Plasma Processing Equipment

The plasma processing apparatus addresses high operating costs by using a dielectric-covered sample stage with a second adhesive to protect against plasma exposure, extending component life and reducing maintenance frequency.

JP7555197B2Active Publication Date: 2024-09-24HITACHI HIGH TECH CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020068770
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-04-07
Publication Date
2024-09-24
Estimated Expiration
2040-04-07

AI Technical Summary

Technical Problem

Conventional plasma processing equipment faces high operating costs due to frequent replacement of sample stage components, as the adhesive layer covering the sintered plate wears out and damages surrounding parts, necessitating premature maintenance.

Method used

A plasma processing apparatus with a sample stage design that includes a cylindrical convex portion covered by a dielectric material, using a second adhesive to fill the gap between the body and cylindrical cover, reducing direct exposure to plasma and corrosion.

Benefits of technology

This design extends the lifespan of the adhesive layer and reduces wear on surrounding components, lowering operating costs by minimizing the frequency of component replacements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555197000002
    Figure 0007555197000002
  • Figure 0007555197000001
    Figure 0007555197000001
  • Figure 0007555197000003
    Figure 0007555197000003
Patent Text Reader

Abstract

To provide a plasma processing device achieving reduced operation cost.SOLUTION: A plasma processing device includes a specimen support which is arranged in a processing chamber at an inside of a vacuum vessel and which has an upper surface where a wafer to be processed is mounted, the plasma processing device forming a plasma in the processing chamber to process the wafer. The specimen support includes: a protrusion arranged on an upper part of a metal base material and having a cylindrical shape; a sintered plate that is a dielectric disc-shaped sintered plate which is joined on the upper surface of the protrusion with a first adhesive sandwiched therebetween, and on which the wafer is put; a cylindrical-shaped dielectric cylindrical cover surrounding and covering a side wall of the protrusion; and a second adhesive filled in a gap between an outer peripheral edge of the sintered plate and the dielectric cylindrical cover on a lower side.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a plasma processing apparatus that processes a wafer placed in a processing chamber in a vacuum vessel by using plasma generated in the processing chamber, and to a plasma processing apparatus that processes the wafer while adjusting the temperature of the wafer to a temperature suitable for processing by adjusting the temperature of a processing table placed in the processing chamber. [Background technology]

[0002] In such a plasma processing apparatus, in order to shorten the time required to process a so-called multi-layer film in which a plurality of films to be processed are formed on the surface of a substrate-like sample such as a semiconductor wafer, it has been considered to process adjacent films in the same processing chamber without removing the wafer from the processing chamber between the processes of each of these films. In addition, since there has been a demand for more fine processing with high precision, the temperature of the wafer has been adjusted so that each film to be processed is suitable for processing in order to improve the uniformity of the shape of the result of processing such as etching the film to be processed in the surface direction (radial direction, circumferential direction) of the wafer.

[0003] As a technique for adjusting such a temperature, for example, as disclosed in JP 2011-258614 A (Patent Document 1), a technique has been known in which the upper part of a sample mounting stage constituting the surface on which a wafer is mounted is made of a ceramic disk-shaped sintered body member, and a dielectric film member connected to the lower part of the ceramic disk through an adhesive and having a film-shaped heater inside, and an etching process is performed while adjusting the temperature of the ceramic disk and the wafer mounted on the upper surface of the ceramic disk-shaped member. In particular, Patent Document 1 discloses a sample mounting stage in which the ceramic disk-shaped member has an electrode built therein to which DC power is supplied in order to generate an electrostatic force that attracts the wafer to the upper surface of the ceramic disk-shaped member, a film-shaped heater is formed on the lower surface of the disk-shaped member with a predetermined thickness, and the side part of the disk-shaped member to which adhesive is applied is pressed against the upper surface of the conductive body of the sample mounting stage with the adhesive sandwiched therebetween to bond the sample mounting stage.

[0004] Furthermore, Japanese Patent Laid-Open Publication No. 2017-041631 (Patent Document 2) discloses that an edge seal made of elastomer silicone or silicone rubber is used to cover the adhesive layer at the recessed portion between the upper and lower layers at the end of a substrate support formed by bonding multiple layers of members with an adhesive sandwiched therebetween. In particular, this conventional technology discloses a technology in which the adhesive is covered with a silicone seal, thereby suppressing the adhesive from being consumed by plasma and preventing damage and particle contamination. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2011-258614 A [Patent Document 2] JP 2017-041631 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, the above-mentioned conventional techniques do not sufficiently consider the following points, which causes problems.

[0007] In other words, even if the life of the adhesive layer can be extended by covering the outer periphery of the layer of adhesive material that joins a plate-shaped component such as a sintered plate that constitutes the wafer mounting surface to the sample stage body with a ring-shaped material that has high plasma resistance and corrosion resistance, if the other coating material wears out and the components that constitute the sample stage around the sintered plate are damaged when the sintered plate is replaced, the interval for replacing the other coating material will become the interval for replacing the sample stage, which will actually shorten the interval for maintenance of the plasma processing device and increase operating costs.This point was not taken into consideration.

[0008] An object of the present invention is to provide a plasma processing apparatus with reduced operating costs. [Means for solving the problem]

[0009] The above object is achieved by a plasma processing apparatus having a sample stage which is placed in a processing chamber inside a vacuum vessel and on whose upper surface a wafer to be processed is placed, and which forms plasma within the processing chamber to process the wafer, wherein the sample stage comprises a cylindrical convex portion which is placed on top of a metal base material, a disk-shaped sintered plate made of dielectric material and bonded to the upper surface of the convex portion with a first adhesive sandwiched therebetween, the sintered plate on which the wafer is placed, a cylindrical dielectric cylindrical cover which surrounds and covers the side wall of the convex portion, and a second adhesive which fills the gap between the outer periphery of the sintered plate and the lower dielectric cylindrical cover. Effect of the Invention

[0010] According to the present invention, it is possible to provide a plasma processing apparatus with reduced operating costs. [Brief description of the drawings]

[0011] [Figure 1] 1 is a vertical cross-sectional view for explaining an outline of the overall configuration of a plasma processing apparatus according to the present invention; [Diagram 2] 2 is an enlarged longitudinal sectional view showing the outline of the configuration of the sample mounting stage of the embodiment shown in FIG. 1. [Diagram 3] 3 is a longitudinal sectional view showing an enlarged schematic configuration of the upper outer peripheral edge portion of the sample stage and the dielectric cover of the embodiment shown in FIG. 2. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. EXAMPLES

[0013] An embodiment of the present invention will be described with reference to the drawings.

[0014] Fig. 1 is a vertical cross-sectional view for explaining the overall configuration of a plasma processing apparatus according to the present invention. In Fig. 1, the plasma processing apparatus 100 includes a vacuum vessel 101, an electromagnetic field supplying means arranged on the upper outer periphery thereof for supplying an electric field or a magnetic field to the inside of the vacuum vessel 101, and an exhausting means arranged below the vacuum vessel 101 for exhausting the inside of the vacuum vessel 101.

[0015] The vacuum vessel 101 is provided inside with a processing chamber 103, which is a space inside where plasma is formed and a sample to be processed placed inside is processed by the plasma, and a sample mounting stage 107, which is located at the bottom of the processing chamber 103 and on whose upper surface the sample is placed and held. Also, above the vacuum vessel 101, there are provided a radio wave source 104 such as a magnetron that forms an electric field of a predetermined frequency such as microwaves or UHF waves as an electromagnetic field supply means, a waveguide 105 that is a pipe that propagates radio waves and leads them into the processing chamber 103, and a resonant vessel 106 that is connected to the waveguide 105 and into which the radio waves propagating inside are introduced and resonate in the internal space.

[0016] Furthermore, a solenoid coil 113 is disposed on the upper part of the vacuum vessel. The solenoid coil 113 is disposed surrounding the outer periphery of the upper part of the cylindrical vacuum vessel 101, and generates a magnetic field by current supplied thereto. In this embodiment, the solenoid coils 113 are disposed in a number of stages, and a magnetic field is introduced inside the processing chamber 103, in which the uniform magnetic field is axially symmetric around the central axis in the vertical direction and diverges downward toward the end.

[0017] Further, a vacuum pump 102 such as a turbo molecular pump serving as an exhaust means is disposed below the vacuum vessel 101, and communicates with a circular exhaust opening disposed immediately below a sample mounting stage 107 at the bottom of the processing chamber 102 inside the vacuum vessel 101. The processing chamber 103 inside the vacuum vessel 101 has a substantially cylindrical shape, and disposed at the center of the bottom thereof and above the opening is a substantially cylindrical sample mounting stage 107 on whose upper surface a wafer is mounted.

[0018] In this embodiment, the processing chamber 103, the sample mounting stage 107, and the opening are arranged vertically so that their axes coincide, and the space between the outer wall of the sample mounting stage 107 and the inner wall of the processing chamber 103 is also ring-shaped with their axes coinciding. The sample mounting stage 107 is supported in the air with a space above the opening by multiple beams extending horizontally outward from the outer wall, and these beams are arranged axially symmetrically around the central axis of the sample mounting stage 107 in the vertical direction.

[0019] A resonance chamber 106', which is a space for resonance within a cylindrical resonance container 106 having an aligned axis, is disposed above the cylindrical processing chamber 103. A disk-shaped window member 114 made of a dielectric material such as quartz and constituting the bottom surface of the resonance chamber 106' is disposed between the resonance chamber 106' and the processing chamber 103, to hermetically separate the two.

[0020] A circular shower plate 115 made of a dielectric material such as quartz is arranged below the window member 114 in parallel with a gap from the lower surface of the window member 114, and the lower surface of the shower plate 115 forms the ceiling surface of the processing chamber 103. The shower plate 115 is arranged in parallel facing the upper surface of the sample mounting table 107, and a plurality of through holes are arranged in the center thereof through which a gas for wafer processing is introduced from above into the processing chamber 103. A pipeline through which a processing gas supplied from a gas source (not shown) installed in a building such as a clean room in which the plasma processing apparatus 100 is installed flows is connected to the gap between the window member 114 and the shower plate 115, and the processing gas from the gas source is introduced into the gap through the pipeline and then flows into the processing chamber 103 in the direction of the sample mounting table 107 below through the through holes.

[0021] The sample mounting stage 107 has an electrode made of a conductive material disposed therein, and this electrode is electrically connected to a bias power supply 108 that outputs high-frequency power of a predetermined frequency. With a wafer placed on the mounting surface on the upper surface of the sample mounting stage 107, a bias potential is formed on the wafer surface by the high-frequency power supplied from the bias power supply 108, and the potential difference with the plasma formed in the processing chamber 103 above the sample mounting stage 107 acts to attract charged particles to the upper surface of the wafer.

[0022] Furthermore, as described later, the sample mounting stage 107 has a heater disposed therein for adjusting the temperature of the mounting surface or the wafer, and this heater is electrically connected to a heater electrode DC power supply 109 for supplying power. 2 O 3 Or Y 2 O 3 A dielectric film made of a dielectric material such as , is disposed inside the dielectric film, and an electrostatic adsorption electrode is disposed inside the dielectric film for adsorbing the wafer onto the surface of the dielectric film by electrostatic force. A DC power supply 110 for electrostatic adsorption electrode is electrically connected to the electrostatic adsorption electrode for supplying DC power to the electrostatic adsorption electrode.

[0023] During wafer processing, heat is transferred from the plasma to the sample stage 107, causing the temperature to rise. In order to regulate the temperature to an appropriate level during processing, a coolant passage through which a coolant is supplied and flows is arranged concentrically or spirally around the vertical central axis of the sample stage 107 inside the sample stage 107. A temperature regulator 111 that regulates the temperature of the coolant is connected to a coolant pipe connected to the coolant inlet and outlet of this coolant passage, and the coolant that flows into the temperature regulator 111 through the coolant passage inside the sample stage 107 and the external pipe is adjusted to a predetermined temperature and is supplied again through the pipe to the coolant passage inside the sample stage 107 for circulation.

[0024] Each part of the plasma processing apparatus 100 is connected to a controller 112, which is a control unit, via communication means, and the operation of each part is appropriately adjusted. The controller 112 is composed of a storage device such as a memory, a computing unit, a communication connector, etc. (not shown), and receives outputs from sensors, which are detection means, arranged at multiple locations in the plasma processing apparatus 100, via the communication means, and transmits commands calculated by the computing unit to each of the above parts to adjust the operation so as to obtain the desired results.

[0025] In this embodiment having the above-mentioned configuration, in the process chamber 103, an inert gas such as argon is introduced from a gas source and exhausted by an exhaust means to reduce the pressure, and then a wafer is transported by a transport means such as a robot arm (not shown) through a gate (not shown) onto the sample mounting stage 107 and handed over thereto. After the wafer is placed on the dielectric film that constitutes the mounting surface of the sample mounting stage 107, power is supplied from the DC power supply 110 for electrostatic attraction electrode to the electrode in the dielectric film, generating an electrostatic force, and the wafer is attracted to and held on the dielectric film.

[0026] While a processing gas is introduced into the processing chamber 103 from the gas source through the through-holes of the shower plate 115, the pressure inside the processing chamber 103 is adjusted to a predetermined range by a balance with exhaust from the opening by the operation of the vacuum pump 102. The microwaves generated by the radio wave source 104 propagate through the waveguide 105 and reach the resonance vessel 106, where an electric field of a predetermined strength is generated in the internal resonance chamber 106'. This electric field is supplied into the processing chamber 103 by transmitting through the window member 114 and the shower plate 115.

[0027] The process gas is excited and turned into plasma by the interaction between the magnetic field (magnetic field) supplied from the solenoid coil 113 and the electric field supplied from the resonant vessel 106, and the plasma is formed in the space above the sample mounting stage 107 in the process chamber 103. A bias potential formed by high-frequency power from the bias power supply 108 attracts charged particles in the plasma to the wafer surface, and a desired process such as etching is performed by physical and chemical reactions that occur in the film to be processed on the wafer surface.

[0028] In this embodiment, plasma is generated using ECR due to the interaction between the electric field and magnetic field caused by the microwaves described above, but this is not limited to this, and plasma generation means using electrostatic coupling means or inductive coupling means using high frequency waves may also be used.

[0029] Fig. 2 is an enlarged longitudinal sectional view showing the outline of the configuration of the sample stage of the embodiment shown in Fig. 1. This figure shows in more detail the configuration of the sample stage 107 shown in Fig. 1.

[0030] The sample stage 107 is made of a disk-shaped base material 201 made of a metal such as Al or Ti, and an Al chuck 202 with a heater and an electrode for electrostatic attraction inside, which is bonded to the upper surface of the base material 201. 2 O 3 The substrate 201 has a cylindrical protrusion in the center of the upper part, the upper surface of which is higher than the surrounding area, and a dielectric cover 202 is disposed on the upper surface of the protrusion. Furthermore, the outer periphery of the cylindrical side wall of the protrusion of the substrate 201 is covered with a dielectric film 202 made of Al. 2 O 3 Or Y 2 O 3 A cylindrical side wall cover 211 made of a sintered ceramic such as SiO 2 is disposed.

[0031] As described above, inside the substrate 201, the coolant grooves 203, which are coolant passages through which the coolant for cooling the substrate 201 flows, are arranged concentrically or spirally around the central axis in the vertical direction of the substrate 201. The coolant grooves 203 have an inlet through which the coolant is introduced and an outlet through which the coolant is discharged, which are connected by pipelines to a temperature regulator 111 outside the vacuum vessel 101, and the temperature regulator 111 adjusts the flow rate (speed) of the coolant circulating through the coolant grooves 203 and the temperature of the coolant in response to a command signal from the controller 112.

[0032] Al 2 O 3The structure of the dielectric cover 202 made of a dielectric material such as the above will be described. The dielectric cover 202 is roughly divided into five layers. The upper layer covering the upper surface of the convex portion is a disk-shaped member made of a sintered ceramic material that has an electrode for electrostatic attraction arranged therein and constitutes the wafer mounting surface, and below, a disk-shaped base material 201 is arranged on the upper surface thereof, with a plurality of layers of dielectric material films including film-shaped heaters formed therein. An adhesive layer is arranged between these upper and lower layers to bond them together.

[0033] In this embodiment, the dielectric material of the lower layer is formed by a thermal spraying method in order to obtain sufficient bonding strength with the upper surface of the metal substrate 201. The film-like heater is also formed by thermal spraying.

[0034] The disk-shaped members constituting the upper layer of this embodiment are made of Al 2 O 3 Or Y 2 O 3 The sintered ceramic plate 209 is a sintered body formed by firing a ceramic material such as a ceramic material having a predetermined thickness and diameter into a disk shape. Inside the sintered ceramic plate 209, a film-like electrostatic attraction electrode film 208 is arranged, which is supplied with DC power to generate electrostatic force, and a connector part electrically connected to the electrostatic attraction electrode film 208 is arranged on the lower surface of the sintered ceramic plate 209, and is connected to a DC power supply 110 for the electrostatic attraction electrode in a state where the connector part is joined to the sample mounting stage 107 on the substrate 201.

[0035] The dielectric film constituting the lower layer is first deposited on the substrate 201 with Al 2 O 3A first dielectric film 204 made of a material such as a ferroelectric material is formed by thermal spraying, and then a metal material is formed in a predetermined shape as heater electrode film 205 by thermal spraying. A mask is used for heater electrode film 205 so that it will have a predetermined shape corresponding to the temperature distribution on the wafer or mounting surface that is desired to be realized when it is sprayed onto first dielectric film 204 by thermal spraying. Metals with controlled resistivity, such as W, nickel-chromium alloys or nickel-aluminum alloys with controlled resistivity, or W mixed with an appropriate additive metal to control the resistivity, are used as the metals to be sprayed to form heater electrode film 205.

[0036] These films formed by thermal spraying are formed by spraying tiny particles of molten or semi-molten material onto the surface of the object to be covered with the film, and the particles are deformed by the impact of colliding with the surface, forming a layered structure. When these particles collide with the surface of the object, the surfaces of the particles come into contact with each other in a molten state, and are joined and fused together, forming tiny spaces between the particles. This makes it difficult for the material to break or crack due to deformation such as expansion and contraction, and makes the material relatively less brittle. In addition, it is easy to change the shape of the film by cutting it after it has been formed.

[0037] In this embodiment, the material of the heater electrode film 205 is sprayed to match the shape of the mask, and then the thickness of the heater electrode film 205 is adjusted by scraping so that the amount of heat generated per unit area at each point is uniform throughout the film. This makes the amount of heat generated uniform in the area where the heater electrode film 208 is arranged, and suppresses unevenness in the temperature distribution in the circumferential and radial directions of the wafer.

[0038] On the sprayed first dielectric film 204 and heater electrode film 205, Al 2 O 3 The dielectric material is sprayed by thermal spraying to form the second dielectric film 206. Thereafter, the upper surface of the second dielectric film 206 may be scraped to adjust the distance between the upper surface of the heater electrode film 208 and the upper surface of the second dielectric film 206 so that the distance is uniform over the entire area where the heater electrode film 208 is disposed.

[0039] Prior to forming the lower film by thermal spraying, the upper film, sintered ceramic plate 209, is separately fired in advance. In this embodiment, the electrostatic attraction electrode film 208 inside the sintered ceramic plate 209 is arranged in two regions, a circular center portion when viewed from above and a ring-shaped outer periphery surrounding the circular center portion, and each of these is electrically connected to the DC power supply 110 for electrostatic attraction electrode and is supplied with different values ​​of power from the DC power supply 110 for electrostatic attraction electrode.

[0040] The sintered ceramic plate 209 is sandwiched between ceramic materials on both the top and bottom in the thickness direction, and has an electrostatic attraction electrode film 208 made of a metal such as W (tungsten) disposed therein. The ceramic material formed into a disk shape with the electrostatic attraction electrode film 208 disposed therein is fired under adjusted sintering conditions so that the ceramic material has a thickness within a range of 0.2 to 0.4 mm when cooled.

[0041] After the second dielectric film 206 is formed into a predetermined shape, a silicone adhesive 207 is applied thereon, and the sintered ceramic plate 209 and the lower layers, the first and second dielectric films 204 and 206, and the heater electrode film 205, are pressed together with the adhesive 207 between them to be integrally formed. The heater electrode film 205 and the electrostatic attraction electrode film 208 are connected to a direct current power supply 109 for the heater electrode and a direct current power supply 110 for the electrostatic attraction electrode, respectively. The base material 201 is also connected to a bias power supply 108. In this embodiment, the electrostatic attraction electrode film 208 may be disposed at the bottom in the thickness direction so as to be exposed on the lower surface of the sintered ceramic plate 209.

[0042] The sintered ceramic plate 209 constitutes the mounting surface of the sample mounting stage 107, and is exposed to the plasma generation space inside the processing chamber 103. For this reason, plasma is generated in the plasma generation space of the processing chamber 103 to remove deposits on the surface inside the processing chamber 103, and if a cleaning wafer is not placed on the mounting surface to cover it, the mounting surface will be subject to increased wear, damage, and contamination due to interactions with the plasma. Furthermore, as the number of product wafers processed in this plasma processing apparatus 100 increases, the upper surface of the sintered ceramic plate 209, which is the wafer mounting surface, will become increasingly damaged and contaminated due to the temperature difference between heating and cooling, interactions with reactive gases, and the like.

[0043] Since such contamination and damage progress reduces the accuracy and yield of wafer processing, the surface of the mounting surface is cleaned and restored to a normal state after a certain number of wafers have been processed or a certain amount of operation time has elapsed. In this embodiment, in order to replace the sintered ceramic plate 209 after such a number of wafers have been processed or after a certain amount of time has elapsed with a new one, the sintered ceramic plate 209 is removed from the top of the sample mounting stage 107. At this time, the members of the sample mounting stage 107 including the base material 201 and the dielectric cover 202 thereon are taken out of the processing chamber 103 as an integrated block, and a new block of the sample mounting stage 107 is replaced and attached. The old block that has been taken out, that is, the sintered ceramic plate 209 is separated from the body of the sample mounting stage 107 by the adhesive 207 and removed.

[0044] Since the adhesive 207 remains partially on the upper surface of the block of the sample stage 107 from which the sintered ceramic plate 209 has been removed and the second dielectric film 206 is exposed on the base, the adhesive 207 or the second dielectric film 206 on the base is removed by polishing or cutting on the block side of the sample stage 107, and the second dielectric film 206 is again formed by thermal spraying and the adhesive 207 is again formed by coating, and the block is joined to a new sintered ceramic plate 209 prepared separately. The block of the sample stage 107 formed again in this way is used as a replacement sample stage 107 for a plasma processing apparatus that needs to be replaced due to the number of processing times or the passage of time, or due to a breakdown or defect.

[0045] Furthermore, the side wall cover 211 arranged to cover the cylindrical side wall of the protruding portion at the top center of the base material 201 is also made of Al, like the sintered ceramic plate 209. 2 O 3 Or Y 2 O 3 The side wall cover 211 is a sintered body formed by firing a ceramic material such as a ceramic material having a predetermined thickness and diameter into a cylindrical shape. The inner peripheral side wall surface of the side wall cover 211 has a diameter slightly larger than the diameter of the side wall of the convex portion of the substrate 201. The side wall of the convex portion is covered with a coating for the side wall of the convex portion, which is made of the same dielectric material as the upper surface of the ring-shaped recess around the convex portion, and the coating is present in the gap between the side wall of the convex portion and the inner peripheral side wall cover 211 when the side wall cover 211 is fitted from above around the convex portion.

[0046] Furthermore, the disk-shaped sintered ceramic plate 209 has a diameter slightly larger than that of the cylindrical protrusion, and when placed on and bonded to the adhesive 207 so that its center coincides with the center of the cylindrical protrusion, its outer periphery protrudes from the outer periphery of the protrusion to the outer periphery, resulting in a so-called overhanging arrangement. In this state, a distance is provided between the lower surface of the outer periphery of the sintered ceramic plate 209 and the upper end of the side wall cover 211 located below, and a second adhesive layer 213 having sufficient resistance to plasma and corrosion and strength against thermal shock is filled between them, covering the inner periphery adhesive 207 or the outer periphery edges of the first and second dielectric films 204, 206.

[0047] The lower end of the sidewall cover 211 is connected to a film of a dielectric material that covers the upper surface of the recess, and thus, plasma, gas, particles of products, etc. in the processing chamber 103 are prevented from penetrating from the lower end into the inside and interacting with the first and second dielectric films 204, 206 and the adhesive 207, thereby preventing contamination of the surfaces of the wafer and the members inside the processing chamber 103. In addition, a quartz or Al (not shown) is provided on the ring-shaped recess on the outer periphery of the protrusion. 2 O 3A susceptor ring having a ring shape made of ceramics such as a ceramic ring is placed on the side wall cover 211 to prevent the side wall cover 211 from being directly exposed to the plasma and causing an interaction therebetween.

[0048] A hole is arranged in the base material 201 from bottom to top, and a temperature sensor 210 is arranged inside the hole to detect the temperature of the top surface of the base material 201. A thermocouple, a platinum resistance thermometer, or the like is used for the temperature sensor 210. The output detected by this temperature sensor 210 is received by the controller 112 via communication means, and from the temperature of the base material 201 detected using a computing unit inside the controller 112, the temperature value or its distribution of the top surface of the sintered ceramic plate 209, which is the mounting surface, or the wafer mounted thereon is estimated using a program stored in the controller 112 or an external storage device such as a hard disk connected to the controller 112 so as to be capable of communication.

[0049] The controller 112 uses a program stored in advance in the storage device to calculate and detect the power value to be output by the heater electrode DC power supply 109 in response to the detection result of the temperature of the sintered ceramic plate 209 or the wafer, and issues a command to the heater electrode DC power supply 109 to output this value, thereby adjusting the amount of heat generated by the heater electrode film 205. Thus, in this embodiment, the detected temperature of the sample mounting stage 107 is fed back to the controller 112, which is a control unit, and the output of the heater electrode film 205 is adjusted via this, thereby achieving the wafer temperature or its distribution that is optimal for processing.

[0050] In this embodiment, the temperature distribution (temperature profile) is changed in the wafer surface direction between each process of a plurality of films to be processed formed on the wafer so as to be suitable for each process. When the process of the upper film is completed and the temperature profile is changed from that for the upper film to that suitable for the lower film, the process is stopped by stopping the supply of bias power from the bias power supply 108, for example, since if the film is processed during this time, the temperature conditions will not be optimal and the processed shape will be significantly different from the intended one. Changing the temperature profile at high speed is important for improving the efficiency of the process.

[0051] In order to change the temperature profile more quickly to the desired one, it is desirable to reduce the heat capacity from the heater electrode film 205 to the electrode surface, and in this embodiment, the thickness of the sintered ceramic plate 209 is set within a predetermined range in order to realize such a high-speed temperature change. On the other hand, it is desirable for the thickness of the sintered ceramic plate 209 to be as thin as possible in order to reduce the heat capacity, but since a voltage for electrostatically attracting the wafer is applied to the electrostatic attraction electrode film 208 built into the sintered ceramic plate 209, there is a lower limit to the thickness of the sintered ceramic plate 209 that does not cause dielectric breakdown.

[0052] Based on findings obtained as a result of the investigation, the inventors set the lower limit of the thickness of the sintered ceramic plate 209 to 0.2 mm by comparing the electric field formed above the sintered ceramic plate 209 by the voltage applied to the electrostatic attraction electrode film 208 in order to obtain the attraction force required to fix the wafer by electrostatic attraction with the electric field at which the ceramic material of the sintered ceramic plate 209 does not cause dielectric breakdown. Also, based on the time required to change the wafer temperature between the multiple films to be processed, the inventors set the upper limit of the thickness of the sintered ceramic plate 209 at 0.4 mm, which can satisfy the required performance.

[0053] Furthermore, in this embodiment, in order to achieve the necessary temperature uniformity within the wafer surface, the heater electrode film 205 is formed by a thermal spraying method, and the thickness of each part of the film as viewed from above is adjusted to improve the uniformity of the distribution of the amount of heat generated by the heater electrode film 205 in the surface direction of the wafer or sample mounting surface. By adjusting the amount of heat generated by each area in this manner, the temperature uniformity within the wafer surface is improved.

[0054] Furthermore, the configuration of the upper edge portion of the dielectric cover 202 of the sample stage 107 shown in the dashed ellipse portion in Fig. 2 will be explained in an enlarged manner with reference to Fig. 3. Fig. 3 is a vertical cross-sectional view showing an enlarged schematic view of the configuration of the upper outer peripheral edge portion of the sample stage and the dielectric cover of the embodiment shown in Fig. 2.

[0055] In this figure, as described above, the outer peripheral edge of the dielectric cover 202 is disposed by bonding the outer peripheral end of the sintered ceramic plate 209 and the cylindrical sidewall cover 211 with the second adhesive layer 213. These members cover the outer peripheral edge of the sidewall and upper surface of the cylindrical protrusion of the base material 201. In particular, the outer peripheral ends of the sintered ceramic plate 209 and the second adhesive layer 213 are aligned in the vertical direction with the outer peripheral sidewall of the sidewall cover 211, and the diameters of the sintered ceramic plate 209 and the sidewall cover 211 are equal or nearly equal to each other.

[0056] Furthermore, the vertical height of the second adhesive layer 213 is set equal to the distance D between the lower surface of the outer periphery of the sintered ceramic plate 209 and the upper end surface of the sidewall cover 211, and the second adhesive layer is filled in the gap between the sidewall cover 211 and the sintered ceramic plate 209 when the former is placed on the adhesive 207 so as to densely fill the gap in the vertical direction (height direction) and the left-right direction (radial direction) in the figure. In this embodiment, the adhesive 207, which is the first adhesive layer, is applied on the second dielectric film 206 with an excess amount so as to protrude from the gap of distance D to the outer periphery of the sidewall cover 211, and the protruding adhesive 207 is removed with a metal brush or the like when the sintered ceramic plate 209 is attached. When the adhesive 207 is removed from the gap, the gap is formed as a ring-shaped space of D1 in the height direction and W in the radial direction, and the ring-shaped space is filled with the adhesive constituting the second adhesive layer.

[0057] In this embodiment, the height D is set to a value within a range of 2.0 to 5.0 mm. The height D is set to be larger than the distance δ between the substrate 201 and the rear surface of the sintered ceramic plate 209, sandwiching the first and second dielectric films 204 and 206, the heater electrode winding 205, and the adhesive 207 (D>δ). When the number of wafers processed within a given period using the plasma generated in the processing chamber 103 while the sintered ceramic plate 209 is placed on the substrate and electrostatically attracted thereon increases, the sintered ceramic plate 209 is consumed due to interaction with the plasma and the reaction product of the highly reactive gas, and the dimensions and material performance are outside the allowable range. Then, the sintered ceramic plate 209 is removed from the sample stage 107, and another unconsumed sintered ceramic plate 209 is replaced and bonded to the sample stage 107 with the newly applied adhesive 207.

[0058] When removing the used sintered ceramic plate 209, the worn sintered ceramic plate 209 may be split from the second adhesive layer 213 and peeled upward, or the sintered ceramic plate 209 and the adhesive 207 may be scraped off together with the second adhesive layer 213. In this case, the distance D is set to be larger than the distance δ so as not to damage the side wall cover 211 which is less likely to be worn. The thickness of the adhesive (first adhesive layer) 207 in this embodiment is set to 0.05 to 1.0 mm.

[0059] With this configuration, the adhesive 207, which is the first adhesive layer, is covered from the lower end of the sidewall of the protruding portion of the base material 201 by the dielectric cover 207 and the second adhesive layer 213 made of a material with high plasma resistance. Therefore, the adhesive 207 and the first and second dielectric films 204, 206 below are not directly exposed to plasma, and wear and contamination are reduced. Furthermore, the thickness D of the filled second adhesive layer 213 (the height of the gap between the sintered ceramic plate 209 and the sidewall cover 211) is made larger than the distance δ between the sintered ceramic plate 209 and the upper surface of the base material 201, and damage to the sidewall cover 211 during replacement of the sintered ceramic plate 209 is reduced. The worn sintered ceramic plate 209 can be replaced, and the wear and deterioration of the adhesive 207 and the first and second dielectric films 204, 206 below are reduced by the sidewall cover 211 with reduced wear, and the operating cost of the plasma processing apparatus 100 is reduced. [Explanation of symbols]

[0060] 100 Plasma treatment device 101 Vacuum container 103 Processing Room 104 Radio source 107 Sample placement table 109 DC power supply for heater electrode 110 DC power supply for electrostatic adsorption electrode 201 Base material 202 Dielectric cover 203 Refrigerant Groove 205 Heater electrode film 207 Adhesive 208 Electrode film for electrostatic adhesion 209 Sintered ceramic plate 210 Temperature sensor.

Claims

1. A plasma processing apparatus having a sample stage disposed in a processing chamber inside a vacuum vessel and having a wafer to be processed placed on an upper surface thereof, the plasma processing apparatus generating plasma in the processing chamber to process the wafer, The plasma processing apparatus includes a sample stage having a cylindrical convex portion disposed on the top of a metal base material, a disk-shaped sintered plate made of dielectric material bonded to the upper surface of the convex portion with a first adhesive layer sandwiched therebetween, on which the wafer is placed, a cylindrical cover which is a cylindrical sintered body made of dielectric material surrounding and covering the side wall of the convex portion, and a ring-shaped second adhesive layer filling the gap between the lower surface of the outer periphery of the sintered plate and the upper end of the cylindrical cover below it.

2. 2. The plasma processing apparatus according to claim 1, wherein the height of the gap between the outer periphery of said sintered plate and the upper end of said cylindrical cover is greater than the distance between said sintered plate and the upper surface of the protruding portion of said base material.

3. 3. The plasma processing apparatus according to claim 1, wherein a different sintered plate, which replaces the sintered plate removed from the sample stage, is attached to the sample stage with the first and second adhesive layers interposed therebetween.

Citation Information

Patent Citations

  • Plasma processing apparatus or sample placing stand

    JP2011258614A

  • Plasma processing apparatus

    JP2012222233A

  • Plasma processing device

    JP2016031956A

  • Annular edge seal with convex inner surface for electrostatic chuck

    JP2017041631A