Method for cleaning substrate processing apparatus
A low-temperature cleaning method using HBr and H2O2 gases with plasma generation effectively removes impurities from substrate processing apparatuses, addressing the issues of corrosion and contamination in high-temperature cleaning methods.
Patent Information
- Application Number
- JP2024509418
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-24
- Filing Date
- 2022-09-20
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2042-09-20
AI Technical Summary
Existing methods for cleaning substrate processing apparatuses involve high-temperature processes that can cause corrosion and additional contamination due to the peeling off of chamber components, leading to a significant amount of impurities remaining after cleaning.
A low-temperature cleaning method using gases such as HBr and H2O2, combined with plasma generation, to decompose and remove impurities without damaging the apparatus surfaces, thereby reducing the amount of impurities and preventing corrosion.
The method effectively removes impurities at temperatures below the deposition process temperature, minimizing the risk of surface peeling and corrosion, resulting in a cleaner substrate processing apparatus.
Smart Images

Figure 2024536686000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for cleaning a substrate processing apparatus, and more particularly to a method for cleaning a substrate processing apparatus capable of reducing the amount of impurities remaining inside the substrate processing apparatus. [Background technology]
[0002] The manufacturing process of a semiconductor device or a display device includes a process of depositing a thin film on a substrate, and the thin film deposition process is carried out inside a chamber of a substrate processing apparatus.
[0003] Meanwhile, when a deposition process is performed to deposit a thin film on a substrate, deposition material is deposited not only on the substrate but also inside a chamber in which the deposition process is performed, for example, on the surfaces of the inner walls of the chamber and a support table that supports the substrate.
[0004] As described above, the thin film deposited inside the chamber peels off as its thickness increases, causing the generation of particles. Furthermore, the particles enter the thin film formed on the substrate or adhere to the surface of the thin film, causing defects and increasing the defective rate of the product. Therefore, it is necessary to remove such deposits before they peel off.
[0005] When performing a cleaning process to remove deposits inside the chamber, a gas containing Cl or a gas containing F is generally used. In this case, the inside of the chamber must be kept at a high temperature in order for the gas containing Cl or the gas containing F to react with the deposits.
[0006] However, when deposits are peeled off from the inner surface of the chamber, the high temperature inside the chamber may cause the surface of the part or structure on which the deposits are deposited to peel off together with the deposits. For this reason, contaminants that act as impurities are generated in addition to the deposits. Therefore, since there is a large amount of impurities, including deposits and additional generated contaminants, inside the chamber, there is a problem that a large amount of impurities remain inside the chamber even after the cleaning process is completed.
[0007] Furthermore, the inside of the chamber is kept at a high temperature, which causes corrosion inside the chamber during the cleaning process. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Korean Patent No. 10-1232904 Summary of the Invention [Problem to be solved by the invention]
[0009] The present invention provides a method for cleaning a substrate processing apparatus that can perform cleaning at a low temperature.
[0010] The present invention provides a method for cleaning a substrate processing apparatus that can be cleaned at a temperature lower than the thin film deposition temperature. [Means for solving the problem]
[0011] A cleaning method for a substrate processing apparatus according to an embodiment of the present invention may include the steps of: loading a substrate into a chamber; injecting a gas containing at least one of Zn, Ga, In, and Sn into the chamber to deposit a thin film on the substrate; unloading the substrate from the chamber; injecting a cleaning gas containing Br into the chamber; and exhausting by-products generated by a reaction between the cleaning gas and impurities deposited inside the chamber other than the substrate during the thin film depositing step.
[0012] A cleaning method for a substrate processing apparatus according to an embodiment of the present invention includes the steps of: loading a substrate into a chamber; injecting a gas into the chamber to deposit a thin film on the substrate; unloading the substrate from the chamber; injecting a cleaning gas containing Br into the chamber; and exhausting by-products generated by a reaction between the cleaning gas and impurities deposited inside the chamber other than the substrate in the step of depositing the thin film. In the step of injecting the cleaning gas, the cleaning gas may be injected in a pulsed manner, or the step of injecting the cleaning gas and the step of exhausting the by-products may be alternately repeated.
[0013] The method for cleaning a substrate processing apparatus may include the step of injecting a first auxiliary gas into the chamber, the first auxiliary gas being configured to decompose the cleaning gas.
[0014] As the first auxiliary gas, at least one of H2 gas and O2 gas may be used.
[0015] The method for cleaning a substrate processing apparatus may include the step of generating plasma inside the chamber.
[0016] The step of generating the plasma may include the step of injecting a second auxiliary gas, which is Ar gas.
[0017] The above-mentioned method for cleaning a substrate processing apparatus may include a step of injecting a nitrogen-containing gas into the inside of the chamber, and the step of injecting the nitrogen-containing gas may be performed between the step of injecting the cleaning gas and the step of exhausting the by-products.
[0018] The cleaning gas may include at least one of HBr, KBr, Br2, HBrO3, and CBrF3.
[0019] The temperature inside the chamber may be lower than the temperature during the deposition process. Effect of the Invention
[0020] According to an embodiment of the present invention, the inside of a substrate processing apparatus can be cleaned at a temperature lower than that of a conventional method and lower than the temperature of a deposition process. That is, thin-film impurities deposited on the surfaces of parts or structures disposed inside the substrate processing apparatus can be peeled off from the surfaces and cleaned at a low temperature.
[0021] This can prevent or inhibit the inner surface of the substrate processing apparatus from peeling off together with the impurities when the impurities are peeled off, thereby reducing the generation of additional contaminants inside the chamber and reducing the amount of impurities remaining inside the substrate processing apparatus after the cleaning process is completed.
[0022] Furthermore, corrosion of the substrate processing apparatus due to high temperature heat can be prevented or suppressed. [Brief description of the drawings]
[0023] [Figure 1] FIG. 2 is a process flow diagram showing in situ cleaning after a deposition process according to a first embodiment of the present invention. [Diagram 2]FIG. 4 is a process flow diagram showing in situ cleaning after a deposition process according to a second embodiment of the present invention. [Diagram 3] 1 is a diagram showing a substrate processing apparatus for performing cleaning by a method according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] Hereinafter, the embodiments of the present invention will be described in more detail with reference to the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below, and may be embodied in various different forms. These embodiments are merely provided to complete the disclosure of the present invention and to fully inform those skilled in the art of the scope of the invention. In order to describe the embodiments of the present invention, the drawings may be exaggerated, and the same reference numerals in the drawings refer to the same components.
[0025] FIG. 1 is a process flow diagram showing in situ cleaning after a deposition process according to a first embodiment of the present invention.
[0026] The cleaning process may be a process for removing a thin film that has been deposited or built up on the surface of a component or structure other than the substrate when a thin film is deposited on the substrate inside the substrate processing apparatus.
[0027] For ease of explanation, hereinafter, a thin film that is evaporated or deposited on the surface of a component or structure other than a substrate inside the substrate processing apparatus and that remains inside the substrate processing apparatus will be referred to as an impurity.
[0028] In an embodiment of the present invention, as shown in Fig. 1, a deposition process (S100) and a cleaning process (S200) are performed in situ in one substrate processing apparatus. That is, after a process (S100) of depositing a thin film on a substrate inside the substrate processing apparatus is completed, a process (S200) of cleaning the inside of the substrate processing apparatus is performed. At this time, the cleaning process may be performed immediately after one deposition process is performed, or may be performed after multiple deposition processes are performed. Also, the cleaning process may be selectively performed between deposition processes.
[0029] Referring to FIG. 1, the deposition process (S100) includes a process of loading a substrate into a chamber of a substrate processing apparatus (S110), a process of depositing a thin film on one side of the substrate (S120), and a process of unloading the substrate after the thin film deposition is completed from the chamber (S120).
[0030] The thin film deposited in the deposition process (S120) may be a zinc oxide (ZnO) thin film on the substrate, or a zinc oxide (ZnO) thin film doped with at least one of In (indium), Ga (gallium), and Sn (tin). More specifically, the deposition process may be a process of depositing any one of a zinc oxide (ZnO: zinc oxide) thin film, an IZO (indium zinc oxide) thin film obtained by doping zinc oxide (ZnO: zinc oxide) with In (indium), a gallium zinc oxide (GZO: gallium zinc oxide) thin film obtained by doping zinc oxide (ZnO: zinc oxide) with Ga (gallium), an indium gallium zinc oxide (IGZO: indium gallium zinc oxide) thin film obtained by doping zinc oxide (ZnO: zinc oxide) with In (indium) and Ga (gallium), and an indium tin zinc oxide (ITZO: indium tin zinc oxide) thin film obtained by doping zinc oxide (ZnO: zinc oxide) with In (indium) and Sn (tin) on the substrate. The deposition process (S100) may be a process for forming a thin film, for example, an active layer of a thin film transistor.
[0031] The deposition step performed before or after the cleaning step according to the embodiment may be a step of depositing a thin film on the substrate by an atomic layer deposition (ALD) method.
[0032] The process temperature for depositing the zinc oxide (ZnO) thin film, the indium zinc oxide (IZO) thin film, the gallium zinc oxide (GZO) thin film, and the indium gallium zinc oxide (IGZO) thin film may be 300°C to 350°C (300°C or more and 350°C or less).The process temperature for depositing the indium tin zinc oxide (ITZO) thin film may be 250°C to 400°C (250°C or more and 400°C or less).
[0033] As shown in FIG. 1, the cleaning process (S200) includes a step of injecting a cleaning gas, which is a gas containing Br (bromine), a step of injecting a first auxiliary gas, which is a gas that decomposes or activates the cleaning gas, and a step of exhausting the gas (S250).
[0034] The cleaning step (S200) may include a step (S230) of generating plasma in the space into which the cleaning gas and the first auxiliary gas are injected. The cleaning step (S200) may further include a step (S240) of injecting a second auxiliary gas, which is a gas different from the cleaning gas and the first auxiliary gas. In this case, the second auxiliary gas may be a gas injected to improve the efficiency of plasma generation.
[0035] When the cleaning process is performed after the deposition process is completed, cleaning is performed at a temperature lower than the process temperature for the deposition process. That is, cleaning is performed at a temperature lower than 300°C (above room temperature) or lower than 250°C (above room temperature). For this purpose, a gas that can be decomposed or activated at a temperature lower than the process temperature for depositing a thin film on a substrate is used as a cleaning gas. In other words, a gas that can be decomposed or activated at a temperature lower than 300°C (above room temperature) is used as a cleaning gas.
[0036] In the embodiment, a gas containing Br (bromine) is used as the cleaning gas. More specifically, a gas containing at least one of HBr, KBr, Br2, HBrO3, and CBrF3 is used as the cleaning gas. A gas containing Br (bromine), such as HBr, KBr, Br2, HBrO3, and CBrF3, can be decomposed or activated at a temperature below 300°C (above room temperature). That is, a cleaning gas containing Br (bromine) can be decomposed at a temperature lower than the temperature required for the reaction between a source gas, which is a gas for depositing a thin film, and a reactant gas.
[0037] The first auxiliary gas is a gas that reacts with the cleaning gas to decompose the cleaning gas, and at least one of H2 gas and O2 gas can be used as the first auxiliary gas. In this case, the first auxiliary gas may be injected through a route different from that of the cleaning gas.
[0038] On the other hand, the impurities may be evaporated or deposited in a thin film on the surfaces of various components or structures inside the substrate processing apparatus, and thus the thin film impurities cannot be easily peeled off or separated from the surfaces of the various components or structures.
[0039] However, a cleaning gas containing Br reacts with impurities or deposits in a thin film to strip the impurity deposits from the surface, and can also react with impurities at a temperature lower than the process temperature during deposition to strip the impurities from the surface.
[0040] The cleaning process using the cleaning gas and the first auxiliary gas will be described below. In this case, the case where HBr gas is used as the cleaning gas and H2 gas is used as the first auxiliary gas will be described as an example. In addition, the case where the cleaning process is performed after the process of depositing a ZnO thin film on a substrate inside a substrate processing apparatus will be described as an example.
[0041] After the process of depositing a ZnO thin film on a substrate in the substrate processing apparatus is performed, the ZnO thin film may be deposited on the surfaces of not only the substrate but also various other components or structures. The ZnO thin film deposited on the surfaces of components or structures other than the substrate in the substrate processing apparatus, i.e., the ZnO deposits, may act as impurities that contaminate the substrate or thin film in the next deposition process.
[0042] For this purpose, after the deposition process (S100) is completed, a cleaning process (S200) is performed. For this purpose, a cleaning gas and a first auxiliary gas are injected into the substrate processing apparatus. That is, HBr gas is injected as the cleaning gas, and H2 gas is injected as the first auxiliary gas. Also, the temperature inside the substrate processing apparatus is adjusted to a temperature less than 300°C.
[0043] When the cleaning gas (HBr gas) and the first auxiliary gas (H2) are injected, the cleaning gas HBr is decomposed by the first auxiliary gas H2, and the decomposed Br from the cleaning gas reacts with the ZnO thin film impurity (see reaction formula 1).
[0044] ZnO+2HBr+H2→ZnBr2·H2O …1
[0045] That is, ZnO, which is a deposit remaining in the substrate processing apparatus, is decomposed to generate ZnBr2·H2O. In other words, there is a possibility that impurities in the form of a ZnO thin film deposited on the surface of the substrate processing apparatus are decomposed into fine particles. Then, as the impurities in the form of a ZnO thin film are decomposed into fine particles, they are peeled off from the surface on which they were deposited. Furthermore, the fine particle impurities are exhausted to the outside of the substrate processing apparatus by the exhaust process (S250), thereby cleaning the inside of the substrate processing apparatus. That is, they are exhausted to the outside by the suction force of an exhaust unit provided in the substrate processing apparatus, thereby cleaning the inside of the substrate processing apparatus.
[0046] Thus, in the embodiment, the cleaning step is performed using a cleaning gas that can be decomposed at a temperature lower than the process temperature, i.e., according to the embodiment, cleaning can be performed at a temperature lower than 300°C.
[0047] On the other hand, during the cleaning process, the higher the temperature inside the substrate processing apparatus, the more likely it is that when impurities are peeled off from a surface, for example, a wall of a chamber, a part of the wall of the chamber may peel off. That is, there is a risk of a problem that the surface inside the substrate processing apparatus may be damaged. This causes additional impurities to be generated in addition to the deposits generated during the deposition process. Therefore, after the cleaning process is completed, a large amount of impurities remain inside the substrate processing apparatus. In addition, there is a risk of corrosion occurring inside the substrate processing apparatus due to the high temperature.
[0048] However, in the embodiment, impurities can be peeled off and cleaned from the surface of the substrate processing apparatus at a temperature lower than that of the conventional method and lower than the deposition process temperature. Therefore, when impurities are peeled off from the surface, it is possible to prevent or reduce the surface inside the substrate processing apparatus from peeling off together. Therefore, it is possible to reduce the amount of impurities remaining inside the substrate processing apparatus after the cleaning process is completed. In addition, by performing cleaning at a low temperature, it is possible to suppress or prevent the occurrence of corrosion due to high temperature heat.
[0049] When the cleaning gas and the first auxiliary gas are injected (S210, S220) to perform cleaning, plasma may be generated inside the substrate processing apparatus (S230). That is, when the cleaning gas and the first auxiliary gas are injected inside the substrate processing apparatus, RF power may be supplied. At this time, at least one of the first auxiliary gases, N2 gas, O2 gas, and H2 gas, may be discharged to generate plasma.
[0050] When plasma is generated, the cleaning gas can be decomposed or activated more easily. That is, compared to when only a heater disposed inside the substrate processing apparatus is operated to heat the inside, when plasma is generated inside the substrate processing apparatus, the cleaning gas can be decomposed or activated at a relatively lower temperature. In other words, compared to when only the cleaning gas and the first auxiliary gas are injected, when plasma is generated together, the cleaning gas can be decomposed at a lower temperature, and thus cleaning can be performed at a lower temperature.
[0051] When performing cleaning by injecting the cleaning gas and the first auxiliary gas (S210, S220) and generating plasma (S230), a second auxiliary gas may be further injected (S240). The second auxiliary gas is a gas for improving the plasma generation efficiency, and may be Ar gas. That is, when the cleaning gas and the first auxiliary gas are injected into the substrate processing apparatus and RF power is supplied to generate plasma, if the second auxiliary gas, which is Ar gas, is further injected, there is an effect that the plasma generation efficiency is improved by the Ar gas.
[0052] Therefore, compared to when only the cleaning gas and the first auxiliary gas are injected to generate plasma, when the second auxiliary gas, Ar gas, is injected together, the cleaning gas can be decomposed at a relatively lower temperature, thereby making it possible to perform cleaning at an even lower temperature.
[0053] FIG. 2 is a process diagram showing in situ cleaning after a deposition process according to a method according to a second embodiment of the present invention.
[0054] In the above-described first embodiment, the cleaning gas containing Br and the first auxiliary gas are injected in the cleaning step (S200). However, the present invention is not limited to this, and only the first cleaning gas may be injected.
[0055] A cleaning method according to the second embodiment of the present invention will be described below with reference to Fig. 2. At this time, the contents that overlap with those of the first embodiment will be omitted or will be described briefly.
[0056] Referring to FIG. 2, the cleaning process (S200) according to the second embodiment includes a step of injecting a cleaning gas, which is a gas containing Br (bromine), (S210), and after the injection of the cleaning gas is stopped, a step of injecting a gas containing nitrogen (S260), and an exhaust step (S270).
[0057] When performing the step of injecting cleaning gas (S210), the cleaning gas is injected in a pulsed manner. That is, a cycle of alternately turning on and off the injection of cleaning gas is repeated multiple times. When the injection of cleaning gas is stopped during the process of alternately turning on and off the injection of cleaning gas, nitrogen gas or a gas containing nitrogen is injected. After the nitrogen gas is injected, exhaust is performed. Then, one cycle consisting of "the step of injecting cleaning gas (S210), the step of injecting nitrogen-containing gas (S260), and the step of exhausting (S270)" is repeated multiple times.
[0058] In this way, nitrogen gas is injected after the injection of cleaning gas is stopped, and cleaning gas is not injected when nitrogen gas is injected, so that it can be explained as the injection of cleaning gas and nitrogen gas in a pulsed manner.
[0059] In this way, when the injection of the cleaning gas is stopped (off) and the nitrogen gas is injected, the impurities are discharged outside the substrate processing apparatus due to the operation of the exhaust unit. That is, the impurities that reacted while the injection of the cleaning gas is on are discharged outside the substrate processing apparatus together with the nitrogen gas when the injected nitrogen gas is discharged by the operation of the exhaust unit after the injection of the cleaning gas is stopped (off). This can be explained as the injection of the cleaning gas (on) and the exhaust of the impurities being performed alternately. In this way, the nitrogen gas injected when the injection of the cleaning gas is stopped plays a role in increasing the exhaust efficiency of the impurities. That is, the impurities are exhausted together with the nitrogen gas due to the flow of the nitrogen gas exhausted to the exhaust unit, which has the effect of improving the exhaust efficiency of the impurities.
[0060] In the above description, the case where the nitrogen gas is injected and then the exhaust is performed has been described, but the present invention is not limited to this at all, and the exhaust may be performed while the nitrogen gas is being injected.
[0061] FIG. 3 is a diagram showing a substrate processing apparatus for performing cleaning by a method according to an embodiment of the present invention.
[0062] Hereinafter, a substrate processing apparatus for performing a cleaning process according to an embodiment of the present invention will be described with reference to FIG.
[0063] Referring to FIG. 3, the substrate processing apparatus may include a chamber 100, a support stage 200 disposed within the chamber 100 for supporting a substrate, an injection unit 300 disposed facing the support stage 200 for injecting gas into the chamber 100, a gas supply unit 400 for providing gas for deposition and cleaning to the injection unit 300, first and second gas supply pipes 500a, 500b connected to the injection unit 300 to have different paths from each other and for supplying gas from the gas supply unit 400 to the injection unit 300, and an RF power supply unit 600 for supplying power to generate plasma within the chamber 100.
[0064] The substrate processing apparatus may further include a drive unit 700 that causes the support stage 200 to perform at least one of a lifting / lowering motion and a rotation motion, and an exhaust unit 800 that is arranged to be connected to the chamber 100.
[0065] The chamber 100 may have an internal space for a reaction or process capable of depositing a thin film on a substrate carried inside. In this case, the internal space of the chamber 100 may have a cross-sectional shape of a rectangle, a pentagon, a hexagon, etc. Needless to say, the shape of the internal space of the chamber 100 can be changed in various ways, and is preferably provided to correspond to the shape of the substrate S.
[0066] The support 200 is disposed inside the chamber 100 to face the spray unit 300, and supports the substrate S that is carried into the chamber 100. A heater 210 may be provided inside the support 200. Thus, when the heater 210 is operated, the substrate S placed on the support 200 and the inside of the chamber 100 can be heated.
[0067] The injection section 300 may include a first plate 310 having a plurality of holes (hereinafter, holes) 311 arranged in the extension direction of the support base 200 and spaced apart from one another, and arranged to face the support base 200 inside the chamber 100, a plurality of nozzles 320 arranged so that at least a portion of each of the plurality of holes 311 is fitted into each of the plurality of holes 311, and a second plate 330 arranged inside the chamber 100 so as to be positioned between an upper wall of the chamber 100 and the first plate 310.
[0068] Additionally, the ejector 300 may further include an insulating portion 340 positioned between the first plate 310 and the second plate 330 .
[0069] The first plate 310 may have a plate shape extending in the extension direction of the support base 200. The first plate 310 is provided with a plurality of holes 311, and each of the plurality of holes 311 may be provided so as to penetrate the first plate 310 in the up-down direction. The plurality of holes 311 may be aligned in the extension direction of the first plate 310 or the support base 200.
[0070] Each of the nozzles 320 may have a shape extending in the vertical direction, a passage through which gas can pass may be provided therein, and the upper and lower ends may be open. Each of the nozzles 320 may be disposed such that at least its lower portion is fitted into a hole 311 provided in the first plate 310, and its upper portion is connected to the second plate 330. For this reason, the nozzles 320 can be described as having a shape protruding downward from the second plate 330.
[0071] The outer diameter of the nozzle 320 may be set to be smaller than the inner diameter of the hole 311. The nozzle 320 may be arranged so that the outer peripheral surface of the nozzle 320 is separated from the wall around the hole 311 (i.e., the inner wall of the first plate 310) when the nozzle 320 is fitted into the inside of the hole 311. Therefore, the inside of the hole 311 can be separated into an outer space of the nozzle 320 and an inner space of the nozzle 320.
[0072] The passage in nozzle 320 in the internal space of hole 311 is a passage through which gas from first gas supply pipe 500a moves and is sprayed. And the outer space of nozzle 320 in the internal space of hole 311 is a passage through which gas from second gas supply pipe 500b moves and is sprayed. Therefore, hereinafter, the passage in nozzle 320 is referred to as first path 360a, and the outer space of nozzle 320 inside hole 311 is referred to as second path 360b.
[0073] The second plate 330 may be disposed such that its upper surface is separated from the upper wall of the chamber 100 and its lower surface is separated from the first plate 310. This allows for an empty space to be provided between the second plate 330 and the first plate 310 and between the second plate 330 and the upper wall of the chamber 100.
[0074] Here, the space above the second plate 330 is a space through which the gas from the first gas supply pipe 500a permeates and moves (hereinafter, diffusion space 350), and may communicate with the upper openings of the multiple nozzles 320. In other words, the diffusion space 350 is a space that communicates with the multiple first paths 360a. Therefore, the gas that has passed through the first gas supply pipe 500a permeates the diffusion space 350 in the extension direction of the second plate 330, and then passes through the multiple first paths 360a to be injected downward.
[0075] In addition, a deep hole (not shown) that is a passage through which gas moves is provided inside the second plate 330, and the deep hole may be connected to the second gas supply pipe 500b and communicated with the second path 360b. Therefore, the gas from the second gas supply pipe 500b can be sprayed toward the substrate S through the deep hole of the second plate 330 and the second path 360b.
[0076] The RF power supply unit 600 is a means for supplying power to generate plasma inside the chamber 100. More specifically, the RF power supply unit 600 is a means for supplying RF power for generating plasma, and may be connected to the first plate 310 of the injection unit 300. In this case, the second plate 330 and the support 200 may be grounded. The RF power supply unit 600 may also include an impedance matching circuit for matching the load impedance and source impedance of the power supply for generating plasma. The impedance matching circuit may include two impedance elements composed of at least one of a variable capacitor and a variable inductor.
[0077] The gas supply unit 400 supplies the gases required for depositing a thin film and cleaning to the injection unit 300 .
[0078] The gas supply unit 400 may include a source gas storage unit 410 storing a source gas for thin film deposition, a reactant gas storage unit 420 storing a reactant gas that reacts with the source gas, a purge gas storage unit 430 storing a purge gas, a cleaning gas storage unit 440 storing a cleaning gas containing Br (bromine), and first and second auxiliary gas storage units 450a and 450b storing first and second auxiliary gases that are sprayed together with the cleaning gas during the cleaning process. The gas supply unit may also include a nitrogen gas storage unit 450c storing a gas containing nitrogen.
[0079] The gas supply section 400 may include a first transfer pipe 470a connecting the source gas storage section 410, the purge gas storage section 430, and the cleaning gas storage section 440 to the first gas supply pipe 500a, and a second transfer pipe 470b connecting the reactant gas storage section 420, the first auxiliary gas storage section 450a, the second auxiliary gas storage section 450b, and the nitrogen gas storage section 450c to the second gas supply pipe 500b.
[0080] The gas supply section 400 may include a plurality of first connecting pipes 480a connecting each of the source gas storage section 410, the purge gas storage section 430, and the cleaning gas storage section 440 to the first transfer pipe 470a, a first valve 490a arranged on each of the plurality of first connecting pipes 480a, and a plurality of second connecting pipes 480b connecting each of the reactant gas storage section 420, the first auxiliary gas storage section 450a, the second auxiliary gas storage section 450b, and the nitrogen gas storage section 450c to the second transfer pipe 470b, and a second valve 490b arranged on each of the plurality of second connecting pipes 480b.
[0081] The gas stored in the source gas storage unit 410 is a gas for depositing a thin film. That is, the source gas storage unit 410 may store at least one of a gas containing zinc (Zn), a gas containing indium (In), a gas containing gallium (Ga), and a gas containing tin (Sn). In this case, a plurality of source gas storage units 410 may be provided. That is, a source gas storage unit storing a zinc (Zn)-containing gas, a source gas storage unit storing an indium (In)-containing gas, a source gas storage unit storing a gallium (Ga)-containing gas, and a source gas storage unit storing a tin (Sn)-containing gas may all be provided. Needless to say, depending on the type of thin film to be deposited, some of a source gas reservoir storing a zinc (Zn)-containing gas, a source gas reservoir storing an indium (In)-containing gas, a source gas reservoir storing a gallium (Ga)-containing gas, and a source gas reservoir storing a tin (Sn)-containing gas may be provided.
[0082] As a gas containing zinc (Zn), at least one of diethyl zinc (Diethyl Zinc; Zn(C2H5)2) (DEZ) and dimethyl zinc (Dimethyl Zinc; Zn(CH3)2) (DMZ) can be used, as a gas containing indium (In), at least one of trimethyl indium (Trimethyl Indium; In(CH3)3) (TMIn) and diethylamino propyl dimethyl indium (Diethylamino Propyl Dimethyl Indium) (DADI) can be used, as a raw material gas containing gallium (Ga), trimethyl gallium (Trimethyl Gallium; Ga(CH3)3) (TMGa) can be used. Also, as a gas containing tin (Sn), tetramethyl tin [tetramethyltin; Sn(Me)4] can be used.
[0083] The reactant gas reservoir 420 stores a gas for depositing a thin film and reacting with the source gas. The reactant gas may be a gas containing oxygen (O). More specifically, at least one of pure oxygen (O2), nitrous oxide (N2O), and ozone (O3) may be used as the reactant gas.
[0084] The purge gas stored in the purge gas storage section 430 may be, for example, N2 gas or Ar gas.
[0085] The cleaning gas stored in the cleaning gas storage section 440 contains Br (bromine). More specifically, the cleaning gas storage section 440 may store a gas containing at least one of HBr, KBr, Br2, HBrO3, and CBrF3.
[0086] The gas stored in the first auxiliary gas storage unit 450a is a first auxiliary gas that reacts with the cleaning gas to decompose the cleaning gas. At this time, at least one of N2 gas, O2 gas, and H2 gas can be used as the first auxiliary gas.
[0087] The second auxiliary gas reservoir 450b stores a second auxiliary gas for improving the efficiency of generating plasma. In this case, the second auxiliary gas may be Ar gas.
[0088] In the above, it has been described that the reactant gas storage section and the first auxiliary gas storage section are provided separately. However, when the same gas is used as the reactant gas and the first auxiliary gas, only one of the reactant gas storage section and the first auxiliary gas storage section may be provided. For example, when O2 is used as the reactant gas during deposition of a thin film and O2 is used as the first auxiliary gas during a cleaning process, only one of the reactant gas storage section and the first auxiliary gas storage section may be provided.
[0089] In the above, the purge gas reservoir and the second auxiliary gas reservoir are provided separately. However, when the same gas is used as the purge gas and the second auxiliary gas, only one of the purge gas reservoir and the second auxiliary gas reservoir may be provided. For example, when Ar is used as the purge gas during the thin film deposition and Ar is used as the second auxiliary gas during the cleaning process, only one of the purge gas reservoir and the second auxiliary gas reservoir may be provided.
[0090] Hereinafter, a deposition process using the substrate processing apparatus and a cleaning process according to the first embodiment will be described with reference to FIGS.
[0091] First, the vapor deposition step (S100) will be described, taking as an example the formation of a ZnO thin film on a substrate.
[0092] The substrate 10 is carried into the chamber 100 and placed on the support stage 200. Then, the heater 210 is operated to heat the substrate S placed on the support stage 200 to 300° C. to 350° C. Needless to say, the substrate S may be placed on the support stage 200 after the support stage 200 is heated to 300° C. to 350° C.
[0093] Next, a ZnO thin film is deposited on the substrate S. That is, a ZnO thin film is formed on the substrate S by atomic layer deposition, which involves the injection of a source gas, the injection of a purge gas (first purge), the injection of a reactant gas, and the injection of a purge gas (second purge) in that order.
[0094] A method for forming a ZnO thin film by injecting gas into the chamber 100 using the injector 300 and the gas supply unit 400 will be briefly described below.
[0095] First, the source gas stored in the source gas storage unit 410, i.e., the Zn-containing gas, is supplied to the first transfer pipe 470a. The source gas supplied to the first transfer pipe 470a flows into the diffusion space 350 in the injection unit 300 through the first gas supply pipe 500a. After the source gas is distributed throughout the diffusion space 350, it passes through the multiple nozzles 320, i.e., the multiple first paths 360a, and is injected toward the substrate S.
[0096] When the injection of the source gas is interrupted or completed, a purge gas is provided through the purge gas reservoir 430 to inject the purge gas into the chamber 100 (first purge). At this time, the purge gas discharged from the purge gas reservoir 430 may pass through the first transfer pipe 470a and the first gas supply pipe 500a, and then be injected downward through the first path 360a. When the purge gas injected into the chamber 100 through the first path 360a is exhausted to the exhaust unit 800, at least a portion of by-products or impurities such as the source gas that could not be adsorbed on the substrate S may be exhausted together.
[0097] Then, a reactant gas, for example, O2 gas, is provided from the reactant gas storage unit 420 and injected into the chamber 100. At this time, the reactant gas may be injected into the chamber 100 through a path different from that of the source gas. That is, the reactant gas may be injected downward through the second path 360b after passing through the second transfer pipe 470b and the second gas supply pipe 500b. When the reactant gas is injected, the RF power supply unit 600 may be operated to generate plasma inside the chamber 100. When the reactant gas is injected, a reaction occurs between the source gas adsorbed on the substrate S and the reactant gas, and a reactant, i.e., ZnO, can be generated. Then, the reactant is deposited or evaporated on the substrate S, and thus a ZnO thin film is evaporated on the substrate S.
[0098] When the injection of the reactant gas is stopped, the purge gas is supplied through the purge gas reservoir 430 to inject the purge gas into the chamber 100 (second purge). At this time, the by-products generated by the reaction between the source gas and the reactant gas can be discharged to the outside of the chamber 100 by the second purge.
[0099] The above-mentioned process cycle of "injection of source gas, injection of purge gas (first purge), injection of reactant gas, injection of purge gas (second purge)" may be repeated multiple times. The number of times the process cycle should be performed may be determined according to the target film thickness.
[0100] When a ZnO thin film having a target thickness is formed on the substrate S, the substrate 10 is carried out of the chamber 100.
[0101] Thereafter, the inside of the chamber 100 is cleaned (S200). That is, cleaning is performed to remove impurities, which are the thin film deposited on the inner wall of the chamber, the surface of the support table, and the like disposed inside the chamber 100 in addition to the substrate S during the process of depositing the ZnO thin film on the substrate S.
[0102] For this purpose, the cleaning gas and the first auxiliary gas are discharged from the cleaning gas storage section 440 and the first auxiliary gas storage section 450a, respectively. The cleaning gas passes through the first transfer pipe 470a and the first gas supply pipe 500a, and is then injected into the chamber 100 through the first path 360a of the injection section 300 (S210). The first auxiliary gas passes through the second transfer pipe 470b and the second gas supply pipe 500b, and is then injected into the chamber 100 through the second path 360b of the injection section 300 (S220). At this time, the cleaning gas may be, for example, HBr gas, and the first auxiliary gas may be H2 gas. At this time, the inside of the chamber 100 is adjusted to a temperature less than 300° C. using the heater 210.
[0103] When the cleaning gas (HBr gas) and the first auxiliary gas (H2) are injected, the cleaning gas is decomposed by the first auxiliary gas. That is, H and Br of the HBr gas are decomposed. Then, the Br decomposed from the cleaning gas reacts with the impurities remaining inside the chamber 100, i.e., the ZnO thin film (see reaction formula 1). That is, the thin film ZnO impurities deposited on the surfaces of various parts or structures inside the chamber 100 react with the Br of the cleaning gas, and ZnBr2·H2O can be generated by this reaction. When ZnBr2·H2O is generated by the reaction between the thin film ZnO impurities and the Br of the cleaning gas, the thin film ZnO impurities can be microparticulated. In addition, the binding or adhesion between the impurities and the surface is weakened by the microparticulation of the thin film impurities, and therefore the impurities in the form of microparticles can be peeled off from the surface of the deposition.
[0104] At this time, a suction force is generated inside the chamber 100 due to the operation of the exhaust unit 800. Therefore, the particulate impurities or the peeled impurities can be discharged to the outside of the chamber 100 through the exhaust unit 800 by the suction force, and the inside of the chamber 100 is thereby cleaned.
[0105] When the cleaning gas and the first auxiliary gas are injected into the chamber 100, the RF power supply unit 600 may be operated to generate plasma inside the chamber 100 (S230). That is, when the RF power supply unit 600 is operated, the first auxiliary gas, for example, O2 gas, may be discharged to generate plasma. When plasma is generated in this manner, cleaning can be performed at a lower temperature than when not generated. That is, compared to when only the heater 210 is operated to heat the inside of the chamber 100, when plasma is generated inside the chamber 100, the cleaning gas can be decomposed at a relatively lower temperature, and the inside of the chamber 100 can be cleaned at an even lower temperature.
[0106] In addition, when the cleaning gas and the first auxiliary gas are injected into the chamber 100 and the RF power supply unit 600 is operated, a second auxiliary gas, i.e., Ar gas, may be further injected (S240). When the second auxiliary gas is injected, the plasma generation efficiency can be improved. Therefore, compared to when only the cleaning gas and the first auxiliary gas are injected into the chamber 100 to generate plasma, when the second auxiliary gas, Ar gas, is injected together, the cleaning gas can be decomposed at a relatively low temperature, and the inside of the chamber can be cleaned at a low temperature.
[0107] Thus, according to the embodiment of the present invention, the inside of the substrate processing apparatus can be cleaned at a temperature lower than the conventional temperature and lower than the deposition process temperature. That is, thin-film impurities deposited on the surface of a part or structure disposed inside the chamber 100 can be decomposed and turned into fine particles at a low temperature of less than 300° C., and thus the impurities can be peeled off from the surface. This allows the inside of the chamber 100 to be cleaned at a temperature lower than the deposition temperature.
[0108] By cleaning at such a low temperature, it is possible to prevent or reduce the amount of impurities that peel off from the inner surface of the substrate processing apparatus when the impurities are peeled off from the surface. Therefore, it is possible to reduce the amount of impurities remaining inside the substrate processing apparatus after the cleaning process is completed. In addition, by performing cleaning at a low temperature, it is possible to suppress or prevent the occurrence of corrosion due to high temperature heat. [Industrial Applicability]
[0109] According to an embodiment of the present invention, the inside of a substrate processing apparatus can be cleaned at a temperature lower than that of the conventional method and lower than the deposition process temperature. That is, thin-film impurities deposited on the surface of a component or structure disposed inside the substrate processing apparatus can be peeled off from the surface at a low temperature and cleaned. This can prevent or suppress the inner surface of the substrate processing apparatus from peeling off together with the impurities when the impurities are peeled off. This can reduce the generation of additional contaminants inside the chamber and reduce the amount of impurities remaining inside the substrate processing apparatus after the cleaning process is completed.
Claims
1. Loading a substrate into a chamber; injecting a gas containing at least one of Zn, Ga, In, and Sn into the chamber to deposit a thin film on the substrate; removing the substrate from the chamber; injecting a cleaning gas containing Br into the chamber; exhausting by-products generated by the reaction of impurities deposited on the substrate and the cleaning gas in the chamber during the thin film deposition; A method for cleaning a substrate processing apparatus, comprising:
2. Loading a substrate into a chamber; injecting a gas into the chamber to deposit a thin film on the substrate; removing the substrate from the chamber; injecting a cleaning gas containing Br into the chamber; exhausting by-products generated by the reaction of impurities deposited on the substrate and the cleaning gas in the chamber during the thin film deposition; Including, In the step of injecting the cleaning gas, the cleaning gas is injected in a pulsed manner, or The method for cleaning a substrate processing apparatus includes alternately repeating the step of spraying the cleaning gas and the step of exhausting the by-products.
3. 2. The method for cleaning a substrate processing apparatus according to claim 1, further comprising the step of injecting a first auxiliary gas into the interior of the chamber, the first auxiliary gas being capable of decomposing the cleaning gas.
4. The first auxiliary gas is H 2 Gas and O 2 4. The method for cleaning a substrate processing apparatus according to claim 3, further comprising the step of:
5. The method for cleaning a substrate processing apparatus according to claim 1 , further comprising the step of generating a plasma inside the chamber.
6. 6. The method for cleaning a substrate processing apparatus according to claim 5, wherein the step of generating the plasma includes the step of injecting a second auxiliary gas which is an Ar gas.
7. injecting a nitrogen-containing gas into the chamber; 3. The method for cleaning a substrate processing apparatus according to claim 2, wherein the step of injecting the nitrogen-containing gas is performed between the step of injecting the cleaning gas and the step of exhausting the by-products.
8. The cleaning gas may be HBr, KBr, Br 2 , HBrO 3 and CBrF 3 8. The method for cleaning a substrate processing apparatus according to claim 1, wherein a gas containing at least one of the following is used.
9. 8. The method for cleaning a substrate processing apparatus according to claim 1, wherein a temperature inside the chamber is lower than a temperature during a deposition process.
Citation Information
Patent Citations
Film forming method and film forming apparatus
JP2009242835A
Manufacturing method of semiconductor device, cleaning method, substrate processing apparatus, and recording medium
JP2013229575A
Chamber cleaning method
WO2021141438A1
A chemical vapor deposition apparatus and cleaning method of chemical vapor deposition
KR101232904B1