Manufacturing method of switching element

The proposed manufacturing method for switching elements addresses miniaturization and cost issues by controlling trench depth and impurity implantation, ensuring low-energy implantation and consistent performance.

JP2024167649AActive Publication Date: 2024-12-04DENSO CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023083868
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-22
Publication Date
2024-12-04
Estimated Expiration
2043-05-22

AI Technical Summary

Technical Problem

Existing methods for manufacturing switching elements face challenges in miniaturization due to limitations in trench formation and high-energy ion implantation, leading to increased manufacturing costs and variations in element characteristics.

Method used

A manufacturing method involving trench formation with controlled depth and impurity implantation in a semiconductor substrate, followed by etching to expose the impurity region at the trench bottom, allowing for low-energy impurity implantation and suppression of channel region contamination, enabling miniaturization and reduced manufacturing costs.

Benefits of technology

The method enables miniaturization of switching elements, suppresses variations in characteristics, and reduces manufacturing costs by using lower energy implantation, while maintaining high breakdown voltage and channel integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024167649000001_ABST
    Figure 2024167649000001_ABST
Patent Text Reader

Abstract

To provide a technique for manufacturing a switching element having a bottom part injection region, capable of suppressing an impurity implantation to a channel region as well as enabling a refining of the switching element.SOLUTION: A manufacturing method of a switching element, includes: a step of forming a trench (14) of which a thickness of a depth is a thickness of a first n type region onto a front surface of a semiconductor substrate within a range where the first n type region is exposed; a step of forming an impurity implantation region (38) into a second n type region by implanting p type or n type impurity to a bottom surface of the trench; and a step of increasing the depth of the trench so that the impurity implantation region is exposed to the bottom surface of the trench by etching the bottom surface of the trench.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technology disclosed in this specification relates to a method for manufacturing a switching element.

[0002] Patent Document 1 discloses a method for manufacturing a switching element having a trench-type gate structure. In this manufacturing method, a semiconductor substrate having an n-type source region and a p-type body region is prepared. In this manufacturing method, a trench is formed on the surface of the semiconductor substrate, penetrating the source region and reaching the body region. Next, a sidewall insulating film is formed to cover the side surface of the trench. Next, impurities are injected into the bottom surface of the trench to form a bottom injection region around the bottom surface of the trench. Next, the sidewall insulating film is removed, and a gate insulating film and a gate electrode are formed in the trench. In a switching element having a trench-type gate structure, the range of the body region on the side surface of the trench is a region where a channel is formed during operation of the switching element (hereinafter referred to as a channel region). In the manufacturing method of Patent Document 1, in the injection step into the bottom injection region, the injection of impurities into the channel region is suppressed by the sidewall insulating film. Therefore, according to the manufacturing method of Patent Document 1, it is possible to suppress the variation in the characteristics of the switching element. Note that, although n-type impurities are injected into the bottom injection region in Patent Document 1, p-type impurities may also be injected into the bottom injection region. Even in this case, by suppressing the injection of impurities into the channel region, it is possible to suppress variations in the characteristics of the switching elements. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2021-027253 Summary of the Invention [Problem to be solved by the invention]

[0004] In the technique of Patent Document 1, the injection range is limited by the sidewall insulating film when impurities are injected into the bottom of the trench. Therefore, in order to form a wide bottom injection region, it is necessary to form a wide trench in advance. Therefore, with this technique, it is difficult to miniaturize the switching element.

[0005] Another manufacturing method is to inject impurities with high energy before forming a trench, and form a bottom implantation region at a deep position. After forming the bottom implantation region, a trench is formed on the surface of the semiconductor substrate, and the bottom implantation region is exposed on the bottom surface of the trench. This manufacturing method can also manufacture a switching element having a bottom implantation region provided around the bottom surface of the trench. However, this manufacturing method requires a special ion implantation device to perform high-energy ion implantation. In addition, the amount of impurities that can be implanted per unit time is low in high-energy ion implantation, so the ion implantation process takes time. Therefore, this manufacturing method increases the manufacturing cost of the switching element.

[0006] This specification proposes a technique for manufacturing a switching element having a bottom injection region, which allows miniaturization of the switching element and easily suppresses impurity injection into the channel region. [Means for solving the problem]

[0007] A method for manufacturing a switching element includes a semiconductor substrate preparation step, a trench formation step, an impurity injection step, a trench depth increase step, a gate insulating film formation step, and a gate electrode formation step. In the semiconductor substrate preparation step, a semiconductor substrate is prepared in which a first n-type region is provided in a range exposed on the surface, a p-type body region is provided below the first n-type region, and a second n-type region is provided below the body region. In the trench formation step, a trench is formed on the surface within the range where the first n-type region is exposed, the depth of the trench being equal to or less than the thickness of the first n-type region. In the impurity injection step, an impurity injection region is formed in the second n-type region by injecting p-type or n-type impurities into the bottom surface of the trench. In the trench depth increase step, after forming the impurity injection region, the bottom surface of the trench is etched to increase the depth of the trench so that the impurity injection region is exposed on the bottom surface of the trench. In the gate insulating film formation step, after exposing the impurity injection region on the bottom surface of the trench, a gate insulating film is formed to cover the inner surface of the trench. In the gate electrode forming step, after the gate insulating film is formed, a gate electrode is formed in the trench.

[0008] In this manufacturing method, a trench having a depth equal to or less than the thickness of the first n-type region is formed, and then an impurity-implanted region is formed in the second n-type region by injecting impurities into the bottom surface of the trench. The impurity-implanted region is formed deep relative to the surface of the semiconductor substrate, but since the trench is formed, the impurity-implanted region can be formed with relatively low implantation energy. Furthermore, since the depth of the trench is equal to or less than the thickness of the first n-type region, the implantation of impurities into the channel region in the body region is suppressed. After the impurity-implanted region is formed, the depth of the trench is increased so that the impurity-implanted region is exposed at the bottom surface of the trench. Then, a gate insulating film and a gate electrode are formed to complete a gate structure having an impurity-implanted region at the bottom of the trench. In this way, according to this manufacturing method, the implantation of impurities into the channel region can be suppressed, and the variation in the characteristics of the switching element can be suppressed. Furthermore, according to this manufacturing method, the impurity-implanted region can be formed with relatively low implantation energy, and the gate structure can be easily formed. Furthermore, according to this manufacturing method, the impurity-implanted region can be formed even if the width of the trench is narrow, so that the switching element can be miniaturized. [Brief description of the drawings]

[0009] [Figure 1] FIG. [Diagram 2] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Diagram 3] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Figure 4] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Diagram 5] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Figure 6] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Figure 7] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Figure 8] 4A to 4C are explanatory views of a manufacturing method according to an embodiment. [Figure 9] FIG. 2 is an explanatory diagram of a manufacturing method of Comparative Example 1. [Figure 10] FIG. 4 is an explanatory diagram of a manufacturing method of Comparative Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The switching element 10 shown in FIG. 1 is a metal oxide semiconductor field effect transistor (MOSFET). The switching element 10 has a semiconductor substrate 12 made of SiC (silicon carbide). The semiconductor substrate 12 may be made of other semiconductor materials such as silicon. A plurality of trenches 14 are provided on an upper surface 12a of the semiconductor substrate 12. The inner surface of each trench 14 is covered with a gate insulating film 16. A gate electrode 18 is disposed in each trench 14. Each gate electrode 18 is insulated from the semiconductor substrate 12 by the gate insulating film 16. An interlayer insulating film 20 and an upper electrode 22 are provided on the upper portion of the semiconductor substrate 12. The interlayer insulating film 20 covers the upper surface of each gate electrode 18. The upper electrode 22 covers the upper surface 12a of the semiconductor substrate 12 and the interlayer insulating film 20. The upper electrode 22 is insulated from each gate electrode 18 by the interlayer insulating film 20. The upper electrode 22 is insulated from each gate electrode 18 by the interlayer insulating film 20. The upper electrode 22 is in contact with the upper surface 12a of the semiconductor substrate 12 at a position where the interlayer insulating film 20 is not present. A lower electrode 24 is provided on the lower part of the semiconductor substrate 12. The lower electrode 24 is in contact with the lower surface 12b of the semiconductor substrate 12.

[0011] The semiconductor substrate 12 has a number of source regions 30 , a number of contact regions 32 , a body region 34 , a drift region 36 , a bottom region 38 , a buffer region 39 , and a drain region 40 .

[0012] Each source region 30 is an n-type region with a high concentration of n-type impurities. A source region 30 is disposed in each of the regions sandwiched between the trenches 14 (hereinafter referred to as inter-trench regions). In each inter-trench region, the source region 30 is disposed at a position including the upper end of the side surface of the trench 14 and the upper surface 12a. Each source region 30 contacts the gate insulating film 16 on the side surface of the trench 14. Each source region 30 is in ohmic contact with the upper electrode 22.

[0013] Each contact region 32 is a p-type region with a high concentration of p-type impurities. A contact region 32 is disposed in each inter-trench region. Each contact region 32 is disposed at a position including the upper surface 12a. Each contact region 32 is in ohmic contact with the upper electrode 22. Each contact region 32 is adjacent to the source region 30.

[0014] The body region 34 is a p-type region having a lower p-type impurity concentration than the contact region 32. The body region 34 is distributed across multiple inter-trench regions. The body region 34 contacts the source region 30 and the contact region 32 from below. The body region 34 contacts the gate insulating film 16 below the source region 30.

[0015] The drift region 36 is an n-type region having a lower n-type impurity concentration than the source region 30. The drift region 36 is distributed across the lower portions of the multiple inter-trench regions. The drift region 36 contacts the body region 34 from below. The drift region 36 contacts the gate insulating film 16 below the body region 34. The drift region 36 is separated from each source region 30 by the body region 34.

[0016] Each bottom region 38 is disposed at a position including the bottom surface of each trench 14. Each bottom region 38 is provided along the bottom surface of the corresponding trench 14. Each bottom region 38 is in contact with the gate insulating film 16 at the bottom surface of the corresponding trench 14. In the cross section shown in FIG. 1, each bottom region 38 is separated from the body region 34 by the drift region 36. Each bottom region 38 may be connected to the potential of the body region 34 or may be floating. When each bottom region 38 is connected to the potential of the body region 34, each bottom region 38 is connected to the body region 34 at a position not shown. Each bottom region 38 is in contact with the drift region 36 at its side and bottom surface.

[0017] The buffer region 39 is an n-type region having a higher n-type impurity concentration than the drift region 36. The buffer region 39 contacts the drift region 36 from below.

[0018] The drain region 40 is an n-type region having a higher n-type impurity concentration than the buffer region 39. The drain region 40 contacts the buffer region 39 from below. The drain region 40 is disposed at a position including the lower surface 12b. The drain region 40 is in ohmic contact with the lower electrode 24.

[0019] When the switching element 10 is in use, a potential higher than that of the upper electrode 22 is applied to the lower electrode 24. When a potential equal to or higher than the gate threshold is applied to the gate electrode 18, a channel is formed in a portion of the body region 34 adjacent to the gate insulating film 16 (hereinafter referred to as a channel region). Each source region 30 is connected to the drift region 36 by the channel. Therefore, electrons flow from the source region 30 to the drain region 40 via the channel, the drift region 36, and the buffer region 39. That is, the switching element 10 is turned on. As described above, when the switching element 10 is turned on, electrons flow through the channel formed in the channel region. Therefore, the channel region has a large effect on the characteristics of the switching element (particularly, the channel resistance, the gate threshold, etc.).

[0020] When the potential of the gate electrode 18 is reduced to a potential below the gate threshold, the channel disappears and the flow of electrons stops. That is, the switching element 10 is turned off. When the switching element 10 is turned off, a depletion layer spreads from the body region 34 and each bottom region 38 to the drift region 36. The depletion layer spreading from each bottom region 38 to the drift region 36 suppresses electric field concentration near the bottom surface of each trench 14. Therefore, the switching element 10 has a high breakdown voltage.

[0021] Next, a description will be given of a method for manufacturing the switching element 10. The switching element 10 is manufactured from a semiconductor substrate 12 entirely constituted by the drift region 36 (that is, the semiconductor substrate 12 before processing).

[0022] First, epitaxial growth, ion implantation, and the like are performed on the semiconductor substrate 12 to form the source region 30, the contact region 32, and the body region 34 as shown in Fig. 2. This results in a structure in which the source region 30 is provided in the range exposed on the upper surface 12a, the body region 34 is provided below the source region 30, and the drift region 36 is provided below the body region 34.

[0023] Next, as shown in FIG. 3, a mask 50 having an opening 50a is formed on the semiconductor substrate 12. Here, the mask 50 is formed so that the opening 50a is located above the center of the source region 30. Next, anisotropic etching is performed on the upper surface 12a of the semiconductor substrate 12 through the mask 50. As a result, trenches 14 are formed in each area of ​​the upper surface 12a where the source region 30 is exposed. Here, the trenches 14 are formed so that the depth D1 of the trenches 14 is smaller than the thickness T1 of the source region 30. In other words, the trenches 14 are formed so that they do not penetrate the source region 30.

[0024] Next, as shown in Fig. 4, p-type impurities (e.g., aluminum ions, etc.) are implanted into the semiconductor substrate 12 through the mask 50. That is, the p-type impurities are implanted into the bottom surface of each trench 14. Here, the p-type impurities are implanted so that they penetrate the body region 34 and stop within the drift region 36, thereby forming the bottom region 38 inside the drift region 36. Note that, although the bottom region 38 is separated from the body region 34 in Fig. 4, the bottom region 38 may be formed so that the upper end of the bottom region 38 overlaps with the body region 34 as shown in Fig. 5.

[0025] Next, as shown in FIG. 6, anisotropic etching is performed on the bottom surface of the trench 14 through a mask 50, thereby increasing the depth of the trench 14. Here, the depth of the trench 14 is increased so that the trench 14 penetrates the body region 34 and the bottom region 38 is exposed on the bottom surface of the trench 14. In either state of FIG. 4 or 5, the trench 14 can be deepened by etching to expose the bottom region 38 on the bottom surface of the trench 14 as shown in FIG. 6. Since the trench 14 penetrates the body region 34, the body region 34 and the drift region 36 are exposed on the side surface of the trench 14. The body region 34 in the range exposed on the side surface of the trench 14 becomes the above-mentioned channel region. After the trench 14 is deepened, the mask 50 is removed.

[0026] Next, as shown in FIG. 7, a gate insulating film 16 is formed to cover the inner surface of the trench 14. Next, as shown in FIG. 8, a gate electrode 18 is formed in the trench 14. Next, an interlayer insulating film 20 and an upper electrode 22 are formed on the upper part of the semiconductor substrate 12. Next, a buffer region 39 and a drain region 40 are formed by ion-implanting n-type impurities into the lower surface 12b of the semiconductor substrate 12. Next, a lower electrode 24 is formed on the lower part of the semiconductor substrate 12. Through the above steps, the switching element 10 shown in FIG. 1 is completed.

[0027] Next, advantages of the above-mentioned manufacturing method will be described. FIG. 9 shows a process of forming the bottom region 38 of Comparative Example 1. In FIG. 9, the bottom region 38 is formed by injecting p-type impurities into the upper surface 12a of the semiconductor substrate 12 without forming the trench 14. In this case, since the injection distance of the p-type impurities (i.e., the distance from the upper surface 12a to the formation position of the bottom region 38) is long, it is necessary to inject the p-type impurities with high energy. In contrast, in the manufacturing method of the embodiment, as shown in FIGS. 4 and 5, the p-type impurities are injected in a state in which the trench 14 is formed, so that the injection distance of the impurities is shorter than that in FIG. 9. Therefore, the bottom region 38 can be formed with lower injection energy than that in FIG. 9. Therefore, the bottom region 38 can be formed at low cost.

[0028] FIG. 10 shows a process of forming the bottom region 38 of Comparative Example 2. In FIG. 10, a trench 14 reaching the drift region 36 is formed, and the bottom region 38 is formed by injecting p-type impurities into the bottom surface of the trench 14. In this method, as shown by the dashed arrow in FIG. 10, p-type impurities reflected and scattered by the mask 50, the semiconductor substrate 12, etc. are injected into the side surface of the trench 14 within the range of the body region 34. That is, the reflected and scattered p-type impurities are directly injected into the channel region. For this reason, in the manufacturing method of FIG. 10, many crystal defects are formed in the channel region, causing problems such as an increase in channel resistance and variations in gate threshold. In contrast, as shown in FIGS. 4 and 5, in the manufacturing method of the embodiment, the body region 34 is not exposed on the side surface of the trench 14 in the injection process of the p-type impurities. For this reason, as shown by the dashed arrow in FIG. 4 and 5, the p-type impurities reflected and scattered by the mask 50, the semiconductor substrate 12, etc. are not directly injected into the channel region. In this way, the injection of the reflected and scattered p-type impurities into the channel region is suppressed. Therefore, according to the manufacturing method of the embodiment, problems such as an increase in channel resistance and variations in gate threshold can be prevented. In the manufacturing method of the embodiment, the p-type impurities reflected and scattered in the process of forming the bottom region 38 are implanted into the source region 30 that constitutes the side surface of the trench 14. However, since the concentration of n-type impurities in the source region 30 is high, the implantation of p-type impurities into the source region 30 has almost no effect on the characteristics of the switching element 10.

[0029] As described above, in the manufacturing method of the embodiment, it is not necessary to form a protective film on the side surface of the trench 14 to prevent the injection of p-type impurities. Therefore, even if the width of the trench 14 is narrow, the step of injecting p-type impurities into the bottom region 38 can be suitably performed. Since the width of the trench 14 can be narrowed, the switching elements can be miniaturized. Therefore, according to this manufacturing method, switching elements that are integrated at high density can be formed.

[0030] In the above-described embodiment, the depth D1 of the trench 14 is smaller than the thickness T1 of the source region 30 before the bottom region 38 is formed. However, the depth D1 of the trench 14 may be equal to the thickness T1 of the source region 30 before the bottom region 38 is formed. Even in this configuration, the body region 34 is not exposed on the side surface of the trench 14 when the bottom region 38 is formed, so that the injection of p-type impurities into the channel region can be suppressed.

[0031] In the above-described embodiment, the switching element 10 is a MOSFET, but the switching element 10 may be an IGBT (i.e., an insulated gate bipolar transistor). By replacing the n-type drain region 40 in FIG. 1 with a p-type collector region, an IGBT structure can be obtained. The manufacturing process of the IGBT can also employ the same manufacturing method as in the above-described embodiment.

[0032] In the above embodiment, the bottom region 38 is a p-type region, but the bottom region 38 may be an n-type region having a higher n-type impurity concentration than the drift region 36. In Figures 4 and 5, the n-type bottom region 38 can be formed by implanting n-type impurities into the bottom surface of the trench 14. In this case, the implantation of n-type impurities into the channel region is suppressed. In this case, too, changes in the characteristics of the switching element (i.e., an increase in channel resistance, an increase in variation in gate threshold, etc.) can be suppressed.

[0033] The source region 30 of the embodiment is an example of a first n-type region. The drift region 36 of the embodiment is an example of a second n-type region. The bottom region 38 of the embodiment is an example of an impurity-implanted region.

[0034] Although the embodiments have been described in detail above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and changes to the specific examples exemplified above. The technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technology exemplified in this specification or drawings achieves multiple objectives simultaneously, and achieving one of the objectives itself has technical utility. [Explanation of symbols]

[0035] 12: semiconductor substrate, 14: trench, 16: gate insulating film, 18: gate electrode, 30: source region, 34: body region, 36: drift region, 38: bottom region

Claims

[Claim 1] A method for manufacturing a switching element, comprising the steps of: A step of preparing a semiconductor substrate having a first n-type region (30) in a range exposed on the surface, a p-type body region (34) below the first n-type region, and a second n-type region (36) below the body region; forming a trench (14) in the surface within an area where the first n-type region is exposed, the trench having a depth equal to or less than a thickness of the first n-type region; forming an impurity-implanted region (38) in the second n-type region by implanting a p-type or n-type impurity into a bottom surface of the trench; after forming the impurity-implanted region, increasing the depth of the trench by etching a bottom surface of the trench so that the impurity-implanted region is exposed at a bottom surface of the trench; forming a gate insulating film covering an inner surface of the trench after exposing the impurity implanted region at a bottom surface of the trench; forming a gate electrode in the trench after forming the gate insulating film; The manufacturing method comprising the steps of:

Citation Information

Patent Citations

  • Method of manufacturing semiconductor device

    JP2011134809A

  • Silicon carbide semiconductor device manufacturing method

    JP2016012683A

  • Semiconductor device including trench structure including a gate electrode for diode region and contact structure

    JP2016163049A

  • Semiconductor device and semiconductor device manufacturing method

    JP2018207101A

  • Silicon carbide semiconductor device and method for manufacturing silicon carbide semiconductor device