Mechanical joining of advanced high strength steels
Laser-assisted and resistive heating systems effectively join AHSS sheets by controlling HAZ temperature and clamping forces, addressing joint failure issues and enhancing manufacturing efficiency.
Patent Information
- Application Number
- JP2024506515
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-08-02
- Filing Date
- 2022-08-03
- Publication Date
- 2024-10-02
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Advanced high-strength steels (AHSS) with high tensile strengths and low ductility pose challenges in traditional mechanical joining methods, leading to joint failures and inefficiencies in automotive applications.
A system utilizing laser-assisted thermal bonding and resistive heating methods to control the heat-affected zone (HAZ) temperature, applying variable clamping forces and electrical currents to form mechanical bonds in AHSS stacks, ensuring optimal bonding without melting the steel.
Enables efficient and reliable mechanical joining of AHSS sheets with maintained strength and ductility, reducing joint failure risks and improving automotive manufacturing efficiency.
Smart Images

Figure 2024535669000001_ABST
Abstract
Description
[Technical field]
[0001] Cross-reference to related applications This application claims priority to U.S. Patent Application No. 17 / 878,993, filed August 2, 2022, which claims the benefit of U.S. Provisional Application No. 63 / 228,726, filed August 3, 2021, the disclosures of which are incorporated herein by reference in their entireties.
[0002] Various embodiments herein relate to the mechanical joining of advanced high strength steels (AHSS). [Background technology]
[0003] U.S. Patent 9,815,109 B2 to Savoy et al., issued to Utica Enterprises, Inc. on November 14, 2017, discloses an apparatus and method for mechanically joining advanced high strength steels. Summary of the Invention
[0004] According to one embodiment, a method applies a variable clamping force to a stack of sheet metal sections that is heated to an optimal mechanical bonding temperature to form a mechanical bond with advanced high strength steels while maintaining its strength and material properties.
[0005] According to another embodiment, a method clamps a stack of sheet metal sections, at least in part made of advanced high strength steel. The stack is heated to a temperature below the melting temperature and mechanically joined together. The temperature of the joining area, known as the heat affected zone (HAZ) portion of the stack, is controlled and monitored during heating.
[0006] According to another embodiment, a tool assembly includes a pair of clamping surfaces for clamping a stack of sheet metal sections including at least a portion of advanced high strength steel, and a pair of electrodes for applying pressure and electrical current to the stack to heat the stack and form a mechanical bond to bond the stack together.
[0007] According to another embodiment, a system is provided that includes a tool assembly for clamping a stack of sheet metal sections, the stack including at least a portion of an advanced advanced steel. An electrode arrangement is provided for heating the stack to a predetermined temperature and providing optimal ductility to the stack to form a mechanical bond. A controller is in electrical communication with the tool assembly and monitors a bond temperature in a heat affected zone of the stack.
[0008] According to a further embodiment, the tool assembly includes a laser assembly that heats the stack to an optimum temperature to form the mechanical bond.
[0009] According to another embodiment, an assembly includes at least a portion of advanced high strength steel having a protective coating thereon, and a metal component is mechanically joined to at least a portion of the advanced high strength steel. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a schematic diagram of an advanced high strength steel mechanical joining system, according to one embodiment. [Diagram 2] FIG. 2 is a schematic diagram of an advanced high strength steel mechanical joining system in another embodiment. [Diagram 3] FIG. 3 is a side view of an advanced high strength steel mechanical joining tool assembly that may employ a C-frame and laser heating in another embodiment. [Figure 4] FIG. 4 is a side view of an advanced high strength steel mechanical joining tool assembly in another embodiment. [Diagram 5] FIG. 5 is a partial cross-sectional view of a tool assembly during a heating operation for mechanically joining advanced high strength steels in another embodiment. [Figure 6] FIG. 6 is an enlarged schematic view of the heat affected zone from the tool assembly of FIG. [Figure 7]FIG. 7 is a graph of a resistive heating cycle of a bonding operation according to one embodiment. [Figure 8] Figure 8 is a common graph (also known as a banana chart) showing typical tensile strength and ductility for various grades of steel plate, including advanced high strength steels. [Figure 9] FIG. 9 is an exploded perspective view of an advanced high strength steel mechanical joining tool assembly in another embodiment. [Figure 10] 10 is a top view of a portion of the tool assembly of FIG. [Figure 11] FIG. 11 is a cross-sectional view of the tool assembly taken along section line 11-11 of FIG. [Figure 12] 12 is an exploded side view of the tool assembly of FIG. [Figure 13] FIG. 13 is a top view of the locking mechanism of the tool assembly of FIG. 9, shown in an unlocked state. [Figure 14] FIG. 14 is an enlarged plan view showing a part of the locking mechanism of FIG. [Figure 15] FIG. 15 is a top view of the locking mechanism of FIG. 13, shown in a locked state. [Figure 16] FIG. 16 is an enlarged plan view of a portion of the locking mechanism shown in FIG. [Figure 17] FIG. 17 is an exploded perspective view of the locking mechanism of FIG. 13, shown in an unlocked state. [Figure 18] FIG. 18 is an exploded perspective view of the locking mechanism of FIG. 13, shown in a locked state. [Figure 19] FIG. 19 is a graph of the heating operation in one embodiment. [Figure 20] FIG. 20 is a graph of the heating operation in another embodiment. [Figure 21] FIG. 21 is a graph of the heating operation in another embodiment. [Figure 22] FIG. 22 is a perspective view of a tool assembly in another embodiment. [Diagram 23]23 is a partial cross-sectional view of the tool assembly of FIG. 22 in a retracted position. [Figure 24] FIG. 24 is a partial cross-sectional view of the tool assembly of FIG. 22 in a heating position. [Diagram 25] FIG. 25 is a partial cross-sectional view of the tool assembly of FIG. 22 in an assembled position. [Figure 26] FIG. 26 illustrates a portion of an apparatus in preparation for clinching a first sheet portion, which is an advanced high strength steel, and a second sheet portion, which is a metal, for a mechanical joint. [Figure 27] FIG. 27 shows an intermediate stage of joining after the punch has made its initial downward movement to clinch the sheet portions together. [Figure 28] FIG. 28 shows the downward movement of the punch completing the mechanical interlocking of the sheet portions and prior to the upward movement of the punch for another cycle. [Figure 29] FIG. 29 is a view similar to FIG. 28 showing the sheet sections after they have been mechanically joined by the clinch rivet die and the clinch rivet moved by the rivet ram. [Diagram 30] FIG. 30 is a view similar to FIG. 29 showing a full punch rivet die and multiple sheet portions after they have been mechanically joined by a full punch rivet moved by a rivet ram. [Diagram 31] FIG. 31 is a view similar to FIGS. 29 and 30 showing multiple sheet portions after they have been mechanically joined together by self-piercing rivets moved by a rivet ram and backed up by a self-piercing rivet die. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Where necessary, detailed embodiments of the present invention are disclosed herein, but it should be understood that the disclosed embodiments are merely exemplary of the present invention, which may be embodied in various alternative forms. The figures are not necessarily to scale, and some features may be exaggerated or minimized to show details of specific components. Therefore, specific structural and functional details disclosed herein should not be construed as limiting, but merely as a representative basis for teaching those skilled in the art how to employ the present invention in various ways.
[0012] The term controller may be provided as one or more controllers or control modules for various components and systems. Controllers and control systems may include any number of controllers, may be integrated into a single controller, or may comprise various modules. Some or all of the multiple controllers may be connected by a controller area network (CAN) or other system. It is recognized that any controller, circuit, or other electrical device disclosed herein may include any number of microprocessors, integrated circuits, memory devices (e.g., FLASH, random access memory (RAM), read-only memory (ROM), electrically programmable read-only memory (EPROM), electrically erasable programmable read-only memory (EEPROM), or other suitable variations thereof), and software that cooperate with each other to perform the operations disclosed herein. Additionally, any one or more of the electrical devices disclosed herein may be configured to execute a computer program embodied in a non-transitory computer-readable medium programmed to perform any number of functions as disclosed herein.
[0013] Recent advances in steel materials offer advanced high-strength steel (AHSS) grades with tensile strengths ranging from 700 megapascals (MPa) to over 2,000 megapascals. Continuing advances in AHSS include high-strength steels with improved ductility and energy absorption capabilities. As shown in Figure 8, AHSS are stronger and stiffer than traditional steels, enabling higher-strength, lighter-weight steel plate materials in automotive applications that provide improved occupant safety and improved fuel economy compared to traditional steels. However, at tensile strengths of 980 megapascals and above, the hardness and ductility of this type of sheet steel material makes it difficult to form mechanical joints using joining methods, systems, and tool assemblies traditionally utilized to mechanically join conventional steel stacks, such as those in vehicle assemblies.
[0014] AHSS are particularly useful for use in vehicle body manufacturing, for example, body-in-white (BIW) components, crash energy absorption, crash protection, and passenger area components. AHSS provide high strength while using thinner gauges, resulting in lightweight structures that increase the energy efficiency of vehicles while having exceptional strength and manufacturability. However, these hard advanced high strength steels are not ductile enough to allow for mechanical joining. For example, resistance spot welding some AHSS can result in undesirable resistance spot weld joints and joint failure, especially in hot stamp press hardened steels like MnB+HF steels.
[0015] 1 illustrates a system 100 for mechanically bonding an AHSS, according to one embodiment. In the illustrated embodiment, the system 100 is a laser assisted thermal bonding system 100. The bonding system 100 includes a flexible automation, such as an industrial robot 102, in electrical communication with an integrator control board or controller 104. The controller 104 may be in electrical communication with a mainline control board 106.
[0016] The joining system 100 includes an end effector 108 for mechanical articulation by an industrial robot 102. The depicted end effector 108 is an arm tool assembly 108 with a Class 1 laser-safe end, shown with a generic clinch joining system that mechanically joins an AHSS by heating a stack of material (including at least one AHSS sheet metal section) with a laser and clinching or riveting the stack. The end effector 108 may be interchangeable with another end effector 110. The end effector 110 is an arm tool assembly 110 with a Class 1 laser-safe end, shown with a generic riveting system 110 that mechanically joins an AHSS by heating a stack of material with a laser and riveting the stack. Each of the end effectors 108, 110 is connected to the controller 104 by power and communication lines 112, 114 for controlling the electrical actuators and positioners of the end effectors 108, 110. Embodiments of the end effectors 108, 110b may employ the teachings of U.S. Patent No. US 9,815,109 B2 to Savoy et al., issued Nov. 14, 2017 to Utica Enterprises, Inc., which is incorporated by reference in its entirety. Other mechanical joining processes may be contemplated for use with the laser heating system 100.
[0017] The joining system 100 includes an integrated laser system 116 with a closed loop chiller. The laser system 116 is connected to the control board 104 by a power line 118 and a communication line 120. The laser system 116 provides a laser beam fiber supply cable 122 and a cooling circuit 124 to each tool 108, 110. The controller 104 communicates with the robot 102, the end effectors 108, 110, and the laser system 116 so that the robot presents the end effectors 108, 110 to a stack of sheet metal portions. The laser system 116 heats the stack with the laser-safe end effectors 108, 110. The end effectors 108, 110 then mechanically join the stack, forming a mechanical interlock. The joining system 100 may employ the teachings of U.S. Patent No. US 9,815,109 B2 to Savoy et al. Alternatively, the pedestal fixture 170 may communicate with the control panel 104 and integrated laser system 116 to perform the heating and mechanical bonding operations without the use of the industrial robot 102 .
[0018] 2 illustrates a system 130 for mechanically bonding an AHSS according to another embodiment. In the illustrated embodiment, the system 130 is a resistive thermal bonding system 130. The bonding system 130 includes an industrial robot 132 in electrical communication with an integrated control and power distribution panel, or controller 134. The controller 134 may be in electrical communication with the mainline control board 106, as in the previous embodiment.
[0019] The joining system 130 includes an end effector 136 for mechanical articulation by the industrial robot 132. The depicted end effector 136 is a thermal joining end of an arm tool assembly 136 and is shown in a typical clinch joining system where an electrode assembly is used to heat and mechanically join a material stack including at least one AHSS sheet metal section. The end effector 136 may also be a riveting end of the arm tool assembly 136. The end effector 136 may be interchangeable with other end effectors. The end effector 136 is connected via power and communication lines 138, 140 to a controller 134 which controls the electrical actuators and positioners of the end effector 136, and the controller 134 is in communication with a timer 142 via communication line 128.
[0020] The joining system 130 includes a timer 142 in electrical communication with an electrode assembly on the end effector 136. A controller 134 communicates with the robot 132, the end effector 136, and the timer 142 to cause the robot 132 to present the end effector 136 to a stack of sheet metal sections. The timer 142 directs electrical current at the heat affected zone (HAZ) joining area at the end effector 136 to heat the stack while monitoring the temperature of the HAZ in the stack. The end effector 136 then mechanically joins the stack. The joining system 130 may employ the teachings of U.S. Patent No. US 9,815,109 B2 to Savoy et al. Alternatively, a pedestal fixture 170 may communicate with the controller 134 and timer 142 to perform the heating and mechanical joining operations without utilizing an industrial robot 132.
[0021] FIG. 3 shows the end effector 108, 110 or 136 in more detail. According to one embodiment, the end effector 136 is a robotic laser assisted clinch and riveting end of the tool assembly 136. The end effector 136 includes a mounting bracket 144 that is attached to a mounting plate at the end of the arm of the industrial robot 132. The bracket 144 is connected to a frame 146, which may be a welded piece to support the functional components of the end effector 136. The frame 146 may be formed in a C-shape, often referred to as a C-frame, and by design, contains all the forces that occur during the mechanical joining operation. The end effector 136 includes an actuator 148 for performing the joining operation, such as clinching or riveting. In the illustrated embodiment, the actuator 148 is a servo driver motor 148. Other actuators, such as pneumatic, hydraulic, etc., may also be applied. The servo actuator 148 is spaced from the bracket 144 on the frame 146 to reach and access the stack.
[0022] A laser collimator 150 is mounted to the frame 146 and includes focusing and collimating optics to generate a coherent laser beam 152. The laser system 116 is utilized to generate the laser beam 152 that illuminates the HAZ of the stack. The laser beam 152 is precisely directed through and safely contained within the C-frame 146. The frame 146 may have recesses to provide a safe path for the laser beam 152. The frame 146 includes a high speed pyrometer and a fixed laser beam bender 154 that safely guide the laser beam 152 through the frame 146. An adjustable laser beam bender 156 is mounted to the frame 146 and spaced from the bender 154 to precisely redirect the laser beam 152 within the HAZ of the stack that is being heated to form the mechanical bond.
[0023] The end effector 136 includes a mechanical joining tool 158 supported on the frame 146 and exposed to process a stack of materials. The tool 158 is utilized to contact the stack and completely seal the laser beam 152 on the stack to create a heat affected zone (HAZ) optimized in that situation. The tool 158 faces away from the output end of the actuator 148 and cooperates with the actuator 148 to cooperatively provide the joining action. A cooling device may be provided at the output end of the actuator 148 and / or the tool 158 to insulate the end effector 136 or the tool from excessive heat during operation. The end effector 136 provides a laser integrated joining assembly that operates with the industrial robot 132, where the laser beam 152 is housed to be classified as Class I laser safe and does not require additional laser safety equipment such as a safety booth or safety merimeter.
[0024] 4, the pedestal fixture 170 is a stand-alone fixture that receives parts / assemblies to be processed robotically or manually by an operator. The pedestal fixture 170 is sized to be supported by a support surface, such as a floor, or other equipment, such as a press. It may also be configured to support one of the tools, such as an actuator 172 having a tool 174, as shown. The tool 174 is a riveting tool system that mechanically joins the AHSS by heating a stack of materials with a laser and then riveting them. The pedestal fixture 170 may be utilized in combination with one of the other tools 108, 136 for mechanical joining of the AHSS. The pedestal fixture 170 supports the tool 174 in an orientation relative to an underlying support surface or other automation, such as a press. The pedestal fixture 170 is in electrical communication with a control board 176, which may be in communication with one of the control boards 104, 106, 134 of the previously described embodiments. Alternatively, the controller 176 may be a module integrated into one of the control boards 104 , 106 , 134 .
[0025] 5 shows a tool assembly 20 for joining AHSS, which may be provided to the end effectors 108, 110, 136, 170 as the fixture 158 and output tool assembly 162 of the previous embodiment. The tool assembly 20 includes a pair of subassemblies 22, 24, which are, in turn, referred to as a first subassembly 22 and a second subassembly 24. The tool assembly 20 may be provided to an automated device, such as a press or fixture, or a robot, which may present the pair of tool subassemblies 22, 24 to workpieces for joining the workpieces.
[0026] The first tool subassembly 22 includes a housing with an electrode 28 and a clamping surface 30. Similarly, the second tool subassembly 24 includes a housing with an electrode 34 and a clamping surface 36. The electrodes 28, 34 are oriented centrally inboard with respect to their respective housings to form an optimized HAZ.
[0027] A stack of mechanically joined sheet metal material is provided, the stack of sheet metal including at least two metal layers joined by a mechanical interlock. In the illustrated embodiment, the stack includes two sheets 38, 40 of steel material pressed in contact with each other. The stack may be provided with different amounts and types of material components or sheets for different mechanical interlocks. The stack 38, 40 may be pressed in contact by automation. Each of the two sheets 38, 40 of the stack may be made of AHSS. According to another embodiment, one sheet 38, 40 of the stack may be made of AHSS and the other sheet 38, 40 may be made of another similar or dissimilar material.
[0028] The two metal sheets 38, 40 of the stack are presented in contact for a joining operation by the tool assembly 20. Although two sheets are shown, additional metal sheets may be added and heated to form a mechanical bond in the HAZ 42. A controlled force is applied to the electrodes 28, 34 to provide the correct resistance to the stack 38, 40 between the clamping faces 30, 36 of the electrodes 28, 34. The electrodes 28, 34 are the only conductive material in contact with the sheets 38, 40 during the heating operation. A controlled current 44 passes through the metal sheets 38, 40 through the electrodes 28, 34, generating heat by resistance and mechanically joining the sheets 38, 40 in the HAZ 42, forming a joint located in the HAZ 42 of the clamping faces 30, 36 in the electrode current path. The HAZ 42 is the area across multiple layers of the stack that is subjected to a heat treatment to perform the joining operation on the stack. A mechanical bond is then formed in the HAZ 42.
[0029] The clamping surfaces 30, 36 of the electrodes 28, 34 are clamped together by an actuator 148. The actuator 148 and controller 104 provide control to adjust or maintain the clamping force during the heating cycle. The servo driver 148, with a drive capacity of, for example, 80 kilonewtons, is light enough to allow efficient robotic articulation while handling all applicable clamping and mechanical joining requirements. By using a controllable actuator 148, the clamping force is not limited by spring return as in typical mechanical joining tools, for example, stripper springs to assist in tool retraction. Various mechanical joining stacks have different clamping and joining force requirements and the actuator 148 is controlled by the controller 64, 104 to provide the correct clamping and joining force for the associated stack of material being processed.
[0030] The second tool subassembly 24 may include a laser beam 46 within the housing. The laser beam 46 may also be utilized to heat the material sheets 38, 40. The addition of the laser beam 46 increases the efficiency of heating the sheets 38, 40 when used in combination with the electrodes 28, 34, which may result in a shorter process time for the thermal bonding operation or alternatively heat and improve cycle time. The laser beam 46 may employ the teachings of U.S. Patent No. US 9,815,109 B2 to Savoy et al. The laser beam 46 irradiates the first sheet 40 to heat the first and second sheets 38, 40. The second sheet 38 may be an incident sheet or a top sheet 38 accessible by the laser subassembly 136. The first sheet 40 may be the top sheet 38 or any of the sheets 38, 40.
[0031] The tool assembly 20 includes at least one sensor 48 for monitoring the temperature of the HAZ 42 to provide the correct bonding temperature in the stack depending on the heating area. The sensor 48 may be provided in the first tool subassembly 22 or the second tool subassembly 24. According to another embodiment, a sensor 48 may be provided in each tool subassembly 22, 24 to monitor the temperature of the HAZ 42 in the first sheet 40 and the second sheet 38. The sensor 48 may be, for example, an infrared pyrometer or the like.
[0032] The sheets 38, 40 are shown diagrammatically in FIG. 6. Each sheet 38, 40 includes a primary layer 50, 52 of steel. Each sheet 38, 40 is coated on its exposed surface with a protective coating layer 54, 56, 58, 60, respectively. The coating layers 54, 56, 58, 60 protect the steel layers 50, 52 from rust and other contamination. The coating layers 54, 56, 58, 60 may be formed of aluminum silicon layers (Al-Si having about 90% aluminum and about 10% silicon) on 22MnB5 steel, zinc alloys, or the like. The AHSS coating may be created by electrogalvanizing coating process, galvanizing coating process, hot dip coating process, or the like during hot forming or other protective coating process.
[0033] 5, the tool assembly 20 is provided with a metal joining and heating system 62 that includes a controller 64. The controller 64 is in electrical communication with the sensor 48 to receive temperature measurements and monitor the temperature of the HAZ 42. The controller 64 also communicates with a timer 142 to regulate the current through the electrodes 28, 34 to control the temperature of the HAZ 42.
[0034] The coating layers 54, 56, 58, 60 may contaminate the steel 38, 40 at the joint, which may cause liquid metal embrittlement (LME) and cracking of the joint, which may result in failure of the joint. The coating layers 54, 56, 58, 60 may have a melting point lower than the melting point of the steel. One way to avoid contamination of the coating layers 54, 56, 58, 60 at the joint is to heat the HAZ 42 to a temperature that is optimal for the particular joint application. According to one embodiment, to protect the coating layers 54, 56, 58, 60 at the HAZ 42, the HAZ 42 is heated to a temperature that is close to the melting temperature of the coating layers 54, 56, 58, 60. For example, the coating layers 54, 56, 58, 60 may be formed from zinc and heated to a temperature below the melting temperature of zinc, e.g., below 420°C. The coating layers 54, 56, 58, 60 are maintained on the stacks 38, 40 to avoid corrosion of the stacks 38, 40 after the bonding operation is completed. The intermediate coatings 56, 58 may be retained in the joint to avoid LME. The heating and bonding operations are performed with a cycle time that is fast enough to maintain the protection of the coatings 54, 56, 58, 60.
[0035] The HAZ 42 is heated to a temperature below the melting temperature of the steel to perform a thermal joining operation such as clinching, self-piercing riveting, or other fastening operation as disclosed in U.S. Patent No. US 9,815,109 B2 to Savoy et al. Alternatively, a flow screw may be attached to the joint as disclosed in U.S. Patent Application 17 / 121,980 to Savoy et al., filed December 15, 2020, which is incorporated herein by reference in its entirety. According to another embodiment, one of the metal sheets 38 or 40 may be attached to a clinch nut as disclosed in U.S. Patent Application 17 / 121,980 to Savoy et al., published September 6, 2018 (Utica Enterprises, Inc., which is incorporated herein by reference in its entirety).
[0036] The variables of clamping force, current amperage, current run time, and laser run time may all be adjusted together or separately to arrive at an optimized process window for the particular joining operation being performed. The sensor 48 monitors the HAZ temperature to ensure that the temperature does not cause excessive damage to the material composition or microstructure. The optimum mechanical joining temperature is below the melting temperature of the steel 38, 40. For example, the laser or current may be turned on and off during the heating operation to control the temperature or to form an optimum HAZ of one or more sheets in the stack 38, 40.
[0037] FIG. 7 is an example schematic of a resistive heating sequence according to one embodiment. In FIG. 7, force and current are graphed over time. At the initial squeeze time in Zone I, the electrodes 28, 34 are clamped onto the stack 38, 40 and the laser beam 46 and current through the electrodes 28, 34 is initiated. The initial squeeze time may take six or more cycles of 1 second to complete this stage. The laser beam 46 and / or electrodes heat the stack 38, 40 up to temperature in approximately 30-75 cycles depending on the thickness of the stack and the grade of the AHSS steel.
[0038] During the heating cycle, the required clamping force is controlled. According to one embodiment, the electrode current may be increased, pulsed or decreased. In this example, the laser beam 46 and electrodes 28, 34 are powered for a variable duration and then turned off. If the temperature indicated by the sensor 48 drops below a certain optimum HAZ temperature, the electrodes 28, 34 may be pulsed. The current to the electrodes 28, 34 is then maintained or pulsed until the sensor 48 reading reaches the bonding temperature of the HAZ 42. The amount of current pulse may be used to control the current level and temperature for the bonding operation, maintaining the bonding temperature controlled by the controller and timer interface. The clamping and heating cycle time is estimated to be 30-75 cycles, which is 0.5-1.25 seconds.
[0039] According to another embodiment, the current may be increased and then maintained during Zone II. A controlled heating operation maintains the optimum joining temperature for the material in the HAZ 42. The temperature is controlled by a controller and timer to vary the current level and duration of the heating operation.
[0040] The bonding operation in Zone III is performed within the temperature range of the process window. However, rapid heating and subsequent cooling can cause the temperature to change during the bonding operation. Therefore, the bonding operation is calculated to occur while the stack temperature is decreasing within the optimal bonding temperature range.
[0041] In a third time range in Zone III, a quench sequence occurs. The mechanical bond is formed at an optimum bonding temperature determined for each particular material combination required to complete the mechanical bonding operation. The heat only operation may be about 60 cycles or about 1 second.
[0042] The heating cycle of Zone II in FIG. 7 shows a rapid temperature rise in a relatively short period of time. It is difficult to control the heating of the metal at such high temperatures and in such short intervals while avoiding the melting temperature of the stack 38, 40 in the HAZ 42. By varying the current or laser in Heating Zone II, the energy can be increased or decreased to stabilize the heating and maintain the appropriate temperature within the range of optimal mechanical bonding for the particular stack. By varying the energy, an even distribution of heat can be created without exceeding the critical temperature (e.g., melting temperature) of the steel stack in the HAZ 42. By monitoring the temperature in Heating Zone II, the temperature can be controlled and maintained to reach the optimal temperature without exceeding the melting temperature of the steel in the stack. By avoiding the molten steel layer 38, 40, the strength and microstructure of the steel layer 38, 40 remains within the typical strength of the AHSS in the graph of FIG. 8.
[0043] To reduce the cost of the tool assembly 20, the laser beam 46 may be omitted, in which case the bonding operation is performed solely by controlled currents to the electrodes 28, 34.
[0044] Figure 8 is a graph showing the tensile strength and ductility of various grades of steel sheets that are particularly desirable in automotive manufacturing. This graph shows the evolution of steel in the industry and is often referred to as the banana chart. Ductility is shown as a percentage of elongation. Conventional steels, such as interstitial-free (IF) steels, mild steels, interstitial-free high-strength (IFHS) steels, bake-hardenable (BH) steels, carbon-manganese (CMn) steels, high-strength low-alloy (HSLA) steels, and ferritic-bainite (FB) steels, have tensile strengths below 1,000 MPa and ductility between 60% and less than 10%.
[0045] The development of AHSS has resulted in a range of tensile strengths that are significantly higher than conventional steels. Twist-induced plasticity (TWIP) steels are said to have 50% to 70% higher ductility than AHSS grades in the tensile strength range up to at least 1,400 megapascals.
[0046] Martensite / hot stamped (MART) steels have low ductility, less than 10%, and tensile strengths in excess of 2,000 MPa. Manganese-boron hot formed (MnB+HF) steels also have low ductility, less than 10%, and tensile strengths can exceed 1,800 MPa. Extreme tensile strengths are available in martensite / hot stamped and manganese-boron hot formed steels, but the low ductility means that these materials cannot typically be mechanically joined without improving the ductility of the material.
[0047] Dual phase (DP) and multi-phase (CP) stainless steels offer up to 30% ductility and up to 1,400 MPa tensile strength. Transformation induced plasticity (TRIP) steels offer less than 40% ductility and ultimate tensile strength less than 1,300 MPa.
[0048] To optimize the ductility of AHSS used in automotive manufacturing, the steel industry is developing third generation AHSS with higher / enhanced ductility that is approaching that of conventional steels. Third generation AHSS have tensile strengths of 1700 megapascals and above. The steel industry is developing third generation AHSS steel grades that will increase ductility by 40% or more and tensile strengths of 2,000 megapascals and above, thereby improving crash energy performance and reducing weight. Third generation steels are also being developed to provide a material that can be conventionally pressed without the need for hot forming in a metal pressing process.
[0049] The flexibility of the tool assembly 20 with electrode heating allows for fast, efficient, and uniform heating through the HAZ 42 of the stack. The laser beam 46 focuses the heating energy on one surface, which requires more time to conduct heat uniformly through all layers of the stack. The reflective surface or coating of the steel sheet may also provide resistance to heating by the laser beam and electrode due to an additional protective layer. The reflective surface or coating of the steel sheet may also inhibit heating by the laser beam and electrode due to its reflective properties and composition. By monitoring the temperature of the HAZ 42, the system 100, 110, 170 can effectively and optimally heat the HAZ 42 while not melting the steel in the stack 38, 40 and maintaining the general characteristics of the microstructure of the material grade in the stack of the HAZ 42.
[0050] Maintaining the general properties of the stack in HAZ42 maximizes mechanical joint strength. Uniform strength within the joint results in a joint with the same general properties as the stack. For every specific grade of AHSS and each specific material combination in the stack, a clamping force, current, and time schedule, as shown in Figure 8, can be charted to provide mechanical joint integrity without exceeding the critical temperature of the steel while minimizing the joint cycle time.
[0051] 9-12 show a tool subassembly 200 according to another embodiment. The tool subassembly 200 can be utilized in one of the end effectors 108, 110, 136, 170 of the previous embodiments. The tool subassembly 200 is one subassembly of the electrode assembly 198. The electrode assembly 198 also includes a second tool subassembly. The first tool subassembly 200 and the second tool subassembly clamp the stack therebetween and pass a current through the stack to heat the HAZ 42. The tool subassembly 200 is connected to the actuator 148. The tool subassembly 200 includes a first body 202 and a second body 204 for holding the components of the clamp subassembly 200.
[0052] The first body 202 includes a receptacle 208 that receives an insulating bushing 206. The tool subassembly 200 includes an electrode 210. The electrode 210 includes a body 212 having an outer diameter that is received within the receptacle 208 of the second body 204. The electrode body 212 is insulated from the first body 202 by the insulating bushing 206. The electrode 210 includes a reduced diameter portion 214 that extends from an opening 216 (FIG. 11) in the second body 204. A clamping surface 218 is provided at a distal end of the electrode 210. An insulating washer 220 is provided within the receptacle 208 between the first body 202 and the axial end of the electrode body 212. Another insulating washer 222 is provided at the other axial end of the electrode body 212.
[0053] The stud 224 is connected to the electrode 210 through a slot 226 in the insulating bushing 206. The stud 224 is provided with another insulating bushing 228 (FIG. 9). A lug 230 is connected to the stud 224 by a fastener 232 to conduct electrical current to the electrode 210.
[0054] An interlock ring 234 is axially stacked on the insulating washer 222 and is connected to the insulating washer by a plurality of pins 236. A stop ring 238 is axially stacked on the interlock ring 234. A spring 240 is axially stacked on the interlock ring 234 and extends into a cavity 244 of the second body 204. A nut 242 is provided on the second body 204 and secures the second body 204 to the first body 202. A punch holder 246 covers the distal end of the second body 204. A punch 248 extends through the punch holder 246 and through the electrode 210.
[0055] The first and second bodies 202, 204 hold together the insulating bushing 206, the electrode 210, the insulating washers 220, 222, the interlock ring 234, the stop ring 238, the spring 240, and the punch 248. The interlock ring 234 and the stop ring 238 cooperate to bypass the spring 240 during the clamping operation, isolating the spring 240 from the clamping force and current. Once heating by the electrode 210 is complete, the rings 234, 238 move, allowing the driver 148 to drive the punch 248 to compress the spring 240 and perform a joining operation, such as clinching. The spring 240 then returns the punch 248.
[0056] 9-12, a shift lever 250 extends radially outward from the stop ring 238. A coupler 249 is connected to the shift lever 250. The coupler 249 is moved by an actuator 251, which may be a linear actuator. As the shift lever 250 rotates about the stop ring 238, the coupler 249 cooperates with the actuator 251 to pivot during translation. The coupler 249 also cooperates with the shift lever 250 to move along with the shift lever 250 as the coupler 249 is shifted.
[0057] Actuation and movement of the coupler 249 and shift lever 250 by the actuator 251 causes the stop ring 238 to rotate between an unlocked position (FIGS. 13, 14, 17) and a locked position (FIGS. 15, 16, 18). Referring now to FIGS. 13-18, the interlock ring 234 includes a plurality of radially arranged outwardly directed lugs 254. The stop ring 238 includes a correspondingly arranged plurality of radially inwardly directed slots 256. Each slot 256 provides clearance for one of the plurality of lugs 254. In the unlocked state of FIGS. 13, 14, and 17, the slots 256 of the stop ring 238 are aligned with the lugs 254, thereby permitting axial movement of the interlock ring 234 relative to the stop ring 238. The axial movement of the interlock ring 234 enables the driver 148 to drive the punch 248 to compress the spring 240. Similarly, axial movement of the interlock ring 234 allows the spring 240 to expand, thereby assisting in the retraction of the punch 248 .
[0058] When the stop ring 238 is shifted to rotate out of phase with the interlock ring 234, the punch 248 of the clamp subassembly 200 is locked. In the locked state shown in Figures 15, 16 and 18, the slots 256 of the stop ring 238 are not aligned with the lugs 254 of the interlock ring 234. In this position, the stop ring 238 blocks the lugs 254, thereby preventing linear movement of the interlock ring 234.
[0059] During the heating operation, the actuator or driver 148 provides a clamping force to ensure sufficient contact at the clamping surfaces 30, 36 for electrode heating. When heating is discontinued, the actuator 148 releases the clamping force, allowing the stop ring 238 to unlock. The stop ring 238 is then moved to the unlocked position. The driver 148 then actuates the punch 248 to perform the mechanical joining operation. The stop ring 238 is then shifted to the locked position for the next clamping and heating operation.
[0060] 19 shows a graph of the thermal heating behavior over time of the AHSS and aluminum sheets using the electrodes of the previous embodiment. The required mechanical bonding temperature of sheet 40 (about 720°C) is reached in 87 milliseconds, while the upper aluminum sheet 38 in this case does not exceed 300°C.
[0061] 20 is a graph of a heating run on press hardened steel using the electrode of the previous embodiment. A temperature above 780° C. is reached in about 0.5 seconds and held for 1.25 seconds. This heating run results in a total joining cycle time of about 2 seconds.
[0062] Figure 21 is a graph of the heating behavior of a hot-dip galvanized third generation AHSS for the introduction of mechanical bonds. The stack is heated to an average of 380°C range, the temperature is maintained within that range for at least 2 seconds, and above 380°C for at least 4 seconds.
[0063] 22-25 show an alternative tool assembly 260 according to another embodiment. The tool assembly 260 includes a base 262, which may be a substrate 262, a base plate 262, or an adapter plate 262 for articulation and movement by an automation device. For example, the plate 262 may be attached to and driven by the actuator 148, which may be articulated by the industrial robot 102, 132.
[0064] The base plate 262 supports a retraction assembly 264 that includes a number of guide shafts 266 and a number of dampers 268. The guide shafts 266 are axially movable relative to the base plate 262. The dampers 268 may be fluid dampers 268, such as gas springs. A drive plate 270 is connected to the retraction assembly 264. An electrode 272 is attached to the drive plate 270 and spaced apart from the drive plate 270 so as to be spaced apart from the retraction assembly 264. A punch 274 is shown in FIGS. 23-25 and is connected to the base plate 262 and extends through a central bore 276 of the electrode 272. The punch 274 may be a clinch punch, a riveting ram, or the like, for performing a mechanical joining operation through the electrode 272.
[0065] During operation of the tool assembly 260, the actuator 148 drives the base plate 262 such that the electrode 272 engages the stack. As the base plate 262 is driven further from Figures 23 and 24, a clamping force is applied, thereby loading and compressing the retraction assembly 264. Further actuation of the base plate 262, shown in Figure 25, further compresses the retraction assembly 264, thereby driving the punch 274 through the electrode 272 to engage the fastener or stack.
[0066] The tool assembly 260 allows for uninterrupted (continuous) operation to clamp and then form the mechanical joint. The tool assembly 260 allows the driver 148 to clamp while heating the electrode 272 and drive the punch 274 in the same linear motion without retracting between clamping and forming. The continuous drive action reduces cycle time and improves tool life cycle by performing both functions without interrupting the operation or output of the driver 148.
[0067] As shown in the progression of Figures 26 and 27, the clinch punch 300 and clinch die 302 of each embodiment cooperate with one another to provide a clinch joint 304, as shown in Figure 28, for joining first and second sheet portions of steel pieces 306 and 308 together.
[0068] Referring to FIG. 29, a clinch rivet die 310 and clinch rivet 312 under the action of a rivet ram 314 provide a clinch riveted joint 316 between an AHSS piece 318 and a metal piece 320 .
[0069] 30, a full punch rivet die 322 and a full punch rivet 324 provide a full punch riveting action that provides a full punch riveted joint 326. In this embodiment, a punched piece falls below the die 322 by actuation of the rivet 324 by a rivet ram 328.
[0070] 31, the self-piercing rivet 332 is shown after being driven by a rivet ram to provide a self-piercing riveted joint 336 between sheet portions 338, 340. The sheet portions 338, 340 may be supported by a die (not shown) during the forming process.
[0071] Although various embodiments have been described above, it is not intended that these embodiments describe all possible forms of the present invention. The words used in this specification are words of description rather than limitation, and it is understood that various changes can be made without departing from the spirit and scope of the present invention. Moreover, features of various embodiments can be combined to form further embodiments of the present invention.
Claims
1. A method for mechanically joining steel materials, comprising the steps of: applying a variable clamping force to a stack of sheet metal sections, the stack including at least a portion of advanced high strength steel (AHSS); and heating the stack to an optimum mechanical bond temperature to maintain strength and material properties of the stack and form a mechanical bond with the AHSS.
2. The method of claim 1 , further comprising the step of heating the stack to a temperature below its melting temperature.
3. The method of claim 2 further comprising heating a heat affected zone (HAZ) portion of the bond area of the stack.
4. The method of claim 3 further comprising controlling and monitoring the temperature of the HAZ portion of the stack during heating.
5. The method of claim 1 , further comprising the step of heating the stack with a laser assembly.
6. The method of claim 1 further comprising the step of heating the stack with a pair of electrodes.
7. The method of claim 6 further comprising applying the variable clamping force with the pair of electrodes.
8. The method of claim 1 , further comprising the step of actuating an actuator to form the mechanical bond.
9. The method of claim 8 further comprising the step of actuating the actuator to apply the variable clamping force and form the mechanical bond by the same actuation.
10. 10. A mechanical joint formed by the method of claim 1.
11. A method for mechanically joining steel materials, comprising the steps of: clamping a stack of sheet metal sections, the stack including at least a portion of advanced high strength steel (AHSS); and heating the stack to a temperature below the melting temperature to mechanically bond the stack.
12. The method of claim 11 further comprising heating a heat affected zone (HAZ) portion of the bond area of the stack.
13. The method of claim 12 further comprising controlling and monitoring a temperature of the HAZ portion of the stack during heating.
14. The method of claim 11 , further comprising heating the stack with a laser assembly.
15. The method of claim 11 further comprising heating the stack with a pair of electrodes.
16. The method of claim 15 further comprising applying a variable clamping force with the pair of electrodes.
17. The method of claim 11 , further comprising the step of actuating an actuator to form the mechanical bond.
18. 20. The method of claim 17, further comprising the steps of actuating the actuator to apply the variable clamping force and form the mechanical bond by the same actuation.
19. a pair of clamping surfaces for clamping a stack of sheet metal sections including at least a portion of advanced high strength steel; a pair of electrodes having the pair of clamping surfaces and configured to pass an electrical current through the stack to heat the stack and form a mechanical bond to bond the stack together.
20. 20. The tool assembly of claim 19, wherein the tool assembly is an end effector adapted for attachment to an automation.
21. The tool assembly of claim 19, further comprising an actuator for performing a mechanical bonding action to form the mechanical bond.
22. The tool assembly of claim 21 , wherein the actuator actuates the pair of clamping surfaces to clamp the stack of sheet metal sections.
23. a tool assembly configured to clamp a stack of a plurality of sheet metal sections, the stack comprising at least a portion of the advanced high strength steel; an electrode array for heating the stack to a predetermined temperature to provide optimal ductility to the stack and form a mechanical bond; a controller in electrical communication with the tool assembly and configured to monitor a bonding temperature of a heat affected zone of the stack.
24. 24. The system of claim 23, wherein the tool assembly further comprises a laser assembly for heating the stack to an optimum temperature to form the mechanical bond.
25. at least a portion of an advanced high strength steel having a protective coating; and a metal component mechanically joined with at least a portion of the advanced high strength steel having said protective coating, said protective coating being between said at least a portion and said metal component in said mechanical joint.
Citation Information
Patent Citations
Device for joining workpieces
DE102011051636A1
Apparatus and method for mechanically joining advanced high strength steels
JP2019505390A
Method and apparatus for clinching metal sheets
US20030037428A1