POLYMER MICROSTRUCTURES AND SYSTEMS AND METHODS FOR MAKING SAME - Patent application
Polymeric microneedles with lattice microstructures produced by DLP-CLIP technology address the limitations of existing microneedle technologies by providing efficient drug delivery and biological fluid collection through rapid, high-resolution manufacturing.
Patent Information
- Application Number
- JP2024519039
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-24
- Filing Date
- 2022-09-22
- Publication Date
- 2024-10-16
AI Technical Summary
Existing microneedle technologies for intradermal drug delivery face limitations in achieving high-resolution lattice microstructures, which are crucial for effective drug delivery and biological fluid collection, while also requiring complex manufacturing processes that are slow and inefficient.
The development of polymeric microneedles with lattice microstructures formed by high-resolution continuous liquid interface generation (DLP-CLIP) technology, enabling rapid production of microneedles with precise lattice cell units, varying densities, and enhanced mechanical integrity, allowing for efficient drug delivery and biological fluid collection.
The high-resolution lattice microstructures enable faster manufacturing times, improved mechanical integrity, and enhanced drug delivery capabilities, including sustained release and biological fluid collection, compared to traditional methods.
Smart Images

Figure 2024537764000001_ABST
Abstract
Description
[Background technology]
[0001] The intradermal (ID) space is being actively explored as a means for minimally invasive drug delivery and diagnostics. Intradermal drug delivery is the process of delivering formulations into layers of the skin. ID access requires puncturing the outermost layer of the skin, called the stratum corneum (StC), which is a strong barrier that provides mechanical integrity to the skin. Human skin is a complex multi-layered organ, including the stratum corneum, epidermis, dermis and subcutaneous tissue. Often, these procedures target either the epidermal or dermal layers of the skin, which lie above the blood vessels and nerve fibers of the skin. It offers an attractive alternative to intravenous (IV) injections, which often cause systemic effects and may be particularly advantageous for targeted, localized drug delivery.
[0002] ID drug delivery can provide the ability to deliver compounds that have significant first-pass effects, or metabolism by the liver, which can degrade therapeutic compounds early when administered systemically. Additionally, ID access can also help reduce the pain associated with subcutaneous injections and eliminate the risk of transmitting blood-borne diseases through the generation of hazardous medical waste. ID access can also be self-administered, eliminating reliance on trained medical professionals.
[0003] Microneedles or microneedle patches or microarray patches (MAPs) are composed of a series of micrometer-sized projections that can painlessly puncture the skin and access the epidermis / skin layer. MAPs are used in cosmetics, for example, for use in the treatment of acne scars and stretch marks by penetrating the stratum corneum to create microconduits that stimulate growth factor secretion and collagen production. Microneedles are generally fabricated by a three-step process of master machining, mold machining, and mold filling to produce hollow metal projections with uniform shape. Microneedles are generally manufactured to be produced in a manner similar to that of conventional hypodermic needles. Summary of the Invention
[0004] Aspects of the present disclosure include polymer structures (e.g., microneedles) having a lattice microstructure composed of one or more lattice cell units. The polymer structures according to certain embodiments have repeating lattice cell units formed by high-resolution continuous liquid interfacial generation. Aspects also include systems for manufacturing polymer structures having lattice microstructures. The systems according to certain embodiments include a micro digital light projection system having a light beam generator component and a light projection monitoring component, and a liquid interfacial polymerization module having a build elevator and a build surface and configured to generate a polymer lattice microstructure from a polymerizable composition positioned therebetween. Methods for making polymer structures having lattice microstructures with the subject systems are also provided. A patch having an array of polymer microneedles for application to a skin surface of a subject is also described. In some embodiments, the patch includes microneedles containing an active agent compound (e.g., an immunogenic active agent). A method for applying a patch to a skin surface of a subject is also described.
[0005] In some embodiments, the lattice microstructure of the polymeric structures described herein has two or more repeating lattice cell units, for example, five or more repeating lattice cell units. In certain embodiments, the lattice microstructure has a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the polymeric structure. In some embodiments, the lattice cell units have a lattice shape that is tetrahedral, kagome, rhombic, icosahedral, Voronoi, or triangular. In embodiments, the lattice cells have a unit size of 10 μm to 1000 μm, for example, 200 μm to 500 μm. In some embodiments, the lattice microstructure comprises a plurality of struts. In some cases, the struts have a thickness of 25 μm to 150 μm, for example, 50 μm to 100 μm, for example, 70 μm to 90 μm. The polymeric structures having the desired lattice microstructures may have a length of 500 μm to 2000 μm, for example, 700 μm to 1200 μm. In some embodiments, the lattice microstructure has a volume of 0.01 μL to 2 μL. In embodiments, the polymeric structure is formed from a polymerizable material such as polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethylmethacrylate, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. In certain embodiments, the polymeric structure is formed from polyethylene glycol dimethacrylate (PEGDMA). In some cases, the polymeric material is biodegradable. In some cases, the polymeric structure is soluble in an aqueous medium.
[0006] In some embodiments, the polymeric structures described herein are polymeric microneedles having a lattice microstructure with one or more lattice cell units. In certain embodiments, the lattice microstructure of the polymeric microneedle has two or more repeating lattice cell units. In certain embodiments, the lattice microstructure of the polymeric microneedle has a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle. In some embodiments, the lattice cell units have a lattice shape that is tetrahedral, kagome, rhombic, icosahedral, Voronoi, or triangular. In embodiments, the lattice cells have a unit size of 10 μm to 1000 μm, such as 200 μm to 500 μm. In some embodiments, the lattice microstructure comprises a plurality of struts. In some cases, the struts have a thickness of 25 μm to 150 μm, such as 50 μm to 100 μm, such as 70 μm to 90 μm. The polymeric structure having the desired lattice microstructure may have a length of 500 μm to 2000 μm, for example 700 μm to 1200 μm. In some embodiments, the lattice microstructure has a volume of 0.01 μL to 2 μL. In some embodiments, the microneedle has a regular square pyramid shape. In other embodiments, the microneedle has a conical projection shape. In still other embodiments, the microneedle has a rectangular prism projection shape. In some embodiments, the microneedle includes a tip portion having a solid structure, a body portion having a lattice structure, and a base portion having a solid structure. In these embodiments, the tip portion may have a length of 25 μm to 500 μm, for example 50 μm to 300 μm. In some cases, the microneedle has a tip diameter of 0.1 μm to 10 μm. In some embodiments, the body portion has a length of 50 μm to 1000 μm, for example 50 μm to 300 μm. In some embodiments, the base portion has a length of 25 μm to 500 μm, for example 50 μm to 300 μm. In certain embodiments, the body portion has a lattice microstructure and has a gradient of increasing lattice cell unit density across the longitudinal axis of the body portion of the microneedle.
[0007] In certain embodiments, the polymeric microneedles described herein are dynamic microneedles that can change geometry or shape in response to an applied stimulus. In certain embodiments, the stimulus is an applied mechanical pressure (e.g., pressure when inserted through the skin surface of a subject). In some cases, the dynamic microneedles are flexible and exhibit movement due to elastic deformation of the polymeric microstructure. In some embodiments, the microneedles deploy a barb structure in response to an applied stimulus.
[0008] In embodiments, the polymeric microneedles are formed from a polymerizable material. In some cases, the polymeric microneedles are biodegradable. In some cases, the polymeric microneedles are dissolvable in an aqueous medium, such as when applied intradermally to a subject.
[0009] Aspects of the present disclosure also include a patch having a backing layer and a plurality of polymeric microneedles in contact with the backing layer, each microneedle including a lattice microstructure having one or more lattice cell units. In some embodiments, the plurality of microneedles form an array of microneedles on the backing layer. In some cases, the microneedles are spaced apart from one another on the backing layer by an average distance of 5 μm to 1000 μm, e.g., 100 μm to 500 μm. The patch may include microneedles having different lattice geometries, for example, the patch includes one or more microneedles having a lattice microstructure having a tetrahedral lattice geometry, one or more microneedles having a lattice microstructure having a Kagome lattice geometry, one or more microneedles having a lattice microstructure having a rhombic lattice geometry, one or more microneedles having a lattice microstructure having an icosahedral lattice geometry, one or more microneedles having a lattice microstructure having a Voronoi lattice geometry, or one or more microneedles having a lattice microstructure having a triangular lattice geometry. In some cases, the patch has microneedles with two or more different lattice shapes, for example, three or more different lattice shapes. In certain cases, one or more of the microneedles of the patch have different lengths or different base widths. In certain embodiments, one or more of the microneedles of the patch have different mechanical integrity (e.g., can withstand different loads). In certain embodiments, the subject patch includes one or more dynamic microneedles, such as one or more microneedles that can change geometry or shape, one or more microneedles that exhibit movement due to elastic deformation, or one or more microneedles that deploy a barb structure. In certain embodiments, the subject patch includes a pressure-sensitive adhesive, for example, to keep the patch in contact with the subject's skin surface for an extended period of time.
[0010] In certain embodiments, the polymeric microneedles also include an active agent compound. In some cases, the active agent compound is coated on one or more surfaces of the microneedle. In some cases, the active agent compound is coated on the tip portion of the microneedle. In some cases, the active agent compound is coated on the body portion of the microneedle. In some cases, the active agent compound is coated on the base portion of the microneedle. In some embodiments, the active agent compound is included within the lattice microstructure of the polymeric microneedle. In some embodiments, the active agent compound fills 1% or more of the void volume of the lattice microstructure, such as 10% or more, such as 25% or more (including 50% or more) of the void volume of the lattice microstructure. In some embodiments, each polymeric microneedle includes 0.01 μL or more of active agent, such as 0.05 μL or more (including 0.1 μL or more) of active agent. In some cases, the active agent compound is a small molecule active agent. In other cases, the active agent is an immunogenic active agent, such as a vaccine.
[0011] The present disclosure also includes a method for applying a patch having a plurality of polymeric microneedles to a skin surface of a subject.In some cases, the patch includes microneedles arranged in an array on a backing layer.In certain cases, the patch is applied to a skin surface of a subject and maintained in contact with the subject for an extended period of time, for example, 30 minutes or more, for example, 1 hour or more (including 6 hours or more).In certain cases, the patch is applied to a skin surface of a subject and removed within 15 minutes, for example, 5 minutes or less (including 1 minute or less).
[0012] In some embodiments, the method includes applying a patch to deliver a therapeutically effective amount of an active agent compound to a subject. In these embodiments, the plurality of polymeric microneedles contain an active agent compound, and the patch is maintained in contact with the subject for a period of time sufficient to deliver one or more doses, such as two or more doses (including five or more doses) of the active agent compound. In certain cases, in some cases, the patch is maintained in contact with the subject for a period of time for sustained release of the active agent to the subject. In some cases, the method includes applying the patch to a skin surface of the subject in a manner sufficient to collect a biological fluid sample from the subject into the microneedle. In some embodiments, the method includes collecting interstitial fluid from the subject into the microneedle. In other embodiments, the method includes collecting skin fluid from the subject into the microneedle. In certain cases, the method includes collecting 0.01 μL to 250 μL, for example 0.01 μL to 2 μL, of biological fluid from the subject. In some embodiments, the methods include collecting a biological fluid sample (e.g., interstitial fluid, skin fluid) from a subject to detect an analyte present in the biological sample, such as to detect glucose.
[0013] Aspects of the present disclosure also include a system for fabricating a polymer structure having a lattice microstructure having one or more lattice cell units, such as a polymer microneedle. A system according to certain embodiments includes a micro digital light projection system having a light beam generator component and a light projection monitoring component, and a liquid interfacial polymerization module configured to generate a lattice microstructure from a polymerizable composition including a build elevator and a build surface and positioned therebetween. In some embodiments, the light beam generator component includes a light source, a tube lens, and one or more projection lenses. In some cases, the light beam generator component includes a digital micromirror device. For example, the light beam generator may include two or more projection lenses, such as where one or more of the projection lenses are magnification lenses (e.g., 2x or greater magnification lenses). In some embodiments, the light source is a laser. In other embodiments, the light source is a light emitting diode. In some cases, the light source is a continuous light source. In other cases, the light source is configured to emit light at a predetermined interval, such as a strobe light source. In some embodiments, the light beam generator component is configured to generate a light sheet, such as a light sheet having a predetermined optical pattern. In some embodiments, the optical projection monitoring component includes a photodetector. In some cases, the photodetector includes a charge-coupled device (CCD).
[0014] In some embodiments, the system also includes a processor having a memory operably coupled to the processor, the memory including instructions stored therein that, when executed by the processor, cause the processor to irradiate a polymerizable composition positioned between a build elevator and a build surface to generate a polymerizable composition having a first polymerized region of the polymerizable composition in contact with the build elevator and a first non-polymerized region of the polymerizable composition in contact with the build surface, move the build elevator away from the build surface, and irradiate the first non-polymerized region of the polymerizable composition to generate a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second non-polymerized region in contact with the build surface. These steps are repeated in a manner sufficient to generate a polymer microstructure having a lattice microstructure. In some embodiments, the memory includes instructions to irradiate the polymerizable composition for a period sufficient to bond the first polymerized region of the polymerizable composition to the build elevator. In some embodiments, the memory includes instructions to move the build elevator in predetermined increments of 0.5 μm to 1.0 μm. In some embodiments, the system also includes a source of the polymerizable composition. In some cases, the source is configured to continuously deliver the polymerizable composition to the build surface. In some cases, the system is configured to apply the polymerizable composition to the build surface after each movement of the build elevator away from the build surface. In some embodiments, the light source is configured to irradiate through the build surface. In some cases, at least a portion of the build surface is permeable to a polymerization inhibitor, for example, the polymerization inhibitor is oxygen.
[0015] In some embodiments, the memory includes instructions for determining a focal plane on the build surface from a micro digital light projection system. In some cases, the memory includes instructions for determining the focal plane by illuminating the build surface with a strobe light source through a tube lens and moving the build surface until the light is focused on the build surface through the tube lens. In some cases, the memory includes instructions for illuminating the build surface with a plane of light having a projected image pattern using a strobe light source. In some embodiments, the memory includes instructions for moving the build surface until the projected image pattern is in focus with the build surface. In some cases, the memory includes instructions for generating an image stack including a plurality of projected image patterns. In certain cases, the memory includes instructions for determining a focal plane of the build surface based on the generated image stack. In certain cases, the memory includes instructions for determining a focal plane through a travel depth of the build surface of 400 μm or less. In an embodiment, the system provides for generating polymer structures (e.g., polymer microneedles) having a grating microstructure resolution of 10 μm or less, such as 5 μm or less. In certain embodiments, the system is configured to provide a resolution of between 1.0 μm and 4 μm, for example between 1.5 μm and 3.8 μm.
[0016] Aspects of the present disclosure also include methods for making polymeric microneedles having a lattice microstructure with one or more lattice cell units. The method according to certain embodiments includes irradiating a polymerizable composition positioned between a build elevator and a build surface to generate a polymerizable composition having a first polymerized region of the polymerizable composition in contact with the build elevator and a first non-polymerized region of the polymerizable composition in contact with the build surface, moving the build elevator away from the build surface, irradiating the first non-polymerized region of the polymerizable composition to generate a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second non-polymerized region in contact with the build surface, and repeating in a manner sufficient to generate a microneedle having a lattice microstructure. In some embodiments, the polymerizable composition is in contact with the build elevator and the build surface. In some cases, the method includes irradiating the polymerizable composition for a period of time sufficient to bond the first polymerized region of the polymerizable composition to the build elevator. In some cases, the build elevator is moved in predetermined increments of 0.5 μm to 1.0 μm. In certain cases, the polymerizable composition is applied to the build surface after each movement of the build elevator away from the build surface. In some embodiments, the polymerizable composition is irradiated through the build surface. In some cases, the polymerizable composition is irradiated in the presence of a polymerization inhibitor. In certain embodiments, the polymerizable composition is polymerized continuously while moving the build elevator away from the build surface. In certain cases, the polymerization inhibitor is oxygen and the build surface is permeable to oxygen.
[0017] In some embodiments, the method includes illuminating the polymerizable composition with a micro-digital light projection system. In some instances, the focal plane on the build surface is determined using the micro-digital light projection system. In some embodiments, determining the focal plane on the build surface includes illuminating the build surface with a strobe light source through a tube lens and moving the build surface until the light is focused on the build surface through the tube lens. In some instances, the build surface is illuminated with a plane of light having a projected image pattern using a strobe light source. In certain instances, the build surface is moved (e.g., continuously or at predetermined intervals) until the projected image pattern is in focus with the build surface. In some embodiments, the focal plane is determined with a photodetector of the micro-digital light projection system. In some instances, an image stack is generated having a plurality of projected image patterns. In some embodiments, the focal plane of the build surface is determined from the generated image stack. In certain embodiments, the focal plane is determined through a moving depth of the build surface of 400 μm or less. In embodiments, the methods described herein for producing polymeric microstructures (e.g., polymeric microneedles) having lattice microstructures provide a resolution of 10 μm or less, e.g., 5 μm or less. In certain embodiments, the subject methods provide a resolution of 1.0 μm to 4 μm, e.g., 1.5 μm to 3.8 μm.
[0018] In some embodiments, the method includes preparing a polymeric microneedle with an active agent compound. In some cases, the active agent compound is coated on the surface of the polymeric microneedle. In some embodiments, the active agent compound is coated on the surface of the polymeric microneedle by dip coating or spray coating. In other cases, the active agent compound is dry cast (e.g., as a powder) on the surface of the polymeric microneedle. In some cases, the active agent compound is incorporated into the interior space of the lattice microstructure of the polymeric microneedle. In some cases, the active agent is injected into the lattice microstructure. In other cases, the active agent is introduced into the polymeric microneedle by contacting the lattice microstructure with a composition containing the active agent compound and incorporating the active agent by capillary action. In still other cases, the active agent compound is incorporated into the polymerizable composition and incorporated into the interior space of the polymeric microneedle while forming the lattice microstructure. [Brief description of the drawings]
[0019] The invention can be best understood from the following detailed description when read in conjunction with the accompanying drawing figures, which include:
[0020] [Figure 1] 1 shows a comparison of single-digit μm resolution capabilities with high-resolution digital light projection continuous liquid interface generation, according to certain embodiments. [Figure 2A] 13 shows a line pattern demonstrating 1.5 μm resolution with high resolution digital light projection continuous liquid interface generation according to a specific embodiment. [Figure 2B] 1 shows a comparison of a line pattern, a square array, and a hole array to demonstrate 1.5 μm resolution with high-resolution digital light projection continuous liquid interface generation, according to certain embodiments. [Figure 3A-1] 1 shows an example of a lattice microneedle according to certain embodiments. [Figure 3A-2] 1 shows an example of a lattice microneedle according to certain embodiments. [Figure 3B] 1 shows an example of a lattice microneedle produced by 1.5 μm resolution digital light projection continuous liquid interface generation, according to a specific embodiment. [Figure 4A] 1 shows an example of a lattice microstructure of a polymer microneedle, according to certain embodiments. [Figure 4B] 1 shows different projection and lattice geometries for the lattice microstructure of polymer microneedles. [Diagram 5] 1 shows SEM images of polymer microneedles having triangular shaped lattice microstructures and Voronoi shaped lattice microstructures, according to certain embodiments. [Figure 6A] 1 illustrates a grating microstructure having different densities of grating cell units, according to certain embodiments. [Figure 6B] 1 illustrates a lattice microstructure having a gradient in density per lattice cell, according to certain embodiments. [Figure 7] 1 shows a comparison of the mechanical integrity of different polymer microneedles generated by 1.5 μm resolution digital light projection continuous liquid interface generation, according to certain embodiments. [Figure 8A] 1 shows a polymeric microneedle with a solid active agent compound, according to certain embodiments. [Figure 8B] 1 illustrates a polymeric microneedle with a liquid activator compound, according to certain embodiments. [Figure 8C] 1 illustrates capillary action due to a lattice microstructure, according to certain embodiments. [Figure 9A] Contrast-based focus algorithm for optimization of the projection focal plane. Shown focusing a strobe light onto the build platform by fine-tuning the tube lens (highlighted in green). (i) Build platform out of focus, (ii) Build platform in focus. Scale bar: 2.5 mm. [Figure 9B]Figure 1 shows the contrast-based focus algorithm for optimization of the projection focal plane. By fine-tuning the vertical position of the build platform (highlighted in green), the projected pattern is brought into focus. (i) The projected pattern on the build platform is out of focus, (ii) the adjusted build platform brings the projected pattern into focus. Scale bar: 2.5 mm. [Figure 9C] 1 illustrates a contrast-based focus algorithm for optimization of the projection focal plane; 2 illustrates an edge profile of a projected pattern; [Figure 9D] 1 shows a contrast-based focus algorithm for optimization of the projection focal plane; 2 shows the calculated Modulation Transfer Function (MTF) of the edge profile; [Figure 9E] A contrast-based focus algorithm for optimization of the projection focal plane is shown. Through-focus sharpness performance obtained from a scan close to a rough estimate of the optimal focal plane of 400 μm is shown. The best focal plane with the highest sharpness performance is found and compared to the actual print. The z-position with the highest sharpness also has the best resolution 3D print. Scale bar: 1.0 mm. [Figure 10A] 1 shows a schematic diagram of a single-digit micron resolution continuous liquid interface generation (CLIP)-based 3D printer setup and printing process according to a specific embodiment. 2 shows a schematic diagram of a single-digit micron resolution CLIP-based 3D printer. The 3D printer consists of a UV projector, a projection lens, a resin vat containing an oxygen-permeable window, and a translation stage. [Figure 10B] FIG. 1 illustrates a schematic diagram of a single-digit micron resolution continuous liquid interface generation (CLIP)-based 3D printer setup and printing process according to a specific embodiment. Projection optics including a UV camera and computer for real-time monitoring are shown, where the projected UV light path (purple) is reflected through a beam splitter and the reflected projection (yellow) is captured by the UV camera, thereby enabling real-time monitoring of the projected image and allowing fine adjustment of the focal plane. [Figure 10C]FIG. 1 illustrates a schematic diagram of a single-digit micron resolution continuous liquid interface generation (CLIP)-based 3D printer setup and printing process according to a specific embodiment. The CLIP process is shown to include an oxygen-permeable window that is not only highly transparent to UV (385 nm) but also permeable to oxygen. The permeated oxygen forms a thin layer of dead zone above the window where photopolymerization is inhibited, allowing for continuous 3D printing. [Figure 11A] FIG. 1 shows a schematic diagram of a CLIP setup and printing process according to certain embodiments. A schematic diagram of a typical CLIP printing setup is shown. The setup includes (from bottom to top) a UV light engine emitting UV projection at a wavelength of 385 nm, an oxygen-permeable window, a dead zone (height h) where uncured resin flows, the cured resin, and a build platform moving with a pulling speed U. [Figure 11B] 1 shows a schematic diagram of a CLIP setup and printing process according to certain embodiments, showing a schematic diagram of a step-by-step printing process including (i) an initial step, (ii) stage movement, (iii) stage stop, and (iv) UV exposure, which is repeated throughout the printing process (v). [Figure 12A] FIG. 1 shows a CLIP printing process model including projection optics, velocity flow field, polymerization gradient, and final 3D printed structure, according to a specific embodiment. Simulations of point spread functions (PSFs) from Zemax and Gaussian approximations ((i) for a 30 μm pixel projection lens), and Gaussian approximations ((ii) for a 1.5 μm pixel projection lens). The inset is a 2D visualization of the PSF. [Figure 12B] Figure 1 shows the CLIP printing process model, including projection optics, velocity flow field, polymerization gradient, and final 3D printed structure, according to a specific embodiment. Simulation of complete 3D printing combining optical Gaussian approximation and photopolymerization to predict the overall printing performance of a square pyramidal structure (500 μm wide, 1000 μm high). Inset is an SEM image of the actual 3D printed part (scale bar 250 μm) for comparison. [Figure 13A]1 illustrates dynamic modeling of the CLIP printing process, according to a specific embodiment. Transient photopolymerization gradient simulations: (i) Transient oxygen concentration profile in the dead zone regime; (ii) Transient converted oligomer concentration in the dead zone regime; (iii) Total component concentration in the dead zone regime at t=0.1(-). [Figure 13B] 1 illustrates dynamic modeling of the CLIP printing process, according to certain embodiments, showing steady-state oxygen concentrations in the dead-zone regime for both the analytical equation and the numerical solution from the PDE. [Figure 13C] 1 illustrates dynamic modeling of the CLIP printing process, according to certain embodiments, showing the dead-zone thickness at various values of Dankeler number (Da) from both the analytical formulation and the numerical solution of the PDE. [Figure 13D] 1 illustrates dynamic modeling of the CLIP printing process, according to certain embodiments, and provides parameters used in the study. [Figure 14A] 1 shows mass transport modeling using lubrication theory for the CLIP printing process, according to certain embodiments. (i) shows velocity flow profile in the dead zone regime for a Newtonian fluid, using derived analytical equations. (ii) shows velocity flow profile in the dead zone regime for a non-Newtonian fluid, using derived analytical equations. Note that the non-Newtonian fluid is modeled with a power law fluid with a shear thinning coefficient of n=0.87. [Figure 14B] Figure 1 shows mass transport modeling using lubrication theory for the CLIP printing process according to a specific embodiment. Figure 2 shows direct measurement of Stefan force. Experimental data is obtained by recording Stefan force during the printing process for different 3D printed part radii ranging from 0.5 mm to 2.2 cm. Inset: Load cell experimental setup for Stefan force measurement. [Figure 15A]A demonstration print from a CLIP-based 3D printer with single-digit micron resolution is shown, showing David by Michelangelo (1.2 cm tall) (Florence, Italy). [Figure 15B] A demonstration print from a CLIP-based 3D printer with single-digit micron resolution is shown, showing a Rocky statue (2 cm tall) (Philadelphia, PA, USA). [Figure 15C] A demonstration print from a CLIP-based 3D printer with single-digit micron resolution is shown, showing the Statue of Liberty (1.5 cm) (New York, NY, USA). [Figure 15D] A demonstration print from a CLIP-based 3D printer with single-digit micron resolution is shown, showing a lattice twisted bar (1.25 cm tall). [Figure 15E] A demonstration print from a CLIP-based 3D printer with single-digit micron resolution is shown, showing the Eiffel Tower (Paris, France). [Figure 15F] Demonstration printing from a CLIP-based 3D printer with single-digit micron resolution is shown, showing terraced microneedles. [Figure 15G] Demonstration prints from a CLIP-based 3D printer with single-digit micron resolution are shown, showing a square block array. [Figure 15H] Demonstration prints from a CLIP-based 3D printer with single-digit micron resolution are shown, showing lattice blocks (scale bar 1 mm). [Figure 16A] 1 illustrates a characterization of resolution and print speed of CLIP-based printing, in accordance with certain embodiments, and shows a comparison plot of print speed and resolution between high-resolution CLIP and other high-resolution 3D printing techniques. [Figure 16B]Characterization of resolution and printing speed of CLIP-based printing, according to certain embodiments, showing twisted lattice bars. High-resolution CLIP 3D printing and two-photon polymerization (TPP) (NanoScribe, Germany) shows that the CLIP technique completed a full print in a much shorter printing time compared to the TPP technique. [Figure 16C] FIGURE 2 illustrates characterization of CLIP-based printing resolution and printing speed, according to certain embodiments, showing sample images of a 1.5 μm resolution CLIP printer resolution characterization design with 30 μm (20 pixels), 15 μm (10 pixels), and 7.5 μm (5 pixels) lines (top row), (inset) side view of line resolution, and (bottom row) holes ranging from 37.5 μm (15 pixels) to 18 μm (12 pixels). [Figure 16D] 1 illustrates characterization of resolution and print speed for CLIP-based printing, according to certain embodiments, and shows a summary table of resolution characterization for single-digit micron resolution CLIP-based 3D printers. [Figure 17A] 13 shows details of mesh design line edge profile extraction by focus contrast based sharpness analysis according to one specific embodiment, showing a sample image at a through-focus position 150 μm away from the start of scan position. [Figure 17B] 1 shows details of mesh design line edge profile extraction with focus contrast based sharpness analysis according to a specific embodiment, and shows feature detection, extraction, and centroid analysis applied for full field of view (FOV) at various distances from the image center. [Figure 17C] 13 shows details of mesh design line edge profile extraction by focus contrast based sharpness analysis according to one particular embodiment, and illustrates full FOV edge profile extraction by finding the nearest neighbors of a given centroid. [Figure 17D]Shows details of mesh design line edge profile extraction using focus contrast based sharpness analysis in accordance with one particular embodiment, showing that a 10 pixel wide averaging box is placed around each sampled edge profile to obtain an average edge profile for each edge. [Figure 18A] 1 provides details regarding extraction of feature sizes from line edge profiles in SEM images according to a specific embodiment, showing critical dimension (CD) extraction using an I50 thresholding method. [Figure 18B] 13 shows details regarding the extraction of feature sizes from line edge profiles in SEM images according to one particular embodiment, and shows a sample line edge profile of a line designed to print at 15 μm width. [Figure 18C] 14 shows details regarding extraction of feature sizes from line edge profiles in SEM images according to certain embodiments.15 shows valley-to-peak intensity profile extraction, where polynomial fitting is applied to obtain the midpoint of the intensity profile. [Figure 18D] 14 shows details regarding extraction of feature sizes from line edge profiles in SEM images according to certain embodiments. 15 shows peak-to-valley intensity profile extraction, where polynomial fitting is applied to obtain the midpoint of the intensity profile. [Figure 19A] 1 shows flow sweeps and stress relaxation characterizations performed on two resins, EPU40 and TMPTA resin, according to certain embodiments, showing the flow sweep of the TMPTA resin. [Figure 19B] 1 shows flow sweeps and stress relaxation characterizations performed on two resins, EPU40 and TMPTA resin, according to certain embodiments, showing the flow sweep of EPU40 resin. [Figure 19C] 1 shows flow sweep and stress relaxation characterization performed on two resins, EPU40 and TMPTA resins, according to certain embodiments, illustrating stress relaxation of uncured TMPTA and EPU40 resins. [Figure 20A]1 shows stress relaxation time for different print diameters according to certain embodiments, and illustrates transient stress relaxation versus print diameter for TMPTA resin at different print diameters ranging from dark, 4 mm, 1 cm, 1.6 cm, and 2.2 cm. [Figure 20B] 1 illustrates stress relaxation times for different print diameters, according to certain embodiments, showing extracted stress relaxation times plotted against print diameter. [Figure 21A] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where the inter-layer time is shown to be 50 ms. [Figure 21B] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where the inter-layer time is shown to be 80 ms. [Figure 21C] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where the inter-layer time is shown to be 100 ms. [Figure 21D] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where an inter-layer time of 200 ms is shown. [Figure 21E] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where an inter-layer time of 500 ms is shown. [Figure 21F] 1 illustrates the effect of lateral print resolution and inter-layer time for resin reflow, according to one particular embodiment, where an inter-layer time of 1000 ms is shown. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] Aspects of the present disclosure include polymer structures (e.g., microneedles) having a lattice microstructure composed of one or more lattice cell units. The polymer structures according to certain embodiments have repeating lattice cell units formed by high-resolution continuous liquid interfacial generation. Aspects also include systems for manufacturing polymer structures having lattice microstructures. The systems according to certain embodiments include a micro digital light projection system having a light beam generator component and a light projection monitoring component, and a liquid interfacial polymerization module having a build elevator and a build surface and configured to generate a polymer lattice microstructure from a polymerizable composition positioned therebetween. Methods for making polymer structures having lattice microstructures with the subject systems are also provided. A patch having an array of polymer microneedles for application to a skin surface of a subject is also described. In some embodiments, the patch includes microneedles containing an active agent compound (e.g., an immunogenic active agent). A method for applying a patch to a skin surface of a subject is also described.
[0022] Before the present invention is described in more detail, it is to be understood that the invention is not limited to particular embodiments described, as such may, of course, vary. It is also to be understood that the terminology used herein is for the purpose of describing particular embodiments only, and is not intended to be limiting, since the scope of the present invention will be limited only by the appended claims.
[0023] Where a range of values is provided, unless the context clearly dictates otherwise, it is understood that each intermediate value between the upper and lower limits of that range, to the tenth of the unit of the lower limit, and any other stated or intermediate value within this stated range, is encompassed within the invention. The upper and lower limits of these smaller ranges may individually be included in the smaller ranges, and are also encompassed within the invention, subject to any specifically excluded limits in the stated range. Where the stated range includes one or both of the limits, ranges excluding either or both of those included limits are also encompassed within the invention.
[0024] In this specification, certain ranges are presented with the term "about" preceding numerical values. In this specification, the term "about" is used to provide literal support for the exact number it precedes and for a number that is close to or approximately the number it precedes. When determining whether a number is close to or approximately a specifically recited number, the close or approximate unrecited number may be a number that provides a substantial equivalent to the specifically recited number in the context in which it is presented.
[0025] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs. In addition, any methods and materials similar or equivalent to those described herein can be used in the practice or testing of the present invention, but representative exemplary methods and materials are described below.
[0026] All publications and patents cited herein are incorporated by reference as if each individual publication or patent was specifically and individually indicated to be incorporated by reference to disclose and describe the methods and / or materials in connection with which the publications are cited. The citation of any publication is for its disclosure prior to the date of the present application and should not be construed as an admission that the present invention is not entitled to antedate such publication by virtue of prior invention. Further, the dates of publication provided may be different from the actual publication dates which may need to be independently confirmed.
[0027] It should be noted that, as used in this specification and the appended claims, the articles "a," "an," and "the" include plural referents unless the context clearly dictates otherwise. It should be further noted that the claims may be drafted to exclude any optional element. Thus, this statement is intended to serve as a predicate for use of exclusive terminology such as "solely" and "only" in connection with the recitation of claim elements, or for use of a "negative" limitation.
[0028] As will be apparent to those skilled in the art upon reading this disclosure, each of the separate embodiments described and illustrated herein has separate components and features which may be readily separated from or combined with the features of any of the other various embodiments without departing from the scope or spirit of the invention. Any recited method may be carried out in the order of events recited or in any other order which is logically possible.
[0029] Although the apparatus and methods have been described or will be described for grammatical fluidity with functional descriptions, it is expressly understood that the claims should not be construed as necessarily limited by "means" or "step" limitation constructions unless expressly formulated under 35 U.S.C. 112, but should be accorded the full scope of meaning and equivalents of the definitions provided by the claims under the statutory foundational principles of equivalents, and that if the claims are expressly formulated under 35 U.S.C. 112, then the full legal equivalents under 35 U.S.C. 112 should be accorded.
[0030] As summarized above, the present disclosure provides polymeric microstructures (e.g., microneedles) having a lattice microstructure composed of one or more lattice cell units. In further describing the embodiments of the present disclosure, the polymeric structures having repeating lattice cell units as formed by high-resolution continuous liquid interface generation are first described in more detail. Next, systems and methods for fabricating polymeric microstructures having lattice microstructures are described. Also provided is a patch having an array of polymeric microneedles for application to a skin surface of a subject. In some embodiments, the patch includes microneedles that include an active agent compound (e.g., an immunogenic active agent). A method of applying the patch to a skin surface of a subject is described.
[0031] Polymer microneedles with lattice microstructures An embodiment of the present disclosure includes a polymer microneedle having a lattice microstructure having one or more lattice cell units. As described in more detail below, in certain cases, the polymer structure is formed by high-resolution digital light projection continuous liquid interface generation (e.g., DLP-CLIP), which provides a microarchitecture having a resolution of 100 μm or less, such as 90 μm or less, such as 75 μm or less (including a resolution of 50 μm or less). Figure 1 shows a comparison of single-digit μm resolution capabilities by high-resolution digital light projection continuous liquid interface generation as described herein. In contrast to conventional additive manufacturing such as stereolithography (SLA), direct ink writing (DIW), and two-photopolymerization (TPP), which cannot provide lattice microstructures with resolution as described herein due to low printing resolution, the polymer structures described herein can have pixel sizes of 150 μm×150 μm or less, such as 75 μm×75 μm or less, such as 30 μm×30 μm or less, such as 7.45 μm×7.45 μm or less, such as 3.7 μm×3.7 μm or less (including pixel sizes of 1.5 μm×1.5 μm or less). Figure 2A shows a line pattern to demonstrate 1.5 μm resolution by high-resolution digital light projection continuous liquid interface generation. Figure 2B shows a comparison of a line pattern, a square array, and a hole array to demonstrate 1.5 μm resolution by high-resolution digital light projection continuous liquid interface generation.
[0032] In some embodiments, the methods for making polymeric structures described herein provide increased speed in additive manufacturing, e.g., fabrication can be accomplished in 200 milliseconds or less, e.g., 190 milliseconds or less, e.g., 180 milliseconds or less, e.g., 170 milliseconds or less, e.g., 160 milliseconds or less, e.g., 150 milliseconds or less, e.g., 100 milliseconds or less (including 50 milliseconds or less). In certain cases, high resolution digital light projection continuous liquid interface generation as described herein is 10 times or more faster, e.g., 20 times or more faster, e.g., 50 times or more faster, e.g., 1 ... 2 More than twice as fast, e.g. 10 3More than double means, for example, 10 4 More than twice as fast (10 5 The present invention provides a method for producing polymer structures having lattice microstructures (including in some cases more than twice as fast).
[0033] Additionally, the subject polymeric microneedles have a microarchitecture that includes struts that provide sufficient mechanical integrity for use as a polymeric microneedle to deliver active agent compounds or to collect biological fluids from a subject (e.g., by fluid wicking). The subject polymeric microneedles provide enhanced drug delivery, e.g., by sustained or controlled release, compared to solid microstructures that can only use active agent surface coatings and better mechanical integrity compared to hollow microneedles. FIG. 3A shows an example of a lattice microneedle according to certain embodiments. In some cases, the microarchitecture has a resolution of 30 μm. In some cases, the microarchitecture has a resolution of 1.5 μm. FIG. 3B shows an example of a lattice microneedle produced by 1.5 μm resolution digital light projection continuous liquid interface generation according to certain embodiments. In some cases, the polymeric microneedle has a cell size of 500 μm or 900 μm and a strut size of 100 μm or 120 μm.
[0034] In some embodiments, the lattice microstructure of the polymeric microneedles described herein has two or more repeating lattice cell units, e.g., three or more repeating lattice cell units, e.g., four or more repeating lattice cell units (including five or more repeating lattice cell units). In some cases, the lattice microstructure has a lattice shape selected from tetrahedron, kagome, rhombic, icosahedron, Voronoi, or triangular. In some cases, the lattice microstructure is composed of two or more lattice cell units having different lattice shapes, and the lattice microstructure is composed of three or more different lattice shapes, e.g., four or more different lattice shapes, including cases where the lattice microstructure is composed of five or more different lattice shapes. Figure 4A shows an example of a lattice microstructure of a polymeric microneedle, according to certain embodiments. Figure 4B shows different projection shapes and lattice shapes for the lattice microstructure of a polymeric microneedle.
[0035] In some embodiments, the lattice microstructure is formed from lattice cells having a unit size of 1 μm to 1000 μm, such as 5 μm to 950 μm, for example, 10 μm to 900 μm, for example, 15 μm to 850 μm, for example, 20 μm to 800 μm, for example, 25 μm to 750 μm, for example, 30 μm to 700 μm, for example, 35 μm to 650 μm, for example, 40 μm to 600 μm, for example, 45 μm to 550 μm (including 50 μm to 500 μm, for example, 200 μm to 500 μm). In an embodiment, the lattice microstructure has a volume of 0.01 μL to 25 μL, such as 0.02 μL to 24.5 μL, for example, 0.03 μL to 24 μL, for example, 0.04 μL to 23.5 μL, for example, 0.05 μL to 23 μL, for example, 0.6 μL to 22.5 μL, for example, 0.07 μL to 22 μL, for example, 0.08 μL to 21.5 μL, for example, 0.09 μL to 21 μL, for example, 0.1 μL to 20 μL, for example, 0.5 μL to 19 μL, for example, 1 μL to 18 μL, for example, 2 μL to 17 μL, for example, 3 μL to 16 μL (including 4 μL to 15 μL). As described in more detail below, the polymeric structure may be configured to contain a composition (e.g., a fluid composition) within the lattice microstructure, and in some embodiments, the lattice microstructure is configured to contain a volume of 0.1 μL to 25 μL, e.g., 0.2 μL to 24 μL, e.g., 0.3 μL to 23 μL, e.g., 0.4 μL to 22 μL, e.g., 0.5 μL to 21 μL, e.g., 0.6 μL to 20 μL, e.g., 0.7 μL to 19 μL, e.g., 0.8 μL to 18 μL, e.g., 0.9 μL to 17 μL, including cases where the lattice microstructure is configured to contain a volume of 1 μL to 15 μL. FIG. 5 shows SEM images of polymeric microneedles having triangular shaped lattice microstructures and Voronoi shaped lattice microstructures, according to certain embodiments. The polymeric microneedles were formed using Keysplint hard resin. (Scale bar = 500 μm. CS = cell size, ST = strut thickness).
[0036] In some embodiments, the density of the lattice cell units remains constant throughout the lattice microstructure of the polymer structure of interest. FIG. 6A shows a lattice microstructure having different densities of lattice cell units according to certain embodiments. As shown in FIG. 6A, a polymer microneedle according to certain embodiments can have a low density of lattice cell units, a medium density of lattice cell units, and a high density of lattice cell units. In other embodiments, the density of the lattice cell units varies in one or more portions of the lattice microstructure. In some embodiments, the lattice microstructure includes regions of increased lattice cell density, e.g., the lattice cell density in these regions increases by 1% or more, e.g., 2% or more, e.g., 3% or more, e.g., 4% or more, e.g., 5% or more, e.g., 10% or more, e.g., 20% or more, e.g., 30% or more, e.g., 40% or more (including 50% or more) across the longitudinal axis of the lattice microstructure. In some cases, the regions of increased lattice cell density are present in various increments across the longitudinal axis of the lattice microstructure. For example, regions of increased lattice cell density may be present in increments of every 10 μm or more, e.g., every 20 μm or more, e.g., every 30 μm or more, e.g., every 40 μm or more (including every 50 μm or more) across the longitudinal axis of the lattice microstructure. Figure 6B shows a lattice microstructure having a gradient in density of lattice cell units, according to certain embodiments.
[0037] In some cases, the density of the lattice cell units exhibits a gradient in one or more portions of the lattice microstructure. In certain cases, the density of the lattice cell units increases gradually across the longitudinal axis of the lattice microstructure. For example, the density of the lattice cell units may increase by 1% or more, such as 2% or more, such as 3% or more, such as 4% or more, such as 5% or more, such as 10% or more, such as 20% or more, such as 30% or more, such as 40% or more (including 50% or more) across the longitudinal axis of the lattice microstructure. In some embodiments, the density of the lattice cell units increases in predetermined increments across the longitudinal axis of the lattice microstructure, for example, the density of the lattice cell units increases every 1% or more, such as every 2% or more, such as every 3% or more, such as every 4% or more, such as every 5% or more, such as every 6% or more, such as every 7% or more, such as every 8% or more, such as every 9% or more (including every 10% or more) of length across the longitudinal axis of the lattice microstructure. Depending on the size of the lattice microstructure, the density of lattice cell units may increase by 1 μm or more, such as every 2 μm or more, such as every 3 μm or more, such as every 4 μm or more, such as every 5 μm or more, such as every 10 μm or more, such as every 20 μm or more, such as every 30 μm or more, such as every 40 μm or more (including every 50 μm or more) across the longitudinal axis. For example, the density of lattice cell units may increase by 1% or more across the longitudinal axis of the lattice microstructure, such as 2% or more across the longitudinal axis of the lattice microstructure, such as 5% or more across the longitudinal axis of the lattice microstructure.
[0038] In some embodiments, the lattice microstructure comprises a plurality of struts. The struts according to certain embodiments provide mechanical integrity to the lattice microstructure. In some cases, the struts have a thickness in the range of 1 μm to 200 μm, e.g., 2 μm to 190 μm, e.g., 3 μm to 180 μm, e.g., 4 μm to 170 μm, e.g., 5 μm to 160 μm, e.g., 6 μm to 150 μm, e.g., 7 μm to 140 μm, e.g., 8 μm to 130 μm, e.g., 9 μm to 120 μm, inclusive. For example, the strut size may be 50 μm to 100 μm, e.g., 70 μm to 90 μm, in certain examples (see, e.g., FIG. 3A).
[0039] In some cases, the lattice microstructure exhibits sufficient mechanical integrity to be load-bearing, for example, as a polymeric microneedle (described below) that can be administered to a subject. Depending on the density of the lattice microstructure, in some embodiments, the polymeric structure exhibits sufficient mechanical integrity to support a load of 0.1 N or more, for example, 0.5 N or more, for example, 1 N or more, for example, 2 N or more, for example, 3 N or more, for example, 4 N or more, for example, 5 N or more, for example, 10 N or more, for example, 15 N or more, for example, 20 N or more, for example, 25 N or more, for example, 50 N or more, for example, 75 N or more (including 100 N or more). In some embodiments, the lattice microstructure includes one or more structural support struts disposed within the lattice microstructure to provide increased mechanical integrity, for example, where the mechanical integrity is increased by 5% or more, for example, 25% or more (including 75% or more). For example, the structural support struts may increase the load that the lattice microstructure can support by 0.5 N or more, e.g., 1 N or more, e.g., 5 N or more, e.g., 10 N or more, e.g., 25 N or more, e.g., 50 N or more (100 N or more). In some cases, the structural support struts are positioned within the interior of the lattice microstructure. In other embodiments, the support struts are positioned along the exterior of the lattice microstructure. FIG. 7 shows a comparison of the mechanical integrity of different polymer microneedles generated by digital light projection continuous liquid interface generation at 1.5 μm resolution, according to certain embodiments. Polymer microneedles with lattice microstructures were load tested against square pyramidal solid and faceted microneedles. As shown in FIG. 7, the mechanical integrity of the microneedles increases as the internal volume decreases, where the coarse microlattice microneedles with large internal volume exhibited the lowest mechanical integrity, while the solid square pyramidal microneedles with no internal volume exhibited the greatest mechanical integrity.
[0040] The polymeric microneedles may be any three-dimensional geometric shape, including, but not limited to, straight cross-sectional shapes, such as square, rectangular, trapezoidal, triangular, hexagonal, etc., curved cross-sectional shapes, such as circular, elliptical, etc., and irregular shapes, such as a parabolic bottom joined to a planar top. The polymeric structures having the desired lattice microstructure may have a length of 50 μm to 2000 μm, such as 75 μm to 1950 μm, such as 100 μm to 1900 μm, such as 125 μm to 1850 μm, such as 150 μm to 1800 μm, such as 175 μm to 1750 μm, such as 200 μm to 1700 μm, such as 225 μm to 1650 μm, such as 250 μm to 1600 μm, such as 275 μm to 1550 μm (including 300 μm to 1500 μm). The polymer structure having the desired lattice microstructure may have a width of 50 μm to 1000 μm, such as 75 μm to 950 μm, for example, 100 μm to 900 μm, for example, 125 μm to 850 μm, for example, 150 μm to 800 μm, for example, 175 μm to 750 μm, for example, 200 μm to 700 μm, for example, 225 μm to 650 μm, for example, 250 μm to 600 μm, for example, 275 μm to 550 μm (including 300 μm to 500 μm).
[0041] In embodiments, the polymeric structure is formed from a polymerizable material that may include, but is not limited to, polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethyl cellulose, and blends or copolymers thereof. In certain embodiments, the polymeric structure is formed from polyethylene glycol dimethacrylate (PEGDMA). In certain embodiments, the polymeric structure is formed from trimethylolpropane triacrylate (TMPTA) monomer. In certain embodiments, the polymeric material is selected from polycarbonate, polyvinyl chloride (PVC), polyurethane, polyether, polyamide, polyimide, or copolymers of these thermoplastics such as PETG (glycol modified polyethylene terephthalate), among other polymeric plastic materials. In certain embodiments, the beamsplitter is formed from a polyester, polyesters of interest include, but are not limited to, poly(ethylene terephthalate) (PET), bottle grade PET (a copolymer made based on monoethylene glycol, terephthalic acid, and other comonomers such as isophthalic acid, cyclohexanedimethanol), poly(alkylene terephthalates) such as poly(butylene terephthalate) (PBT) and poly(hexamethylene terephthalate), poly(ethylene adipate), poly(1,4-butylene terephthalate), poly(ethylene glycol adipate), poly(ethylene glycol terephthal ... poly(alkylene adipates) such as poly(hexamethylene adipate), poly(alkylene suberates) such as poly(ethylene suberate), poly(alkylene sebacates) such as poly(ethylene sebacate), poly(ε-caprolactone) and poly(β-propiolactone), poly(alkylene isophthalates) such as poly(ethylene isophthalate), poly(alkylene 2,6-naphthalene-dicarboxylate) such as poly(ethylene 2,6-naphthalene-dicarboxylate), poly(ethylenesulfonyl-4,poly(alkylenesulfonyl-4,4'-dibenzoates) such as poly(4'-dibenzoate), poly(p-phenylene alkylene dicarboxylates) such as poly(p-phenylene ethylene dicarboxylate), poly(trans-1,4-cyclohexanediyl alkylene dicarboxylates) such as poly(trans-1,4-cyclohexanediyl ethylene dicarboxylate), poly(1,4-cyclohexane-dimethylene alkylene dicarboxylates) such as poly(1,4-cyclohexane-dimethylene ethylene dicarboxylate), poly([2.2.2]-bicyclooctane-1,4-dimethylene ethylene dicarboxylate), [2.2.2]-bicyclooctane-1,4-dimethylene alkylene dicarboxylate), lactic acid polymers and copolymers such as (S)-polylactide, (R,S)-polylactide, poly(tetramethylglycolide), and poly(lactide-co-glycolide), as well as polycarbonates of bisphenol A, 3,3'-dimethylbisphenol A, 3,3',5,5'-tetrachlorobisphenol A, 3,3',5,5'-tetramethylbisphenol A, polyamides such as poly(p-phenylene terephthalamide), polyethylene terephthalate (e.g., Mylar™ polyethylene terephthalate), combinations thereof, and the like.
[0042] In some embodiments, the polymeric structure is formed from a polymerizable material that is biodegradable. The term "biodegradable" is used herein in its conventional sense to refer to a material that can be eroded, decomposed, or modified by organisms such as microorganisms, e.g., bacteria. In certain embodiments, the polymerizable material is dissolvable in an aqueous medium. In embodiments in which the polymeric structure is formed from a dissolvable material, the lattice microstructure can be dissolved in water for a period of 0.01 hours or more, such as for example, ...
[0043] In some embodiments, the microneedle comprises a tip portion, a body portion, and a base portion. In embodiments, one or more of the tip portion, body portion, and base portion of the polymeric microneedle have a lattice microstructure as described above. In some cases, one or more of the tip portion, body portion, and base portion have a solid structure (i.e., a completely filled interior space). In some cases, one or more of the tip portion, body portion, and base portion have a hollow interior space. In certain embodiments, the microneedle comprises a tip portion having a solid structure, a body portion having a lattice microstructure, and a base portion having a solid structure. In an embodiment, the tip portion may have a length of 10 μm to 500 μm, for example, 20 μm to 490 μm, for example, 30 μm to 480 μm, for example, 40 μm to 470 μm, for example, 50 μm to 460 μm, for example, 60 μm to 450 μm, for example, 70 μm to 440 μm, for example, 80 μm to 430 μm, for example, 90 μm to 420 μm, for example, 100 μm to 410 μm, for example, 110 μm to 400 μm, for example, 120 μm to 390 μm, for example, 130 μm to 380 μm, for example, 140 μm to 370 μm (including 150 μm to 360 μm). In some cases, the microneedles have a tip diameter of from 0.1 μm to 10 μm, such as from 0.5 μm to 9 μm, such as from 1 μm to 8 μm (including from 2 μm to 7 μm). In some embodiments, the main body portion has a length of 10 μm to 500 μm, for example, 20 μm to 490 μm, for example, 30 μm to 480 μm, for example, 40 μm to 470 μm, for example, 50 μm to 460 μm, for example, 60 μm to 450 μm, for example, 70 μm to 440 μm, for example, 80 μm to 430 μm, for example, 90 μm to 420 μm, for example, 100 μm to 410 μm, for example, 110 μm to 400 μm, for example, 120 μm to 390 μm, for example, 130 μm to 380 μm, for example, 140 μm to 370 μm (including 150 μm to 360 μm).In some embodiments, the base portion has a length of 10 μm to 500 μm, for example, 20 μm to 490 μm, for example, 30 μm to 480 μm, for example, 40 μm to 470 μm, for example, 50 μm to 460 μm, for example, 60 μm to 450 μm, for example, 70 μm to 440 μm, for example, 80 μm to 430 μm, for example, 90 μm to 420 μm, for example, 100 μm to 410 μm, for example, 110 μm to 400 μm, for example, 120 μm to 390 μm, for example, 130 μm to 380 μm, for example, 140 μm to 370 μm (including 150 μm to 360 μm).
[0044] In some embodiments, the lattice microstructure of the polymeric microneedles is formed from lattice cells having a unit size of 1 μm to 1000 μm, such as 5 μm to 950 μm, for example, 10 μm to 900 μm, for example, 15 μm to 850 μm, for example, 20 μm to 800 μm, for example, 25 μm to 750 μm, for example, 30 μm to 700 μm, for example, 35 μm to 650 μm, for example, 40 μm to 600 μm, for example, 45 μm to 550 μm (including 50 μm to 500 μm, for example, 200 μm to 500 μm). In an embodiment, the polymer microneedle has a volume of 0.01 μL to 25 μL, for example, 0.02 μL to 24.5 μL, for example, 0.03 μL to 24 μL, for example, 0.04 μL to 23.5 μL, for example, 0.05 μL to 23 μL, for example, 0.6 μL to 22.5 μL, for example, 0.07 μL to 22 μL, for example, 0.08 μL to 21.5 μL, for example, 0.09 μL to 21 μL, for example, 0.1 μL to 20 μL, for example, 0.5 μL to 19 μL, for example, 1 μL to 18 μL, for example, 2 μL to 17 μL, for example, 3 μL to 16 μL (including 4 μL to 15 μL). In some embodiments, the polymeric microneedle is configured to deliver (e.g., administer an active agent to a subject by injection) a volume of between 0.1 μL and 25 μL, such as between 0.2 μL and 24 μL, such as between 0.3 μL and 23 μL, such as between 0.4 μL and 22 μL, such as between 0.5 μL and 21 μL, such as between 0.6 μL and 20 μL, such as between 0.7 μL and 19 μL, such as between 0.8 μL and 18 μL, such as between 0.9 μL and 17 μL, including where the lattice microstructure is configured to contain a volume of between 1 μL and 15 μL.
[0045] In certain embodiments, the polymeric microneedles described herein are dynamic microneedles that can change geometry or shape in response to an applied stimulus. In certain embodiments, the stimulus is an applied mechanical pressure (e.g., pressure when inserted through the skin surface of a subject). In some cases, the dynamic microneedles are flexible and exhibit movement due to elastic deformation of the polymeric microstructure. In some embodiments, the microneedles deploy a barb structure in response to an applied stimulus.
[0046] In certain embodiments, the polymeric microneedles also include an active agent compound. The amount of active agent compound that can be incorporated into the lattice microstructure of the polymeric microneedles described herein can vary from picogram levels to milligram levels depending on the size of the microneedle. In some embodiments, the active agent compound is a solid. In some cases where the active agent is a solid, the active agent is coated onto the surface of the lattice microstructure of the polymeric microneedle (e.g., by spray coating or dip coating). In some embodiments, the active agent compound is a liquid. In some cases where the active agent compound is a liquid, the active agent is incorporated into the lattice microstructure by liquid injection or dip coating. In certain cases, the liquid active agent compound is incorporated into the lattice microstructure by capillary action. Figure 8A shows a polymeric microneedle with a solid active agent compound according to certain embodiments. The solid active agent compound shown in Figure 8A is coated onto the surface of the lattice microstructure. Figure 8B shows a polymeric microneedle with a liquid active agent compound according to certain embodiments. The solid active agent compound shown in Figure 8B is incorporated into the interior of the lattice microstructure by capillary action. 8C shows capillary action due to a lattice microstructure, according to certain embodiments. A polymeric microneedle having a lattice microstructure as described herein is placed in a dyed solution. After leaving the lattice microstructure in the dyed solution for a period of time, the dyed solution fills the interior volume of the lattice microstructure.
[0047] Active agent compounds of interest include horseradish peroxidase, phenolsulfonphthalein, nucleotides, nucleic acids (e.g., oligonucleotides, polynucleotides, siRNA, shRNA), aptamers, antibodies or portions thereof (e.g., antibody-like molecules), hormones (e.g., insulin, testosterone), growth factors, enzymes (e.g., peroxidases, lipases, amylases, organophosphate dehydrogenases, ligases, restriction endonucleases, ribonucleases, RNA or DNA polymerases, glucose oxidase, lactase). , cells (e.g., red blood cells, stem cells), bacteria or viruses, other proteins or peptides, small molecules (e.g., drugs, dyes, amino acids, vitamins, antioxidants), lipids, carbohydrates, chromophores, luminescent organic compounds (e.g., luciferin, carotene), and luminescent inorganic compounds (e.g., chemical dyes and / or contrast enhancing agents such as indocyanine green), immunogenic substances such as vaccines, antibiotics, antifungals, antivirals, therapeutic agents, diagnostic agents or prodrugs, analogs, or combinations of any of the foregoing.
[0048] Examples of immunogenic vaccine materials that may be included in the microneedles described herein include BIOTHRAX® (anthrax vaccine adsorbed, Emergent Biosolutions, Rockville, Md.); TICE® BCG Live (Bacillus Calmette-Guerin for intravesical use, Organon Tekina Corp. LLC, Durham, NC); MYCOBAX® BCG Live (Sanofi Pasteur Inc); DAPTACEL® (diphtheria and tetanus toxins and acellular pertussis [DTaP] adsorbed, Sanofi Pasteur Inc.); INFANRIX® (DTaP vaccine adsorbed, GlaxoSmithKline); TRIPEDIA® (DTaP vaccine, Sanofi Pasteur); TRIHIBIT® (DTaP / Hib, Sanofi Pasteur); pasteur); KINRIX® (diphtheria and tetanus toxins, adsorbed acellular pertussis and inactivated poliovirus vaccine, GlaxosmithKline); PEDIARIX® (DTaP-HepB-IPV, GlaxoSmithKline); PENTACEL® (diphtheria and tetanus toxins and adsorbed acellular pertussis), inactivated poliovirus and Haemophilus b conjugate [tetanus toxin conjugate] vaccine, sanofi pasteur); adsorbed diphtheria and tetanus toxins (for children, Sanofi Pasteur); DECAVAC® (adsorbed diphtheria and tetanus toxins, for adults, Sanofi Pasteur); ACTHIB® (Haemophilus b tetanus toxin conjugate vaccine, Sanofi Pasteur; PEDVAXHIB® (Hib vaccine, Merck); Hiberix (Haemophilus b tetanus toxin conjugate vaccine, booster dose, GlaxoSmithKline); COMVAX® (Hepatitis B-Hib vaccine, Merck); HAVRIX® (Hepatitis A vaccine, for children, GlaxoSmithKline); VAQTA (Hepatitis A vaccine, for children, Merck); ENGERIX-B® (HepB, Pediatric, Adolescent, GlaxoSmithKline; RECOMBIVAX® (Hepatitis B vaccine, Merck), TWINRIX® (HepA / HepB vaccine, ages 18 and older, GlaxoSmithKline), CERVARIX® (Human papillomavirus bivalent [types 16 and 18] vaccine, recombinant, GlaxoSmithKline), GARDASIL® (Human papillomavirus bivalent [types 6, 11, 16 and 18] vaccine, recombinant, Merck), AFLURIA® (Influenza vaccine, ages 18 and older, CSL), AGRIFLU™ (Influenza virus vaccine for intramuscular injection, Novartis Vaccines), FLUARIX® (Influenza Vaccine, Ages 18 and Up, GlaxoSmithKline), FLULAVAL® (Influenza Vaccine, Ages 18 and Up, GlaxoSmithKline), FLUVIRIN® (Influenza Vaccine, Ages 4 and Up, Novartis Vaccine), FLUZONE® (Influenza Vaccine, Ages 6 Months and Up, Sanofi Pasteur), FLUMIST® (Influenza Vaccine, Ages 2 and Up, Medimmune), IPOL® (e-IPV Polio Vaccine, Sanofi Pasteur), JE VAX® (Inactivated Japanese Encephalitis Virus Vaccine, BIKEN, Japan), IXIARO® (Inactivated Japanese Encephalitis Virus Vaccine, Novartis), MENACTRA® (Meningococcal [Groups A, C, Y and W-135] and Diphtheria Vaccine, Sanofi Pasteur), MENOMUNE®-A / C / Y / W-135 (Meningococcal polysaccharide vaccine, sanofi pasteur), MMRII® (MMR vaccine, Merck), MENVEO® (Meningococcal [groups A, C, Y and W-135] oligosaccharide diphtheria CRM197 conjugate vaccine, NovartisSanofi Pasteur), POLIO VAX™ (Inactivated Poliovirus, Sanofi Pasteur), IMOVAX™ (Rabies Vaccine, Sanofi Pasteur), RABAVERT™ (Rabies Vaccine, Chiron), ROTATEQ™ (Rotavirus Vaccine, Live, Oral Pentavalent, Merck), ROTARIX™ (Rotavirus, Live, Oral Vaccine, GlaxoSmithKline), DECAVAC™ (Tetanus and Diphtheria Toxic Vaccine, Sanofi Pasteur), PROQUAD™ (MMR and Varicella Vaccine, Merck), PNEUMOVAX23™ (Pneumococcal Polysaccharide Vaccine, Merck), PREVNAR™ (Pneumococcal Vaccine, 7-valent, Wyeth / Lederle), PREVNAR-13™ (Pneumococcal Vaccine, 13-valent, Wyeth / Lederle), POLIO VAX™ (Inactivated Poliovirus, Sanofi Pasteur), IMOVAX™ (Rabies Vaccine, Sanofi Pasteur), RABAVERT™ (Rabies Vaccine, Chiron), ROTATEQ™ (Rotavirus Vaccine, Live, Oral Pentavalent, Merck), ROTARIX™ (Rotavirus, Live, Oral Vaccine, GlaxoSmithKline), DECAVAC™ (Tetanus and Diphtheria Toxic Vaccine, Sanofi Pasteur), pasteur), Td(generic) (tetanus and diphtheria toxins, adsorbed, Massachusetts Biol. Labs), TYPHIMV1® (Typhoid Vi Polysaccharide Vaccine, Sanofi Pasteur), ADACEL® (tetanus toxin, reduced diphtheria toxin and acellular pertussis, sanofi pasteur), BOOSTRIX® (tetanus toxin, reduced diphtheria toxin and acellular pertussis, GlaxoSmithKline), VIVOTIF® (Tetanus Vaccine Live Oral Ty21a, Bema Biotech), ACAM2000™ (Smallpox (Cowpox) Vaccine, Live, Acambis, Inc.), DRYVAX (Smallpox (Cowpox) Vaccine), VARIVAX® (Varicella [Live] Vaccine, Merck), YF-VAX® (Yellow Fever Vaccine, Sanofi Pasteur); ZOSTAVAX®, (Varicella Zoster, Merck), or combinations thereof. Any vaccine product listed in the Centers for Disease Control and Prevention (CDC) database may also be included in the compositions described herein.
[0049] The term small molecule is used herein in its conventional sense to refer to naturally occurring or synthetic molecules, including, but not limited to, peptides, peptidomimetics, amino acids, amino acid analogs, polynucleotides, polynucleotide analogs, aptamers, nucleotides, nucleotide analogs, organic or inorganic compounds (i.e., including heteroorganic and organometallic compounds) having a molecular weight of less than about 10,000 grams per mole, organic or inorganic compounds having a molecular weight of less than about 5,000 grams per mole, organic or inorganic compounds having a molecular weight of less than about 1,000 grams per mole, organic or inorganic compounds having a molecular weight of less than about 500 grams per mole, as well as salts, esters, and other pharma- ceutically acceptable forms of such compounds.
[0050] The term "antibiotic" is used herein to describe a compound that acts as an antibacterial, bacteriostatic, or bactericidal agent. Exemplary antibiotics include, but are not limited to, penicillins, cephalosporins, penems, carbapenems, monobactams, aminoglycosides, sulfonamides, macrolides, tetracyclines, lincosides, quinolones, chloramphenicol, vancomycin, metronidazole, rifampin, isoniazid, spenquinomycin, trimethoprim, and sulfamethoxazole.
[0051] In some embodiments, the active agent compounds include steroids and steroid esters (e.g., estrogen, progesterone, testosterone, androsterone, cholesterol, norethindrone, digoxigenin, cholic acid, deoxycholic acid, and chenodeoxycholic acid), boron-containing compounds (e.g., carboranes), chemotherapeutic nucleotides, drugs (e.g., antibiotics, antivirals, and antifungals), enediynes (e.g., calicheamicin, esperamicin, dynemicin, neocarzinostatin chromophore, and kedarcidin chromophore), heavy metal complexes, e.g., cisplatin, cyclohexyl esters ... Examples of suitable therapeutic agents include, but are not limited to, ribozymes (e.g., ribozymes), hormone antagonists (e.g., tamoxifen), non-specific (non-antibody) proteins (e.g., sugar oligomers), oligonucleotides that bind to a target nucleic acid sequence (e.g., an antisense oligonucleotide (e.g., an mRNA sequence)), peptides, proteins, antibodies, photodynamic agents (e.g., rhodamine 123), radionuclides (e.g., I-131, Re-186, Re-188, Y-90, Bi-212, At-211, Sr-89, Ho-166, Sm-153, Cu-67, and Cu-64), toxins (e.g., ricin), and transcription-based pharmaceuticals.
[0052] In certain embodiments, the polymeric microneedles include an active agent compound selected from acetaminophen, nonsteroidal anti-inflammatory drugs (NSAIDs), corticosteroids, narcotics, anticonvulsants, local anesthetics, and any combination thereof.Various aspects of the microneedles provided herein include, but are not limited to, ibuprofen, naproxin, aspirin, fenoprofen, flurbiprofen, ketoprofen, oxaprozin, diclofenac sodium, etodolac, indomethacin, ketorolac, sulindac, tolmetin, meclofenamate, mefenamic acid, nabumetone, piroxicam, and COX-2 inhibitors.In some cases, the analgesic may include a combination of acetaminophen (e.g., acetaminophen and a narcotic), such as acetaminophen and codeine, acetaminophen and hydrocodone, and acetaminophen and oxycodone.
[0053] In some cases, the active agent compound is coated on one or more surfaces of the microneedle. In some cases, the active agent compound is coated on the tip portion of the microneedle. In some cases, the active agent compound is coated on the body portion of the microneedle. In some cases, the active agent compound is coated on the base portion of the microneedle. In some embodiments, the active agent compound is contained within the lattice microstructure of the polymer microneedle. In some embodiments, the active agent compound fills 1% or more, such as 2% or more, such as 3% or more, such as 4% or more, such as 5% or more, such as 6% or more, such as 7% or more, such as 8% or more, such as 9% or more, such as 10% or more, such as 15% or more, such as 20% or more, such as 25% or more (including 50% or more of the void volume of the lattice microstructure). In some embodiments, each polymeric microneedle comprises 0.01 μL or more of active agent compound, such as 0.05 μL or more, such as 0.1 μL or more, for example, 0.2 μL or more, such as 0.3 μL or more, for example, 0.4 μL or more, such as 0.5 μL or more, such as 1 μL or more, for example, 2 μL or more, such as 3 μL or more, for example, 4 μL or more, such as 5 μL (including 10 μL or more) of active agent compound.
[0054] In certain embodiments, the active agent compound further comprises one or more excipients, such as one or more pharma- ceutically acceptable excipients. In certain embodiments, the excipient comprises a stabilizing excipient. In certain cases, the excipient allows the active agent compound to dissolve. A wide variety of pharma-ceutically acceptable excipients are known in the art and need not be discussed in detail herein. Pharmaceutically acceptable excipients are well described in a variety of publications, including, for example, A. Gennaro (2000) "Remington: The Science and Practice of Pharmacy, 20th edition, Lippincott, Williams, & Wilkins, Pharmaceutical Dosage Forms and Drug Delivery Systems (1999) H. C. Ansel et al., eds., 7.sup.th ed., Lippincott, Williams, & Wilkins, and Handbook of Pharmaceutical Excipients (2000) A. H. Kibbe et al., eds., 3.sup.rd ed. Amer. Pharmaceutical Assoc.For example, the one or more excipients may be sucrose, starch, mannitol, sorbitol, lactose, glucose, cellulose, talc, calcium phosphate or calcium carbonate, a binder (e.g., cellulose, methylcellulose, hydroxymethylcellulose, polypropylpyrrolidone, polyvinylpyrrolidone, gelatin, gum arabic, poly(ethylene glycol), sucrose or starch), a disintegrant (e.g., starch, carboxymethylcellulose, hydroxypropyl starch, low-substituted hydroxypropyl cellulose, sodium bicarbonate, calcium phosphate or calcium citrate), a lubricant (e.g., sucrose, starch, hydroxypropyl starch, low-substituted hydroxypropyl cellulose, sodium bicarbonate, calcium phosphate or calcium citrate), a binder (e.g., cellulose, methylcellulose, hydroxymethylcellulose, polypropylpyrrolidone, polyvinylpyrrolidone, gelatin, gum arabic, poly(ethylene glycol), sucrose or starch), a disintegrant (e.g., starch, carboxymethylcellulose, hydroxypropyl starch, low-substituted hydroxypropyl cellulose, sodium bicarbonate, calcium phosphate or calcium citrate), a binder (e.g., cellulose, methylcellulose, hydroxypropyl starch, low-substituted hydroxypropyl cellulose, sodium bicarbonate, calcium phosphate or calcium citrate), a binder (e.g., cellulose, methylcellulose, hydroxypropyl cellulose ... Magnesium tearate, light anhydrous silicic acid, talc or sodium lauryl sulfate), flavoring agents (e.g., citric acid, menthol, glycine or orange powder), preservatives (e.g., sodium benzoate, sodium bisulfite, methylparaben or propylparaben), stabilizers (e.g., citric acid, sodium citrate or acetic acid), suspending agents (e.g., methylcellulose, polyvinylpyrrolidone or aluminum stearate), dispersing agents (e.g., hydroxypropylmethylcellulose), diluents (e.g., water), and base waxes (e.g., cocoa butter, white petrolatum or polyethylene glycol).
[0055] The active agent compound can be formulated into a pharmaceutical composition by combining with a suitable pharma- ceutically acceptable carrier or diluent, and can be formulated into a solid, semi-solid, liquid or gaseous preparation, such as powder, granule, solution, injection, inhalant, etc. In certain embodiments, the active agent compound is formulated for injection. For example, the subject composition can be formulated for interstitial or dermal administration.
[0056] In the pharmaceutical dosage form, the active agent compound may be administered in the form of its pharma- ceutically acceptable salt, or may be used alone or in suitable associations, as well as in combination with other pharma- ceutically active compounds. The following methods and excipients are merely illustrative and in no way limiting.
[0057] In some embodiments, the composition of interest comprises an aqueous buffer. Suitable aqueous buffers include, but are not limited to, acetate, succinate, citrate, and phosphate buffers, ranging in strength from about 5 mM to about 100 mM. In some embodiments, the aqueous buffer comprises a reagent that provides an isotonic solution. Such reagents include, but are not limited to, sodium chloride, and sugars, such as mannitol, dextrose, sucrose, and the like. In some embodiments, the aqueous buffer further comprises a non-ionic surfactant, such as polysorbate 20 or 80. In some cases, the composition of interest further comprises a preservative. Suitable preservatives include, but are not limited to, benzyl alcohol, phenol, chlorobutanol, benzalkonium chloride, and the like. In many cases, the composition is stored at about 4° C. The formulation may also be lyophilized, which generally includes a cryoprotectant, such as sucrose, trehalose, lactose, maltose, mannitol, and the like. Lyophilized formulations can be stored for extended periods of time, even at ambient temperatures.
[0058] In some embodiments, the compositions contain other additives such as lactose, mannitol, corn starch or potato starch, binders such as crystalline cellulose, cellulose derivatives, acacia, corn starch or gelatin, disintegrating agents such as corn starch, potato starch or sodium carboxymethylcellulose, lubricants such as talc or magnesium stearate, and optionally diluents, buffers, wetting agents, preservatives and flavorings.
[0059] When the composition is formulated for injection (subcutaneous or cutaneous injection), the active agent compound can be formulated by dissolving, suspending or emulsifying in an aqueous or non-aqueous solvent such as vegetable or other similar oils, synthetic fatty acid glycerides, esters of higher fatty acids or propylene glycol, and may contain conventional additives such as solubilizers, isotonicity agents, suspending agents, emulsifying agents, stabilizers and preservatives, as necessary.
[0060] Patch with multiple polymer microneedles Aspects of the present disclosure also include patches having a backing layer and a plurality of polymeric microneedles (described in detail above) in contact with the backing layer. In some embodiments, the patch provides transdermal administration of one or more active agent compounds. In other embodiments, the patch can be used to collect a biological fluid sample by applying the patch to a skin surface of a subject. The term "transdermal" is used in its traditional sense to refer to a route of administration in which an active agent (i.e., a drug) is delivered across the skin (e.g., topical administration) or mucosa, or a biological sample such as interstitial fluid is collected from a subject (e.g., for analyte detection in the biological sample).
[0061] In embodiments, the patch comprises a plurality of polymeric microneedles. In some embodiments, the patch comprises 5 or more microneedles, such as 10 or more microneedles, such as 15 or more microneedles, such as 20 or more microneedles, such as 25 or more microneedles, such as 50 or more microneedles, such as 100 or more microneedles, such as 250 or more microneedles, such as 500 or more microneedles (including 1000 or more microneedles). In some embodiments, the plurality of microneedles forms an array of microneedles on the backing layer. In some cases, the polymeric microneedles are arranged in one or more lines on the backing layer. For example, the polymeric microneedles may be arranged along two or more parallel lines, such as three or more, such as four or more, such as five or more, such as six or more, such as seven or more, such as eight or more, such as nine or more, such as ten or more, such as fifteen or more, such as twenty or more (including twenty-five or more) parallel lines of microneedles. In certain cases, the polymeric microneedles are arranged in geometric configurations, including, but not limited to, square, rectangular, trapezoidal, triangular, hexagonal, heptagonal, octagonal, nonagonal, decagonal, dodecagonal, circular, elliptical, and irregular shaped configurations.
[0062] In some embodiments, the microneedles are spaced apart from one another on the backing layer by an average distance of 1 μm to 1000 μm, such as 2 μm to 950 μm, for example, 3 μm to 900 μm, for example, 4 μm to 850 μm, for example, 5 μm to 800 μm, for example, 6 μm to 750 μm, for example, 7 μm to 700 μm, for example, 8 μm to 650 μm, for example, 9 μm to 600 μm, for example, 10 μm to 550 μm, for example, 15 μm to 500 μm, for example, 20 μm to 450 μm (including 25 μm to 400 μm). The multiple polymeric microneedles may each be the same size, or the patch may include multiple polymeric microneedles having different sizes. Each polymeric microneedle may independently have a length of 50 μm to 2000 μm, such as 75 μm to 1950 μm, for example, 100 μm to 1900 μm, for example, 125 μm to 1850 μm, for example, 150 μm to 1800 μm, for example, 175 μm to 1750 μm, for example, 200 μm to 1700 μm, for example, 225 μm to 1650 μm, for example, 250 μm to 1600 μm, for example, 275 μm to 1550 μm (including 300 μm to 1500 μm). Each polymeric microneedle may independently have a width (or diameter if the polymeric microneedle has a circular cross section) of 50 μm to 1000 μm, such as 75 μm to 950 μm, for example 100 μm to 900 μm, for example 125 μm to 850 μm, such as 150 μm to 800 μm, for example 175 μm to 750 μm, such as 200 μm to 700 μm, for example 225 μm to 650 μm, such as 250 μm to 600 μm, for example 275 μm to 550 μm (including 300 μm to 500 μm).
[0063] The multiple polymeric microneedles may each have a lattice microstructure that is the same shape, or the patch may include multiple polymeric microneedles with lattice microstructures that have different shapes. In some embodiments, the patch includes microneedles with different lattice shapes, for example, the patch includes one or more microneedles with a lattice microstructure with a tetrahedral lattice shape, one or more microneedles with a lattice microstructure with a Kagome lattice shape, one or more microneedles with a lattice microstructure with a rhombic lattice shape, one or more microneedles with a lattice microstructure with an icosahedral lattice shape, one or more microneedles with a lattice microstructure with a Voronoi lattice shape, or one or more microneedles with a lattice microstructure with a triangular lattice shape. In some cases, the patch has microneedles with two or more different lattice shapes, for example, three or more different lattice shapes. In certain cases, one or more of the microneedles of the patch have different lengths or different base widths. In certain embodiments, one or more of the microneedles of the patch have different mechanical integrity (e.g., can withstand different loads). In certain embodiments, the subject patch comprises one or more dynamic microneedles, such as one or more microneedles that can change geometry or shape, one or more microneedles that exhibit movement due to elastic deformation, or one or more microneedles that deploy a barbed structure.
[0064] In certain embodiments, the patch comprises one or more polymeric microneedles comprising an active agent compound, for example, 1% or more of the polymeric microneedles of the patch, for example, 2% or more, for example, 3% or more, for example, 4% or more, for example, 5% or more, for example, 10% or more, for example, 15% or more, for example, 20% or more, for example, 25% or more, for example, 50% or more, for example, 75% or more, for example, 90% or more, for example, 95% or more, for example, 97% or more (including 99% or more) of the polymeric microneedles of the patch comprise an active agent compound. Active agents of interest are described in detail above. In some cases, the active agent compound is a small molecule active agent. In some cases, the active agent compound is an immunogenic active agent, such as a vaccine.
[0065] In some cases, the active agent compound is coated on a surface of one or more of the plurality of microneedles. In some cases, the active agent compound is coated on a tip portion of one or more of the plurality of microneedles. In some cases, the active agent compound is coated on a body portion of one or more of the plurality of microneedles. In some cases, the active agent compound is coated on a base portion of one or more of the plurality of microneedles. In some embodiments, the active agent compound is included within a lattice microstructure of one or more of the plurality of microneedles. In some embodiments, the active agent compound fills 1% or more, such as 2% or more, such as 3% or more, such as 4% or more, such as 5% or more, such as 6% or more, such as 7% or more, such as 8% or more, such as 9% or more, such as 10% or more, such as 15% or more, such as 20% or more, such as 25% or more (including 50% or more of the void volume of the lattice microstructure). In some embodiments, each polymeric microneedle independently comprises 0.01 μL or more of active agent compound, such as 0.05 μL or more, such as 0.1 μL or more, for example, 0.2 μL or more, such as 0.3 μL or more, for example, 0.4 μL or more, such as 0.5 μL or more, such as 1 μL or more, such as 2 μL or more, for example, 3 μL or more, such as 4 μL or more, for example, 5 μL (including 10 μL or more) of active agent compound.
[0066] In some embodiments, the polymeric microneedles are configured to release the active agent compound from the lattice microstructure over a period of 0.01 hours or more, such as over 0.05 hours or more, for example, over 0.1 hours or more, for example, over 0.5 hours or more, for example, over 1 hour or more, such as over 2 hours or more, for example, over 6 hours or more, for example, over 12 hours or more, for example, over 18 hours or more, for example, over 24 hours or more, such as over 36 hours or more, for example, over 48 hours or more, for example, over 72 hours or more, for example, over 96 hours or more, for example, over 120 hours or more, such as over 144 hours or more (including 168 hours or more). In certain cases, the active agent compound is released from the microneedle upon insertion or over a period of time, for example, the active agent compound is released over a period of about 1 minute to about 6 months, over a period of about 1 minute to about 3 months, over a period of about 1 minute to about 1 month, over a period of about 1 minute to about 2 weeks, over a period of about 1 minute to about 1 week, over a period of about 1 minute to about 3 days, over a period of about 1 minute to about 1 day, over a period of about 1 minute to about 12 hours, over a period of about 1 minute to about 6 hours, over a period of about 1 minute to about 1 hour. For example, the active agent compound is released from the microneedle over a period of about 1 minute to about 30 minutes, over a period of about 30 minutes to about 6 months, over a period of about 1 hour to about 6 months, over a period of about 6 hours to about 6 months, over a period of about 12 hours to about 6 months, over a period of about 1 day to about 6 months, over a period of about 3 days to about 6 months, over a period of about 1 week to about 6 months, over a period of about 2 weeks to about 6 months, over a period of about 1 month to about 6 months, or over a period of about 3 months to about 6 months. In certain embodiments, the active agent compound is released from the microneedle over a period of less than about 1 minute, over a period of about 1 second to about 1 minute, over a period of about 1 second to about 30 seconds, over a period of about 1 second to about 10 seconds, over a period of about 10 seconds to about 1 minute, or over a period of about 30 seconds to about 1 minute.
[0067] In some cases, the patch includes a polymeric microneedle configured to collect a biological fluid sample from a subject. In some embodiments, the polymeric microneedle is configured to draw the biological fluid into the microneedle, such as through capillary action. Depending on the size of the lattice microstructure, the polymeric microneedle includes 0.01 μL or more of biological fluid, such as 0.05 μL or more, such as 0.1 μL or more, such as 0.2 μL or more, such as 0.3 μL or more, such as 0.4 μL or more, such as 0.5 μL or more, such as 1 μL or more, such as 2 μL or more, such as 3 μL or more, such as 4 μL or more, such as 5 μL (including 10 μL or more). The biological fluid may be collected within the polymeric microneedle for 1 second or more, such as 5 seconds or more, for example, 10 seconds or more, such as 15 seconds or more, for example, 30 seconds or more, such as 1 minute or more, for example, 5 minutes or more, such as 10 minutes or more, for example, 15 minutes or more, such as 30 minutes or more, for example, 1 hour or more, such as 2 hours or more, for example, 3 hours or more, such as 6 hours or more, for example, 12 hours or more, for example, 18 hours or more (including periods of 24 hours or more).
[0068] In certain embodiments, the above-mentioned patch further comprises a backing layer. The backing layer can be flexible so that it can be in intimate contact with the desired application site on the subject. The backing can be made of a material that does not absorb the active agent compound or the biological fluid collected from the subject into the microneedle and does not allow the active agent compound to leach out from inside the lattice microstructure of the polymer microneedle. The backing layer of interest can include, but is not limited to, nonwoven fabric, woven fabric, film (including sheet), porous body, foam, paper, composite material obtained by laminating a film to a nonwoven fabric or fabric, and combinations thereof.
[0069] The nonwoven fabric may include polyolefin resins such as polyethylene and polypropylene, polyester resins such as polyethylene terephthalate, polybutylene terephthalate, and polyethylene naphthalate, rayon, polyamide, poly(ester ether), polyurethane, polyacrylic resin, polyvinyl alcohol, styrene-isoprene-styrene copolymer, and styrene-ethylene-propylene-styrene copolymer, and combinations thereof. The fabric may include cotton, rayon, polyacrylic resin, polyester resin, polyvinyl alcohol, and combinations thereof. The film may include polyolefin resins such as polyethylene and polypropylene, polyacrylic resins such as polymethyl methacrylate and polyethyl methacrylate, polyester resins such as polyethylene terephthalate, polybutylene terephthalate, and polyethylene naphthalate, as well as cellophane, polyvinyl alcohol, ethylene-vinyl alcohol copolymer, polyvinyl chloride, polystyrene, polyurethane, polyacrylonitrile, fluororesin, styrene-isoprene-styrene copolymer, styrene-butadiene rubber, polybutadiene, ethylene-vinyl acetate copolymer, polyamide, and polysulfone, and combinations thereof. The paper may include impregnated paper, coated paper, wood-free paper, kraft paper, Japanese paper, glassine paper, synthetic paper, and combinations thereof.
[0070] Depending on the size of the patch, the size of the backing may vary, and in some cases, the size is such that it covers the entire application site of the subject.Thus, the backing layer may have a length ranging from 2 to 100 cm, for example, from 4 to 60 cm, and a width ranging from 2 to 100 cm, for example, from 4 to 60 cm.In certain instances, the backing layer may be insoluble in water.By insoluble in water, it is meant that the backing layer may be immersed in water for one day or more, for example, one week or more (including one month or more), and show little if any dissolution, for example no observable dissolution.
[0071] In certain embodiments, the subject patches include a pressure sensitive adhesive, for example to maintain the patch in contact with the skin surface of the subject for an extended period of time, including, but not limited to, polyisobutene adhesives, polyisobutylene adhesives, polyisobutene / polyisobutylene adhesive blends, carboxylated polymers, acrylic or acrylate copolymers, such as carboxylated acrylate copolymers.
[0072] When the pressure sensitive adhesive comprises polybutene, the polybutene may be a saturated polybutene. Alternatively, the polybutene may be an unsaturated polybutene. Additionally, the polybutene may be a mixture or combination of saturated and unsaturated polybutenes. In some embodiments, the pressure sensitive adhesive is selected from the group consisting of Indopol® L-2, Indopol® L-3, Indopol® L-6, Indopol® L-8, Indopol® L-14, Indopol® H-7, Indopol® H-8, Indopol® H-15, Indopol® H-25, Indopol® H-35, Indopol® H-50, Indopol® H- The polybutene pressure sensitive adhesive may include compositions that are or are substantially the same as compositions of Indopol® H-100, Indopol® H-300, Indopol® H-1200, Indopol® H-1500, Indopol® H-1900, Indopol® H-2100, Indopol® H-6000, Indopol® H-18000, Panalane® L-14E, Panalane® H-300E, and combinations thereof. In certain embodiments, the polybutene pressure sensitive adhesive is Indopol® H-1900. In other embodiments, the polybutene pressure sensitive adhesive is Panalane® H-300E.
[0073] Acrylate copolymers of interest include copolymers of various monomers such as "soft", "hard" or "functional" monomers. Acrylate copolymers may be composed of copolymers including bipolymers (i.e. made with two monomers), terpolymers (i.e. made with three monomers), or tetrapolymers (i.e. made with four monomers), or copolymers with more monomers. Acrylate copolymers may be crosslinked or uncrosslinked. The polymers may be crosslinked by known methods to provide the desired polymer. The monomers of the acrylate copolymer may include at least two or more exemplary components selected from the group including acrylic acid, alkyl acrylates, methacrylates, copolymerizable secondary monomers, or monomers with functional groups. The monomers ("soft" and "hard" monomers) can be methoxyethyl acrylate, ethyl acrylate, butyl acrylate, butyl methacrylate, hexyl acrylate, hexyl methacrylate, 2-ethylbutyl acrylate, 2-ethylbutyl methacrylate, isooctyl acrylate, isooctyl methacrylate, 2-ethylhexyl acrylate, 2-ethylhexyl methacrylate, decyl acrylate, decyl methacrylate, dodecyl acrylate, dodecyl methacrylate, tridecyl acrylate, tridecyl methacrylate, acrylonitrile, methoxyethyl acrylate, methoxyethyl methacrylate, and the like. Additional examples of acrylic adhesive monomers are described in Satas, "Acrylic Adhesives," Handbook of Pressure-Sensitive Adhesive Technology, 2nd ed., pp. 396-456 (D. Satas, ed.), Van Nostrand Reinhold, New York (1989), the disclosure of which is incorporated herein by reference. In some embodiments, the pressure sensitive adhesive is an acrylate-vinyl acetate copolymer.In some embodiments, the pressure sensitive adhesive is Duro-Tak® 87-9301, Duro-Tak® 87-200A, Duro-Tak® 87-2353, Duro-Tak® 87-2100, Duro-Tak® 87-2051, Duro-Tak® 87-2052, Duro-Tak® 87-2194, Duro-Tak® 87-2677, Duro-Tak® The acrylic pressure sensitive adhesive may include compositions that are or are substantially the same as compositions of Duro-Tak® 87-201A, Duro-Tak® 87-2979, Duro-Tak® 87-2510, Duro-Tak® 87-2516, Duro-Tak® 87-387, Duro-Tak® 87-4287, Duro-Tak® 87-2287, and Duro-Tak® 87-2074, and combinations thereof. As used herein, the term "substantially the same" refers to a composition that is an acrylate-vinyl acetate copolymer in an organic solvent solution. In certain embodiments, the acrylic pressure sensitive adhesive is Duro-Tak® 87-2054.
[0074] In some embodiments, one or more of the polymeric microneedles of the patch are dissolvable. In some cases, the entire microneedle is dissolvable. In other cases, a portion of the microneedle, such as the tip of the microneedle, is dissolvable. In some embodiments, the microneedles dissolve at a rate of from about 1 minute per patch to about 2 weeks per patch, from about 1 minute per patch to about 1 week per patch, from about 1 minute per patch to about 3 days per patch, from about 1 minute per patch to about 1 day per patch, from about 1 minute per patch to about 12 hours per patch, from about 1 minute per patch to about 6 hours per patch, from about 1 minute per patch to about 1 hour per patch, from about 1 minute per patch to about 30 minutes per patch, from about 30 minutes per patch to about 1 month per patch, from about 1 hour per patch to about 1 month per patch, from about 6 hours per patch to about 1 month per patch, from about 12 hours per patch to about 1 month per patch, from about 1 day per patch to about 1 month per patch, from about 3 days per patch to about 1 month per patch, from about 1 week per patch to about 1 month per patch (including from about 2 weeks per patch to about 1 month per patch).
[0075] In some embodiments, one or more of the polymeric microneedles are fragile. In some cases, the polymeric microneedles are fragile due to the shape of the microneedles (e.g., due to the presence of holes or thinner structures). In some cases, the polymeric microneedles are fragile due to differences in the mechanical properties of the support compared to the rest of the microneedles. The fragile microneedles can be intentionally broken to remove the microneedles embedded in the skin from the patch backing on the skin surface. In certain embodiments, removal of the patch backing can allow verification that the intended payload is delivered to the sample and / or subject by ensuring that the active agent compound is not present on the fragile support after patch administration.
[0076] In certain embodiments, one or more of the polymeric microneedles include a frangible support. In some cases, the microneedle sidewall includes a frangible support. For example, the support may resist breaking under application of normal force, but allow separation by twisting, shearing, or other energy input. In some cases, the microneedle includes a frangible perforation, such as, for example, a physical perforation or a chemical perforation. In certain cases, the microneedle includes a perforated sidewall. The term "perforation" is used herein in its conventional sense to refer to a particular plane within the microneedle that is chemically or physically different from the rest of the array. In this way, a portion of the microneedle (e.g., the tip) may be separated from the remainder of the microneedle (e.g., the base). In some cases, the perforation includes a hole or a slit.
[0077] In some embodiments, polymeric microneedles that can be mechanically or chemically fragmented or removed provide rapid administration of active agent compounds with long-term drug release without long-term patch application. For example, if a patch releases an active agent compound over a period of one week, frangible microneedles can be applied to the skin, fragmented, the patch backing removed, the microneedle fragments embedded in the skin, and the drug released. This allows patients to enjoy the benefits of long-term drug delivery without having to wear a patch for the entire duration of treatment.
[0078] Method for applying a patch having a plurality of polymeric microneedles - Patent application Aspects of the present disclosure also include methods for applying a patch having a plurality of polymeric microneedles to a skin surface of a subject. In some embodiments, applying a patch described herein provides transdermal administration of one or more active agent compounds. In some embodiments, the patch can be used to collect a biological fluid sample by applying the patch to a skin surface of a subject. Transdermal refers to a route of administration in which an active agent (i.e., a drug) is delivered across the skin (e.g., topical administration) or mucosa, or a biological sample, such as interstitial fluid, is collected from a subject. Thus, the patches described herein are configured to deliver an active agent compound or collect a biological sample from a subject through one or more of the subcutaneous, dermis, and epidermis, including the stratum corneum, stratum granulosum, stratum spinosum, and stratum basale. Thus, a patch comprising a plurality of polymeric microneedles can be applied to any convenient location, such as, for example, the arms, legs, buttocks, abdomen, back, neck, scrotum, vagina, face, behind the ears, buccal, and under the tongue. In describing the methods of the present invention, the term "subject" refers to a person or organism to which the patch is applied and maintained in contact. Thus, the subjects of the present invention may include, but are not limited to, mammals, such as humans and other primates, such as chimpanzees and other ape and monkey species, and in certain embodiments, the subject is a human. The term "subject" is also meant to include a person or organism of any age, weight, or other physical characteristic, and the subject may be an adult, child, infant, or newborn.
[0079] In some embodiments, the method includes extended delivery of the active agent compound to the subject. By "extended delivery" is meant that the patch is configured to provide administration of the active agent compound for an extended period of time, for example, several hours, days (including weeks), for example, 1 hour or more, for example, 2 hours or more, for example, 4 hours or more, for example, 8 hours or more, for example, 12 hours or more, for example, 24 hours or more, for example, 48 hours or more, for example, 72 hours or more, for example, 96 hours or more, for example, 120 hours or more, for example, 144 hours or more (including 168 hours or more). In some embodiments, the polymeric microneedles are configured for sustained release of the active agent compound, including multi-day delivery of a therapeutically effective amount of the active agent compound. By multi-day delivery is meant that the polymeric microneedles of the patch are formulated to provide a therapeutically effective amount of the active agent compound to the subject when applied to the skin of the subject for a period of 1 day or more, for example, 2 days or more, for example, 4 days or more, for example, 7 days or more, for example, 14 days (including 30 days or more). In certain embodiments, the patch provides a therapeutically effective amount of the active agent compound to a subject for a period of 10 days or more. For multi-day administration, the upper period is in some cases 30 days or less, e.g., 28 days or less, e.g., 21 days or less, e.g., 14 days or less, e.g., 7 days or less, including 3 days or less. In certain embodiments, the multi-day delivery is in the range of, e.g., 2 to 30 days, e.g., 3 to 28 days, e.g., 4 to 21 days, e.g., 5 to 14 days, including 6 to 10 days.
[0080] In certain embodiments, the protocol can include multiple dosing intervals. "Multiple dosing intervals" means that two or more patches are applied and maintained in contact with the subject continuously. Thus, the patch is removed from contact with the subject, and a new patch is reapplied to the subject. In carrying out the method of the present invention, the treatment regimen can include two or more dosing intervals, for example, three or more dosing intervals, for example, four or more dosing intervals, for example, five or more dosing intervals (including ten or more dosing intervals).
[0081] The duration of the dosing interval in a multiple dosing interval treatment protocol may vary depending on the subject's physiology or treatment protocol as determined by a medical professional. For example, the duration of the dosing interval in a multiple dosing treatment protocol may be predetermined and followed at regular intervals. Thus, the time between dosing intervals may vary, for example, 2 days or more, for example, 3 days or more, for example, 4 days or more, for example, 5 days or more, for example, 6 days or more, for example, 7 days or more, for example, 10 days or more (including 30 days or more). The upper limit of the time between dosing intervals is, in some cases, 30 days or less, for example, 28 days or less, for example, 21 days or less, for example, 14 days or less, for example, 7 days or less (including 3 days or less). In certain embodiments, the time between dosing intervals is, for example, in the range of 2 days to 30 days, for example, 3 days to 28 days, for example, 4 days to 21 days, for example, 5 days to 14 days (including 6 days to 10 days).
[0082] In certain embodiments, the method further comprises removing the patch from contact with the subject at the end of the dosing interval.For example, the patch can be removed from contact with the subject after maintaining the patch in contact with the subject for 0.5 hours or more, for example, 1 hour or more, for example, 2 hours or more, for example, 4 hours or more, for example, 8 hours or more, for example, 12 hours or more, for example, 24 hours or more, for example, 36 hours or more, for example, 48 hours or more, for example, 60 hours or more, for example, 72 hours or more, for example, 96 hours or more, for example, 120 hours or more, for example, 144 hours or more (including 168 hours or more).The upper limit of the time that the patch continues to contact with the subject before removal is, in some cases, 168 hours or less, for example, 144 hours or less, for example, 120 hours or less, for example, 96 hours or less, for example, 72 hours or less, for example, 48 hours or less, for example, 12 hours or less, for example, 8 hours or less, for example, 4 hours or less (including 2 hours or less).
[0083] The location on the subject for reapplication of a subsequent patch in a multiple dosage treatment regimen may be the same or different from the location on the subject from which the previous patch was removed. For example, if the first patch is applied and maintained on the subject's leg, one or more subsequent patches may be reapplied to the same location on the subject's leg. On the other hand, if the first patch is applied and maintained on the subject's leg, one or more subsequent patches may be reapplied to a different location, such as the subject's abdomen or back. Subsequent dosages applied in a multiple dosage interval regimen may have the same or different active agent compound. In certain cases, subsequent dosage intervals in a treatment regimen may contain a higher or lower concentration of active agent compound than the previous dosage interval. For example, the concentration of active agent compound may be increased by 10% or more in the subsequent dosage interval, such as 20% or more, such as 50% or more, such as 75% or more, such as 90% or more (including 100% or more). The upper limit of the increase in concentration of the active agent compound in subsequent dosing intervals is, in some cases, 10-fold or less, e.g., 5-fold or less, e.g., 2-fold or less, e.g., 1-fold or less, e.g., 0.5-fold or less (including 0.25-fold or less).
[0084] On the other hand, the amount of the active agent compound may be reduced in a subsequent dosing interval, for example, by 10% or more, for example, 20% or more, for example, 50% or more, for example, 75% or more, for example, 90% or more (including 100% or more). The upper limit of the reduction in the amount of the active agent compound in a subsequent dosing interval is, in some cases, 10-fold or less, for example, 5-fold or less, for example, 2-fold or less, for example, 1-fold or less, for example, 0.5-fold or less (including 0.25-fold or less). In other cases, a subsequent dosing interval may contain a different active agent compound than the previous dosing interval.
[0085] In some embodiments, the method includes applying one or more patches to a skin surface of a subject in a manner to collect a biological fluid sample from the subject. The biological fluid sample can be collected in the polymeric microneedles of the patch by any convenient protocol, such as, for example, capillary action. In embodiments, the biological fluid sample is collected from one or more of the subcutaneous, dermis, and epidermis, including the stratum corneum, stratum granulosum, stratum spinosum, and stratum basale of the subject. In certain cases, the biological fluid sample is interstitial fluid. In certain cases, the biological fluid sample is dermal fluid. In certain cases, the biological fluid sample is blood. In some embodiments, the method includes collecting a biological fluid sample (e.g., interstitial fluid, dermal fluid) from a subject to detect an analyte present in the biological sample, such as to detect glucose.
[0086] In some embodiments, the patch is maintained in contact with the subject for an extended period of time sufficient to collect a biological fluid sample from the subject, such as hours, days (including weeks), for example, 1 hour or more, such as 2 hours or more, for example, 4 hours or more, such as 8 hours or more, for example, 12 hours or more, such as 24 hours or more, for example, 48 hours or more, such as 72 hours or more, for example, 96 hours or more, such as 120 hours or more, for example, 144 hours or more (including 168 hours or more). In some embodiments, the polymeric microneedles are configured for multi-day collection of biological fluid samples. Multi-day collection means that the polymeric microneedles of the patch are configured to collect biological samples from the subject continuously or at predetermined intervals when applied to the skin of the subject for a period of 1 day or more, such as 2 days or more, for example, 4 days or more, such as 7 days or more, for example, 14 days or more (including 30 days or more). In certain embodiments, the patch is maintained in contact with the subject for a period of 10 days or more. For multi-day collection of biological samples, the upper time period, in some cases, is 30 days or less, e.g., 28 days or less, e.g., 21 days or less, e.g., 14 days or less, e.g., 7 days or less (including 3 days or less). In certain embodiments, the multi-day transdermal delivery is in the range of, e.g., 2 to 30 days, e.g., 3 to 28 days, e.g., 4 to 21 days, e.g., 5 to 14 days (including 6 to 10 days).
[0087] In certain embodiments, the protocol can include multiple collection intervals. By "multiple collection intervals" is meant that two or more patches are applied and maintained in contact with the subject continuously. Thus, the patch is removed from contact with the subject, and a new patch is reapplied to the subject. In carrying out the method of the present invention, the treatment regimen can include two or more collection intervals, for example, three or more collection intervals, for example, four or more collection intervals, for example, five or more collection intervals (including ten or more collection intervals).
[0088] The duration of the collection intervals in a treatment protocol with multiple collection intervals may vary depending on the subject's physiology or treatment protocol as determined by a medical professional. For example, the duration between collection intervals in a treatment protocol with multiple collection intervals may be predetermined and follow a regular interval. Thus, the time between collection intervals may vary, for example, 2 days or more, for example, 3 days or more, for example, 4 days or more, for example, 5 days or more, for example, 6 days or more, for example, 7 days or more, for example, 10 days or more (including 30 days or more). The upper period between collection intervals is, in some cases, 30 days or less, for example, 28 days or less, for example, 21 days or less, for example, 14 days or less, for example, 7 days or less (including 3 days or less). In certain embodiments, the time between collection intervals is, for example, in the range of 2 days to 30 days, for example, 3 days to 28 days, for example, 4 days to 21 days, for example, 5 days to 14 days (including 6 days to 10 days).
[0089] In certain embodiments, the method further comprises removing the patch from contact with the subject at the end of the collection interval.For example, the patch can be removed from contact with the subject after maintaining the patch in contact with the subject for 0.5 hours or more, for example, 1 hour or more, for example, 2 hours or more, for example, 4 hours or more, for example, 8 hours or more, for example, 12 hours or more, for example, 24 hours or more, for example, 36 hours or more, for example, 48 hours or more, for example, 60 hours or more, for example, 72 hours or more, for example, 96 hours or more, for example, 120 hours or more, for example, 144 hours or more (including 168 hours or more).The upper limit of the time that the patch continues to contact with the subject before removal is, in some cases, 168 hours or less, for example, 144 hours or less, for example, 120 hours or less, for example, 96 hours or less, for example, 72 hours or less, for example, 48 hours or less, for example, 24 hours or less, for example, 12 hours or less, for example, 8 hours or less, for example, 4 hours or less (including 2 hours or less).
[0090] The patch having multiple polymeric microneedles according to the embodiment of the present invention is not irritating to the skin of the subject at the application site. Skin irritation is referred to in its general sense herein to refer to adverse effects, discoloration or damage to the skin, such as redness, pain, swelling or dryness. Thus, when practicing the method with the patch of the subject, the quality of the skin remains normal and consistent throughout the entire dosage or collection interval.
[0091] In some embodiments, skin irritation is evaluated to determine the quality and color of the skin at the application site, and to determine whether any damage, pain, swelling, or dryness is caused by contacting the patch with the subject.Skin can be evaluated for irritation by any convenient and easy protocol using the Draize scale, for example, as disclosed in Draize, JH, Appraisal of the Safety of Chemicals in Foods, Drugs and Cosmetics, pp.46-49, The Association of Food and Drug Officials of the United States: Austin, Texas, the disclosure of which is incorporated herein by reference.Specifically, skin can be evaluated for erythema or edema at the patch application site.For example, erythema and edema grades can be assigned based on visual observation or palpation.
[0092] [Table 1]
[0093] The application site can be evaluated for skin irritation at any time during the subject method. In some cases, the skin is evaluated for irritation by observing or palpating the skin while the patch is in contact with the subject, for example, every 0.25 hours, every 0.5 hours, every 1 hour, every 2 hours, every 4 hours, every 12 hours, every 24 hours (including every 72 hours), or some other interval. For example, the application site can be evaluated for skin irritation while the patch is in contact with the subject, for example, 15 minutes after applying the patch to the subject, 30 minutes after applying the patch, 1 hour after applying the transdermal delivery device, 2 hours after applying the patch, 4 hours after applying the patch, 8 hours after applying the patch, 12 hours after applying the patch, 24 hours after applying the patch, 48 hours after applying the patch, 72 hours after applying the patch, 76 hours after applying the patch, 80 hours after applying the patch, 84 hours after applying the patch, 96 hours after applying the patch, 120 hours after applying the patch (including 168 hours after applying the patch).
[0094] System for fabricating polymer microneedles Aspects of the present disclosure also include a system for fabricating a polymer structure having a lattice microstructure having one or more lattice cell units, such as a polymer microneedle. The system, according to certain embodiments, includes a micro-digital light projection system having a light beam generator component and a light projection monitoring component, and a liquid interfacial polymerization module including a build elevator and a build surface, and configured to generate the lattice microstructure from a polymerizable composition positioned therebetween.
[0095] In some embodiments, the light beam generator component includes a light source. In some embodiments, the light source is a broadband light source that emits light having a wide range of wavelengths, for example, ranging from 50 nm or more, such as, for example, 100 nm or more, for example, 150 nm or more, for example, 200 nm or more, for example, 250 nm or more, for example, 300 nm or more, for example, 350 nm or more, for example, 400 nm or more, and 500 nm or more. For example, one suitable broadband light source emits light having a wavelength between 200 nm and 1500 nm. Another example of a suitable broadband light source includes a light source that emits light having a wavelength between 400 nm and 1000 nm. Any convenient broadband light source protocol may be employed, such as halogen lamps, deuterium arc lamps, xenon arc lamps, stabilized fiber-coupled broadband light sources, broadband LEDs with continuous spectrum, super-bright light emitting diodes, semiconductor light emitting diodes, broad spectrum LED white light sources, multi-LED integrated white light sources, or any combination thereof, among other broadband light sources.
[0096] In some embodiments, the light source is a narrowband light source that emits a specific wavelength or a narrow range of wavelengths. In some cases, the narrowband light source includes a light source that emits light having a narrow range of wavelengths, such as, for example, 50 nm or less, for example, 40 nm or less, for example, 30 nm or less, for example, 25 nm or less, for example, 20 nm or less, for example, 15 nm or less, for example, 10 nm or less, for example, 5 nm or less, for example, 2 nm or less, and emits light of a specific wavelength (i.e., monochromatic light). Any convenient narrowband light source protocol can be used, such as a narrow wavelength LED, a laser diode, or a narrowband light source coupled to one or more optical bandpass filters, a diffraction grating, a monochromator, or any combination thereof. The subject systems can include one or more light sources, such as two or more light sources, for example, three or more light sources, for example, four or more light sources, for example, five or more light sources (including ten or more light sources), as desired. The light source may include a combination of light source types, for example, if two light sources are used, the first light source may be a broadband white light source (e.g., a broadband white light LED) and the second light source may be a broadband near infrared light source (e.g., a broadband near infrared LED). In other cases where two light sources are used, the first light source may be a broadband white light source (e.g., a broadband white light LED) and the second light source may be a narrow spectrum light source (e.g., a narrow band visible or near infrared LED). In still other cases, the light source is a narrow band light source, each emitting a specific wavelength, for example, an array of two or more LEDs, for example, an array of three or more LEDs, for example, an array of five or more LEDs (including an array of ten or more LEDs).
[0097] In certain embodiments, the light source is a strobe light source, where the polymerizable composition is illuminated with a periodic flash of light. Depending on the light source (e.g., flash lamp, pulsed laser), the frequency of the light strobe can vary and can be 0.01 kHz or more, such as 0.05 kHz or more, such as 0.1 kHz or more, such as 0.5 kHz or more, such as 1 kHz or more, such as 2.5 kHz or more, such as 5 kHz or more, such as 10 kHz or more, such as 25 kHz or more, such as 50 kHz or more (including 100 kHz or more). In these embodiments, the strobe light can be operatively coupled to a processor having a frequency generator that adjusts the strobe frequency. In some cases, the frequency generator of the strobe light is operatively coupled to the projection monitoring component of the micro digital light projection system such that the frequency of the strobe light is synchronized with the frequency of the image capture on the build surface of the light interface polymerization module. In certain instances, suitable strobe light sources and frequency controllers include, but are not limited to, those described in U.S. Pat. Nos. 5,700,692 and 6,372,506, the disclosures of which are incorporated herein by reference.
[0098] In some embodiments, the light beam generator includes one or more lasers. Lasers of interest may include pulsed or continuous wave lasers. The type and number of lasers used in the subject methods may be gas lasers such as helium neon lasers, argon lasers, krypton lasers, xenon lasers, nitrogen lasers, CO2 lasers, CO2 lasers, argon-fluorine (ArF) excimer lasers, krypton-fluorine (KrF) excimer lasers, xenon chlorine (XeCl) excimer lasers, or xenon-fluorine (XeF) excimer lasers, or combinations thereof. In other cases, the light beam generator includes dye lasers such as stilbene, coumarin, or rhodamine lasers. In yet other cases, the optical beam generator includes a metal vapor laser, such as a helium-cadmium (HeCd) laser, a helium-mercury (HeHg) laser, a helium-selenium (HeSe) laser, a helium-silver (HeAg) laser, a strontium laser, a neon-copper (NeCu) laser, a copper laser, or a gold laser, and combinations thereof. In yet other cases, the optical beam generator includes a solid-state laser, such as a ruby laser, a Nd:YAG laser, a NdCrYAG laser, an Er:YAG laser, a Nd:YLF laser, a Nd:YVO4 laser, a Nd:YCa4O(BO3)3 laser, a Nd:YCOB laser, a titanium sapphire laser, a thulium YAG laser, a YAG laser, an ytterbium YAG laser, a Yb2O3 laser, or a cerium-doped laser, and combinations thereof. In still other cases, the optical beam generator comprises a semiconductor diode laser, an optically pumped semiconductor laser (OPSL), or a frequency doubled or frequency tripled implementation of any of the above mentioned lasers.
[0099] In some embodiments, the light beam generator includes one or more tube lenses configured with an adjustable focal length. In some cases, the tube lens is a telecentric lens. In certain examples, the tube lens is configured for wide field imaging. In some examples, the tube lens has an adjustable focal length in the range of 10 mm to 1000 mm, e.g., 20 mm to 900 mm, e.g., 30 mm to 800 mm, e.g., 40 mm to 700 mm, e.g., 50 mm to 600 mm, e.g., 60 mm to 500 mm, e.g., 70 mm to 400 mm, e.g., 80 mm to 300 mm (including an adjustable focal length of 100 mm to 200 mm).
[0100] In some embodiments, the light beam generator includes one or more projection lenses, e.g., two or more projection lenses, e.g., three or more projection lenses, e.g., four or more projection lenses (including five or more projection lenses). In some cases, the projection lenses provide a magnification of 2x or more, e.g., 3x or more, e.g., 4x or more, e.g., 5x or more, e.g., 6x or more, e.g., 7x or more, e.g., 8x or more, e.g., 9x or more (including 10x or more magnification). In some instances, the projection lenses provide a reduction having a magnification of 0.1-0.95, e.g., 0.2-0.9, e.g., 0.3-0.85, e.g., 0.35-0.8, e.g., 0.5-0.75 (including 0.55-0.7), e.g., 0.6.
[0101] In some embodiments, the light beam generator component includes one or more beam splitters. The beam splitter may be any optical component configured to propagate a beam of light along two or more distinct, spatially separated optical paths such that a predetermined portion of the light is propagated along each optical path. The beam splitter may be any convenient beam splitter protocol, such as a triangular prism, a half mirror prism, a dichroic mirror prism, among other types of beam splitters. The beam splitter may be formed from any suitable material, so long as it is capable of propagating the desired amount and wavelength of light along each optical path. For example, the subject beam splitter may be formed from glass (e.g., N-SF10, N-SF11, N-SF57, N-BK7, N-LAK21, or N-LAF35 glass), silica (e.g., fused silica), quartz, crystal (e.g., CaF2 crystal), zinc selenide (ZnSe), F2, germanium titanate (Ge) (e.g., S-TIH11), borosilicate (e.g., BK7). In certain embodiments, the beam splitter is formed from a polymeric material such as, but not limited to, polycarbonate, polyvinyl chloride (PVC), polyurethane, polyether, polyamide, polyimide, or copolymers of these thermoplastics such as PETG (glycol modified polyethylene terephthalate), among other polymeric plastic materials. In certain embodiments, the beamsplitter is formed from a polyester, polyesters of interest include, but are not limited to, poly(ethylene terephthalate) (PET), bottle grade PET (a copolymer made based on monoethylene glycol, terephthalic acid, and other comonomers such as isophthalic acid, cyclohexanedimethanol), poly(alkylene terephthalates) such as poly(butylene terephthalate) (PBT), and poly(hexamethylene terephthalate), poly(ethylene adipate), poly(1,poly(alkylene adipates) such as poly(4-butylene adipate) and poly(hexamethylene adipate); poly(alkylene suberates) such as poly(ethylene suberate); poly(alkylene sebacates) such as poly(ethylene sebacate); poly(ε-caprolactone) and poly(β-propiolactone); poly(alkylene isophthalates) such as poly(ethylene isophthalate); poly(ethylene 2,6-naphthalene-dicarboxylate); poly(alkylene 2,6-naphthalene dicarboxylate), poly(alkylenesulfonyl-4,4'-dibenzoate) such as poly(ethylenesulfonyl-4,4'-dibenzoate), poly(p-phenylene alkylene dicarboxylate) such as poly(p-phenylene ethylene dicarboxylate), poly(trans-1,4-cyclohexanediyl alkylene dicarboxylate) such as poly(trans-1,4-cyclohexanediyl ethylene dicarboxylate), poly(1,4-cyclohexane-dimethylene alkylene dicarboxylates) such as poly(1,4-cyclohexane-dimethylene ethylene dicarboxylate), poly([2.2.2]-bicyclooctane-1,4-dimethylene alkylene dicarboxylates) such as poly([2.2.2]-bicyclooctane-1,4-dimethylene ethylene dicarboxylate), (S)-polylactide, (R,S)-polylactide, poly(tetramethyl glycolide), and Included may be lactic acid polymers and copolymers such as poly(lactide-co-glycolide), as well as polycarbonates of bisphenol A, 3,3'-dimethylbisphenol A, 3,3',5,5'-tetrachlorobisphenol A, 3,3',5,5'-tetramethylbisphenol A, polyamides such as poly(p-phenylene terephthalamide), polyethylene terephthalate (e.g., Mylar™ polyethylene terephthalate), combinations thereof, and the like.
[0102] In an embodiment, the micro digital light projection system includes a light projection monitoring component having a light detector. The light detector may be any convenient light detection protocol, including, but not limited to, light sensors or light detectors such as active pixel sensors (APS), avalanche photodiodes (APD), quadrant photodiodes, image sensors, charge-coupled devices (CCD), intensified charge-coupled devices (ICCD), light-emitting diodes, photon counters, bolometers, pyroelectric detectors, photoresistors, solar cells, photodiodes, photomultiplier tubes, phototransistors, quantum dot photoconductors or photodiodes, and combinations thereof, among other light detectors. In one particular embodiment, the light detector is a photomultiplier tube, e.g., a 0.01 cm 2 ~10cm 2 , e.g., 0.05 cm 2 ~9cm 2 , e.g., 0.1 cm 2 ~8cm 2 , e.g., 0.5 cm 2 ~7cm 2 (1cm 2 ~5cm 2 The photomultiplier tube has an active detection surface area in each region of the range including the area of the active detection surface area.
[0103] In a particular embodiment, the optical projection monitoring component includes one or more photodetectors optically coupled to the slit. Depending on the size of the active detection surface of the photodetector, the slit in a particular case has a rectangular (or other polygonal shaped) aperture having a width of 0.01 mm to 2 mm, e.g., 0.1 mm to 1.9 mm, e.g., 0.2 mm to 1.8 mm, e.g., 0.3 mm to 1.7 mm, e.g., 0.4 mm to 1.6 mm (including width of 0.5 mm to 1.5 mm) and a length of 0.01 mm to 2 mm, e.g., 0.1 mm to 1.9 mm, e.g., 0.2 mm to 1.8 mm, e.g., 0.3 mm to 1.7 mm, e.g., 0.4 mm to 1.6 mm (including length of 0.5 mm to 1.5 mm). In certain cases, the width of the slit is 1 mm or less, e.g., 0.9 mm or less, e.g., 0.8 mm or less, e.g., 0.7 mm or less, e.g., 0.6 mm or less, e.g., 0.5 mm or less (including widths of 0.4 mm or less). In certain cases, the light detection system includes a light detector optically coupled to a slit having multiple apertures, e.g., two or more apertures, e.g., three or more apertures, e.g., four or more apertures, e.g., five or more apertures, e.g., six or more apertures, e.g., seven or more apertures, e.g., eight or more apertures, e.g., nine or more apertures (including a slit having ten or more apertures).
[0104] The light may be measured by a photodetector at one or more wavelengths, e.g., two or more wavelengths, e.g., five or more different wavelengths, e.g., 10 or more different wavelengths, e.g., 25 or more different wavelengths, e.g., 50 or more different wavelengths, e.g., 100 or more different wavelengths, e.g., 200 or more different wavelengths, e.g., 300 or more different wavelengths (including measuring light at 400 or more different wavelengths). The light may be measured continuously or at discrete intervals. In some cases, the detector in question is configured to measure the light continuously. In other cases, the detector in question is configured to measure at discrete intervals, such as measuring light every 0.001 milliseconds, every 0.01 milliseconds, every 0.1 milliseconds, every 1 millisecond, every 10 milliseconds, every 100 milliseconds, or some other interval, including every 1000 milliseconds.
[0105] In one particular embodiment, the micro digital light projection system is a digital light processing (DLP) system having a digital micromirror device as described in U.S. Patent Publication Nos. 2017 / 0095972, 2022 / 0250313, 2022 / 0048242, and U.S. Patent Nos. 11,358,342 and 11,141,910, the disclosures of which are incorporated herein by reference.
[0106] In some embodiments, the system also includes a processor having a memory operatively coupled to the processor, the memory including instructions stored thereon that, when executed by the processor, cause the processor to irradiate a polymerizable composition positioned between the build elevator and the build surface to generate a polymerizable composition having a first polymerized region of the polymerizable composition in contact with the build elevator and a first non-polymerized region of the polymerizable composition in contact with the build surface, move the build elevator away from the build surface, and irradiate the first non-polymerized region of the polymerizable composition to generate a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second non-polymerized region in contact with the build surface. These steps are repeated in a manner sufficient to generate polymeric microneedles having a lattice microstructure. For example, a step may be repeated 2 or more times, such as 3 or more times, for example 4 or more times, such as 5 or more times, for example 10 or more times, such as 20 or more times, for example 30 or more times, such as 40 or more times, for example 50 or more times, such as 100 or more times, for example 250 or more times, such as 500 or more times (including 1000 or more times).
[0107] In some embodiments, the memory includes instructions for irradiating the polymerizable composition for a period of time sufficient to bond a first polymerized region of the polymerizable composition to the build elevator. In some cases, the memory includes instructions for irradiating the polymerizable composition for 1 second or more, e.g., 5 seconds or more, e.g., 10 seconds or more, e.g., 20 seconds or more, e.g., 30 seconds or more, e.g., 1 minute or more, e.g., 5 minutes or more, including 10 minutes or more, to bond the first polymerized region of the polymerizable composition to the build elevator.
[0108] In some embodiments, the memory includes instructions to move the build elevator in predetermined increments to build a lattice microstructure of polymer microneedles. In some examples, the memory includes instructions to move the build elevator in increments of 0.001 μm or more, such as 0.005 μm or more, such as 0.01 μm or more, such as 0.05 μm or more, such as 0.1 μm or more, such as 0.5 μm or more, such as 1 μm or more, such as 2 μm or more, such as 3 μm or more, such as 4 μm or more, such as 5 μm or more (including increments of 10 μm or more). In certain cases, the memory includes instructions to move the build elevator in increments of 0.001 μm to 20 μm, such as 0.005 μm to 19 μm, for example, 0.01 μm to 18 μm, such as 0.05 μm to 17 μm, for example, 0.1 μm to 16 μm, such as 0.2 μm to 17 μm, for example, 0.3 μm to 16 μm, such as 0.4 μm to 15 μm, for example, 0.5 μm to 14 μm, for example, 0.6 μm to 13 μm, such as 0.7 μm to 12 μm, for example, 0.8 μm to 11 μm (including 0.9 μm to 10 μm).
[0109] In some embodiments, the system also includes a source of polymerizable composition. In some cases, the source is configured to continuously deliver the polymerizable composition to the build surface. In some cases, the system is configured to apply the polymerizable composition to the build surface after each movement of the build elevator away from the build surface. In some embodiments, the polymerizable composition is selected from polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethylmethacrylate, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. In certain embodiments, the polymeric microneedles are formed from polyethylene glycol dimethacrylate (PEGDMA).
[0110] In some embodiments, the light source is configured to irradiate through the build surface, in some cases, at least a portion of the build surface is permeable to the polymerization inhibitor, for example, the polymerization inhibitor is oxygen.
[0111] In certain embodiments, the liquid interfacial polymerization module is a continuous liquid interface generation (CLIP) system, as described in International Patent Publication No. WO2014 / 126837, U.S. Patent Publication Nos. 2018 / 0064920, 2017 / 0095972, 2021 / 0246252, and U.S. Patent Publication Nos. 10,155,882 and 10,792,857, the disclosures of which are incorporated herein by reference.
[0112] In certain embodiments, the memory includes instructions for determining a focal plane on the build surface using a micro-digital light projection system. In some cases, the memory includes instructions for determining a focal plane by illuminating the build surface with a strobe light source through a tube lens and moving the build surface until the light is focused on the build surface through the tube lens. In certain embodiments, the memory includes instructions for determining a focal plane on the build surface by illuminating the build surface with a strobe light source with periodic flashing of light. For example, the frequency of each light pulse may be 0.0001 kHz or more, such as 0.0005 kHz or more, such as 0.001 kHz or more, such as 0.005 kHz or more, such as 0.01 kHz or more, such as 0.05 kHz or more, such as 0.1 kHz or more, such as 0.5 kHz or more, such as 1 kHz or more, such as 2.5 kHz or more, such as 5 kHz or more, such as 10 kHz or more, such as 25 kHz or more, such as 50 kHz or more (including 100 kHz or more). In certain cases, the frequency of the pulsed irradiation by the light source is in the range of 0.00001 kHz to 1000 kHz, such as 0.00005 kHz to 900 kHz, for example, 0.0001 kHz to 800 kHz, for example, 0.0005 kHz to 700 kHz, for example, 0.001 kHz to 600 kHz, for example, 0.005 kHz to 500 kHz, for example, 0.01 kHz to 400 kHz, for example, 0.05 kHz to 300 kHz, for example, 0.1 kHz to 200 kHz (including 1 kHz to 100 kHz).The duration of light illumination of each light pulse (i.e., pulse width) may vary and may be 0.000001 milliseconds or more, such as 0.000005 milliseconds or more, such as 0.00001 milliseconds or more, such as 0.00005 milliseconds or more, such as 0.0001 milliseconds or more, such as 0.0005 milliseconds or more, such as 0.001 milliseconds or more, such as 0.005 milliseconds or more, such as 0.01 milliseconds or more, such as 0.05 milliseconds or more, such as 0.1 milliseconds or more, such as 0.5 milliseconds or more, such as 1 millisecond or more, such as 2 milliseconds or more, such as 3 milliseconds or more, such as 4 milliseconds or more, such as 5 milliseconds or more, such as 10 milliseconds or more, such as 25 milliseconds or more, such as 50 milliseconds or more, such as 100 milliseconds or more (including 500 milliseconds or more). For example, the duration of the light illumination may be in the range of 0.000001 ms to 1000 ms, such as 0.00005 ms to 950 ms, such as 0.0001 ms to 900 ms, such as 0.00005 ms to 850 ms, such as 0.0001 ms to 800 ms, such as 0.0005 ms to 750 ms, such as 0.0005 ms to 650 ms, such as 0.01 ms to 600 ms, such as 0.05 ms to 550 ms, such as 0.1 ms to 500 ms, such as 0.5 ms to 450 ms, such as 1 ms to 400 ms, such as 5 ms to 350 ms, inclusive. In some cases, the memory includes instructions for illuminating the build surface with a plane of light having a projected image pattern using a strobe light source.
[0113] In some cases, determining the focal plane on the build surface includes adjusting the focus of the tube lens. In some cases, the focus of the tube lens is increased to adjust the focus on the build surface. For example, the focus can be increased, e.g., by 1 μm or more, e.g., 5 μm or more, e.g., 10 μm or more, e.g., 50 μm or more, e.g., 100 μm or more, e.g., 500 μm or more, e.g., 1 mm or more, e.g., 5 mm or more, e.g., 10 mm or more, e.g., 5 mm or more, e.g., 10 mm or more, e.g., 50 mm or more (including 100 mm or more). In some cases, the focus of the tube lens is decreased to adjust the focus on the build surface. For example, the focal spot may be reduced by, for example, 1 μm or more, such as 5 μm or more, for example 10 μm or more, such as 50 μm or more, for example 100 μm or more, such as 500 μm or more, for example 1 mm or more, such as 5 mm or more, for example 10 mm or more, such as 5 mm or more, for example 10 mm or more, such as 50 mm or more (including 100 mm or more).
[0114] In some embodiments, the memory includes instructions for moving the build surface until the projected image pattern is in focus with the build surface. The build surface and build elevator may be moved using any convenient movement protocol, such as manually (i.e., directly moving the build surface or build elevator by hand), with assistance from a mechanical device or a motorized movement device. For example, in some embodiments, the build surface or build elevator is moved within the subject systems with a mechanically driven translation stage, a mechanical lead screw assembly, a mechanical sliding device, a mechanical lateral motion device, or a mechanically operated geared translation device. In other embodiments, the build surface or build elevator is moved by a motorized translation stage, a lead screw translation assembly, a geared translation device, such as those using stepper motors, servo motors, brushless electric motors, brushed DC motors, microstep drive motors, high resolution stepper motors, among other types of motors. In some cases, the build surface is moved by 1 μm or more, such as 5 μm or more, such as 10 μm or more, such as 50 μm or more, such as 100 μm or more (including 500 μm or more). In certain embodiments, the build surface is moved by 400 μm or less, such as 350 μm or less, such as 300 μm or less, such as 250 μm or less, such as 200 μm or less, such as 150 μm or less, such as 100 μm or less (including 50 μm or less).
[0115] In some cases, the memory includes instructions to generate an image stack having a plurality of projected image patterns. The image stack can include two or more projected image patterns, e.g., three or more, e.g., four or more, e.g., five or more, e.g., ten or more, and twenty-five or more projected image patterns. In certain cases, the memory includes instructions to determine a focal plane of the build surface based on the generated image stack.
[0116] Aspects of the present disclosure further include a computer control system, the system further comprising one or more computers for full or partial automation of the methods described herein. In an embodiment, the system comprises an input module, a processing module, and an output module. The subject systems may include both hardware and software components, where the hardware components may take the form of one or more platforms, e.g., in the form of servers, such that the functional elements of the system, i.e., those elements of the system that perform specific tasks (e.g., managing the input and output of information, processing information, etc.), may be performed by the execution of software applications on and across one or more computer platforms represented in the system.
[0117] The system may include a display and an operator input device. The operator input device may be, for example, a keyboard, a mouse, etc. The processing module includes a processor that accesses a memory having instructions stored therein to perform the steps of the subject method. The processing module may include an operating system, a graphical user interface (GUI) controller, a system memory, a memory storage device, and an input / output controller, a cache memory, a data backup unit, and many other devices. The processor may be a commercially available processor or one of other processors that are available or that become available. The processor executes an operating system, which interfaces with firmware and hardware in a well-known manner to facilitate the processor's coordination and execution of functions of various computer programs, which may be written in a variety of programming languages, such as Java, Perl, C++, other high-level or low-level languages, and combinations thereof, as is known in the art. The operating system typically cooperates with the processor to coordinate and execute the functions of the other components of the computer. The operating system also provides scheduling, input / output control, file and data management, memory management, and communication control and related services, all in accordance with known techniques. The processor may be any suitable analog or digital system.
[0118] The system memory can be any of a variety of known or future memory storage devices. Examples include any commonly available random access memory (RAM), magnetic media such as a resident hard disk or tape, optical media such as a read and write compact disk, flash memory devices, or other memory storage devices. The memory storage device can be any of a variety of known or future devices including a compact disk drive, tape drive, removable hard disk drive, or disk drive. Such types of memory storage devices typically read from and / or write to a program storage medium (not shown), such as a compact disk, magnetic tape, removable hard disk, or magnetic disk, respectively. Any of these program storage media, or others currently in use or that may later be developed, may be considered a computer program product. As will be appreciated, these program storage media typically store computer software programs and / or data. Computer software programs, also referred to as computer control logic, are typically stored in the system memory and / or in program storage devices used in conjunction with the memory storage devices.
[0119] In some embodiments, a computer program product is described that includes a computer usable medium having control logic (a computer software program including program code) stored thereon. The control logic, when executed by a computer, processor, causes the processor to perform the functions described herein. In other embodiments, some functions are implemented primarily in hardware, for example, using hardware state machines. The implementation of hardware state machines to perform the functions described herein will be apparent to one of ordinary skill in the relevant art.
[0120] The memory may be any suitable device from which the processor can store and retrieve data, such as a magnetic, optical, or solid-state storage device (including a magnetic or optical disk, or tape, or RAM, or any other suitable device, either fixed or portable). The processor may include a general-purpose digital microprocessor suitably programmed from a computer-readable medium carrying the necessary program code. The programming may be provided remotely to the processor over a communication channel, or may be pre-stored in a computer program product, such as a memory or some other portable or fixed computer-readable storage medium, using any of those devices together with the memory. For example, a magnetic or optical disk may carry the programming and can be read by a disk writer / reader. The system of the present invention also includes programming, for example in the form of a computer program product, algorithms for use in implementing the above-described methods. The programming according to the present invention may be recorded on a computer-readable medium, for example any medium that can be directly read and accessed by a computer. Such media include, but are not limited to, magnetic storage media such as magnetic disks, hard disk storage media, and magnetic tape, optical storage media such as CD-ROMs, electrical storage media such as RAM and ROM, portable flash drives, and hybrids of these categories such as magnetic / optical storage media.
[0121] The processor may also have access to a communication channel for communicating with a user at a remote location, meaning that the user does not have direct contact with the system, but rather relays input information to the input manager from an external device, such as a computer connected to a wide area network ("WAN"), a telephone network, a satellite network, or any other suitable communication channel, including a cellular phone (i.e., a smartphone).
[0122] In some embodiments, a system according to the present disclosure may be configured to include a communication interface. In some embodiments, the communication interface includes a receiver and / or a transmitter for communicating with a network and / or another device. The communication interface may be configured for wired or wireless communication, including, but not limited to, radio frequency (RF) communication (e.g., radio frequency identification (RFID), ZigBee communication protocol, WiFi, infrared, wireless universal serial bus (USB), ultra-wideband (UWB), Bluetooth® communication protocol, and cellular communication, such as Code Division Multiple Access (CDMA) or Global System for Mobile Communications (GSM).
[0123] In one embodiment, the communications interface is configured to include one or more communications ports, e.g., a physical port or interface such as a USB port, an RS-232 port, or any other suitable electrical connection port, to enable data communications between the subject system and other external devices, such as computer terminals (e.g., in a clinic or hospital environment) configured for similar complementary data communications.
[0124] In one embodiment, the communications interface is configured for infrared communications, Bluetooth® communications, or any other suitable wireless communications protocol, thereby enabling the subject system to communicate with other devices, such as computer terminals and / or networks, communications-enabled mobile telephones, personal digital assistants, or any other communications device that a user may use in conjunction with.
[0125] In one embodiment, the communication interface is configured to provide a connection for data transfer utilizing the Internet Protocol (IP) through a cellular network, a Short Message Service (SMS), a wireless connection to a personal computer (PC) on a local area network (LAN) connected to the Internet, or a WiFi connection to the Internet at a WiFi hotspot.
[0126] In one embodiment, the subject system is configured to communicate wirelessly with the server device via a communications interface using common standards such as, for example, 802.11 or Bluetooth RF protocols, or IrDA infrared protocol. The server device may be another portable device, such as a smart phone, personal digital assistant (PDA) or notebook computer, or a larger device, such as a desktop computer, appliance, etc. In some embodiments, the server device has a display, such as a liquid crystal display (LCD), and input devices, such as buttons, a keyboard, a mouse, or a touch screen.
[0127] In some embodiments, the communications interface is configured to automatically or semi-automatically communicate data stored within the subject system, e.g., within the optional data storage unit, with a network or server device using one or more of the communications protocols and / or mechanisms described above.
[0128] The output controller may include a controller for any of a variety of known display devices for presenting information to a user, whether human or machine, local or remote. When one of the display devices provides visual information, this information may be logically and / or physically organized, typically as an array of pixels. The graphical user interface (GUI) controller may include any of a variety of known or future software programs for providing a graphical input and output interface between the system and the user, and for processing user input. The functional elements of the computer may communicate with each other via a system bus. Some of these communications may be accomplished using a network or other type of remote communication in alternative embodiments. The output manager may also provide information generated by the processing module to a user at a remote location, for example, via the Internet, telephone, or satellite networks, in accordance with known techniques. Presentation of data by the output manager may be performed in accordance with a variety of known techniques. As some examples, the data may include SQL, HTML, or XML documents, emails or other files, or other forms of data. The data may include Internet URL addresses so that the user can retrieve additional SQL, HTML, XML, or other documents or data from remote sources. The one or more platforms present in the subject system are typically of a class of computers commonly referred to as servers, but may be any type of known or future developed computer platform. However, they may be mainframe computers, workstations, or other computer types. They may be connected via any known or future type of cabling or other communication systems, including wireless systems, either networked or not. They may be co-located or physically separate.In some cases, depending on the type and / or configuration of the computer platform selected, various operating systems may be employed on any of the computer platforms. Suitable operating systems include Windows NT, Windows XP, Windows 7, Windows 8, iOS, Sun Solaris, Linux, OS / 400, Compaq Tru64 Unix, SGI IRIX, Siemens Reliant Unix, etc.
[0129] Methods for making polymeric microneedles Aspects of the present disclosure also include a method for making a polymeric microneedle having a lattice microstructure having one or more lattice cell units. The method according to certain embodiments is a high-resolution continuous additive process that includes irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition having a first polymerized region of the polymerizable composition in contact with the build elevator and a first non-polymerized region of the polymerizable composition in contact with the build surface, moving the build elevator away from the build surface, irradiating the first non-polymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second non-polymerized region in contact with the build surface, and repeating in a manner sufficient to produce a microneedle having a lattice microstructure. These steps are repeated in a manner sufficient to produce a polymeric microneedle having a lattice microstructure. For example, a step may be repeated 2 or more times, such as 3 or more times, for example 4 or more times, such as 5 or more times, for example 10 or more times, such as 20 or more times, for example 30 or more times, such as 40 or more times, for example 50 or more times, such as 100 or more times, for example 250 or more times, such as 500 or more times (including 1000 or more times).
[0130] In some embodiments, the polymerizable composition is irradiated with a light beam generator component of a micro-digital light projection system. In some cases, the light source is a broadband light source emitting light having a wavelength between 400 nm and 1000 nm. In some cases, the broadband light source is a halogen lamp, a deuterium arc lamp, a xenon arc lamp, a stabilized fiber-coupled broadband light source, a broadband LED with a continuous spectrum, an ultra-bright light emitting diode, a semiconductor light emitting diode, a broad spectrum LED white light source, a multi-LED integrated white light source, or any combination thereof, among other broadband light sources. In some cases, the light source is a narrowband light source emitting a specific wavelength or a narrow range of wavelengths. In some cases, the narrowband light source includes a light source that emits light having a narrow range of wavelengths, such as, for example, 50 nm or less, such as, for example, 40 nm or less, such as, for example, 30 nm or less, such as, for example, 25 nm or less, such as, for example, 20 nm or less, such as, for example, 15 nm or less, such as, for example, 10 nm or less, such as, for example, 5 nm or less, such as, for example, 2 nm or less, emitting light of a specific wavelength. In some cases, the polymerizable composition is irradiated with a narrow band light source, such as a narrow wavelength LED, a laser diode, or a broad band light source coupled to one or more optical bandpass filters, a diffraction grating, a monochromator, or any combination thereof.
[0131] In certain embodiments, the light source is a strobe light source and the polymerizable composition is irradiated with a periodic light ceiling, for example, the polymerizable composition is irradiated with a frequency of 0.01 kHz or more, such as 0.05 kHz or more, for example 0.1 kHz or more, such as 0.5 kHz or more, for example 1 kHz or more, such as 2.5 kHz or more, for example 5 kHz or more, such as 10 kHz or more, for example 25 kHz or more, for example 50 kHz or more, including 100 kHz or more. In certain cases, the polymerizable composition is irradiated with a laser, such as a pulsed laser or a continuous wave laser.
[0132] In some embodiments, the polymerizable composition is in contact with the build elevator and the build surface, and in some cases, the method includes irradiating the polymerizable composition for 1 second or more, such as 5 seconds or more, such as 10 seconds or more, such as 20 seconds or more, such as 30 seconds or more, such as 1 minute or more, such as 5 minutes or more, including 10 minutes or more, to bond a first polymerized region of the polymerizable composition to the build elevator.
[0133] In some embodiments, the build elevator is moved away from the build surface after the first polymerized region of the polymerizable composition is coupled to the build elevator. In some cases, the build elevator is moved in increments of 0.001 μm or more, such as 0.005 μm or more, such as 0.01 μm or more, such as 0.05 μm or more, such as 0.1 μm or more, such as 0.5 μm or more, such as 1 μm or more, such as 2 μm or more, such as 3 μm or more, such as 4 μm or more, such as 5 μm or more (including increments of 10 μm or more). In certain cases, the build elevator is moved in increments of 0.001 μm to 20 μm, such as 0.005 μm to 19 μm, for example, 0.01 μm to 18 μm, such as 0.05 μm to 17 μm, for example, 0.1 μm to 16 μm, such as 0.2 μm to 17 μm, for example, 0.3 μm to 16 μm, such as 0.4 μm to 15 μm, for example, 0.5 μm to 14 μm, for example, 0.6 μm to 13 μm, such as 0.7 μm to 12 μm, for example, 0.8 μm to 11 μm (including 0.9 μm to 10 μm).
[0134] In certain cases, the polymerizable composition is applied to the build surface after each movement of the build elevator away from the build surface. In some cases, the polymerizable composition is added to the build surface continuously. In other cases, the polymerizable composition is added to the build surface at discrete intervals, each having a predetermined amount. In some embodiments, the polymerizable composition is selected from polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethylmethacrylate, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl ester, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. In certain embodiments, the polymeric microneedles are formed from polyethylene glycol dimethacrylate (PEGDMA).
[0135] In some embodiments, the polymerizable composition is irradiated through the build surface. In some cases, the polymerizable composition is irradiated in the presence of a polymerization inhibitor. In certain embodiments, the polymerizable composition is polymerized continuously while moving the build elevator away from the build surface. In certain cases, the polymerization inhibitor is oxygen and the build surface is permeable to oxygen. In certain cases, polymerizing the polymerizable composition in the presence of a polymerization inhibitor such as oxygen allows for the continuous (i.e., not layer-by-layer) generation of lattice microstructures with liquid "dead zones" at the interface between the build surface and the build polymer microneedles. In some cases, the dead zones are generated because oxygen acts as a polymerization inhibitor and passes through the oxygen-permeable build surface. Photopolymerization cannot occur in the oxygen-containing "dead zone" region, so this region remains fluid and the polymerized components are in contact with the build surface, and therefore the build lattice microstructure does not physically attach to the build surface. Thus, the movement of the build elevator generates a continuous polymer lattice microstructure that exhibits sufficient mechanical integrity and surface isotropy for use as a polymer microneedle.
[0136] In certain embodiments, the polymerizable composition is polymerized using a liquid interfacial polymerization module that is a continuous liquid interface generation (CLIP) system, as described in International Patent Publication No. WO2014 / 126837, U.S. Patent Publication Nos. 2018 / 0064920, 2017 / 0095972, 2021 / 0246252, and U.S. Patent Publication Nos. 10,155,882, 10,792,857, the disclosures of which are incorporated herein by reference.
[0137] In some embodiments, the method includes illuminating the polymerizable composition with a micro-digital light projection system as described in detail above. In some cases, the method includes determining a focal plane on the build surface using the micro-digital light projection system. In some embodiments, determining the focal plane on the build surface includes illuminating the build surface with a strobe light source through a tube lens and moving the build surface until the light is focused on the build surface through the tube lens. In certain embodiments, the method for determining the focal plane on the build surface includes illuminating the build surface with a strobe light source with periodic flashing of the light. For example, the frequency of each light pulse may be 0.0001 kHz or more, such as 0.0005 kHz or more, for example, 0.001 kHz or more, for example, 0.005 kHz or more, for example, 0.01 kHz or more, for example, 0.05 kHz or more, for example, 0.1 kHz or more, for example, 0.5 kHz or more, for example, 1 kHz or more, for example, 2.5 kHz or more, for example, 5 kHz or more, for example, 10 kHz or more, for example, 25 kHz or more, for example, 50 kHz or more (including 100 kHz or more). In certain cases, the frequency of the pulsed irradiation by the light source is in the range of 0.00001 kHz to 1000 kHz, such as 0.00005 kHz to 900 kHz, for example, 0.0001 kHz to 800 kHz, for example, 0.0005 kHz to 700 kHz, for example, 0.001 kHz to 600 kHz, for example, 0.005 kHz to 500 kHz, for example, 0.01 kHz to 400 kHz, for example, 0.05 kHz to 300 kHz, for example, 0.1 kHz to 200 kHz (including 1 kHz to 100 kHz).The duration of light illumination of each light pulse (i.e., pulse width) may vary and may be 0.000001 milliseconds or more, such as 0.000005 milliseconds or more, such as 0.00001 milliseconds or more, such as 0.00005 milliseconds or more, such as 0.0001 milliseconds or more, such as 0.0005 milliseconds or more, such as 0.001 milliseconds or more, such as 0.005 milliseconds or more, such as 0.01 milliseconds or more, such as 0.05 milliseconds or more, such as 0.1 milliseconds or more, such as 0.5 milliseconds or more, such as 1 millisecond or more, such as 2 milliseconds or more, such as 3 milliseconds or more, such as 4 milliseconds or more, such as 5 milliseconds or more, such as 10 milliseconds or more, such as 25 milliseconds or more, such as 50 milliseconds or more, such as 100 milliseconds or more (including 500 milliseconds or more). For example, the duration of the light illumination may be in the range of 0.000001 ms to 1000 ms, such as 0.000005 ms to 950 ms, for example, 0.00001 ms to 900 ms, for example, 0.00005 ms to 850 ms, for example, 0.0001 ms to 800 ms, for example, 0.0005 ms to 750 ms, for example, 0.001 ms to 700 ms, for example, 0.005 ms to 650 ms, for example, 0.01 ms to 600 ms, for example, 0.05 ms to 550 ms, for example, 0.1 ms to 500 ms, for example, 0.5 ms to 450 ms, for example, 1 ms to 400 ms, for example, 5 ms to 350 ms, including 10 ms to 300 ms. In some cases, the method includes illuminating the build surface with a plane of light having a projected image pattern using a strobe light source.
[0138] In some cases, determining the focal plane on the build surface includes adjusting the focus of the tube lens. In some cases, the focus of the tube lens is increased to adjust the focus on the build surface. For example, the focus may be increased, for example, by 1 μm or more, for example, 5 μm or more, for example, 10 μm or more, for example, 50 μm or more, for example, 100 μm or more, for example, 500 μm or more, for example, 1 mm or more, for example, 5 mm or more, for example, 10 mm or more, for example, 50 mm or more (including 100 mm or more). In some cases, the focus of the tube lens is decreased to adjust the focus on the build surface. For example, the focus may be decreased, for example, by 1 μm or more, for example, 5 μm or more, for example, 10 μm or more, for example, 50 μm or more, for example, 100 μm or more, for example, 500 μm or more, for example, 1 mm or more, for example, 5 mm or more, for example, 10 mm or more, for example, 50 mm or more (including 100 mm or more).
[0139] In some embodiments, the method includes moving the build surface until the projected image pattern is in focus with the build surface. The build surface and build elevator may be moved using any convenient movement protocol, such as manually (i.e., moving the build surface or build elevator directly by hand), with assistance from a mechanical device or a motorized movement device. For example, in some embodiments, the build surface or build elevator is moved with a mechanically driven translation stage, a mechanical lead screw assembly, a mechanical sliding device, a mechanical lateral motion device, or a mechanically operated geared translation device. In other embodiments, the build surface or build elevator is moved by a motorized translation stage, a lead screw translation assembly, a geared translation device, such as those using stepper motors, servo motors, brushless electric motors, brushed DC motors, microstep drive motors, high resolution stepper motors, among other types of motors. In some cases, the build surface is moved by 1 μm or more, e.g., 5 μm or more, e.g., 10 μm or more, e.g., 50 μm or more, e.g., 100 μm or more (including 500 μm or more). In certain embodiments, the build surface is moved by 400 μm or less, such as 350 μm or less, such as 300 μm or less, such as 250 μm or less, such as 200 μm or less, such as 150 μm or less, such as 100 μm or less (including 50 μm or less).
[0140] In some cases, the method includes generating an image stack having a plurality of projected image patterns. The image stack can include two or more projected image patterns, e.g., three or more, e.g., four or more, e.g., five or more, e.g., ten or more, and twenty-five or more projected image patterns. In certain cases, the method includes determining a focal plane of the build surface based on the generated image stack. In embodiments, the methods described herein for generating polymeric microstructures (e.g., polymeric microneedles) having grating microstructures provide a resolution of 10 μm or less, e.g., 5 μm or less. In certain embodiments, the subject methods provide a resolution of 1.0 μm to 4 μm, e.g., 1.5 μm to 3.8 μm.
[0141] As mentioned above, in some cases, the polymeric microneedles include an active agent compound. A method according to certain embodiments includes preparing a polymeric microneedle with an active agent compound. In some cases, the method includes coating the active agent compound on the surface of the polymeric microneedle. In some cases, the active agent compound is coated on the surface of the polymeric microneedle as a fluid composition. In these embodiments, the fluid composition may be applied to the surface of the polymeric microneedle, for example, by dip coating or spray coating the active agent composition. In some embodiments, the method includes coating the surface of the polymeric microneedle with a solid active agent compound, such as by dry casting a powder containing the active agent compound.
[0142] In some cases, the method includes coating 5% or more, such as 10% or more, such as 15% or more, such as 20% or more, such as 25% or more, such as 50% or more, such as 75% or more, such as 90% or more of the surface of the polymeric microneedle with the active agent compound (including coating 95% or more of the surface of the polymeric microneedle). In certain cases, the entire surface of the polymeric microneedle is coated with the active agent compound. In some cases, the method includes coating the active agent compound on the tip of the polymeric microneedle. In some cases, the method includes coating the active agent on the surface of the body portion of the polymeric microneedle. In some cases, the method includes coating the active agent on the surface of the base portion of the polymeric microneedle. In certain cases, the lattice microstructure component of the polymeric microneedle is coated with the active agent compound.
[0143] Depending on the desired dosage of active agent compound, the amount of active agent compound coated on the surface can vary, for example, 0.001 μg or more, for example, 0.005 μg or more, such as 0.01 μg or more, for example, 0.05 μg or more, such as 0.1 μg or more, for example, 0.5 μg or more, such as 1 μg or more, for example, 5 μg or more, such as 25 μg or more, for example, 50 μg or more, such as 100 μg or more (including coating 500 μg or more) of active agent compound coated on the surface of the polymeric microneedle.
[0144] In some embodiments, the active agent compound is incorporated into the internal space of the lattice microstructure of the polymeric microneedle. In some cases, the method includes microfluidic injection loading of the active agent compound into the lattice microstructure of the polymeric microneedle. In other cases, the method includes contacting the lattice microstructure with a composition containing the active agent compound and incorporating the active agent by capillary action. In some embodiments, the polymeric microneedle is immersed in a composition containing the active agent compound and an amount of the active agent is incorporated into the void space of the lattice microstructure by capillary action. Depending on the density of the lattice cell units in the lattice microstructure, the polymeric microneedle may be contacted with (impregnated in) the active agent composition for 0.01 minutes or more, such as 0.05 minutes or more, such as 0.1 minutes or more, such as 0.5 minutes or more, such as 1 minute or more, such as 5 minutes or more, such as 10 minutes or more, such as 30 minutes or more, such as 60 minutes or more (including 6 hours or more) to incorporate the active agent composition into the lattice microstructure.
[0145] In some embodiments, the method includes preparing a polymeric microneedle, the lattice microstructure includes regions of increased active agent compound concentration, for example, the concentration of the active agent compound in these regions increases by 1% or more, for example, 2% or more, for example, 3% or more, for example, 4% or more, for example, 5% or more, for example, 10% or more, for example, 20% or more, for example, 30% or more, for example, 40% or more (including 50% or more) across the longitudinal axis of the lattice microstructure. In some cases, the regions of increased active agent concentration are present at various increments across the longitudinal axis of the lattice microstructure. For example, the regions of increased active agent concentration can be present at increments of every 10 μm or more, for example, every 20 μm or more, for example, every 30 μm or more, for example, every 40 μm or more (including every 50 μm or more) across the longitudinal axis of the lattice microstructure.
[0146] In some embodiments, the method for preparing a polymeric microneedle containing an activator compound includes incorporating an activator compound into the polymerizable composition such that when the polymeric microneedle is formed from the polymerizable composition (e.g., by the high-resolution digital light projection continuous liquid interface processing described above), the activator compound is present in the void space of the lattice microstructure. For example, the activator composition may be present in the polymerizable composition at a concentration of 0.01 μg / μL or more, such as 0.005 μg / μL or more, such as 0.01 μg / μL or more, such as 0.01 μg / μL or more, such as 0.1 μg / μL or more, such as 0.5 μg / μL or more, such as 1 μg / μL or more, such as 5 μg / μL or more, such as 25 μg / μL or more, such as 50 μg / μL or more, such as 100 μg / μL or more (including a coating of 50 μg / μL or more). In some cases, where the lattice microstructure has regions of increased concentration of active agent compound, the method includes increasing the amount of active agent composition present in the source of polymerizable composition while preparing the polymer microneedles, e.g., by increasing the amount of active agent in the polymerizable composition by 1% or more, e.g., 2% or more, e.g., 5% or more, e.g., 10% or more, e.g., 25% or more, e.g., 50% or more (including 75% or more).
[0147] kit Also provided is a kit for use in implementing certain methods described herein.In certain embodiments, the kit comprises one or more patches comprising a plurality of polymeric microneedles having the above-mentioned lattice microstructure.In certain embodiments, the kit comprises an adhesive overlay.In a given kit that comprises two or more of the subject patches, the patches may be individually packaged or may be in a common container.
[0148] In certain embodiments, the kits further include instructions for practicing the subject methods or means for obtaining same (e.g., a website URL that directs a user to a web page providing the instructions), which may be printed on a substrate, which may be one or more of a package insert, packaging, reagent containers, etc. Yet another form for these instructions is a computer readable medium having the information recorded thereon, such as a diskette, compact disc (CD), portable flash drive, USB storage, DVD, Blu-ray disc, etc. Yet another form for these instructions that may be present is a website address that may be used via the internet to access the information at a remote site.
[0149] Notwithstanding the appended claims, the disclosure described herein is also defined by the following caveats:
[0150] 1. A polymeric microneedle comprising a lattice microstructure having one or more lattice cell units. 2. The microneedle of claim 1, comprising two or more repeating lattice cell units. 3. The microneedle of claim 2, comprising 5 or more repeating lattice cell units. 4. The microneedle of any one of claims 1 to 3, comprising a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle. 5. The microneedle of any one of appendixes 1 to 4, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle.
[0151] 6. The microneedle according to any one of claims 1 to 5, comprising lattice cell units having a size of 100 μm to 1000 μm. 7. The microneedle of claim 6, comprising lattice cell units having a size of 200 μm to 500 μm. 8. The microneedle of any one of claims 1 to 7, wherein the lattice microstructure comprises a plurality of struts. 9. The microneedle of claim 8, wherein the lattice microstructure comprises struts having a thickness of 25 μm to 150 μm. 10. The microneedle of claim 8, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm.
[0152] 11. The microneedle of claim 8, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 12. The microneedle according to any one of claims 1 to 11, having a square pyramid or conical protrusion shape. 13. The microneedle according to any one of claims 1 to 11, having a rectangular prism shape. 14. The microneedle according to any one of claims 1 to 13, having a length of 500 μm to 2000 μm. 15. The microneedle of claim 14, having a length of 700 μm to 1200 μm.
[0153] 16. The microneedle according to any one of claims 1 to 15, having a base width of 100 μm to 700 μm. 17. The microneedle of claim 16, having a base width of 200 μm to 400 μm. 18. The microneedle of any one of claims 1 to 17, wherein the lattice microstructure has a volume of 0.01 μL to 2 μL. 19. The microneedle of claim 18, wherein the lattice microstructure has a volume of 0.1 μL. 20. A tip portion having a solid structure; A main body portion having a lattice structure; A base portion having a solid structure; 20. The microneedle according to any one of claims 1 to 19, comprising:
[0154] 21. The microneedle according to claim 20, wherein the tip portion has a length of 25 μm to 500 μm. 22. The microneedle described in appendix 20 or 21, wherein the tip portion has a base width of 50 μm to 300 μm. 23. The microneedle of claim 20 or 21, having a tip diameter of 0.1 μm to 10 μm. 24. The microneedle according to any one of appendices 20 to 23, wherein the main body portion has a length of 50 μm to 1000 μm. 25. The microneedle of any one of appendices 20 to 23, wherein the main body portion has a width of 50 μm to 300 μm.
[0155] 26. The microneedle of any one of appendixes 20 to 25, wherein the base portion has a length of 25 μm to 500 μm. 27. The microneedle of any one of appendices 20 to 25, wherein the base portion has a base width of 50 μm to 300 μm. 28. A microneedle according to any one of claims 1 to 27, wherein the lattice structure is formed from a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. 29. A microneedle according to any one of claims 1 to 28, wherein the lattice structure is formed from polyethylene glycol dimethacrylate (PEGDMA). 30. A microneedle according to any one of claims 1 to 29, formed from a biodegradable polymerizable material. 31. A microneedle according to any one of claims 1 to 30, which is soluble in an aqueous medium.
[0156] 32. A patch, A backing layer; a plurality of polymeric microneedles in contact with a backing layer, each microneedle including a lattice microstructure having one or more lattice cell units; A patch comprising: 33. The patch of claim 32, wherein the plurality of microneedles form an array of microneedles on a backing layer. 34. The patch of claim 32 or 33, wherein the microneedles are spaced apart from each other on the backing layer by an average distance of 5 μm to 1000 μm. 35. The patch of claim 34, wherein the microneedles are spaced apart from each other on the backing layer by an average distance of 100 μm to 500 μm. 36. The patch of any one of claims 32 to 35, wherein the microneedles further comprise an active agent compound.
[0157] 37. The patch of claim 36, wherein the active agent comprises a small molecule active agent compound. 38. The patch of claim 36, wherein the active agent comprises an immunogenic active agent compound. 39. The patch of claim 38, wherein the active agent compound comprises a vaccine. 40. A patch described in any one of notes 32 to 39, wherein the backing layer further comprises a pressure-sensitive adhesive. 41. A patch according to any one of claims 32 to 40, wherein each microneedle comprises two or more repeating lattice cell units.
[0158] 42. The patch of any one of claims 32 to 40, wherein each microneedle comprises five or more repeating lattice cell units. 43. The patch of any one of claims 32-42, wherein one or more microneedles have a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle. 44. A patch according to any one of appendices 32 to 43, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle. 45. A patch according to any one of claims 32 to 44, wherein each microneedle comprises a lattice cell unit having a size of 100 μm to 1000 μm. 46. The patch of claim 45, wherein each microneedle comprises a lattice cell unit having a size of 200 μm to 500 μm.
[0159] 47. A patch described in any one of notes 32 to 46, wherein the lattice microstructure comprises a plurality of struts. 48. The patch of claim 47, wherein the lattice microstructure comprises struts having a thickness between 25 μm and 150 μm. 49. The patch of claim 47, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm. 50. The patch of claim 47, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 51. A patch described in any one of appendices 32 to 50, wherein each microneedle has a regular pyramidal or conical protrusion shape.
[0160] 52. A patch according to any one of claims 32 to 50, wherein each microneedle has a rectangular prism shape. 53. A patch according to any one of appendices 32 to 52, wherein each microneedle has a length of between 500 μm and 2000 μm. 54. The patch of claim 53, wherein each microneedle has a length of 700 μm to 1200 μm. 55. A patch according to any one of claims 32 to 54, wherein each microneedle has a base width of between 100 μm and 700 μm. 56. The patch of claim 55, wherein each microneedle has a base of 200 μm to 400 μm.
[0161] 57. A patch described in any one of notes 32 to 56, wherein the lattice structure has a volume of 0.01 μL to 2 μL. 58. The patch of claim 57, wherein the lattice microstructure has a volume of 0.1 μL. 59. Each microneedle is A tip portion having a solid structure; A main body portion having a lattice structure; A base portion having a solid structure; The patch according to any one of appendices 32 to 58, comprising: 60. The patch described in claim 59, wherein the tip portion has a length of 25 μm to 500 μm. 61. A patch as described in appendix 59 or 60, wherein the tip portion has a base width of 50 μm to 300 μm.
[0162] 62. A patch described in any one of notes 59 to 61, wherein the microneedles have a tip diameter of 0.1 μm to 10 μm. 63. A patch according to any one of notes 59 to 62, wherein the main body portion has a length of 50 μm to 1000 μm. 64. A patch according to any one of notes 59 to 62, wherein the main body portion has a width of 50 μm to 300 μm. 65. A patch according to any one of notes 59 to 64, wherein the base portion has a length of 25 μm to 500 μm. 66. A patch according to any one of notes 59 to 65, wherein the base portion has a base width of 50 μm to 300 μm.
[0163] 67. A patch according to any one of claims 32 to 66, wherein each microneedle is formed from a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. 68. A patch described in any one of claims 32 to 67, wherein the one or more microneedle lattice microstructures are formed from polyethylene glycol dimethacrylate (PEGDMA). 69. A patch according to any one of claims 32 to 68, wherein one or more microneedles are formed from a biodegradable polymeric material. 70. A patch according to any one of claims 32 to 69, wherein one or more microneedles are soluble in an aqueous medium.
[0164] 71. A method of making a polymeric microneedle comprising a lattice microstructure having one or more lattice cell units, comprising: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) moving the build elevator away from the build surface; and c) irradiating a first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; d) repeating steps a) through c) in a manner sufficient to produce microneedles comprising a lattice microstructure; The method includes: 72. The method of claim 71, wherein the polymerizable composition is in contact with a build elevator and a build surface. 73. The method of claim 72, comprising irradiating the polymerizable composition for a period of time sufficient to bond a first polymerized region of the polymerizable composition to the build elevator. 74. The method of any one of claims 71 to 73, wherein the build elevator is moved in predetermined increments of 0.5 μm to 1.0 μm. 75. The method of claim 74, further comprising applying a polymerizable composition to the build surface after each movement of the build elevator away from the build surface.
[0165] 76. The method of any one of claims 71 to 75, wherein the polymerizable composition is irradiated through the build surface. 77. The method of any one of claims 71 to 76, wherein the polymerizable composition is irradiated in the presence of a polymerization inhibitor. 78. The method of any one of claims 71 to 77, wherein the polymerizable composition is polymerized continuously while moving the build elevator away from the build surface. 79. The method of any one of claims 77 to 78, wherein the build surface is permeable to the polymerization inhibitor. 80. The method of claim 76, wherein the polymerization inhibitor is oxygen.
[0166] 81. The method of any one of claims 71 to 80, wherein the polymerizable composition is irradiated with light. 82. The method of claim 81, wherein the polymerizable composition is irradiated with a micro-digital light projection system. 83. Micro digital light projection system an optical beam generator component; 83. The method of claim 82, comprising a light projection monitoring component. 84. An optical beam generator component comprising: light source, Tube lenses, and 84. The method of claim 83, comprising one or more projection lenses. 85. The method of claim 84, wherein the light beam generator component comprises two projection lenses.
[0167] 86. The method of claim 85, wherein the projection lens is a magnifying lens. 87. The method of claim 86, wherein the projection lens provides a magnification between 2x and 10x. 88. The method of any one of notes 84-87, wherein the optical projection monitoring component comprises an optical detector. 89. The method of claim 88, wherein the photodetector comprises a charge-coupled device (CCD). 90. The method of any one of claims 82-89, comprising determining a focal plane on the build surface from a micro digital light projection system.
[0168] 91. Determining a focal plane on a build surface from a micro-digital light projection system illuminating a build surface with a strobe light source through a tube lens; moving the build surface until the light is focused onto the build surface through the tube lens; 91. The method of claim 90, comprising: 92. The method of claim 91, wherein the build surface is illuminated with a plane of light having an image pattern projected using a strobe light source. 93. The method of claim 91 or 92, wherein the build surface is moved until the projected image pattern is in focus with the build surface. 94. The method of any one of claims 91 to 93, wherein the focal plane on the build surface is determined with a photodetector. 95. The method of any one of claims 91 to 93, comprising generating an image stack comprising a plurality of projected image patterns.
[0169] 96. The method of claim 95, wherein the focal plane of the build surface is determined from the generated image stack. 97. The method of any one of claims 91 to 96, wherein the focal plane is determined through a travel depth of the build surface of 400 μm or less. 98. The method of any one of notes 82 to 97, wherein the micro digital light projection system provides a grating microstructure resolution of 1.0 μm to 4 μm. 99. The method of claim 98, wherein the micro digital light projection system provides a grating microstructure resolution of 1.5 μm to 3.8 μm. 100. The method of any one of claims 71 to 99, wherein the polymerizable composition comprises a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof.
[0170] 101. The method of claim 100, wherein the polymerizable composition comprises polyethylene glycol dimethacrylate (PEGDMA). 102. The method of any one of claims 71 to 101, wherein the microneedle comprises two or more repeating lattice cell units. 103. The method of any one of claims 71 to 101, wherein the microneedle comprises five or more repeating lattice cell units. 104. The method of any one of claims 71 to 103, comprising providing a gradient of lattice cell units such that the density of the lattice cell units increases along the longitudinal axis of the microneedle. 105. The method of any one of appendixes 71 to 104, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle.
[0171] 106. The method of any one of claims 71 to 105, wherein the microneedle has a lattice cell unit having a size of 100 μm to 1000 μm. 107. The method of claim 106, wherein the microneedle comprises lattice cell units having a size of 200 μm to 500 μm. 108. The method of any one of claims 71 to 107, wherein the lattice microstructure comprises a plurality of struts. 109. The method of claim 108, wherein the lattice microstructure comprises struts having a thickness of 25 μm to 150 μm. 110. The method of claim 108, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm.
[0172] 111. The method of claim 108, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 112. The method of any one of appendices 71 to 111, wherein the microneedle has a square pyramid or conical protrusion shape. 113. The method of any one of claims 71 to 111, wherein the microneedles have a rectangular prism shape. 114. The method of any one of appendices 71 to 113, wherein the microneedle has a length of 500 μm to 2000 μm. 115. The method of claim 114, wherein the microneedle has a length of 700 μm to 1200 μm.
[0173] 116. The method of any one of notes 71 to 115, wherein the microneedles have a base width of 100 μm to 700 μm. 117. The method of claim 116, wherein the microneedles have a base width of 200 μm to 400 μm. 118. The method of any one of notes 71 to 117, wherein the lattice microstructure has a volume of 0.01 μL to 2 μL. 119. The method of claim 118, wherein the lattice microstructure has a volume of 0.1 μL. 120. Microneedles, A tip portion having a solid structure; A main body portion having a lattice structure; A base portion having a solid structure; The method of any one of appendices 71 to 119, comprising:
[0174] 121. The method of claim 120, wherein the tip portion has a length of 25 μm to 500 μm. 122. The method of claim 120 or 121, wherein the tip portion has a base width of 50 μm to 300 μm. 123. The method of claim 120 or 121, wherein the microneedle has a tip diameter of 0.1 μm to 10 μm. 124. The method of any one of notes 120 to 123, wherein the body portion has a length of 50 μm to 1000 μm. 125. The method of any one of notes 120 to 123, wherein the body portion has a width of 50 μm to 300 μm.
[0175] 126. The method of any one of notes 120 to 125, wherein the base portion has a length of 25 μm to 500 μm. 127. The method of any one of notes 120 to 125, wherein the base portion has a base width of 50 μm to 300 μm. 128. The method of any one of claims 71 to 127, wherein the microneedles are soluble in an aqueous medium.
[0176] 129. On the subject's skin surface, A backing layer; a plurality of polymeric microneedles in contact with a backing layer, each microneedle including a lattice microstructure having one or more lattice cell units; 23. A method comprising applying a patch, comprising: 130. The method of claim 129, wherein the microneedles contain an active agent compound and applying the patch to the skin surface of the subject is sufficient to deliver a therapeutically effective amount of the active agent compound to the subject. 131. The method of claim 130, wherein the active agent comprises a small molecule active agent compound. 132. The method of claim 130, wherein the active agent comprises an immunogenic active agent compound. 133. The method of claim 132, wherein the active agent compound comprises a vaccine.
[0177] 134. The method of claim 129, comprising applying a patch to a skin surface of a subject in a manner sufficient to collect a biological fluid sample from the subject into the microneedle. 135. The method of claim 134, wherein the biological fluid sample comprises interstitial fluid. 136. The method of claim 134, wherein the biological fluid sample comprises skin fluid. 137. The method of any one of claims 134 to 136, comprising collecting between 0.01 μL and 250 μL of biological fluid from the subject. 138. The method of any one of claims 134 to 136, comprising collecting between 0.01 μL and 2 μL of biological fluid from a subject using each of a plurality of microneedles.
[0178] 139. The method of any one of claims 129 to 138, comprising maintaining the patch on the subject's skin surface for an extended period of time. 140. The method of claim 139, comprising maintaining the patch on the subject's skin surface for 6 hours or more. 141. The method of claim 139, comprising maintaining the patch on the subject's skin surface for 12 hours or more. 142. The method of claim 139, comprising maintaining the patch on the subject's skin surface for 24 hours or more. 143. The method of any one of claims 129 to 138, comprising removing the patch within 15 minutes after applying the patch to the skin surface of the subject.
[0179] 144. The method of claim 143, comprising removing the patch within 5 minutes after applying the patch to the skin surface of the subject. 145. The method of claim 143, comprising removing the patch within 1 minute after applying the patch to the subject's skin surface. 146. The method of any one of claims 129 to 145, wherein the plurality of microneedles forms an array of microneedles on the backing layer. 147. The method of any one of claims 129 to 146, wherein the microneedles are spaced apart from one another on the backing layer by an average distance of 5 μm to 1000 μm. 148. The method of claim 147, wherein the microneedles are spaced apart from each other on the backing layer by an average distance of 100 μm to 500 μm.
[0180] 149. The method of any one of notes 129-148, wherein the backing layer further comprises a pressure-sensitive adhesive. 150. The method of any one of claims 129 to 149, wherein each microneedle comprises two or more repeating lattice cell units. 151. The method of any one of claims 129 to 149, wherein each microneedle comprises five or more repeating lattice cell units. 152. The method of any one of claims 129 to 151, wherein the microneedle comprises a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle. 153. The method of any one of appendixes 129-152, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle.
[0181] 154. The method of any one of claims 129 to 153, wherein each microneedle comprises a lattice cell unit having a size of 100 μm to 1000 μm. 155. The method of claim 154, wherein each microneedle comprises a lattice cell unit having a size of 200 μm to 500 μm. 156. The method of any one of notes 129 to 155, wherein the lattice microstructure comprises a plurality of struts. 157. The method of claim 156, wherein the lattice microstructure comprises struts having a thickness of 25 μm to 150 μm. 158. The method of claim 156, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm.
[0182] 159. The method of claim 156, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 160. The method of any one of claims 129 to 159, wherein each microneedle has a square pyramid or conical protrusion shape. 161. The method of any one of claims 129 to 159, wherein each microneedle has a rectangular prism shape. 162. The method of any one of appendices 129 to 161, wherein each microneedle has a length of 500 μm to 2000 μm. 163. The method of claim 162, wherein each microneedle has a length of between 700 μm and 1200 μm.
[0183] 164. The method of any one of notes 129 to 163, wherein each microneedle has a base width of between 100 μm and 700 μm. 165. The method of claim 164, wherein each microneedle has a base width of between 200 μm and 400 μm. 166. The method of any one of notes 129 to 165, wherein the lattice structure has a volume of 0.01 μL to 2 μL. 167. The method of claim 166, wherein the lattice microstructure has a volume of 0.1 μL. 168. Each microneedle is A tip portion having a solid structure; A main body portion having a lattice structure; A base portion having a solid structure; The method of any one of appendices 129 to 167, comprising:
[0184] 169. The method of claim 168, wherein the tip portion has a length of 25 μm to 500 μm. 170. The method of claim 168 or 169, wherein the tip portion has a base width of 50 μm to 300 μm. 171. The method of any one of claims 168 to 170, wherein the microneedle has a tip diameter of 0.1 μm to 10 μm. 172. The method of any one of clauses 168-171, wherein the body portion has a length of 50 μm to 1000 μm. 173. The method of any one of clauses 168-172, wherein the body portion has a width of 50 μm to 300 μm.
[0185] 174. The method of any one of notes 168-172, wherein the base portion has a length of 25 μm to 500 μm. 175. The method of any one of clauses 168-172, wherein the base portion has a base width of 50 μm to 300 μm. 176. The method of any one of claims 129 to 175, wherein each microneedle is formed from a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. 177. The method of any one of claims 129 to 175, wherein the lattice microstructure of one or more microneedles is formed from polyethylene glycol dimethacrylate (PEGDMA). 178. The method of any one of claims 129 to 177, wherein the one or more microneedles are formed from a biodegradable polymerizable material. 179. The method of any one of claims 129 to 177, wherein the one or more microneedles are soluble in an aqueous medium.
[0186] 180. A system for fabricating a polymeric microneedle comprising a lattice microstructure having one or more lattice cell units, comprising: 1. A micro digital light projection system, comprising: an optical beam generator component; a micro digital light projection system including a light projection monitoring component; a liquid interfacial polymerization module configured to generate microneedles from a polymerizable composition positioned therebetween, the liquid interfacial polymerization module comprising a build elevator and a build surface; A system comprising: 181. An optical beam generator component comprising: light source, Tube lenses, and 181. The system of claim 180, comprising one or more projection lenses. 182. The system of any one of claims 180 to 181, wherein the optical beam generator component comprises two projection lenses. 183. The system of claim 182, wherein the projection lens is a magnifying lens. 184. The system of claim 183, wherein the projection lens provides a magnification between 2x and 10x.
[0187] 185. The system of any one of notes 180-184, wherein the optical projection monitoring component comprises an optical detector. 186. The system of claim 185, wherein the photodetector comprises a charge-coupled device (CCD). 187. The system further comprises a processor having a memory operatively coupled to the processor, the memory having instructions stored therein, the instructions, when executed by the processor, causing the processor to: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) moving the build elevator away from the build surface; c) irradiating a first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; and d) repeating steps a) through c) in a manner sufficient to produce polymeric microneedles with lattice microstructures; 187. A system according to any one of appendices 180 to 186. 188. The system of claim 187, wherein the memory comprises instructions stored therein that, when executed by the processor, cause the processor to irradiate the polymerizable composition for a period of time sufficient to bond a first polymerized region of the polymerizable composition to the build elevator. 189. The system of claim 187 or 188, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to move the build elevator in predetermined increments of between 0.5 μm and 1.0 μm.
[0188] 190. The system of any one of notes 180-189, further comprising a source of a polymerizable composition. 191. The system of claim 190, configured to apply a polymerizable composition to the build surface after each movement of the build elevator away from the build surface. 192. The system of any one of notes 181 to 191, wherein the light source is configured to illuminate through the build surface. 193. The system of any one of notes 180 to 192, wherein at least a portion of the build surface is permeable to the polymerization inhibitor. 194. The system of claim 193, wherein the polymerization inhibitor is oxygen.
[0189] 195. The system of any one of notes 180-194, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to determine a focal plane on the build surface from the micro digital light projection system. 196. A memory having instructions stored therein, the instructions, when executed by a processor, causing the processor to: illuminating a build surface with a strobe light source through a tube lens; moving the build surface until the light is focused onto the build surface through the tube lens; 196. The system of claim 195, comprising: 197. The system of claim 196, wherein the memory comprises instructions stored thereon that, when executed by the processor, cause the processor to illuminate the build surface with a plane of light having a projected image pattern using a strobe light source. 198. The system of claim 196 or 197, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to illuminate the build surface with a plane of light having a projected image pattern using a strobe light source. 199. The system of any one of notes 196-198, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to move the build surface until the projected image pattern is in focus with the build surface.
[0190] 200. The system of any one of notes 196-199, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to generate an image stack including a plurality of projected image patterns. 201. The system of claim 200, wherein the memory comprises instructions stored therein that, when executed by the processor, cause the processor to determine a focal plane of the build surface based on the generated image stack. 202. The system of any one of claims 196-201, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to determine the focal plane through a travel depth of the build surface of 400 μm or less. 203. The system of any one of clauses 180-202, providing for generating a grating microstructure resolution of 1.0 μm to 4 μm. 204. The system of any one of clauses 180-202, providing for generating a grating microstructure resolution of 1.5 μm to 3.8 μm.
[0191] 205. The system of any one of appendixes 180-204, wherein the polymerizable composition comprises a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. 206. The system of claim 205, wherein the polymerizable composition comprises polyethylene glycol dimethacrylate (PEGDMA). 207. The system of any one of notes 180-206, wherein the microneedle comprises two or more repeating lattice cell units. 208. The system of any one of claims 180 to 206, wherein the microneedle comprises five or more repeating lattice cell units. 209. The system of any one of claims 180 to 208, comprising a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle.
[0192] 210. The system of any one of appendixes 180-209, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle. 211. A system according to any one of claims 180 to 210, wherein the microneedle has a lattice cell unit having a size of 100 μm to 1000 μm. 212. The system of claim 211, wherein the microneedle comprises lattice cell units having a size of 200 μm to 500 μm. 213. The system of any one of notes 180-212, wherein the lattice microstructure comprises a plurality of struts. 214. The system of claim 213, wherein the lattice microstructure comprises struts having a thickness between 25 μm and 150 μm.
[0193] 215. The system of claim 213, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm. 216. The system of claim 213, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 217. A system described in any one of notes 180 to 216, wherein the microneedle has a square pyramid or conical protrusion shape. 218. The system of any one of notes 180 to 216, wherein the microneedles have a rectangular prism shape. 219. A system according to any one of notes 180 to 218, wherein the microneedle has a length of 500 μm to 2000 μm.
[0194] 220. The system of claim 219, wherein the microneedle has a length of 700 μm to 1200 μm. 221. The system of any one of claims 180 to 220, wherein the microneedles have a base width of 100 μm to 700 μm. 222. The system of claim 221, wherein the microneedle has a base width of 200 μm to 400 μm. 223. The system of any one of notes 180 to 222, wherein the lattice microstructure has a volume of 0.01 μL to 2 μL. 224. The system of claim 223, wherein the grating microstructure has a volume of 0.1 μL.
[0195] 225. Microneedles, A tip portion having a solid structure; A main body portion having a lattice structure; A base portion including a solid structure; The system of any one of appendices 180 to 224, comprising: 226. The system of claim 225, wherein the tip portion has a length of 25 μm to 500 μm. 227. The system of claim 225 or 226, wherein the tip portion has a base width of 50 μm to 300 μm. 228. A system described in any one of notes 225 to 227, wherein the microneedle has a tip diameter of 0.1 μm to 10 μm. 229. The system of any one of notes 225 to 228, wherein the body portion has a length of 50 μm to 1000 μm.
[0196] 230. The system of any one of notes 225-228, wherein the body portion has a width of 50 μm to 300 μm. 231. The system of any one of notes 225 to 230, wherein the base portion has a length of 25 μm to 500 μm. 232. The system of any one of notes 225 to 230, wherein the base portion has a base width of 50 μm to 300 μm. 233. A system according to any one of claims 180 to 232, wherein the microneedles are soluble in an aqueous medium.
[0197] 234. A method for making a polymer structure having a lattice microstructure having one or more lattice cell units, comprising: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) moving the build elevator away from the build surface; and c) irradiating a first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; d) repeating steps a) through c) in a manner sufficient to produce a polymer structure having a lattice microstructure; The method includes: 235. The method of claim 234, wherein the polymerizable composition is in contact with the build elevator and the build surface. 236. The method of claim 235, comprising irradiating the polymerizable composition for a period of time sufficient to bond a first polymerized region of the polymerizable composition to the build elevator. 237. The method of any one of notes 234-236, wherein the build elevator is moved in predetermined increments of 0.5 μm to 1.0 μm. 238. The method of claim 237, further comprising applying a polymerizable composition to the build surface after each movement of the build elevator away from the build surface.
[0198] 239. The method of any one of notes 234-238, wherein the polymerizable composition is irradiated through the build surface. 240. The method of any one of claims 234 to 239, wherein the polymerizable composition is irradiated in the presence of a polymerization inhibitor. 241. The method of any one of claims 234-240, wherein the polymerizable composition is polymerized continuously while moving the build elevator away from the build surface. 242. The method of any one of claims 240 to 241, wherein the build surface is permeable to the polymerization inhibitor. 243. The method of claim 242, wherein the polymerization inhibitor is oxygen.
[0199] 244. The method of any one of appendices 234-243, wherein the polymerizable composition is irradiated with light. 245. The method of claim 244, wherein the polymerizable composition is irradiated with a micro-digital light projection system. 246. Micro digital light projection system an optical beam generator component; 26. The method of claim 245, comprising a light projection monitoring component. 247. An optical beam generator component comprising: light source, Tube lenses, and 27. The method of claim 246, comprising one or more projection lenses. 248. The method of claim 247, wherein the light beam generator component comprises two projection lenses.
[0200] 249. The method of claim 248, wherein the projection lens is a magnifying lens. 250. The method of claim 249, wherein the projection lens provides a magnification between 2x and 10x. 251. The method of any one of notes 246-250, wherein the optical projection monitoring component comprises an optical detector. 252. The method of claim 251, wherein the photodetector comprises a charge-coupled device (CCD). 253. The method of any one of clauses 246-252, including determining a focal plane on the build surface from a micro digital light projection system.
[0201] 254. Determining a focal plane on a build surface from a micro digital light projection system; illuminating a build surface with a strobe light source through a tube lens; moving the build surface until the light is focused onto the build surface through the tube lens; 254. The method of claim 253, comprising: 255. The method of claim 254, wherein the build surface is illuminated with a plane of light having an image pattern projected using a strobe light source. 256. The method of any one of notes 254-256, wherein the build surface is moved until the projected image pattern is in focus with the build surface. 257. The method of any one of notes 254-256, wherein the focal plane on the build surface is determined with a photodetector. 258. The method of any one of notes 254 to 257, comprising generating an image stack including a plurality of projected image patterns.
[0202] 259. The method of claim 258, wherein the focal plane of the build surface is determined from the generated image stack. 260. The method of any one of notes 254-259, wherein the focal plane is determined through a travel depth of the build surface of 400 μm or less. 261. The method of any one of notes 245-260, wherein the micro digital light projection system provides a grating microstructure resolution of 1.0 μm to 4 μm. 262. The method of claim 261, wherein the micro digital light projection system provides a grating microstructure resolution of 1.5 μm to 3.8 μm. 263. The method of any one of appendices 234 to 262, wherein the polymerizable composition comprises a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof.
[0203] 264. The method of claim 263, wherein the polymerizable composition comprises polyethylene glycol dimethacrylate (PEGDMA). 265. The method of any one of claims 234 to 264, wherein the polymer structure is formed from a biodegradable polymerizable material. 266. The method of any one of claims 234 to 264, wherein the polymer structure is soluble in an aqueous medium. 267. The method of any one of notes 234 to 266, wherein the polymer structure comprises two or more repeating lattice cell units. 268. The method of claim 267, wherein the polymer structure comprises five or more repeating lattice cell units.
[0204] 269. The method of any one of claims 234 to 268, wherein the polymer structure comprises a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the polymer structure. 270. The method of any one of notes 234 to 269, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle. 271. The method of any one of notes 234 to 270, wherein the polymer structure has lattice cell units having a size of 100 μm to 1000 μm. 272. The method of claim 271, wherein the polymer structure has lattice cell units having a size of 200 μm to 500 μm. 273. The method of any one of notes 234-272, wherein the lattice microstructure comprises a plurality of struts.
[0205] 274. The method of claim 273, wherein the lattice microstructure comprises struts having a thickness of 25 μm to 150 μm. 275. The method of claim 273, wherein the lattice microstructure comprises struts having a thickness of 50 μm to 100 μm. 276. The method of claim 273, wherein the lattice microstructure comprises struts having a thickness of 70 μm to 90 μm. 277. The method of any one of notes 234 to 276, wherein the polymer structure has a length of 500 μm to 2000 μm. 278. The method of claim 277, wherein the polymer structure has a length of 700 μm to 1200 μm.
[0206] 279. The method of any one of notes 234 to 278, wherein the polymer structure has a base width of 100 μm to 700 μm. 280. The method of claim 279, wherein the polymer structure has a base of 200 μm to 400 μm. 281. The method of any one of claims 234 to 280, wherein the lattice microstructure has a volume of 0.01 μL to 2 μL. 282. The method of claim 281, wherein the lattice microstructure has a volume of 0.1 μL.
[0207] 283. A system for fabricating a polymer structure including a lattice microstructure having one or more lattice cell units, comprising: 1. A micro digital light projection system, comprising: an optical beam generator component; a micro digital light projection system including a light projection monitoring component; a liquid interfacial polymerization module configured to generate a polymer structure from a polymerizable composition positioned therebetween, the liquid interfacial polymerization module comprising a build elevator and a build surface; A system comprising: 284. An optical beam generator component comprising: light source, Tube lenses, and 284. The system of claim 283, comprising one or more projection lenses. 285. The system of any one of claims 283 to 284, wherein the light beam generator component comprises two projection lenses. 286. The system of claim 285, wherein the projection lens is a magnifying lens. 287. The system of claim 286, wherein the projection lens provides a magnification between 2x and 10x.
[0208] 288. The system of any one of notes 283-287, wherein the optical projection monitoring component comprises an optical detector. 289. The system of claim 288, wherein the light detector comprises a charge-coupled device (CCD). 290. The system further comprises a processor having a memory operatively coupled to the processor, the memory having instructions stored therein, the instructions, when executed by the processor, causing the processor to: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) moving the build elevator away from the build surface; c) irradiating a first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; and d) repeating steps a)-c) in a manner sufficient to produce a polymer microstructure comprising a lattice microstructure. 291. The system of claim 290, wherein the memory comprises instructions stored therein that, when executed by the processor, cause the processor to irradiate the polymerizable composition for a period of time sufficient to bond a first polymerized region of the polymerizable composition to the build elevator. 292. The system of any one of claims 290 to 291, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to move the build elevator in predetermined increments of between 0.5 μm and 1.0 μm.
[0209] 293. The system of any one of claims 291 to 292, further comprising a source of a polymerizable composition. 294. The system of claim 293, configured to apply a polymerizable composition to the build surface after each movement of the build elevator away from the build surface. 295. The system of any one of notes 283 to 294, wherein the light source is configured to illuminate through the build surface. 296. The system of any one of notes 283 to 295, wherein at least a portion of the build surface is permeable to the polymerization inhibitor. 297. The system of claim 296, wherein the polymerization inhibitor is oxygen.
[0210] 298. The system of any one of notes 283-297, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to determine a focal plane on the build surface from a micro digital light projection system. 299. A memory having instructions stored therein that, when executed by a processor, cause the processor to: illuminating the build surface with a strobe light source through a tube lens; 299. The system of claim 298, wherein the focal plane is determined by moving the build surface until light is focused onto the build surface through a tube lens. 300. The system of claim 299, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to illuminate the build surface with a plane of light having a projected image pattern using a strobe light source. 301. The system of claim 299 or 300, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to illuminate the build surface with a plane of light having a projected image pattern using a strobe light source. 302. The system of any one of notes 299-301, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to move the build surface until the projected image pattern is in focus with the build surface.
[0211] 303. A system described in any one of notes 299 to 302, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to generate an image stack including a plurality of projected image patterns. 304. The system of claim 303, wherein the memory comprises instructions stored thereon that, when executed by the processor, cause the processor to determine a focal plane of the build surface based on the generated image stack. 305. The system of any one of notes 299-304, wherein the memory has instructions stored therein that, when executed by the processor, cause the processor to determine the focal plane through a travel depth of the build surface of 400 μm or less. 306. The system of any one of clauses 283-305, providing for generating a grating microstructure resolution of 1.0 μm to 4 μm. 307. The system of any one of clauses 283-305, providing for generating a grating microstructure resolution of 1.5 μm to 3.8 μm.
[0212] 308. The system of any one of claims 283 to 307, wherein the polymerizable composition comprises a polymerizable material selected from the group consisting of polycaprolactone, polyalicholic acid, polylactic acid, polylactic-co-glycolic acid, polyethylene glycol, thiol-ene, anhydrides, polyacrylic acid, polymethyl methacrylate, trimethylolpropane triacrylate (TMPTA) monomer, polyvinyl alcohol, polyvinylpyrrolidone, vinyl carbonate, vinyl esters, acrylamide, hyaluronic acid, chitosan, collagen, gelatin, carboxymethylcellulose, and blends or copolymers thereof. 309. The system of claim 308, wherein the polymerizable composition comprises polyethylene glycol dimethacrylate (PEGDMA).
[0213] experiment The following examples are presented by way of illustration and not by way of limitation. Specifically, the following examples are examples of specific embodiments for carrying out the present disclosure. The examples are for illustrative purposes only and are not intended to limit the scope of the present disclosure in any way. Efforts have been made to ensure accuracy with respect to the numbers used (e.g., amounts, temperatures, etc.), but some experimental error and deviation should be allowed for.
[0214] Example 1 Combining a reduction lens optical system for single-digit micron resolution, an in-line camera system for contrast-based sharpness optimization, and continuous liquid interface generation (CLIP) technology for high scalability, a single-digit micron resolution CLIP-based 3D printer is provided that can create millimeter-scale 3D prints with single-digit micron resolution features in just a few minutes. Simulation models are developed in parallel to explore the underlying key principles of optics, chemical kinetics, and material transport in the 3D printing process. A printing strategy with adjustable parameters informed by the simulation models is employed to achieve both optimal resolution and maximum printing speed. Taken together, the high-resolution 3D CLIP printer presented herein provides applications including, but not limited to, biomedical, MEMS, and microelectronics.
[0215] In this embodiment, the 3D printer is 10 times faster than commercially available high-resolution 3D printers (e.g., NanoScribe). 5A high-resolution CLIP technique that allows the fabrication of 3D structures containing single-digit micron features at fast printing speeds. This is achieved by combining the CLIP technique with a custom-designed projection optics and an in-line contrast-based focusing system. To manipulate the shallow depth of focus of the high-magnification objective lens, a robust calibration platform is developed to find the optimal focal plane and thus reproducibly resolve the fine details of the projected pattern. To understand the effect of photopolymerization kinetics and resin transport on printing speed on the printing resolution in this system, a numerical model is introduced that considers all the fundamental elements of a high-resolution 3D CLIP printing system, including optical projection, photopolymerization reaction kinetics, and resin mass transport. The model utilizes an understanding of the fundamental transport phenomena and provides a printing strategy that determines the printing parameters of the printer software control system. In addition, the model described herein provides fundamental insights into 3D CLIP printing in general and provides accurate predictions of the surface finish of the printed part, dead zone thickness, and resin curing during the 3D printing process. A new single-digit micron resolution 3D CLIP-100-based printer is demonstrated using a custom-designed projection optical lens system, an in-line focusing system, and a software-controlled printing process informed by parameters from a first-principles-based model.
[0216] Materials and Methods High resolution CLIP hardware design The hardware components of a CLIP-based 3D printer with single-digit micron resolution can be divided into four components:
[0217] (1) Projection optics components: light engine (3DLP9000, Digital Light Innovations, TX), tube lenses (SM1L10, Thorlabs, NJ; 54-774 Edmund Optics, NJ), projection lenses (5x Mitutoyo Plan Apo Infinity Corrected Long WD Objective for 1.5 μm resolution; 2x Mitutoyo Plan Apo Infinity Corrected Long WD Objective for 3.8 μm resolution, Edmund optics, NJ).
[0218] (2) Oxygen-permeable resin vat: A custom-designed 3D printed resin vat (Teflon AF2400 film, Random Technology, CA) with an oxygen-permeable window is a key component to achieve the CLIP technique, allowing UV to pass through for photopolymerization and oxygen to permeate to inhibit photopolymerization directly above the window within a dead zone thickness of approximately 50–80 μm.
[0219] (3) Build platform: A high-precision vertical translation stage (GTS70V, Newport, CA) was used to fine-tune the vertical position, and an SEM mount (TedPella Inc, Reddings, CA) was used as the build platform on which the printed part was attached.
[0220] (4) Real-time projection monitoring subsystem for focusing: The focusing subsystem consists of a beam splitter cube (CCM1-4ER, Thorlabs, NJ) equipped with a UVFS plate beam splitter 30:70 (R:T) (BSS10R, Thorlabs, NJ), a strobe light illumination system (RL3536-WHIIC, Advanced Illumination, Rochester, VT), and a UV camera (CS126MU, Thorlabs, NJ) mounted on an adjustable tube lens (SM1V10, Thorlabs, NJ) to focus and monitor the UV projection detector.
[0221] High resolution CLIP software design Control of the single-digit micron resolution CLIP-based 3D printer is handled by CLIP3DGUI, a custom software application developed in the Qt framework (Qt Creator, Finland) using C++. CLIP3DGUI controls the operation of the light engine, translation stages, and printing process through a set of user-controlled parameters optimized for each print.
[0222] Light Engine: 2560x1600 1-bit binary image slices generated from a 3D CAD design are imported and then processed by an image encoding pipeline where the 1-bit binary images are encoded into 24-bit RGB images, resulting in 24 1-bit images stored in a single frame. Image encoding provides high image throughput while allowing low frame rates of streaming images to the light engine, thus avoiding common pitfalls including dropped frames and inconsistent frame rates. The encoded images are streamed to the light engine via an HDMI cable, and exposure time, dark time, and LED intensity are all programmatically controlled via lookup tables uploaded to the light engine flash memory.
[0223] Stage: The translation stage parameters, including velocity, acceleration, and jerk, must be optimized to allow fast and precise movement between layers (736). However, increasing the velocity, acceleration, and jerk parameters introduces larger forces into the parts, increasing mechanical wear inside the translation stage.
[0224] Printing Process: A series of printing process parameters are used to further optimize the printing, including layer thickness, first exposure time for adhesion to the build platform, system resynchronization speed, translation stage limits, and start position.
[0225] Print script: Exposure time, dark time, LED intensity, stage speed, and stage acceleration can all be controlled on a layer-by-layer basis to optimize for the exact feature being printed at the time. This makes it possible to print very different geometries requiring very different parameters within the same print.
[0226] Preparation of high-resolution CLIP materials and resin formulation The resin used in the experiments was formulated with trimethylolpropane triacrylate (TMPTA) monomer, diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide (TPO) photoinitiator, and phenol, 2-750(5-chloro-2H-benzotriazol-2-yl)-6-(1,1-dimethylethyl)-4-methyl (BLS1326) benzotriazole type ultraviolet (UV) light absorber, all of which were purchased from Sigma-Aldrich (MO, USA). Various resins with different mixing ratios were used: 2.5 wt% TPO photoinitiator, 0.3 wt% BLS1326 with TMPTA. The cup of mixed solution was placed in a THINKY ARE-310 centrifugal mixer (THINKY, CA, USA) and centrifuged at 2200 rpm for 30 min while simultaneously rotating the cup in the opposite direction at 2000 revolutions per minute (rpm). EPU-40 elastomer resin was purchased from Carbon 3D (CA, USA). Isopropyl alcohol (IPA, 99%) was used as the washing solvent for all printed samples and was obtained from Fisher Scientific (MA, USA).
[0227] High-resolution CLIP material rheology measurements Rheological measurements were performed with a TA Instrument (ARES-G2) Rheometer (TA Instruments, New Castle, DE). Rheological characterization was performed for TMPTA + 2.5 wt% TPO photoinitiator, 0.3 wt% BLS1326, and EPU-40. Parallel plates with a diameter of 25 mm were used, and approximately 250 μL of solution was used for each experiment. Characterization included: (1) Flow sweep of TMPTA resin was performed at a temperature of 20°C with a shear rate sweep of 0.01-100 1 / s, a soak time of 120 seconds, and a shear rate sweep of 0.01-1000 1 / s, a soak time of 120 seconds, and a shear rate sweep of 20°C with a shear rate sweep of 0.01-1000 1 / s, and a shear rate sweep of 20°C with ... (4) The stress relaxation property of EPU40 resin is evaluated under a strain of 500%, a stress relaxation duration of 100 seconds, a dipping time of 60 seconds, and a temperature of 20°C.
[0228] High-resolution CLIP Stefan force measurements Measurements of the Stefan force experienced by the build platform are made using a load cell (Futek, Irvine, CA) with a maximum load of 1 lb. The load cell is rigidly mounted between the build platforms and force readings are taken at a frequency of 0.005 Hz. The Stefan force is extracted in a regime where the force has reached a steady state. The force experienced for each print radius is obtained from calculating the force amplitude readouts from each step movement and averaged over 100 seconds.
[0229] High-resolution CLIP data collection with NanoScribe The printing speed of high resolution 3D printers was compared using NanoScribe's TPP technology as a reference. The 3D structure was printed on the DiLL substrate with the IPO coated side. The IPO side was identified and checked using a multimeter, the resistance reading was 200 Ohm. The objective lens used to pattern the design is a 25x objective lens with an adjustable ring placed on the mark Glyc, and the resin used for this work is IP-S. Once printing was completed, the printed parts were cleaned by immersion in PGMEA developer for 20 minutes, quickly rinsed in IPA, and air dried with a compressed air gun.
[0230] High-resolution contrast-based focal plane optimization Contrast-based focal plane optimization includes the following steps: First, a coarse adjustment is performed to focus the CCD camera on the build platform. The coarse adjustment is performed by fixing the build platform at a specific position while rotating an adjustable tube lens. While manually flashing a strobe light on the build platform, the tube lens is adjusted to focus on the build platform (SEM mount) (Figure 9A). Figure 9A(i) and Figure 9A(ii) show the difference between the in-focus and out-of-focus states.
[0231] Next, project a mesh pattern from the UV light engine with a minimum feature width of 45 pixels (67.5 µm with the 5x magnification objective, 168 µm with the 2x magnification objective) onto the empty vat and drive the build platform in the z-axis until the projected pattern is approximately in focus (Figure 9B).
[0232] Finally, perform a fine adjustment with the resin material excluding the photoinitiator and analyze the through-focus image stack using a sharpness analysis algorithm (Figure 9C).
[0233] High-resolution CLIP image slicing and 3D printing procedure 3D CAD designs were either (1) custom designed using SolidWorks or Fusion360 in-house or (2) retrieved from online repositories (GRABCAD and cgtrader). A specific lattice design was generated using nTopology (nTopology, NY). Once the designs were generated, they were sliced to a specific layer thickness using Netfabb (Autodesk, CA). All prints in this study were sliced at a layer thickness of 0.5 μm. Because Netfabb was not able to slice at 0.5 μm, each design was scaled vertically by a factor of 2 and then sliced at a layer thickness of 1 μm. No modifications to the slices were applied. The slices were then applied to our custom software for 3D printing.
[0234] result Projection optical system for achieving single-digit micron resolution. A CLIP-based 3D printer system with single-digit micron resolution has been designed and implemented in our lab. The system is based on the combination of CLIP printing technology and a reduction optical system to achieve fast printing speed, smooth surface, and high-resolution printing (Figure 10A). The projection optical system consists of a tube lens and a microscope objective lens with built-in 2× and 5× magnification to reduce the original pixel size of 7.6 μm of the digital micromirror device (DMD) to 3.8 μm or 1.5 μm, respectively. A real-time projection pattern monitoring and focal plane adjustment system, including a beam splitter and a charge-coupled device (CCD) camera, is designed in the projection optical path (Figure 10B) (as described in the "Materials and Methods" section above).
[0235] The CLIP printing process is accomplished through an oxygen-permeable window that creates a thin dead zone that inhibits photopolymerization for the continued processing of the printed part (Figure 10C). This dead zone allows for a continuous flow of resin replenishment, thus eliminating the delamination of the printed part from the window, which is known to be the rate-limiting step in SLA, DLP, and PμSL.
[0236] Contrast-based focusing mechanism to optimize focal plane and print resolution Due to the shallow depth of focus (14 μm) of the high-magnification objective lens, a precise contrast-based focusing mechanism is implemented into the 3D printer system to achieve single-digit micron resolution and optimize the overall projection optics setup. The in-line focusing subsystem consists of a beam splitter, a tube lens, two potential microscope objective lenses, and a CCD camera (Figures 9A and 9B). This subsystem acquires the through-focus sharpness of the projected patterns, and we validated the performance by comparing the sharpness modulation transfer function (MTF) and the printed patterns side-by-side. The contrast-based focusing approach demonstrated that the projection optical system can rapidly and reproducibly achieve the optimal focal plane for multiple setups involving different microscope objective lenses (2× and 5×).
[0237] The contrast-based focal plane optimization method includes three distinct steps: (1) Coarse adjustment I: Coarsely adjust the tunable tube lens with strobe light illumination to focus on the build platform (Figure 9A). (2) Coarse adjustment II: Coarsely adjust the translational z-stage of the build platform to focus on the projected pattern (Figure 9B), and repeat (1) and (2) until both the build platform surface and the projected image are in focus. (3) Fine adjustment: Finely scan in the z-direction (400 μm) with the translational z-stage to obtain a through-focus projection image z-stack (Figures 9C-9E). Further details of the implementation of the contrast-based focusing algorithm can be found in the Materials and Methods section. An analysis scheme to extract sharpness information from the projection images is presented.
[0238] The MTF calculation is similar to the conventional optical transfer function (OTF) obtained from the slanted edge image. The line edge profile of the projected mesh image is extracted from the center of the strut, and the line spread function (LSF) is calculated with the first derivative of the line edge profile. After obtaining the LSF, a fast Fourier transform (FFT) is applied to the LSF to obtain the number of line pairs (lp) / mm. 2 The MTF is obtained in units of 12.6 lp / mm. 2 The through-focus MTFs are then compared to obtain the optimum focal plane. The details of the algorithm are described in detail below.
[0239] Finally, a set of through-focus printing results was obtained and compared with the projected image sharpness analysis. The through-focus sharpness results obtained from this analysis support our experimental findings (Figure 9E). From a total scanning distance of 400 μm, we observed an optimal focus position 150 μm away from the initial scanning position. Due to the shallow depth of focus (14 μm) of the high magnification objective lens, it is observed that both the printing performance and sharpness degrade rapidly away from the optimal focal plane. Through this contrast-based z-direction focusing method, the optimal focus position for high-resolution 3D printing is identified.
[0240] High-resolution CLIP modeling of optical systems, momentum, and mass transport Compared to commercial CLIP 3D printers with projected optical resolutions of 75-160 μm, the newly developed single-digit micron resolution CLIP-based 3D printer has a target resolution of 1.5-3.8 μm. With a 50-fold improvement in resolution, the physical properties of the CLIP printing process are described and optimal printing parameters are assigned to resolve the smallest possible features. To fully understand the high-resolution CLIP printing process, three main physical models are involved: (1) optical model: estimation of single pixel projected width from the projection lens optics, (2) fluid model: uncured resin flow profile during vertical translation stage movement, and (3) chemical model: describing photopolymerization (curing) including a gradient of oxygen concentration.
[0241] The components involved in the high-resolution CLIP printing process are shown in Figure 11A. These include a UV light engine that emits UV projections at a wavelength of 385 nm (from bottom to top), an oxygen-permeable window, a dead zone (height H) where uncured resin flows, a cured resin part, and a build platform that moves with a step size Δh at a pulling speed U. A general model is developed to cover a wide range of CLIP printers with various print resolution capabilities of 30 μm resolution and 1.5 μm resolution. After developing a numerical model to fully understand the CLIP process, the model is employed to a real 3D printing scenario, and the process is repeated through three fundamental steps (stage movement, stage stop, and UV exposure) (Figure 11B). Collectively, the multiphysics simulation tool allows for the estimation of many important factors required to achieve successful 3D printing, such as the spatial resolution of the 3D printed part, the maximum peel force experienced for a given projection area, and the dead zone thickness, which depends on printing parameters including dark time, exposure time, and UV intensity.
[0242] High-resolution 3D CLIP printing strategy Using knowledge of the high-resolution 3D CLIP printing process, a general description of the printing strategy is developed as follows: For the first layer of the print, the photocurable resin undergoes a longer initial exposure step that overcomes the gap between the uncured resin and the build platform, allowing the resin to successfully bond and attach to the build platform. The remaining layers are repeated through the following process (Figure 11B(i)). For the nth layer of the print, the stage moves upwards (z direction) in an increment of Δh (layer thickness, typically 0.5 μm to 1 μm). This upward stage movement temporarily creates a negative pressure in the dead zone, which results in resin refilling from both the left and right edges of the cured part until resin flow into the gap is completed and uniform pressure is restored (Figure 11B(ii)). There is a minimum amount of time required for the resin to travel to the center of the build part. Thus, there is a pause after the vertical stage movement to allow the uncured resin to fully refill the gap that has thickened by the increment of Δh (Figure 11B(iii)). After the fluid reaches the deepest pixel region (center of the cured resin) and the resin flow is essentially stationary, the resin is then exposed to a UV pattern for the (n+1)th layer, curing an additional Δh of resin (Figure 11B(iv)). These three printing steps, including stage movement, stage stop, and UV exposure, are repeated until the full 3D print is completed. The overall timeline and printing process is shown in Figure 11B(v). The estimates of the required stage movement and dwell times are grouped together as "dark time", and the duration of this "dark time" is informed by the model.
[0243] High-resolution CLIP optical modeling: Projection optics simulation Factors that govern the printing resolution include the spatial distribution of the projection optics, the exposure energy per unit area, the physicochemical properties of the photopolymer resin, and the printing parameters. First, we focus on the projection optics simulation. Due to the incoherence of the UV reflection pattern from the DMD of the light engine, we can model the final energy dispersion at the projection plane as a superposition of the point spread functions (PSFs) of all pixels on the DMD surface via a spatial convolution equation.
[0244]
number
[0245] where f(x,y) is the spatial intensity pattern projected through the DMD. Thus, a single pixel f(x,y) is:
[0246]
number
[0247] where 、 d x and d y are the lengths of the micromirrors along the x and y axes, m is the magnification of the projection optics, and grayscale is the intensity of a single DMD pixel. The spatial convolution equation (Eq. (1)) determines the equivalent Gaussian distribution function (ω0) at the focal plane of the projection optics. In FIG. 12A, 2D cross-sections of the fitted Gaussian curves and the effect of spatial convolution of the pixels are shown for both the 30 μm pixel and 1.5 μm pixel projection optics. The width of the spot diameter is 1 / e of the maximum intensity. 2 Under the assumption that , the single pixel projection width is simulated as 33.3 μm and 1.42 μm for the 30 μm pixel and 1.5 μm pixel projection systems, respectively. Finally, the spot diameter at the focal plane can be expressed as a Gaussian distribution, where the UV intensity of an ideal point source at a given position on the projection plane is:
[0248]
number
[0249] In the formula, I(J / cm 2 s) is the UV light intensity distribution, P (J / s) is the total power of the UV228 light, and ω0 (Gauss radius) is 1 / e of the Gauss maximum intensity (Imax). 2The xy plane is the focal plane of the projection optics, which in our experimental setup lies just above the deadzone surface.
[0250] High-resolution CLIP kinetic modeling: Photopolymerization gradient studies To develop our process model, we first employ a basic set of reactions commonly used to describe free radical polymerization, similar to that presented by Dendukuri et al. In the first step, UV light incident on the sample photolyzes a photoinitiator to generate a pair of radicals. The UV light intensity varies with the height of the sample according to Beer's law.
[0251]
number
[0252] where φ is the quantum yield formation of the initiating radical, ε is the molar extinction coefficient of the photoinitiator at 385 nm, I0 is the UV intensity at the surface of the window, and [PI] is the concentration of the photoinitiator. When the oxygen concentration falls below a certain threshold, the photoinitiator radical reacts with unreacted monomers to initiate chain polymerization. In the chain propagation step, the growing radicals (R, RM n ) are summarized in the term [X], and their formation propagates through a series of reactions with other monomer molecules with a rate constant k p The radical then undergoes two separate reactions with a rate constant k t (the biomolecule in the polymer radical), and (2) the rate constant k o The radicals are consumed and terminated through an oxygen inhibition reaction at . In this model, only bimolecular termination is considered and other modes of radical loss, such as trapping of radical species in the resulting polymer gel, are ignored, but likely play some role in reducing the rate of termination relative to propagation.
[0253]
number
[0254] To describe the concentration of radicals, a quasi-steady approximation (radical concentration remains constant, i.e., the initiation rate is equal to the termination rate, r a =r c ), we obtain the following:
[0255]
number
[0256] By constructing mass transport equations for oxygen and unconverted oligomers [M], their space-time concentrations can be solved. The transport and consumption of oxygen and oligomers in the system are described by:
[0257]
number
[0258] Since no flow is assumed, transport is by diffusion only, and the diffusion of oligomers is assumed to be small and is therefore neglected.
[0259]
number
[0260] where D0 is the diffusivity of oxygen in the oligomer, H is the height of the dead zone thickness, and [O 2,eqb
[0046] is the equilibrium concentration of oxygen at the surface of the oxygen permeable window), we obtain
[0261]
number
[0262] In the above, Da1 is the dimensionless Dankeler number that quantifies the ratio of oxygen inhibition to oxygen diffusion into the resin. The boundary and initial conditions of our system are as follows:
[0263]
number
[0264] Here, we assume that the initial resin region is oxygenated and that the oxygen flux through the build platform is zero. Because the diffusivity of oxygen in the Teflon AF2400 window is greater than that in the resin TMPTA, oxygen can flow freely through the window and the oxygen concentration at the window surface is [O 2,eqb ].
[0265]
number
[0266] By non-dimensionalizing (equation (8)) using and setting [M0] to the initial monomer concentration, we obtain
[0267]
number
[0268] The initial conditions are set as follows, where Da2 is the second dimensionless Dankeler number:
[0269]
number
[0270] By solving both PDEs (Eqs. (9, 10)) simultaneously using the parameters in (Figure 13D), the numerical PDE solutions for the transient oxygen and unconverted oligomer concentrations can be found in Figure 13A(i-ii), and a snapshot of all active components in the dead zone regime at t = 0.1(-) can be found in Figure 13A(iii). α = 290 8.09 × 10 -7 Assuming that is small (Fig. 13D), a steady-state solution can be obtained, and an analytical expression for the steady-state oxygen concentration is derived and compared with the numerical solution (Fig. 13D). It is found that the steady-state numerical solution is consistent with the analytical solution, indicating that the steady-state oxygen concentration profile is independent of the boundary conditions of the build platform (Fig. 13). The oxygen concentration threshold for the formation of the dead zone (or oxygen inhibition zone) is set at 10 -5 Assuming that, we can vary the parameter Da1 involved in the CLIP printing process and estimate the corresponding dead zone thickness under different values of Da1. The dead zone thickness is about 3-5 μm from our model prediction, and the thickness is determined by the appropriate Dankeler number.
[0271]
number
[0272] It is observed that the eigenvalue scales with the −0.5 power of eigenvalue (FIG. 13C).
[0273]
number
[0274] The Dankeler number is a measure of the ratio of the oxygen diffusion rate and the kinetic rate (rate of photopolymerization and oxygen depletion). We provide a justification for this scaling by calculating the steady-state value of the oxygen concentration (and therefore the dead zone thickness) as follows:
[0275] Analytical solution of oxygen concentration profile To provide a deeper understanding of the oxygen concentration profile at steady state, an approximate steady state analytical solution is solved. The dimensionless governing equation for the steady state oxygen concentration is (from Eq. (9)):
[0276]
number
[0277] However, note that both β and α are small parameters. Due to the fact that β is small, it can be approximated as follows (Equation (12)):
[0278]
number
[0279] Now, for small values of \mathbb {\displaystyle ...O}}\) we can expand the terms under the radical we assumed for the Taylor expansion, and keep only the leading order terms to get:
[0280]
number
[0281] this is
[0282]
number
[0283] However,
[0284]
number
[0285] If , the right hand side of Eq. 13 still represents a positive reactive sink for oxygen. Therefore, we conclude that we enter the regime of near-zero oxygen concentration when Eq. 14 is no longer accurate. To define that region and connect it to the region of finite oxygen concentration, we apply the following boundary conditions:
[0286]
number
[0287] where h denotes the end of the region of finite oxygen concentration. Note that the last two conditions are the continuity of oxygen concentration and oxygen flux across the two regions. Therefore, the actual value of η>h(
[0288]
number
[0289] ), we assume that the value of β is essentially zero.
[0290] In other words
[0291]
number
[0292] Then, applying the boundary conditions above, we can solve for θ in the region of finite oxygen concentration.
[0293]
number
[0294] It is also possible to use the last condition to solve for the value of (h), the steady-state dead-zone thickness.
[0295]
number
[0296] Solving, we get the following:
[0297]
number
[0298] The solution is now complete, and Figure 13C shows that it is in excellent agreement with the numerical solution for the parameters appropriate for the printing conditions. Based on this analysis, an estimate of the exposure time until the resin reaches a steady cure height at the dead zone thickness follows the equation:
[0299]
number
[0300] Overall, this study provides fundamental insights into the CLIP printing process, including how the dead-zone thickness depends on the oxygen permeability of the window, the oxygen concentration at the window surface, the applied light intensity, and the photoinitiator concentration.
[0301] High-resolution CLIP optical and dynamics modeling: 3D printed part predictions An understanding of the photopolymerization model (Eqs. (4-17)) was combined with the projection optics model (Eqs. (1-3)) to predict the final 3D printed structure. The photopolymerization model served as a prediction of the cure height, while the 2D projection optics model provided a prediction of the minimum lateral resolution achievable by the optical design. To validate the model's performance, a regular square pyramid microstructure was designed and the simulation model was used to compare the height and surface finish between the 3D printed part from a CLIP-based 3D printer with one-digit micro-resolution and the simulated 3D printed object. The simulation results and corresponding SEM images of the 3D printed structures 30 μm (Figure 12B(i)) and 1.5 μm (Figure 12B(ii)) CLIP printers are compared to provide a better understanding of how the optical resolution affects the surface finish. The same parameters were used for both the simulation and the actual 3D printing. The simulation was able to capture the final print height and surface finish of both high-resolution CLIP printers. Importantly, the increase in lateral resolution from 30 μm resolution to 1.5 μm resolution in CLIP led to a significant improvement in surface finish.
[0302] High-resolution CLIP modeling: mass transport and printing speeds We describe the predicted flow field development during stage translation, and an estimate of the forces experienced between each printed layer. The inward flow field of uncured resin into the gap between the build platform and the window was modeled using lubrication theory. Although "squeezing flow lubrication" of power-law fluids has been studied previously, for completeness we provide a derivation of the full velocity profile. Note that we considered both Newtonian and non-Newtonian (power-law) fluids in determining the velocity flow profile and Stefan forces in the dead zone regime. It is worth mentioning that both of our resins exhibit shear thinning behavior (rheometer data in Figure 19) and are more accurately modeled as power-law fluids. Solving the analytical velocity flow profile for Newtonian fluids in the dead zone regime yields the following equation:
[0303]
number
[0304] During the ceremony,
[0305]
number
[0306] is the dimensionless velocity field in the r and z directions, U is the dimensionless build platform travel speed, r and z are the dimensionless coordinates of r and z, h is the height of the dead-380 zone, and ε is the ratio of the height of the dead zone to the radius of the printed part (or build 381 platform) (L). Solving for the non-Newtonian (power law fluid) velocity flow profile in the dead zone regime gives the following for the field:
[0307]
number
[0308] where n is the flow sweep rheology,
[0309]
number
[0310] where is the shear-thinning power-law exponent obtained from, and all remaining parameters are the same as those described in the Newtonian section. The velocity profile of the high-resolution CLIP of a Newtonian fluid based on (Eqs. (19-20)) is shown in Figure 14A(i), and the velocity profile of the high-resolution CLIP of a non-Newtonian power-law fluid based on (Eqs. (21-22)) is shown in Figure 14A(ii).
[0311] As discussed in the High Resolution 3D CLIP printing strategy section, a stepwise printing process (move-stop-expose) was employed to allow for resin replenishment followed by a stationary state before curing. Therefore, it is important to understand the normal forces experienced during the movement steps of each printing process. Based on the lubrication theory, the Stefan forces involved in each printing step were calculated. Here, we focus on the analytical expression and experimental validation of the Stefan forces.
[0312] The dimensional Stefan force for Newtonian and power law fluids is:
[0313]
number
[0314] where μ is the viscosity of a Newtonian fluid and μ0 is the zero shear viscosity coefficient of a non-Newtonian fluid (see Equation (16)). We verify the applicability of the lubrication theory on a high-resolution 3D CLIP printer system by directly measuring the experienced forces (Figure 14B). For printed part radii above 1.2 cm, a power-law dependence of the Stefan force with a 405 printed part radius is observed to be 3.5. For printed part radii below 1 cm, the 4-n power-law dependence predicted by lubrication theory no longer holds, and a power-law scaling of <1 is observed. This indicates that simple lubrication theory is not applicable for printed part radii below 1 cm, even though it is still several times the dead zone thickness (estimates of the dead zone thickness are approximately 3-5 μm in high-resolution CLIP modeling; see the Photopolymerization Gradient Study section).
[0315] It has been found that if the interlayer time is insufficient for the resin to reflow, several printing artifacts can be inferred, such as reduced print height, deformation of the printed pattern due to liquid flow upon incomplete photopolymerization, and surface roughness. For Newtonian fluids, the critical time scale for the resin to replenish the vacuum region at the deepest pixel location is h 2 / v, almost instantly, about 10 -6where ms, h is the dead zone thickness and v is the kinematic viscosity. However, for non-Newtonian resins, the critical time scale is determined by the strain% experienced by the resin, the evolution of the material properties during photopolymerization, and the stress relaxation time related to the printing diameter. We show the characterization of the resin stress relaxation time before (Figure 19) and during the printing process (Figure 20). To print structures with a diameter of 4-5 mm, the relaxation time measured by force sensor measurements is found to be around 300-400 ms, and it is observed that insufficient stress relaxation time (<200 ms) for the resin to relax and reflow results in a reduced printing resolution (Figure 21).
[0316] Demonstration of high-resolution CLIP printing To demonstrate the ability of our single-digit micron resolution CLIP-based 3D printer to print complex miniature 3D models with high surface smoothness at high speed, we explored multiple CAD designs and printed them in various materials. We explored the fabrication of 3D structures with minimum feature sizes on the micrometer length scale (Figures 15A-15C), a twisted lattice structure with a strut thickness of 100 μm with a height of 1.25 cm (Figure 15D), and a 3 mm tall micro Eiffel Tower structure with a minimum strut thickness of 50 μm (Figure 15C). We also explored structures with engineering and biomedical practical applications, such as a terraced microneedle design (Figure 15F), and a square block array (Figure 15G). All parts in Figures 15A-15G were printed using a resin formulation of TMPTA + 0.3 wt% BLS1326 + 2.5 wt% TPO, with a viscosity of 0.2 Pa·S. We also printed the lattice blocks with a viscous elastomer material (EPU-40) with a viscosity of 20 Pa·S (Figure 15H). As discussed in the High Resolution CLIP Modeling: Mass Transport and Printing Speed section, it is important to note that the corresponding printing parameters, especially the interlayer time, are very different for materials with different viscoelastic properties. The total printing time depends on the height (z) of the design and the viscoelastic properties of the selected material. For example, the parts printed with low viscosity resin, such as the microneedle design or the micro square block (Figures 15F and 15G), took 3 minutes to complete. Furthermore, the tallest print (2 cm) of the lattice twisted bar design printed with low viscosity resin (Figure 15D) took 90 minutes. In contrast, the short (2 mm) lattice block printed with viscoelastic elastomer resin (Figure 15H) also took 90 minutes to complete the print. The increased viscosity and stronger non-Newtonian fluid properties of EPU40 resin indicate that it experiences stronger Stefan adhesion forces and requires longer interlayer stress relaxation times during the printing process. This experimentally validates the simulation model with respect to the significant role of resin viscosity (Eqs. (23-24)) and the corresponding Stefan force and resin relaxation time in determining the printing speed. (Detailed discussion can be found in the Discussion section on printing speed and its role in the scalability of high-resolution 3D printing technology.)
[0317] Single-digit micron resolution and high-speed printing achieved with high-resolution CLIP 3D printing technology Among current high-resolution 3D printing technologies, it is generally difficult to achieve high printing resolution while maintaining high printing speed. Nanometer-scale or micron-scale patterning has been achieved by technologies such as electron beam induced deposition (EBID), electrohydrodynamic (EHD) jet printing, DIW, TPP, and microstereolithography (PμSL), but their printing speeds are slower compared to IJ, selective laser sintering (SLS&SLM), HARP, and CLIP printing technologies, resulting in reduced throughput and scalability. Volumetric 3D printing (V3D) can achieve faster printing speeds than TPP, but current geometries and resolutions are still limited. Compared to other high-resolution 3D printers, the single-digit micron resolution CLIP-based 3D printer described herein provides a technology platform with fast printing speeds and excellent resolution (Figure 16A).
[0318] To compare the practicality of the newly developed single-digit micron resolution CLIP-based 3D printer and a commercial TPP printer (NanoScribe Photonics GT, NanoScribe, Germany), we designed a twisted lattice bar structure (2 cm high, minimum strut thickness 100 μm) and compared the total printing time and quality. Since TPP is primarily used for nanometer-scale printing, but there are no other commercially available single-digit micron resolution 3D printers, we chose the NanoScribe Photonics GT as a baseline for comparison. The single-digit micron resolution CLIP-based 3D printer took 1.5 h to completely print a 2 cm high design, while the TPP took more than 48 h to print only 200 μm (Figure 16B). The ratio of printing times was approximately 10 5 The significantly shorter print times and single-digit micron resolution highlight CLIP's printing speed and ultimate scalability.
[0319] To characterize and understand the high-resolution printability of our single-digit micron resolution CLIP-based 3D printer, 2D patterns containing lines and holes were designed. Sample SEM images and geometric analysis of the printed patterns are shown in Figure 16C. The designed length scales of the tested line patterns range from 135 μm to 4.5 μm (90 pixels to 3 pixels). It is observed that the printing accuracy of the line patterns is optimal at length scales of 6 μm (4 pixels) and above, with the dimensional accuracy degrading below this value. As observed in the inset of Figure 16C, the printed lines are nicely resolved for both 30 μm and 15 μm structures, and the boundaries become less sharp for the 7.5 μm structures, supporting a larger standard deviation in the printed width. The analysis of μm / pixel also shows a degradation of the nominal resolution of our designed projection optics from 1.5 μm / pixel to 1.12 μm / pixel, indicating that the current limit for resolving line patterns is 6 μm (Figures 16C and 16D). The designed length scales of the tested hole patterns range from 45 μm to 18 μm (30 pixels to 12 pixels). The printing accuracy of the hole patterns is observed to be optimal at 22.5 μm and to degrade at smaller length scales, as shown qualitatively and quantitatively in Figures 16C and 16D, respectively.
[0320] Consideration Here, we present a CLIP-based 3D printer with single-digit micron resolution that can produce millimeter-scale 3D prints with single-digit micron resolution in just a few minutes. For single-digit micron resolution, we designed and implemented a custom projection lens system, including a tube lens and a microscope objective lens. Furthermore, because our high-magnification microscope objective lens has a very thin depth of field (tens of micrometers), we incorporate a focusing algorithm with an in-line beam splitter and an adjustable tube lens to enable visualization of the projected pattern with a CCD camera. Taking advantage of a digitally designed mesh pattern, we developed a contrast-based algorithm to search for the optimal focal plane position. After scanning a depth of 400 μm and analyzing the through-focus projection image stack, we identify the maximum sharpness position and confirm the performance with actual print results. This contrast-based focusing system overcomes the challenge of focusing from a high-magnification projection optics to a very thin depth of field and can be easily re-adjusted to the optimal focal plane reproducibly.
[0321] The resolution performance of a CLIP-based 3D printer with single-digit micron resolution was evaluated with line and hole patterns with dimensions ranging from 4.5 μm to 13.5 μm. While the designed optical resolution is 1.5 μm, the smallest features successfully printed and repeatedly printed were 6 μm lines and 18 μm holes. It is observed that the printer resolution and printing performance are strongly dependent on the optical resolution, resin formulation, printing strategy, design pattern, and finally cleaning strategy.
[0322] A simulation model was then developed with the goal of improving understanding of the CLIP printing process and providing guidance for developing optimal printing strategies for a variety of materials and designs. The model incorporates optical simulation of the projection optics via a Gaussian-approximated point spread function (PSF), prediction of momentum transport and flow fields using lubrication theory, and photopolymerization kinetics modeling to predict dead zone thickness, oxygen concentration gradient, and cure height. The model provides insights for improving the printing process, including employing a step-wise process (stop-move-expose) printing strategy to enable efficient resin reflow, and an estimation of the interlayer time required to eliminate resin convection-induced printing artifacts. The model also provides estimates of parameter values (light intensity, oxygen diffusion coefficient) required to maintain a stable dead zone for continuous printing. Finally, a 3D printing demonstration of a CLIP-based 3D printer with single-digit micron resolution, and the capability to print with viscoelastic materials, was presented.
[0323] Realization of Auto-Focusing and Its Role in High Resolution 3D Printing Technology Due to the shallow depth of focus of the high-magnification projection optical system of a single-digit micron resolution CLIP-based 3D printer and the micron-scale features we are trying to resolve, we demonstrate a robust focus adjustment mechanism to ensure print repeatability and monitor the occurrence of focus drift. Furthermore, it has been experimentally observed that the focal plane of the projection optics at the surface of the dead zone is strongly dependent on the window material, the resin refractive index, and the build platform reflectivity. Changing any material between the path of the projection optics requires an entirely new recalibration process. Currently, our method requires several steps of manual focusing, including (1) focusing the CCD camera onto the build platform, (2) focusing the projected pattern onto the build platform, and (3) acquiring a through-focus image stack to find the optimal z-position with the best focus performance. Although this method allowed us to achieve single-digit micron resolution, many of the procedures still require successive steps of manual focusing. Therefore, it is desirable for a single-digit micron resolution CLIP-based 3D printer to have the ability to autofocus. To achieve autofocus in our current system, we need to design and implement real-time feedback control of the camera imaging system along with a motorized translational Z-stage actuator for the microscope objective lens. As 3D printing technology advances into single-digit micron and nanometer length scales and automated alignment and multilayer 3D patterning become increasingly common, autofocusing systems have grown to be one of the key components for resolving small printed parts.
[0324] Printing speed and its role in scalability of high-resolution 3D printing technologies For a long time, despite its many advantages, 3D printing technology has been considered a non-scalable manufacturing process, limited to applications in low-volume production for customized use cases. This is mainly due to the limited resolution and slow printing speed of conventional 3D printers. The newly developed high-resolution and high-speed CLIP-based 3D printer presented here can solve the main challenges that have limited the scalability of additive manufacturing. 5 With print speeds up to 25-100 times faster than DLP and PμSL, and exceptional resolution capabilities, CLIP-based 3D printers with single-digit micron resolution could enable scalability in many modalities and ultimately elevate the additive manufacturing industry to a mainstream manufacturing process. These advantages could play an important role especially in biomedical and microelectronics applications where it is highly desirable to create millimeter-length scale 3D objects with micrometer patterning resolution within minutes.
[0325] The current dependency of printing speed and resolution can be further investigated. In the section on high-resolution CLIP modeling of optics, momentum, and mass transport, it is mentioned that a stepwise printing process was adopted. Therefore, the printing speed is determined by the interlayer time, which includes (1) the exposure time and dark time, which consist of (2) the stage movement time, and (3) the resin reflow time. Based on the dynamics simulation, the exposure time required for a z-resolution of 0.5 μm is about 1 ms, with a stage speed of 1 mm / s and acceleration of 1 mm / s. 2 The stage movement time at is measured to be about 50 ms, and the resin stress relaxation time during the printing process is measured to be in the range of 200-1000 ms depending on the printing diameter. It can be concluded that the major time-consuming step (also known as the rate-limiting step) is the resin stress relaxation time between each layer. Although a simple scaling relationship between printing resolution and printing speed cannot yet be obtained, a relationship between experimentally measured stress relaxation time and printing diameter has been established.
[0326] It is important to mention that the current printing speed can be further improved. Methods to reduce the interlayer time include (1) reducing or eliminating the vacuum pressure experienced in the deepest pixel regime, or (2) increasing the thickness of the dead zone. Based on equation (11), considerations for increasing the dead zone thickness include (3) increasing the oxygen diffusivity through the oxygen permeable window, or (4) increasing the oxygen concentration at the window surface. Besides overcoming the limitations of mass transport in the dead zone regime, there are other potential methods to develop a complete automated cycle of the 3D printing process. Streamlining cleaning, collection, in-line inspection, and storage into a complete cycle can reduce waiting time and speed up turnaround time. In-line inspection, especially paired with high-resolution 3D CLIP model development, can create machine learning algorithms that adjust printing parameters to achieve optimal printing accuracy and minimize printing defects.
[0327] Print Area and Its Impact on High Resolution 3D Printers One of the trade-offs of UV projection-based vat photopolymerization (e.g. DLP and CLIP) is that as the resolution increases, the total print area decreases linearly with pixel size. For example, for a light engine with a 2560 x 1600 pixel array (>4M pixels), the corresponding area can be reduced by applying reduction optics methods to a size of 5 mm 2 ~500cm 2 There are resolution printers that can modify the pixel size of the user's chosen resolution from a few μm to hundreds of μm to be in the range of 100 μm. One can implement an xy translation stage that moves the bat a certain distance to add multiple projections in one layer, similar to the stepping motion introduced in the field of lithography. While the overall printing area is larger while preserving the high resolution, the entire 605 manufacturing process is slowed down by either the speed of the translation stage or post-processing steps, which may introduce additional alignment errors. Recent advances in scan lens projection and the introduction of lens arrays in PμSL have significantly improved the build area and scalability.
[0328] CLIP-based 3D printer with single-digit micro-resolution achieves 1.5μm resolution The difference between the theoretical resolution in x, y, and z and the actual printing resolution is important to understand the limits of the system. Due to the Abbe diffraction limit, the theoretical minimum resolvable distance d for x and y resolution for our 5x objective lens system is (Figure 12):
[0329]
number
[0330] However, the minimum x,y resolution currently achievable is approximately 6 μm (Figure 16). Although our current model only considers the light transmission distance in Beer's law (Eq. (4)), the effects of resin formulation, reaction diffusion termination rate, and light scattering in the cured part are all believed to play important roles in the x,y printing resolution. The minimum radical diffusion length scale can be used as an estimate of the minimum x,y resolution. Previous studies have shown that the termination reaction coefficient and radical diffusion coefficient are viscosity dependent, and it can be estimated that the diffusion coefficient slows down based on the degree of conversion and increasing resin viscosity. From existing measurements, the estimated radical diffusion coefficient D~10 -9 m 2 / s (which increases by about 1–2 orders of magnitude after photocuring), and the diffusion length scale
[0331]
number
[0332] With this, we can estimate that the radical lifetime is t~10-20 ms and the minimum resolution is about 4.5-6.3 μm, which is supported by our current observations (Figure 16). Our current modeling does not consider reaction-diffusion termination kinetics and light scattering, and future studies on Fourier transform infrared spectroscopy (FTIR) and photorheology will help understand the resolution limits. Meanwhile, the z-resolution in our current system is only limited by the minimum stage travel distance of 0.1 μm. The prediction of the steady-state dead-zone thickness from our kinetic model after the first exposure is about 3 μm. The dead-zone thickness governs the boundary of the photopolymerization reaction, and the cure height and z-resolution in each layer are determined by the stage step size Δh after the first exposure.
[0333] supplement Contrast-based focusing algorithm for searching for the optimal focal plane An image sharpness assessment algorithm is developed to extract edge profiles in the entire field of view (FOV) to obtain a complete FOV sharpness analysis. A mesh design is selected for spatial resolution characterization (Figure 17A). Feature detection and centroid extraction are applied to find all triangular elements in the projected image (Figure 17B). Then, distances are calculated for each centroid, which are further characterized based on their distance to the image center in the range of 30% FOV, 65% FOV, and 85% FOV. A nearest neighbor calculation is performed for each centroid to obtain line pairs for edge profile extraction. The edge profile extraction line segments are colored by their respective FOV (Figure 17C). Finally, the average box of each line segment 10 pixels away from the center of the line segment is calculated and plotted (Figure 17D). This allows us to obtain the average edge profile of each edge. The obtained edge profile is therefore the edge spread function (ESF) required for the line spread function (LSF) and modulation transfer function (MTF) for image sharpness through focus.
[0334] An image analysis scheme for extracting 2D printing features from SEM images An image analysis scheme is applied to extract line widths from SEM images. Here we show sample line edge profiles extracted from a 15 μm wide line design obtained from SEM. SEM images are first imported into ImageJ and edge profiles of single lines or holes are extracted (Figures 18A-18D). The edge profiles are then subjected to a simple algorithm via peak and valley extraction. Critical dimensions (CDs) extracted from SEM are based on the 50% intensity threshold method and reported line widths are based on the x-coordinate extracted at the 50% intensity threshold of the outer edge.
[0335] Model parameters used in the transport and dynamics models The final solution of the coupled partial differential equations (PDEs) for both the unreacted monomer concentration and the oxygen concentration is obtained through the MATLAB® PDE solver, and the parameters used can be found in Figures 13A-13D. Some parameters are obtained directly through references, while others are estimated or directly measured. A brief description of the estimated parameters is provided below.
[0336] The first exposure time for the resin to harden on the build platform is experimentally about 3 seconds, depending on the design. This therefore gives a rough estimate of H, which should be about 10 μm, considering that 3 seconds is enough for the printed part to adhere to the build platform in order to proceed with the continuous printing.
[0337] A rough estimate from the intensity configured for a 30 μm lens is that the intensity I0 is approximately 40 mW / cm 2The values are obtained using an approximation of the known maximum intensity of our light engine for a 30μm printer, which is 1.1W / m2 for the 3.5μm lens. The current values are assumed to be linearly scaled by the associated Lightcrafter 0-255 control. Non-linearities of the LEDs themselves as well as temperature variations of the final light intensity are not taken into account. To get a rough estimate of the light intensity, the single pixel projected area reduction (30μm:30; 3.5μm:3.75; 1.5μm:1.5) was taken into account along with the f# difference (30μm:1.3; 3.5μm:12; 1.5μm:16). With the details listed, the first exposure with UV intensity 1 was 1.1W / m2 for the 3.5μm lens. 2 and 4 W / m for a 1.5 μm lens. 2 It was estimated that.
[0338] The [PI] concentration is derived from the known photoinitiator concentration of 2.5 wt % used in our system.
[0339] The oxygen concentration at the surface of the window is estimated to be three times that of the PDMS surface due to the fact that Teflon AF 2400 has a three times higher permeability to oxygen than PDMS. Further experimental validation of the modeling parameters is important for more accurate predictions. It is also noted that several important factors of oxygen transport are ignored here, including the solubility of oxygen in the TMPTA resin and the permeability of oxygen through the Teflon AF 2400 window. We use the model parameters obtained from known references as a reasonable framework for understanding the CLIP printing process and dead zone formation.
[0340] Therefore, we can calculate the critical dimensionless parameter Da1 = 7.34 x 10 7 , Da2 = 5.51 × 10 3 , α = 8.09 × 10 -7 , β = 7.8 × 10 -4 Also, taking the above parameters into account, a rough estimate of the steady-state dead-zone thickness can be obtained as approximately 3 μm.
[0341] Derivation of lubrication theory applied to CLIP technology - Newtonian fluid From the CLIP schematic in (Figure 4), the appropriate scaling
[0342]
number
[0343] By applying the above and deriving the lubrication theory after assuming ε<<1, we obtain the following simplified governing equations for Newtonian fluids:
[0344]
number
[0345]
number
[0346] During the ceremony,
[0347]
number
[0348] is the gradient operator in the xy plane, and the corresponding boundary condition for the velocity is
[0349]
number
[0350] and u z (h) is used to describe the velocity of the top plate. Therefore, from (Eq. (3)), the pressure is simply p (0) (x s t)
[0351] Equation (2) can then be integrated and boundary conditions applied.
[0352]
number
[0353] u s and integrate from 0 to h to determine p (equation (4)).
[0354]
number
[0355] Applying the boundary conditions we get:
[0356]
number
[0357] From (Equation (4)), we can see the following:
[0358]
number
[0359] Substituting into equation (6), we get the following:
[0360]
number
[0361] Assuming the gap thickness h is constant, we get:
[0362]
number
[0363] u z can be further expressed as follows:
[0364]
number
[0365] Therefore, the result is as follows:
[0366]
number
[0367] Assuming that at the surface of the plate, both velocity and height are maximum and normalized to 1, u z We can set (h)=1 and h=1, and obtain the velocity profiles in both x and z directions in the dead-zone regime as follows:
[0368]
number
[0369] First, assuming that the footprint of the part is instantaneously cylindrical and L is the radius of the cylinder, we can solve for the pressure field in the dead zone regime.
[0370]
number
[0371] Then, by integrating (equation (9)), we get:
[0372]
number
[0373] The pressure within a circular build area can be integrated to obtain the Stefan force.
[0374]
number
[0375] Derivation of lubrication theory applied to CLIP technology - Non-Newtonian fluids We assume a non-Newtonian power law fluid. Note that for Newtonian fluids, n=0.
[0376]
number
[0377] Using (Equation (16)) and (Equation (18)), u for z>h / 2 r The formula for can be obtained as follows:
[0378]
number
[0379] boundary condition u r (h)=0 and u r Solving this, we get the following:
[0380]
number
[0381] By symmetry, z <h / 2でのu r can be obtained as follows:
[0382]
number
[0383] Next, we solve for dP / dr using the continuity equation. From the continuity equation (equation (17)), we obtain:
[0384]
number
[0385] By integrating from 0 to h in z (equation (23)), we get:
[0386]
number
[0387]
number
[0388] To obtain the formula, u from h / 2 to h r Integrating, we get:
[0389]
number
[0390] Due to symmetry,
[0391]
number
[0392] can be expressed as follows:
[0393]
number
[0394]
number
[0395] and rewrite (equation (24)) as follows:
[0396]
number
[0397] After integrating (equation (27)) and applying the boundary conditions P(0) → 0 and P(0) = 0, we obtain the expression for pressure P as follows:
[0398]
Number
[0399] After obtaining the expression for P, then for z > h / 2, u r can be rewritten as follows.
[0400]
Number
[0401] Also, for z < h / 2, u r is as follows.
[0402]
Number
[0403] Then, for u at z > h / 2 z can be solved. Using the continuity equation, u z can be expressed as follows.
[0404]
Number
[0405] Subsequently, for simplicity, set as follows.
[0406]
Number
[0407] Proceeding to the solution of (Equation (23)), the boundary condition u z (b) = U can be applied.
[0408]
Number
[0409] Therefore, K1 is obtained as follows:
[0410]
number
[0411] Then, u for z>h / 2 as follows: z can be obtained.
[0412]
number
[0413] Similarly, the boundary condition u z (0)=0, z <h / 2でのu z can be obtained.
[0414]
number
[0415] Finally, the Stefan force for non-Newtonian fluids can be solved as follows:
[0416]
number
[0417] Rheological property evaluation of resins In this example, two resins are used for printing: TMPTA+0.3 wt% BLS1326+2.5 wt% TPO and EPU40 (Carbon Inc.). Rheological characterization was performed including flow sweeps of viscosity as a function of shear rate. A parallel plate device with a diameter of 25 mm was used, and approximately 250 μL of solution was used for each experiment.
[0418] All rheological properties were characterized using an ARES G2 (TA Instruments, New Castle, DE). Flow sweeps of TMPTA resins are performed at a temperature of 20°C with a shear rate sweep of 0.01-100 (1 / s) and a soak time of 120 seconds. Flow sweeps of EPU40 resins are performed at a temperature of 20°C with a shear rate sweep of 0.01-1000 (1 / s) and a soak time of 120 seconds. Shear thinning is observed for both TMPTA and EPU40 resins with different shear thinning coefficients of -0.87 and -0.72, indicating that both resins are non-Newtonian (Figures 19A-19B). Stress relaxation characterization of TMPTA resins is performed under 500% strain %, stress relaxation duration of 100 seconds, soak time of 60 seconds, and temperature of 20°C. Stress relaxation characterization of EPU40 resin is performed under 500% strain, stress relaxation duration of 100 s, soak time of 60 s, and temperature of 20° C. The longest relaxation time of TMPTA resin is characterized to be 112 ms, and the longest relaxation time of EPU40 resin is characterized to be 221 ms (FIG. 19C).
[0419] Resin stress relaxation time and printing radius The transient stress relaxation times required for resins (TMPTA+0.3wt% BLS1326+2.5wt% TPO) with printing diameters ranging from 0.4cm to 2.2cm are plotted in Figure 21A. The longest relaxation times are extracted by replotting Figure 21A on a semi-log plot to extract the average longest relaxation time within the transient stress relaxation process. It can be seen that the stress relaxation time increases with increasing diameter. There is an effect of resin shrinkage during curing, which has a potential impact on the stress relaxation. However, no observable relaxation occurs from Figures 20A-20B within 100ms during the exposure time.
[0420] Resin reflow and printing defects due to insufficient interlayer time Characterization of defects versus interlayer time was performed based on prediction of the time required for resin reflow in a 8.9 mm x 5.6 mm square area for resin (TMPTA + 0.3 wt% BLS1326 + 2.5 wt% TPO) with a viscosity of about 0.2 PaS and a shear rate of 0.1 (1 / s). The measured interlayer time showed that the defects disappeared in more than about 200 ms (Figure 20).
[0421] Although the foregoing invention has been described in some detail by way of illustration and example for purposes of clarity of understanding, it will be readily apparent to those skilled in the art that, in light of the teachings of this invention, certain changes and modifications can be made thereto without departing from the spirit or scope of the appended claims.
[0422] Thus, the above merely illustrates the principles of the present invention. It is understood that those skilled in the art can devise various arrangements that embody the principles of the present invention and are included within its spirit and scope, although not expressly described or shown herein. Furthermore, all examples and conditional language recited herein are intended primarily to aid the reader in understanding the principles of the present invention and the concepts contributed by the inventor to further advance the art, and should not be construed as being limited to such specifically recited examples and conditions. Furthermore, all statements herein that describe principles, aspects, and embodiments of the present invention, as well as specific examples thereof, are intended to encompass both structural and functional equivalents thereof. Additionally, such equivalents are intended to include both currently known equivalents and equivalents developed in the future, i.e., any elements developed to perform the same function, regardless of structure. Furthermore, nothing disclosed herein is intended to be dedicated to the public, regardless of whether such disclosure is expressly recited in the claims.
[0423] Therefore, the scope of the present invention is not intended to be limited to the exemplary embodiments shown and described herein. Rather, the scope and spirit of the present invention is embodied by the appended claims. In the claims, 35 U.S.C. 112(f) or 35 U.S.C. 112(6) is expressly defined as being invoked for a limitation in a claim only when the precise phrase "means for" or the precise phrase "step for" is recited at the beginning of such limitation in the claim, and if such precise phrase is not used in the limitation in the claim, 35 U.S.C. 112(f) or 35 U.S.C. 112(6) is not invoked.
[0424] CROSS-REFERENCE TO RELATED APPLICATIONS Pursuant to 35 U.S.C. §119(e), this application claims priority to the filing date of U.S. Provisional Patent Application No. 63 / 248,280, filed September 24, 2021, the entire disclosure of which is incorporated herein by reference.
Claims
1. A polymeric microneedle comprising a lattice microstructure having one or more lattice cell units.
2. The microneedle of claim 1 , comprising two or more repeating lattice cell units.
3. 3. The microneedle of claim 1 or 2, comprising a gradient of lattice cell units such that the density of the lattice cell units increases across the longitudinal axis of the microneedle.
4. The microneedle according to any one of claims 1 to 3, wherein the lattice cell units have a lattice shape selected from the group consisting of tetrahedron, kagome, rhombic, icosahedron, Voronoi, and triangle.
5. The microneedle according to any one of claims 1 to 4, comprising lattice cell units having a size of 200 μm to 500 μm.
6. The microneedle of any one of claims 1 to 5, wherein the lattice microstructure comprises a plurality of struts.
7. A tip portion having a solid structure; a body portion having a lattice structure; A base portion having a solid structure; The microneedle according to any one of claims 1 to 6, comprising:
8. The microneedle of any one of claims 1 to 7, wherein the lattice microstructure is formed from polyethylene glycol dimethacrylate (PEGDMA).
9. A patch, A backing layer; a plurality of polymeric microneedles in contact with the backing layer, each microneedle comprising a lattice microstructure having one or more lattice cell units; A patch comprising:
10. The patch of claim 9 , wherein one or more of the microneedles further comprises an active agent compound.
11. A method comprising applying a patch according to claim 9 or 10 to a skin surface of a subject.
12. 1. A method of making a polymeric microneedle comprising a lattice microstructure having one or more lattice cell units, comprising: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) displacing the build elevator away from the build surface; and c) irradiating the first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; d) repeating steps a) through c) in a manner sufficient to produce microneedles comprising a lattice microstructure; A method comprising:
13. The polymerizable composition comprises: an optical beam generator component comprising a light source, a tube lens, and one or more projection lenses; an optical projection monitoring component comprising a charge-coupled device (CCD); 13. The method of claim 12, wherein the imaging system is illuminated with a micro digital light projection system comprising:
14. The method according to claim 12 or 13, wherein the micro digital light projection system provides a grating microstructure resolution of 1.5 μm to 3.8 μm.
15. 1. A system for fabricating a polymeric microneedle comprising a lattice microstructure having one or more lattice cell units, comprising: a micro digital light projection system including a light beam generator component and a light projection monitoring component; a liquid interfacial polymerization module configured to generate said polymeric microneedles from a polymerizable composition positioned therebetween, said liquid interfacial polymerization module comprising a build elevator and a build surface; a processor, the processor comprising a memory operatively coupled to the processor; Equipped with The memory has instructions stored therein that, when executed by the processor, cause the processor to: a) irradiating a polymerizable composition positioned between a build elevator and a build surface to produce a polymerizable composition comprising a first polymerized region of the polymerizable composition in contact with the build elevator and a first unpolymerized region of the polymerizable composition in contact with the build surface; b) moving the build elevator away from the build surface; c) irradiating the first unpolymerized region of the polymerizable composition to produce a second polymerized region of the polymerizable composition in contact with the first polymerized region and a second unpolymerized region in contact with the build surface; d) repeating steps a) through c) in a manner sufficient to produce said polymeric microneedles comprising a lattice microstructure; system.
Citation Information
Patent Citations
Preparation method of exenatide microneedle
CN112641931A
Polymeric Microneedles and Rapid Additive Manufacturing of the Same
US20210031439A1
Microneedle having structure of three or more layers, and method for manufacturing same