Warp-direction elastic nonwoven fabric and its manufacturing equipment
The innovative manufacturing process for nonwoven fabrics uses differential gears and wind suction gears to form uniform wrinkles, achieving a single-layer elastic fabric with improved warp direction elasticity, addressing issues of bulkiness and cost in conventional methods.
Patent Information
- Application Number
- JP2024002703U
- Authority / Receiving Office
- JP · JP
- Patent Type
- Utility models
- Current Assignee / Owner
- Priority Date
- 2024-04-19
- Filing Date
- 2024-08-13
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2034-08-13
AI Technical Summary
Conventional methods for producing elastic nonwoven fabrics face issues such as uneven wrinkling, bulkiness, increased costs, and reduced user comfort due to the need for lamination and adhesive bonding, which also leads to peeling and uneven fabric surfaces.
A manufacturing process using a specialized equipment with differential gears and wind suction gears to form uniform waving wrinkles on nonwoven fabrics, followed by heating, stretching, and cooling to create a single-layer elastic nonwoven fabric with improved warp direction elasticity, eliminating the need for additional layers and bonding.
The process results in a flat-surfaced, highly elastic nonwoven fabric with enhanced warp direction resilience, reducing manufacturing costs, improving user comfort, and minimizing storage and transportation space requirements.
Smart Images

Figure 0003248704000001_ABST
Abstract
Description
[Technical field]
[0001] This invention relates to a warp-direction elastic nonwoven fabric in which wavy wrinkles are formed, then heat-softened, stretched in the weft direction, and cooled to set, thereby changing the direction of the nonwoven fiber, imparting elasticity, and smoothing out the wavy wrinkles, and to a method for manufacturing the same. [Background technology]
[0002] Common sanitary products, such as masks, washless pants, baby diapers, adult diapers, kinesio tape, medical bandages, etc., are generally disposable products in order to avoid contamination by pathogens or harmful substances, considering hygiene and safety in use. Since these products are in contact with the skin for a long time, the requirements for breathability are relatively strict to prevent discomfort due to stuffiness or dampness, or skin allergies, itching, and even rashes.
[0003] Nonwoven fabrics made of plastic materials are widely used in sanitary products due to the advantages of easy production and processing, good chemical resistance, good durability, and low cost. However, nonwoven fabrics have relatively poor extensibility, lacking comfort and covering performance, which causes inconvenience when worn (e.g., diapers). Therefore, those skilled in the art have developed composite nonwoven fabrics that can improve extensibility, so to speak, called elastic composite nonwoven fabrics. In the conventional method of producing elastic composite nonwoven fabrics, a sheet of elastic material is stretched as an intermediate layer, and then two sheets of non-elastic normal nonwoven fabrics are laminated as upper and lower layers, respectively, like a sandwich, and after lamination, the application of external force for stretching is stopped to form wavy wrinkles on the upper and lower surfaces of the elastic composite nonwoven fabric. Another commonly used method is to use a layer of elastic material as the middle layer when not stretched, and then sandwich two non-elastic regular nonwoven fabrics together as the top and bottom layers, forming a flat three-layer structure. After bonding, the material surfaces of the regular nonwoven fabrics are destroyed (e.g., activated) to give the regular nonwoven fabric a little extensibility.
[0004] However, the lamination process not only adds a step to the manufacturing process, but also makes the nonwoven product thicker, less comfortable for the user, and increases the space and cost required for storage and transportation. In addition, the product may peel off due to incomplete lamination. Furthermore, when adhesive is used for lamination, the uneven distribution of the adhesive may easily cause peeling.
[0005] In other prior art, elastic materials are used as raw materials to manufacture single-layer elastic nonwoven fabrics through nonwoven fabric manufacturing processes such as meltblown or spunbond, but the cost is very high. Therefore, the present invention aims to develop an elastic nonwoven fabric that imparts elasticity to a single-layer nonwoven fabric only through the thermoplasticity of man-made fibers, thereby greatly reducing costs.
[0006] In addition to the spunbond method, other conventional nonwoven fabric manufacturing methods include spunlace, needle punch, hot melt, etc. In the spunbond method, raw materials are melted through an extrusion facility and extruded from a nozzle, stretched through an air passage, cooled to form ultrafine fibers, sprayed onto a collection net to deposit in a mesh structure, and the long fibers in the random mesh structure are passed through a heated roller to be thermocompressed into a fiber layer.
[0007] Due to the thermoplasticity of nonwoven fabrics made of plastic materials (the property of softening when heated and hardening after cooling) and the dispersed non-orientation of the fiber structure of ordinary nonwoven fabrics (as shown in Figure 1a, the fiber structure 11 of the nonwoven fabric is randomly oriented), the fibers can be heated to the corresponding softening temperature by penetrating the fiber structure using a hot air flow, and the dispersed fibers are mechanically stretched continuously in the weft direction while being heated and softened, thereby changing the forward direction of the fiber structure (the nonwoven fabric in Figure 1a is stretched along the weft direction, so that the fiber structure 11 is oriented along the weft direction to the state shown in Figure 1b, and the nonwoven fabric is necked along the warp direction).
[0008] Since the fiber direction in the fiber structure 11 of the nonwoven fabric provides the source of elasticity, after the elastic nonwoven fabric that has been heat-softened and stretched along the weft direction is cooled, its fiber structure is formed into the shape of a telescopic robot arm as shown in FIG. 1b. When a stretching force is applied in the warp direction, the fiber structure 11 oriented along the weft direction of the nonwoven fabric (as shown in FIG. 1b) can be stretched in a state in which the forward direction of the fibers is not changed along the warp direction (as shown in FIG. 1a), so it has warp extensibility. In addition, after the application of the stretching force in the warp direction is stopped, the fiber structure 11 of the elastic nonwoven fabric returns to a state in which it is oriented along the weft direction again (as shown in FIG. 1b), so it has warp recovery. In other words, such an elastic nonwoven fabric has elasticity that can be stretched and restored in the warp direction.
[0009] On the other hand, Figures 2a and 2b show microscopic images of a conventional spunlace nonwoven fabric before and after it is stretched in the weft direction, respectively, and show how the fiber structure of the nonwoven fabric is oriented along the weft direction after it is stretched.
[0010] In addition, after mechanically stretching the nonwoven fabric in the weft direction, necking deformation (as shown in the necking region N in Figure 3) occurs, and the area of the nonwoven fabric material in the warp direction shrinks due to the Poisson's effect. Therefore, by overfeeding the nonwoven fabric in the warp direction in advance (i.e., the fabric feeding speed is faster than the needle chain operating speed), the nonwoven fabric is made wavy and the tension in the warp direction of the fabric is reduced. This compensates for the necking phenomenon and makes it advantageous to expand the weft direction to avoid the nonwoven fabric becoming too thin due to the necking phenomenon after stretching.
[0011] However, due to the conventional overfeeding performed simply in a differential manner, the nonwoven fabric has uneven wavy wrinkles, and the fabric surface becomes uneven after being spread in the weft direction. Therefore, there is a need for an improved method for producing elastic nonwoven fabrics. Summary of the Invention [Problem to be solved by the invention]
[0012] In view of the problems faced by the prior art, the present invention aims to provide a method for producing a warp elastic nonwoven fabric and a single-layer elastic nonwoven fabric produced by the method. The method for producing warp elastic nonwoven fabric can pre-form uniform wavy wrinkles on the nonwoven fabric and combine with an air suction device to compensate for the phenomenon of the area shrinkage or thickness thinning of the nonwoven fabric caused by necking in the subsequent stretching, and improve the unevenness of the conventional overfeed method. The elastic nonwoven fabric itself has strong resilience in the warp direction and a flat surface, so that it can be directly used in products without being bonded to another elastic substrate, greatly improving the production rate, improving the comfort of users, and reducing the space and cost of storage and transportation. [Means for solving the problem]
[0013] In order to solve the above problems, the present invention provides an elastic nonwoven fabric manufacturing equipment, the manufacturing equipment having an inlet, an internal space, and an outlet in the warp direction, the internal space being divided into a preheating section adjacent to the inlet, a width expanding section located in the middle, and a stabilizing section adjacent to the outlet along the warp direction, the internal space being in the form of a heating device, the conveyor being located on both sides of the heating device in the weft direction, and extending from the inlet of the heating device to the outlet along the warp direction through the preheating section, the width expanding section, and the stabilizing section in that order, and each of the plurality of needles is installed. At least two needle chains are connected to the heating device, at least two feed gear sets are respectively installed above the needle chains at the inlet of the heating device, and at least two roll brushes are respectively installed above the needle chains downstream of the feed gear sets in the radial direction, each of the feed gear sets includes a differential gear and a wind suction gear which mesh with each other, each of the differential gears has a plurality of first teeth and a plurality of first grooves which are offset along the outer circumferential surface of the differential gear, and the wind suction teeth are arranged in a direction parallel to the outer circumferential surface of the differential gear. A hollow groove is provided in the center of the latitudinal direction on the outer surface of each of the wheels, and each of the plurality of wind suction gears has a plurality of second teeth, a plurality of second grooves, and a plurality of wind suction holes on both sides of the latitudinal direction of the hollow groove, and the plurality of second grooves and the plurality of second teeth are arranged to be offset from each other along both sides of the latitudinal direction of the outer peripheral surface of the wind suction gear, and the plurality of wind suction holes are provided at least in the plurality of second grooves, and the plurality of differential gears move along the warp direction on both sides of the latitudinal direction of the nonwoven fabric at a feed speed higher than that of the plurality of needle chains. A plurality of differential gears and the plurality of wind suction gears are respectively fed between the plurality of differential gears and the plurality of wind suction gears, and the plurality of differential gears and the plurality of wind suction gears rotate while meshing with each other so that the plurality of first tooth portions are inserted into the plurality of second groove portions and the plurality of second tooth portions are inserted into the plurality of first groove portions, so that both sides in the weft direction of the nonwoven fabric are respectively bitten between the plurality of first tooth portions and the plurality of second groove portions, and between the plurality of first groove portions and the plurality of second tooth portions, thereby forming regular wavy wrinkles in the nonwoven fabric along the warp direction, and the plurality of wind suction gears are:By providing suction force through the plurality of wind suction holes, both sides of the nonwoven fabric in the weft direction are brought into close contact with the outer surfaces of the plurality of second tooth portions and the plurality of second groove portions, respectively. The plurality of hollow grooves are configured to pierce the plurality of needles into the nonwoven fabric fed by the plurality of needle chains when the plurality of wind suction gears rotate and operate in a conveyor manner, so that the nonwoven fabric is inserted into the plurality of hollow grooves, and the wavy wrinkles of the nonwoven fabric fed are fixed. The plurality of wind suction gears are configured to fix the wavy wrinkles of the nonwoven fabric fed by the plurality of needles when the plurality of needle chains rotate on the plurality of wind suction gears and operate in a conveyor manner. The suction force is stopped after the nonwoven fabric is pierced by the nonwoven fabric, and the nonwoven fabric is smoothly transferred from the plurality of wind suction gears to the plurality of needle chains. The plurality of roll brushes crush the wavy wrinkles of the nonwoven fabric on the plurality of needle chains by rotating the plurality of needle chains in a conveyor manner. The plurality of needle chains feed the nonwoven fabric having the crushed wavy wrinkles from the inlet of the heating device along a warp direction into the internal space of the heating device. In the preheating section, the plurality of roll brushes are rotated while the plurality of needle chains are operated in a conveyor manner. When the plurality of needle chains maintain a constant weft pitch, the nonwoven fabric is transported in the warp direction and heated by the heating device until the nonwoven fabric is softened. Then, in the widening section, the heating device continues to heat the nonwoven fabric, and when the weft pitch gradually widens, the plurality of needle chains transport the softened nonwoven fabric in the warp direction to stretch it in the weft direction, thereby generating a necking compensation action in the warp direction of the nonwoven fabric, flattening the wavy wrinkles that extend in the warp direction and are crushed, and smoothing the fibers of the nonwoven fabric. By orienting the fiber structure along the weft direction, the nonwoven fabric is in a flat state and has an elongation recovery force along the warp direction; then, in the stabilization section, the heating device continuously heats and the multiple needle chains stabilize the softened and stretched nonwoven fabric by transporting it along the warp direction while maintaining the expanded weft pitch; finally, the needle chains send the stabilized nonwoven fabric out of the heating device through the outlet, thereby cooling and setting the stabilized nonwoven fabric to form a warp-direction elastic nonwoven fabric.
[0014] In an embodiment of the present invention, the plurality of wind suction holes are further disposed in the plurality of second teeth.
[0015] In an embodiment of the present invention, the heating temperature of the heating device is 120°C to 180°C, preferably 130°C to 150°C.
[0016] In an embodiment of the present invention, the weft expansion ratio in the expansion section of the nonwoven fabric is between 15% and 100%.
[0017] In an embodiment of the present invention, the needles on the needle chain are each oriented toward a peak and / or a valley of the waviness.
[0018] In an embodiment of the present invention, the pitch between the first teeth, the pitch between the second teeth, and the pitch between the needles are 1:1:1 or 1:1:0.5.
[0019] In an embodiment of the present invention, the nonwoven fabric is made by a spunbonding process, a spunlace process, a thermal bonded process, a meltblown process, or a needle punching process.
[0020] In an embodiment of the present invention, the nonwoven fabric is made of a material selected from the group consisting of PP, PE, PET, PP / PE, PP / PET, or combinations thereof.
[0021] In order to solve the above problems, the present invention further provides a warp elastic nonwoven fabric having a flat surface and an elongation recovery force along the warp direction by having a fiber structure oriented essentially along the weft direction.
[0022] In an embodiment of the present invention, the warp direction elongation rate of the warp direction elastic nonwoven fabric is between 50% and 350%. Effect of the Invention
[0023] The effects of the present invention are: 1) by feeding the nonwoven fabric through the meshing differential gear and the wind suction gear, regular wavy wrinkles can be formed on the nonwoven fabric, which is advantageous for ensuring the flatness of the surface of the finished elastic nonwoven fabric; 2) by using the suction force of the wind suction gear to make the nonwoven fabric adhere to the outer surface of the teeth and grooves of the wind suction gear, the wavy wrinkles of the nonwoven fabric can be transferred directly to the subsequent manufacturing process, which is advantageous for improving the uniformity of the finished fabric surface; 3) by providing a hollow groove in the center of the outer surface of the wind suction gear, it is possible to provide an accommodation space after the needles on the needle chain are inserted into the nonwoven fabric; 4) by slightly stretching the weft direction during heating to change the forward direction of the fibers, and then cooling and setting, it is possible to make the nonwoven fabric contain elasticity in the warp direction that is superior to that of the prior art; 5) by forming uniform wavy wrinkles in advance, it is possible to compensate for the phenomenon of the nonwoven fabric shrinking in area or thinning due to necking in the subsequent stretching operation. Sixth, by making the single-layer nonwoven fabric have excellent elasticity after processing, it is possible to eliminate the need for extra lamination materials and lamination steps, thereby reducing production costs, making the product thinner and improving user comfort, and reducing the space and costs required for storage and transportation.
[0024] The effects of the present invention are not limited to those described above, and those skilled in the art can clearly understand other effects not mentioned in the claims. [Brief description of the drawings]
[0025] [Figure 1] (a) shows an image (taken with a handheld low-noise, high-resolution digital microscope) of a typical spunbond nonwoven fabric before it is stretched in the weft direction, and (b) shows an image (taken with a handheld low-noise, high-resolution digital microscope) of a typical spunbond nonwoven fabric after it is stretched in the weft direction. [Diagram 2](a) shows an image (taken with a handheld low-noise, high-resolution digital microscope) of a normal spunlace nonwoven fabric before it is stretched in the weft direction, and (b) shows an image (taken with a handheld low-noise, high-resolution digital microscope) of a normal spunlace nonwoven fabric after it is stretched in the weft direction. [Diagram 3] 1 is a perspective view showing a manufacturing equipment for a warp-direction elastic nonwoven fabric according to the present invention. [Figure 4] 1 is a schematic diagram showing a needle entering a hollow groove in the manufacturing equipment of the present invention (nonwoven fabric not shown). [Figure 5a] FIG. 1 is a schematic diagram showing how wavy wrinkles caused only by a differential gear having a flat surface are crushed by a roll brush in a setting machine of the prior art. [Figure 5b] 1 shows a differential gear of a prior art setting machine. [Figure 6] 1A is a schematic diagram showing uneven wavy wrinkles caused by a setting machine of the prior art, and FIG. 1B is a schematic diagram showing uneven wavy wrinkles caused by a setting machine of the prior art being crushed by a roll brush. [Figure 7] FIG. 2 is a schematic diagram showing the ripples caused by a feed gear set including a gear-type differential gear and a wind suction gear being crushed by a roll brush in the manufacturing equipment of the present invention. [Figure 8] 1A is a schematic diagram showing uniform wavy wrinkles produced by the manufacturing equipment of the present invention, and FIG. 1B is a schematic diagram showing the uniform wavy wrinkles produced by the manufacturing equipment of the present invention being crushed by a roll brush. [Figure 9] (a) shows a photograph of a finished woven fabric produced using a prior art setting machine, and (b) shows a photograph of a finished nonwoven fabric produced using the manufacturing equipment of the present invention. [Figure 10] 1 shows a flow chart of a method for producing a warp elastic nonwoven fabric of the present invention. [Figure 11] FIG. 1 is a schematic diagram showing the appearance of a warp-direction elastic nonwoven fabric according to the present invention. [Figure 12] FIG. 12 is an enlarged view of a portion of region a in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] The advantages and features of the present invention and the implementation method thereof will be more clearly understood with reference to the following embodiments illustrated in the accompanying drawings. However, the present invention is not limited to the following embodiments, and may be implemented in various different forms.
[0027] Where no contradiction arises, any technical feature in any aspect of the present invention may be combined with any other aspect of the present invention.
[0028] As used herein, "machine direction (MD)" means the direction parallel to the direction in which the manufacturing equipment transports the nonwoven fabric, also called the machine direction, and "transverse direction (TD)" means the direction perpendicular to the direction in which the manufacturing equipment transports the nonwoven fabric.
[0029] As used herein, "broaden ratio" refers to the ratio of the final elongation that a material (e.g., a raw nonwoven fabric) is stretched from its original width during the broadening step to the original width of the material.
[0030] As used herein, "Elongation" refers to the ratio of the maximum extension that a material (eg, a warp elastic nonwoven) can be stretched from its natural width to the natural width of the material.
[0031] Referring to FIG. 3, the present invention provides a manufacturing equipment for warp elastic nonwoven fabric, which includes a heating device 60, a conveyor-type needle chain 40, a feed gear set F, and a roll brush 50.
[0032] The heating device 60 has an inlet 61, an internal space 62, and an outlet 63, which are arranged in the warp direction, and the internal space 62 is divided in the warp direction into a preheating section 62a adjacent to the inlet 61, an expansion section 62b located in the middle, and a stabilization section 62c adjacent to the outlet 63.
[0033] In the present invention, the heating device 60 can be used to heat and soften the nonwoven fabric for processing modeling, and the heating device 60 can be, for example, but not limited to, an oven. The inner space 62 of the heating device 60 is the space that is actually heated, but the inlet 61 and outlet 63 of the heating device 60 can be designed to be heated or not heated as required.
[0034] Since the nonwoven fabrics 10 of different components have different softening points, the heating temperature of the heating device 60 may be between 120°C and 180°C, preferably between 130°C and 150°C.
[0035] The number of needle chains 40 is at least two, one located on each side of the heating device 60 in the weft direction, and extending from an inlet 61 of the heating device 60 in the warp direction to an outlet 63 via a preheating section 62a, a widening section 62b, and a stabilizing section 62c in that order. Each needle chain 40 has a plurality of needles 41 installed thereon.
[0036] Referring to FIG. 3, the number of the feed gear sets F is at least two, which are installed above the needle chains 40 on both sides at the inlet 63 of the heating device 60, respectively.
[0037] Each feed gear set F includes a differential gear 20 and a wind suction gear 30 which mesh with each other.
[0038] Each differential gear 20 has a plurality of first teeth 21 and a plurality of first grooves 22 that are arranged in a staggered manner along the outer circumferential surface of the differential gear 20 .
[0039] Referring to FIG. 4, a hollow groove 34 is provided in the latitudinal center of the outer surface of each wind suction gear 30. Each wind suction gear 30 has a plurality of second teeth 31, a plurality of second grooves 32, and a plurality of wind suction holes 33 on both latitudinal sides of the hollow groove 34. The plurality of second grooves 32 and the plurality of second teeth 31 are arranged staggered along both latitudinal sides of the outer peripheral surface of the wind suction gear 30, and the wind suction holes 33 are provided in at least the second grooves 32.
[0040] Referring to FIG. 3, the number of roll brushes 50 is at least two, and each roll brush 50 is disposed above each needle chain 40 downstream of each feed gear set F in the radial direction.
[0041] In the manufacturing equipment of the present invention, preferably, the plurality of needle chains 40, the plurality of feed gear sets F, and the plurality of roll brushes 50 are configured symmetrically to each other on both sides of the weft direction of the heating device 60, so as to ensure smooth transportation of the nonwoven fabric and to avoid the phenomenon of the nonwoven fabric being pulled or unevenly processed.
[0042] In addition, in the specification of the present invention, a configuration of two needle chains 40, two feed gear sets F, and two roll brushes 50 is described as an example, but as can be understood by those skilled in the art, additional needle chains 40, feed gear sets F, and roll brushes 50 can be appropriately added between the above elements in order to balance product needs, equipment costs, and processing precision.
[0043] In this invention, a normal nonwoven fabric 10 is processed using equipment for manufacturing warp elastic nonwoven fabrics, and after heat softening, stretching in the weft direction, and cooling and setting (stabilizing the shape of the nonwoven fabric), the fiber direction is changed and the fabric is oriented in the weft direction to impart warp elasticity.
[0044] Preferably, nonwoven fabric 10 includes, but is not limited to, nonwoven fabrics made by spunbond, spunlace, thermal bond, meltblown, or needlepunch processes.
[0045] In order to meet the required softening-when-heated and setting-when-cooled properties of the manufacturing process, the nonwoven fabric 10 employed in the present invention is made of a thermoplastic material, such as, but not limited to, polypropylene (PP), polyethylene (PE), polyethylene terephthalate (PET), bicomponent PP / PE, bicomponent PP / PET, or combinations thereof.
[0046] The operation of the equipment for manufacturing warp-directional elastic nonwoven fabric of the present invention will be described below.
[0047] First, the differential gear 20 feeds both sides of the weft direction of the nonwoven fabric 10 between the differential gear 20 and the wind suction gear 30 in the warp direction at a higher feed speed than the needle chain 40 (i.e., in an overfeed manner). The differential gears 20 and the wind suction gears 30 rotate while meshing with each other so that the first tooth portion 21 is inserted into the second groove portion 32 and the second tooth portion 31 is inserted into the first groove portion 22, so that both sides of the weft direction of the nonwoven fabric 10 are respectively bitten between the first tooth portion 21 and the second groove portion 32, and between the first groove portion 22 and the second tooth portion 31, thereby forming regular wavy wrinkles in the nonwoven fabric 10 in the warp direction.
[0048] Next, the wind suction gear 30 provides suction force through wind suction holes 33 installed at least in the second groove portion 32, thereby adhering both sides of the weft direction of the fed nonwoven fabric 10 to the outer surfaces of the second tooth portion 31 and the second groove portion 32, respectively.
[0049] Preferably, in order to enhance the effect of closely adhering the nonwoven fabric 10 to the outer surface of the second tooth portion 31 and the second groove portion 32 of the gear 30, an air suction hole 33 may be further provided in the second tooth portion 31.
[0050] Thereafter, the hollow groove 34 of the wind suction gear 30 is configured so that when the needle chain 40 rotates on the wind suction gear 30 and operates in a conveyor manner, the needles 41 of the needle chain 40 are inserted into the fed nonwoven fabric 10, the nonwoven fabric 10 is inserted into the hollow groove 34, and the wavy wrinkles of the fed nonwoven fabric 10 are fixed.
[0051] In addition, the wind suction gear 30 stops providing suction force after the needles 41 have pierced the fed nonwoven fabric 10, thereby smoothly transferring the nonwoven fabric 10 from the wind suction gear 30 to the needle chain 40.
[0052] Next, the roll brush 50 rotates while the needle chain 40 operates in a conveyor manner, thereby squashing wavy wrinkles in the nonwoven fabric 10 on the needle chain 40. To ensure smooth processing, the height of the roll brush 50 is set so that the roll brush 50 can squash wavy wrinkles in the nonwoven fabric 10 fixed to the needle chain 40 when it rotates above the needle chain 40.
[0053] In addition, in order to crush wavy wrinkles in the nonwoven fabric 10 before the nonwoven fabric 10 is stretched and widened (described later), the specific position of the roll brush 50 may be set within the range of the softening section 62a of the heating device 60 from the radial downstream of the feed gear set F.
[0054] In the conventional technology, when a fabric is dyed with hot water, it shrinks. Therefore, a setting machine is used to expand the fabric during the high-temperature drying process to compensate for the shrinkage and set it, so that the width of the fabric surface is consistent and the linear arrangement of the warp and weft yarns is stabilized. In addition, by using overfeed technology, the arrangement of the warp and weft yarns can be more finely adjusted during the expansion so that the feel of the fabric surface can be adjusted.
[0055] The above-mentioned conventional techniques are applied to woven fabrics having warp and weft yarn arrangements, and in the woven fabric spread set manufacturing process using the overfeed technique, the conditions and adjustable ranges of the woven fabric fineness (tensile strength), warp and weft yarn arrangement (tensile strength of weave arrangement) and weave number (tensile strength of density) are fixed and cannot be adjusted more widely.
[0056] During the development of the present invention, it was found that when the above-mentioned conventional setting machine and overfeeding technology are applied to nonwoven fabrics, the fibers of nonwoven fabrics have a random arrangement, unlike woven fabrics with warp and weft yarn arrangements, so the widening effect of setting and the tightening effect of overfeeding are more pronounced. However, the overfeeding technology applied in the above-mentioned conventional technology lacks the design of the gears and wind suction device, which affects the uniformity of the nonwoven fabric (as shown in Figure 9a).
[0057] In the present invention, by improving the differential gear 20 and the wind suction gear 30, uniform wavy wrinkles can be formed on the nonwoven fabric 10 and then transferred to the needle chain as is, thereby avoiding the problems in the prior art in the widening set manufacturing process, such as uneven wavy wrinkles caused by fabric overfeeding performed simply in a differential manner, and uneven thickness of the finished fabric surface caused by widening in the weft direction.
[0058] As shown in Figures 5a and 5b, the prior art fabric setting machine only has a configuration in which a differential gear 20' is combined with a roll brush 50', and does not have an air suction gear. The belt roller group B' and the differential gear 20' overfeed the nonwoven fabric 10' and push it between the differential gear 20' and the roll brush 50', and the feed speed of the belt roller group B' and the differential gear 20' is greater than the feed speed of the needle chain 40', so an overfeed differential is formed, and the belt roller group B' and the differential gear 20' are used to sandwich the nonwoven fabric 10' and generate a differential push, thereby forming wavy wrinkles, and then the roll brush 50' is used to push the nonwoven fabric 10' into the needle chain 40'. Preferably, as shown in FIG. 5b, the differential gear 20' has a friction surface 20a' on one side of its circumferential surface, and a brush 20b' on the other side, and the brush 20b' on the differential gear 20' can also push the nonwoven fabric 10' into the needle chain 40'.
[0059] However, since the surface of the prior art differential gear 20' is flat and has no teeth, the friction force between the nonwoven fabric 10' can be provided only through the friction surface (eg, made of a rubber material).
[0060] As a result, the above configuration has a problem that the wavy wrinkles of the nonwoven fabric become irregular, and furthermore, after the fabric is expanded in the weft direction, the fabric surface becomes uneven. Specifically, as the differential gear 20' rotates, the needles 41' on the needle chain 40' penetrate and fix the irregular wavy wrinkles of the nonwoven fabric 10' as shown in FIG. 6a, and after the roll brush 50' further crushes the wavy wrinkles, only the nonwoven fabric 10' with the appearance of unevenly crushed wavy wrinkles is obtained as shown in FIG. 6b. Therefore, the subsequent manufacturing process cannot achieve uniform expansion, and the finished fabric surface becomes uneven.
[0061] 7 to 8b, the manufacturing equipment of the present invention differs from the prior art in that the present invention replaces the flat differential gear 20' of the prior art with a gear-type differential gear 20, and further includes a wind suction gear 30.
[0062] As the differential gear 20 and the wind suction gear 30 mesh and rotate, the nonwoven fabric 10 is wedged between the teeth and grooves of the differential gear 20 and the wind suction gear 30, causing the nonwoven fabric 10 to form regular wavy wrinkles along the warp direction.
[0063] Then, wind suction holes 33 are installed on the surface of the wind suction gear 30, and the suction force through the wind suction holes 33 causes the nonwoven fabric 10 to adhere to the outer surfaces of the second tooth portion 31 and the second groove portion 32 of the wind suction gear 30, temporarily fixing the wavy wrinkles of the nonwoven fabric 10 by the suction force, so that the wavy wrinkles of the nonwoven fabric 10 can be transferred as they are to the subsequent manufacturing process, which is advantageous for the fixing work by the subsequent needle chain 40, and by preventing the nonwoven fabric 10 from shifting in the subsequent manufacturing process, the evenness of the fabric surface of the finished nonwoven fabric can be improved.
[0064] Then, with the rotation of the wind suction gear 30, the wavy wrinkles of the nonwoven fabric 10 move up the needle chain 40, and while the needle chain 40 operates in the manner of a conveyor, the needles 41 on the needle chain 40 pierce and fix the regular wavy wrinkles of the nonwoven fabric 10 (as shown in FIG. 8a). Then, after the roll brush 50 further crushes the wavy wrinkles, a nonwoven fabric 10 with an appearance of uniform and crushed wavy wrinkles (as shown in FIG. 8b) can be obtained, so that a uniform width expansion can be realized in the subsequent manufacturing process to produce a warp elastic nonwoven fabric with a uniform fabric surface.
[0065] 9a and 9b show photographs of the finished fabric produced using the prior art manufacturing equipment and the finished nonwoven fabric produced using the manufacturing equipment of the present invention, respectively. When using the prior art differential gear 20', there are uneven wrinkles on the surface of the finished fabric, whereas when using the differential gear 20 and wind suction gear 30 of the present invention, the finished nonwoven fabric has a flat surface appearance.
[0066] Preferably, the degree of fixation of the needle chain 40 to the nonwoven fabric 10 can be increased by adjusting the pitch and arrangement density of the needles 41 on the needle chain 40.
[0067] Preferably, multiple sets of needle chains 40 are provided, and the number of teeth and the size of the needle pitch can be adjusted according to the need for elastic extension.
[0068] Preferably, the differential gear 20 and the wind suction gear 30 can be designed to have the same diameter and have the same number of teeth, so that the rotation speed ratio of the differential gear 20 and the wind suction gear 30 can be 1:1.
[0069] Preferably, compared with the prior art warp elastic nonwoven fabric manufacturing equipment, the number of teeth of the differential gear 20 and the wind suction gear 30 may be increased or decreased, or the overall structure may be replaced by a module, and the number and height of the tooth grooves may be combined correspondingly with the needle chain 40.
[0070] Preferably, the manufacturing equipment of the present invention may be designed such that the needles 41 are each aimed at the peaks and / or valleys of the ripples of the nonwoven fabric 10 (as shown in FIG. 8a), which can better fix the ripples in the subsequent manufacturing process.
[0071] Preferably, the pitch between the plurality of first tooth portions 21, the pitch between the plurality of second tooth portions 31, and the pitch between the plurality of needles 41 may be set to 1:1:1, thereby allowing the needles 41 to be directed toward each peak or valley of the ripples of the nonwoven fabric 10, respectively.
[0072] Alternatively, in a more preferred embodiment, the pitch between the first tooth portions 21, the pitch between the second tooth portions 31, and the pitch between the needles 41 may be set to 1:1:0.5, so that the needles 41 can be respectively directed to each peak and each valley of the ripples of the nonwoven fabric 10 (as shown in FIG. 8a).
[0073] Preferably, in the manufacturing equipment of the present invention, the height or width of the wavy wrinkles of the nonwoven fabric 10 can be adjusted by adjusting the height and width of the first tooth portion 21 and the second tooth portion 31, the width of the first groove portion 22 and the second groove portion 32, and the pitch between the differential gear 20 and the wind suction gear 30, that is, the shape of the wavy wrinkles of the nonwoven fabric 10 can be changed.
[0074] By varying the wavy shape of the nonwoven fabric, the thickness, warp elasticity and uniformity of the finished warp elastic nonwoven fabric can be adjusted.
[0075] The height and width of the wavy wrinkles and the spacing between the two gears are absolutely related to the evenness of the fabric surface. For example, when the number of teeth and the spacing between the gears are constant, if the weft width is wide, the spacing between the two gears is close (high wavy wrinkles), there are sufficient fibers stretching toward both sides, the fabric is slightly thicker, the shrinkage is large, and the warp elasticity is excellent. If the weft width is narrow, the distance between the two gears is wide (low wavy wrinkles), the shrinkage is small, and the warp elasticity is poor. The warp elasticity may be controlled and adjusted as necessary to maintain an even basis weight of the fabric surface.
[0076] On the other hand, if the weft width is wide, the gap between the two gears is large (low waviness), the contraction width is large, and there are few wrinkles, resulting in a shortage of fiber, unevenness of the fabric surface, and variations in basis weight.If the weft width is narrow, the gap between the two gears is close (high waviness), the fabric is thick, and the elasticity is low.
[0077] Specifically, at the same expansion ratio, the depth and uniformity of the wavy wrinkles affect the flatness of the fabric surface (i.e., the basis weight of the fabric is uneven), and in the process of weft expansion and necking under appropriate temperature conditions, fibers with high wavy wrinkles and uniform arrangement tend to expand uniformly. However, when the wavy wrinkles are low and unevenly arranged, the fibers in the thin fabric surface are drawn first, resulting in unevenness and a thin fabric surface. In addition, when the wavy wrinkles are dense or loose, the necking of the warp direction continuity is uneven.
[0078] The improvements of this invention compared to the prior art are that it can control the height and uniformity of the wavy wrinkles, and by precisely controlling the conditions of the manufacturing process, it can promote continuous and stable necking in the warp direction of the nonwoven fabric, thereby making the warp continuous shrinkage ratio (continuous elasticity) consistent in various parts of the fabric surface, and it can control the elastic stretch recovery effect of the nonwoven fabric to achieve a uniform basis weight on the fabric surface.
[0079] Thereafter, the needle chain 40 feeds the nonwoven fabric 10 having the crushed wavy wrinkles from the inlet 61 of the heating device 60 into the internal space 62 of the heating device 60 along the warp direction.
[0080] Then, in the preheating section 62a of the heating device 60, when the needle chains 40 fixing both sides of the nonwoven fabric 10 maintain a constant weft pitch, i.e., when the width of the nonwoven fabric 10 is not changed, the nonwoven fabric 10 is transported along the warp direction to the width expansion section 62b, and the nonwoven fabric 10 is heated by the heating device 60 until it softens, thereby facilitating subsequent processing and modeling.
[0081] Thereafter, in the width-widening section 62b of the heating device 60, the heating device 60 continues to heat the nonwoven fabric 10 to maintain it at the softening temperature, while the needle chains 40 fixing both sides of the weft direction of the nonwoven fabric 10 continue to transport the softened nonwoven fabric 10 along the warp direction as the weft pitch gradually widens, thereby stretching the nonwoven fabric 10 along the weft direction by utilizing the gradually widening weft pitch, thereby increasing the weft width of the nonwoven fabric 10.
[0082] Preferably, the weft expansion ratio in the widening section 62b of the nonwoven fabric 10 may be, for example, between 15% and 100% (i.e., the weft expansion section 62b ultimately extends to a weft width that is 1.15 to 2 times the original weft width).
[0083] For example, if the weft width of the nonwoven fabric is 100 cm and the weft width is 115 cm after it is weft-stretched, the weft width ratio is 115%. Also, if the weft width of the nonwoven fabric is 100 cm and the weft width is 200 cm after it is weft-stretched, the weft width ratio is 200%.
[0084] In addition, commercially available setting machines can achieve a weft expansion ratio of up to 450%, for example.
[0085] During the weft stretching process, the gradually widening weft pitch of the needle chain 40 is used to mechanically stretch the fibers of the nonwoven fabric 10 continuously in the weft direction, changing the forward direction of the fiber structure and orienting the fiber structure of the nonwoven fabric 10 along the weft direction, so that the nonwoven fabric 10 has an extension recovery force along the warp direction. At the same time, the weft stretching creates a necking compensation action along the warp direction due to the Poisson effect, so that the nonwoven fabric 10 extends along the warp direction, flattening out the crushed wavy wrinkles and presenting a flat fabric surface.
[0086] Next, in the stabilization section 62c of the heating device 60, the heating device 60 continues to heat the nonwoven fabric 10 to maintain it at the softening temperature, and the needle chain 40 fixing both sides of the weft direction of the nonwoven fabric 10 transports the softened and stretched nonwoven fabric 10 along the warp direction when the expanded weft pitch is maintained, i.e., when the nonwoven fabric 10 is maintained at its expanded width, thereby stabilizing the stretched and expanded nonwoven fabric 10 by maintaining the nonwoven fabric 10 in a softened and expanded state for a certain period of time.
[0087] Finally, the needle chain 40, which fixes both sides of the nonwoven fabric 10 in the weft direction, sends the stabilized nonwoven fabric 10 through an outlet 63 to a heating device 60, where the stabilized nonwoven fabric 10 is cooled and set, i.e., stretched and expanded, and set in a state having warp elasticity, thereby forming the warp elastic nonwoven fabric of the present invention.
[0088] After cooling and setting, the fiber structure of the nonwoven fabric 10 is oriented along the weft direction and formed into an ultra-hand-like shape (as shown in FIG. 1b). When a stretching force is applied in the warp direction, the fiber structure oriented along the weft direction of the nonwoven fabric 10 is stretched along the warp direction and can be returned to a state in which the fiber forward direction is not changed, so that it has warp extensibility. After the application of the warp stretching force is stopped, the elastic nonwoven fabric returns to a state in which it is oriented along the weft direction, so that it has warp recovery. Therefore, since the weft direction orientation is formed by stretching and widening along the weft direction, the warp elastic nonwoven fabric of the present invention is given the high stretch recovery property of elastic nonwoven fabrics superior to that of the prior art.
[0089] 10, a flow chart of the manufacturing method of the warp elastic nonwoven fabric of the present invention is shown. The manufacturing method of the elastic nonwoven fabric of the present invention includes a feeding step S10, a corrugating step S20, a fixing step S30, a squeezing step S40, a preheating step S50, a width expanding step S60, a stabilizing step S70, and a cooling step S80.
[0090] The components used in the following steps, such as the heating device, the needle chain, the feed gear set, and the roll brush, may be the components mentioned above, such as the heating device 60, the needle chain 40, the feed gear set F, and the roll brush 50. Therefore, the features and details of said components will be omitted.
[0091] In the feeding step S10, at least two feed gear sets are used to feed the nonwoven fabric, and the differential gears of the feed gear sets feed both sides of the weft direction of the nonwoven fabric along the warp direction between the differential gears of the feed gear sets and the wind suction gears, respectively.
[0092] In the feeding step 10, the nonwoven fabric fed may be the nonwoven fabric 10 described above, so the characteristics and details of the nonwoven fabric are omitted.
[0093] In the wave forming step S20, the differential gear and the wind suction gear rotate while meshing with each other so that the first teeth of the differential gear are inserted into the second grooves of the wind suction gear, and the second teeth of the wind suction gear are inserted into the first grooves of the differential gear. As a result, both sides of the nonwoven fabric in the weft direction are respectively sandwiched between the plurality of first teeth and the plurality of second grooves, and between the plurality of first grooves and the plurality of second teeth, thereby forming regular wave wrinkles in the nonwoven fabric along the warp direction.
[0094] In the fixing step S30, the wavy wrinkles of the nonwoven fabric are fixed using an air suction gear and at least two conveyor-type needle chains, and suction force is provided through the air suction holes of the air suction gear to make both sides of the nonwoven fabric in the weft direction adhere to the outer surfaces of the second tooth portion and the second groove portion of the air suction gear, respectively; and as the air suction gear rotates, the needle chain operates in a conveyor manner to make the multiple needles penetrate the nonwoven fabric, and the nonwoven fabric is inserted into the hollow grooves of the air suction gear, thereby fixing the wavy wrinkles of the nonwoven fabric; and the air suction gear stops providing suction force after the multiple needles penetrate the nonwoven fabric, thereby smoothly transferring the nonwoven fabric from the air suction gear to the needle chain.
[0095] In the squashing step S40, the wavy wrinkles of the nonwoven fabric are squashed by at least two roll brushes, which rotate together with the needle chain moving in a conveyor manner to squash the wavy wrinkles of the nonwoven fabric on the needle chain.
[0096] In the preheating step S50, the nonwoven fabric is transported in the warp direction while keeping the weft pitch constant by using a needle chain, and is heated by a heater until the nonwoven fabric is softened.
[0097] In the widening step S60, when the heating device is used to continue heating, the needle chain is used to gradually widen its weft pitch, and the softened nonwoven fabric is transported along the warp direction to stretch the nonwoven fabric along the weft direction, and the nonwoven fabric is stretched along the weft direction by generating a necking compensation action along the warp direction due to the Poisson effect in order to stretch the nonwoven fabric in the weft direction, thereby extending along the warp direction and flattening out the crushed wavy wrinkles, and the fiber structure of the nonwoven fabric is oriented along the weft direction, so that the fabric surface is flat and the nonwoven fabric has extension recovery force along the warp direction.
[0098] In the stabilization step S70, the heating device is used to continue heating and the softened and stretched nonwoven fabric is transported along the warp direction while maintaining the weft pitch after being spread by the needle chain, thereby stabilizing the nonwoven fabric.
[0099] In a cooling step S80, the stabilized nonwoven fabric is cooled and allowed to set, thereby forming a warp elastic nonwoven fabric.
[0100] In the manufacturing method of the warp elastic nonwoven fabric of the present invention, in the feeding step S10, the differential gear feeds the nonwoven fabric in the warp direction between the differential gear and the wind suction gear, so that the feeding speed of the differential gear is higher than that of the needle chain.
[0101] Preferably, the warp elastic nonwoven fabric of the present invention produced by the above apparatus or method has a warp extensibility of between 50% and 350% (i.e., it can be stretched to a warp width of 1.5 to 4.5 times its natural warp width).
[0102] Preferably, in the above method, the plurality of wind suction holes are further provided in the plurality of second teeth.
[0103] Preferably, the heating temperature in the preheating step S50, the width-widening step S60, and the stabilization step S70 is from 120°C to 180°C, preferably from 130°C to 150°C.
[0104] Preferably, in the width-spreading step S60, the weft-direction width-spreading ratio of the nonwoven fabric 10 is between 15% and 100%.
[0105] Preferably, in the cooling step S80, nonwoven fabric 10 that has undergone stabilization step S70 is cooled in the air or left to stand at room temperature, for example, so that nonwoven fabric 10 returns to an unsoftened state and the shape of nonwoven fabric 10 is fixed.
[0106] Preferably, in the fixing step S30, each of the needles on the needle chain is aimed at a peak and / or a valley of the waviness of the nonwoven fabric.
[0107] Preferably, in the above method, the ratio of the pitch between the first teeth:the pitch between the second teeth:the pitch between the needles is adjusted to 1:1:1 or 1:1:0.5.
[0108] Referring to FIG. 11 and FIG. 12, the present invention provides a warp elastic nonwoven fabric 100 produced by the above-mentioned production equipment or production method, and having the above-mentioned characteristics and technical effects.
[0109] Specifically, referring to Fig. 11, the warp elastic nonwoven fabric 100 of the present invention has a flat surface. Further, referring to Fig. 12, an enlarged view of a portion of region a in Fig. 11 is shown. The fiber structure 110 of the warp elastic nonwoven fabric 100 is basically oriented along the weft direction.
[0110] When stretched by an external force in the warp direction, the fiber structure 110 oriented along the weft direction of the nonwoven fabric 100 is stretched so as to return to a state in which the fiber forward orientation is not changed along the warp direction. Therefore, after the stretching by the external force is stopped, the fiber structure 110 of the nonwoven fabric 100 returns to a state in which it is oriented along the weft direction, so that the nonwoven fabric has superior warp stretch recovery properties, i.e., has high stretch recovery force, as compared to elastic nonwoven fabrics of the prior art.
[0111] To sum up, the effects of the present invention are as follows: First, the nonwoven fabric is fed by the meshing differential gear and the wind suction gear, so that regular wavy wrinkles can be formed on the nonwoven fabric, which is advantageous for ensuring the surface flatness of the finished elastic nonwoven fabric. Second, the suction force of the wind suction gear makes the nonwoven fabric adhere to the outer surface of the teeth and grooves of the wind suction gear, so that the wavy wrinkles of the nonwoven fabric can be maintained and transferred to the subsequent manufacturing process, which is advantageous for improving the uniformity of the finished fabric surface. Third, a hollow groove is provided in the center of the outer surface of the wind suction gear, so that a storage space can be provided after the needles on the needle chain are inserted into the nonwoven fabric. Fourth, the forward direction of the fibers is changed by slight stretching in the weft direction during heating, and then cooled and set, so that the nonwoven fabric has better elasticity in the warp direction than the conventional technology. Fifth, the uniform wavy wrinkles can be formed in advance, which can compensate for the phenomenon of the nonwoven fabric shrinking in area or thinning due to necking in the subsequent stretching operation. Sixth, the single-layer nonwoven fabric has excellent elasticity after processing, eliminating the need for additional lamination materials or steps, thereby reducing production costs, making the product thinner and improving user comfort, and reducing the space and costs required for storage and transportation.
[0112] Those skilled in the art can make various modifications and changes to the above embodiments, such as combinations, separations, substitutions and arrangements, without departing from the basic characteristics of the present invention.
[0113] Therefore, although the embodiments of the present invention are intended to illustrate the scope of the technical idea of the present invention, the scope of the present invention is not limited to the above embodiments, and any modifications or changes to the present invention in the same spirit as the present invention should be included within the intended scope of protection of the present invention. [Explanation of symbols]
[0114] a area 10. Nonwoven Fabrics 11 Fibrous Tissue 20 Differential gear 20' Prior Art Differential Gear 20a' Friction surface 20b' Brush 21 First tooth 22 First groove 30 Wind suction gear 31 Second tooth 32 Second groove 33 Wind suction hole 34 Hollow groove 40,40' needle chain 41,41' needle 50,50' Roll Brush 60 Heating device 61 Entrance 62 Interior Space 62a Preheating section 62b Widening section 62c Stabilization Section 63 Exit 100 Warp-direction elastic nonwoven fabric 110 Fibrous Tissue B' Belt roller set F Feed Gear Set N necking region MD warp direction TD latitude direction S10 Supply step S20 Wave formation step S30 Fixed Step S40 Crushing Step S50 Preheat step S60 Widening Step S70 Stabilization Step S80 Cooling Step
Claims
1. A manufacturing facility for a warp direction elastic nonwoven fabric, comprising: A heating device having an inlet, an internal space, and an outlet in sequence along a warp direction, the internal space being divided along the warp direction into a preheating section adjacent to the inlet, a widening section located in the middle, and a stabilization section adjacent to the outlet; At least two needle chains are in the form of a conveyor, each of which is located on either side of the heating device in the latitudinal direction and extends from an entrance of the heating device in the warp direction through the preheating section, the widening section, and the stabilization section in sequence to the exit of the heating device, each of which has a plurality of needles; at least two feed gear sets each disposed above the plurality of needle chains at an inlet of the heating device; at least two roll brushes each disposed radially downstream of the plurality of feed gear sets and above the plurality of needle chains; Each of the plurality of feed gear sets includes a differential gear and a wind suction gear that mesh with each other; Each of the differential gears has a plurality of first teeth and a plurality of first grooves arranged along an outer circumferential surface of the differential gear, the first teeth and the first grooves being offset from one another; A hollow groove is provided in the latitudinal center of the outer surface of each of the plurality of wind suction gears, and each of the plurality of wind suction gears is provided with a plurality of second teeth, a plurality of second grooves, and a plurality of wind suction holes on both sides of the hollow groove in the latitudinal direction, the plurality of second grooves and the plurality of second teeth are respectively arranged in a shifted manner along both sides of the latitudinal direction of the outer peripheral surface of the wind suction gear, and the plurality of wind suction holes are provided in at least the plurality of second grooves, The plurality of differential gears feed the nonwoven fabric between the plurality of differential gears and the plurality of wind suction gears along the warp direction on both sides of the weft direction at a higher feed speed than the plurality of needle chains, the plurality of differential gears and the plurality of wind suction gears rotate while meshing with each other such that the plurality of first tooth portions are inserted into the plurality of second groove portions and the plurality of second tooth portions are inserted into the plurality of first groove portions, whereby both sides of the nonwoven fabric in the weft direction are respectively engaged between the plurality of first tooth portions and the plurality of second groove portions, and between the plurality of first groove portions and the plurality of second tooth portions, thereby forming regular wavy wrinkles in the nonwoven fabric along the warp direction; The plurality of wind suction gears provide suction force through the plurality of wind suction holes to bring both sides of the nonwoven fabric in the weft direction into close contact with the outer surfaces of the plurality of second tooth portions and the plurality of second groove portions, respectively; In addition, the plurality of hollow grooves are configured such that, when the plurality of needle chains rotate around the plurality of wind suction gears and operate in a conveyor manner, the plurality of needles are inserted into the nonwoven fabric fed thereto, the nonwoven fabric is inserted into the plurality of hollow grooves, and the wavy wrinkles of the nonwoven fabric fed thereto are fixed; In addition, the plurality of wind suction gears stop providing the suction force after the plurality of needles have pierced the fed nonwoven fabric, thereby smoothly transferring the nonwoven fabric from the plurality of wind suction gears to the plurality of needle chains, The plurality of roll brushes are rotated together with the plurality of needle chains operating in a conveyor manner to crush the wavy wrinkles of the nonwoven fabric on the plurality of needle chains; and The plurality of needle chains feed the nonwoven fabric having the crushed wavy wrinkles from the inlet of the heating device into the internal space of the heating device along a warp direction, In the preheating section, the nonwoven fabric is transported in a warp direction while the plurality of needle chains maintain a constant weft pitch, and the nonwoven fabric is heated by the heating device until it is softened; Then, in the widening section, the heating device continues to heat, and the multiple needle chains transport the softened nonwoven fabric along the warp direction when the weft pitch gradually widens, stretching it along the weft direction, generating a necking compensation effect on the nonwoven fabric along the warp direction, flattening the wavy wrinkles extending along the warp direction, and orienting the fiber structure of the nonwoven fabric along the weft direction, so that the nonwoven fabric is in a flat state and has an elongation recovery force along the warp direction; Then, in the stabilization section, the heating device continuously heats the nonwoven fabric, and the needle chains transport the softened and stretched nonwoven fabric along a warp direction while maintaining an expanded weft pitch, thereby stabilizing the nonwoven fabric; Finally, the needle chain sends the stabilized nonwoven fabric out of the heating device through the outlet, thereby cooling and setting the stabilized nonwoven fabric, thereby forming a warp elastic nonwoven fabric.
2. The equipment for manufacturing warp-direction elastic nonwoven fabrics according to claim 1 , wherein the plurality of air suction holes are further installed in the plurality of second teeth.
3. The equipment for producing warp-direction elastic nonwoven fabrics according to claim 1 , wherein the heating temperature of the heating device is from 120° C. to 180° C.
4. The equipment for manufacturing a warp-direction elastic nonwoven fabric according to claim 1 , wherein the weft-direction expansion ratio in the width-expanding section of the nonwoven fabric is between 15% and 100%.
5. The equipment for manufacturing warp-direction elastic nonwoven fabrics according to claim 1 , wherein the plurality of needles on the needle chain are each directed toward a peak and / or a valley of the waviness.
6. The manufacturing equipment for warp-direction elastic nonwoven fabrics according to claim 1 , wherein the pitch between the plurality of first tooth portions, the pitch between the plurality of second tooth portions, and the pitch between the plurality of needles are 1:1:1 or 1:1:0.
5.
7. The equipment for producing a warp-direction elastic nonwoven fabric according to claim 1 , wherein the nonwoven fabric is produced by a spunbond method, a spunlace method, a thermal bond method, a meltblown method, or a needle punch method.
8. The equipment for producing warp elastic nonwoven fabrics according to claim 1 , wherein the nonwoven fabric is made from a material selected from the group consisting of PP, PE, PET, PP / PE, PP / PET, or combinations thereof.
9. A warp direction elastic nonwoven fabric produced by the manufacturing equipment for warp direction elastic nonwoven fabric according to any one of claims 1 to 8, The warp direction elastic nonwoven fabric has a flat surface and has an extensible recovery force along the warp direction due to the fiber structure being essentially oriented along the weft direction.
10. 10. The warp elastic nonwoven fabric of claim 9, wherein the warp elastic nonwoven fabric has a warp extensibility of between 50% and 350%.