Optical fiber preform and method for producing same
By controlling alkali metal diffusion in silica glass tubes with chlorine-free compounds and a controlled process, the method addresses impurity-induced losses in optical fibers, achieving reduced attenuation and improved fiber performance.
Patent Information
- Application Number
- JP2024532436
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-30
- Filing Date
- 2022-11-28
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for diffusing alkali metals into silica glass for optical fibers suffer from simultaneous diffusion of impurities, leading to higher-than-expected optical losses due to contaminants like transition metals and water, which are difficult to avoid during the doping process.
A method involving the use of a silica glass tube with controlled diffusion of alkali metals, minimizing impurities by using chlorine-free alkali metal source compounds and a controlled diffusion process to form an optical fiber preform with a cladding jacket, reducing contaminants and enhancing the optical properties.
Significantly reduces attenuation in optical fibers by minimizing impurity-induced losses, achieving lower optical losses by exponentially decreasing contaminants with radial position, resulting in improved fiber performance.
Smart Images

Figure 2024542689000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of priority under 35 U.S.C. § 119 to U.S. Provisional Application No. 63 / 284,270, filed November 30, 2021, the contents of which are incorporated by reference in their entirety and are hereby incorporated by reference. FIELD OF THE DISCLOSURE The present disclosure relates generally to methods for manufacturing optical fibers, and more particularly to methods for producing alkali metal oxide doped optical fibers. [Background technology]
[0002] Attenuation is the main limiting characteristic of optical fibers. Optical fiber loss plays a key role in setting the limiting distance between, for example, optical fiber amplifiers. This is particularly important in long-haul and ultra-long-haul networks, for example in undersea applications, where such amplifiers are a major factor in significant system cost as well as system reliability. As a result, there is enormous commercial interest in reducing attenuation to the lowest possible level. For silica-based optical fibers used in long-distance telecommunications transmission networks, attenuation losses have been reduced to the point where most of the remaining attenuation is due to intrinsic scattering within the glass material, which is a combination of losses associated with density and dopant concentration variations. One means of lowering the attenuation is to add modifiers to the core glass. Such modifiers, if properly selected, can significantly reduce the scattering losses in the fiber core and therefore the attenuation of the fiber. Alkali metal oxides can act as efficient modifiers.
[0003] Silica-based glasses containing alkali metal oxide dopants, either alone or in combination with other compounds such as CaO, Al2O3 or F, have been proposed as core materials for optical fibers with lower intrinsic scattering losses than high-purity vitreous SiO2. In both single- and multi-dopant glasses, high levels of contaminants, such as transition metals and -OH, make it difficult to achieve the desired low attenuation. Often these contaminants are introduced unintentionally during the doping process. One technique for incorporating alkali metal oxides into silica glass is by direct diffusion of the alkali metal into the consolidated glass. However, attempts to diffuse alkali metals into silica glass suffer from the simultaneous diffusion of impurities, including transition metals and water, resulting in losses well above the theoretical minimum. It would be desirable to develop a method of doping silica glass optical fiber precursors with alkali metals such that fibers extending from the silica glass optical fiber precursors have low optical losses. Summary of the Invention
[0004] In one embodiment, a method of forming an optical fiber precursor includes forming an alkali metal doped tube, inserting an optical fiber core rod into the alkali metal doped tube, forming a cladding jacket around the alkali metal doped tube, and diffusing alkali metal from the alkali metal doped tube across a surface of the optical fiber core rod. A second embodiment of the present disclosure may include the first embodiment, where the optical fiber core rod comprises pure silica. A third embodiment of the present disclosure may include the first embodiment, where the optical fiber core rod includes silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P). A fourth embodiment of the present disclosure may include any of the first to third embodiments, wherein the optical fiber core rod includes a cladding surrounding the optical fiber core rod. A fifth embodiment of the present disclosure may include the fourth embodiment, wherein the cladding surrounding the optical fiber core rod comprises fluorine-doped silica. A sixth embodiment of the present disclosure may include any of the first to fifth embodiments, wherein the cladding jacket includes pure silica.
[0005] A seventh embodiment of the present disclosure may include any of the first to fifth embodiments, wherein the cladding jacket includes fluorine-doped silica. An eighth embodiment of the present disclosure may include any of the first to seventh embodiments, wherein the alkali metal doped tube comprises sodium (Na) doped silica. A ninth embodiment of the present disclosure relates to an optical fiber preform having an optical fiber core rod, an alkali metal doped tube surrounding the optical fiber core rod, and a cladding jacket surrounding the alkali metal doped tube. A tenth embodiment of the present disclosure may include the ninth embodiment, wherein the optical fiber core rod comprises pure silica. An eleventh embodiment of the present disclosure may include the ninth embodiment, wherein the optical fiber core rod includes silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P).
[0006] A twelfth embodiment of the present disclosure may include any of the ninth to eleventh embodiments, wherein the optical fiber core rod includes a cladding surrounding the optical fiber core rod. A thirteenth embodiment of the present disclosure may include the twelfth embodiment, wherein the cladding surrounding the optical fiber core rod comprises fluorine-doped silica. A fourteenth embodiment of the present disclosure may include any of the ninth to thirteenth embodiments, wherein the cladding jacket includes pure silica. A fifteenth embodiment of the present disclosure may include any of the ninth to thirteenth embodiments, wherein the cladding jacket includes fluorine-doped silica. A sixteenth embodiment of the present disclosure may include any of the ninth to fifteenth embodiments, wherein the alkali metal doped tube is doped with sodium (Na). The silica is preferably oxidized.
[0007] A seventeenth embodiment of the present disclosure relates to an optical fiber preform having an optical fiber core rod including a cladding surrounding the optical fiber core rod, the cladding surrounding the optical fiber core rod comprising fluorine-doped silica; an alkali metal-doped tube surrounding the optical fiber core rod; and a cladding jacket surrounding the alkali metal-doped tube. An eighteenth embodiment of the present disclosure may include the seventeenth embodiment, wherein the optical fiber core rod comprises pure silica. A nineteenth embodiment of the present disclosure may include the seventeenth embodiment, wherein the optical fiber core rod includes silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P). A twentieth embodiment of the present disclosure may include any of the seventeenth to nineteenth embodiments, wherein the alkali metal doped tube comprises sodium (Na) doped silica. The foregoing will be apparent from the following more particular description of exemplary embodiments, as illustrated in the accompanying drawings, in which like reference characters refer to the same parts throughout the different views, and in which the drawings are not necessarily to scale, emphasis instead being placed on illustrating exemplary embodiments. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 illustrates an apparatus for diffusing alkali into a silica glass tube showing the relationship between the burner and the alkali metal source compound location. [Diagram 2]1 illustrates an exemplary optical fiber preform. [Diagram 3] 13 is a graph showing the calculated attenuation reduction as a function of radial position of the tube. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The present invention relates to a method for producing a low-loss optical fiber. More specifically, the present invention relates to preparing an optical fiber precursor by diffusing an alkali metal into a silica glass article. Optical fiber precursor refers to a complete optical fiber preform or a precursor of a complete optical fiber preform, such as, for example, a core cane or a deposition tube. Core cane refers to a consolidated glass precursor of an optical fiber preform that is not a complete optical fiber preform but includes at least a portion of a core. Optical fiber preform refers to a consolidated glass article that is ready to be drawn into an optical fiber. It has been shown that silica glass doped with alkali metal oxides can provide losses below the theoretical lower limit for pure silica glass. "Doped" or "doping", or synonyms, refer to the intentional addition of a substance or substances to glass to achieve desired characteristics (as set forth herein) in such glass. One means of producing low-loss optical fiber is by diffusing alkali metals into a suitable silica glass article that is a precursor to optical fiber.
[0010] In an embodiment, an illustration of which is given in FIG. 1, a silica glass tube 10 suitable for the manufacture of optical fiber is mounted on a glass working lathe. One example of a suitable apparatus is a conventional modified chemical vapor deposition (MCVD) glass forming lathe. A reservoir 16 for containing an alkali metal source is formed near one end of the tube 10 by constructing two neck-like deformations 6 and 8 in the wall of the tube 10, approximately 2 cm apart from each other. The exact composition of the tube 10 depends on the desired optical fiber design, but generally such tubes contain as much as or more than about 80 mole percent silicon dioxide (SiO2). In the manufacture of many optical fibers, the tube 10 preferably contains at least about 90 mole percent SiO2. Such tubes may contain dopants, either alone or in combination. Such dopants may include, for example, fluorine (F), aluminum oxide (Al2O3), calcium oxide (CaO), germanium dioxide (GeO2), or phosphorus (P). Prior to diffusing the alkali metal into the tube 10, additional silica glass may be added to the interior surface of the glass tube 10 by chemical vapor deposition means. Such additional glass may contain dopants including, for example, F, Al2O3, CaO, GeO2, or P. In an embodiment, the tube 10, and any additional glass deposited therein, are substantially chlorine-free. Substantially chlorine-free refers to exhibiting a chlorine content sufficiently low that optical losses due to alkali chloride crystallization are avoided, for example, a chlorine content of preferably less than about 500 ppm is desirable for this purpose. More preferably, the chlorine content is less than about 100 ppm, and most preferably less than about 50 ppm. In addition, the silica glass tube 10, and any additional glass deposited therein, are substantially free of hydroxyl groups. - The glass should be free of "water" (OH). Water causes an absorption peak at or about 1383 nm, which may extend into the operating wavelength region of optical fibers. This peak has a detrimental effect on fiber attenuation. -It is desirable to reduce the absorption peak, also called the water peak, by reducing the OH content as much as possible. This requires that the starting material be substantially free of water, preferably less than about 100 ppb, more preferably less than about 20 ppb. - OH content. This can be achieved, for example, by utilizing conventional chlorine drying techniques during the manufacture of silica glass tubes and suitable precautions after their manufacture to prevent the tubes from rewetting. However, the use of chlorine should be minimized to reduce the chlorine concentration in the glass. For porous soot glass articles, drying is preferably achieved by exposing the article to a fluorine-containing atmosphere, such as, for example, carbon tetrafluoride (CF4) or silicon tetrafluoride (SiF4), or a combination thereof, after chlorine drying or instead of chlorine drying. Exposure to a fluorine-containing atmosphere is preferably performed at a temperature less than about 1100°C to avoid doping the glass with high levels of fluorine. Preferably, the glass has a water content less than about 100 ppb, more preferably less than about 20 ppb.
[0011] Once the silica glass tube 10 is prepared, including any optional deposition of additional glass, an alkali source compound 12 is introduced into the tube 10 at reservoir 16 and heated by heat source 18 to form a vapor while the tube 10 rotates. The alkali metal source compound 12 may be introduced into the reservoir 16 as a liquid or solid. Oxygen flows through the rotating seal 4 into the inlet 2 and into the tube 10, and the portion of the tube 10 downstream of the alkali metal source compound 12 is heated to drive diffusion of the alkali metal to the interior surface of the tube 10. The portion of the tube 10 downstream of the alkali metal source compound 12 should be heated to a temperature sufficient to promote rapid diffusion of the alkali and prevent devitrification. Preferably, the portion of the tube 10 downstream of the alkali metal source compound 12 is heated by heat source 20 to at least about 1500° C., more preferably at least about 1700° C., and most preferably at least about 2000° C. The alkali metal source compound 12 is a chlorine-free compound having an element selected from the group consisting of potassium (K), sodium (Na), lithium (Li), cesium (Cs), and rubidium (Rb) as a component. Preferably, the alkali metal source compound 12 is a bromide, iodide, or fluoride. More preferably, the alkali metal source compound 12 is a bromide, iodide, or fluoride of K or Na.
[0012] The diffusion process may be followed by further heating the doped tube 10 to promote partial collapsing of the doped tube 10, thereby reducing the internal surface area through which the alkali metal may be lost and thickening the glass layer into which the alkali metal is diffused. The doped tube 10 is cut to remove a portion of the glass containing the reservoir 16. An optical fiber core rod (i.e., core cane) is inserted into the doped tube 10. In an embodiment, the optical fiber core rod is pure silica. In an embodiment, the optical fiber core rod is silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P). In an embodiment, the optical fiber core rod contains a cladding surrounding the optical fiber core rod. In an embodiment, the cladding is doped with fluorine. After inserting the optical fiber core rod into the tube, a cladding jacket (e.g., a protective coating) is formed around the tube 10 and collapsed to form an optical fiber preform. In an embodiment, the cladding jacket is pure silica. In an embodiment, the cladding jacket is silica doped with fluorine. 2 shows an example of an optical fiber preform 20 as described herein having an optical fiber core rod 22 surrounded by a tube 10. The tube 10 is surrounded by a cladding jacket 24.
[0013] One advantage of the proposed method described herein is that the attenuation due to contaminants in alkali doped glass tubes is significantly reduced. Figure 3 shows the calculated attenuation reduction as a function of radial position in the tube. The attenuation due to contaminants decreases exponentially with radial position. For example, at a radial position of 5 μm the attenuation is reduced to 10%, and at a radial position of 10 μm the attenuation is reduced to less than 1%. Although exemplary embodiments have been disclosed herein, it will be understood by those skilled in the art that various changes in form and details may be made therein without departing from the scope of the invention as encompassed by the appended claims.
Claims
1. 1. A method of forming an optical fiber precursor, comprising: forming an alkali metal doped tube; inserting an optical fiber core rod into the alkali metal doped tube; forming a cladding jacket around the alkali metal doped tube; and diffusing alkali metal from the alkali metal doped tube over the surface of the optical fiber core rod. A method comprising:
2. The method of claim 1 , wherein the optical fiber core rod comprises pure silica.
3. The method of claim 1 , wherein the optical fiber core rod comprises silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P).
4. The method of claim 1 , wherein the optical fiber core rod includes a cladding surrounding the optical fiber core rod.
5. The method of claim 4 , wherein the cladding surrounding the optical fiber core rod comprises fluorine-doped silica.
6. The method of claim 1 , wherein the cladding jacket comprises pure silica.
7. The method of claim 1 , wherein the cladding jacket comprises fluorine-doped silica.
8. The method of claim 1 , wherein the alkali metal doped tube comprises sodium (Na) doped silica.
9. Optical fiber core rod, an alkali metal doped tube surrounding the optical fiber core rod; and a cladding jacket surrounding said alkali metal doped tube; 13. An optical fiber preform comprising:
10. 10. The optical fiber preform of claim 9, wherein the optical fiber core rod comprises pure silica.
11. 10. The optical fiber preform of claim 9, wherein the optical fiber core rod comprises silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P).
12. The optical fiber preform according to claim 9 , wherein the optical fiber core rod includes a cladding surrounding the optical fiber core rod.
13. The optical fiber preform of claim 12 , wherein the cladding surrounding the optical fiber core rod comprises fluorine-doped silica.
14. 10. The optical fiber preform of claim 9, wherein the cladding jacket comprises pure silica.
15. 10. The optical fiber preform of claim 9, wherein the cladding jacket comprises fluorine-doped silica.
16. 10. The optical fiber preform of claim 9, wherein the alkali metal doped tube comprises sodium (Na) doped silica.
17. an optical fiber core rod, comprising a cladding surrounding the optical fiber core rod, the cladding surrounding the optical fiber core rod comprising fluorine-doped silica; an alkali metal doped tube surrounding the optical fiber core rod; and a cladding jacket surrounding said alkali metal doped tube; 13. An optical fiber preform comprising:
18. 20. The optical fiber preform of claim 17, wherein the optical fiber core rod comprises pure silica.
19. 20. The optical fiber preform of claim 17, wherein the optical fiber core rod comprises silica doped with one of chlorine (Cl), germanium (Ge), or phosphorus (P).