Method for manufacturing three-dimensional metal bodies having an open-cell metal sponge structure

JP2024540519APending Publication Date: 2024-10-31GRILLO WERKE AG
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024529503
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-16
Filing Date
2022-11-11
Publication Date
2024-10-31

AI Technical Summary

Benefits of technology

【0023】 更なる実施形態では、本発明の目的は、本発明の製造方法によって得られた開放セル孔によるスポンジ構造を有する金属成形部材によって達成される。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024540519000001_ABST
    Figure 2024540519000001_ABST
Patent Text Reader

Abstract

The present invention relates to a method for producing open cell porosity metal bodies from zinc, tin, lead, indium, aluminum, magnesium or bismuth, or an alloy of any of these metals, and to the use of said metal bodies thus obtained as anodes.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a metal shaped part having an open cell pore structure made of zinc, tin, lead, indium, aluminum, magnesium, bismuth or a suitable alloy of any of these metals, to the metal shaped part produced thereby and to its use, in particular as an anode in batteries, rechargeable batteries and all-solid-state batteries. [Background technology]

[0002] Batteries, especially rechargeable batteries, play an important role in the so-called energy cycle. Applications of rechargeable batteries are being considered both as stationary storage batteries and as power network stabilization storage systems (energy storage systems). Energy storage systems are also used in the domestic sector, especially for storing solar energy, but increasingly also in the vehicle and consumer sectors.

[0003] Rechargeable batteries using porous metal molded members have great potential as replacements for nickel-metal hydride secondary batteries, lead-acid batteries, and even lithium-ion rechargeable batteries, the most widespread and most commonly known being the lithium-ion rechargeable battery in the consumer field and the lead-acid battery in the vehicle field.

[0004] However, rechargeable batteries (or secondary batteries) that contain lithium in particular are increasingly being criticized, as lithium mining is often associated with high levels of environmental pollution. Furthermore, rare earth elements such as cerium and lanthanum are used in nickel-metal hydride secondary batteries, although these are limited resources.

[0005] In recent years, zinc has become increasingly important as an alternative material for primary and secondary batteries. For example, zinc-based sponge-structured anodes have a significant density advantage over lead anodes. When zinc is used as a battery material, there is no need to worry about raw material shortages, even in mass production. Furthermore, since it does not use rare metals or rare earth elements and is recyclable, the use of zinc is highly sustainable. Furthermore, zinc electrodes have great potential because they can be used in the field of primary batteries.

[0006] Zinc batteries do not have the same safety concerns (risks from flammable components) as, for example, lithium-ion secondary batteries. Zinc batteries most commonly contain aqueous electrolytes and are therefore non-flammable.

[0007] For batteries (such as Ni / Zn batteries, Zn / air batteries, Zn / Ag batteries, Zn / Mn batteries, or Zn / bromine batteries), zinc electrodes are usually produced from powder (Non-Patent Document 1). Specifically, zinc powder is pressed or mixed with additives and then pressed, for example, by a calendaring method (Non-Patent Document 2). Alternatively, they may be produced by a sintering method (Patent Document 1).

[0008] One of the essential conditions for the technical feasibility of zinc rechargeable batteries, i.e., rechargeable batteries with zinc electrodes, especially zinc anodes, is whether they have cycle stability as a fundamental high-power battery. Conventional zinc electrodes have problems due to structural changes that occur during the charge / discharge process.

[0009] Known causes include "dendrite growth" and the so-called "shape change effect." "Dendrite growth" refers to the growth of long crystalline structures on the zinc electrode during charging, which can cause an internal short circuit and lead to battery failure. "Shape change effect" refers to the localized deposition of zinc in the lower region of the electrode, caused by an uneven distribution of current and / or the effect of gravity. This change in the shape of the electrode can also eventually cause an internal short circuit and lead to battery failure.

[0010] According to the above mentioned documents, it is already known to structure the electrodes as a measure to avoid battery failure (Non-Patent Document 1). By making the anode structure three-dimensional, structural defects are avoided and the charge / discharge capacity is greatly improved. The preparation of three-dimensional electrode structures has been investigated using battery powders, and zinc porous structures have been prepared by wet processing (Non-Patent Document 3).

[0011] The nature of the above manufacturing methods limits the pore size and structure of such structures, which are essentially characterized by the powdered raw materials used and often require the use of binders to maintain the porous structure. The structures thus manufactured have the disadvantage that they are not entirely metallic throughout, which can lead to uneven charge dissipation and localized precipitation of zinc during charging (Patent Document 2). [Prior art documents] [Patent documents]

[0012] [Patent Document 1] U.S. Patent No. 3,663,297A [Patent Document 2] German Patent No. 60014465T2 [Non-patent literature]

[0013] [Non-Patent Document 1] Trueb & Ruetschi, 1998, Batteries and Accumulators, Springer publishers [Non-Patent Document 2] Birke & Schiemann, 2013, Akkumulatore Vergangenheit, Gegenwart und Zukunft Energiespeicher.Munich: Herbert Utz Verlag GmbH [Non-Patent Document 3] Joseph F. Parker, CN (April 28, 2017). Rechargeable nickel-3D zinc batteries: An energy-dense, safer alternative to lithium-ion. Science Summary of the Invention [Problem to be solved by the invention]

[0014] There is therefore a need for new structures or methods for their manufacture which avoid the drawbacks of the prior art, in particular methods which allow for porosity, while at the same time allowing the diameter of the resulting pores to be set over as wide a range as possible, independent of the size of the subsequently formed part itself. [Means for solving the problem]

[0015] Surprisingly, it has been found that the pressure difference method allows the production of three-dimensional molded parts with an open cell pore structure. The "open cell pore" structure used in this application means that the molded part is in a sponge-like form, i.e. has an open metal sponge structure. "Open cell pore" refers independently only to the structure of the metal, regardless of whether the metal sponge structure is filled with a material other than the metal. Such molded parts can be used as anodes, in particular as anodes of primary or secondary batteries.

[0016] In a first embodiment, the present invention provides a method for producing a pharmaceutical composition comprising the steps of: a) using a molten metal; b) using a three-dimensional casting mold having a first opening and a second opening, the first opening facing the bore forming a lower end thereof and the second opening facing the bore forming an upper end thereof; c) filling the casting mold with a solid particulate void former at the melting point of the metal; d) contacting the molten metal with the first opening of the casting mold; e) providing a pressure differential between the first and second openings of the casting mold, thereby causing the molten metal to flow into the interior of the casting mold; followed by f) allowing the molten metal to solidify within the casting mold. and a method for producing a three-dimensional open-cell porosity metal shaped member for use as an anode, in particular an anode in primary batteries, secondary batteries and all-solid-state batteries, characterized in that the metal is selected from zinc, tin, lead, indium, aluminum, magnesium or bismuth, or an alloy of any of these metals.

[0017] The method of the invention allows the production of metal mouldings having a metal sponge structure with open cell porosity, the term "open cell porosity" referring to the structure of the metal sponge itself, independently and independently of whether its voids or pores are filled with a material other than the metal.

[0018] According to the present invention, the method further comprises: g) removing the void-forming agent from the three-dimensional shaped member.

[0019] Said removal of the void former can be complete or partial, or according to the invention, said void former can be left as process material within the filled metal sponge structure without being removed.

[0020] Thus, in a preferred embodiment, the process of the present invention comprises the steps of: a) using a molten metal; b) using a three-dimensional casting mold having a first opening and a second opening, the first opening facing the bore forming a lower end thereof and the second opening facing the bore forming an upper end thereof; c) filling the casting mold with a solid particulate void former at the melting point of the metal; d) contacting the molten metal with the first opening of the casting mold; e) providing a pressure differential between the first and second openings of the casting mold, thereby causing the molten metal to flow into the interior of the casting mold; followed by f) solidifying the molten metal within the casting mold; and g) partially removing said void former from said three-dimensional metal shaped part. may include.

[0021] Particularly preferably, the process of the invention comprises the steps of: a) using a molten metal; b) using a three-dimensional casting mold having a first opening and a second opening, the first opening facing the bore forming a lower end thereof and the second opening facing the bore forming an upper end thereof; c) filling the casting mold with a solid particulate void former at the melting point of the metal; d) contacting the molten metal with the first opening of the casting mold; e) providing a pressure differential between the first and second openings of the casting mold, thereby causing the molten metal to flow into the interior of the casting mold; followed by f) solidifying the molten metal within the casting mold; and g) completely removing said void former from said three-dimensional metal shaped part. It includes.

[0022] After solidification of the molten metal according to step f) of the manufacturing method according to the invention, the metal molding part can be removed from the casting mold. However, according to the invention, it is also possible to leave the metal molding part in the casting mold or, if necessary, to remove the void-forming agent from the metal molding part in the casting mold while the metal molding part remains in the casting mold. Furthermore, according to the invention, the void-forming agent can be completely or partially removed from the metal molding part outside the casting mold. Effect of the Invention

[0023] In a further embodiment, the object of the invention is achieved by a metal molding having a sponge structure with open cell porosity, which is obtainable by the manufacturing method according to the invention.

[0024] In yet another embodiment, the object of the present invention is achieved by the use of said metal shaped part having a sponge structure with open cell pores as an anode, in particular as an anode in a primary battery, a secondary battery or an all-solid-state battery. [Brief description of the drawings]

[0025] [Figure 1] FIG. 1 shows a schematic diagram of the process of the present invention. [Diagram 2] FIG. 2 shows a cross section of a molded member having a pore size and distribution of a structure produced by the production method of the present invention. [Diagram 3] FIG. 3 shows a cross section of a molded member having a pore size and distribution of a structure produced by the production method of the present invention. [Figure 4] FIG. 4 shows images for the metallographic determination of the specific surface area of ​​the structure. [Diagram 5] FIG. 5 shows the charge / discharge curves of the test secondary battery. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0026] In the following, embodiments and preferred configurations of the present invention are described in more detail. The features described below can be combined in any combination and, even if only shown for individual embodiments, apply to all embodiments unless expressly stated otherwise.

[0027] According to the manufacturing method of the present invention, a metal molded part having a metal sponge structure with open cell pores can be manufactured by a refining metallurgy method using a functional void former. The metals forming the metal sponge structure can be battery alloys, i.e. metals and alloys used in electrodes of primary or secondary batteries can be used. According to the present invention, these metals and alloys include zinc, tin, lead, indium, aluminum, magnesium, bismuth or suitable alloys of any of these metals.

[0028] The functional void formers are solid granules at the melting point of the corresponding metal or alloy. The size and shape of the granules, i.e. the individual particles, determine the porosity of the metal molded part produced. Thus, by appropriately selecting void formers with different sizes and shapes and their statistical distribution, the resulting three-dimensional structure can be freely set.

[0029] According to the invention, a salt or oxide, preferably a salt, more preferably an inorganic salt, is used as a functional void former. The choice of salt depends on the one hand on whether the salt is to be removed after the molten metal has solidified. On the other hand, the desired structure of the molded part, which will be described later, is a factor influencing the choice of the void former. In particular, sodium chloride, potassium fluoride, potassium chloride, calcium hydroxide, lithium hydroxide, lead(IV) oxide, zinc oxide, or zinc sulfate, or a mixture of two or more of these compounds, can be used as the void former.

[0030] In a preferred embodiment, the grains are free of binders, and therefore, according to the invention, they can be introduced into the casting mould without any specific pretreatment, without the need to remove binders after production of the metal part, and without having to take into account possible side reactions caused by binders.

[0031] In the manufacturing method of the present invention, the liquid molten metal can be made to penetrate from the bottom to the top of the casting mold against gravity, and the addition of a binder can be omitted. If the molten metal is added from above the casting mold filled with a void former, the void former will rise to the top. Then, the initially envisaged sponge structure that the void former should bring about is no longer present, and it is almost impossible to create the envisaged structure. To avoid this, a binder that prevents the void former from rising to the top may be used. However, in this case, the paths between the void former compound and its particles are filled with the binder, making it difficult to predict the exact structure of the resulting metal molded part. Furthermore, the binder must be selected so as not to cause inconvenience in the subsequent application. Although many suitable binders have been disclosed in the prior art, the manufacturing method of the present invention makes it possible to eliminate the binder for the first time. Therefore, in a preferred embodiment, the void former according to the present invention does not include a binder.

[0032] In one embodiment of the method according to the invention, the method comprises a step g) of completely or partially removing the void-forming agent from the three-dimensional metal shaped part, which is preferably carried out by rinsing off the void-forming agent, and in another preferred embodiment, the void-forming agent may remain in the network structure of the three-dimensional metal shaped part as a process material.

[0033] Thus, the manufacturing method of the invention makes it possible to provide a metal molded part having a metal sponge structure with open cell pores. The void former is present in the form of grains and is introduced into the three-dimensional casting mold as a filling type, forming voids between the grains. These voids are then filled by applying a pressure difference with liquid metal, which is the molten metal. By solidifying the liquid metal, a three-dimensional structure is obtained that is a metal sponge structure with open cell pores containing the functional void former. According to the invention, the functional void former can be completely or partially removed or can also remain in the molded part.

[0034] If it is desired to remove the void-forming agent from the solidified metal molded part, it is preferable to select a salt soluble in a solvent as the void-forming agent. Particularly suitable solvents include water, alcohol, acid or alkali, ethanol, methanol, diethyl ether, and tetrahydrofuran. In a particularly preferred embodiment, a water-soluble inorganic salt is used as the salt. This allows the void-forming agent to be removed by rinsing with water.

[0035] The salts may be, for example, chloride salts such as sodium chloride, potassium chloride, etc. The size of the crystals of each salt may be preset during the preparation of the respective salt. Alternatively, the salt crystals may be adjusted to the desired size, for example, by grinding and sieving.

[0036] These salts with the desired particle size and particle size distribution are then introduced into the casting mold, which has a first opening and a second opening. To retain the void former inside the casting mold, the casting mold is equipped with a device that ensures that the void former is retained in at least one opening of the casting mold, preferably in the first opening and the second opening. This device can be, for example, a grid, ceramic filter, net, glass wool, steel wool, etc., whose openings are determined by the void former or the particle size of the void former.

[0037] The casting mold is designed three-dimensionally so that its interior corresponds to the design of the molded part to be subsequently molded. The casting mold thus has an upper end and a lower end facing the bore. The height h between these two ends can be chosen freely. The bottom surface can be designed in any desired shape. The shape of the bottom surface can be circular, elliptical or polygonal. According to the invention, the cross section of the casting can be the same over the entire height h. According to the invention, the cross section can also be different. Furthermore, it can taper from the bottom to the top or from the top to the bottom. Furthermore, the cross section can change continuously or discontinuously in several places during the height h of the casting mold. The obtained metal molded part can also be post-processed, whereby complex structures can also be obtained.

[0038] According to the invention, a pressure difference is applied inside the casting mold. In the present invention, this can be achieved, for example, by connecting a device for creating a pressure difference, such as a vacuum pump, to the second opening of the casting mold, which is not in contact with the molten metal. However, according to the invention, it is also possible to create a positive pressure higher than the ambient pressure, so that the molten metal is forced up into the casting mold against gravity through the first opening, which is the lower end of the casting mold immersed in the molten metal.

[0039] In one embodiment of the invention, the vacuum pump can be connected to the casting mold in any of different ways. For example, a connection member can be used for this purpose, which connects to the second opening of the casting mold. Again, this type of connection depends on the shape of the casting mold.

[0040] The device for providing a pressure difference may be a pump that generates a positive pressure. Thus, a pump that can be connected to the casting mold can provide a negative or positive pressure inside the casting mold. Such negative or positive pressure refers to a pressure difference with respect to the surroundings. The actual pressure will vary depending on the type of molten metal, the type of void former, and the actual spatial design of the casting mold.

[0041] According to the invention, the casting mold filled with the void former is immersed in the molten metal with its lower end formed by the first opening facing the bore. The casting mold is immersed in the molten metal so that at the end of the process it is filled with the corresponding metal or metal alloy. It is neither necessary nor desirable to completely immerse the casting mold in the molten metal over its entire height, as this would result in the metal adhering to the outside of the casting mold, leading to material losses. Preferably, the casting mold is immersed in the molten metal for about 10-35% of its height.

[0042] A pressure difference is then applied. The molten metal is sucked into the interior of the casting mold by the negative pressure, completely filling the gaps between the void formers. The metal then solidifies in the casting mold. The solidification behavior can be influenced by the suction speed, which is controlled by the flow through valves and nozzles. The negative pressure remains during solidification, ensuring complete filling of the casting mold and its voids.

[0043] In the present invention, negative pressure means that the pressure is reduced to less than 1 bar, which is atmospheric pressure. The negative pressure is preferably set in the range of 50-900 mbar, more preferably 250-750 mbar, even more preferably 400-600 mbar. The actual pressure will vary depending on the type of metal or alloy employed, but also on the actual three-dimensional design of the casting mold.

[0044] According to the invention, applying a positive pressure means that the molten metal is forced into the casting mould by a positive pressure, for example via a pouring furnace, where the positive pressure is preferably set in the range of 10-900 mbar, more preferably 40-500 mbar, which means that the pressure is higher than the ambient pressure by that amount.

[0045] The manufacturing method of the present invention makes it possible to obtain a uniform and dimensionally stable three-dimensional structure made of a metal molded member having a sponge structure of the adopted metal. This metal sponge structure has voids inside. By appropriately selecting the void-forming agent, the shape of the voids can be adjusted in a controlled manner. The voids can also be adjusted to a spherical or cubic shape. Thereby, it is possible to adjust the porosity to 10 to 90% by volume. The shape of the voids and the porosity of the molded member can be combined or exchanged. By selectively distributing the particles of the void-forming agent, the diameter of the voids and the structure of the voids inside the molded member can be controlled. Thus, for example, the molded member may have a fine void structure in one region and a coarse void structure in another region. For example, it can be manufactured by appropriately selecting different types of salts as the void-forming agent. It is also possible to use the same type of salt with different sizes and / or shapes. Therefore, by filling the void formers in the casting mold, the regions in which the void formers having each of the diameters / shapes are present can be determined, which will later be reflected in the corresponding void diameter distribution in the metal forming part.

[0046] By appropriately selecting different types of salts, it is also possible to produce metal moldings in which the void former is washed out of the voids of the metal sponge structure only in some sub-regions, while in other sub-regions the void former remains present as a process material. This is possible by appropriately selecting different salts that dissolve in different solvents. Furthermore, in the manufacturing method of the present invention, it is possible to use no components other than the void former and the molten metal. A binder as disclosed in the prior art is not necessarily required. The manufacturing method of the present invention is preferably characterized in that no binder is used, and the void former or the metal or alloy used does not contain a binder.

[0047] The porosity also determines the density of the molded member. According to the manufacturing method of the present invention, the density of the molded member not containing a void-forming agent is 0.5 to 9.5 g / cm 3 When zinc or a zinc alloy with a zinc content of at least 98% by weight is used as the metal, it is possible to produce molded parts having a density in the range of 0.7 to 6.5 g / cm. 3 Densities in the range of can be achieved.

[0048] The method of the present invention allows the production of continuous conductive metal structures, which have a metal sponge structure with open cell pores that allows liquids or gases to pass through, and does not require any other materials, additives, binders, etc., apart from the casting mold, the void former, and the molten metal, regardless of the size of the metal molded part produced.

[0049] The manufacturing method of the present invention allows the metal molding produced according to the present invention to be used as the anode of a primary battery, a secondary battery, or an all-solid-state battery. The structure of the metal molding can immediately and greatly improve the capacity of the battery and greatly extend the life of the battery. For example, the rearrangement of the active material in the lower region of the anode is suppressed, which stabilizes the shape of the anode and increases its service life.

[0050] Surprisingly, it has been found that zinc remains near the discharge site during discharge and can be recovered near the discharge site during charging, making it particularly suitable for use in secondary batteries. It has also been found that zinc is concentrated in the center of the anode, i.e., zinc does not diffuse into the electrolyte and remains uniformly distributed within the anode.

[0051] Furthermore, it was observed that dendrite growth was significantly reduced, reducing the risk of internal short circuits.

[0052] The casting, cast using a pressure difference, produces a metal molded part with open cell pores, with a three-dimensional shape predetermined by the casting mold and a void distribution predetermined inside the metal sponge structure by the void former employed. Thus, complex three-dimensional network structures of zinc, tin, lead, indium, aluminum, magnesium or bismuth or alloys of these metals can be obtained. Such structures are particularly suitable for use as anodes in primary batteries (disposable batteries), secondary batteries (rechargeable batteries, accumulators) or (three-dimensional) all-solid-state batteries.

[0053] The resulting metal molded part has high strength and dimensional stability, so that it can be subjected to mechanical treatments before or after the removal of the void former, thereby making it possible to produce electrodes with very special geometries.

[0054] According to the manufacturing method of the present invention, the metal molded part can be manufactured with a pore size in the range of 0.01-20 mm, preferably 0.04-18 mm, more preferably 0.06-16 mm, and even more preferably 0.1-14 mm. The porosity is preferably 10-90 vol.%, more preferably 50-75 vol.%, and even more preferably 60-70 vol.%. Due to the metal foam structure with open cell pores, all the voids inside the molded part are interconnected. When the molded part is applied as an anode, the electrolyte solution is sucked into the molded part by the capillary force. Therefore, a large surface area is obtained, and therefore a good interaction is obtained between the anode and the electrolyte of the battery. According to the present invention, the obtained metal molded part can also be used as an anode for cathodic corrosion prevention of steel and steel-reinforced concrete due to its large surface area. EXAMPLES

[0055] Examples of the present invention will be described in detail below, but the scope of the present invention is not limited to these examples.

[0056] [Example] A zinc anode for a battery was produced according to the method of the present invention.The pressure difference was set by applying a negative pressure.

[0057] For this purpose, a cylindrical casting mold with an inner diameter of 55 mm and a length of 1,000 mm was used. The casting mold was filled with sodium chloride having an average particle size of 0.4 to 1.25 mm. The casting mold had a ceramic filter at the opening forming the lower end in order to retain the sodium chloride, which is the void-forming agent, inside the mold.

[0058] The upper end of the casting mold (the end facing upwards in the bore, in the longitudinal direction) had an opening therein with a nozzle connected thereto, which was connected to a vacuum pump via a flexible tube.

[0059] A negative pressure of 500 mbar was set. The casting mould was completely filled with the molten metal and after the molten metal had solidified, the sodium chloride was washed out with water.

[0060] FIG. 1 shows a schematic diagram of the above steps.

[0061] 2 and 3 show cross sections of molded members having different pore sizes and distributions produced by the production method of the present invention described in the above examples.

[0062] The molded part has a fine metal bubble structure and pores with diameters of 0.15 to 0.7 mm. The density is 1.9 g / cm. 3 The molded part shown in FIG. 3 had a coarse metal foam structure. The pore size was 0.4 to 1.25 mm, and the density was 3.0 g / cm. 3 The porosity was 58.0 volume %.

[0063] Figure 4 shows the images that served as the basis for the metallographic determination of the specific surface area of ​​the structure shown in Figures 2 and 3. In Figure 4, the molded part from Figure 2 is reproduced on the left and the molded part from Figure 3 is reproduced on the right.

[0064] The results are shown in the table below.

[0065] [Table 1] [Industrial Applicability]

[0066] To test the cycling stability of the metal sponge structure, a test secondary battery was used that was constructed with nickel hydroxide (Ni(OH)2) as the cathode. This test secondary battery was subjected to a cycling test of charging and discharging, and the current and voltage were recorded. The charging and discharging capacities are shown in Figure 5. The results show that the test secondary battery thus fabricated can function over many cycling cycles without power loss.

Claims

1. The process is as follows: a) using a molten metal; b) using a three-dimensional casting mold having a first opening and a second opening, the first opening facing the bore forming a lower end thereof and the second opening facing the bore forming an upper end thereof; c) filling the casting mold with a granular void former at the melting point of the metal; d) contacting the molten metal with the first opening of the casting mold; e) providing a pressure differential between the first and second openings of the casting mold, thereby causing the molten metal to flow into the interior of the casting mold; followed by f) solidifying the molten metal within the casting mold. a) forming a three-dimensional metal shaped part for use as an anode in primary batteries, secondary batteries and all-solid-state batteries, the three-dimensional metal shaped part having a metal sponge structure with open cell pores, the metal being selected from zinc, tin, lead, indium, aluminum, magnesium or bismuth, or an alloy of any of these metals.

2. Furthermore, 2. The method of claim 1, further comprising the step of: g) completely or partially removing said void former from said three-dimensional metal shaped part.

3. 3. The method for producing a three-dimensional metal formed part according to claim 1, wherein the metal is zinc or a zinc alloy.

4. The method for producing a three-dimensional metal formed part according to any one of claims 1 to 3, characterized in that in step e), a negative pressure is applied, the negative pressure being preferably set in the range of 50 to 900 mbar, more preferably 250 to 750 mbar, and even more preferably 400 to 600 mbar.

5. 5. The method for producing a three-dimensional metal shaped part according to claim 1, characterized in that in step e) a positive pressure is applied, which is preferably set in the range of 20 mbar to 10 bar.

6. The method for producing a three-dimensional metal shaped part according to any one of claims 1 to 5, characterized in that the void-forming agent is a salt, preferably an inorganic salt.

7. The method for manufacturing a three-dimensional metal formed part according to any one of claims 1 to 6, characterized in that the diameter of the pores in the metal formed part after solidification is 0.01 to 20 mm, preferably 0.04 to 18 mm, more preferably 0.06 to 16 mm, and even more preferably 0.1 to 14 mm.

8. The method for producing a three-dimensional metal formed part according to any one of claims 1 to 7, characterized in that the porosity of the metal formed part is 10 to 90 volume %, preferably 50 to 75 volume %, and more preferably 60 to 70 volume %.

9. The density of the metal molded part made of zinc or a zinc alloy having a zinc ratio of 98% by weight is 0.7 to 6.3 g / cm 3 The method for producing a three-dimensional metal formed part according to any one of claims 1 to 8, characterized in that

10. 10. The method for producing a three-dimensional metal formed part according to claim 1, wherein the contact in step d) comprises immersing the casting mold together with the lower end of the first opening into the molten metal.

11. The method of claim 10, wherein the casting mold is immersed in the molten metal to 10-35% of its height.

12. The method for producing a three-dimensional metal formed part according to any one of claims 1 to 11, characterized in that no binder is used.

13. Use of a metal shaped part obtainable by the method according to any one of claims 1 to 12 as an anode in a primary, secondary or all-solid-state battery.

14. Use of a metal molded part obtainable by the process according to any one of claims 1 to 12 as an anode for the cathodic corrosion protection of steel and steel-reinforced concrete.

15. 15. Use according to claim 13 or 14, characterized in that the metal part consists of zinc or a zinc alloy.

Citation Information

Patent Citations

  • Negative pressure casting method for preparing foam zinc-aluminum alloy

    CN108193070A

  • Foam metal preparation method and foam metal preparation device

    CN110052594A

  • Negative pressure casting method for preparing foamed zinc-aluminium alloy

    CN1935414A

  • Stent

    JP2001190688A

  • Primary battery