Measurement method for estimating the temperature of a power semiconductor module
The method addresses temperature non-uniformity in power semiconductor modules by using flat band voltage measurements to estimate temperature distribution, enhancing accuracy and simplifying calibration without individual die access.
Patent Information
- Application Number
- JP2024556826
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-03-23
- Filing Date
- 2022-07-22
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2042-07-22
AI Technical Summary
Existing methods for estimating junction temperature in power semiconductor modules, particularly in multi-chip modules, face challenges due to temperature non-uniformity among parallel dies, leading to inaccurate measurements and requiring complex calibration systems that are impractical for real-world applications.
A method involving multiple series of operations using flat band voltage measurements across the gate and emitter of power semiconductor modules, allowing for estimation of temperature distribution without individual die access, by comparing voltage waveforms under reference and operational conditions.
Accurately estimates temperature non-uniformity within power semiconductor modules, improving measurement accuracy and simplifying calibration processes, even in critical operating conditions.
Smart Images

Figure 2024544351000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to the field of power semiconductor monitoring. [Background technology]
[0002] It is known to monitor temperature in metal oxide semiconductor (MOS) type power semiconductors or in parallel-connected MOS type power semiconductors, especially in power semiconductor devices / modules such as multi-chip power modules, for protection, status and health monitoring. Generally, the free surface of the die is very small. Fixing a sensor on it is difficult and in some cases even impossible. It is theoretically clear to use the individual gate accesses of the power die to measure the individual gate resistance, which is a heat-sensitive parameter. However, it leads to a large number of external connections and a complex system to implement. It is very difficult to do it at laboratory level. In real industrial and operational situations, it is not practical to use individual PN junction sensors.
[0003] In addition, because the sensors need to be integrated inside the power module's packaging, their presence must be planned for initially during the module's conception and they cannot be retrofitted onto existing power modules.
[0004] There are many known Temperature Sensitive Electrical Parameter (TSEP) based methods and on-chip sensors for estimating the junction temperature of power semiconductors online. Below are examples of measurements and actions used to estimate the TSEP: Gate voltage plateau detection during turn-on Turn-off delay time (t dOff ) Turn-on delay time (t dOn ) Duration of the Miller Plateau Sub-threshold voltage via auxiliary emitter (source) and power emitter (source) Transient gate current peak at turn-on Apply a sinusoidal gate-emitter voltage and measure the instantaneous voltage drop across the external gate resistor Injecting a DC current into the gate path of the power die and measuring the voltage across the gate-emitter
[0005] In any of these known methods, the necessary calibration of the TSEP is only possible at uniform temperature. However, since only a single TSEP is available for the parallel dies, temperature non-uniformity during normal operation leads to erroneous estimation of the junction temperature. The accuracy of the TSEP depends on the average temperature, the maximum temperature, or the minimum temperature. As explained in Non-Patent Document 1, the collector-emitter voltage (V ce ) is one of the most accurate TSEPs for average temperature, but dV CE Using other TSEPs such as / dt completely fails to estimate the junction temperature. The main reason is that the hottest die has the highest Miller capacitance and therefore V CE This is because the rise of the lowest threshold voltage (V th ) is measured, and all dies have the same V th If the temperature is 100°C, this is the maximum junction temperature (T j ), but this is not the case (measurements have shown errors of up to 25K for a 50K increase). Furthermore, since die performance is temperature-dependent, temperature imbalances change the sensitivity and linearity of the TSEP.
[0006] Loss and thermal models can be used to compensate the estimated virtual junction temperature up to or including the die-to-die temperature difference. Nevertheless, these methods require complex calibration systems of loss and thermal models and lose accuracy during operation of the power module if the solder layers degrade or, in general, if differences arise between the operating conditions and the initial model during operation of the module. [Prior art documents] [Non-patent literature]
[0007] [Non-Patent Document 1] C. Chen, V. Pickert, B. Ji, C. Ji, A. Knoll and C. Ng, “Comparison of TSEP Performances Operating at Homogeneous and Inhomogeneous Temperature Distribution in Multichip IGBT Power Modules” IEEE Journal of Emerging and Selected Topics in Power Electronics [Non-Patent Document 2] M. Hoeer, F. Filsecker, M. Wagner and S. Bernet, “Application issues of an online temperature estimation method in a high-power 4.5 kV IGBT module based on the gate-emitter threshold voltage”, 2016, 18th European Conference on Power Electronics and Applica Summary of the Invention [Problem to be solved by the invention]
[0008] The present disclosure improves this situation. [Means for solving the problem]
[0009] A measurement method for estimating the temperature of a power semiconductor module comprising a single metal-oxide semiconductor, a single metal-insulator semiconductor or a set of parallel-connected metal-oxide semiconductors or metal-insulator semiconductors is proposed, the method comprising: a. Positive current I from the emitter / source to the gate of the module g,ref, and an initial gate-emitter / source voltage V 0,ref is the flat band voltage V fb and b. The voltage across the current source, V ig,ref Measuring (t); and c. The module voltage is the flat band voltage V fb When the current I g,ref and ceasing the infusion of at least one first series of operations while the module is in a reference state, d. A positive current I flows from the emitter / source of the module to the gate. g,op , and an initial gate-emitter / source voltage V 0,op is the flat band voltage V fb and e. Voltage across the current source V ig,op Measuring (t); and f. The module voltage is the flat band voltage V fb When the current I g,op and ceasing the infusion of at least one second series of operations while the module is in an operational state, Next, g. The voltage V measured during one first series ig,ref (t) and the voltage V measured during one second series ig,op (t) and h.Comparison of temperature dispersion across the module T j,dev and estimating At least one third series of operations, including: Includes.
[0010] In another aspect, a power semiconductor module is proposed comprising a single metal oxide semiconductor, a single metal insulator semiconductor, or a set of parallel connected metal oxide semiconductors or metal insulator semiconductors and configured to perform the methods described herein.
[0011] In another aspect, proposed is computer software comprising instructions which, when executed by a processor, perform a method as defined herein.In another aspect, proposed is a computer readable non-transitory recording medium having software stored thereon, which, when executed by a processor, performs a method as defined herein.
[0012] The following features can optionally be implemented separately or in combination with each other.
[0013] Each of the at least one first series and the at least one second series comprises: i. Average module temperature T av,ref and T av,op
[0023] The second series is a series of at least one average temperature T obtained during the first series. av,ref and the average temperature T obtained during the second series av,op The difference between the two is a given value ΔT lim This is repeated until the following is true:
[0014] The first series may be divided into two series with different average temperatures T av,ref,n It is executed in The first series is executed during a state different from the operational state of the module.
[0015] The first series may be divided into two series with different average temperatures T av,ref,n It is executed in Each of the first series is executed during the baseline and operational states of the module and prior to reaching a predetermined operational deadline in the operational operation of the module.
[0016] The third series, before the comparison, g'. The voltage V measured during at least one first series ig,refFor the waveform of (t), the voltage V measured during at least one second series ig,op Adjusting (t) in time and offset Further includes.
[0017] Each of the at least one first series is executed when the power transmitted by the module is below a predetermined limit that is below a nominal maximum load of the module.
[0018] Other features, details and advantages are set forth in the following detailed description and figures. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1 is a temperature distribution diagram of a semiconductor device at the beginning of operation (new product). [Diagram 2] FIG. 1 is a temperature distribution diagram of a semiconductor device during use (deterioration). [Diagram 3] 1 is a thermal view of a semiconductor module containing six parallel-connected semiconductor devices. [Figure 4] 4 is an equivalent circuit of the module shown in FIG. 3. [Diagram 5] 1 is a circuit according to one embodiment. [Figure 6] 1 is a graph of some data obtained during one embodiment. [Figure 7] 1 is a graph of some data obtained during one embodiment. [Figure 8] 1 is a flow chart executed during one embodiment. [Figure 9] 4 is a flow chart of an algorithm executed during one embodiment. [Figure 10] 1 is a graph of voltage as a function of time. [Figure 11] 11 is the same graph as FIG. 10 after adjusting the values / curves. [Figure 12] 1 is a graph of voltage deviation as a function of temperature deviation. [Figure 13]1 is a graph of gate-emitter voltage as a function of time. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] Reference is now made to Figs. 1 to 4. Figs. 1 and 2 are temperature distribution diagrams of a power semiconductor module 1 having the same architecture but photographed at two steps of their different usage times. The module 1 in Fig. 1 is new and in a short-term operating state, while the module 1 in Fig. 2 has been degraded by long-term operation. Such photographs clearly show that significant non-uniformity of temperature in a single device (here a die) appears during operation of the module 1. Figs. 3 and 4 show another power semiconductor module 1 with six parallel-connected semiconductor elements 11 (dies). Such photographs clearly show that non-uniformity of temperature appears between devices (here dies) in the same module 1 during operation of the module 1.
[0021] Several measurement methods can be used to monitor such temperatures at laboratory level. Here, a measurement method is proposed for estimating the temperature of a power semiconductor module 1, which is typically not used on a test bench but in operating conditions when the module is integrated and interconnected in its operating and application environment.
[0022] In the following, a power semiconductor module is an assembly comprising a single metal oxide semiconductor (MOS) transistor, a single metal insulator semiconductor (MIS) or a set of parallel-connected MOS / MIS transistors. Here, the transistors are MOSFETs (metal oxide semiconductor field effect transistors), but IGBTs (insulated gate bipolar transistors) can also be used. If several MOS / MIS are connected in parallel, there is a common gate G, a common source S and a common drain D. For this reason, in the following, the single gate, single source and single drain are referred to without distinction between embodiments with one or several MOS transistor elements. The term "power" is used in its general sense in the technical field of energy conversion (power electronics).
[0023] The method comprises: at least one first series of operations I during which module 1 is in a reference state; at least one second series of operations II while the module 1 is in an operational state; At least one third series operation III; Includes.
[0024] The reference state corresponds to a state in which the MOS elements are in a known state, and the temperature non-uniformity within the module 1 is limited to a predetermined maximum value ΔT ref It is known that the reference condition is less than 100%, and the smaller the better. For example, all dies are heated to the same temperature and no power is dissipated on the dies. Such a reference condition makes it possible to obtain a reference value for module 1.
[0025] In the examples below, such a reference state is controlled, but in various embodiments, the reference state may correspond to a particular period of operation of the module 1 during which the MOS elements 11 are in a known stable state, e.g., an off state.
[0026] In the following example, the module 1 comprises (or is connected to) a control circuit 2, which: The voltage of the MOS element 11 of the module 1 is its flat band voltage V fb Higher than V 0,ref Voltage source 21 (V drive ), such a voltage source 21 is not specifically dedicated to the method described herein, in other words the voltage source 21 is a normal component of the module that is also active during conventional operation of the module. drive )and, For example, a current source 22 (I g )and, a control unit 23 configured to start and stop the current source 22 via a control line CTRL2; A voltage measuring means; a computing unit 24 configured to perform a third series of operations III; Includes.
[0027] Fig. 5 shows an example of an implementation of the control circuit 2 and the module 1. For simplicity, a single MOS element 11 is shown in Fig. 5. However, instead of one MOS element 11, several MOS elements 11 may be connected in parallel. In this example, the control circuit 2 further comprises an analog-to-digital converter (ADC) 25 associated to the control unit 23 and a switch 26 configured to control the powering of the MOS element 11 by the current source 22 and controlled by the control unit 23 via a control line CTRL2.
[0028] Electrical isolation may also be provided between the switch 26 and the ADC 25, and / or between the ADC 25 and the control unit 23, and / or between the signal lines CTRL1 and CTRL2.
[0029] The first series of operations I is for example executed by the control circuit 2 and in particular driven by its control unit 23. The control unit 23 may include a central processing unit (CPU) and / or a logic port and / or a field programmable gate array (FPGA).
[0030] The first series of operations I a. A positive current I from the emitter / source of module 1 to the gate g,ref , and an initial gate-emitter / source voltage V 0,ref is the flat band voltage V fb and b. The voltage across the current source, V ig,ref Measuring (t); and c. The voltage of module 1 is the flat band voltage V fb When the current I g,ref and ceasing the infusion of Includes.
[0031] In one embodiment in which the first series of operations I is performed by the control circuit 2, the voltage V across the current source ig,ref The measurement of (t) is performed by a voltage measuring means. The current I g,ref The condition can be monitored and detected by the control unit 23 via the ADC 25 of the control circuit 2, or a condition can be imposed for a certain time, for example 2 μs, before stopping the injection of the current. fb , the control unit 23 sends a control signal to the switch 26 of the control circuit 2 to close the switch 26 so that the current source 22 stops supplying power to the MOS device 11.
[0032] A first series of operations I is performed at a known average temperature of the module 1, for example the maximum nominal average temperature of the module 1 during its operation, thereby making it possible to obtain a measurement value of said average temperature. In the following example, the average temperature is 135° C., said temperature being adapted depending on the functionality of each architecture of the module 1 and the operating circumstances (application and design). Optionally, the first series of operations can be repeated at different known average temperatures of the module 1 in order to obtain a number of measurement sets, each related to a known average temperature.
[0033] Thereafter (or before), a second series of operations II is performed. The second series of operations II is substantially similar to the first series I, but is performed while the MOS elements are in an unknown state or at least during an operating state in which the temperature non-uniformity within the module 1 is desired. Preferably, the average temperature of the module 1 is known.
[0034] The second series of operations II d. A positive current I flows from the emitter / source of module 1 to the gate. g,op (Typically, the injection current I of the first series I g,ref (equal to the gate-emitter / source initial voltage V 0,op is the flat band voltage V fb and e. Voltage across the current source V ig,op Measuring (t); and f. The voltage of module 1 is the flat band voltage V fb When the current I g,op and ceasing the infusion of Includes.
[0035] In one embodiment in which the second series of operations II is performed by the control circuit 2, the voltage V across the current source ig,op The measurement of (t) is performed by a voltage measuring means. The current I g,op The condition can be monitored and detected by the control unit 23 via the ADC 25 of the control circuit 2, or a certain time, e.g. 2 μs, can be imposed before stopping the injection of . The condition is met (the voltage of the module 1 exceeds the flat band voltage V fb , the control unit 23 sends a control signal to the switch 26 of the control circuit 2 to close the switch 26 so that the current source 22 stops supplying power to the MOS device 11.
[0036] During the second series of operation II, during the operation of the MOS device, especially at the maximum operating point, the junction temperature may be different on a particular power semiconductor surface or on multiple dies in parallel. Therefore, the measured voltage V across the current source ig,op (t) differs from the measurements taken during the first series of operations I. In other words, the waveforms as a function of time t are not equally shaped.
[0037] The operation of the module 1 can be driven by a central processing unit (CPU), preferably the same as during the first series of operations I, such as the control unit 23 of the control circuit 2 .
[0038] Then, the third series of operations III: g. The voltage V measured during one first series I ig,ref (t) and the voltage V measured during one second series II ig,op (t) and h. From the comparison, the temperature variance T across module 1 j,dev and estimating Includes.
[0039] The third series of operations III is performed by a processing unit, e.g. a calculation unit 24 of the control circuit 2. In the examples described here, the calculation unit 24 is considered to be separate from the control unit 23 (see FIG. 5 ) in order to better understand their respective functions. In some embodiments, the calculation unit 24 may be part of the control unit 23 (integrated in the control unit 23) or may be structurally the same component, especially in embodiments in which isolation is provided between the control unit 23 and the ADC 25.
[0040] Voltage V ig,ref (t) and voltage V ig,opThe comparison of (t) is preferably made against a similar or close average temperature of the module 1. The aim is to identify the variation of the acquired voltage given the temperature gradient between the power semiconductor elements 11 or within the individual power semiconductor elements of the module 1. FIG. 6 shows an example of such a comparison. In the example of FIG. 6, the graph shows the difference in the acquired voltage (|V ig,ref (t)-V ig,op (t)|) as a function of time (t). In the example, all curves correspond to an average temperature of the module 1 of 130° C., and each curve corresponds to a temperature gradient between the power semiconductor elements 11 (here from 0° C. to 20° C. in steps of 2° C.).
[0041] In one example, the junction temperature dispersion T j,dev The estimation of voltage V ig,ref (t) and V ig,op (t) multiplied by a given coefficient K, e.g. K=11800° C. / V, calculated from a simulation of the flatband behavior. This is shown in FIG.
[0042] The graphical representation of the comparison in FIG. 7 is merely an example to aid the reader in understanding, and the method is not limited to any particular method of performing such a comparison; the comparison may be made solely by measured numerical data and / or graphical analysis.
[0043] The temperature distribution in a semiconductor region or an array of semiconductor elements 11 connected in parallel can be estimated using a unique index (the voltage across a current source). No individual access is required. Moreover, the estimation is performed in the most critical operating conditions.
[0044] Voltage V ig,ref (t) and V ig,op The comparison of (t) is preferably performed against a similar or close average temperature of the module 1. To ensure this, each of the at least one first series I and at least one second series II is i. Average temperature of module 1 T av,ref and T av,op The method further includes obtaining the
[0045] The second series II is the average temperature T obtained during at least one of the first series. av,ref and the average temperature T obtained during the second series av,op The difference between the two is a given value ΔT lim This is repeated until the following is true:
[0046] For example, the average temperature can be determined as a function of the internal gate resistance using a TSEP-based method known per se. Such a method is described in the non-patent document 1. The voltage V ig,ref (t) or V ig,op The measurement at (t) represents the average junction temperature. In fact, the initial voltage immediately after current injection is g,in This method is known to represent the average junction temperature. V ig,ref (t1) or V ig,op (t1) can be correlated to the junction temperature between the first series I and the second series II.
[0047] Advantageously, the temperature non-uniformity is calculated without knowing the operating point of the power semiconductor. g By using the above, a specific circuit is sufficient to measure the average and the variance of the junction temperature in a specific power semiconductor or in a parallel power semiconductor element 11.
[0048] In some embodiments, V ig,ref The first series I of operations to obtain V(t) is performed when the module 1 is in a reference state and not in an operational condition (typically in a laboratory, in a production calibration phase, or in a maintenance state). The first series I is performed to obtain V(t) under various temperatures. ig,refIt can be repeated (N times) at different temperatures to obtain a measurement of (t). In such a condition, the temperature is independent of the operating conditions and can be selected / driven. For example, an external heating element such as a heating plate can be disposed in the vicinity of the module 1. In another example, the temperature of a heat sink on which the power die is attached can be selected / driven.
[0049] When the first series of operations I is performed in non-operating conditions, the temperature variance is estimated with good accuracy for any average temperature during use of the power module.
[0050] This is shown in Figure 8. In the first loop 81, V ig,ref is the first average temperature T av,ref,y The above temperatures are measured in a situation where T is known to be uniform in module 1 (module 1 is offline). This means that it is the same at each junction of module 1 (T av,ref,y =T j1,dev =T j2,dev =...=T jN,dev ). Then each average temperature T av,ref,y+N for another average temperature T av,ref,y+1 The loop is repeated for Next, in substep 82, the average temperature T av,op is determined, for example, using a TSEP-based method, as a function of the internal gate resistance. Next, the voltage across module 1, V ig,op A measurement of (t) is performed (operation e corresponding to 83 in FIG. 8). Next, preferably, the determined average temperature T av,op The closest average temperature T av,ref,y The reference voltage V obtained ig,ref 8. Then, a comparison is performed with (operation g corresponding to 84 in FIG. 8). Then, the temperature variance T across module 1 is calculated as the minimum of the product of the coefficient K and the difference between the two voltages. j,dev (T j,dev =K·max(|V ig,op -V ig,ref|)) (operation h corresponding to 85 in FIG. 8).
[0051] In some other embodiments, V ig,ref The first series of operations I to obtain (t) is performed when the module 1 is in a reference state during an operating situation, at an early stage of its use, e.g., before a predetermined number of years of operation of the module 1 is reached. By way of example only, the predetermined number of years of operation can be set as a percentage of the target / nominal life limit (strictly less than 100%, e.g., 5%, 10%, or 20%), or as a number of hours, such as 1000 hours, 2000 hours, or 10000 hours, depending on the module, the operating conditions, and / or the target safety level. The first series I is performed to obtain V under various temperatures. ig,ref This can be repeated (N times) at different temperatures to obtain a measurement of (t). In such a condition, a set of measurements for different known temperatures can be obtained.
[0052] Here, we define the "initial phase" as the number of hours during operation. In such a case, a counter is installed in the control unit 23 that allows to define a limit of the time during which the first series is carried out. In our example, that number is set as 100 hours. Within this time, no degradation occurs on the power semiconductor packaging (module 1) and the temperature of the power semiconductor elements is considered to be uniform by design. The skilled person can adapt such a limit taking into account the context.
[0053] When the first series of operations I is performed at the initial stage of the operating situation, it is possible to extract the variation of temperature non-uniformity during operation in case of degradation of the power semiconductor elements. Furthermore, an optional commissioning phase is necessary before the use of the power semiconductors. As a result, V, which is used as a reference ig,ref (t) is generated during on-site application, reducing manufacturing complexity.
[0054] In some embodiments, the third series III is subjected to, prior to comparison, g'. The voltage V measured during at least one first series I ig,ref For the waveform of (t), the voltage V measured during at least one second series II ig,op (t) in time and offset.
[0055] Such behavior can be explained by the principle that the flatband voltage varies in time and voltage amplitude depending on the drain-source voltage and / or the average temperature. However, it does not affect the shape of the waveform. An example of an algorithm to perform the offset and time shift is shown in Figure 9. The algorithm searches for the instant t3 at which the waveform has the same amplitude for the first time. For this purpose, the algorithm first calculates, in step 91, the amplitude of V ig,op (t0), V ig,ref Then, proceed to step 92 or 93 accordingly to search for a voltage where Vx(t0) is equal to Vy(t3) (in step 92, Vx is V ig,op and Vy is V ig,ref (and vice versa in step 93). Thus, the time delay t3 is ig,op (t0)=V ig,ref Based on the maximum Vx(t0) that ensures that Vx(t0) is equal to Vx(t0), the smaller amplitude waveform can be compensated. The algorithm then proceeds to step 94 where the amplitude offset is removed. The offset is V ig,ref (t) is defined as the voltage difference at time t2 located in the middle of the plateau of the waveform, e.g., 1 μs. If this offset is small enough, e.g., 4 mV, the algorithm has converged the waveform, otherwise the algorithm returns to step 91. The algorithm can be stopped after multiple iterations. Experiments show that five iterations are sufficient. Figures 10 and 11 show the measured voltage V before and after the adjustment operation, respectively. ig,op (t), and then the function Adj(V ig,op In these figures, V ig,op (t) and V ig,refThe difference between Adj(Vt) and Adj(Vt) is obtained at different bus voltages and average junction temperatures in the absence of non-uniformity. As will be demonstrated, this adjustment makes it possible to remove offsets and delays introduced by external factors such as average temperature or drain-source voltage. Since only temperature non-uniformity changes the shape of the waveform, “Adj(Vt)” is a linear function of “Adj(Vt).” ig,op (t))" and V ig,op The difference between (t) gives the same difference as shown in Figure 6, and the result is utilized in Figure 7 by taking the maximum value. The variation obtained after adjustment as a function of the standard deviation of the junction temperature is shown in Figure 12. In such an example, the temperature gradient can be obtained using the coefficient K = 1650 °C / V.
[0056] In some embodiments, V ig,ref A single measurement of (t) is made. An arbitrary average junction temperature is determined. This shortens the time for post-manufacture calibration of the module.
[0057] In some embodiments, each first series I is executed when the power delivered by module 1 is below a predefined limit below the nominal maximum load of module 1. By way of example only, the predefined limit can be set as a percentage of the target / nominal maximum load (strictly less than 100%, e.g. 5%, 10% or 20%). In various embodiments, the limit condition is set as a maximum allowed power dissipation, such as 5%, 10% or 20% of the nominal maximum power dissipation, depending on the module, the operating conditions and / or the target safety level. A combination of such limits can be implemented. For example, the predefined condition can be set in the control unit 23 to: ig,ref The acquisition of (t) can be triggered. The following conditions give good results: The power semiconductor element is not switching and has a non-zero drain-source voltage V ds , or a non-zero collector-emitter voltage V ce exists across both ends of the power semiconductor element, or When a non-zero drain-source or collector-emitter voltage exists across the power semiconductor devices and the last device is switching, a small collector-emitter current I ce or a small drain-source current I ds flows through the power semiconductor element.
[0058] V ce Or V ds Measure the voltage V ig,ref (t) can be stored in a table linked to (t). In such a case, the obtained V ig,ref V ce Or V ds When it is equal to or close to, a comparison (operation g) can be made.
[0059] Advantageously, the voltage V ce and voltage V ds The sensitivity of the flatband voltage to the input current can be compensated for, and the degradation of the flatband caused by charge build-up on the gate oxide is also compensated for.
[0060] {theory} Flat band voltage V fb represents the voltage applied to the gate when there are no charges in the oxide or at the oxide-semiconductor interface that would result in flat-band energy in the semiconductor. The voltage is the difference between the work function of the gate metal and the work function of the semiconductor. The work function is the voltage required to pull an electron from the Fermi energy to the vacuum level. This voltage separates the accumulation mode from the depletion mode of the MOS (metal oxide semiconductor) structure. During accumulation mode, the MOS capacitance C is related only to the oxide capacitance. During depletion mode, the MOS equivalent capacitance is the oxide capacitance plus the variable capacitance of the depletion layer C eq It is a series connection with.
[0061] In operation, power semiconductors are typically coupled to a positive voltage V ge (e.g., 15V) and a negative voltage V ge The LEDs are operated by a master controller that alternates between on-state and off-state modes by applying a minimum of 10 V (e.g., −15 V) to the LEDs, respectively.
[0062] Here, the temperature dispersion is the voltage V that the MOS capacitor experiences when it is at a voltage higher than the MOS flat band voltage (e.g., about -2V). ge A low amplitude current source (e.g., 1mA to 100mA) is applied to the ge The flat-band voltage V varies between the power semiconductor standard and a known range, typically contained within, for example, -10V to -3V. fb This is measured by considering the change in the gate-emitter voltage behavior when discharging a MOS capacitor until the gate-emitter voltage V V of the IGBT is lower than ge The flat-band characteristic can be seen in Figure 1. Discharging a MOS capacitor shows a plateau in the flat-band voltage, which can be easily identified and depends on the junction temperature. The flat-band voltage V fb and junction temperature T j This particular relationship between the temperature variance T as a function of the voltage variance j,dev This makes it possible to estimate
[0063] The flat band voltage V of a die (or any semiconductor device) fb To determine this, the input impedance of the power semiconductor element is calculated using the equivalent capacitor C eq Therefore, the charge Q injected into the gate of the power semiconductor element can be modeled as t Since the amount of (see equation (1)) is controlled and proportional to the equivalent capacitance (see equation (2)), the current source I g It is advantageous in this method to use
number
[0064] Q n is the charge stored in the nth semiconductor, t0 is the initial time, and t is the current time. The equivalent capacitor C eq depends on each flat band voltage Vnfb, so the voltage V igMeasurement of the voltage V obtained at a uniform temperature makes it possible to determine the equivalent capacitor coefficient at each instant of time t. ig Using the voltage V obtained in the unknown state, ig By comparing with the flat band voltage V fb Therefore, to extract the flat-band inhomogeneity related to the temperature inhomogeneity, the variation of V ig A method is proposed here to investigate the variation of [Industrial Applicability]
[0065] The technical solution presented herein is used to estimate the junction temperature dispersion (temperature non-uniformity) of at least one MOS type power semiconductor or parallel connected MOS type power semiconductors by using a flatband voltage measurement method on the parallel gate / source-emitter accesses of the parallel power elements to identify the signatures of the individual flatband voltages and thus estimate the individual junction temperatures. Since the flatband voltage signatures are also affected by the operating points (e.g. drain-source / collector-emitter voltages) of the power semiconductor elements, the individual temperatures are estimated in relative values.
[0066] Advantageously, the temperature distribution within a semiconductor region or an array of semiconductors connected in parallel can be estimated using a unique indicator (the voltage across a current source), thus eliminating the need for any individual access.
[0067] The present disclosure is not limited to the methods, modules, components, and computer software described herein, which are merely examples, and the present invention encompasses all alternatives that one of ordinary skill in the art would contemplate upon reading this document. [Explanation of symbols]
[0068] 1: Module 2: Control circuit 11: Element 21: Voltage source 22: Current source 23: Control unit 24: Computational unit 25: Analog-to-Digital Converter (ADC) 26: Switch 81: Loop 82: Substep 83: Operation 84: Operation 85: Operation
Claims
1. 1. A method of measurement for estimating a temperature of a power semiconductor module comprising a single metal-oxide semiconductor, a single metal-insulator semiconductor, or a set of parallel-connected metal-oxide semiconductors or metal-insulator semiconductors, the method comprising: a. A positive current I flows from the emitter / source of the power semiconductor module to the gate. g,ref and injecting an initial voltage V between the gate and the emitter / source of the power semiconductor module. 0,ref is the flat band voltage V fb and b. The voltage across the current source, V ig,ref (t); and c. The voltage of the power semiconductor module is the flat band voltage V fb When the current I g,ref and ceasing the infusion of at least one first series of operations while the power semiconductor module is in a reference state, d. A positive current I flows from the emitter / source of the power semiconductor module to the gate. g,op and injecting an initial voltage V between the gate and the emitter / source of the power semiconductor module. 0,op is the flat band voltage V fb and e. The voltage across the current source, V ig,op (t); and f. The voltage of the power semiconductor module is the flat band voltage V fb When the current I g,op and ceasing the infusion of at least one second series of operations while the power semiconductor module is in an operational state, Next, g. The voltage V measured during one of the first series ig,ref (t) and the voltage V measured during one of the second series ig,op (t) and h. From the comparison, the temperature dispersion T across the power semiconductor module j,dev and estimating At least one third series of operations, including: A method comprising:
2. Each of the at least one first series and the at least one second series comprises: i. The average temperature T of the power semiconductor module av,ref and T av,op [0023] The second series includes at least one of the average temperatures T obtained during the first series. av,ref and the average temperature T obtained during the second series av,op The difference between the two is a predetermined value ΔT lim The method of claim 1 , wherein the method is performed repeatedly until:
3. The first series of multiple temperatures have different average temperatures T av,ref,n It is executed in the first series being performed during a state different from an operational state of the power semiconductor module; The method of claim 2.
4. The first series of multiple temperatures have different average temperatures T av,ref,n It is executed in each of the first series is performed during a reference and operational state of the power semiconductor module and before a predetermined operational deadline in the operation of the power semiconductor module is reached; The method according to any one of claims 1 to 3.
5. The third series, prior to the comparison, g'. The voltage V measured during at least one of the first series ig,ref For the waveform of (t), the voltage V measured during at least one of the second series ig,op (t) in time and offset The method of any one of claims 1 to 3, further comprising:
6. 6. The method according to claim 5, wherein each of the at least one first series is executed when the power delivered by the power semiconductor module is below a predetermined limit that is below a nominal maximum load of the power semiconductor module.
7. 4. A power semiconductor module comprising a single metal oxide semiconductor, a single metal insulator semiconductor, or a set of parallel connected metal oxide semiconductors or metal insulator semiconductors and configured to perform the method according to any one of claims 1 to 3.
8. Computer software comprising instructions for carrying out the method of any one of claims 1 to 3 when said computer software is executed by a processor.
9. A non-transitory computer readable recording medium having stored thereon software which, when executed by a processor, performs the method according to any one of claims 1 to 3.
Citation Information
Patent Citations
Charge-up evaluation element
JP1996298276A
Method and apparatus for evaulating semiconductor
JP1997306962A
Method and device for testing semiconductor device
JP2009194218A
Compound semiconductor device and manufacturing method of the same
JP2014063917A