Method for estimating retained concrete and method for constructing concrete structure

The method estimates concrete retention in tremie pipes by calculating external and internal pressures, addressing inefficiencies in concrete construction by ensuring accurate switching depths and strengths, thus enabling efficient and economical construction.

JP7561096B2Active Publication Date: 2024-10-03TAISEI CORP
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2021116898
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-07-15
Publication Date
2024-10-03
Estimated Expiration
2041-07-15

AI Technical Summary

Technical Problem

Existing methods for constructing concrete structures using tremie pipes fail to accurately estimate the amount of concrete retained in the pipe, leading to inefficiencies and inaccuracies in the construction process, particularly when different types of concrete are poured sequentially.

Method used

A method to estimate the retention height of concrete in a tremie pipe by calculating the external and internal pressures, considering the frictional resistance and rheological properties of the concrete, allowing for precise determination of the amount of concrete remaining in the pipe, and adjusting the pouring process accordingly.

Benefits of technology

Enables efficient and economical construction by accurately accounting for retained concrete, ensuring proper switching depths and strengths, thereby facilitating rational and safe concrete placement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007561096000004
    Figure 0007561096000004
  • Figure 0007561096000005
    Figure 0007561096000005
  • Figure 0007561096000006
    Figure 0007561096000006
Patent Text Reader

Abstract

To provide a staying concrete estimation method estimating concrete quantity staying in a tremie pipe when installing concrete by using a tremie pipe, and to provide a construction method of a concrete structure utilizing the staying concrete estimation method.SOLUTION: Based on an insertion depth T of a tremie pipe 5 into installed concrete, a pressure outside a tremie pipe that is applied from an outside of the tremie pipe 5 is calculated. A pressure inside a tremie pipe is calculated by dividing a value obtained by deducting a frictional resistance force of concrete and an inner face of the tremie pipe 5 from a force calculated from a self-weight of concrete staying in the tremie pipe 5, by a hollow cross section area of the tremie pipe 5. Assuming that the pressure outside a tremie pipe is equal to the pressure inside a tremie pipe, a staying height H is calculated.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for estimating retained concrete and a method for constructing a concrete structure. [Background technology]

[0002] When constructing a concrete structure, concrete may be poured from a high position using a tremie pipe. For example, Patent Document 1 discloses a method for constructing a cast-in-place concrete pile using a tremie pipe. When pouring concrete using a tremie pipe, it is common to insert the tip of the tremie pipe into the already poured concrete. For example, in the concrete structure construction method of Patent Document 1, when pouring different types of concrete above and below, a tremie pipe is used to pour the lower concrete to a predetermined height (pre-pouring height), and then pouring of the upper concrete is started with the tip of the tremie pipe inserted into the lower concrete, pushing up part of the lower concrete to the switching completion height, and then the upper concrete is subsequently poured above the switching completion height. When concrete is poured from a high place using a tremie pipe, the concrete inside the tremie pipe is generally treated as having fallen to the pouring location. On the other hand, concrete may remain inside the tremie pipe when the tip is inserted into the already poured concrete due to the frictional force generated between the inner surface of the tremie pipe and the concrete. Therefore, when concrete is poured up to the designed height, excess concrete will remain inside the tremie pipe. Therefore, when pouring concrete from a high place to a low place using a tremie pipe, it is desirable to set the concrete pouring completion height (pre-pouring height, etc.) taking into account the amount of concrete remaining inside the tremie pipe. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-020192 A Summary of the Invention [Problem to be solved by the invention]

[0004] The present invention aims to propose a method for estimating the amount of concrete retained in a tremie pipe when pouring concrete using the tremie pipe, and a method for constructing a concrete structure utilizing this method for estimating retained concrete. [Means for solving the problem]

[0005] The method for estimating retained concrete of the present invention is a method for estimating retained concrete in a case where concrete is poured by allowing the concrete to freely fall inside the tremie pipe with the tip of the tremie pipe inserted into already-placed concrete, and a retained height, which is a height difference between the top surface of the concrete retained in the tremie pipe and the top surface of the already-placed concrete, is calculated. calculation This is what we do. The retention height is calculated assuming that the tremie pipe external pressure and the tremie pipe internal pressure are equal when concrete is retained in the tremie pipe. The tremie pipe external pressure is , which acts from the outside of the tremie pipe based on the insertion depth of the tremie pipe into the poured concrete The internal pressure of the tremie tube is The force obtained by subtracting the frictional resistance between the concrete and the inner surface of the tremie pipe from the force obtained from the weight of the concrete remaining in the tremie pipe is divided by the inner hollow cross-sectional area of ​​the tremie pipe 5. This is the value . The tremie pipe external pressure is preferably a value obtained by multiplying the insertion depth by the unit volume weight of the concrete and a value obtained by multiplying the depth of the stabilizing liquid retained above the cast concrete by the unit volume weight of the stabilizing liquid. The tremie pipe internal pressure is preferably a value obtained by multiplying the sum of the retention height and the insertion depth by the unit volume weight of the concrete and the inner cross-sectional area of ​​the tremie pipe, minus a value obtained by multiplying the sum of the retention height and the insertion depth by the friction resistance stress of concrete and the inner circumference of the tremie pipe, and dividing the result by the inner cross-sectional area of ​​the tremie pipe. Furthermore, the friction resistance force is a rheological constant when concrete is assumed to be a Bingham fluid, and is preferably a value based on the limit shear stress at which the concrete begins to flow. According to this method for estimating retained concrete, the amount (height) of concrete retained in the tremie pipe can be estimated, so that concrete can be poured taking into consideration the amount of concrete retained in the tremie pipe, which in turn enables rational construction. For example, when pouring different types of concrete one above the other in succession, the concrete can be appropriately switched at the designed switching depth.

[0006] In addition, the method for constructing a concrete structure of the present invention constructs a concrete structure by pouring an upper concrete made of a different type of concrete on top of a lower concrete, and includes a first step of setting a pouring switching depth, which is a position where pouring of the lower concrete is completed, below a switching completion depth, which is a position where switching from the lower concrete to the upper concrete is completed, and pouring the lower concrete up to the pouring switching depth, a second step of starting the supply of upper concrete with the lower end of the tremie pipe positioned below the pouring switching depth and supplying the upper concrete up to the switching completion depth, and a third step of pouring the upper concrete above the switching completion depth. In the first step, it is desirable to pour the lower concrete to a depth that takes into account the influence of the amount of concrete equivalent to the retained height obtained by the retained concrete estimation method. In addition, in the second step, it is desirable to perform a first pouring operation to supply upper concrete into the tremie pipe in an amount of concrete equal to or greater than the retained height determined by the retained concrete estimation method, a tremie pipe adjustment operation to adjust the insertion depth of the tremie pipe into the lower concrete, and a second pouring operation to resume the supply of upper concrete into the tremie pipe and pour the upper concrete up to the switching completion depth. moreover ,to Set the insertion length below the pouring switching depth of the Remy pipe, and In anticipation of the volume of upper concrete supplied from the tremie pipe below the pouring switching depth and the amount of concrete corresponding to the retention height, It is desirable to calculate a switching length which is the difference between the switching completion depth and the pouring switching depth. According to this method for constructing a concrete structure, the pouring depth of the lower concrete (pouring switching depth) is set taking into account the amount of concrete remaining in the tremie pipe, so that the switching length can be set on the safe side. Effect of the Invention

[0007] According to the retained concrete estimation method of the present invention, when concrete is poured using a tremie pipe, it is possible to appropriately estimate the amount of concrete retained in the tremie pipe. Also, according to the method for constructing a concrete structure using this retained concrete estimation method, efficient and economical construction is possible by taking into account the concrete retained in the tremie pipe. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a cross-sectional view showing a portion of a cast-in-place concrete pile according to an embodiment of the present invention. [Diagram 2] 2A to 2C are cross-sectional views showing the construction status of the cast-in-place concrete pile shown in FIG. 1, where (a) is a first step, (b) is a second step, and (c) is a third step. [Diagram 3] FIG. 1 is a perspective view showing upper concrete supplied below the advance pouring height. [Figure 4] FIG. [Diagram 5]FIG. 1 shows an overview of the first evaluation method, where (a) shows the state in which the lower concrete remains in the tremie pipe, and (b) shows the state in which the lower concrete has been discharged from the tremie pipe. [Figure 6] 11 is a cross-sectional view showing an overview of the second step in the second evaluation method, where (a) is the first concrete pouring work, (b) is the tremie pipe adjustment work, and (c) is the second concrete pouring work. [Figure 7] FIG. 1 is a plan view showing the arrangement of measurement points during on-site construction testing, where (a) is the case where one tremie pipe is used, and (b) is the case where two tremie pipes are used. [Figure 8] 1 is a graph showing the results of a field construction test. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] In this embodiment, a case will be described in which two types of concrete with different strengths are cast continuously in the depth direction (up and down) in a cast-in-place concrete pile (concrete structure) 1 for the purpose of constructing an efficient pile. Fig. 1 shows a part of the cast-in-place concrete pile 1 of this embodiment. The cast-in-place concrete pile 1 of this embodiment is formed by continuously pouring an upper concrete 3, which has a higher design standard strength than the lower concrete 2, on top of a lower concrete 2 in order to increase the concrete strength in the upper part of the pile where stress increases during an earthquake. Fig. 2 shows each construction stage of the method for constructing a concrete structure of this embodiment. The method for constructing a concrete structure in this embodiment includes a first step (see Figure 2(a)) of pouring a lower concrete 2 up to a predetermined height (hereinafter referred to as the "pouring switching depth H1"), a second step (see Figure 2(b)) of starting to supply an upper concrete 3 from below the concrete pouring surface (top surface of already poured concrete) 2a of the lower concrete 2 and supplying the upper concrete 3 until the top surface of the already poured concrete reaches the switching completion depth H2, and a third step (see Figure 2(c)) of pouring the upper concrete 3 above the switching completion depth H2.

[0010] In the first step, as shown in FIG. 2(a), the lower concrete 2 is supplied until the top surface of the already-cast concrete (concrete casting surface) reaches the casting switching depth H1. The lower concrete 2 is supplied from the bottom end of the borehole 6 formed in the ground using a tremie pipe 5 inserted into the borehole 6. A stabilizing liquid sl is stored in the borehole 6 to ensure the stability of the hole wall. The tremie pipe 5 is raised with its tip inserted into the already-cast concrete in accordance with the rise of the concrete casting surface 2a. The casting switching depth H1 is set below the switching completion depth H2, which is the position where the supply of the lower concrete 2 is completed and where the switching from the lower concrete 2 to the upper concrete 3 is completed. The pouring switching depth H1 is set at a switching completion depth H2 (range in which concrete strength is increased) based on an estimated value (design value) of the stress acting on the cast-in-place concrete pile 1, and the pouring switching depth H1 is set so that the concrete is completely switched from the lower concrete 2 to the upper concrete 3 at this switching completion depth H2.

[0011] Here, the pouring switching depth H1 is calculated by Equation 1. The pouring switching depth H1 is calculated by subtracting the switching length h from the switching completion depth H2, which is set based on the acting stress of the cast-in-place concrete pile 1. The switching length h is the section from when the supply of the upper concrete 3 begins after the lower concrete 2 is poured until all of the already poured concrete is switched to the upper concrete 3, and is the height difference between the pouring switching depth H1 and the switching completion depth H2. H1=H2-h ··· Formula 1 H1 :Pouring switching depth H2 :Switching completion depth h : Switching length

[0012] In the second step, as shown in FIG. 2(b), the supply of the upper concrete 3 is started with the lower end of the tremie pipe 5 positioned below the pouring switching depth H1, and the upper concrete 3 is supplied until the top surface of the already poured concrete reaches the switching completion depth H2. When the upper concrete 3 is supplied below the pouring switching depth H1, the upper concrete 3 is poured while pushing aside the lower concrete 2. The upper concrete 3 is supplied in a semi-elliptical or semi-circular shape (tip portion 31) directly below the tremie pipe 5 at the start of supply in the lower concrete 2, and then the upper concrete 3 is supplied in a cylindrical shape (cylindrical portion 32) directly above the tip portion 31 (see FIG. 3). Meanwhile, as the upper concrete 3 is supplied, the lower concrete 2, which has a volume equivalent to the upper concrete 3 supplied below the pouring switching depth H1, moves from below the pouring switching depth H1 to above the pouring switching depth H1. At this time, the lower concrete 2 that has moved above the pouring switching depth H1 moves to the outer portion (annular region 21 centered on the tremie pipe 5) above the pouring switching depth H1 (see FIG. 2(c)). The upper end of the lower concrete 2 (annular region 21) that has moved above the pouring switching depth H1 is located below the switching completion depth H2.

[0013] As a conventional method for evaluating the switching length h (the pouring switching depth H1 and the switching completion depth H2), for example, there is the following method (see Patent Document 1). The annular region 21 is a section where the lower concrete 2 and the upper concrete 3 are mixed, and the height of the annular region 21 (annular region height h T ) is the basis for the switching length h. The height of the annular region h T As shown in Equation 2, the volume of the annular region 21 is calculated by assuming that the volume V of the upper concrete 3 supplied below the pouring switching depth H1 is the volume of the lower concrete 2 that has moved to the annular region 21. Here, the upper concrete 3 supplied below the pouring switching depth H1 is the sum of the volumes of the tip portion 31 and the cylindrical portion 32, as shown in Fig. 3. Meanwhile, the annular region 21 has an inner diameter φ i , a cylindrical body with an outer diameter of φ0. h=h T hT =V / S...Equation 2 V=V1+V2 S = π / 4 × (φ o 2 -φ i 2 ) V1 = πφ r 2 / 4×T V2=2 / 3×πφ r 2 / 4×Δh0 h T : Height of the annular region V : Volume of upper concrete supplied below the pre-cast height V1 : Volume of the cylindrical part of the upper concrete supplied below the pre-cast height V2 : Volume of the tip of the upper concrete supplied below the pre-cast height S : Cross-sectional area of ​​the annular region φ o :Outer diameter of cast-in-place concrete pile φ i :Inner diameter of the annular region φ r : Diameter of the cylindrical part of the upper concrete supplied below the pre-cast height T : Depth of the tremie pipe inserted into the lower concrete in the second step Δh0: Lower outflow depth, which is the distance from the bottom end of the upper concrete supplied in the second process to the tip of the tremie pipe In addition, it is also possible to evaluate the switching length h from the results of experiments or analysis using flow analysis (CFD).

[0014] In the third step, as shown in FIG. 2(c), with the lower end inserted into the already poured concrete (upper concrete 3), the tremie pipe 5 is pulled up and the upper concrete 3 is supplied above the switching completion depth H2.

[0015] As a method based on this patent for taking into account the influence of concrete remaining in the tremie pipe 5 on the switching length h (pouring switching depth H1 and switching completion depth H2), for example, the following three methods (first evaluation method to third evaluation method) may be used. (1) First evaluation method The switching length h is calculated by Equation 3, which takes into account the amount of concrete equivalent to the retention height H of the concrete retained in the tremie pipe 5 after the first process. Figure 5 shows an overview of the first evaluation method. The retention height H is the height difference from the top surface of the concrete retained in the tremie pipe 5 to the top surface of the already-cast concrete when concrete is poured by allowing it to freely fall into the tremie pipe 5 with the tip of the tremie pipe 5 inserted into the already-cast concrete, as shown in Figure 5(a). When pouring of the upper concrete 3 begins, the lower concrete 2 remaining in the tremie pipe 5 is discharged first, so the timing of switching to the upper concrete 3 is calculated, including the amount of this lower concrete 2 (see Figure 5(b)). The switching length h is the height of the lower concrete (switching length increment Δh) that increases due to the amount of concrete equivalent to the retention height H, multiplied by the height of the annular region h T The height is the sum of the above. h=h T +Δh...Equation 3 Δh=α×ΔT h: Switching length h T : Height of the annular region Δh: Switching length increment ΔT: Increment of embedded length corresponding to retained concrete α: Coefficient for the increment of embedment obtained by fluid analysis (CFD) or experiment

[0016] (2) Second evaluation method The switching length h in the second evaluation method is calculated by multiplying the embedment length increment ΔT corresponding to the amount of concrete equivalent to the retention height H by the height of the annular region h, as shown in Equation 4. T That is, in the second evaluation method, the switching length increment Δh is set to the penetration length increment ΔT. h=h T +ΔT...Equation 4 h: Switching length h T : Height of the annular region ΔT: Increment of penetration length

[0017] In addition, when using the second evaluation method, it is desirable to perform, in the second step, a first pouring operation of supplying an amount of upper concrete 3 into the tremie pipe 5 that is equal to or greater than the amount of concrete equivalent to the retention height H, as shown in Figures 6(a) and (b), a tremie pipe adjustment operation of adjusting the insertion depth T of the tremie pipe 5 into the lower concrete 2, as shown in Figures 6(b) and (c), and a second pouring operation of resuming the supply of upper concrete 3 into the tremie pipe 5 and pouring the upper concrete 3 up to the switching completion depth H2, as shown in Figure 2(b).

[0018] (3) Third evaluation method In the third evaluation method, as shown in Equation 5, the increment in embedment length ΔT corresponding to the amount of concrete equivalent to the retention height H in Equation 1 is taken into consideration. H1=H2-h-ΔT ··· Equation 5 h=V / S V=V1+V2 S = π / 4 × (φ o 2 -φ i 2 ) V1 = πφ r 2 / 4×(T+ΔT) V2=2 / 3×πφ r 2 / 4×Δh0 H1 :Pouring switching depth H2 :Switching completion depth h : Switching length h T : Height of the annular region V : Volume of upper concrete supplied below the pre-cast height V1 : Volume of the cylindrical part of the upper concrete supplied below the pre-cast height V2 : Volume of the tip of the upper concrete supplied below the pre-cast height S : Cross-sectional area of ​​the annular region φ o :Outer diameter of cast-in-place concrete pile φ i :Inner diameter of the annular region φ r : Diameter of the cylindrical part of the upper concrete supplied below the pre-cast height T : Depth of the tremie pipe inserted into the lower concrete in the second step Δh0: Lower outflow depth, which is the distance from the bottom end of the upper concrete supplied in the second process to the tip of the tremie pipe

[0019] Here, the retention height H is calculated by the ratio of the tremie pipe external pressure p0 and the tremie pipe internal pressure p when concrete is retained in the tremie pipe 5, as shown in Equation 6. t The calculation is made assuming that the above are equal. p0=p t ··· Equation 6 p0: External pressure of tremie tube p t : Internal pressure of tremie tube

[0020] The tremie pipe external pressure p0 is the pressure acting from outside the tremie pipe 5 based on the insertion depth T of the tremie pipe 5 into the poured concrete (see FIG. 2(b)). As shown in Equation 7, the tremie pipe external pressure p0 is calculated by multiplying the insertion depth T by the unit volume weight of concrete γ c and the depth H of the stabilizing liquid sl that remains above the concrete that has already been poured. sl The unit weight of the stabilizing liquid sl is γ sl The value is obtained by multiplying and adding the value. p0=γ c T+γ sl H sl ...Formula 7 Gamma c :Unit weight of concrete T :Insertion depth Gamma sl : unit weight of stabilizing liquid H sl : Depth of stabilizing solution

[0021] Tremie tube internal pressure p t As shown in Equation 8, is the pressure calculated from the weight of the concrete (lower concrete) retained in the tremie pipe 5 minus the frictional resistance between the concrete and the inner surface of the tremie pipe 5. The pressure calculated from the weight of the concrete retained in the tremie pipe 5 is calculated by multiplying the unit volume weight of the concrete γ by the sum of the retention height H and the insertion depth T. c The frictional resistance force between the concrete and the inner surface of the tremie pipe 5 is calculated by multiplying the sum of the retention height H and the insertion depth T by the frictional resistance stress f of the concrete, and then multiplying this value by the inner circumference φ of the tremie pipe. And the internal pressure of the tremie tube p t is calculated by subtracting the frictional resistance force from the force calculated from the weight, and dividing the result by the inner cross-sectional area of ​​the tremie tube 5. In this embodiment, the concrete yield value τ is used as the friction resistance stress f of the concrete. The concrete yield value τ (=friction resistance f) is a rheological constant when the concrete is assumed to be a Bingham fluid, and is a value based on the limit shear stress at which the concrete begins to flow.

[0022]

number

[0023] From Equations 6 to 8, the retention height H can be expressed by Equation 9. Here, R is the inner diameter of the tremie pipe.

[0024]

number

[0025] As described above, according to the method for constructing a concrete structure of this embodiment, the switching of concrete can be completed near the design switching completion height, so that when concretes of different strengths are poured continuously in the height direction, it is possible to set the point where the strength of the poured concrete changes rationally. As a result, the cast-in-place concrete pile 1 with the required strength can be constructed economically. Furthermore, according to this embodiment, the amount of concrete remaining in the tremie pipe 5 (retention height H) can be estimated, so that concrete can be poured taking into account the amount of concrete remaining in the tremie pipe 5, thereby enabling rational construction.

[0026] Below, we will show the results of a field construction test that confirmed the validity of the method for estimating the amount of concrete remaining in the tremie pipe 5 using Equation 9. In the construction test, the top level of the concrete inside and outside the tremie pipe 5 was measured for four test specimens after concrete was poured. Figure 7(a) shows test specimens 1 and 2, and Figure 7(b) shows test specimens 3 and 4. In test specimens 1 and 2, the tremie pipe 5 was installed in the center of the borehole 6 as shown in Figure 7(a), and in test specimens 3 and 4, two tremie pipes 5,5 were installed facing each other across the center of the borehole 6. Measurement points P were measured inside the tremie pipe 5, one point near the center of the borehole 6 outside the tremie pipe 5, and four points set at approximately equal intervals on the outer periphery. That is, as shown in Figure 7(a), a total of six points were measured for test specimens 1 and 2, and a total of seven points were measured for test specimens 3 and 4 as shown in Figure 7(b). The concrete height was calculated from the measurement value inside the tremie pipe 5 (average value for test specimens 3 and 4) and the average value of the measurement values ​​at each measurement point outside the tremie pipe 5.

[0027] The calculation conditions are as follows: Stable liquid level GL-0m Stabilizing liquid unit weight γ sl =10kN / m 3 Bottom concrete unit weight γ c =22.6kN / m 3 Yield value of the lower concrete τ=325Pa Upper concrete unit volume weight γ c =23.5kN / m 3 Yield value of upper concrete τ=100Pa

[0028] The yield values ​​τ of the upper concrete 3 and the lower concrete 2 were set so that the slump or slump flow would be the target value by separately conducting flow analysis of the slump test. Figure 8 shows the relationship between the test results for concrete height and the estimated results. As shown in Fig. 8, the estimated results largely correspond. In addition, since the estimated results (dotted line in Fig. 8) are greater than the test results (since they are located above the estimated straight line (dotted line)), it was confirmed that the estimated results are on the safe side.

[0029] Next, the pile diameter of the cast-in-place concrete pile and the switching depth for pouring were used as parameters to calculate the height H of the concrete remaining in the tremie pipe 5 and the increment in embedded length ΔT. The calculation conditions are shown below. The calculation results are shown in Table 1. Pile diameter: 1.6m, 2.0m, 2.4m, 3.0m Pouring switching depth: GL-10m, -20m, -30m, -40m, -50m Stable liquid level GL-0m Stabilizing liquid unit weight γ sl =10kN / m 3 Tremie pipe: inner diameter 25cm, embedded length 2m Concrete unit weight γ c =22.6kN / m 3 Concrete yield value τ=325Pa

[0030] [Table 1]

[0031] As shown in Table 1, regardless of the pile diameter, the deeper the driving switching depth, the larger the embedded length increment ΔT. Also, the smaller the pile diameter, the larger the embedded length increment ΔT.

[0032] Although an embodiment of the present invention has been described above, the present invention is not limited to the above-described embodiment, and each of the above-described components can be appropriately modified without departing from the spirit of the present invention. For example, in the above embodiment, a cylindrical cast-in-place concrete pile 1 is constructed, but the concrete structure is not limited thereto. Furthermore, the retained concrete estimation method is not limited to cases where different types of concrete are poured continuously in the depth direction, but may be used when pouring one type of concrete. In addition, in the above embodiment, a case has been described in which a single tremie pipe 5 is used for construction on a single cast-in-place concrete pile 1, but the number of tremie pipes 5 is not limited, and for example, multiple tremie pipes 5 may be used. In the above embodiment, the upper concrete 3 is poured using concrete having a higher design standard strength than the lower concrete 2, but the upper concrete 3 is not limited to this as long as it is a different type of concrete from the lower concrete 2, for example, one having a higher fluidity than the lower concrete 2. In the above embodiment, in the first step, the lower concrete is poured to a depth that anticipates the amount of concrete equivalent to the retention height, but the method of setting the pouring switching depth is not limited. In addition, in the above embodiment, the second step includes a first pouring operation of supplying upper concrete into the tremie pipe with an amount of concrete equivalent to the retention height or more, a tremie pipe adjustment operation of adjusting the insertion depth of the tremie pipe into the lower concrete, and a second pouring operation of resuming the supply of upper concrete into the tremie pipe and pouring the upper concrete up to the switching completion depth, but the work procedure of the second step is not limited. [Explanation of symbols]

[0033] 1. Cast-in-place concrete piles 2. Lower concrete 3. Upper Concrete 4 Reinforced Concrete Cage 5 Ptolemy tube 6. Borehole

Claims

1. A method for estimating retained concrete, in which concrete that has been allowed to freely fall into a tremie pipe is poured while the tip of the tremie pipe is inserted into already-placed concrete, calculates a retained height, which is a height difference between an upper surface of the concrete retained in the tremie pipe and an upper surface of the already-placed concrete, The retention height is calculated assuming that the external pressure of the tremie pipe and the internal pressure of the tremie pipe are equal when concrete is retained in the tremie pipe, The tremie pipe external pressure is a pressure acting from the outside of the tremie pipe based on the insertion depth of the tremie pipe into the already-cast concrete, A method for estimating retained concrete, characterized in that the internal pressure of the tremie pipe is a value obtained by subtracting the frictional resistance force between the concrete and the inner surface of the tremie pipe from the force calculated from the weight of the concrete retained in the tremie pipe, and dividing the result by the internal cross-sectional area of ​​the tremie pipe.

2. The tremie pipe external pressure is a value obtained by multiplying the insertion depth by the unit volume weight of the concrete and a value obtained by multiplying the depth of the stabilizing liquid retained above the cast concrete by the unit volume weight of the stabilizing liquid, The method for estimating retained concrete as described in claim 1, characterized in that the internal pressure of the tremie pipe is a value obtained by multiplying the sum of the retained height and the insertion depth by the unit volume weight of the concrete and the internal cross-sectional area of ​​the tremie pipe, minus the value obtained by multiplying the sum of the retained height and the insertion depth by the frictional resistance stress of concrete and the inner circumference of the tremie pipe, and dividing the result by the internal cross-sectional area of ​​the tremie pipe.

3. 3. The method for estimating retained concrete according to claim 2, wherein the friction resistance stress is a rheological constant when the concrete is assumed to be a Bingham fluid, and is a value based on the limit shear stress at which the concrete begins to flow.

4. A method for constructing a concrete structure by pouring an upper concrete made of a different type of concrete onto a lower concrete, comprising: A first step of setting a pouring switching depth, which is a position where pouring of the lower concrete is completed, below a switching completion depth, which is a position where switching from the lower concrete to the upper concrete is completed, and pouring the lower concrete up to the pouring switching depth; A second step of starting to supply upper concrete with the lower end of the tremie pipe positioned below the pouring switching depth and pouring the upper concrete up to the switching completion depth; and a third step of pouring upper concrete above the switching completion depth, A method for constructing a concrete structure, characterized in that in the first step, lower concrete is poured to a depth that takes into account the influence of the amount of concrete equivalent to the retained height obtained by the retained concrete estimation method described in any one of claims 1 to 3.

5. A method for constructing a concrete structure by pouring an upper concrete made of a different type of concrete onto a lower concrete, comprising: A first step of setting a pouring switching depth, which is a position where pouring of the lower concrete is completed, below a switching completion depth, which is a position where switching from the lower concrete to the upper concrete is completed, and pouring the lower concrete up to the pouring switching depth; A second step of starting to supply upper concrete with the lower end of the tremie pipe positioned below the pouring switching depth and pouring the upper concrete up to the switching completion depth; and a third step of pouring upper concrete above the switching completion depth, In the second step, a first pouring operation is performed to supply an upper concrete amount equivalent to the retained concrete height obtained by the retained concrete estimation method according to any one of claims 1 to 3 into the tremie pipe; a tremie pipe adjustment operation for adjusting the insertion depth of the tremie pipe into the lower concrete; a second pouring operation of resuming the supply of upper concrete into the tremie pipe and pouring the upper concrete up to the switching completion depth.

6. A method for constructing a concrete structure as described in claim 4 or claim 5, characterized in that an insertion length below the pouring switching depth of the tremie pipe is set, and a switching length which is the difference between the switching completion depth and the pouring switching depth is calculated by anticipating the volume of upper concrete supplied from the tremie pipe below the pouring switching depth and the amount of concrete equivalent to the retention height.

Citation Information

Patent Citations

  • Tremie pipe

    JP1976140307A

  • Casting method of roottconsolidating cement

    JP1980138517A

  • Casting method for underwater cement hardening material

    JP1988198826A

  • Concrete covering depth measuring device and underwater concrete placing method

    JP1994200528A

  • Cast-in-place pile driving method

    JP1995138948A