.
14. The method further includes a cleaning step of cleaning the cured curable composition laminated on the member.
2. The method for removing foreign matter according to claim 1.
15. A step of preparing a substrate from which foreign matter has been removed by the foreign matter removal method according to any one of claims 1 to 14; a substrate processing step of performing an imprint process or a planarization process on the prepared substrate; and processing the substrate processed in the substrate processing step, A method for manufacturing an article, comprising the steps of: manufacturing an article from the processed substrate;
16. A foreign matter removal apparatus for removing foreign matter on a substrate, comprising: A substrate holder for holding a substrate; A member holding portion for holding a member; a curing section for curing the curable composition; a drive unit capable of changing a relative position between the substrate holding unit and the member holding unit; A control unit that controls the curing unit and the drive unit, The control unit is controlling the driving unit to perform a contact operation of bringing the member into contact with the curable composition supplied onto the substrate; controlling the curing unit to perform a curing operation in which the curable composition is cured in a state in which the curable composition is in contact with the member; controlling the driving unit to separate the member from the substrate, thereby performing a removing operation to remove the curable composition including the foreign matter from the substrate; A foreign matter removal device characterized in that, in the removal operation, the foreign matter is removed from the substrate by separating the member from the substrate while the curable composition containing the foreign matter adheres to the member.
Citation Information
Patent Citations
Substrate processing apparatus and substrate processing method
JP2016072517A
Imprint method, imprint device, and manufacturing method of material
JP2019021875A
Foreign matter removal method, foreign matter removal device, and manufacturing method of article
JP2023072644A
Pattern formation method
JP2012243805A