Selective Silicon Deposition

The selective deposition of silicon-containing materials in patterned features within a single chamber addresses the challenge of maintaining structural integrity during etching in semiconductor processing, enhancing efficiency and reducing defects by using controlled plasma processes.

JP2024539605AActive Publication Date: 2024-10-29APPLIED MATERIALS INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024521127
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-13
Filing Date
2022-10-10
Publication Date
2024-10-29
Estimated Expiration
2042-10-10

AI Technical Summary

Technical Problem

Conventional semiconductor processing methods struggle to maintain structural integrity of small features due to etching processes that cause unwanted structures and defects, particularly when dealing with metal oxide photoresists, and often require multiple chambers, leading to contamination and inefficiency.

Method used

A method involving the selective deposition of silicon-containing materials in patterned features using a plasma process within a single chamber, which includes using silicon-containing and hydrogen-containing precursors at controlled power levels and pressures to protect patterned features during etching, ensuring minimal undercut and structural integrity.

Benefits of technology

This approach allows for precise deposition of silicon-containing materials that act as a protective layer, maintaining the integrity of patterned features during etching, reducing defects and enabling efficient, contamination-free processing in a single chamber.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024539605000001_ABST
    Figure 2024539605000001_ABST
Patent Text Reader

Abstract

An exemplary semiconductor processing method may include providing a silicon-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed within the processing region. The substrate may include one or more patterned features separated by exposed regions of the substrate. The method may include providing a hydrogen-containing precursor to a processing region of the semiconductor processing chamber. The method may include forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor. The forming of the plasma of the silicon-containing precursor and the hydrogen-containing precursor may be performed at a plasma power of about 1000 W or less. The method may include depositing a silicon-containing material in the one or more patterned features along the substrate. The silicon-containing material may be deposited in the patterned features at a ratio of at least 2:1 relative to deposition on exposed regions of the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0001] This application claims the benefit of U.S. patent application Ser. No. 17 / 500,664, filed Oct. 13, 2021, the entire contents of which are incorporated herein by reference.

[0002]

[0002] The present technology relates to semiconductor systems, processes, and equipment. More specifically, the present technology relates to processes and systems for selectively depositing silicon-containing materials. [Background technology]

[0003]

[0003] Integrated circuits are made possible by processes that form intricately patterned layers of material on a substrate surface. Forming patterned materials on a substrate requires controlled methods for forming and removing materials. As device sizes continue to shrink, features in integrated circuits may become smaller and aspect ratios of structures may become larger, and maintaining the dimensions of these structures during processing steps can be a challenge. Some processes involve etching of materials to form recessed features. However, this etching can result in the formation of unwanted structures in the recessed features and in the material near the recessed features. It has been difficult to develop materials that can avoid the creation of undesirable side effects.

[0004]

[0004] Accordingly, there is a need for improved systems and methods that can be used to manufacture high quality devices and structures. These and other needs are addressed by the present technique. Summary of the Invention

[0005]

[0005] An exemplary semiconductor processing method may include delivering a silicon-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed within the processing region of the semiconductor processing chamber. The substrate may include one or more patterned features separated by exposed regions of the substrate. The method may include delivering a hydrogen-containing precursor to the processing region of the semiconductor processing chamber. The method may include forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor. The forming of the plasma of the silicon-containing precursor and the hydrogen-containing precursor may be performed at a plasma source power of about 1000 W or less. The method may include depositing a silicon-containing material in the one or more patterned features along the substrate. The silicon-containing material may be deposited in the patterned features at a ratio of at least 2:1 relative to deposition on exposed regions of the substrate.

[0006] In some embodiments, the silicon-containing material may be or may include silicon tetrachloride (SiCl4). The one or more patterned features may be or may include tin oxide, silicon, silicon oxide, silicon oxynitride, or a silicon-containing antireflective layer (SiARC). The one or more patterned features may be on a carbon-containing layer. The one or more patterned features may protrude from the carbon-containing layer by about 5 nm or more. A temperature within the semiconductor processing chamber may be maintained at about 100° C. or less during deposition of the silicon-containing material into the one or more patterned features. A pressure within the semiconductor processing chamber may be maintained at about 50 mTorr or less during deposition of the silicon-containing material into the one or more patterned features. The method may include applying a bias power to a processing region of the semiconductor processing chamber during deposition of the silicon-containing material into the one or more metal-containing features. The bias power may be about 100 W or less.

[0007]

[0007] Some embodiments of the present technique may include a semiconductor processing method. The method may include delivering a silicon-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed within the processing region of the semiconductor processing chamber. The substrate may define one or more patterned features along the substrate. The method may include forming a plasma of the silicon-containing precursor. The forming of the plasma of the silicon-containing precursor may be performed at a plasma power of about 1000 W or less. The method may include depositing a discontinuous silicon-containing layer on the substrate. The silicon-containing layer may be selectively deposited into the one or more patterned features along the substrate.

[0008] In some embodiments, the temperature in the semiconductor processing chamber may be maintained at about 75° C. or less during deposition of the silicon-containing material. The pressure in the semiconductor processing chamber may be maintained at about 50 mTorr or less during deposition of the silicon-containing material. The method may include, after depositing the discontinuous silicon-containing layer on the substrate, etching one or more recesses in the carbon-containing layer deposited on the substrate using a plasma of an oxygen-containing precursor. The oxygen-containing precursor may be or may include diatomic oxygen. After etching, the one or more recesses may be characterized by an undercut of about 2 nm or less.

[0009] Some embodiments of the present technique may include a semiconductor processing method. The method may include providing a silicon-containing precursor and a hydrogen-containing precursor to a processing region of a semiconductor processing chamber. A substrate may be disposed in the processing region of the semiconductor processing chamber. The substrate may include a layer of a carbon-containing material. The substrate may include a patterned metal-containing photoresist overlying the layer of carbon-containing material. At least a portion of the layer of carbon-containing material may be exposed through the patterned metal-containing photoresist. The method may include forming a plasma of a silicon-containing precursor and a hydrogen-containing precursor. The forming of the plasma of a silicon-containing precursor and a hydrogen-containing precursor may be performed at a plasma power of about 1000 W or less. The method may include depositing a silicon-containing material on the patterned metal-containing photoresist along the substrate. The method may include providing an oxygen-containing precursor to a processing region of a semiconductor processing chamber. The method may include forming a plasma of the oxygen-containing precursor. The method may include etching one or more recesses using the plasma of the oxygen-containing precursor.

[0010] In some embodiments, the silicon-containing material is silicon tetrachloride (SiCl4). The method may include applying a bias power to a processing region of the semiconductor processing chamber during deposition of the silicon-containing material on the patterned metal-containing photoresist. The bias power may be about 100 W or less. The method may include reducing a pressure in the semiconductor processing chamber prior to delivering the oxygen-containing precursor to the processing region of the semiconductor processing chamber. Forming a plasma of the oxygen-containing precursor may be performed at a plasma power of about 300 W or more.

[0011]

[0011] The above techniques may provide numerous advantages over conventional methods and techniques. For example, the process may selectively deposit silicon-containing materials, such as metal-containing or silicon-containing features, onto non-carbon materials. Additionally, the process may reduce or limit removal of patterned features or undercuts when etching recesses in material beneath the patterned features. These and other embodiments, along with their many advantages and features, are described in more detail in conjunction with the following description and accompanying figures.

[0012] A further understanding of the nature and advantages of the disclosed technology may be realized by reference to the remaining portions of the specification and the drawings. [Brief description of the drawings]

[0013] [Figure 1] 1 is a schematic top view illustrating an exemplary processing system according to some embodiments of the present technique. [Diagram 2] 1 is a schematic cross-sectional view of an exemplary processing system according to some embodiments of the present technique; [Diagram 3] 1A-1D illustrate selected steps in a semiconductor processing method according to some embodiments of the present technique. [Figure 4] 1A-C are schematic diagrams illustrating exemplary cross-sectional structures including and formed from layers of material, according to some embodiments of the present technology. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014]

[0017] Some of the figures are included as schematic diagrams. It should be understood that the figures are for illustrative purposes and should not be considered to scale unless scale is specifically stated. Furthermore, as schematic diagrams, the figures are provided to aid in understanding and may not include all aspects or information as compared to realistic representations and may include exaggerated material for illustrative purposes.

[0015]

[0018] In the accompanying figures, similar components and / or features may be labeled with the same reference label. Additionally, various components of the same type may be distinguished by following the reference label with a letter that distinguishes the similar components. If only a first reference label is used herein, the description is applicable to any one of the similar components having the same first reference label, regardless of the letter.

[0016]

[0019] As device sizes continue to decrease, many layers of materials may decrease in thickness and width and size to scale the devices. As the size of features in semiconductor structures decreases, it may become more difficult to perform various processes such as lithography, deposition, and etching while maintaining structural integrity.

[0017]

[0020] Prior art has struggled to etch recesses between patterned features such as metal oxide photoresists. Metal oxide photoresists can be useful in many etching processes, but their films are formed to a much thinner thickness than traditional photoresist materials. Thus, an etching process to pattern a material that is two to three times thicker than the thickness of a metal oxide photoresist may cause the photoresist to be removed or altered, which may result in tapered etch features or incomplete processing. Etching recesses may undesirably etch the patterned feature itself, may undercut the feature, or may etch recesses with angled sidewalls. Any of these side effects during etching may result in undesirable structures. Additionally, prior art may require performing an etching process in one chamber, releasing the vacuum to transfer the structure, and performing a deposition process in another chamber. This transfer may result in undesirable contamination during processing. Thus, many prior art techniques have been limited in their ability to prevent structural defects in the final device.

[0018]

[0021] The present technique overcomes these problems by depositing a silicon-containing material on a metal oxide photoresist material or other silicon-containing material, such as selectively on the patterned features. The deposition can be performed in the same chamber as the etching process, which can limit wait times and improve structural integrity by limiting exposure to the atmosphere. By depositing the silicon-containing material on the patterned features as a protective layer, the present technique can ensure that the photoresist remains intact during processing. During the subsequent etching process, the silicon-containing material can protect the patterned material from being removed and act as a second mask to form recesses in the underlying material deposited on the substrate. By depositing the silicon-containing material, the present technique can prevent problems in any subsequent integration processes and / or defects in the final device.

[0019]

[0022] While the remaining disclosure will always identify specific deposition and etching processes utilizing the disclosed technology, it will be readily understood that the systems and methods are equally applicable to a variety of other processes, such as may be performed in the described chambers. Thus, the present technology should not be considered limited to use with only the described deposition or etching processes. Before describing the systems and methods or steps of an exemplary process sequence according to some embodiments of the present technology, the present disclosure will describe one possible system and chamber that may be used with the present technology. It should be understood that the present technology is not limited to the described equipment, and the described processes may be performed in any number of processing chambers and systems.

[0020]

[0023] Figure 1 illustrates a top view of one embodiment of a deposition, etch, bake, and / or cure chamber processing system 10 according to an embodiment. The tool or processing system 10 illustrated in Figure 1 may include multiple process chambers 24a-d, a transfer chamber 20, a service chamber 26, an integrated metrology chamber 28, and a pair of load lock chambers 16a-b. The process chambers may include any number of structures or components and any number or combination of process chambers.

[0021]

[0024] To transfer substrates between chambers, the transfer chamber 20 may include a robotic transport mechanism 22. The transport mechanism 22 may have a pair of substrate transport blades 22a each attached to a distal end of an extendable arm 22b. The blades 22a may be used to transport individual substrates into and out of the process chambers. In a process, one of the substrate transport blades, such as blade 22a of the transport mechanism 22, may retrieve a substrate W from one of the load lock chambers, such as chambers 16a-b, and transport the substrate W to a first stage of processing, such as a treatment process, in chambers 24a-d, as described below. The chambers may be included to perform individual or combinations of steps of the described techniques. For example, one or more chambers may be configured to perform a deposition or etching step, while one or more other chambers may be configured to perform a pre-treatment step and / or one or more post-treatment steps described. Any number of configurations capable of performing any number of additional manufacturing steps typically performed in semiconductor processing are encompassed by the present technology.

[0022]

[0025] If a chamber is occupied, the robot can wait until processing is complete, then remove the processed substrate from the chamber with one blade 22a and insert a new substrate with a second blade. Once the substrate has been processed, it can then be moved to the second stage of processing. For each move, the transport mechanism 22 can generally have one blade carrying the substrate and one empty blade to perform the substrate swap. The transport mechanism 22 can wait in each chamber until the swap can be completed.

[0023]

[0026] Once processing is completed in the process chambers, the transport mechanism 22 can move the substrate W from the last process chamber and transport the substrate W to a cassette in the load lock chamber 16a-b. From the load lock chamber 16a-b, the substrate can be moved into the factory interface 12. The factory interface 12 can be operable to transfer substrates between the pod loaders 14a-d and the load lock chambers 16a-b, which are generally in a clean environment at atmospheric pressure. The clean environment of the factory interface 12 can generally be obtained through an air filtration process, such as HEPA filtration. The factory interface 12 can also include a substrate orienter / aligner that can be used to properly align the substrate prior to processing. At least one substrate robot, such as robots 18a-b, can be positioned within the factory interface 12 to transport substrates between various locations / locations within the factory interface 12 and to other locations associated therewith. The robots 18a-b may be configured to move along a track system within the factory interface 12 from a first end to a second end of the factory interface 12.

[0024]

[0027] The processing system 10 may further include an integrated metrology chamber 28 for providing control signals that may provide adaptive control for any of the processes being performed in the processing chambers. The integrated metrology chamber 28 may include any of a variety of metrology devices for measuring various film properties such as thickness, roughness, composition, etc., and the metrology devices may further be capable of characterizing lattice parameters such as critical dimensions, sidewall angles, and feature heights under vacuum in an automated manner.

[0025]

[0028] Each of the processing chambers 24a-d may be configured to perform one or more process steps in the fabrication of a semiconductor structure, and any number and combination of processing chambers may be used in the multi-chamber processing system 10. For example, any of the processing chambers may be configured to perform a number of substrate processing steps, including cyclic layer deposition, atomic layer deposition, chemical vapor deposition, physical vapor deposition, and any number of deposition processes, including etching, pre-cleaning, pre-treatment, post-treatment, annealing, plasma treatment, degassing, orientation, and other steps including other substrate processes. Specific processes that may be performed in any of the chambers, or any combination of the chambers, may include metal deposition, surface cleaning and pre-treatment, thermal annealing such as rapid thermal processing, plasma treatment, and the like. As one of ordinary skill in the art would readily appreciate, any other process may similarly be performed in a particular chamber incorporated in the multi-chamber processing system 10, including any of the processes described below.

[0026]

[0029] 2 shows a schematic cross-sectional view of an exemplary processing chamber 100 suitable for patterning a layer of material disposed on a substrate 302 in the processing chamber 100. While the exemplary processing chamber 100 is suitable for performing a patterning process, it should be understood that aspects of the present technology may be performed in any number of chambers, and the substrate support according to the present technology may be included in an etch chamber, a deposition chamber, a treatment chamber, or any other processing chamber. The plasma processing chamber 100 may include a chamber body 105 that defines a chamber region 101 in which a substrate may be processed. The chamber body 105 may have sidewalls 112 and a bottom 118 coupled to a ground 126. The sidewalls 112 may have a liner 115 to protect the sidewalls 112 and extend the time between maintenance cycles of the plasma processing chamber 100. The dimensions of the chamber body 105 and associated components of the plasma processing chamber 100 are not limited and may generally be proportionally larger than the size of the substrate 302 to be processed therein. Examples of substrate sizes include 200 mm diameter, 250 mm diameter, 300 mm diameter, 450 mm diameter, among others, as well as display substrates, solar cell substrates, and the like.

[0027]

[0030] The chamber body 105 may support a chamber lid assembly 110 to enclose the chamber region 101. The chamber body 105 may be made of aluminum or other suitable material. A substrate access port 113 may be formed through the sidewall 112 of the chamber body 105 to facilitate transfer of the substrate 302 into and out of the plasma processing chamber 100. The access port 113 may be coupled to a transfer chamber and / or other chambers of a substrate processing system, as previously described. A pumping port 145 may be formed through the sidewall 112 of the chamber body 105 and connected to the chamber region 101. A pumping apparatus may be coupled to the chamber region 101 through the pumping port 145 to evacuate and control the pressure in the processing region. The pumping apparatus may include one or more pumps and a throttle valve.

[0028]

[0031] A gas panel 160 may be coupled to the chamber body 105 by gas lines 167 to supply process gases into the chamber region 101. The gas panel 160 may include one or more process gas sources 161, 162, 163, 164 and may additionally include inert, non-reactive, and reactive gases to be utilized for any number of processes. Examples of process gases that may be supplied by the gas panel 160 include, but are not limited to, methane, sulfur hexafluoride, silicon chloride, carbon tetrafluoride, hydrogen bromide, hydrocarbon-containing gases, including argon gas, chlorine, nitrogen, helium, or oxygen gas, as well as any number of additional materials. Additionally, the process gas may include nitrogen, chlorine, fluorine, oxygen, and hydrogen-containing gases such as BCl3, C2F4, C4F8, C4F6, CHF3, CH2F2, CH3F, NF3, NH3, CO2, SO2, CO, N2, NO2, N2O, and H2, among any number of additional precursors.

[0029]

[0032] The valves 166 can control the flow of process gas from the sources 161, 162, 163, 164 from the gas panel 160 and can be managed by the controller 165. The flow of gas supplied to the chamber body 105 from the gas panel 160 can include a combination of gas from one or more sources. The lid assembly 110 can include a nozzle 114. The nozzle 114 can be one or more ports for introducing process gas from the sources 161, 162, 164, 163 of the gas panel 160 into the chamber region 101. After the process gas is introduced into the plasma processing chamber 100, a voltage can be applied to the gas to form a plasma. An antenna 148, such as one or more inductive coils, can be provided adjacent the plasma processing chamber 100. An antenna power supply 142 can provide power to the antenna 148 through a matching circuit 141 to inductively couple energy, such as RF energy, to the process gas to maintain a plasma formed from the process gas in the chamber region 101 of the plasma processing chamber 100. Instead of, or in addition to, the antenna power supply 142, a process electrode below and / or above the substrate 302 can be used to capacitively couple RF power to the process gases to maintain a plasma in the chamber region 101. The operation of the power supply 142 can be controlled by a controller, such as controller 165, which also controls the operation of the other components of the plasma processing chamber 100.

[0030]

[0033] A substrate support pedestal 135 may be disposed in the chamber region 101 to support the substrate 302 during processing. The substrate support pedestal 135 may include an electrostatic chuck 122 for holding the substrate 302 during processing. The electrostatic chuck ("ESC") 122 may hold the substrate 302 to the substrate support pedestal 135 using electrostatic attraction. The ESC 122 may be powered by an RF power supply 125 integrated with a matching network 124. The ESC 122 may include an electrode 121 embedded in a dielectric. The electrode 121 may be coupled to the RF power supply 125 and may provide a bias that attracts plasma ions formed by process gases in the chamber region 101 to the ESC 122 and the substrate 302 seated on the pedestal. The RF power supply 125 is cycled on and off or pulsed during processing of the substrate 302. The ESC 122 may include an isolator 128 to prevent the plasma from being attracted to the sidewalls of the ESC 122, thereby extending the maintenance life of the ESC 122. Additionally, the substrate support pedestal 135 may include a cathode liner 136 to protect the sidewalls of the substrate support pedestal 135 from the plasma gases, thereby extending the maintenance interval of the plasma processing chamber 100.

[0031]

[0034] The electrode 121 may be coupled to a power supply 150. The power supply 150 may provide a chucking voltage of about 200 volts to about 2000 volts to the electrode 121. The power supply 150 may also include a system controller for controlling the operation of the electrode 121 by directing a direct current to the electrode 121 for chucking and dechucking the substrate 302. The ESC 122 may include a heater disposed in a pedestal and connected to a power supply for heating the substrate, and the cooling base 129 supporting the ESC 122 may include conduits for circulating a heat transfer fluid to maintain the temperature of the ESC 122 and the substrate 302 disposed thereon. The ESC 122 may be configured to operate in a temperature range as required by the thermal budget of the devices fabricated on the substrate 302. For example, the ESC 122 may be configured to maintain the substrate 302 at a temperature of about −150° C. or less to about 500° C. or more, depending on the process being performed.

[0032]

[0035] A cooling base 129 may be provided to assist in controlling the temperature of the substrate 302. To mitigate process drift and time, the temperature of the substrate 302 may be maintained substantially constant by the cooling base 129 throughout the time the substrate 302 is in the cleaning chamber. In some embodiments, the temperature of the substrate 302 may be maintained at a temperature of about -150°C to about 500°C throughout the subsequent cleaning process, although any temperature may be utilized. A cover ring 130 may be disposed on the ESC 122 and along the periphery of the substrate support pedestal 135. The cover ring 130 may be configured to confine the etching gas to a desired portion of the exposed upper surface of the substrate 302 while shielding the upper surface of the substrate support pedestal 135 from the plasma environment inside the plasma processing chamber 100. Lift pins may selectively translate through the substrate support pedestal 135 to lift the substrate 302 above the substrate support pedestal 135 to facilitate access to the substrate 302 by a transfer robot or other suitable transfer mechanism, as previously described.

[0033]

[0036] The controller 165 may be utilized to control process sequences, regulate gas flow from the gas panel 160 into the plasma processing chamber 100, and control other process parameters. The software routines, when executed by the CPU, transform the CPU into a special purpose computer, such as a controller, that can control the plasma processing chamber 100 such that processes are performed in accordance with the present disclosure. The software routines may also be stored and / or executed by a second controller that may be associated with the plasma processing chamber 100.

[0034]

[0037] The processing chambers described above can be used in the method according to the embodiment of the present technology. FIG. 3 shows a method 300 of semiconductor processing in which the steps can be performed in one or more chambers 100, for example, integrated in a multi-chamber processing system 10, as described above. Any other chamber capable of performing one or more steps of any of the described methods or processes can also be utilized. The method 300 can include one or more steps before the start of the described method steps, including front-end processing, deposition, etching, polishing, cleaning, or any other steps that can be performed before the described steps. The method can include a number of optional steps as shown in the figure, which may or may not be specifically related to the method according to the present technology. For example, in order to provide a broader scope of semiconductor processing, many steps are described, but are not critical to the present technology, or can be performed by alternative methodologies, as described further below.

[0035]

[0038] Method 300 may include multiple steps that may be performed in multiple variations, including starting at different steps of processing. Method 300 may generally include a deposition step that may be performed in a chamber in which an etching process may be performed. In many cases, deposition may be performed prior to etching. Thus, while method 300 is described in a particular order, it should be understood that the method may be performed in multiple different variations in accordance with embodiments of the present technology. Method 300 may be described in the steps shown generally in Figures 4A-4C, which illustrations will be described in conjunction with the steps of method 300. It should be understood that structure 400 in Figures 4A-4C is shown only in partial schematic view, and substrate 405 may include any number of structural portions having the illustrated aspects, as well as alternative structural aspects that may also benefit from the steps of the present technology.

[0036]

[0039] The substrate 405 may be disposed in a processing region of the semiconductor processing chamber 100 or in any other processing chamber in which the steps of the present technology may be performed. The substrate 405 may have a substantially flat or textured surface in embodiments. The substrate 405 may be a material such as crystalline silicon, silicon oxide, strained silicon, silicon germanium, silicon oxycarbide, silicon oxycarbonitride, silicon carbonitride, doped or undoped polysilicon, doped or undoped silicon wafer, patterned or unpatterned wafer, silicon-on-insulator, carbon doped silicon oxide, silicon nitride, doped silicon, germanium, gallium arsenide, or sapphire. The substrate 405 may have a variety of dimensions, such as 200 mm or 300 mm diameter wafers, as well as rectangular or square panels. As shown in FIG. 4A, the substrate 405 may include one or more patterned features 415, such as patterned metal-containing photoresist, separated by exposed areas of the substrate 405. That is, the patterned material may be a patterned metal-containing photoresist. The patterned feature 415 may be or include any number of metals. For example, the patterned feature 415 may include a metal oxide, or any material composed of a metal and oxygen. In an embodiment, the patterned feature 415 may be or include tin oxide, silicon, silicon oxide, silicon oxynitride, or silicon-containing antireflective layer (SiARC), or tungsten. The remaining disclosure will always refer to metal oxide photoresist, but it should be understood that the technology may encompass additional materials on which selective deposition may occur. It should therefore be understood that features 415 are not limited to metal oxide photoresist, but may be or include silicon oxide (SiO), silicon nitride (SiN), silicon carbide (SiC), tin oxide (SnO), silicon oxycarbide (SiOC), silicon oxycarbonitride (SiOCN), and crystalline silicon in embodiments encompassed by the present technology.

[0037]

[0040] In an embodiment, the patterned features 415 may be on a carbon-containing layer 410 deposited on the substrate 405. The carbon-containing layer 410 may be, for example, a spin-on carbon hard mask, chemical vapor deposited carbon, or plasma vapor deposited carbon. The carbon-containing layer 410 may be characterized by a thickness of about 20 nm or more, about 25 nm or more, about 30 nm or more, or more. Similarly, the carbon-containing layer 410 may be characterized by a thickness of about 40 nm or less, about 35 nm or less, about 30 nm or less, or less. The one or more patterned features 415 may protrude from the carbon-containing layer 410 by about 5 nm or more, e.g., about 6 nm or more, about 7 nm or more, about 8 nm or more, about 9 nm or more, about 10 nm or more, or more. In an embodiment, at least a portion of the carbon-containing layer 410 layer may be exposed through the patterned features 415, such as a patterned metal-containing photoresist.

[0038]

[0041] 4A-4B, in step 305, the method 300 may include providing a silicon-containing precursor to a processing region of a semiconductor processing chamber. The silicon-containing precursor that may be used in step 305 may be or may include any number of silicon-containing precursors. For example, the silicon-containing precursor may be or may include silane (SiH4), disilane (Si2H6), silicon tetrachloride (SiCl4), or any other precursor capable of forming, for example, silicon oxide (SiO), silicon nitride (SiN), or silicon carbide (SiC) materials. The silicon-containing precursor selected may affect the deposition rate or film properties. The flow rate of the silicon-containing precursor may be about 5 sccm or more, such as about 10 sccm or more, about 15 sccm or more, or more. The flow rate of the silicon-containing precursor may be adjusted depending on the desired growth rate.

[0039]

[0042] In step 310, the method 300 can include providing a hydrogen-containing precursor to a processing region of a semiconductor processing chamber. The hydrogen-containing precursor that can be used in step 310 can be or can include any number of hydrogen-containing precursors, such as, but not limited to, diatomic hydrogen. The flow rate of the hydrogen-containing precursor can be about 40 sccm or more, such as about 50 sccm or more, about 60 sccm or more, or more.

[0040]

[0043] The flow rates of the silicon-containing precursor and the hydrogen-containing precursor may be related. For example, the flow rate of the hydrogen-containing precursor may be maintained at a flow rate ratio of about 1:1 or more to the silicon-containing precursor during deposition of the silicon-containing material 420, as described below. At higher flow rate ratios, the selectivity of the silicon-containing material 420 may decrease, resulting in decreased deposition, as described below. At higher flow rate ratios, more silicon-containing precursor is delivered to the semiconductor processing chamber, and therefore more silicon-containing material 420 is available for deposition. Additionally, depending on the silicon-containing precursor used, the deposited silicon-containing material 420 may have a lower atomic % of silicon and may be richer in other components of the silicon-containing precursor, which may not be selective to the patterned features 415. Thus, the flow rate ratio may be about 2:1 or more, about 3:1 or more, about 4:1 or more, about 5:1 or more, about 6:1 or more, about 7:1 or more, about 8:1 or more, about 9:1 or more, about 10:1 or more, or more.

[0041]

[0044] In step 315, the method 300 may include forming a plasma. The plasma may be formed from a silicon-containing precursor and / or a hydrogen-containing precursor. Forming the plasma of the silicon-containing precursor and / or the hydrogen-containing precursor may be performed at a plasma power of about 3000 W or less. At higher plasma powers, it may be difficult to maintain the line width even during the deposition process due to the energy of the radical effluent and the etchant capacity. Furthermore, the silicon-containing material 420 deposited on the patterned feature 415 may grow so quickly that the resulting material on the patterned feature 415 may be prone to topping. Furthermore, high plasma powers may result in shorter step times and may make it difficult to control the amount of silicon-containing material 420 deposited. Thus, the plasma power can be maintained at about 2000 W or less, about 1000 W or less, about 900 W or less, about 800 W or less, about 700 W or less, about 600 W or less, about 500 W or less, about 400 W or less, about 300 W or less, about 200 W or less, or less.

[0042]

[0045] At step 320, the method 300 may include depositing a silicon-containing material 420 in one or more patterned features 415. The silicon-containing material 420 may be selectively deposited in the patterned material and not in the underlying carbon-containing layer 410, which may be based on hydrogen interactions, as described further below. However, it is contemplated that some silicon-containing material 420 may deposit in the carbon-containing layer 410. The silicon-containing material 420 may be deposited in the patterned features 415 in a ratio of at least 2:1 relative to deposition on exposed areas of the substrate 405, and may be deposited in the patterned features in a ratio of about 5:1 or more, about 10:1 or more, about 15:1 or more, about 20:1 or more, or more.

[0043]

[0046] In step 320, the method 200 may include applying a bias power to the plasma while depositing the silicon-containing material 420 on one or more patterned features 415. The application of the bias power may be used to increase the selectivity of the deposition of the silicon-containing material 420 on the patterned features 415 instead of on exposed areas of the substrate 405, such as the carbon-containing layer 410. With the bias applied, the plasma effluent of the hydrogen-containing precursor may react and interact more readily with the carbon-containing layer 410, such that not enough hydrogen is available at those locations to react with the silicon-containing precursor, and silicon may combine with the carbon. Without the bias power applied, the silicon-containing material 420 may deposit more conformally with less selectivity to the patterned features 415. However, as the bias power increases, the deposition rate of the silicon-containing material 420 may decrease, and the already deposited silicon-containing material 420 or the patterned features 415 may be etched during step 320. Thus, bias power can be applied at about 90 W or less, about 80 W or less, about 70 W or less, about 60 W or less, about 50 W or less, about 40 W or less, about 30 W or less, about 20 W or less, about 10 W or less, or less.

[0044]

[0047] The bias power may be applied continuously or pulsed according to some embodiments of the present technology. In embodiments where the bias power is pulsed, the pulsing frequency may be about 2000Hz or less, and may be pulsed at a frequency of about 1500Hz or less, about 1000Hz or less, or about 500Hz or less. Furthermore, the duty cycle at the pulsing frequency may be maintained at about 50% or less, about 40% or less, about 30% or less, about 20% or less, about 10% or less, or less. This can further reduce the effective bias power applied during the deposition process. By using a higher flow rate of the hydrogen-containing precursor than the silicon-containing precursor, a much lower bias power can be used to control the formation on the carbon material, further limiting the etching of the material deposited on the photoresist.

[0045]

[0048] During deposition of the silicon-containing material 420 into one or more patterned features 415, the temperature within the semiconductor processing chamber, such as the substrate support temperature or the substrate temperature, may be maintained at about 100° C. or less. At higher temperatures, the deposition rate may decrease and the silicon-containing material 420 may deposit on the sidewalls of the patterned features 415. At higher temperatures, the silicon-containing material 420 may become more fluid and may not be able to be deposited directly on top of the patterned features 415. Thus, the temperature may be maintained at about 90° C. or less, about 80° C. or less, about 70° C. or less, about 60° C. or less, about 50° C. or less, or less.

[0046]

[0049] The pressure in the semiconductor processing chamber 100 may be maintained at about 50 mTorr or less during deposition of the silicon-containing material 420 into the one or more patterned features 415. At higher pressures, the deposition may be more conformal and the silicon-containing material 420 may not be selectively deposited onto the patterned material. Thus, in some embodiments, the pressure may be maintained at about 40 mTorr or less, about 30 mTorr or less, about 20 mTorr or less, about 10 mTorr or less, or less.

[0047]

[0050] Referring to FIG. 4C, in optional step 325, the method 300 may include an etching process. The etching process of optional step 325 may be performed in the same chamber as step 320 or in a separate chamber. Step 325 may include etching one or more recesses in the carbon-containing layer 410 deposited on the substrate 405. More specifically, the etching process may include providing an oxygen-containing precursor, such as diatomic oxygen, to a processing region of the semiconductor processing chamber. After providing the oxygen-containing precursor, the process may include forming a plasma of the oxygen-containing precursor. Finally, the process may include etching the exposed regions of the carbon-containing layer 410 with the plasma of the oxygen-containing precursor to form recesses in the silicon-containing material 420. The etching process may cause reduction or removal of the mask layer due to collisions or other interactions, but some or all of the silicon-containing material and photoresist may remain during etching.

[0048]

[0051] During the etching process of this embodiment, the patterned features may remain intact and the etching may result in vertical recesses due to the deposited silicon-containing material 420 described above. This allows the structure 400 to have improved structural integrity for use in subsequent steps or in a final product. After etching, the recesses may be characterized by an undercut of about 3 nm or less.

[0049]

[0052] The etching process may be performed at a higher process power compared to the deposition. For example, both the source power and the bias power may be increased between the deposition and etching steps in the processing chamber. For example, the source power may be increased from the power during deposition to a second power of about 300 W or more, about 350 W or more, about 400 W or more, or more. Similarly, the bias power may be increased from a first bias power during deposition to a second bias power of about 50 W or more, about 60 W or more, about 70 W or more, about 80 W or more, about 90 W or more, about 100 W or more, or more. Furthermore, the duty cycle applied to the bias pulsing frequency may be increased from a first duty cycle during deposition to a second duty cycle of about 20% or more, about 30% or more, about 40% or more, about 50% or more, or more. As the bias decreases, the etching may result in a larger undercut due to the increased isotropy of the plasma. However, by increasing the power between deposition and etching, an improved etch profile may be obtained.

[0050]

[0053] Conventional embodiments that do not deposit a silicon-containing material prior to the etching process may result in a final structure that is reduced in thickness or completely removed from the remaining patterned features and / or undercutting of the etched recesses. Embodiments of the present disclosure may avoid or reduce these problems, as discussed above. With the deposited silicon-containing material 420 described above, the present disclosure may reduce the amount of patterned features 415 consumed during step 325 and may allow bias power to be maintained during step 325, which may result in straighter sidewalls in the recesses.

[0051]

[0054] In the foregoing specification, for purposes of explanation, numerous details have been set forth in order to provide an understanding of various embodiments of the present technology. However, it will be apparent to one of ordinary skill in the art that particular embodiments may be practiced without some of these details or with additional details.

[0052]

[0055] Although several embodiments have been disclosed, it will be recognized by those skilled in the art that various modifications, alternative structures, and equivalents may be used without departing from the spirit of the embodiments. Moreover, in order to avoid unnecessarily obscuring the present technology, some well-known processes and elements have not been described. Thus, the above specification should not be construed as limiting the scope of the present technology.

[0053]

[0056] Where a range of values ​​is provided, it is understood that each intervening value between the upper and lower limit of that range, to the smallest fraction of the unit of the lower limit, is also specifically disclosed, unless the context clearly dictates otherwise. Any narrower range between any stated value or unstated intervening value in a stated range and any other stated or intervening value in that stated range is included. The upper and lower limits of these smaller ranges may be independently included or excluded, and each range in which the smaller range includes one or both limits of the range, or neither limit of the range, is also included within the technology, subject to any specifically excluded limit in the stated range. When one or both limits are included in a stated range, ranges excluding one or both of those included limits are also included.

[0054]

[0057] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural references unless the context clearly dictates otherwise. Thus, for example, reference to a "silicon-containing precursor" includes a plurality of such precursors, reference to a "silicon-containing material" includes a reference to one or more materials and equivalents thereof known to those skilled in the art, and so forth.

[0055]

[0058] Additionally, as used in this specification and the claims that follow, the terms "comprise," "comprising," "contain," "containing," "include," and "including" specify the presence of stated features, integers, components, or steps, but do not exclude the presence or addition of one or more other features, integers, components, steps, operations, or groups.

Claims

1. 1. A semiconductor processing method comprising: providing a silicon-containing precursor to a processing region of a semiconductor processing chamber, the substrate being disposed within the processing region of the semiconductor processing chamber, the substrate including one or more patterned features separated by exposed regions of the substrate; providing a hydrogen-containing precursor to a processing region of the semiconductor processing chamber; forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor, the plasma being performed at a plasma power of about 1000 W or less; depositing a silicon-containing material into the one or more patterned features, the silicon-containing material being deposited into the patterned features at a ratio of at least 2:1 relative to deposition onto exposed areas of the substrate; The method includes:

2. The silicon-containing material is silicon tetrachloride (SiCl 4 2. The semiconductor processing method of claim 1 .

3. 10. The semiconductor processing method of claim 1, wherein the one or more patterned features comprise tin oxide, silicon, silicon oxide, silicon oxynitride, or a silicon-containing antireflective layer (SiARC).

4. The semiconductor processing method of claim 1 , wherein the one or more patterned features are overlying a carbon-containing layer.

5. 5. The semiconductor processing method of claim 4, wherein the one or more patterned features protrude from the carbon-containing layer by about 5 nm or more.

6. 10. The semiconductor processing method of claim 1, wherein a temperature within the semiconductor processing chamber is maintained at or below about 100° C. while depositing the silicon-containing material in the one or more patterned features.

7. 10. The semiconductor processing method of claim 1, wherein a pressure in the semiconductor processing chamber is maintained at or below about 50 mTorr while depositing the silicon-containing material in the one or more patterned features.

8. 10. The semiconductor processing method of claim 1, further comprising applying a bias power to a processing region of the semiconductor processing chamber while depositing the silicon-containing material into one or more metal-containing features, wherein the bias power is about 100 W or less.

9. providing an oxygen-containing precursor to a processing region of the semiconductor processing chamber; forming a plasma of the oxygen-containing precursor; etching a portion of the silicon-containing material and the exposed area of ​​the substrate with a plasma of the oxygen-containing precursor to form a recess in the silicon-containing material, wherein after the etching, the recess is characterized by an undercut of about 3 nm or less. The semiconductor processing method of claim 1 further comprising:

10. 10. The semiconductor processing method of claim 9, wherein forming the plasma of the oxygen-containing precursor is performed at a plasma power of about 200 W or greater.

11. 1. A semiconductor processing method comprising: providing a silicon-containing precursor to a processing region of a semiconductor processing chamber, the substrate being disposed within the processing region of the semiconductor processing chamber, the substrate defining one or more patterned features along the substrate; forming a plasma of the silicon-containing precursor, the plasma being performed at a plasma power of about 1000 W or less; depositing a discontinuous silicon-containing layer on the substrate, the silicon-containing layer being selectively deposited into the one or more patterned features along the substrate; The method includes:

12. maintaining a temperature within the semiconductor processing chamber at or below about 75° C. during deposition of the silicon-containing material; 12. The semiconductor processing method of claim 11, wherein a pressure in the semiconductor processing chamber is maintained at or below about 50 mTorr while depositing the silicon-containing material.

13. 12. The semiconductor processing method of claim 11, further comprising, after depositing the discontinuous silicon-containing layer on the substrate, etching one or more recesses in a carbon-containing layer deposited on the substrate using a plasma of an oxygen-containing precursor.

14. The semiconductor processing method of claim 13 , wherein the oxygen-containing precursor comprises diatomic oxygen.

15. 14. The semiconductor processing method of claim 13, wherein after said etching, said one or more recesses are characterized by an undercut of about 2 nm or less.

16. 1. A semiconductor processing method comprising: providing a silicon-containing precursor and a hydrogen-containing precursor to a processing region of a semiconductor processing chamber, wherein a substrate is disposed in the processing region of the semiconductor processing chamber, the substrate comprising a layer of carbon-containing material, the substrate comprising a patterned metal-containing photoresist overlying the layer of carbon-containing material, at least a portion of the layer of carbon-containing material being exposed through the patterned metal-containing photoresist; forming a plasma of the silicon-containing precursor and the hydrogen-containing precursor, the plasma being performed at a plasma power of about 1000 W or less; depositing a silicon-containing material onto the patterned metal-containing photoresist along the substrate; providing an oxygen-containing precursor to a processing region of the semiconductor processing chamber; forming a plasma of the oxygen-containing precursor; Etching one or more recesses using a plasma of the oxygen-containing precursor. The method includes:

17. The silicon-containing material is silicon tetrachloride (SiCl 4 20. The semiconductor processing method of claim 16, wherein

18. 20. The semiconductor processing method of claim 16, further comprising applying a bias power to a processing region of the semiconductor processing chamber while depositing the silicon-containing material on the patterned metal-containing photoresist, wherein the bias power is about 100 W or less.

19. 20. The semiconductor processing method of claim 16, further comprising reducing the pressure in the semiconductor processing chamber prior to delivering the oxygen-containing precursor to a processing region of the semiconductor processing chamber.

20. 20. The semiconductor processing method of claim 16, wherein forming the plasma of the oxygen-containing precursor is performed at a plasma power of about 300 W or greater.

Citation Information

Patent Citations

  • Halogen-free amorphous carbon mask etching having high selectivity to photoresist

    JP2008263186A

  • Resist composition

    JP2019517025A

  • Method for depositing insulating material in vias

    JP2020531695A

  • Method for forming an EUV patternable hard mask

    JP2021523403A

  • Methods of patterning small features

    US20210183656A1