Method for manufacturing coated metal strip
By welding and transporting the welding point downstream before stopping its conveyance, the method addresses the inefficiencies in restarting painted metal strip production, improving efficiency and reducing downtime.
Patent Information
- Application Number
- JP2018198655
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2018-10-22
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2038-10-22
AI Technical Summary
The conventional method of manufacturing painted metal strips involves stopping the welding point at the welder position, leading to increased waiting times and reduced efficiency when the equipment is restarted, particularly due to frequent shutdowns for changes in paint or testing.
A method that includes welding the tip of the product material to the tail end of a threaded material, transporting the welding point downstream, and then stopping its conveyance, allowing for efficient storage and processing of materials upon restart.
This approach significantly reduces waiting times and enhances manufacturing efficiency by enabling quicker processing and pretreatment of materials, even during frequent equipment shutdowns.
Smart Images

Figure 0007554547000002 
Figure 0007554547000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a coated metal strip. By law Regarding. [Background technology]
[0002] Conventionally used manufacturing methods and equipment for this type of coated metal strip include, for example, the configuration shown in Patent Document 1 below. That is, in the conventional configuration, when the manufacturing equipment for coated metal strip is stopped, a threaded material (dummy material) is passed through the manufacturing equipment, and the leading end of a product material is welded to the trailing end of the threaded material by a welder. After the leading end of the product material is welded to the trailing end of the threaded material by the welder, the welding point between the threaded material and the product material is stopped at the position of the welder. This is to enable an immediate response in the event that a production schedule is changed during the stoppage and the product material needs to be replaced. When the manufacturing equipment for coated metal strip is restarted, the threaded material is flushed away, and the product material is introduced into the manufacturing equipment. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2017-30021 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the conventional configuration as described above, the welding of the threaded material and the product material is stopped at the position of the welder, so the waiting time from when the production equipment for coated metal strip is restarted until the processing of the product material starts is long, and the production efficiency of the coated metal strip is deteriorated. In the case of the production equipment for coated metal strip, the operation may be stopped more than 100 times a month due to the change of paint, etc. Even a slight increase in the waiting time significantly deteriorates the production efficiency.
[0005] The present invention has been made to solve the above-mentioned problems, and an object of the present invention is to provide a method for producing a coated metal strip, which can shorten the waiting time from when the production equipment for a coated metal strip is restarted until the processing of a product material is started, and can improve the production efficiency of the coated metal strip. Law The aim is to provide. [Means for solving the problem]
[0006] The method for manufacturing a painted metal strip according to the present invention includes a step of creating a weld by using a welder to weld the leading end of a product material to the trailing end of a worn material being transported on a continuous painting line, and a step of pausing transportation of the weld after creating the weld, while transporting the weld downstream of the welder. Effect of the Invention
[0008] Method for producing coated metal strip of the present invention By law According to this method, after the leading end of the metal strip is welded to the tail end of the worn material to create a weld, the transportation of the weld point is stopped while the weld point is transported downstream of the welder, thereby shortening the waiting time from when the painted metal strip manufacturing equipment is restarted until processing of the product material begins, thereby improving the manufacturing efficiency of painted metal strip. [Brief description of the drawings]
[0009] [Figure 1] 1 is a configuration diagram showing a coated metal strip manufacturing facility in which a coated metal strip manufacturing method according to an embodiment of the present invention is carried out. [Diagram 2] 4 is a flowchart showing a pause control operation by the control device of FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the embodiments for carrying out the present invention will be described with reference to the drawings. The present invention is not limited to each embodiment, and the components can be modified and embodied without departing from the gist of the present invention. In addition, various inventions can be formed by appropriately combining multiple components disclosed in each embodiment. For example, some components may be deleted from all the components shown in the embodiments. Furthermore, components of different embodiments may be appropriately combined.
[0011] Fig. 1 is a configuration diagram showing a production facility for a coated metal strip in which a method for producing a coated metal strip according to an embodiment of the present invention is carried out. As shown in Fig. 1, the production facility for a coated metal strip of this embodiment is provided with an inlet section 1, a central section 2, an outlet section 3 and a control device 4.
[0012] The entry section 1 is a section where the metal strip 5 is paid out from the pay-off reels 100, 101. The central section 2 is provided after the entry section 1, and is a section where the metal strip 5 is subjected to a chemical conversion treatment, and then painted and baked. The exit section 3 is provided after the central section 2, and is a section where the painted metal strip 5 is wound onto a tension reel 302. The entry section 1, central section 2, and exit section 3 constitute a continuous coating line along which the metal strip 5 is transported. The entry section 1, central section 2, and exit section 3 will be described in more detail below.
[0013] <Input section> The entry section 1 is provided with first and second payoff reels 100, 101, a welder 102 and an entry looper 103.
[0014] A metal strip coil around which a metal strip 5 is wound is inserted into each of the first and second payoff reels 100, 101. The metal strip coil is inserted into the first and second payoff reels 100, 101 by a coil car (not shown). The coil car transports the metal strip coil horizontally and raises and lowers it. Although not shown, a lead-out device is provided near the first and second payoff reels 100, 101 to scoop up the tip of the metal strip coil inserted into the first and second payoff reels 100, 101.
[0015] The metal strip 5 includes product material and worn material. The product material is a metal strip that is to be painted as a product. The worn material is a metal strip that is passed through a continuous painting line when the manufacturing facility for painted metal strip is stopped. The worn material is also called dummy material.
[0016] The welder 102 is a welding machine that welds the leading end of a succeeding metal strip to the tail end of a preceding metal strip. Welding by the welder 102 includes welding between product materials, welding between frayed materials, welding the leading end of a frayed material to the tail end of a product material, and welding the leading end of a product material to the tail end of a frayed material. By performing such welding, the metal strip 5 is continuously transported in the continuous coating line. The welded points between the metal strips are called welding points. When the welder 102 is welding the metal strip 5, the transport of the metal strip 5 is stopped at the welder 102.
[0017] The entrance looper 103 is a device that adjusts the conveying length of the metal strip 5. The entrance looper 103 includes a plurality of fixed rolls 103a and a plurality of movable rolls 103b arranged above the fixed rolls 103a. The metal strip 5 is alternately wound around the fixed rolls 103a and the movable rolls 103b.
[0018] Each movable roll 103b is provided so as to be displaceable in the vertical direction. The conveying length of the metal strip 5 is shortened by lowering each movable roll 103b so as to approach the fixed roll 103a, and the conveying length of the metal strip 5 is lengthened by raising each movable roll 103b so as to move away from the fixed roll 103a. By adjusting the conveying length by the inlet looper 103, it is possible to maintain the supply of the metal strip 5 to the rear stage of the inlet looper 103 even when the welder 102 is welding the metal strip 5. In other words, before the welder 102 welds the metal strip 5, each movable roll 103b is raised to store the metal strip 5 in the entry looper 103, and when the welder 102 welds the metal strip 5, each movable roll 103b is lowered to send out the metal strip 5 from the entry looper 103, making it possible to maintain the supply of metal strip 5 to the rear stage of the entry looper 103 even when the welder 102 is welding the metal strip 5.
[0019] <Central Section> The central section 2 includes a paint pre-treatment equipment 200, a chemi-coater 201, a drying furnace 202, a first coater 203, a first oven 204, a first water quench 205, a second coater 206, a second oven 207, a second water quench 208 and a tension leveler 209.
[0020] The paint pretreatment equipment 200 is equipment that performs paint pretreatment on the metal strip 5. The paint pretreatment equipment 200 of this embodiment performs alkaline degreasing on the metal strip 5, rinses the metal strip 5 with water, and then performs phosphate treatment on the metal strip 5.
[0021] The chemi-coater 201 is equipment that applies a chemical conversion treatment liquid to the metal strip 5 that has been subjected to pre-painting treatment in the pre-painting treatment equipment 200, thereby performing chemical conversion treatment on the metal strip 5.
[0022] The drying furnace 202 is a furnace for drying the metal strip 5 at the rear of the chemi-coater 201 .
[0023] The first coater 203 is a facility that applies an undercoat to the metal strip 5. The first oven 204 and the first water quench 205 are facilities that bake and cool the coating film on the metal strip 5 that has been undercoated by the first coater 203.
[0024] The second coater 206 is equipment that applies a top coat to the metal strip 5. The second oven 207 and the second water quench 208 are equipment that bake and cool the coating film on the metal strip 5 that has been applied by the second coater 206.
[0025] The tension leveler 209 is a device that stretches the metal strip 5 after painting and baking to correct the shape.
[0026] <Output section> The exit section 3 is provided with an exit looper 300, an exit shear 301, and a tension reel 302.
[0027] The exit looper 300 is a device that adjusts the conveying length of the metal strip 5, similar to the entry looper 103. The adjustment of the conveying length by the exit looper 300 makes it possible to accumulate the metal strip 5 in the exit looper 300, for example, when the metal strip 5 is cut by the exit shear 301, which will be described later.
[0028] The exit shear 301 is disposed after the exit looper 300, and is a device that cuts the metal strip 5 to a predetermined length. When the metal strip 5 is cut by the exit shear 301, the conveyance of the metal strip 5 is stopped at the exit shear 301.
[0029] The tension reel 302 is disposed after the exit shear 301, and is a reel body that winds up the metal strip 5 that has passed through the exit shear 301 into a coil. When a certain amount of metal strip 5 has been wound around the tension reel 302, the metal strip 5 is cut by the exit shear 301. The metal strip coil is removed from the tension reel 302 and transported by a coil car (not shown).
[0030] The control device 4 is configured with, for example, a computer that performs calculation processing based on a program. The control device 4 controls the operation of the devices included in the inlet section 1, the central section 2, and the outlet section 3. The control device 4 also controls the transportation of the metal strip 5.
[0031] As mentioned above, when the painted metal strip manufacturing facility is shut down, the worn material is run through the continuous coating line. The worn material is welded to the tail end of the product material that was running through the continuous coating line before the painted metal strip manufacturing facility was shut down, and is run through the continuous coating line together with that product material. The product material to which the worn material is welded to its tail end is called the first product material. The next product material is welded to the tail end of the worn material in preparation for when the painted metal strip manufacturing facility is restarted. The next product material is run through the continuous coating line together with the worn material. The product material welded to the tail end of the worn material is called the second product material.
[0032] As described below, the control device 4 of this embodiment performs a control operation to shorten the standby time from when the painted metal strip manufacturing equipment is restarted until the processing of the product material is started. The painted metal strip manufacturing equipment is stopped at least when, for example, the paint used in the first or second coater 203, 206 is changed and / or when test painting is performed to test painting of the product material. The metal strip used in test painting is sometimes called a test material. In this specification, the product material also includes the test material used in test painting.
[0033] Next, Fig. 2 is a flowchart showing the pause control operation by the control device 4 of Fig. 1. The control device 4 performs the pause control operation shown in Fig. 2 when it receives a pause command from the outside. The pause command is input to the control device 4 from an input unit such as a control panel operated by an operator. As shown in Fig. 2, when the control device 4 starts the pause control operation, it welds the leading end of the threaded material to the trailing end of the first product material with the welder 102 to create a first weld point (step S1). Next, the control device 4 passes the threaded material through a continuous coating line (step S2), and welds the leading end of the second product material to the trailing end of the threaded material with the welder 102 to create a second weld point (step S3).
[0034] After creating the second welding point, the control device 4 transports the second welding point (step S4), and pauses transport of the welding point with the second welding point transported downstream of the welder 102 (step S5). By pausing transport of the welding point with the second welding point transported downstream of the welder 102 in this manner, the waiting time from when the production equipment for coated metal strip is restarted until processing of the product material begins can be shortened compared to the case where the second welding point is left at the position of the welder 102, and the production efficiency of the coated metal strip can be improved.
[0035] The control device 4 suspends the transportation of the second welding point when the second welding point is located upstream of the paint pretreatment equipment 200. By locating the second welding point upstream of the paint pretreatment equipment 200, it is possible to perform pretreatment of the second product material for an appropriate period of time when the production equipment for coated metal strips is restarted.
[0036] The control device 4 has information indicating the transport speed at which the second welding point (second metal strip) should be transported when the painted metal strip manufacturing equipment is restarted. The control device 4 changes the position of the second welding point when the transport of the second welding point is paused in accordance with the transport speed of the second welding point after the transport of the second welding point is resumed, so that the time from when the transport of the second welding point is resumed to when the second welding point reaches the first oven 204 is equal to or longer than a predetermined time. By changing the position of the second welding point when the transport of the second welding point is paused in this manner, the second product material can enter the first oven 204 after the conditions inside the first oven 204 have been adjusted, and the second product material can be painted more appropriately.
[0037] The control device 4 of this embodiment suspends the transportation of the second welding point in a state where the second welding point has been transported to the downstream of the entry looper 103. After suspending the transportation of the second welding point, the control device 4 causes the second product to accumulate in the entry looper 103 (step S6). That is, while the second product is being sent out from the first or second pay-off reel 100, 101, the movable roll 103b of the entry looper 103 is raised to accumulate the second product in the entry looper 103. At this time, the second product is preferably accumulated to 60% or more of the predetermined maximum storage amount of the metal strip in the entry looper 103, more preferably 80% or more, and even more preferably 100%. By accumulating the second product in the entry looper 103 before resuming the transportation of the second welding point, the second product can be processed more quickly after the production facility for coated metal strip is restarted.
[0038] After storing the second welding point in the entry looper 103, the control device 4 resumes the transportation of the second welding point when an external restart command is detected (step S7). The transportation of the second welding point is preferably resumed after the second metal strip has been stored in the entry looper 103 up to a predetermined storage amount, but may be resumed before the second product material has been stored in the entry looper 103 up to the predetermined storage amount depending on the timing when the painted metal strip manufacturing equipment is restarted.
[0039] The manufacturing method for the painted metal strip in this embodiment includes a step (step S3) of welding the leading end of the second product material to the tail end of the worn material transported on the continuous painting line using a welder 102 to create a second weld point, and a step (step S4) of pausing transportation of the second weld point after creating the second weld point while the second weld point is transported downstream of the welder 102. In addition, the manufacturing method for coated metal strip in this embodiment further includes a process (step S6) of storing the second product material in the inlet looper 103 after creating the second welding point and before resuming transportation of the second welding point. Furthermore, in the method for producing a coated metal strip of this embodiment, when the second welding point is located upstream of the paint pre-treatment equipment 200, transportation to the second welding point is stopped. Furthermore, in the manufacturing method of the coated metal strip of this embodiment, the position of the second welding point when the transportation of the second welding point is paused is changed depending on the transport speed of the second welding point after the transportation of the second welding point is resumed, so that the time from when the transportation of the second welding point is resumed to when the welding point reaches the first oven 204 is greater than or equal to a predetermined time. In addition, transportation to the second welding point is suspended when changing paint and when performing test painting.
[0040] Such a manufacturing method and equipment for coated metal strip includes a step (step S3) of welding the leading end of a second product material to the trailing end of a worn material transported on a continuous coating line with a welder 102 to create a second weld point, and a step (step S5) of pausing transportation of the second weld point after creating the second weld point and transporting the second weld point downstream of the welder 102, thereby shortening the wait time from when the manufacturing equipment for coated metal strip is restarted until processing of the product material begins, and improving the manufacturing efficiency of coated metal strip. In the case of a manufacturing equipment for coated metal strip, the equipment may be shut down more than 100 times a month. By shortening the wait time, the manufacturing efficiency can be greatly improved.
[0041] In addition, since the second product material can be stored in the inlet looper 103 after the second welding point is created and before transport of the second welding point is resumed, processing of the second product material can be carried out more quickly after transport of the second welding point is resumed.
[0042] Furthermore, since transportation to the second welding point is suspended while the second welding point is located upstream of the paint pretreatment equipment 200, pretreatment of the second product material can be carried out for an appropriate period of time when the painted metal strip manufacturing equipment is restarted.
[0043] Furthermore, the position of the second welding point when the transportation of the second welding point is paused is changed according to the transportation speed of the second welding point after the transportation of the second welding point is resumed so that the time from when the transportation of the second welding point is resumed to when the welding point reaches the first oven 204 is equal to or longer than a predetermined time. Therefore, the second product material can enter the first oven 204 after the conditions inside the first oven 204 have been adjusted, and the second product material can be painted more appropriately.
[0044] Furthermore, since the transportation to the second welding point is halted when changing paint or performing test painting, the waiting time after changing paint or performing test painting can be shortened, and the production efficiency of the coated metal strip can be improved. [Explanation of symbols]
[0045] 4. Control device 5 Metal strips (wear and tear, finished products) 102 Welder 103 Inlet looper (looper) 200 Paint pre-treatment equipment 203 No. 1 Coater (painting equipment, coater) 204 No. 1 oven (painting equipment, oven)
Claims
1. A process of welding the leading end of a product material to the trailing end of a threaded material conveyed on a continuous coating line by a welder to create a welded point; a step of pausing transportation of the welding point while the welding point is transported downstream of the welder after the welding point is created; A method for producing a coated metal strip, comprising:
2. The continuous coating line includes a coating pretreatment facility arranged downstream of the welder, and a coating facility arranged downstream of the coating pretreatment facility, The transportation of the welding point is stopped in a state where the welding point is located upstream of the paint pretreatment equipment. A method for producing a coated metal strip according to claim 1.
3. The continuous coating line includes a looper disposed downstream of the welder, storing the product material within the looper after creating the weld and before resuming transport of the weld; The method for producing a coated metal strip according to claim 1 or claim 2, further comprising:
4. The continuous coating line includes a coating pretreatment facility arranged downstream of the welder, and a coating facility arranged downstream of the coating pretreatment facility, The coating equipment includes a coater that coats the product material, and an oven disposed downstream of the coater; a position of the welding point when the transportation of the welding point is paused is changed according to a transportation speed of the welding point after the transportation of the welding point is resumed so that the time from when the transportation of the welding point is resumed until the welding point reaches the oven is equal to or longer than a predetermined time. A method for producing a coated metal strip according to any one of claims 1 to 3.
5. The stop of the transportation of the welding point is performed when changing paint and when performing test painting. A method for producing a coated metal strip according to any one of claims 1 to 4.
Citation Information
Patent Citations
Continuous etching equipment train for metallic strip
JP1998060700A
Strip coater
JP2005238033A
Coating metal strip manufacturing facility
JP2017030021A