Method for manufacturing power storage device

By laminating electrode sheets with non-active material layers and collecting current collector foils at bending points, the method reduces foil distortion, thereby improving the reliability of electricity storage devices.

JP2024160755AActive Publication Date: 2024-11-15PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023076058
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-02
Publication Date
2024-11-15
Estimated Expiration
2043-05-02

AI Technical Summary

Technical Problem

Existing terminal welding methods for electricity storage devices risk distortion of current collector foils due to sliding and applied loads, compromising device reliability.

Method used

A method involving laminating positive and negative electrode sheets with separator sheets, forming non-active material layers that protrude, and collecting the current collector foils by shifting a pressing member to contact bending points, reducing sliding and load on the foils during collection.

Benefits of technology

This approach minimizes foil distortion, enhancing the reliability of the electricity storage device by preventing breakage and improving overall device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024160755000001_ABST
    Figure 2024160755000001_ABST
Patent Text Reader

Abstract

To provide a technique for obtaining a power storage device with suitably improved reliability.SOLUTION: A method for manufacturing a power storage device disclosed herein includes a preparation step (S1) of preparing an electrode body, a collection step (S2) of collecting an electrode current collecting foil laminate in at least one of a positive electrode current collecting foil laminate and a negative electrode current collecting foil laminate while sequentially shifting the pressing member so as to abut against the vicinity of the bending point from the end side opposite to the side where the core part of the electrode current collecting foil laminate is located toward the core part side in the width direction, and a joining step (S3) of joining the electrode current collecting foil laminate collected in the collection step to the current collecting terminal on the corresponding pole side.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing an electricity storage device. [Background technology]

[0002] For example, the following Patent Document 1 discloses a terminal welding method for welding a terminal to a laminated portion of the exposed current collecting foil of an electrode body formed by stacking electrodes having a portion in which an active material is carried on the current collecting foil and a portion in which the current collecting foil is exposed and protruding from the portion in which the active material is carried. The terminal welding method describes that when welding the laminated portion and the terminal, the portion in which the active material is carried on the current collecting foil is pressed and restrained, and the active material-carrying portion of the laminated portion is pressed from both sides in the stacking direction by a pressing means, rather than the welded portion of the laminated portion, to collect the current collecting foil of the laminated portion. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5751218 Summary of the Invention [Problem to be solved by the invention]

[0004] However, according to the inventors' investigation, it was found that in the above-mentioned terminal welding method, sliding may occur between the current collecting foil and the pressing means when collecting the current collecting foil, which may cause distortion (load) in the current collecting foil. In other words, it was found that there is still room for improvement in the above-mentioned terminal welding method from the viewpoint of obtaining a highly reliable electricity storage device.

[0005] The present disclosure has been made in consideration of the above circumstances, and a main objective thereof is to provide a technique that can obtain an electricity storage device with suitably improved reliability. [Means for solving the problem]

[0006] In order to achieve this object, the present disclosure provides a method for manufacturing an electricity storage device including an electrode assembly in which a positive electrode sheet and a negative electrode sheet are laminated via a separator sheet, and current collector terminals corresponding to the positive electrode sheet and the negative electrode sheet, which are joined to the electrode assembly. The method for manufacturing such an electricity storage device includes a preparation step of preparing the electrode assembly, in which a core portion where a positive electrode active material layer and a negative electrode active material layer face each other is present in a central portion in a predetermined width direction of the electrode assembly, and a positive electrode current collector foil laminated portion is present in one of both ends in the width direction, in which a positive electrode active material layer non-forming portion where the positive electrode active material layer is not formed protrudes from the negative electrode sheet, and a negative electrode current collector foil laminated portion is present in which a negative electrode active material layer non-forming portion where the negative electrode active material layer is not formed protrudes from the positive electrode sheet, at the other end of both ends. The method for producing such an electricity storage device preferably includes a foil collecting step of collecting the electrode current collecting foil laminated parts of at least one of the positive current collecting foil laminated parts and the negative current collecting foil laminated parts while sequentially shifting a pressing member so as to abut against the vicinity of a bending point of the electrode current collecting foil laminated parts from the end side opposite to the side where the core part is present in the width direction toward the core part side. The method for producing such an electricity storage device preferably includes a joining step of joining the electrode current collecting foil laminated parts collected in the foil collecting step to the current collecting terminal on the corresponding electrode side. Although details will be described later, the method for producing an electricity storage device having such a configuration can suitably reduce the load on the current collecting foil during foil collection, and therefore it is possible to obtain an electricity storage device with suitably improved reliability. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a front view showing a schematic internal structure of a battery according to an embodiment. [Diagram 2] FIG. 2 is a perspective view showing a schematic diagram of a wound electrode body according to one embodiment. [Diagram 3] 2 is a flowchart showing each step of a battery manufacturing method according to one embodiment. [Figure 4] 11 is a graph for explaining a method for calculating a bending point in a positive electrode current collector foil laminate portion according to one embodiment. [Diagram 5] FIG. 4 is a schematic diagram for explaining a bending point in a positive electrode current collector foil laminate according to one embodiment. [Figure 6] FIG. 2 is a schematic diagram illustrating a positive electrode current collector foil laminate according to one embodiment before foil collection. [Figure 7] FIG. 2 is a schematic diagram illustrating a positive electrode current collector foil laminate according to one embodiment after foil collection. [Figure 8] 4 is a side view showing a schematic diagram of a connection portion between a wound electrode body and a current collecting terminal according to one embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, some embodiments of the technology disclosed herein will be described with reference to the drawings. In the following drawings, the same reference numerals are used to describe members and parts that perform the same function. In addition, the dimensional relationships (length, width, thickness, etc.) in each drawing do not reflect the actual dimensional relationships. In addition, matters other than those specifically mentioned in this specification and necessary for implementing the technology disclosed herein (for example, the general configuration and manufacturing process of an electricity storage device that does not characterize this disclosure) can be understood as design matters of a person skilled in the art based on the conventional technology in the field. The technology disclosed herein can be implemented based on the contents disclosed in this specification and the technical common sense in the field. In addition, the following description is not intended to limit the present disclosure to the following forms. In addition, the manufacturing method of the battery disclosed herein may further include other steps at any stage, and if the steps are not described as essential, they can be appropriately deleted. In addition, the order of the steps can be changed as long as the effect of the technology disclosed herein is exerted.

[0009] In this specification, the expression "A to B" indicating a range means "A or more and B or less". It also includes the meanings of "greater than A" and "less than B". In this specification, the term "electricity storage device" refers to a device that can perform charging and discharging. The electricity storage device includes batteries such as primary batteries and secondary batteries (for example, non-aqueous electrolyte secondary batteries such as lithium ion secondary batteries, nickel-metal hydride batteries), and capacitors (physical batteries) such as electric double layer capacitors. The electrolyte may be any of a liquid electrolyte (electrolytic solution), a gel electrolyte, and a solid electrolyte. Hereinafter, a lithium ion secondary battery (hereinafter simply referred to as "battery 100"), which is one embodiment of the electricity storage device disclosed herein, will be described as an example.

[0010] <Overall battery configuration> First, the configuration of a battery 100 obtained by the manufacturing method of a battery according to this embodiment will be briefly described. Here, Fig. 1 is a front view showing a schematic internal structure of a battery according to one embodiment. Fig. 2 is a perspective view showing a schematic wound electrode body according to one embodiment. As shown in Fig. 1, the battery 100 includes a flat-shaped electrode body 20 (here, a wound electrode body), a non-aqueous electrolyte 80, and a battery case (i.e., an outer container) 30 that contains the electrode body 20 and the non-aqueous electrolyte 80.

[0011] 2, the electrode body 20 has a configuration in which a laminate in which a long positive electrode sheet 50 and a long negative electrode sheet 60 are laminated with two long separator sheets 70 interposed therebetween is wound in the longitudinal direction. The positive electrode sheet 50 has a configuration in which a positive electrode active material layer 54 is formed along the longitudinal direction on one or both sides (both sides here) of a long positive electrode current collector foil 52. The negative electrode sheet 60 has a configuration in which a negative electrode active material layer 64 is formed along the longitudinal direction on one or both sides (both sides here) of a long negative electrode current collector foil 62. The positive electrode active material layer non-forming portion 52a (i.e., a portion where the positive electrode active material layer 54 is not formed and the positive electrode current collector foil 52 is exposed) and the negative electrode active material layer non-forming portion 62a (i.e., a portion where the negative electrode active material layer 64 is not formed and the negative electrode current collector foil 62 is exposed) are formed so as to protrude outward from both ends in the winding axis direction (i.e., the width direction perpendicular to the longitudinal direction) of the electrode body 20. In addition, a core portion 20a where the positive electrode active material layer 54 and the negative electrode active material layer 64 face each other is present in the center in the winding axis direction. A positive electrode current collector terminal 42a and a negative electrode current collector terminal 44a are respectively joined to the positive electrode current collector foil laminated portion 52A in which a plurality of positive electrode active material layer non-forming portions 52a are laminated and the negative electrode current collector foil laminated portion 62A in which a plurality of negative electrode active material layer non-forming portions 62a are laminated. Note that WL in FIG. 2 indicates the winding axis.

[0012] A known positive electrode current collector foil used in lithium ion secondary batteries may be used as the positive electrode current collector foil 52 constituting the positive electrode sheet 50, and examples of such a foil include aluminum foil, aluminum alloy foil, etc. The thickness of the positive electrode current collector foil 52 is not particularly limited and is, for example, 3 μm to 35 μm, and preferably 5 μm to 20 μm.

[0013] The positive electrode active material layer 54 contains a positive electrode active material. As the positive electrode active material, a known positive electrode active material used in a lithium ion secondary battery may be used. Specifically, for example, as the positive electrode active material, a lithium composite oxide, a lithium transition metal phosphate compound, or the like may be used. The crystal structure of the positive electrode active material is not particularly limited, and may be a layered structure, a spinel structure, an olivine structure, or the like. Examples of the lithium composite oxide include a lithium nickel composite oxide, a lithium cobalt composite oxide, a lithium manganese composite oxide, a lithium nickel manganese composite oxide, a lithium nickel cobalt manganese composite oxide, a lithium nickel cobalt aluminum composite oxide, and a lithium iron nickel manganese composite oxide. These positive electrode active materials may be used alone or in combination of two or more. The positive electrode active material is preferably a lithium nickel cobalt manganese composite oxide.

[0014] The average particle diameter (median diameter: D50) of the positive electrode active material is not particularly limited, but is, for example, 0.05 μm to 25 μm, preferably 1 μm to 20 μm, and more preferably 3 μm to 15 μm. The average particle diameter (D50) of the positive electrode active material can be determined, for example, by a laser diffraction scattering method.

[0015] The content of the positive electrode active material in the positive electrode active material layer 54 (i.e., the content of the positive electrode active material relative to the total mass of the positive electrode active material layer 54) is not particularly limited, but is, for example, 80 mass % or more, preferably 85 mass % or more, and more preferably 90 mass % or more.

[0016] The positive electrode active material layer 54 may contain a component (i.e., an optional component) other than the positive electrode active material. Examples of the optional component include a conductive material, a binder, and the like. As the conductive material, for example, a carbon material such as carbon black (e.g., acetylene black), carbon nanotubes (CNT), graphite, and the like may be suitably used. As the binder, for example, polyvinylidene fluoride (PVDF) and the like may be used. When CNT is used as the conductive material, the positive electrode active material layer 54 may further contain a dispersant for CNT.

[0017] The content of the conductive material in the positive electrode active material layer 54 is not particularly limited, but is preferably 0.1% by mass to 15% by mass, and more preferably 0.5% by mass to 13% by mass. The content of the binder in the positive electrode active material layer 54 is not particularly limited, but is preferably 1% by mass to 15% by mass, and more preferably 1.5% by mass to 10% by mass. The thickness of the positive electrode active material layer 54 is not particularly limited, but is, for example, 10 μm to 300 μm, and preferably 20 μm to 200 μm. The positive electrode sheet 50 may contain an insulating layer (not shown) at the boundary between the positive electrode active material layer non-forming portion 52a and the positive electrode active material layer 54. The insulating layer contains, for example, ceramic particles.

[0018] A known negative electrode current collector foil used in lithium ion secondary batteries may be used as the negative electrode current collector foil 62 constituting the negative electrode sheet 60, and an example of such a foil is copper foil. The thickness of the negative electrode current collector foil 62 is not particularly limited and is, for example, 3 μm to 35 μm, and preferably 5 μm to 20 μm.

[0019] The negative electrode active material layer 64 contains a negative electrode active material. As the negative electrode active material, for example, a carbon material such as graphite, hard carbon, soft carbon, etc. The graphite may be natural graphite or artificial graphite, or may be amorphous carbon-coated graphite in which graphite is coated with an amorphous carbon material.

[0020] The average particle diameter (median diameter: D50) of the negative electrode active material is not particularly limited, but is, for example, 0.1 μm to 50 μm, preferably 1 μm to 25 μm, and more preferably 5 μm to 20 μm. The average particle diameter (D50) of the negative electrode active material can be determined, for example, by a laser diffraction scattering method.

[0021] The negative electrode active material layer 64 may contain components other than the active material, such as a binder and a thickener. As the binder, for example, styrene butadiene rubber (SBR), polyvinylidene fluoride (PVDF), etc. may be used. As the thickener, for example, carboxymethyl cellulose (CMC), etc. may be used. The content of the negative electrode active material in the negative electrode active material layer 64 is preferably 90 mass% or more, more preferably 95 mass% to 99 mass%. The content of the binder in the negative electrode active material layer 64 is preferably 0.1 mass% to 8 mass%, more preferably 0.5 mass% to 3 mass%. The content of the thickener in the negative electrode active material layer 64 is preferably 0.3 mass% to 3 mass%, more preferably 0.5 mass% to 2 mass%. The thickness of the negative electrode active material layer 64 is not particularly limited, but is, for example, 10 μm to 300 μm, and preferably 20 μm to 200 μm.

[0022] The separator sheet 70 may be a porous sheet (film) made of a resin such as polyethylene (PE), polypropylene (PP), polyester, cellulose, or polyamide. Such a porous sheet may have a single-layer structure or a laminated structure of two or more layers (for example, a three-layer structure in which a PP layer is laminated on both sides of a PE layer). A heat-resistant layer (HRL) may be provided on the surface of the separator sheet 70. The thickness of the separator sheet 70 is not particularly limited, but is, for example, 5 μm to 50 μm, and preferably 10 μm to 30 μm.

[0023] The nonaqueous electrolyte 80 typically contains a nonaqueous solvent and a supporting salt (electrolyte salt). As the nonaqueous solvent, various organic solvents such as carbonates, ethers, esters, nitriles, sulfones, and lactones that are used in general electrolytes of lithium ion secondary batteries can be used without any particular limitation. Among them, carbonates and esters are preferable, and specific examples thereof include ethylene carbonate (EC), propylene carbonate (PC), diethyl carbonate (DEC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), methyl acetate, and methyl propionate. Such nonaqueous solvents can be used alone or in appropriate combination of two or more.

[0024] As the supporting salt, for example, a lithium salt such as LiPF6, LiBF4, lithium bis(fluorosulfonyl)imide (LiFSI) (preferably LiPF6) can be suitably used. The concentration of the supporting salt is preferably 0.7 mol / L to 1.3 mol / L.

[0025] In addition, the non-aqueous electrolyte 80 may contain various additives other than the above-mentioned components, such as film-forming agents such as vinylene carbonate (VC) and oxalate complexes; gas generating agents such as biphenyl (BP) and cyclohexylbenzene (CHB); thickeners, etc., so long as the effects of the present disclosure are not significantly impaired.

[0026] The battery case 30 has a case body 32 and a lid body 34. The battery case 30 is made of, for example, a metal (e.g., aluminum, stainless steel, nickel-plated steel, etc.). The battery case 30 is preferably made of aluminum because it has good electrical conductivity, thermal conductivity, strength, and is lightweight. The case body 32 has a flattened rectangular parallelepiped shape, and one of its faces (the upper face in the figure) is an opening. The lid body 34 has a substantially rectangular shape that fits the shape of the opening. The lid body 34 is provided with a positive electrode terminal 42 and a negative electrode terminal 44 for external connection, and a thin-walled safety valve 36 that is set to release the internal pressure when the internal pressure of the battery case 30 rises to a predetermined level or higher. The lid body is also provided with an injection hole (not shown) for injecting the non-aqueous electrolyte 80. The positive electrode terminal 42 is electrically connected to the positive electrode current collector terminal 42a. The negative electrode terminal 44 is electrically connected to the negative electrode current collector terminal 44a. The positive electrode terminal 42 and the positive electrode current collector terminal 42a are made of, for example, aluminum, an aluminum alloy, etc. The negative electrode terminal 44 and the negative electrode current collector terminal 44a are made of, for example, copper, a copper alloy, etc.

[0027] <Battery manufacturing method> Next, a method for manufacturing a battery according to this embodiment will be described. Here, Fig. 3 is a flow chart showing each step of the method for manufacturing a battery according to one embodiment. First, the method for manufacturing a battery 100 according to this embodiment is a method for manufacturing a battery including an electrode assembly 20 (here, a wound electrode assembly) in which a positive electrode sheet 50 and a negative electrode sheet 60 are stacked with a separator sheet 70 interposed therebetween, and current collector terminals (here, positive electrode current collector terminal 42a and negative electrode current collector terminal 44a) corresponding to the positive electrode sheet 50 and the negative electrode sheet 60, respectively, joined to the electrode assembly 20. 3, the manufacturing method of the battery 100 according to this embodiment includes a preparation step (step S1) of preparing an electrode body 20, in which a core portion 20a, in which the positive electrode active material layer 54 and the negative electrode active material layer 64 face each other, is present in the center of a predetermined width direction (here, corresponding to the X direction in FIG. 2) of the electrode body 20, and a positive electrode current collector foil laminate portion 52A is present at one of both ends in the width direction, in which a positive electrode active material layer non-forming portion 52a, in which the positive electrode active material layer 54 is not formed, protrudes from the negative electrode sheet 60, and a negative electrode current collector foil laminate portion 62A is present at the other of both ends, in which a negative electrode active material layer non-forming portion 62a, in which the negative electrode active material layer 64 is not formed, protrudes from the positive electrode sheet 50. The manufacturing method for battery 100 according to this embodiment also includes a foil collecting step (step S2) of collecting the electrode current collecting foil laminated parts of at least one of positive current collecting foil laminated part 52A and negative current collecting foil laminated part 62A (here, positive current collecting foil laminated part 52A and negative current collecting foil laminated part 62A) while sequentially shifting pressing member 202 from the end side opposite to the side where core part 20a of the electrode current collecting foil laminated part in the width direction toward core part 20a side so as to abut against the vicinity of bending point P. The manufacturing method for battery 100 according to this embodiment also includes a joining step (step S3) of joining the electrode current collecting foil laminated part collected in the foil collecting step to the corresponding pole side current collecting terminal.

[0028] According to the manufacturing method of the battery having the above-mentioned configuration, in the foil collecting step, the electrode current collecting foil is collected while tracing a trajectory that passes through the point where the electrode current collecting foil bends (i.e., the bending point), so that sliding (in other words, slippage) is unlikely to occur between the electrode current collecting foil and the pressing member. This suitably reduces distortion caused in the electrode current collecting foil, and therefore damage (breakage) of the electrode current collecting foil can be suitably prevented. In other words, according to the manufacturing method of the battery disclosed herein, it is possible to obtain an electricity storage device (e.g., a battery) with suitably improved reliability. Each step will be described in detail below.

[0029] <Preparation process: Step S1> In this step, the electrode body 20 having the above-mentioned configuration is prepared. Specifically, the electrode body 20 (here, a wound electrode body) is prepared according to a known method. For example, a positive electrode sheet 50, a negative electrode sheet 60, and two separator sheets 70 are prepared. Using a known winding machine, the positive electrode sheet 50 and the negative electrode sheet 60 are laminated and wound so that the separator sheet 70 is interposed between them. The obtained wound body is processed into a flat shape by pressing from its side direction, and the electrode body 20 as shown in FIG. 2 is produced.

[0030] <Foil collecting process: Step S2> In this step, in at least one of the electrode current collector foil laminate parts 52A and 62A (here, in the positive current collector foil laminate part 52A and the negative current collector foil laminate part 62A), the electrode current collector foil laminate part is collected while sequentially shifting the pressing member 202 from the end R side opposite to the side where the core part 20a of the electrode current collector foil laminate part exists in the width direction (corresponding to the X direction in FIG. 5) toward the core part 20a side (here, toward the direction of the outline arrow in FIG. 5) so as to abut against the vicinity of the bending point P. It can be said that the bending point P is the point at which each positive electrode active material layer non-forming portion 52a constituting the positive electrode current collector foil laminate part 52A buckles when the pressing member 202 is moved while sequentially shifting from the end side opposite to the side where the core part 20a of the positive current collector foil laminate part 52A exists in the width direction toward the core part 20a side.

[0031] Here, FIG. 4 is a graph for explaining a method for calculating a bending point in a positive current collector foil laminated portion according to an embodiment. FIG. 5 is a schematic diagram for explaining a bending point in a positive current collector foil laminated portion according to an embodiment. FIG. 6 is a schematic diagram showing a positive current collector foil laminated portion according to an embodiment before foil collection. FIG. 7 is a schematic diagram showing a positive current collector foil laminated portion according to an embodiment after foil collection. Note that in FIGS. 4 to 7, the explanation focuses on the positive current collector foil laminated portion 52A of the electrode current collector foil laminated portion, but the negative current collector foil laminated portion 62A can also be collected by a similar method. That is, the positive current collector foil laminated portion and the portion without the positive active material layer in the following explanation can be read as the negative current collector foil laminated portion and the portion without the negative active material layer, respectively. Also, in FIGS. 5 to 7, the negative electrode sheet 60 and the separator sheet 70 are omitted for ease of viewing.

[0032] First, in this step, bending points P are determined in each of the positive electrode active material layer non-forming portions 52a to be collected as shown in FIG. 5. Here, distances l1 to l4 in FIG. 5 indicate the distances from the end S on the core portion 20a side in the width direction of the positive electrode current collector foil laminated portion 52A to the bending points P1 to P4, respectively. Distance s indicates the distance between each of the positive electrode active material layer non-forming portions 52a. Thickness t indicates the thickness of the positive electrode active material layer non-forming portion 52a. As an example of a method for calculating the bending point P, for example, the following method can be mentioned. Specifically, first, the value of the distance l1 is determined. Although not particularly limited, the distance l1 can be set to be within a range of approximately 40 to 80% (for example, within a range of 50 to 70%) when the length Q in the width direction of the positive electrode current collector foil laminated portion 52A (more specifically, the positive electrode active material layer non-forming portion 52a constituting the positive electrode current collector foil laminated portion 52A) is taken as 100%. It is preferable to change the value of the distance l1 appropriately depending on the foil collecting conditions, etc. Next, the following formula: l2 = (l1 2 +s 2 ) 1 / 2 ,l3={l1 2 +(2s+t) 2} 1 / 2 ,l4={l1 2 +(3s+2t) 2} 1 / 2Based on this, distances l2 to l4 are calculated. n =[l1 2 +{(n-1)s+(n―2)t} 2 ] 1 / 2 (where n is an integer of 2 or more). In this way, a graph as shown in FIG. 4 is obtained. Here, the vertical axis of the graph shown in FIG. 4 indicates the number of positive current collector foils 52 (in other words, the positive active material layer non-forming portion 52a), and the horizontal axis indicates the distance from the end S to the bending point P in the width direction X of the positive current collector foil laminated portion 52A. In addition, in this embodiment, since there is no bending point in the central positive active material layer non-forming portion 52a1 of the positive active material layer non-forming portions 52a constituting the positive current collector foil laminated portion 52A, the positive active material layer non-forming portions 52a present above the positive active material layer non-forming portion 52a1 are sequentially designated as the first, second, third, and fourth sheets. And the bending points P in each positive active material layer non-forming portion 52a are sequentially designated as P1, P2, P3, and P4. The bending points P11, P12, P13, and P14 in each of the positive electrode active material layer-free portions 52a1 present below the positive electrode active material layer-free portion 52a1 can be respectively corresponding to P1, P2, P3, and P4. In the manner described above, each bending point P in the positive electrode active material layer-free portion 52a constituting the positive electrode current collector foil laminated portion 52A can be determined. The bending point in the negative electrode current collector foil laminated portion 62A can also be determined by a similar method. However, the method of calculating the bending point P is not limited to the above-mentioned method. The bending point P can also be determined by performing a preliminary test or the like.

[0033] 6, the pressing member 202 is moved from the end R side opposite to the side where the core portion 20a of the positive current collector foil laminated portion 52A exists in the width direction to the core portion 20a side so as to abut against the vicinity of the bending point P determined as described above in the positive current collector foil laminated portion 52A while being shifted in sequence. In this way, the positive current collector foil laminated portion 52A can be collected as shown in FIG. 7. According to this foil collecting step, the positive active material layer non-forming portions 52a are collected while tracing a trajectory that passes through the bending point P, so that sliding is unlikely to occur between the positive active material layer non-forming portions 52a and the pressing member 202. This suitably reduces distortion occurring in the positive active material layer non-forming portions 52a, and therefore suitably prevents damage to the positive active material layer non-forming portions 52a. Note that, when the length Q in the width direction of the positive current collector foil laminate 52A (more specifically, the positive active material layer non-forming portion 52a constituting the positive current collector foil laminate 52A) collected in the foil collecting step is taken as 100%, "near the bending point P" preferably means a range of 5% or less in the front-to-rear direction (i.e., the width direction) of the bending point P, more preferably 3% or less, 1% or less, and particularly preferably 0% (i.e., on the bending point P). Note that the same applies to the negative current collector foil laminate 62A.

[0034] Next, the foil pressing movable part 200 used in the foil collecting step according to this embodiment will be described. As shown in FIG. 6, in this embodiment, there are two pressing members 202 in the Y direction. The foil pressing movable part 200 is controlled by a control unit (not shown). In addition, the control unit stores information about the bending point P calculated by the above-mentioned method or the like. The pressing member 202 (which can also be called a foil pressing member) is a member for collecting the positive electrode active material layer non-forming parts 52a constituting the positive electrode current collector foil laminated part 52A. The pressing member 202 is connected to a linearly moving cylinder (not shown) via a spring 204. The pressing strength of the pressing member 202 can be set, for example, according to a conventionally known pressing strength. The pressing member 202 is on a guide (also called a linear motion guide: LM guide) 208 that can move in the X direction in FIG. 6. In addition, a box-shaped unit 206 provided in the guide 208 has a cam floor 210 that can move in the X direction. The cam floor 210 is configured to be movable along the cam groove 212. As shown in FIG. 6 and FIG. 7, when the pressing member 202 approaches the vicinity of the foil collecting position, the cam floor 210 moves along the cam groove 212, and in conjunction with this, the pressing member 202 moves so as to abut against the bending point P of each of the positive active material layer non-forming portions 52a constituting the positive current collector foil laminated portion 52A. The movement of the pressing member 202 is performed by making full use of a cylinder. In this way, the positive current collector foil laminated portion 52A can be collected while drawing a predetermined miracle. The negative current collector foil laminated portion 62A can also be collected by a similar method.

[0035] In FIG. 5, the shorter the length in the width direction (here, the X direction in FIG. 5) of the positive current collector foil laminated portion 52A (more specifically, the positive active material layer non-forming portion 52a constituting the positive current collector foil laminated portion 52A) that is collected in the foil collecting step, the more likely the foil is to be broken by sliding between the positive current collector foil laminated portion 52A and the pressing member 202, and therefore the more suitable it is for application of the technology disclosed herein. From this viewpoint, although not particularly limited, the length Q in the width direction of the positive current collector foil laminated portion 52A that is collected in the foil collecting step is preferably 30 mm or less, more preferably 25 mm or less, and more preferably 20 mm or less. The lower limit of the length Q is, for example, 5 mm or more, and may be 10 mm or more. The same applies to the negative current collector foil laminated portion 62A.

[0036] Here, the number of turns of the electrode body 20 (here, the wound electrode body) is not particularly limited as long as the effect of the technology disclosed herein can be obtained. On the other hand, for example, the more the number of turns of the electrode body 20, the more likely the electrode current collector foil near the outermost surface of the electrode body 20 is to break due to sliding between the electrode current collector foil and the pressing member 202, and therefore it can be said that the electrode body 20 is suitable for application of the technology disclosed herein. From this viewpoint, although not particularly limited, the number of turns of the electrode body 20 is preferably 10 or more, more preferably 20 or more, 30 or more, or 40 or more. In addition, the number of layers of the electrode body 20 may be, for example, 60 or less, or 50 or less. In addition, when the electrode body is a laminated electrode body, the "number of turns" in the above description is replaced with the "number of layers", and each numerical value is replaced with a numerical value obtained by multiplying each numerical value by two.

[0037] The positive current collector foil 52 constituting the positive current collector foil laminate 52A is generally made of a metal foil with low rigidity (in other words, soft), such as an aluminum foil or an aluminum alloy foil, and therefore the foil is easily broken. That is, the embodiment in which at least the positive current collector foil laminate 52A is collected in the foil collecting step is suitable as a subject to which the technology disclosed herein can be applied. <Joining process: Step S3>

[0038] Next, the positive collector terminal 42a and the negative collector terminal 44a are attached to the electrode collector foil laminated parts (here, the positive collector foil laminated part 52A and the negative collector foil laminated part 62A) collected in the foil collecting process by pressure welding, resistance welding, ultrasonic welding, or the like (see FIG. 8). For example, when ultrasonic welding is performed between the foil collecting part 26 and the collector terminals (the positive collector terminal 42a and the negative collector terminal 52a), it is preferable that a horn is built into one of a pair of pressing jigs (not shown) and the other pressing jig is an anvil (receiving jig). This allows the collector terminals to be connected while the foil collecting part 26 is being pressed and molded. Note that here, it is assumed that the positive terminal 42, the negative terminal 44, the positive collector terminal 42a, and the negative collector terminal 44a are attached to the lid body 34 of the battery case 30. This connects the electrode body 20 to the lid body 34 of the battery case 30. Then, the electrode body 20 is inserted into the inside of the case body 32 through the opening of the case body 32. Thereafter, the case body 32 and the lid 34 are sealed together by laser welding or the like.

[0039] Next, the non-aqueous electrolyte 80 is prepared according to a known method. The non-aqueous electrolyte 80 is injected into the battery case 30 through the injection hole in the lid 34 of the battery case 30, and the injection hole is sealed. In this manner, the battery 100 can be obtained.

[0040] The battery 100 can be used for various purposes. Specific applications include portable power sources for personal computers, portable electronic devices, portable terminals, etc.; power sources for driving vehicles such as electric vehicles (BEVs), hybrid vehicles (HEVs), and plug-in hybrid vehicles (PHEVs); and storage batteries for small power storage devices, among which a power source for driving vehicles is preferable. The lithium ion secondary battery 200 can also be used in the form of a battery pack in which a plurality of batteries are typically connected in series and / or parallel.

[0041] Although one embodiment of the present disclosure has been described above, the above embodiment is merely an example. The present disclosure can be implemented in various other forms. The present disclosure can be implemented based on the contents disclosed in this specification and the technical common sense in the field. The technology described in the claims includes various modifications and changes to the above-exemplified embodiments. For example, it is possible to replace a part of the above-mentioned embodiment with another modified form, and it is also possible to add another modified form to the above-mentioned embodiment. In addition, if the technical feature is not described as essential, it is also possible to delete it as appropriate.

[0042] For example, in the above embodiment, the technology disclosed herein is applied to both the positive current collector foil laminate 52A and the negative current collector foil laminate 62A, but is not limited thereto. In other embodiments, the technology disclosed herein may be applied to only one of the positive current collector foil laminate and the negative current collector foil laminate.

[0043] For example, in the above embodiment, the electrode body 20 is a wound electrode body, but is not limited to this. In other embodiments, the electrode body may be a laminated electrode body in which a positive electrode sheet and a negative electrode sheet are laminated with a separator sheet interposed therebetween.

[0044] For example, in the above embodiment, a rectangular battery 100 including a flat electrode body 20 has been described. However, the battery may have another shape, such as a cylindrical shape.

[0045] Although the embodiment of the present disclosure has been described above, the above embodiment is merely an example. The present disclosure can be implemented in various other forms. The present disclosure can be implemented based on the contents disclosed in this specification and the technical common sense in the relevant field. The technology described in the claims includes various modifications and changes of the above-exemplified embodiment. [Explanation of symbols]

[0046] 20 Electrode body 20a Core 26 Foil Collection Department 30 Battery case 32 Case body 34 Lid 36 Safety valve 42 Positive terminal 42a Positive collector terminal 44 Negative terminal 44a Negative current collector terminal 50 Positive electrode sheet (positive electrode) 52 Positive electrode current collector foil 52a Portion where positive electrode active material layer is not formed 52A Positive current collector foil laminate 54 Cathode active material layer 60 Negative electrode sheet (positive electrode) 62 Negative electrode current collector foil 62a Part where negative electrode active material layer is not formed 62A Negative electrode current collector foil laminate 64 Negative electrode active material layer 70 Separator sheet 80 Non-aqueous electrolytes 100 Lithium-ion secondary battery 200 Foil holder movable part 202 Pressing member (foil pressing member) 204 Spring 206 units 208 Guide 210 Cam Floor 212 Cam groove P bending point

Claims

1. an electrode assembly in which a positive electrode sheet and a negative electrode sheet are laminated with a separator sheet interposed therebetween; current collecting terminals connected to the electrode body and corresponding to the positive electrode sheet and the negative electrode sheet; A method for producing an electricity storage device comprising the following steps: a preparation step of preparing the electrode body, in which a core portion where a positive electrode active material layer and a negative electrode active material layer face each other is present in a central portion in a predetermined width direction of the electrode body, a positive electrode current collector foil laminated portion is present in one of both end portions in the width direction, in which a positive electrode active material layer non-formed portion where the positive electrode active material layer is not formed protrudes from the negative electrode sheet, and a negative electrode current collector foil laminated portion is present in the other end portion, in which a negative electrode active material layer non-formed portion where the negative electrode active material layer is not formed protrudes from the positive electrode sheet; a foil collecting step of collecting the electrode current collecting foil laminate in at least one of the positive current collecting foil laminate and the negative current collecting foil laminate while sequentially shifting a pressing member from an end side of the electrode current collecting foil laminate opposite to a side where the core portion is present in the width direction to the core portion side so as to abut against the vicinity of a bending point of the electrode current collecting foil laminate; and a joining step of joining the electrode current collecting foil laminated portion collected in the foil collecting step to the current collecting terminal on the corresponding electrode side; A method for producing an electricity storage device comprising the steps of:

2. The method for producing an electricity storage device according to claim 1 , wherein the electrode current collector foil laminate collected in the foil collecting step has a length in the width direction of 30 mm or less.

3. The method for producing an electricity storage device according to claim 1 , wherein in the foil collecting step, at least the positive electrode current collector foil laminate portion is collected.

Citation Information

Patent Citations

  • Secondary battery

    JP2013178997A

  • Manufacturing method of battery

    JP2019102215A

  • Battery

    JP2020095797A

  • Secondary battery