Absorbent article and package
By using a polyolefin resin layer with biodegradation additives and controlled packaging, the absorbent articles achieve both strength and efficient decomposition, addressing cost and durability issues in conventional biodegradable materials.
Patent Information
- Application Number
- JP2023085309
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-12-05
AI Technical Summary
Conventional absorbent articles with biodegradable materials face issues of high cost and insufficient material strength, making them difficult to decompose efficiently when disposed of in soil.
Incorporating a polyolefin resin layer in the outer sheet that is not biodegradable on its own, but made biodegradable with additives that promote decomposition using oxygen, water, and ultraviolet light, along with a packaging sheet that limits oxygen and UV permeability to control biodegradation timing.
Ensures necessary material strength while reducing costs and accelerating the decomposition of absorbent articles after disposal, maintaining functionality and environmental compatibility.
Smart Images

Figure 2024168547000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to absorbent articles and packages. [Background technology]
[0002] Conventionally, there has been known an absorbent article comprising an inner sheet member that faces the wearer's skin, an outer sheet member that is positioned on the opposite side of the inner sheet member from the skin side, and an absorbent body that is positioned between the inner sheet member and the outer sheet member and absorbs the wearer's excrement (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2020-195428 A Summary of the Invention [Problem to be solved by the invention]
[0004] The absorbent article as described above generally has a structure in which a plurality of sheet materials are laminated, and is folded up so as to confine excrement inside when disposed of. For this reason, for example, when a used absorbent article (for example, an absorbent article disposed of in a folded state as described above) is buried in soil, microorganisms in the soil are unlikely to penetrate into the absorbent article, and the decomposition process of the absorbent article may take a long time. Therefore, in order to promote the decomposition process of the absorbent article (i.e., to promote the introduction of microorganisms into the absorbent article), it is considered that the outer sheet member of the absorbent article is made of a biodegradable resin such as polylactic acid resin. However, the above-mentioned biodegradable resin generally has problems in that it is expensive and has insufficient material strength.
[0005] Therefore, an object of the present disclosure is to provide an absorbent article that can ensure the necessary material strength while suppressing increases in costs and promote the biodegradation of the absorbent article after disposal, and a packaging body that can suitably package the absorbent article. [Means for solving the problem]
[0006] An absorbent article according to one aspect of the present disclosure is an absorbent article that absorbs excrement excreted by a wearer, comprising: an inner sheet member including one or more sheets facing the skin of the wearer; an outer sheet member including one or more sheets arranged on the opposite side of the inner sheet member from the skin side; an absorbent body arranged between the inner sheet member and the outer sheet member and absorbing the excrement of the wearer; and a fixing member for fixing the shape of the absorbent article so as to maintain a folded state in which the absorbent article is folded so that the inner sheet member is surrounded on the inside, wherein at least one of the outer sheet member and the fixing member has an outer exposed portion that is exposed to the outside in the folded state, and a first portion that is at least a part of the outer exposed portion is composed of a polyolefin resin that is not biodegradable by itself, and the first portion contains an additive that biodegrades the polyolefin resin using at least one of oxygen, water, and ultraviolet rays as an accelerating factor, and is configured to satisfy the biodegradation condition that the carbonyl index of the first portion is 1 or more within 28 days from the start of the biodegradability evaluation test specified in PAS9017:2020.
[0007] The packaging body according to the first aspect of the present disclosure is a packaging body for packaging a plurality of the above-mentioned absorbent articles collectively, and includes a packaging sheet for packaging the plurality of absorbent articles, and the oxygen permeability of the packaging sheet is lower than the oxygen permeability of the first portion.
[0008] A packaging body according to a second aspect of the present disclosure is a packaging body for packaging a plurality of the above-mentioned absorbent articles together, and includes a packaging sheet for packaging the plurality of absorbent articles, and the ultraviolet transmittance of the packaging sheet is lower than the ultraviolet transmittance of the first portion.
[0009] A packaging body relating to a third aspect of the present disclosure is a packaging body for packaging a plurality of the above-mentioned absorbent articles together, and includes a packaging sheet for packaging the plurality of absorbent articles, the packaging sheet sealing an internal space in which the absorbent articles are contained. Effect of the Invention
[0010] According to the present disclosure, it is possible to provide an absorbent article that can ensure the necessary material strength while suppressing increases in costs and promote the biodegradation of the absorbent article after disposal, and a packaging body that can suitably package the absorbent article. [Brief description of the drawings]
[0011] [Figure 1] 1 is a plan view of an absorbent article according to one embodiment, viewed from the non-skin facing side. [Diagram 2] FIG. 2 is a plan view of the absorbent article of FIG. 1, viewed from the skin facing side. [Diagram 3] 3 is a cross-sectional view of the absorbent article taken along line III-III in FIG. 2. [Figure 4] FIG. 2 is a diagram showing an example of a folded state of the absorbent article of FIG. [Diagram 5] FIG. 11 is a perspective view of an absorbent article according to a modified example. [Figure 6] FIG. 6 is a diagram showing an example of a folded state of the absorbent article of FIG. 5. [Figure 7] FIG. 2 is a perspective view of a package according to one embodiment. [Figure 8] FIG. 8 is a side view of the package of FIG. 7. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The present disclosure includes the following aspects 1 to 27.
[0013] (Aspect 1) An absorbent article for absorbing bodily waste discharged by a wearer, comprising: an inner sheet member including one or more sheets facing the wearer's skin; an outer sheet member including one or more sheets disposed on the opposite side to the skin side of the inner sheet member; an absorbent body disposed between the inner sheet member and the outer sheet member for absorbing bodily waste of the wearer; a fixing member for fixing the shape of the absorbent article so as to maintain the folded state in which the absorbent article is folded so that the inner sheet member is enclosed inside, At least one of the outer sheet member and the fixing member has an outer exposed portion that is exposed to the outside in the folded state, a first portion which is at least a part of the outer exposed portion is configured to contain a polyolefin resin which is not biodegradable by itself; The first part contains an additive that causes the polyolefin resin to biodegrade using at least one of oxygen, water, and ultraviolet light as an accelerating factor, thereby satisfying the biodegradation condition that the carbonyl index of the first part is 1 or more within 28 days from the start of the biodegradability evaluation test specified in PAS9017:2020. An absorbent article.
[0014] In the above absorbent article, by forming the first portion, which is at least a part of the outer exposed portion, from a polyolefin resin that does not have biodegradability by itself, the cost of the absorbent article can be reduced and the material strength of the first portion can be ensured, compared to when the first portion is formed from a biodegradable resin such as a polylactic acid resin. In addition, the absorbent article after use is usually discarded with the outer exposed portion exposed to the outside and the inner sheet member and the absorbent rolled up inward. In the above absorbent article, since the first portion contains an additive that promotes biodegradation so as to satisfy the above biodegradation conditions, the first portion of the absorbent article after disposal can be decomposed early. As a result, microorganisms can be permeated early into the absorbent article after disposal, and the biodegradation of the entire absorbent article can be promoted. Therefore, according to the above absorbent article, it is possible to ensure the necessary material strength while suppressing an increase in cost, and to promote the biodegradation of the absorbent article after disposal.
[0015] (Aspect 2) 2. The absorbent article of embodiment 1, wherein the additive comprises a phenolic antioxidant stabilizer. (Aspect 3) The absorbent article of aspect 2, wherein the content of the phenol-based antioxidant stabilizer in the additive is 0.02 to 0.15% by weight based on the total weight of the polyolefin resin and the additive. According to the second and third aspects, the start time of biodegradation can be appropriately adjusted so that decomposition starts after an expected certain product storage period has elapsed.
[0016] (Aspect 4) The outer sheet member includes a plurality of sheets, The additive is added to at least two or more sheets of the plurality of sheets, The absorbent article of aspect 2 or 3, wherein the content of the phenolic antioxidant stabilizer in each of the two or more sheets is greater in the sheet disposed on the outside. According to aspect 4, by increasing the degree of inhibition of biodegradation in the parts (outer parts) that are more likely to come into contact with outside air under normal conditions (during storage or use), it is possible to appropriately prevent unexpected promotion of biodegradation in the outer parts of the outer sheet member.
[0017] (Aspect 5) The tensile strength of the first portion is MD: 0.3N / mm 2 Above and CD: 0.07N / mm 2 The absorbent article according to any one of aspects 1 to 4, as described above. (Aspect 6) The absorbent article of any one of aspects 1 to 5, wherein the first portion has durability such that no pilling occurs when rubbed 50 times back and forth under a load of 200 g in a surface rub fastness test specified in JIS L0849. According to aspects 5 and 6, the material strength of the first portion can be suitably ensured, and therefore the stability of the absorbent article against deformation, breakage, etc. under normal circumstances (during storage or use) can be improved.
[0018] (Aspect 7) The absorbent article of any one of aspects 1 to 6, wherein the first portion has a thickness of 0.1 mm or more and 2.0 mm or less. If the thickness of the first portion (outer exposed member) is thinner than 0.1 mm, the texture is likely to be poor. Also, if the thickness of the first portion is thicker than 2.0 mm, the large thickness reduces the decomposition rate of the first portion. Therefore, according to the seventh aspect, by setting the thickness of the first portion in the range of 0.1 mm to 2.0 mm, it is possible to suppress the decrease in the decomposition rate while maintaining a good texture.
[0019] (Aspect 8) The absorbent article of any one of aspects 1 to 7, wherein the first portion has an ultraviolet ray transmittance of 15% or more. According to the eighth aspect, ultraviolet light, which may be a factor in promoting biodegradation of a member inside the first portion of the absorbent article, can be suitably guided through the first portion to the inner member, thereby accelerating the start of biodegradation inside the absorbent article and improving the decomposition rate of the entire absorbent article.
[0020] (Aspect 9) the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; The absorbent article of any one of aspects 1 to 8, wherein the first portion has a higher air permeability as measured by a Frazier test than the intermediate sheet has a higher air permeability as measured by a Frazier test. (Aspect 10) the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; The absorbent article of any one of aspects 1 to 9, wherein the density of the first portion is lower than the density of the intermediate sheet. According to the ninth and tenth aspects, water, oxygen, and the like, which may be factors accelerating the biodegradation of the intermediate sheet, can be suitably guided to the intermediate sheet through the first portion, thereby accelerating the start of biodegradation inside the absorbent article (intermediate sheet), and improving the decomposition rate of the entire absorbent article.
[0021] (Aspect 11) The air permeability of the first portion measured by the Frazier test is 3 / (cm 2 ·s) or more than 700cm 3 / (cm 2 The absorbent article of any one of aspects 1 to 10, wherein: According to embodiment 11, the air permeability is set to 700 cm 3 / (cm 2 By keeping the air permeability below 100 cm s, the functions of the absorbent article (such as preventing leakage of excrement) are prevented from being impaired, while the air permeability is kept at 100 cm 3 / (cm 2 By setting the first portion at or above 0.1·s, water, oxygen, and the like, which may be factors promoting biodegradation, can be properly guided to the inside of the absorbent article through the first portion. As a result, the start of biodegradation inside the absorbent article can be accelerated, and the decomposition rate of the entire absorbent article can be improved.
[0022] (Aspect 12) The density of the first portion is 0.02 g / m 3 More than 0.1g / m 3 An absorbent article according to any one of aspects 1 to 11, which is as follows: According to a twelfth aspect, the density is 0.1 g / m 3 By keeping the density below 0.02 g / m, the functionality of the absorbent article (e.g., preventing leakage of excrement) is not impaired. 3 By doing so, water, oxygen, and the like, which may be factors promoting biodegradation, can be properly guided to the inside of the absorbent article through the first portion, and as a result, the start of biodegradation inside the absorbent article can be accelerated, and the decomposition speed of the entire absorbent article can be improved.
[0023] (Aspect 13) 13. The absorbent article according to any one of aspects 1 to 12, wherein the absorbent body comprises a biodegradable highly absorbent polymer. According to the thirteenth aspect, the first portion of the absorbent article is biodegraded to allow the microorganisms to reach the absorbent body, thereby allowing the absorbent body to be appropriately biodegraded.
[0024] (Aspect 14) 14. The absorbent article of embodiment 13, wherein the biodegradation promoter of the superabsorbent polymer is the same as the biodegradation promoter of the first portion. According to the fourteenth aspect, it is possible to prevent the occurrence of a situation in which only one of the first portion and the highly water-absorbent polymer remains without being decomposed in the same environment.
[0025] (Aspect 15) The factor promoting the biodegradation of the superabsorbent polymer includes a substance derived from the excrement, 14. The absorbent article of embodiment 13, wherein the biodegradation promoting agent of the first portion does not include substances derived from the bodily waste. According to the fifteenth aspect, since the decomposition of the absorbent (superabsorbent polymer) can be started from the time when the wearer excretes bodily waste in the absorbent article, the time until the biodegradation of the absorbent is completed can be shortened. Meanwhile, since the factor promoting the biodegradation of the first part does not contain a substance derived from the bodily waste, it is possible to prevent the first part from starting to decompose before the appropriate decomposition start time (i.e., the time after the disposal of the absorbent article) triggered by the excretion treatment.
[0026] (Aspect 16) The absorbent article of any one of aspects 1 to 15, wherein the first portion is rendered biodegradable by the additive, such that a portion accounting for 90% or more of the total weight of the absorbent article is biodegradable. According to the sixteenth aspect, the biodegradation of the discarded absorbent article can be promoted more effectively.
[0027] (Aspect 17) the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; 17. The absorbent article of any one of aspects 1 to 16, wherein a degree of deterioration of the intermediate sheet measured by the evaluation test is higher than a degree of deterioration of the first portion measured by the evaluation test. (Aspect 18) The intermediate sheet also contains the additive, 18. The absorbent article of embodiment 17, wherein the content of the additive in the intermediate sheet is greater than the content of the additive in the first portion. In order to prevent leakage of bodily waste, the intermediate sheet generally has a structure that is difficult to decompose. According to aspects 17 and 18, such an intermediate sheet can be made to have a structure that is easily biodegradable. As a result, the decomposition speed of the entire absorbent article can be improved.
[0028] (Aspect 19) The fixing member includes a base sheet and an engagement portion provided on a surface of the base sheet, The first portion includes the base sheet, The absorbent article according to any one of aspects 1 to 18, wherein the engagement portion is configured to be able to engage with an outer surface of the outer sheet member or the fixing member so as to maintain the folded state. According to the 19th aspect, in the absorbent article after disposal, the biodegradation of the base sheet of the engaging member is promoted, so that the inside of the absorbent article can be exposed to the outside by releasing the folded state. As a result, microorganisms can easily come into contact with the inner member of the absorbent article, and the decomposition speed of the entire absorbent article can be improved.
[0029] (Aspect 20) An absorbent article of aspect 19, wherein the engagement strength between the engagement portion and the outer surface after a predetermined period of time has elapsed since the start of the evaluation test of the first part is lower than the engagement strength between the engagement portion and the outer surface before the evaluation test is started. The engagement strength acts to maintain the folded state. In aspect 20, the biodegradability (e.g., the amount of additive added) of at least a part of the first part is adjusted so that the engagement strength between the engagement part and the outer surface after a predetermined period from the start of the evaluation test of the first part (i.e., the start of the promotion of biodegradation) is lower than the engagement strength before the evaluation test is started. This makes it easier for the engagement part and the outer surface to be disengaged after a predetermined period from the start of the promotion of biodegradation, thereby increasing the possibility that the folded state will be released.
[0030] (Aspect 21) 21. The absorbent article of any one of aspects 1 to 20, wherein the biodegradation conditions further include the condition that, within 14 days from the start of the evaluation test, the number average molecular weight of the first portion becomes 5000 or less, the z average molecular weight of the first portion becomes 30000 or less, and the loss of the weight average molecular weight of the first portion becomes 90% or more. According to the twenty-first aspect, the biodegradation of the first part can be promoted more effectively.
[0031] (Aspect 22) A package for packaging a plurality of absorbent articles according to any one of aspects 1 to 21, A packaging sheet for packaging a plurality of the absorbent articles is provided, The packaging sheet has an oxygen permeability lower than that of the first portion. (Aspect 23) the outer sheet member of the absorbent article has an intermediate sheet disposed between the first portion and the absorbent body, 23. The package of embodiment 22, wherein the packaging sheet has an oxygen permeability lower than the oxygen permeability of the intermediate sheet. (Aspect 24) A package in which a plurality of absorbent articles according to any one of aspects 1 to 21 are packaged together, A packaging sheet for packaging a plurality of the absorbent articles is provided, The packaging sheet has an ultraviolet ray transmittance lower than an ultraviolet ray transmittance of the first portion. (Aspect 25) the outer sheet member of the absorbent article has an intermediate sheet disposed between the first portion and the absorbent body, 25. The package of embodiment 24, wherein the packaging sheet has an ultraviolet light transmittance lower than the ultraviolet light transmittance of the intermediate sheet. (Aspect 26) A package in which a plurality of absorbent articles according to any one of aspects 1 to 21 are packaged together, A packaging sheet for packaging a plurality of the absorbent articles is provided, The packaging sheet seals an internal space in which the absorbent article is contained. According to the packages of aspects 22 to 26, when the absorbent article is contained and stored in the packaging sheet before use (packaged state), it is possible to prevent oxygen, ultraviolet rays, etc., which may be factors that promote biodegradation, from entering the inside of the package. This makes it possible to prevent the start of biodegradation of the absorbent article (first part) from being accelerated, that is, to prevent the product life of the absorbent article from becoming shorter than expected. Therefore, the above packages can suitably package the absorbent article described above.
[0032] [Embodiment] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. In the following description, the same or corresponding elements are designated by the same reference numerals, and duplicated description will be omitted.
[0033] (Absorbent articles) FIG. 1 is a plan view of an absorbent article 1 according to one embodiment, as viewed from the non-skin-facing side. FIG. 2 is a plan view of the absorbent article 1 as viewed from the skin-facing side. FIG. 3 is a cross-sectional view taken along line III-III in FIG. 2. The plan views of FIG. 1 and FIG. 2 show the absorbent article 1 in an elongated state in which it has been elongated to a state in which no wrinkles are formed. In this embodiment, the "skin-facing side" refers to the side that faces the skin of a wearer when the absorbent article 1 is in use (worn), and the "non-skin-facing side" refers to the side that faces away from the skin of the wearer when the absorbent article 1 is in use (worn). In this embodiment, the "wearer" refers to a person who wears the absorbent article 1, and the "wearer" refers to a person who puts the absorbent article 1 on the wearer.
[0034] In the following description, the longitudinal direction (MD: machine direction) of the absorbent article 1 in a stretched state (see Figs. 1 and 2) is defined as the front-rear direction L, and the width direction (CD: cross direction) of the absorbent article 1 in a stretched state, which is perpendicular to the front-rear direction L, is defined as the width direction W. The front-rear direction L is a direction extending from the front to the rear of the wearer's body when the absorbent article 1 is in use. The width direction W is a direction that corresponds to the left-right direction of the wearer when the absorbent article 1 is in use.
[0035] The absorbent article 1 is an article that absorbs waste such as urine excreted by a wearer, and is, for example, a disposable diaper. The absorbent article 1 may be a disposable diaper for children or a disposable diaper for adults. As an example, the absorbent article 1 is configured as a so-called tape-type disposable diaper.
[0036] The absorbent article 1 includes an absorbent main body 10, a pair of fastening tapes 21A, 21B (fixing members), and a target tape 30. In the absorbent article 1, the absorbent main body 10 is a portion having a function of absorbing bodily waste, and the pair of fastening tapes 21A, 21B and the target tape 30 are portions having a function of attaching and fixing the absorbent main body 10 to a wearer. The fastening tapes 21A, 21B also have a function of fixing the shape of the absorbent article 1 so that the absorbent article 1 is maintained in a folded state described below after use of the absorbent article 1, etc.
[0037] The absorbent main body 10 is divided into a front waist region 101, a rear waist region 102, and a crotch region 103. The front waist region 101 is a region located on the front waist side of the wearer when in use (when worn). The rear waist region 102 is a region located on the rear waist side of the wearer when in use. The crotch region 103 is a region located between the front waist region 101 and the rear waist region 102 in the front-to-rear direction L, and is a region located under the crotch of the wearer when in use.
[0038] As shown in FIG. 3, the absorbent body 10 includes an inner sheet member 11, an outer sheet member 12, and an absorbent body 13.
[0039] The absorbent body 13 is disposed between the inner sheet member 11 and the outer sheet member 12, and is a portion that absorbs the wearer's excrement. The absorbent body 13 includes an absorbent core 13a and a core wrap 13b. As an example, the absorbent core 13a is a laminate of an absorbent material including pulp (crushed pulp) and a superabsorbent polymer (SAP). The core wrap 13b is formed of, for example, a tissue or a nonwoven fabric sheet, and is disposed so as to cover the skin-facing side and non-skin-facing side of the absorbent core 13a. The absorbent body 13 is provided in the central portion of the absorbent main body 10 in the width direction W, over substantially the entire area in the front-rear direction L, except for both ends in the front-rear direction L.
[0040] The SAP contained in the absorbent core 13a is biodegradable. Examples of biodegradable SAP materials include cellulose, cellulose nanofiber, carboxymethyl cellulose, starch, polyaspartic acid, polyglutamic acid, etc. The pulp contained in the absorbent core 13a is also derived from biomass and is therefore biodegradable. The core wrap 13b is also formed of a biodegradable material, such as tissue made of cellulose. As a result, the absorbent 13 as a whole is biodegradable.
[0041] The inner sheet member 11 is a member including one or more sheets facing the skin of the wearer. In this embodiment, the inner sheet member 11 includes a top sheet 11a and a side sheet 11b. The top sheet 11a is a liquid-permeable sheet arranged on the skin side so as to cover the absorbent body 13, and allows waste matter such as urine to pass through to the absorbent body 13. The top sheet 11a is made of, for example, a liquid-permeable nonwoven fabric. The side sheet 11b is a liquid-impermeable sheet arranged over the entire area in the front-rear direction L so as to cover both sides of the top sheet 11a in the width direction W, outside the central part of the absorbent body 13 in the width direction W. The side sheet 11b is made of, for example, a hydrophobic nonwoven fabric.
[0042] Both the top sheet 11a and the side sheet 11b are biodegradable. The top sheet 11a and the side sheet 11b may be configured to be biodegradable by, for example, blending an additive (an additive for promoting biodegradation blended in the outer nonwoven fabric 12b described below) described later, or may be configured to be biodegradable by being made of a biodegradable material such as cotton, regenerated cellulose such as rayon or lyocell, PBAT, PLA, PBS, PHA, PVA, PBSA, PGA, PETS, cellulose acetate, or a mixture of these blended in any ratio.
[0043] An elastic member 116a (see FIG. 2) such as rubber thread is provided at the inner end portion of the side sheet 11b in the width direction W along the front-rear direction L. The front end of the elastic member 116a reaches the front waist region 101, and the rear end of the elastic member 116a reaches the rear waist region 102. Both ends of the side sheet 11b in the front-rear direction L are attached (fixed) to the top sheet 11a by adhesive or the like. The method of fixing the side sheet 11b to the top sheet 11a is not limited to pasting, and may be ultrasonic bonding or heat fusion by an embossing roll. An elastic member 115a such as a stretchable sheet is provided at the outer end portion of the side sheet 11b in the width direction W along the front-rear direction L between the side sheet 11b and the outer nonwoven fabric 12b described later. The front end of the elastic member 115a reaches the front waist region 101, and the rear end of the elastic member 115a reaches the rear waist region 102.
[0044] The outer sheet member 12 is a member including one or more sheets arranged on the opposite side to the skin side of the inner sheet member 11. That is, the outer sheet member 12 is arranged on the opposite side to the inner sheet member 11 with the absorbent body 13 sandwiched therebetween. The outer sheet member 12 includes a leakproof sheet 12a (middle sheet) and an outer nonwoven fabric 12b. The leakproof sheet 12a is a liquid-impermeable sheet arranged on the non-skin side so as to cover the absorbent body 13, and is a part having a function of preventing leakage of excrement to the outside. That is, the leakproof sheet 12a is arranged between the outer nonwoven fabric 12b and the absorbent body 13. The leakproof sheet 12a is made of, for example, a film. The outer nonwoven fabric 12b is a liquid-impermeable sheet arranged on the non-skin side of the leakproof sheet 12a. The outer nonwoven fabric 12b is made of, for example, a nonwoven fabric having hydrophobic properties. The outer nonwoven fabric 12b is an outer surface sheet that constitutes the outer surface of the outer sheet member 12 (i.e., the outermost surface on the non-skin side).
[0045] Both the leakproof sheet 12a and the outer nonwoven fabric 12b are biodegradable. The outer nonwoven fabric 12b is made of a degradable polymer composition that is adjusted to have biodegradability (for example, the degradable polymer composition described in JP2020-500254A).
[0046] The outer nonwoven fabric 12b contains a polyolefin resin derived from petroleum or biomass that is not biodegradable by itself as a main material (e.g., a material constituting 50% by weight or more of the entire outer nonwoven fabric 12b). The polyolefin resin is a type of polymer containing a repeating unit of the general formula -[CH2CRR']-. Preferably, R and R' are individually selected from the list including hydrogen, methyl, ethyl, acetate, vinyl acetate, methyl methacrylate, vinyl alcohol, and acrylic acid. The polyolefin resin constituting the outer nonwoven fabric 12b contains, for example, ethylene and / or propylene monomers, and may further contain monomers selected from the list including acetate, vinyl acetate, methyl methacrylate, vinyl alcohol, and acrylic acid. The polyolefin resin constituting the outer nonwoven fabric 12b may also be selected from LDPE, LLDPE, HDPE, MDPE, VLDPE, EVA, EVOH, EMMA, and EAA.
[0047] Here, "not having biodegradability" means that when left in a natural environment such as in the air, soil, or sea, over a long period of time (e.g., 2 years), the material is not broken down into inorganic substances (water, carbon dioxide, methane, etc.) due to the absence of microbial action (i.e., it is not decomposed by microorganisms), in other words, microplastics remain without being decomposed. In other words, the polyolefin resin constituting the outer nonwoven fabric 12b itself does not have biodegradability, unlike, for example, polylactic acid resin. More specifically, the polyolefin resin constituting the outer nonwoven fabric 12b has a viscosity of 1.0 g / m 3The outer nonwoven fabric 12b has a density below 100 μm and has a strength higher than that of general biodegradable resins (such as polylactic acid resins). The outer nonwoven fabric 12b contains such a polyolefin resin as a main material and is configured as a nonwoven fabric sheet having heat fusion points or fusion joints between fibers. The heat fusion points are fusion parts formed by heat fusion (point bonding) by hot embossing or the like. The fusion joints are joints formed by joining the surfaces of resin fibers melted by heat. As a result, the outer nonwoven fabric 12b has a material strength (such as tensile strength) higher than that of a biodegradable resin such as polylactic acid resin that is biodegradable by itself.
[0048] As described above, the polyolefin resin constituting the outer nonwoven fabric 12b is not biodegradable by itself. For this reason, in this embodiment, an additive for modifying the entire outer nonwoven fabric 12b to be biodegradable is added to the polyolefin resin constituting the outer nonwoven fabric 12b. The additive is configured to promote biodegradation using at least one of oxygen, water, and ultraviolet light as a promotion factor. In the additive of this embodiment (i.e., the additive exemplified below), all of oxygen, water, and ultraviolet light function as promotion factors for the decomposition reaction (breakage of C-C bonds).
[0049] As an example, the additive contained in the outer nonwoven fabric 12b is, relative to the total weight of the polyolefin resin and the additive constituting the outer nonwoven fabric 12b, (a) 0.15 to 0.6% by weight of a total of two or more transition metal compounds; (b) mono- or polyunsaturated C in an amount of 0.04 to 0.08% by weight 14 -C 24 a carboxylic acid, or an ester, anhydride, or an amide thereof; (c) synthetic rubber in an amount of 0.04 to 0.2% by weight; In addition, optionally, (d) dry starch in an amount of 0 to 20% by weight, and / or (e) calcium oxide in an amount of 0 to 1% by weight, and / or (f) containing a phenolic antioxidant stabilizer in an amount of 0 to 0.2 weight percent. The two or more transition metal compounds in (a) are selected from iron compounds, manganese compounds, copper compounds, cobalt compounds and cerium compounds, and the transition metals in the two or more transition metal compounds are different.
[0050] The leakproof sheet 12a is a resin film, and like the outer nonwoven fabric 12b, contains polyolefin resin, which is not biodegradable by itself, as its main material (e.g., a material constituting 50% by weight or more of the entire leakproof sheet 12a). In other words, the leakproof sheet 12a is a film member formed by melting polyolefin resin and forming it into a sheet. Like the outer nonwoven fabric 12b, the polyolefin resin constituting the leakproof sheet 12a also contains the above-mentioned additives blended therein.
[0051] As shown in FIG. 2, the absorbent body 10 has, as its functional components, leg stretchable sections 115 and leg side gathers 116.
[0052] The leg stretchable section 115 has elastic members 115a which are stretchable parts stretchable in the front-rear direction L on both sides (both ends in the width direction W) of the absorbent main body 10. In the leg stretchable section 115, the elastic members 115a contract to form leg gathers which improve the fit around the legs of the wearer in the crotch region 103 when in use.
[0053] The leg side gathers 116 are provided on the inside in the width direction W of the leg stretchable portions 115, have both ends in the front-rear direction L fixed, and are configured to be able to stand up by contracting in the front-rear direction L. The leg side gathers 116 include the above-mentioned side sheets 11b. In the leg side gathers 116, both ends in the front-rear direction L of the side sheets 11b are fixed to the top sheet 11a, and the elastic members 116a contract to form a pair of leakage-proof cuffs in the crotch region 103 in the used state that stand up toward the wearer's skin and prevent excrement from leaking along the surface of the top sheet 11a.
[0054] The fastening tapes 21A and 21B are configured to attach and fix the absorbent main body 10 to the wearer by being attached to the target tape 30 in a worn state. As shown in Figs. 1 and 2, the fastening tapes 21A and 21B are members provided at both ends in the width direction W of the rear waist region 102 of the absorbent main body 10 and extend outward in the width direction W. The fastening tapes 21A and 21B are fixed by being sandwiched between the side sheet 11b and the outer nonwoven fabric 12b of the absorbent main body 10, and are provided rearward of the rear end of the elastic member 115a. The fastening tapes 21A and 21B are provided symmetrically with respect to the central portion of the absorbent main body 10 in the width direction W, and are provided at the same position in the front-rear direction. The fastening tapes 21A and 21B have similar shapes and structures. Each of the fastening tapes 21A, 21B has a base sheet 211 which is a main body, and an engagement portion 212 provided on the skin-facing surface of the base sheet 211. The engagement portion 212 is a portion which is fastened to the target tape 30. The engagement portion 212 is, for example, a hook sheet provided with a plurality of engagement hooks.
[0055] 1, the target tape 30 is provided in the front waist region 101 of the absorbent main body 10, and is a target portion to which the fastening portions 210 of the fastening tapes 21A, 21B are fastened. The target tape 30 is attached to the outer nonwoven fabric 12b in the front waist region 101.
[0056] As shown in FIG. 4, the fastening tapes 21A and 21B also function as fixing members for fixing the shape of the absorbent article 1 so that the absorbent article 1 maintains a folded (rolled) state in which the inner sheet member 11 is surrounded on the inside. For example, after use of the absorbent article 1, as shown in FIG. 4(A), the fastening tapes 21A and 21B are removed from the target tape 30 to put the absorbent article 1 in an unfolded state, and then the absorbent article 1 is rolled up from the front side (the front waist region 101 side) so that the inner sheet member 11 is on the inside. Thereafter, as shown in FIG. 4(B), the fastening tapes 21A and 21B are engaged with the outer surface of the outer nonwoven fabric 12b. This maintains the absorbent article 1 in a folded state. Thus, in this embodiment, the engaging portions 212 of the fastening tapes 21A and 21B are configured to be engageable with the outer surface of the outer nonwoven fabric 12b facing each other in the folded state. The engaging portions 212 of the fastening tapes 21A, 21B may be configured to be engageable with the outer surface of the fastening tapes 21A, 21B (base material sheet 211). In this case, the folded state can also be achieved by engaging the engaging portion 212 of one fastening tape with the outer surface (the surface opposite to the side on which the engaging portion 212 is provided) of the base material sheet 211 of the other fastening tape. In either case, the absorbent article 1 is maintained in the folded state by engaging the engaging portions 212 of the fastening tapes 21A, 21B with the outer surface of the base material sheet 211 or the outer nonwoven fabric 12b.
[0057] The outer sheet member 12 and the fastening tapes 21A, 21B have outer exposed portions that are exposed to the outside in the above-mentioned folded state (see FIG. 4B). In this embodiment, the outer nonwoven fabric 12b of the outer sheet member 12 and the base sheet 211 of the fastening tapes 21A, 21B configure the outer exposed portions.
[0058] In addition, the first portion, which is at least a part of the outer exposed portion, is composed of a polyolefin resin that is not biodegradable by itself, and is configured to be biodegradable by blending the above-mentioned additive. As described above, in this embodiment, the entire outer nonwoven fabric 12b constitutes the first portion. The first portion is configured to satisfy the biodegradation condition that the carbonyl index of the first portion is 1 or more within 28 days from the start of the biodegradability evaluation test (ultraviolet accelerated weathering test) specified in PAS9017:2020 due to the inclusion of the above-mentioned additive.
[0059] The biodegradation conditions may further include, in addition to the above-mentioned conditions (the condition that the carbonyl index of the first portion is 1 or more), the condition that the number average molecular weight of the first portion is 5000 or less, the z-average molecular weight of the first portion is 30000 or less, and the loss of the weight average molecular weight of the first portion is 90% or more within 14 days from the start of the evaluation test. In this case, the biodegradation of the first portion can be promoted more effectively.
[0060] Whether the first part satisfies the above-mentioned biodegradation conditions can be confirmed by a test method conforming to PAS9017:2020 as described below. This test method includes a part conforming to the laboratory weathering standards of ASTM D4329-13 or BS EN ISO4892-1. The sample (first part) is mounted on a jig. In addition, an ultraviolet accelerated weathering device capable of irradiating a combination of air, heat, and ultraviolet light is used. The calibration and test procedures of the device are as described in BS EN ISO 4892-3 or ASTM D4329-13. <When the sample thickness is less than 0.25 mm> The UV accelerated weathering cycle is set to the following test conditions: (1) Irradiance: 0.8 W / m 2 ±0.02W / m 2 (2) UV cycle time: 1 hour (3) Dark cycle time: 23 hours (4) Air chamber temperature: Set at 60℃±2℃, ensure that the test period is within 14 consecutive days, and ensure that each sample is N3. <When the sample thickness is 0.25 mm or more> The above test conditions are adjusted as follows according to the laboratory weathering standards of ASTM D2565-16 or BS EN ISO 4892-1: (1) Irradiance: 0.35W / m 2 ±0.02W / m 2 , using a daylight filter (340 nm) (2) UV cycle time: 8 hours (3) Dark cycle time: 16 hours (4) Air chamber temperature: 60℃±2℃ (5) Non-insulated black panel temperature: Set to 70°C ± 2°C, and ensure that the test period is within 28 consecutive days. The Carbonyl Index is determined using infrared spectroscopy and the resulting IR spectrum. The spectrum is measured between 500 and 3000 cm -1 In the region of 1420-1500 cm -1 and 1650~1850cm -1 The area of the carbonyl index is the focus. The resolution is set to 4 cm or less, and the number of scans is set to 32 or more. The measurement is performed using software that can eliminate background noise and calculate the integral of the peak area. The carbonyl index is measured at least three times. The carbonyl index is calculated from the 1850-1650 cm -1 and 1500~1420cm -1 The average carbonyl index of each sample is determined from the three spectra collected. The molecular weight (number average, z-average, weight average) of the samples is measured by gel permeation chromatography (GPC) or size exclusion chromatography (GPC-SEC). The measurements are carried out with preparation according to BS ISO 16014-4 or ASTM D6474-20. The analysis of each sample shall be reported as the average of three runs. The samples collected shall cover one third of the total polyolefin material tested. The sample shall be completely dissolved in the solvent used for molecular weight analysis.
[0061] Furthermore, the following biodegradability evaluation using the entire absorbent article 1 may be performed in accordance with ASTM D 5988-18 and BS EN ISO 17556:2019. In that case, the evaluation may be performed using a sample prepared by adding the following additional conditions to the conditions of the above-mentioned test method. It is preferable to secure samples of N3 or higher, and if an invasive test is performed, it is preferable to secure even higher. <Additional conditions> The absorbent material (absorbent body 13) contained in the sample (absorbent article 1) is made to be 100% hydrated with physiological saline. Put the sample in a state that mimics the state it will be in when discarded, for example, by folding the sample as shown in Figure 4(B). The sheet materials constituting the sample (in this embodiment, the inner sheet member 11, the outer sheet member 12, the leakproof sheet 12a, the outer nonwoven fabric 12b, etc.) are maintained in a stacked state (this condition is met when an actual absorbent article 1 is used as the sample and placed in the above-mentioned folded state).
[0062] In the above additional conditions, "physiological saline" refers to a 0.9% NaCl aqueous solution (aq) made with distilled water. Also, "100% water retention state" refers to a state after a sample is immersed in the physiological saline for 30 minutes, placed on a mesh with the water-absorbing surface (i.e., the inner sheet member 11 on the absorbent body 13) facing downward, an acrylic plate (weight) is placed on the sample, a load of 10 kg is applied for 20 minutes, and then dehydrated for 90 seconds at a rotation speed of 540 rpm using a centrifugal dehydrator (e.g., top discharge centrifuge H-130E manufactured by Kokusan Co., Ltd.).
[0063] Such biodegradation evaluation of the entire absorbent article 1 is performed by placing the sample (absorbent article 1) in an evaluation device having a space large enough to place the entire sample therein, and irradiating the sample with ultraviolet light under the same test conditions as those of the ultraviolet accelerated weathering device described above. Note that the sample may be rotated every predetermined period (e.g., every 3 days) to ensure uniformity of ultraviolet light irradiation on the sample.
[0064] (Action and effect) In the absorbent article 1, the first portion, which is at least a part of the outer exposed portion (in this embodiment, the entire outer nonwoven fabric 12b), is made of a polyolefin resin that does not have biodegradability by itself, and this makes it possible to reduce the cost of the absorbent article 1 and ensure the material strength of the first portion, compared to when the first portion is made of a biodegradable resin such as a polylactic acid resin. In addition, the absorbent article 1 after use is usually discarded in a state in which the outer exposed portion is exposed to the outside and the inner sheet member 11 and the absorbent body 13 are rolled up inward (i.e., in a folded state as shown in FIG. 4(B)). In the absorbent article 1, an additive that promotes biodegradation is contained in the first portion so as to satisfy the above-mentioned biodegradation conditions, and therefore the first portion of the absorbent article 1 after disposal can be decomposed early. As a result, microorganisms can be permeated early into the absorbent article 1 after disposal, and therefore the biodegradation of the entire absorbent article 1 can be promoted. Therefore, according to the absorbent article 1, it is possible to ensure the necessary material strength while suppressing an increase in cost, and to promote the biodegradation of the absorbent article 1 after disposal.
[0065] The additives blended in the first portion preferably contain the above-mentioned (f) phenol-based antioxidant stabilizer. As the phenol-based antioxidant stabilizer, known antioxidant stabilizers (e.g., Irganox 1076, Irganox 1010, etc.) can be used. Such phenol-based antioxidant stabilizers have the function of suppressing the biodegradation promotion function of the additive for a certain period of time, delaying the start of decomposition, and extending the shelf life of the product. Therefore, according to the above-mentioned configuration, the start time of biodegradation can be appropriately adjusted so that decomposition starts after the expected shelf life of the product has elapsed. Note that, from the viewpoint of suitably exerting the above-mentioned function of suppressing biodegradation, the content of the phenol-based antioxidant stabilizer in the additive is preferably set to 0.02 to 0.15% by weight with respect to the total weight of the polyolefin resin and the additive.
[0066] As described above, in this embodiment, the additive for promoting biodegradation is added to two sheets (the outer nonwoven fabric 12b and the leakproof sheet 12a). Here, the content (wt%) of the phenolic antioxidant stabilizer in each sheet may be greater in the sheet disposed on the outside. That is, in this embodiment, the content (wt%) of the phenolic antioxidant stabilizer in the outer nonwoven fabric 12b may be greater than the content (wt%) of the phenolic antioxidant stabilizer in the leakproof sheet 12a. In this way, the content of the phenolic antioxidant stabilizer is increased in the portion (outer portion) that is more likely to come into contact with the outside air under normal circumstances (during storage or use) to increase the degree of inhibition of biodegradation, thereby making it possible to appropriately prevent unexpected promotion of biodegradation in the outer portion (outer nonwoven fabric 12b) of the outer sheet member 12. More specifically, the biodegradation of the outer nonwoven fabric 12b can be prevented from proceeding much faster than the biodegradation of the leakproof sheet 12a, and the biodegradation of the outer nonwoven fabric 12b and the leakproof sheet 12a can be adjusted so as to proceed in a well-balanced manner.
[0067] The tensile strength of the first portion (outer nonwoven fabric 12b) is preferably 0.3 N / mm 2 Above CD (tensile strength in the width direction W): 0.07N / mm 2That is all. The tensile strength is measured by the following method. That is, a test piece having a length (length in the front-rear direction L) of about 160 mm and a width (length in the width direction W) of 25 mm is taken, and the test piece is pulled in the vertical direction at a pulling speed of 100 mm / min and a chuck distance of 100 mm using a tensile tester (for example, a constant-speed extension type tensile tester) until the test piece breaks. The maximum force applied to the test piece when the test piece breaks is obtained as the tensile strength value. Note that, if the test piece cannot be secured to have a sufficient length or width, the length and width of the test piece and the chuck distance may be changed arbitrarily. In addition, the first part has durability such that no fuzzing occurs after 50 reciprocating rubs under a load of 200 g in a surface rub fastness test. The abrasion resistance of such a first part is measured using a dyed material rub fastness tester based on JIS L0849. That is, a test piece cut to a width (length in the width direction W) of 300 mm and a length (length in the front-rear direction L) of 150 mm is taken and attached to the stage of the testing machine with cellophane tape. Cloth tape is attached to the friction surface of the friction element, and the friction element is placed on the center surface of the test piece. The number of reciprocations is set to 50, and the evaluation is started. After completion, the test piece is removed from the stage, and the surface condition is observed. With the above configuration, the material strength of the first portion can be suitably secured, and therefore the stability of the absorbent article 1 against deformation and damage during normal times (storage or use) can be improved.
[0068] The first portion (outer nonwoven fabric 12b) preferably has a thickness of 0.1 mm or more and 2.0 mm or less. If the thickness of the first portion is thinner than 0.1 mm, it is likely to become uncomfortable to the touch. Also, if the thickness of the first portion is thicker than 2.0 mm, the large thickness will slow down the decomposition rate of the first portion. Therefore, by setting the thickness of the first portion in the range of 0.1 mm or more and 2.0 mm or less, it is possible to suppress a decrease in the decomposition rate while maintaining a good feel to the touch. From the viewpoint of improving the decomposition rate of the first portion, the thickness of the first portion is preferably set to 0.25 mm or less.
[0069] The ultraviolet transmittance of the first portion (outer nonwoven fabric 12b) is preferably 15% or more. Whether or not the above condition is satisfied can be confirmed, for example, as follows. For example, ultraviolet rays of several wavelengths in the wavelength range of 280 to 400 nm are irradiated onto a sample, and the ultraviolet transmittance of each wavelength is measured using a spectrophotometer. The minimum value of the ultraviolet transmittance of each wavelength is 15% or more. According to the above configuration, ultraviolet rays that may be a factor in promoting biodegradation of members (in this embodiment, the leakproof sheet 12a, the absorber 13, the inner sheet member 11, etc.) inside the first portion of the absorbent article 1 can be suitably guided to the members inside. As a result, the start of biodegradation inside the absorbent article 1 can be accelerated, and the decomposition speed of the entire absorbent article 1 can be improved.
[0070] The first portion (outer nonwoven fabric 12b) and the leakproof sheet 12a are preferably configured so that the air permeability of the first portion measured by a Frazier test is higher than the air permeability of the leakproof sheet 12a measured by a Frazier test. The Frazier test is a test to determine the air permeability (1 cm) based on the test method (Fragile method) specified in the air permeability test (JIS L 1096). 2 This is a test to measure the density (a numerical value indicating how much air passes through an area of the first portion in one second). In addition, the first portion and the leakproof sheet 12a are preferably configured so that the density of the first portion is lower than the density of the leakproof sheet 12a. The density is measured, for example, as follows. That is, the thickness of the first portion is measured using a thickness gauge, the dimensions (area) of the first portion are measured using a ruler, and the mass of the first portion is measured using an electronic balance. Finally, the "mass / volume (=thickness x area)" of the first portion is calculated as the density. According to the above configuration, water, oxygen, etc., which may be factors promoting the biodegradation of the leakproof sheet 12a, can be suitably guided to the leakproof sheet 12a by passing through the first portion. As a result, the start of biodegradation of the inside of the absorbent article 1 (the leakproof sheet 12a) can be accelerated, and the decomposition speed of the entire absorbent article 1 can be improved.
[0071] The air permeability of the first portion (outer nonwoven fabric 12b) measured by the Frazier test is preferably 100 cm 3 / (cm 2 ·s) or more than 700cm 3 / (cm 2 The air permeability is 700 cm 3 / (cm 2 By keeping the air permeability to 100 cm or less, the function of the absorbent article 1 (for example, preventing leakage of body excrement from the first portion) is prevented from being impaired, and the air permeability is kept at 100 cm or less. 3 / (cm 2 By making the first portion 101·s or more, water, oxygen, and the like, which may be factors promoting biodegradation, can be properly guided through the first portion to the inside of the absorbent article 1. As a result, the start of biodegradation inside the absorbent article 1 can be accelerated, and the decomposition speed of the entire absorbent article 1 can be improved.
[0072] The density of the first portion (outer nonwoven fabric 12b) is preferably 0.02 g / m 3 More than 0.1g / m 3 The density is 0.1 g / m or less. 3 By suppressing the density to 0.02 g / m or less, it is possible to prevent the loss of the functions of the absorbent article 1 (for example, prevention of leakage of body waste from the first portion, etc.) while maintaining the density at 0.02 g / m 3 By doing so, water, oxygen, and the like, which may be factors promoting biodegradation, can be properly guided through the first portion to the inside of the absorbent article 1. As a result, the start of biodegradation inside the absorbent article 1 can be accelerated, and the decomposition speed of the entire absorbent article 1 can be improved.
[0073] Since the absorbent body 13 (absorbent core 13a) contains a biodegradable superabsorbent polymer (SAP), the first part (outer nonwoven fabric 12b) of the absorbent article 1 is biodegraded to allow microorganisms to reach the absorbent body 13, thereby allowing the absorbent body 13 to be properly biodegraded.
[0074] The biodegradation promoter of SAP contained in the absorber 13 may be the same as the biodegradation promoter of the first portion. In this embodiment, the first portion contains the additive described above, and decomposition (i.e., cleavage of carbon bonds, etc.) is initiated by each of water, oxygen, and ultraviolet light as a promoter. In this case, the SAP may be configured to initiate decomposition by the same promoter as that of the first portion (water, oxygen, and ultraviolet light in this embodiment). This configuration makes it possible to prevent a situation in which only one of the first portion and the absorber 13 (SAP) remains undecomposed in the same environment.
[0075] Alternatively, the factor promoting the biodegradation of SAP contained in the absorbent body 13 may be different from the factor promoting the biodegradation of the first portion. More specifically, the factor promoting the biodegradation of SAP contained in the absorbent body 13 may be configured to include a substance derived from excrement (e.g., urea), while the factor promoting the biodegradation of the first portion may be configured not to include a substance derived from excrement. With this configuration, the decomposition of the absorbent body 13 (superabsorbent polymer) can be started from the time when the wearer excretes excrement on the absorbent article 1, so that the period until the biodegradation of the absorbent body 13 is completed can be shortened. On the other hand, since the factor promoting the biodegradation of the first portion does not include a substance derived from excrement, it is possible to prevent the first portion from starting decomposition before the appropriate decomposition start time (i.e., the time after the absorbent article 1 is discarded) triggered by excretion processing.
[0076] In the absorbent article 1, the first portion is configured to have biodegradability by the additive, so that a portion that accounts for 90% or more of the total weight of the absorbent article 1 is configured to have biodegradability. As described above, the first portion is modified to have biodegradability by blending the additive, but the portions of the absorbent article 1 other than the first portion may be modified to have biodegradability by blending the additive like the first portion, or may be configured to have biodegradability by being formed of a material having biodegradability other than the additive. An example of a portion of the absorbent article 1 that does not have biodegradability is the elastic member 116a such as the above-mentioned rubber thread. According to the above-mentioned configuration, the biodegradation of the absorbent article 1 after disposal can be promoted more effectively.
[0077] The degree of deterioration of the leakproof sheet 12a measured by the above evaluation test (ultraviolet accelerated weather resistance test) is preferably higher than the degree of deterioration of the first portion measured by the above evaluation test. Specifically, the degrees of deterioration of the above-mentioned leakproof sheet 12a and the first portion are compared based on the magnitude of the carbonyl index value after the above evaluation test is performed. It can be said that the larger the carbonyl index value, the higher the degree of deterioration. More preferably, the content (wt%) of the additive in the leakproof sheet 12a is higher than the content (wt%) of the additive in the first portion. From the viewpoint of preventing leakage of excrement, the leakproof sheet 12a generally has a structure that is difficult to decompose. According to the above configuration, such a leakproof sheet 12a can be made to have a structure that is easily biodegradable. As a result, the decomposition speed of the entire absorbent article 1 can be improved.
[0078] In addition, the base sheet 211 of the fastening tapes 21A, 21B may contain, as the main material, a polyolefin resin that is not biodegradable by itself, similar to the outer nonwoven fabric 12b. In addition, the fastening tapes 21A, 21B may be configured to have biodegradability that satisfies the above-mentioned biodegradation conditions by blending an additive similar to that of the outer nonwoven fabric 12b. In other words, the above-mentioned first portion may contain the base sheet 211 of the fastening tapes 21A, 21B. According to the above configuration, in the absorbent article 1 after disposal, by promoting the biodegradation of the base sheet 211 of the fastening tapes 21A, 21B that functions as a fixing member for fixing the shape of the absorbent article 1 so as to maintain the folded state, the base sheet 211 can be broken or the like, and the folded state (see FIG. 4(B)) can be released to expose the inside of the absorbent article 1 to the outside. As a result, microorganisms can easily come into contact with the inner members of the absorbent article 1, and the decomposition speed of the entire absorbent article 1 can be improved.
[0079] The engagement strength between the engaging portion 212 and the outer surface (the outer surface of the outer nonwoven fabric 12b or the surface of the base sheet 211 of the other fastening tape) engaged with the engaging portion 212 after a predetermined period of time has elapsed since the start of the evaluation test (ultraviolet accelerated weather resistance test) of the first portion (here, the outer nonwoven fabric 12b or the base sheet 211 of the fastening tapes 21A and 21B) is preferably lower than the engagement strength between the engaging portion 212 and the outer surface before the evaluation test is started. The above-mentioned "predetermined period" is, for example, a period determined by the above-mentioned biodegradation conditions (i.e., 28 days from the start of biodegradation). In addition, the "engagement strength between the engaging portion 212 and the outer surface" is a value indicating the degree of engagement (difficulty in separating) between the engaging portion 212 and the outer surface of the outer nonwoven fabric 12b or the base sheet 211 with which the engaging portion 212 is engaged. The above-mentioned engagement strength is evaluated, for example, in an incubator at 40 degrees. For example, the value is measured by cutting the engagement portion 212 and the outer nonwoven fabric 12b, or the engagement portion 212 and the base sheet 211, into pieces each measuring 50 mm square, engaging them together, hanging an 800 g weight on the side of the engagement portion 212, and measuring the durability time until the weight falls.
[0080] The engagement strength acts to maintain the folded state (see FIG. 4(B)). In addition, the biodegradability (e.g., the amount of additive) of at least a part of the first part is adjusted so that the engagement strength between the engagement part 212 and the outer surface engaged with the engagement part 212 after a predetermined period of time from when the promotion of biodegradation of the first part is started is lower than the engagement strength before the evaluation test is started. That is, the material strength of the first part (including at least one of the outer nonwoven fabric 12b and the base sheet 211 of each fastening tape 21A, 21B) is reduced by biodegradation, so that the engagement strength is configured to be lower than before the biodegradation of the first part. This makes it easier for the engagement part 212 to be disengaged from the outer surface after a predetermined period of time from when the promotion of biodegradation is started, thereby increasing the possibility of releasing the folded state.
[0081] (Modification of absorbent article) Although the embodiment of the absorbent article of the present disclosure has been described above, the materials and shapes of the components of the absorbent article are not limited to those described above, and various materials and shapes can be used. In addition, some of the components included in the configurations of the above-mentioned embodiments may be changed or omitted, or other components may be added.
[0082] For example, in the above embodiment, a configuration was exemplified in which both the outer nonwoven fabric 12b and the base sheet 211 correspond to the first portion, but only one of the outer nonwoven fabric 12b and the base sheet 211 may be configured to correspond to the first portion.
[0083] The type of absorbent article is not limited to the tape-type disposable diaper exemplified in the above embodiment. FIG. 5 is a perspective view of an absorbent article 1A according to a modified example. As shown in FIG. 5, the absorbent article 1A may be a pants-type disposable diaper. The absorbent main body 10A of the absorbent article 1A is mainly different from the absorbent main body 10 of the absorbent article 1 in that it is provided with a waist opening H1 and a pair of left and right leg openings H2. The waist opening H1 is a portion through which the wearer's torso is inserted, and the pair of leg openings H2 are portions through which the wearer's left and right legs are inserted. When the absorbent article 1A is worn by a wearer, a locking portion E extending in the vertical direction is provided at the portion located on both the left and right sides of the wearer's torso. The absorbent article 1A can be unfolded like the above-mentioned tape-type absorbent article 1 (see FIGS. 1 and 2) by tearing the locking portion E after use.
[0084] The absorbent article 1A does not include the fastening tapes 21A, 21B and the target tape 30 that are included in the absorbent article 1. On the other hand, as shown in FIG. 6, a fastening tape 22 is provided in the widthwise center of the back side of the outer nonwoven fabric 12b of the absorbent article 1A to keep the absorbent article 1A in a compactly rolled folded state. In the absorbent article 1A, this fastening tape 22 functions as a fixing member for fixing the shape of the absorbent article 1A so as to keep the folded state. For example, as shown in FIG. 6(A), the absorbent article 1A is rolled up so that the inner sheet member 11 is on the inside and the back side part of the outer nonwoven fabric 12b on which the fastening tape 22 is provided is exposed to the outside, and then, as shown in FIG. 6(B), the adhesive surface of the fastening tape 22 is adhered to the outer surface of the outer nonwoven fabric 12b. This keeps the absorbent article 1A in a folded state. Although Figure 6(A) shows an example of rolling up absorbent article 1A without tearing engagement portion E, absorbent article 1A may be rolled up in the same manner as absorbent article 1 (see Figure 4(A)) after tearing engagement portion E.
[0085] The absorbent article may be a disposable absorbent pad to be attached to the inside of a worn article such as cloth underwear, or a sanitary napkin for women. When the absorbent article is a sanitary napkin, the sheet member corresponding to the outer nonwoven fabric 12b described above may be omitted, and a sheet member (film) corresponding to the leakproof sheet 12a may constitute the outermost layer of the absorbent article. In this case, the sheet member corresponding to the leakproof sheet 12a may correspond to the first portion described above.
[0086] (packaging) 7 and 8 are diagrams showing an example of a package 50 in which a plurality of absorbent articles 1 (for example, 26 pieces) are collectively housed. The package 50 includes a package sheet 51 for packaging the plurality of absorbent articles 1. The package sheet 51 is formed, for example, in the shape of a bag having a substantially rectangular parallelepiped shape when the plurality of absorbent articles 1 are housed. The package sheet 51 is made of a synthetic resin such as polyethylene, polypropylene, or polyethylene terephthalate. As an example, the package 50 may house a plurality of absorbent articles 1 in two stages as shown in FIG. 8. The housed absorbent articles 1 are folded in half so that the inner sheet member 11 is on the inside. In each stage, the plurality of absorbent articles 1 are arranged such that the outer surfaces of the outer nonwoven fabrics 12b of adjacent absorbent articles 1 are in surface contact with each other.
[0087] The oxygen permeability of the packaging sheet 51 is preferably lower than that of a first portion (e.g., the outer nonwoven fabric 12b) of the absorbent article 1. More preferably, the oxygen permeability of the packaging sheet 51 is lower than that of the leakproof sheet 12a of the absorbent article 1. The oxygen permeability is measured by gas chromatography or electrolytic sensor method based on JIS K 7126-2 or ISO15105-2.
[0088] The UV transmittance of the packaging sheet 51 is preferably lower than that of the first portion (e.g., the outer nonwoven fabric 12b) of the absorbent article 1. More preferably, the UV transmittance of the packaging sheet 51 is lower than that of the leakproof sheet 12a of the absorbent article 1. The UV transmittance for the above comparison can be obtained, for example, as follows. For example, a sample is irradiated with UV rays of several wavelengths in the wavelength range of 280 to 400 nm, and the UV transmittance of each wavelength is measured using a spectrophotometer. Then, the minimum value of the UV transmittances of each wavelength can be used as the comparison target.
[0089] The packaging sheet 51 preferably seals the internal space (i.e., the space inside the packaging sheet 51) in which the absorbent article 1 is housed. More specifically, the packaging sheet 51 does not have perforations formed therein that are generally provided for opening.
[0090] The packaging body 50 can prevent oxygen, ultraviolet rays, and the like, which may be factors promoting biodegradation, from entering the packaging body 50 when the absorbent article 1 is housed and stored in the packaging sheet 51 before use (packaged state). This can prevent the start of biodegradation of the absorbent article 1 (first part) from being accelerated, that is, the product life of the absorbent article 1 from being shorter than expected. Therefore, the packaging body 50 can suitably package the absorbent article 1 described above. The absorbent article housed in the packaging body 50 may be a pants-type absorbent article 1A, or an absorbent article other than a disposable diaper (for example, an absorbent pad, a sanitary napkin, etc.). The shape of the packaging sheet 51 may be changed depending on the type and number of absorbent articles to be housed. [Explanation of symbols]
[0091] DESCRIPTION OF THE SYMBOLS 1,1A...absorbent article, 11...inner sheet member, 12...outer sheet member, 12a...leakproof sheet (middle sheet), 12b...outer nonwoven fabric (outer exposed portion, first part), 13...absorbent body, 21A,21B...fastening tape (fixing member, outer exposed portion, first part), 22...fastening tape (fixing member, outer exposed portion, first part), 50...packaging body, 51...packaging sheet, 211...base material sheet, 212...engagement portion.
Claims
1. An absorbent article for absorbing bodily waste discharged by a wearer, comprising: an inner sheet member including one or more sheets facing the wearer's skin; an outer sheet member including one or more sheets disposed on the opposite side to the skin side of the inner sheet member; an absorbent body disposed between the inner sheet member and the outer sheet member for absorbing bodily waste of the wearer; a fixing member for fixing the shape of the absorbent article so as to maintain the folded state in which the absorbent article is folded so that the inner sheet member is enclosed inside, At least one of the outer sheet member and the fixing member has an outer exposed portion that is exposed to the outside in the folded state, a first portion which is at least a part of the outer exposed portion is configured to contain a polyolefin resin which is not biodegradable by itself; The first part contains an additive that biodegrades the polyolefin resin using at least one of oxygen, water, and ultraviolet light as an accelerating factor, and is configured to satisfy the biodegradation condition that the carbonyl index of the first part is 1 or more within 28 days from the start of the evaluation test specified in PAS9017:2020. Absorbent articles.
2. The additive comprises a phenolic antioxidant stabilizer. The absorbent article of claim 1.
3. The content of the phenol-based antioxidant stabilizer in the additive is 0.02 to 0.15% by weight based on the total weight of the polyolefin resin and the additive; The absorbent article of claim 2.
4. The outer sheet member includes a plurality of sheets, The additive is added to at least two or more sheets of the plurality of sheets, The content of the phenolic antioxidant stabilizer in each of the two or more sheets is higher in the sheet disposed on the outside. The absorbent article according to claim 2 or 3.
5. The tensile strength of the first portion is MD: 0.3 N / mm 2 or more and CD: 0.07 N / mm 2 That's all. The absorbent article of claim 1.
6. The first portion has a durability such that no fuzzing occurs when rubbed 50 times back and forth under a load of 200 g in a surface rub fastness test specified in JIS L0849. The absorbent article of claim 1.
7. The first portion has a thickness of 0.1 mm or more and 2.0 mm or less. The absorbent article of claim 1.
8. The ultraviolet transmittance of the first portion is 15% or more. The absorbent article of claim 1.
9. the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; The air permeability of the first portion measured by a Frazier test is higher than the air permeability of the intermediate sheet measured by a Frazier test. The absorbent article of claim 1.
10. the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; The density of the first portion is lower than the density of the intermediate sheet. The absorbent article of claim 1.
11. The air permeability of the first portion measured by the Frazier test is 3 / (cm 2 ・s) or more 700cm 3 / (cm 2 s) or less, The absorbent article of claim 1.
12. The density of the first portion is 0.02 g / m 3 0.1g / m or more 3 Below is the The absorbent article of claim 1.
13. The absorbent body includes a biodegradable highly absorbent polymer. The absorbent article of claim 1.
14. The biodegradation promoter of the superabsorbent polymer is the same as the biodegradation promoter of the first portion; 14. The absorbent article of claim 13.
15. The factor promoting the biodegradation of the superabsorbent polymer includes a substance derived from the excrement, The factor promoting biodegradation of the first part does not include substances derived from the excrement.
14. The absorbent article of claim 13.
16. The first portion is biodegradable due to the additive, so that a portion occupying 90% or more of the total weight of the absorbent article is configured to be biodegradable. The absorbent article of claim 1.
17. the outer sheet member has a biodegradable intermediate sheet disposed between the first portion and the absorbent body; The degree of deterioration of the intermediate sheet measured by the evaluation test is higher than the degree of deterioration of the first portion measured by the evaluation test. The absorbent article of claim 1.
18. The intermediate sheet also contains the additive, The content of the additive in the intermediate sheet is greater than the content of the additive in the first portion; 18. The absorbent article of claim 17.
19. The fixing member includes a base sheet and an engagement portion provided on a surface of the base sheet, The first portion includes the base sheet, The engagement portion is configured to be able to engage with an outer surface of the outer sheet member or the fixing member so as to maintain the folded state. The absorbent article of claim 1.
20. an engagement strength between the engagement portion and the outer surface after a predetermined period of time has elapsed since the start of the evaluation test of the first portion is lower than an engagement strength between the engagement portion and the outer surface before the start of the evaluation test; 20. The absorbent article of claim 19.
21. The biodegradation conditions further include a condition that, within 14 days from the start of the evaluation test, the number average molecular weight of the first portion is 5,000 or less, the z-average molecular weight of the first portion is 30,000 or less, and the loss of the weight average molecular weight of the first portion is 90% or more. The absorbent article of claim 1.
22. A package for packaging a plurality of absorbent articles according to claim 1, A packaging sheet for packaging a plurality of the absorbent articles is provided, The oxygen permeability of the packaging sheet is lower than the oxygen permeability of the first portion. packaging.
23. The outer sheet member of the absorbent article has an intermediate sheet disposed between the first portion and the absorbent body, The oxygen permeability of the packaging sheet is lower than the oxygen permeability of the intermediate sheet.
23. The package of claim 22.
24. A package for packaging a plurality of absorbent articles according to claim 1, A packaging sheet for packaging a plurality of the absorbent articles is provided, The packaging sheet has an ultraviolet transmittance lower than an ultraviolet transmittance of the first portion. packaging.
25. The outer sheet member of the absorbent article has an intermediate sheet disposed between the first portion and the absorbent body, The packaging sheet has an ultraviolet ray transmittance lower than that of the intermediate sheet.
25. The package of claim 24.
26. A package for packaging a plurality of absorbent articles according to claim 1, A packaging sheet for packaging a plurality of the absorbent articles is provided, The packaging sheet seals an internal space in which the absorbent article is contained. packaging.
Citation Information
Patent Citations
Disposable diaper
JP2020195428A