Molding apparatus, molding method, and method for manufacturing an article
The molding apparatus addresses non-uniformity in imprint material by controlling volatilization based on time, ensuring consistent film thickness and volume, thus stabilizing the imprinting process and enhancing productivity.
Patent Information
- Application Number
- JP2020106234
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-06-19
- Publication Date
- 2024-09-25
- Estimated Expiration
- 2040-06-19
AI Technical Summary
Existing imprint technologies face issues with non-uniform film thickness and volume of imprint material due to time differences between application and imprinting, leading to incomplete filling and uneven film thickness, which can affect subsequent processing steps.
A molding apparatus with a control unit that adjusts the amount of volatilization of the imprint material based on the time until it contacts the mold, ensuring uniform volume and film thickness across multiple shot areas by promoting volatilization in a controlled manner.
The solution ensures consistent volume and film thickness of the imprint material, preventing incomplete filling and unevenness, thereby stabilizing the imprinting process and improving productivity.
Smart Images

Figure 0007555735000001 
Figure 0007555735000002 
Figure 0007555735000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a molding apparatus, a molding method, and a method for manufacturing an article. [Background technology]
[0002] In recent years, there has been an increasing demand for miniaturization of semiconductor devices and MEMS (Micro Electro Mechanical Systems). In addition to conventional photolithography technology, microfabrication technology has been attracting attention, in which an imprint material (composition) on a substrate is molded with a mold and the imprint material pattern is formed on the substrate. This technology, also known as imprint technology, is capable of forming fine structures on the order of a few nanometers on a substrate.
[0003] For example, one imprinting technique is the photocuring method. In an imprinting apparatus that employs this photocuring method, a photocurable imprinting material is first applied to a shot area, which is an imprinting area on a substrate. Next, while aligning the pattern portion of a mold (master) with the shot area, the mold and the imprinting material applied to the substrate are brought into contact (imprinted) and the mold is filled with the imprinting material. The imprinting material is then hardened by irradiation with light, and the mold and imprinting material are then separated (mold release), thereby forming a pattern of the imprinting material on the substrate.
[0004] In recent years, in order to improve the productivity of equipment, an imprinting method has become known in which imprinting material is applied to multiple areas at once, followed by continuous imprinting and release. However, the time between application of the imprinting material and imprinting differs for each area. As a result, the applied imprinting material in each area evaporates, and the volume of the imprinting material differs before imprinting, resulting in problems such as a lack of imprinting material, which results in the pattern being unfilled, or a distribution in the film thickness of the imprinting material within the substrate.
[0005] On the other hand, in order to solve problems related to the volatilization of the imprint material, Patent Document 1 describes a method in which the imprint material is applied to each imprint region immediately before imprinting in that imprint region. Furthermore, Patent Document 2 describes a method in which the gas supply conditions during imprinting are different between the imprint regions on the outer side of the substrate and the imprint regions near the center. Furthermore, Patent Document 2 describes a method in which the amount of the imprint material discharged is adjusted depending on the time after the imprint material is applied. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent No. 5275419 [Patent Document 2] Patent No. 4654224 Summary of the Invention [Problem to be solved by the invention]
[0007] However, Patent Document 1 does not consider the problem of a difference in the thickness of the imprint material occurring due to the time difference between applying the imprint material and imprinting, since the imprint method does not apply the imprint material continuously to a plurality of regions. Patent Document 2 also does not consider the problem of a difference in the thickness of the imprint material occurring due to the time difference between applying the imprint material and imprinting.
[0008] Therefore, an object of the present invention is to provide a molding apparatus capable of making the volume or film thickness of a composition uniform regardless of the time from when the composition is applied until it comes into contact with a mold. [Means for solving the problem]
[0009] A molding apparatus according to one aspect of the present invention for solving the above-mentioned problems is a molding apparatus that molds a composition on a substrate using a mold, and determines the amount of the composition based on the time from when the composition is applied to a shot region on the substrate to when the composition comes into contact with the mold. To promote evaporation A control unit for adjusting the amount of volatilization. 、 The control unit is characterized by adjusting the amount of evaporation so that the volume or film thickness of the composition when the mold is brought into contact with the composition is uniform across a plurality of shot regions. Effect of the Invention
[0010] According to the present invention, it is possible to provide a molding apparatus capable of making the volume or film thickness of a composition uniform regardless of the time from when the composition is applied until when it comes into contact with a mold. [Brief description of the drawings]
[0011] [Figure 1] 1 is a schematic cross-sectional view of an imprint apparatus according to a first embodiment. [Diagram 2] 1A to 1C are schematic cross-sectional views illustrating a coating step, an imprinting step, and a demolding step in a general imprint process. [Diagram 3] 11A and 11B are diagrams showing an example of the volatilization amount of the imprint material in each shot region. [Figure 4] 1A to 1C are schematic cross-sectional views illustrating a coating step, a stamping step, and a demolding step in Example 1. [Diagram 5] 1 is a flowchart illustrating a coating step, a stamping step, and a demolding step in the first embodiment. [Figure 6] FIG. 2 is a schematic diagram of the volatilization mechanism in Example 1. [Figure 7] 13 is a diagram showing an example of the volatilization distribution and illuminance distribution of the imprint material in Example 2. FIG. [Figure 8] FIG. 1 is a schematic diagram of the volatilization mechanism in Example 3. [Figure 9] 13A to 13C are diagrams illustrating a process performed by a planarization apparatus according to a fourth embodiment. [Figure 10] FIG. 2 is a schematic diagram for explaining a method for manufacturing an article. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Preferred embodiments of the present invention will be described in detail below with reference to the drawings. In the following examples, an imprinting apparatus is used as a molding apparatus for molding a composition on a substrate using a mold. In each drawing, the same members are given the same reference numbers, and duplicated descriptions are omitted.
[0013] Example 1 1 is a diagram showing an example of the configuration of an imprinting apparatus (lithography apparatus) 1 as a molding apparatus that uses a mold to mold a composition on a substrate 10 in this embodiment. The imprinting apparatus 1 brings an imprinting material (composition) supplied onto the substrate 10 into contact with a mold 7 (original, template, mold). Then, by applying energy for curing to the imprinting material 9, the apparatus molds a cured composition onto which the concave-convex pattern of the mold 7 has been transferred.
[0014] Here, a curable composition (sometimes referred to as an imprint material in an uncured state) that is cured by application of curing energy is used as the imprint material 9. As the curing energy, electromagnetic waves, heat, etc. are used. As the electromagnetic waves, for example, infrared rays, visible rays, ultraviolet rays, etc., whose wavelengths are selected from the range of 150 nm or more and 1 mm or less are used.
[0015] The curable composition is a composition that is cured by irradiation with light or by heating. Among them, the photocurable composition that is cured by light contains at least a polymerizable compound and a photopolymerization initiator, and may contain a non-polymerizable compound or a solvent as necessary. The non-polymerizable compound is at least one selected from the group consisting of a sensitizer, a hydrogen donor, an internal mold release agent, a surfactant, an antioxidant, a polymer component, and the like.
[0016] The imprint material 9 is applied in the form of a film on the substrate 10 by a spin coater or a slit coater. Alternatively, the imprint material 9 may be applied in the form of droplets, or in the form of islands or a film formed by a plurality of droplets joining together, on the substrate 10 by a liquid ejecting head. The viscosity of the imprint material 9 (viscosity at 25° C.) is, for example, 1 mPa s or more and 100 mPa s or less.
[0017] In this embodiment, the imprint apparatus 1 will be described as employing a photocuring method in which the imprint material 9 is cured by irradiation with light. In the following, the direction parallel to the optical axis of an irradiation optical system, which will be described later, that irradiates light onto the imprint material 9 on the substrate 10 is defined as the Z-axis direction, and two directions that are orthogonal to each other in a plane perpendicular to the Z-axis direction are defined as the X-axis direction and the Y-axis direction.
[0018] Here, each part of the imprinting apparatus 1 will be described with reference to Fig. 1. The imprinting apparatus 1 may include a mold holding section 3, an irradiation section 2, a substrate stage (moving section) 4, an application section (composition supplying section) 5, an auxiliary member 15, a control section 6, and an alignment measurement section 21. The imprinting apparatus 1 also includes a base plate 22 on which the substrate stage 4 is placed and which forms a reference plane, a bridge base plate 23 to which the mold holding section 3 is fixed, and a support 25 extending from the base plate 22 and supporting the bridge base plate 23 via a vibration isolator 24 to remove vibrations from the floor surface. The imprinting apparatus 1 may also include a mold transport section for transporting the mold 7 between the outside of the apparatus and the mold holding section 3, a substrate transport section for transporting the substrate 10 between the outside of the apparatus and the substrate stage 4, and the like, both of which are not shown.
[0019] The mold holding unit 3 includes a mold chuck 11 that attracts and holds the mold 7 by vacuum suction force or electrostatic force, and a mold moving mechanism 12 that holds the mold chuck 11 and moves the mold 7 (mold chuck 11). The mold chuck 11 and the mold moving mechanism 12 have openings in the center (inside) so that the light from the irradiation unit 2 is irradiated onto the imprint material 9 on the substrate 10.
[0020] The mold moving mechanism 12 moves the mold 7 in the Z-axis direction so as to selectively press (impress) the mold 7 onto the imprint material 9 on the substrate 10, or pull (release) the mold 7 away from the imprint material 9 on the substrate 10. Actuators that can be used for the mold moving mechanism 12 include, for example, a linear motor or an air cylinder.
[0021] The mold moving mechanism 12 may be composed of a plurality of drive systems, such as a coarse movement drive system and a fine movement drive system, in order to position the mold 7 with high accuracy. The mold moving mechanism 12 may be configured to be capable of moving the mold 7 not only in the Z-axis direction, but also in the X-axis direction or the Y-axis direction. Furthermore, the mold moving mechanism 12 may be configured to have a tilt function for adjusting the position of the mold 7 in the θ (rotation around the Z-axis) direction and the inclination of the mold 7.
[0022] The mold 7 has a rectangular outer periphery, and has a pattern portion 7a with a three-dimensional pattern (a concave-convex pattern to be transferred to the substrate 10, such as a circuit pattern) formed on the surface (pattern surface) facing the substrate 10. The mold 7 is made of a material capable of transmitting the light 8, such as quartz. The mold 7 may also have a cavity, which is circular in plan view and has a certain depth, on the surface onto which the light 8 is irradiated.
[0023] The irradiation unit 2 has a light source and an irradiation optical system (not shown), and the irradiation optical system is equipped with a combination of optical elements described later. The irradiation unit 2 irradiates the imprint material 9 on the substrate 10 with light 8 through the mold 7 in the imprint process (molding process). The irradiated light is, for example, ultraviolet light, but is not limited to this and may be light other than ultraviolet light as long as it has a wavelength that can appropriately harden the imprint material 9. The irradiation unit 2 may include a light source and optical elements (lens, mirror, light shield, etc.) for adjusting the light irradiated from the light source to a state of light 8 appropriate for the imprint process (light intensity distribution, illumination area, etc.). In this embodiment, since the photocuring method is adopted, the imprint device 1 has the irradiation unit 2. However, for example, when the thermal curing method is adopted, the imprint device 1 will have a heat source for curing the imprint material (thermosetting imprint material) instead of the irradiation unit 2.
[0024] The substrate stage 4 may include a substrate chuck 14 that attracts and holds the substrate 10 by vacuum suction force or electrostatic force, and a stage driving mechanism 16 that holds the substrate chuck 14 and moves the mold 7. The substrate stage 4 is movable within the XY plane. When pressing the pattern portion 7a of the mold 7 against the imprint material 9 on the substrate 10, the position of the substrate stage 4 is adjusted to align the positions of the mold 7 and the substrate 10 with each other. Actuators that can be applied to the substrate stage 4 include, for example, a linear motor and an air cylinder. Furthermore, the substrate stage 4 may be configured to be able to move the substrate 10 not only in the X-axis direction or the Y-axis direction, but also in the Z-axis direction.
[0025] Note that the imprinting and release of the mold 7 in the imprint apparatus 1 is achieved by moving the mold 7 in the Z-axis direction. However, it may also be achieved by moving the substrate 10 in the Z-axis direction. Also, imprinting and release of the mold 7 may also be achieved by moving both the mold 7 and the substrate 10 relatively in the Z-axis direction. Also, the substrate stage 4 may be configured to have a tilt function for adjusting the position of the substrate 10 in the θ (rotation around the Z-axis) direction and the inclination of the substrate 10.
[0026] The substrate stage 4 also has a plurality of reference mirrors 17 on its side corresponding to the X, Y, Z, ωx, ωy, and ωz directions. In contrast, the imprint apparatus 1 has a plurality of laser interferometers 18 that measure the position of the substrate stage 4 by irradiating each of these reference mirrors 17 with a beam of helium neon or the like. Note that FIG. 1 illustrates only one pair of the reference mirror 17 and the laser interferometer 18. The laser interferometer 18 measures the position of the substrate stage 4 in real time, and the control unit 6, which will be described later, executes positioning control of the substrate 10 (substrate stage 4) based on the measurement value at that time. An encoder may also be used to measure the position of the substrate stage 4.
[0027] The auxiliary member 15 is disposed around the substrate chuck 14 so as to surround the substrate 10 held by the substrate chuck 14. In addition, the auxiliary member 15 is disposed so that the upper surface of the auxiliary member 15 and the upper surface of the substrate 10 held by the substrate chuck 14 are at approximately the same height. The substrate chuck 14 is mounted on a stage driving mechanism 16.
[0028] The auxiliary member 15 has a function of preventing the intrusion of gas having at least one of the properties of high solubility or high diffusion in at least the imprint material 9 described later into the optical path between the reference mirror 17 and the laser interferometer 18. In addition, the presence of the auxiliary member 15 has the effect of keeping the concentration of the gas supplied from the first gas supply unit high when imprinting a shot area arranged around the substrate 10. Here, there may be a difference in height between the upper surface of the auxiliary member 15 and the upper surface of the substrate 10 held by the substrate chuck 14, as long as the difference in gas concentration between the space on the upper surface of the auxiliary member 15 and the space on the upper surface of the substrate 10 does not exceed 1%. For example, the difference in height between the upper surface of the auxiliary member 15 and the upper surface of the substrate 10 held by the substrate chuck 14 may be 1 mm or less. More preferably, the difference in height between the upper surface of the auxiliary member 15 and the upper surface of the substrate 10 held by the substrate chuck 14 may be 0.1 mm or less.
[0029] The substrate 10 is made of glass, ceramics, metal, an imprint material, or the like, and may have a member made of a material different from that of the substrate 10 formed on its surface as necessary. Specific examples of the substrate 10 include silicon wafers, compound semiconductor wafers, and glass wafers containing quartz as a material. The substrate 10 may also be a glass substrate for producing a replica mask from a master mask by imprint processing.
[0030] The application unit 5 is installed near the mold holding unit 3, and applies the imprint material 9 to at least one shot region (molding region, imprint region) present on the substrate 10. The application unit 5 employs an inkjet method as a coating method, and may include a container 19 that stores the imprint material 9 in an uncured state, and a discharge unit 20. The container 19 is preferably one that can manage the imprint material 9 while maintaining an atmosphere inside the container 19 that does not cause a curing reaction of the imprint material 9, for example, containing a small amount of oxygen. In addition, the material of the container 19 is preferably one that does not allow particles or chemical impurities to be mixed into the imprint material 9. The discharge unit 20 has, for example, a piezo-type discharge mechanism (inkjet head) that includes a plurality of discharge ports. The application amount (discharge amount) of the imprint material 9 can be adjusted in the range of 0.1 to 10 pL / drop, and is usually used at about 1 pL / drop in many cases. The total application amount of the imprint material 9 is determined by the density of the pattern portion 7a and the desired remaining film thickness.
[0031] The alignment measurement unit 21 irradiates the alignment marks formed on the mold 7 and the substrate 10 with light 8 and detects the alignment light reflected from the mold 7, thereby measuring (detecting) the amount of relative positional deviation between the mold 7 and the substrate 10. The measurement of the amount of relative positional deviation is performed while the mold 7 and the imprint material 9 are in contact with each other. The amount of relative positional deviation measured here is used to reduce the positional deviation by adjusting the mold moving mechanism 12 and the stage driving mechanism 16. In addition, the positional deviation can also be reduced by deforming the shape of the pattern portion 7a of the mold 7 or the shot area of the substrate 10 using a shape correction unit (mold correction unit) not shown.
[0032] The control unit 6 is composed of at least one computer including a CPU, memory, etc. The control unit 6 is connected to each component of the imprint apparatus 1 via a line, and performs overall control of the operation and adjustment of each component of the imprint apparatus 1 according to a program stored in the memory. The control unit 6 may be configured integrally with other parts of the imprint apparatus 1 (in a common housing), or may be configured separately from other parts of the imprint apparatus 1 (in a different housing).
[0033] Here, a general imprint method (imprint process) performed by the imprint apparatus 1 will be described.
[0034] First, the control unit 6 causes the substrate transport unit to place and fix the substrate 10 on the substrate stage 4. Next, the control unit 6 drives the stage drive mechanism 16 to appropriately change the position of the substrate 10, while causing the alignment measurement unit 21 to sequentially measure the alignment marks on the substrate 10, thereby detecting the position of the substrate 10 with high accuracy. The control unit 6 then calculates each transfer coordinate from the detection results, and causes sequential formation of patterns for each predetermined shot based on the calculation results (step and repeat).
[0035] Here, as a flow of pattern formation for one shot area, the control unit 6 first uses the stage driving mechanism 16 to position an application position on the substrate 10 (a specific position on the shot area) under the outlet of the discharge unit 20 that discharges the imprint material 9. The control unit 6 then controls the application unit 5 to apply the imprint material 9 to the shot area on the substrate 10 (application step). Next, the control unit 6 uses the stage driving mechanism 16 to move and position the substrate 10 so that the shot area is located at a pressing position directly under the pattern unit 7a.
[0036] Next, the control unit 6 performs alignment between the pattern portion 7a and the pattern on the substrate 10 side on the shot area, and performs magnification correction of the pattern portion 7a by the magnification correction mechanism. After that, the mold moving mechanism 12 is driven. When the pattern portion 7a is pressed (contacted) against the imprint material 9 on the shot area, the pattern portion 7a is deformed into a convex shape toward the substrate 10 and pressed against the imprint material 9 (imprinting process). By this pressing, the imprint material 9 fills the concave-convex pattern of the pattern portion 7a. The control unit 6 judges the completion of pressing by a load sensor (not shown) installed inside the mold holding unit 3. In this state, the control unit 6 controls the irradiation unit 2 to irradiate the imprint material 9 with light 8 from the back surface (upper surface) of the mold 7 for a predetermined time, and hardens the imprint material 9 by the light 8 transmitted through the mold 7 (hardening process). Then, after the imprint material 9 is hardened, the control unit 6 drives the mold moving mechanism 12 again to separate the pattern portion 7a from the substrate 10 (mold releasing process).
[0037] As a result, a pattern (layer) of the imprint material 9 having a three-dimensional shape following the uneven pattern of the pattern portion 7a is formed on the surface of a certain shot area on the substrate 10. By performing such a series of imprint operations multiple times while changing the shot area by driving the substrate stage 4, the imprint apparatus 1 can form multiple patterns of the imprint material 9 on a single substrate 10.
[0038] Furthermore, when the mold 7 is pressed against the imprint material 9 on the substrate 10 to fill the pattern portion 7a with the imprint material 9, air present between the mold 7 and the substrate 10 may get into the pattern portion 7a, causing defects in the formed pattern after hardening. Therefore, it is preferable to supply a gas having at least one of the properties of being highly soluble or highly diffusible in the imprint material 9 to the space between the mold 7 and the substrate 10.
[0039] 2A and 2B are schematic diagrams showing the coating step, the imprinting step, and the demolding step in the general imprinting process. FIG. 2A is a schematic diagram for explaining the coating step in the general imprinting process. FIG. 2B is a schematic diagram showing the imprinting step and the demolding step in the general imprinting process. FIG. 2C shows the state of the substrate 10 after the general imprinting process has been completed.
[0040] 2(A), in a typical coating process, the imprint material 9 is continuously applied to a plurality of shot areas on a substrate 10. In this embodiment, the shot area to which the imprint material 9 is first applied is defined as shot area A. The shot area to which the imprint material 9 is second applied is defined as shot area B, and the imprint material 9 is applied to a plurality of shot areas, and the xth shot area to which the imprint material 9 is last applied is defined as shot area X. In this manner, the imprint material 9 is continuously applied on the substrate 10 from shot area A to shot area B, up to the final shot area X.
[0041] Next, as shown in FIG. 2B, in a typical imprinting process, the mold 7 is pressed against the imprint material 9 in succession in a plurality of shot regions. In a typical demolding process, the mold 7 is released from the imprint material 9 after pressing the mold 7. Before the demolding, a hardening process is performed to harden the imprint material 9. FIG. 2C shows the state of the substrate 10 after the typical imprinting process is completed. In this way, when typical imprinting processes are performed sequentially, the time from application of the imprint material 9 to imprinting the mold 7 and releasing it is significantly different between the shot region A where the imprinting process was performed first and the shot region X where the imprinting process was performed last. This is because the application of the imprint material 9 can be performed in a relatively short time, whereas the imprinting process takes a relatively long time.
[0042] Many types of imprint material 9 have the property of volatilizing over time. Therefore, by the time the shot area X is imprinted, the imprint material 9 applied to each shot area on the substrate 10 gradually volatilizes based on the time elapsed from application to imprinting. As the imprint material 9 volatilizes, the volume of the imprint material 9 applied to each shot area gradually decreases. Here, in a state in which the volume of the imprint material 9 has decreased, the mold 7 is imprinted onto the imprint material 9 and released. In that case, the volume (or film thickness) of the imprint material 9 required for the pattern portion 7a may be insufficient, and a state in which the imprint material 9 is not completely filled in the pattern portion 7a (pattern unfilled) may occur.
[0043] Furthermore, if the volume of the imprint material 9 is reduced as described above, the residual layer thickness (RLT) of the imprint material 9 after the imprint process is also reduced. If the residual layer thickness is reduced, it may affect the subsequent processing steps, and may result in a situation where the desired processing cannot be performed.
[0044] As described above, in conventional imprinting processes, the time from application of the imprinting material 9 to imprinting of the mold 7 differs for each shot area, which can result in unfilled patterns in the substrate 10 or a decrease in the remaining film thickness (unevenness in the remaining film thickness). On the other hand, if the amount of imprinting material 9 applied is increased too much from the beginning, there is a problem that the overflowing imprinting material 9 can adversely affect other imprinting processes.
[0045] Therefore, in this embodiment, a volatilization control process (volatilization adjustment process) is provided that controls (adjusts) the amount of volatilization of the imprint material 9 applied to each shot area so as to differ depending on the time from the application process of applying the imprint material 9 to the imprinting process. Specifically, the volume or film thickness of the imprint material 9 before imprinting of each shot area is made uniform (evened) by intentionally promoting the volatilization of the imprint material 9 in a predetermined shot area on the substrate 10. By making the imprint material 9 uniform, it is possible to make the imprint material 9 in each shot area have a desired volume or film thickness when performing the imprint process.
[0046] The imprint process of the imprint apparatus 1 in this embodiment will be described in detail below with reference to Figs. 3 to 5. Fig. 3 is a diagram showing an example of the amount of volatilization of the imprint material 9 in each shot area. Fig. 4 is a schematic diagram showing the coating process, imprinting process, volatilization process, and release process of the imprint process in this embodiment. Fig. 4(A) is a schematic diagram showing the coating process in the imprint process in this embodiment. Fig. 4(B) is a schematic diagram showing the volatilization process in the imprint process in this embodiment. Fig. 4(C) is a schematic diagram showing the imprinting process in the imprint process in this embodiment. Fig. 4(D) is a schematic diagram showing the release process in the imprint process in this embodiment.
[0047] Fig. 5 is a flowchart of each step corresponding to the imprint process shown in Fig. 4. The imprint process of this embodiment will be described below with reference to Fig. 5. Each operation (process) shown in the flowchart of Fig. 5 is controlled by the control unit 6 executing a computer program.
[0048] First, in step S101, the control unit 6 determines the number of shot areas to be subjected to the imprint process continuously, and calculates the time from when the imprint material 9 is applied to each shot area until the mold 7 is imprinted, depending on the number.
[0049] Next, in step S102, the control unit 6 calculates the volume of the imprint material 9 that volatilizes and remains in each shot area from when the imprint material 9 is applied to when the mold 7 is imprinted, based on the time calculated in step S101. That is, the control unit 6 calculates the remaining volume of the imprint material 9 after volatilization in each shot area based on the time for each shot area from when the imprint material 9 is applied to when the mold 7 is imprinted, calculated in step S101.
[0050] Next, in step S103, the control unit 6 calculates the shot area in which the volume of the imprint material 9 in the multiple shot areas calculated in step S102 is the smallest. After the calculation, the volatilization amount of the imprint material 9 in each shot area is calculated so that the volume of the imprint material 9 in the multiple shot areas in which the imprint process is performed successively is the same as the volume of the shot area in which the volume is the smallest. That is, the volume of the shot area in which the time from application of the imprint material 9 to contact with the mold 7 is the longest is used as a reference. Then, the volatilization amount is calculated so that the volume of the imprint material 9 in each shot area other than the shot area is approximately the same as the minimum volume at the time of each imprint. Here, the relationship between each shot area in which the imprint process is performed successively and the volatilization amount of the imprint material 9 is, for example, as shown in FIG. 3.
[0051] Next, in step S104, as shown in Fig. 4(A), the imprint material 9 is applied continuously to the multiple shot regions calculated in step S101. When applying the imprint material 9, the dispensing arrangement of the imprint material 9 is changed so that the remaining film thickness (film thickness after imprinting) in the shot region where the volume of the imprint material 9 is smallest is the desired remaining film thickness. Alternatively, it is desirable to apply a larger amount of the imprint material 9 in advance. However, as described above, problems arise if the amount of application is too large, so the amount of application is kept within an appropriate range. The desired remaining film thickness is, for example, in the range of about 30 nm to 50 nm.
[0052] Next, in step S105, based on the amount of volatilization of the imprint material 9 in the multiple shot regions calculated in step S103, as exemplified in Fig. 4(B), a volatilization mechanism (adjustment unit) 30 is used to promote volatilization of the imprint material 9 in the multiple shot regions (volatilization step). In the process of promoting volatilization of the imprint material 9 in the multiple shot regions, it is preferable to volatilize the imprint material 9 in the reverse order to the order in which the imprint material 9 was applied to the multiple shot regions in step S104. This reduces unnecessary operations during the imprint process and improves throughput.
[0053] At this time, gas is supplied to or recovered from each shot area at a pressure that results in the amount of volatilization shown in Fig. 3. As a result, at the stage where the process of controlling the amount of volatilization in Fig. 4(B) is completed, the magnitude relationship of the volumes of the imprint material 9 becomes shot area A<shot area B< ~ <shot area X. As a result, as shown in Fig. 4(C), the volumes (film thickness) of the imprint material 9 when the imprinting operation is performed on each shot area become approximately the same. Also, as shown in Fig. 4(D), the remaining film thickness of each shot area after the imprinting process becomes approximately uniform.
[0054] The volatilization mechanism 30 is a mechanism having a function of supplying or recovering gas to the atmosphere in the vicinity (surroundings) of the imprint material 9 applied to the substrate 10. The volatilization mechanism 30 supplies gas to the atmosphere in the vicinity of the imprint material 9 through a gas supply port 31. When recovering gas from the atmosphere in the vicinity of the imprint material 9, the gas is recovered through a gas recovery port 31 provided in the volatilization mechanism 30. Furthermore, the volatilization mechanism 30 can be driven in the X-axis direction, Y-axis direction, and Z-axis direction by a drive unit (actuator) not shown.
[0055] In this embodiment, the gas supply port 31 and the gas recovery port 31 are configured to selectively supply and recover gas using a common hole structure (hole portion). However, the gas supply port 31 and the gas recovery port 31 may be provided in the volatilization mechanism as different hole structures. In the volatilization mechanism 30 of this embodiment, the same flow path is used for the gas supplied from the gas recovery port 31 and the gas recovered by the gas recovery port 31. However, this is not limited to this, and two or more flow paths may be formed in the volatilization mechanism 30 by providing, for example, a partition plate or a tube so that the flow path when supplying gas and the flow path when recovering gas are separate flow paths.
[0056] FIG. 6 is a schematic diagram of the volatilization mechanism 30 of this embodiment. The volatilization mechanism 30 may have a structure in which the gas supply port 31 and the gas recovery port 31 that supply or recover gas are arranged in a line as shown in FIG. 6(A), or may have a structure that can cover one entire shot area as shown in FIG. 6(B). The vertical length of the volatilization mechanism 30 in FIG. 6(A) and FIG. 6(B) corresponds to the vertical width of one shot area. However, this is not limited to this, and one or more gas supply ports 31 and gas recovery ports 31 may have a substantially rectangular structure. In addition, the gas supply port 31 and the gas recovery port 31 have a hole structure, but in order to supply and recover gas more uniformly, they may have a mesh structure or a porous structure. When the volatilization mechanism 30 has a structure as shown in FIG. 6(A), in step S105, the volatilization mechanism 30 supplies or recovers gas while driving the substrate stage 4 to scan as shown in FIG. 4(B). When the volatilization mechanism 30 has the structure shown in FIG. 5B, the substrate stage 4 is driven in step S105 by stepping it for each shot area, while the volatilization mechanism 30 supplies or recovers gas.
[0057] The volatilization mechanism 30 supplies or recovers gas to the atmosphere in the vicinity of the imprint material 9, thereby lowering the vapor pressure of the volatile components of the imprint material 9 and promoting the volatilization of the imprint material 9. Furthermore, the control unit 6 controls the amount of gas supplied, the amount of gas recovered, the gas supply time, or the gas recovery time in a linked manner, thereby promoting the volatilization of the imprint material 9 and enabling control to efficiently adjust the amount of volatilization of the imprint material 9. Note that the vicinity of the imprint material 9 may be any range in which the volatilization of the imprint material 9 applied to each shot area can be promoted (covered) for each shot area.
[0058] Furthermore, the type of gas to be supplied is not particularly limited as long as it does not adversely affect the imprint material 9, but for example, a gas containing a volatile component of the imprint material 9 may be supplied. By changing the concentration of the volatile component of the imprint material 9, it is possible to control the amount of evaporation of the imprint material 9 by promoting the evaporation of the imprint material 9.
[0059] Returning to FIG. 5, next, in step S106, the control unit 6 brings the mold 7 into contact with the imprint material 9 for the shot area (shot area A) where the imprint material 9 was applied first, as shown in FIG. 4(C) (imprinting process). Next, in step S107, while the imprint material 9 is in contact with the mold 7, the irradiation unit 2 irradiates the imprint material 9 with light, thereby hardening the imprint material 9. Next, in step S108, the mold 7 is separated from the imprint material 9 (mold releasing process). This is also performed for the next shot area, shot area B, and after performing the process up to the final shot area X, the imprint process is terminated.
[0060] In this manner, in this embodiment, the imprint material 9 is applied continuously to a plurality of shot regions. After application, gas is supplied to or recovered from the atmosphere near the imprint material 9 depending on the time from application of the imprint material 9 to contact of the mold 7 with the imprint material 9. This allows control to be performed to promote volatilization of the imprint material 9 in a plurality of shot regions and adjust the volatilization amount of the imprint material 9 to be different, and makes it possible to uniformize the volume or film thickness of the imprint material 9 before imprinting. Furthermore, it is possible to reduce a state in which the imprint material 9 is not completely filled in the pattern portion 7a and to reduce unevenness in the remaining film thickness.
[0061] As described above, in this embodiment, an imprinting apparatus (molding apparatus) can be provided that can uniformize the volume or film thickness of the imprinting material 9 in multiple shot areas before imprinting by adjusting the amount of volatilization of the imprinting material 9 in multiple shot areas.
[0062] Example 2 In the first embodiment, a volatilization mechanism using a method of supplying or recovering gas to promote volatilization of the imprint material 9 was described, but in the present embodiment, a volatilization mechanism having a function of irradiating light to the imprint material 9 will be described. Note that matters not mentioned here and the configuration of the imprint apparatus 1 are the same as those in the first embodiment. In the present embodiment, the method of promoting volatilization of the imprint material 9 is different from that in the first embodiment, but since promoting volatilization of the imprint material 9 itself is the same as in the first embodiment, a description of the process shown in FIG. 5 will be omitted.
[0063] The volatilization mechanism 30 of this embodiment has at least one or more light sources 32 that irradiate light to the imprint material 9. The light sources 32 use light sources with a wavelength band (wavelength region) that does not include the wavelength that hardens the imprint material 9. The volatilization mechanism 30 of this embodiment also functions as an irradiation unit that irradiates light to the imprint material 9. Here, if the volatilization mechanism 30 of this embodiment irradiates the imprint material 9 with light that includes a wavelength that hardens (chemically reacts) the imprint material 9, as with the irradiation unit 2, the physical properties of the imprint material 9 will change, causing adverse effects in the imprinting process, etc.
[0064] That is, in the stamping process or the like, for example, the viscosity of the imprint material 9 may change, making it difficult for the imprint material 9 to wet and spread when stamped, and as a result, air bubbles may be easily trapped. Furthermore, it takes longer for the air bubbles to disappear, resulting in a decrease in productivity. And if the imprint material 9 hardens, problems such as the mold 7 being unable to be stamped onto the imprint material 9 and being unable to form a pattern arise. Therefore, the volatilization mechanism 30 of this embodiment needs to use a light source with a wavelength band (wavelength region) that does not harden the imprint material 9.
[0065] Examples of light sources used in the volatilization mechanism 30 include LEDs, laser diodes (LDs), halogen lamps, excimer lamps, cold cathode fluorescent lamps, and HID lamps. Other light source configurations may be used, but in this embodiment, small and lightweight LEDs and LDs are suitable. The volatilization mechanism 30 of this embodiment irradiates light onto the imprint material 9 applied on the substrate 10 and its surroundings. This increases the temperature near the imprint material 9, and promotes the volatilization of the imprint material 9.
[0066] In this embodiment, light is irradiated onto the imprint material 9 in the multiple shot regions or onto the periphery thereof from the volatilization mechanism 30. The control unit 6 controls the illuminance and irradiation time of the irradiated light for each of the multiple shot regions, thereby accelerating the volatilization of the imprint material 9 in the multiple shot regions and adjusting the amount of volatilization of the imprint material 9.
[0067] FIG. 7 is a diagram showing an example of the volatilization distribution and illuminance distribution of the imprint material 9 in the second embodiment. The light sources 32 of the volatilization mechanism 30 may be arranged in a line as in FIG. 6(A) of the first embodiment, or may be arranged to cover the entire shot area as in FIG. 6(B), but are not limited thereto. Furthermore, when the amount of volatilization of the imprint material 9 is distributed in one shot area as in FIG. 7(A), the illuminance of each of the multiple light sources 32 is changed. Alternatively, an optical system for forming an illuminance distribution in the shot area is provided in the volatilization mechanism 30. Then, by irradiating the imprint material 9 in the shot area with light, an illuminance distribution is formed in the shot area as in FIG. 7(B), and a distribution is generated in the amount of volatilization of the imprint material 9 in the shot area. As a result, even if the amount of volatilization of the imprint material 9 is distributed in one shot area, the volume or film thickness of the imprint material 9 before imprinting can be made uniform.
[0068] In this manner, in this embodiment, the imprint material 9 is applied continuously to multiple regions. After application, light is irradiated onto the imprint material 9 or its periphery depending on the time from application of the imprint material 9 to contact of the mold 7 with the imprint material 9. This allows control to promote volatilization of the imprint material 9 in multiple shot regions and adjust the amount of volatilization of the imprint material 9, making it possible to uniformize the volume or film thickness of the imprint material 9 before imprinting. Furthermore, it is possible to reduce a state in which the imprint material 9 is not completely filled in the pattern portion 7a and to reduce unevenness in the remaining film thickness.
[0069] As described above, in this embodiment, the amount of volatilization of the imprint material 9 in multiple shot areas is adjusted in the same manner as in embodiment 1. This makes it possible to provide an imprint apparatus (molding apparatus) that can uniformize the volume or film thickness of the imprint material 9 in multiple shot areas before imprinting.
[0070] Example 3 In the second embodiment, a volatilization mechanism using a method of irradiating light from a light source 32 to promote volatilization of the imprint material 9 was described, but in the present embodiment, a temperature adjustment mechanism having a temperature adjustment function such as a heater will be described. Note that matters not mentioned here and the configuration of the imprint apparatus 1 are similar to those in the first and second embodiments. In the present embodiment, the method of promoting volatilization of the imprint material 9 is different from that in the first or second embodiment, but since promoting volatilization of the imprint material 9 itself is similar to that in the first and second embodiments, a description of the process shown in FIG. 5 will be omitted. Note that the temperature adjustment mechanism 33 in the present embodiment also functions as the volatilization mechanism 30.
[0071] FIG. 8 is a schematic diagram of the temperature adjustment mechanism 33 of the third embodiment. The temperature adjustment mechanism 33 is provided on the substrate stage 4 as shown in FIG. 8, and is disposed between the substrate 10 and the stage driving mechanism 16. Furthermore, as described above, the temperature adjustment mechanism 33 has a temperature adjustment function such as a heater. The temperature adjustment mechanism 33 of this embodiment also functions as a heating unit that applies heat to warm the atmosphere near the imprint material 9. The control unit 6 controls the temperature adjustment mechanism 33 to adjust the heating temperature and heating time of the substrate 10. The amount of volatilization of the imprint material 9 can be adjusted by heating the atmosphere near the imprint material 9, thereby promoting the volatilization of the imprint material 9. This makes it possible to make the volume or film thickness of the imprint material 9 before imprinting uniform. Note that heating to a temperature at which the physical properties of the imprint material 9 change is not preferable because it adversely affects the imprinting process and the like. The adverse effects in the imprinting process and the like are the same as those in the first embodiment.
[0072] In this embodiment, one temperature adjustment mechanism 33 is disposed between the substrate 10 and the stage driving mechanism 16, and has a size sufficient to cover the entire substrate 10. The controller 6 controls the atmosphere in the vicinity of the shot region and the imprint material 9 therearound to be heated, thereby adjusting the amount of volatilization of the imprint material 9. This makes it possible to adjust the amount of volatilization of the imprint material 9 in each of a plurality of shot regions without simultaneously heating the entire imprint material 9 applied to the substrate 10. Furthermore, the temperature adjustment mechanism 33 in this embodiment is not limited to one, and a plurality of temperature adjustment mechanisms 33 having a temperature adjustment function may be disposed between the substrate 10 and the stage driving mechanism 16 to perform the control as described above.
[0073] In the first and second embodiments, the substrate stage 4 is driven in a stepwise manner or a scanwise manner for the multiple shot regions to which the imprint material 9 is applied, thereby controlling the volatilization of the imprint material 9 for each shot region. In the present embodiment, the volatilization amount of the imprint material 9 may be adjusted for each shot region, but the volatilization amount of the imprint material 9 applied to each of the multiple shot regions may be adjusted collectively. When adjusting the volatilization amount collectively, the control unit 6 calculates the volatilization amount of each of the imprint materials 9 applied to the multiple shot regions, as in step S103. Then, based on the calculated volatilization amount of each of the imprint materials 9, the atmosphere of the imprint material 9 of each of the multiple shot regions is controlled to be heated at a different temperature, thereby adjusting the volatilization amount of the imprint material 9 collectively. This allows the time for the imprint process to be shortened, thereby improving the throughput.
[0074] The temperature adjustment mechanism 33 is not limited to being disposed between the substrate 10 and the stage driving mechanism 16. For example, similar to the volatilization mechanism 30 of the first or second embodiment, the temperature adjustment mechanism 33 may be disposed above the substrate 10 and irradiated with light such as infrared light. Furthermore, the temperature adjustment mechanism 33 may be provided with a driving unit and configured to be drivable in the X-axis direction, the Y-axis direction, and the Z-axis direction. Furthermore, the volatilization mechanism 30 may be provided with a temperature adjustment mechanism 33 such as a heater, and adjustments may be made to promote volatilization of the imprint material 9 in the same manner as in the first and second embodiments.
[0075] Furthermore, the temperature adjustment mechanism 33 is used to heat the atmosphere near the imprint material 9 to promote the volatilization of the imprint material 9, but the temperature adjustment mechanism 33 may be provided with a cooling function for lowering the temperature of the atmosphere of the imprint material 9. The temperature adjustment mechanism 33 equipped with a cooling function can adjust the cooling temperature and cooling time of the substrate 10 to cool the atmosphere near the imprint material 9 and suppress the volatilization of the imprint material 9. Therefore, the amount of volatilization of the imprint material 9 can be adjusted in the same way as when the atmosphere near the imprint material 9 is heated, and the volume or film thickness of the imprint material 9 in multiple shot regions before imprinting can be made uniform. Note that cooling to a temperature at which the physical properties of the imprint material 9 change is not preferable because it has an adverse effect on the imprinting process and the like. The adverse effect on the imprinting process and the like is the same as in Example 1.
[0076] 7A, when there is a distribution in the amount of volatilization of the imprint material 9 within one shot region, a temperature distribution is formed by heating (or cooling) the atmosphere near the imprint material 9 within the shot region. This causes a distribution in the amount of volatilization of the imprint material 9 within the shot region. This makes it possible to uniformize the volume or film thickness of the imprint material 9 before imprinting in multiple shot regions, even when there is a distribution in the amount of volatilization of the imprint material 9 within the shot region.
[0077] In this manner, in this embodiment, the imprint material 9 is applied continuously to a plurality of regions. After application, the atmosphere near the imprint material 9 is heated according to the time from application of the imprint material 9 to contact of the mold 7 with the imprint material 9. This makes it possible to control the amount of volatilization of the imprint material 9 by promoting volatilization of the imprint material 9 in a plurality of shot regions, and to uniformize the volume or film thickness of the imprint material 9 before imprinting. Furthermore, it is possible to reduce a state in which the imprint material 9 is not completely filled in the pattern portion 7a, and to reduce unevenness in the remaining film thickness.
[0078] As described above, in this embodiment, the amount of volatilization of the imprint material 9 in multiple shot areas is adjusted in the same manner as in embodiments 1 and 2. This makes it possible to provide an imprint apparatus (molding apparatus) that can uniformize the volume or film thickness of the imprint material 9 in multiple shot areas before imprinting.
[0079] Incidentally, the volatilization may be controlled so as to be promoted or suppressed by appropriately combining heating, cooling, gas supply or recovery, light irradiation, etc. The amount of volatilization of the imprint material 9 may be adjusted based on the time from when the imprint material 9 is applied to the shot region on the substrate 10 until the imprint material 9 comes into contact with the mold 7. That is, by promoting or suppressing the volatilization, the amount of volatilization is adjusted so that the volume or film thickness of the imprint material 9 when the mold 7 is brought into contact with the imprint material 9 is uniform in multiple shot regions, thereby enabling stable imprinting (imprinting).
[0080] Furthermore, not only the amount of volatilization but also the amount of application of the imprint material 9 may be controlled based on the time from when the imprint material 9 is applied to the shot regions on the substrate 10 until the imprint material 9 comes into contact with the mold 7. By combining both, the volume or film thickness of the imprint material 9 when the mold 7 is brought into contact with the imprint material 9 can be made more uniform across multiple shot regions.
[0081] Example 4 In Example 4, as an example of a molding device, a planarizing device that performs a forming process to form a planarizing layer on a substrate W will be described. The matters not mentioned here are the same as those in the above-mentioned embodiments. In the above-mentioned embodiments, a mold for transferring a circuit pattern provided with a concave-convex pattern has been described as the mold 7, but a mold (flat template) having a flat portion without a concave-convex pattern may also be used. The flat template is used in a planarizing device (molding device) that performs a planarizing process (molding process) to mold the composition on the substrate W so as to flatten it with the flat portion. The planarizing process includes a step of curing the curable composition by irradiation with light or by heating in a state where the flat portion of the flat template is brought into contact with the curable composition supplied onto the substrate W.
[0082] In the planarization device, a planarization layer is formed on the substrate W using a flat template. The base pattern on the substrate W has an unevenness profile caused by the pattern formed in the previous process, and in particular, with the recent trend toward multi-layered structures for memory elements, some process substrates have steps of around 100 nm. The steps caused by the gentle undulation of the entire substrate W can be corrected by the focus tracking function of the scanning exposure device used in the photo process. However, fine-pitched unevenness that falls within the exposure slit area of the exposure device consumes the DOF (Depth Of Focus) of the exposure device as it is. Conventional methods for smoothing the base pattern on the substrate include methods for forming a flattening layer such as SOC (Spin On Carbon) and CMP (Chemical Mechanical Polishing). However, there is a problem that sufficient flattening performance cannot be obtained with conventional technologies, and the unevenness difference of the base due to multi-layering is likely to increase further in the future.
[0083] To solve this problem, the planarization apparatus of this embodiment presses a flat template (flat plate) against the uncured composition that has been applied in advance to the substrate W to locally planarize the substrate surface. In this embodiment, the configuration of the planarization apparatus can be generally similar to that of the imprint apparatus 1 shown in FIG. 1. However, in the planarization apparatus, instead of a mold having a pattern portion on which a concave-convex pattern is formed, a flat plate having an area equal to or larger than that of the substrate W is used, and is brought into contact with the entire surface of the composition layer on the substrate W. The mold holding unit is configured to hold such a flat plate.
[0084] FIG. 9 is a diagram for explaining the process by the planarization apparatus according to the fourth embodiment. FIG. 9(A) is a diagram showing a substrate W on which a base pattern 600 is formed before planarization processing is performed. In the isolated pattern area 601, the area of the pattern convex portion is small, and in the dense area 602, the area occupied by the pattern convex portion is 1:1 with the area occupied by the concave portion. FIG. 9(B) shows a state before a composition (imprint material) 603 is supplied onto the substrate W and a flat plate 604 is brought into contact with the substrate W. The supply pattern of the composition 603 is calculated in consideration of unevenness information on the entire surface of the substrate W, such as the isolated pattern area 601 and the dense area 602. FIG. 9(C) shows a state in which the flat plate 604 is brought into contact with the composition 603 on the substrate W, and the composition 603 is irradiated with light from a light source 605 to cure the composition 603. FIG. 9(D) shows a state in which the flat plate 604 is separated from the cured composition 603.
[0085] As described above, an actual substrate W has not only step differences in the pattern, but also unevenness over the entire surface of the substrate W, and the timing at which the flat plate 604 comes into contact with the composition 603 differs due to the influence of the unevenness. In this embodiment, at the position of first contact, the composition 603 starts to move immediately after contact, and a large amount of the composition 603 is placed depending on the degree of movement. At the position of last contact, the movement of the composition starts slowly, and the composition flowing in from the periphery is added, and the amount of the composition 603 is reduced depending on the degree of movement. By taking such measures, a planarization layer of uniform thickness can be formed over the entire surface of the substrate W.
[0086] The invention according to each of the above-mentioned embodiments can be similarly applied to the planarization apparatus of this embodiment, and the same effects as those of the above-mentioned embodiments can be obtained.
[0087] [Example of an article manufacturing method] The pattern of the cured product formed using the imprint apparatus 1 is used permanently for at least a part of various articles, or temporarily when manufacturing various articles. The articles include electric circuit elements, optical elements, MEMS, recording elements, sensors, molds, etc. Examples of electric circuit elements include volatile or non-volatile semiconductor memories such as DRAM, SRAM, flash memory, and MRAM, and semiconductor elements such as LSI, CCD, image sensors, and FPGAs. Examples of molds include molds for imprinting.
[0088] The pattern of the cured product is used as it is as at least a part of a component of the article, or is used temporarily as a resist mask, which is removed after etching or ion implantation in a substrate processing step.
[0089] Next, a specific method for manufacturing an article will be described with reference to Fig. 10. As shown in Fig. 10(A), a substrate 1z such as a silicon wafer having a workpiece 2z such as an insulator molded on its surface is prepared, and then an imprint material 3z is applied to the surface of the workpiece 2z by an inkjet method or the like. Here, a state in which multiple droplets of the imprint material 3z are applied onto the substrate is shown.
[0090] As shown in Fig. 10(B), the imprinting mold 4z is placed facing the imprinting material 3z on the substrate with the side on which the concave-convex pattern is formed. As shown in Fig. 10(C), the substrate 1z to which the imprinting material 3z has been applied is brought into contact with the mold 4z, and pressure is applied (contact step). The imprinting material 3z fills the gap between the mold 4z and the workpiece 2z. When light is irradiated through the mold 4z in this state as hardening energy, the imprinting material 3z hardens (hardening step).
[0091] 10(D), after the imprint material 3z is cured, the mold 4z and the substrate 1z are separated, and a pattern of the cured product of the imprint material 3z is formed on the substrate 1z (pattern formation process, molding process). In this cured product pattern, the recesses of the mold correspond to the protruding parts of the cured product, and the recesses of the mold correspond to the protruding parts of the cured product, i.e., the recessed and protruding pattern of the mold 4z is transferred to the imprint material 3z.
[0092] As shown in Fig. 10(E), when etching is performed using the pattern of the cured material as an etching-resistant mask, the portions of the surface of the workpiece 2z where there is no cured material or where only a thin layer remains are removed, forming grooves 5z (treatment process). As shown in Fig. 10(F), when the pattern of the cured material is removed, an article is obtained in which grooves 5z are formed on the surface of the workpiece 2z. Here, the pattern of the cured material is removed, but it may be used as an interlayer insulating film included in a semiconductor element or the like, that is, a component of an article, without being removed after processing.
[0093] Although the example has been described in which a mold for transferring a circuit pattern having a concave-convex pattern is used as the mold 4z, a mold having a flat portion without a concave-convex pattern (blank template) may also be used.
[0094] In the above-mentioned embodiments, the imprinting method and the imprinting apparatus 1 have been described using a photocuring method. The step of curing by irradiating light may be changed to a step of curing by applying heat using a thermal curing method. In other words, the above-mentioned embodiments can also be applied to the thermal curing method. In the imprinting apparatus 1 and the imprinting method using the thermal curing method, the imprinting material 9 is prevented from curing by heating.
[0095] Note that the uniformity (evenness) in each of the above examples does not necessarily have to be the same, and a difference of about 10% from the set volume or film thickness is also considered to fall within the range of uniformity. For example, if the film thickness (or remaining film thickness) of the imprint material 9 before imprinting is set to 15 nm, then a thickness within the range of 15 nm ±10% is considered to fall within the range of uniformity (evenness).
[0096] Furthermore, a computer program that realizes all or part of the control in the above-described embodiments may be supplied to the imprinting apparatus 1 or the like via a network or various storage media. Then, a computer (or a CPU, MPU, or the like) in the imprinting apparatus 1 or the like may read and execute the program. In this case, the program and the storage medium storing the program constitute the present invention.
[0097] The present invention has been described in detail above based on its preferred embodiments, but the present invention is not limited to the above embodiments, and various modifications are possible based on the gist of the present invention, and these modifications are not excluded from the scope of the present invention. [Explanation of symbols]
[0098] 1 Imprinting device Type 7 7a Pattern section 9 Imprint material 10 Substrate 20 Discharge part 30 Volatilization mechanism 31 Gas supply port, gas recovery port 32 light source 33 Temperature control mechanism
Claims
1. A molding apparatus for molding a composition on a substrate using a mold, comprising: and a control unit that adjusts an amount of evaporation of the composition so as to promote evaporation of the composition based on a time from when the composition is applied to the shot area on the substrate to when the composition comes into contact with the mold, the control unit adjusts the volatilization amount so that the volume or film thickness of the composition when the mold is brought into contact with the composition is uniform in a plurality of shot regions. A molding apparatus comprising:
2. The molding apparatus according to claim 1 , wherein the control unit controls an adjustment unit including at least one supply port that supplies a gas around the composition in order to adjust the amount of volatilization.
3. The molding apparatus according to claim 1 , wherein the control unit controls an adjustment unit including at least one recovery port for recovering gas surrounding the composition in order to adjust the amount of volatilization.
4. The molding apparatus according to any one of claims 1 to 3, characterized in that the control unit controls an irradiation unit that irradiates the composition with light of a wavelength band that does not harden the composition in order to adjust the amount of volatilization.
5. The molding apparatus according to any one of claims 1 to 4, wherein the control unit controls a heating unit that applies heat to the surroundings of the composition in order to adjust the amount of volatilization.
6. The molding apparatus according to any one of claims 1 to 5, characterized in that the control unit controls the amount of evaporation of the composition in the multiple shot areas based on the time in the shot area that is the longest time from when the composition is applied to the shot area on the substrate to when the composition comes into contact with the mold.
7. A molding apparatus for molding a composition on a substrate using a mold, comprising: and a control unit that adjusts the amount of evaporation of the composition based on the time from when the composition is applied to the shot area on the substrate to when the composition comes into contact with the mold, the control unit adjusts the volatilization amounts of the plurality of shot regions in an order different from the order in which the composition was applied to the shot regions, so that the volume or film thickness of the composition when the mold is brought into contact with the composition is uniform in the plurality of shot regions. A molding apparatus comprising:
8. A molding method for molding a composition on a substrate using a mold, comprising the steps of: and a control step of adjusting an amount of evaporation of the composition so as to promote evaporation of the composition based on a time from when the composition is applied to the shot region on the substrate to when the composition comes into contact with the mold, In the control step, the volatilization amount of the composition is adjusted so that the volume or film thickness of the composition is uniform in a plurality of shot regions when the mold is brought into contact with the composition. A molding method comprising the steps of:
9. A molding method for molding a composition on a substrate using a mold, comprising the steps of: and a control step of adjusting the amount of evaporation of the composition based on the time from when the composition is applied to the shot area on the substrate to when the composition comes into contact with the mold, In the controlling step, a volume or a film thickness of the composition when the mold is brought into contact with the composition is uniformed in the plurality of shot regions. A molding method comprising adjusting the volatilization amounts of a plurality of shot regions in an order different from the order in which the composition was applied to the shot regions.
10. The molding method according to claim 8 or 9, characterized in that the control step adjusts the volatilization amount of the composition by controlling at least one of a supply amount or a supply time of a gas supplied around the composition.
11. The molding method according to any one of claims 8 to 10, wherein the control step adjusts the volatilization amount of the composition by controlling at least one of a recovery amount or a recovery time of gas surrounding the composition.
12. The molding method according to any one of claims 8 to 11, wherein the control step includes at least one of a step of applying heat to the composition and a step of irradiating the composition with light in order to adjust the amount of volatilization.
13. A molding step of molding a composition on a substrate using the molding apparatus according to any one of claims 1 to 7; a treatment step of treating the substrate on which the composition has been molded in the molding step; manufacturing an article from the substrate processed in the processing step; A method for producing an article, comprising:
Citation Information
Patent Citations
Magnetic head
JP1977075419A
Gas environment for imprint lithography
JP2012506146A
Resist material for imprint, patterning method, and imprint device
JP2013055146A
Imprint apparatus and article manufacturing method
JP2019054210A
Imprint lithography
JP4654224B2