Flycutting Equipment
The fly-cutting device addresses issues of uneven grinding and peeling in semiconductor wafer processing by cutting protective films uniformly, ensuring stable holding and consistent line depth, thus preventing cracks and damage.
Patent Information
- Application Number
- JP2020139473
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-08-20
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2040-08-20
AI Technical Summary
Existing methods for processing semiconductor wafers with surface bumps result in insufficient adsorption and holding, leading to potential damage, fluttering, and formation of minute cracks due to uneven grinding and peeling processes.
A fly-cutting device that cuts the protective film on semiconductor wafers from the center to the periphery, using a fly-cutting tool and chuck configuration to ensure uniform thickness and stable holding, preventing cracks and ensuring consistent modification line depth during processing.
The device ensures safe grinding and dicing of semiconductor wafers by preventing cracks and maintaining uniform thickness, allowing for stable formation of modification lines and safe transport without damage.
Smart Images

Figure 0007562333000001 
Figure 0007562333000002 
Figure 0007562333000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a flycutting device that cuts a protective film attached to a workpiece having bumps formed on its surface. [Background technology]
[0002] In the field of semiconductor manufacturing, semiconductor wafers such as silicon wafers (hereinafter referred to as "workpieces") are ground thinly and flat by pressing the grinding surface of a rotating grinding wheel against the workpiece to grind the backside of the workpiece. When grinding the backside of the workpiece, a film for protecting the surface is attached to the workpiece to protect the chips and bumps formed on the surface of the workpiece.
[0003] After grinding the back surface of the workpiece is completed, a dicing film is attached to the back surface of the workpiece in a dicing film attachment device, and the workpiece and dicing frame are integrated. Next, the protective film attached to the front surface of the workpiece is peeled off, and the workpiece is diced into a dice shape. The chips formed by dicing are picked up and mounted on a lead frame (see, for example, Patent Document 1).
[0004] Specifically, the workpiece 100 is processed according to the procedure shown in Fig. 9. That is, bumps 102 are formed on the front surface 101 of the workpiece 100, and a BG film 103 is attached to cover the bumps 102 (BG film attachment process). Thereafter, the workpiece 100 is held by suction on a chuck table 105 so that the back surface 104 faces upward, and the back surface 104 is ground by a grinding wheel 106 (workpiece grinding process). Then, a laser is focused inside the workpiece 100 to form a modification line 107 at a predetermined depth from the back surface 104 (laser dicing (ML) process). Thereafter, the back surface 104 of the workpiece 100 is suctioned by a chuck 108 of a transport arm, and the workpiece 100 is transported to a DC tape attachment device (workpiece transport process). Then, while the workpiece 100 is held by the transposed chuck 109, a rolling roller 110 presses and attaches a DC tape 111 to the back surface 104 of the workpiece 100, and after the workpiece 100 is held by a dicing frame 112, the BG film 103 is peeled off via a peeling tape 113 (DC tape application, BG film peeling process). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2009-206475 A Summary of the Invention [Problem to be solved by the invention]
[0006] 9, the center of the workpiece 100 rises higher than the outer periphery by the amount of the bumps 102, so that leakage occurs from the gap between the outer periphery of the BG film 103 and the chuck table 105, and the workpiece 100 tends to be insufficiently held by suction, which makes the workpiece 100 more likely to flutter during grinding, and there is a risk of damaging the workpiece 100. Furthermore, since the outer periphery of the workpiece 100 tends to be ground thicker than the center, in the subsequent ML process, the modification line 107 is formed with a large deviation in the depth direction of the workpiece 100, and negative pressure is generated between the chuck 108 and the workpiece 100 in the transport process, or if a peeling force exceeding the adhesive force of the BG film 103 acts on the workpiece 100 in the peeling process, there is a risk of microscopic cracks occurring in the workpiece 100 that cannot be detected even by image inspection.
[0007] Therefore, a technical problem arises that must be solved in order to safely process a workpiece having bumps formed on its surface, and an object of the present invention is to solve this problem. [Means for solving the problem]
[0008] In order to achieve the above-mentioned object, the fly-cutting device of the present invention is a fly-cutting device that cuts the top surface of a protective film attached to a workpiece including a bump area having bumps formed on the surface and a peripheral area around the bump area, and is equipped with a fly-cutting tool, a tool spindle to which the fly-cutting tool is attached at its lower end and which can be raised and lowered while rotating the fly-cutting tool, and a chuck that rotatably holds the workpiece, and the fly-cutting tool cuts the top surface of the protective film from the center toward the peripheral area.
[0009] According to this configuration, the central region of the protective film is cut relatively thinner than the outer peripheral region, so that when the upper side of the protective film is adsorbed and held by a chuck, the entire protective film can be adsorbed and held by the chuck, allowing the workpiece to be ground safely.In addition, since the modification line is formed at an approximately constant depth from the back surface of the workpiece in the ML process, the occurrence of microcracks in the workpiece during the transport process and peeling process can be suppressed. Effect of the Invention
[0010] In the present invention, the bumped workpiece is formed to a substantially uniform thickness over its entire surface, so that the entire protective film is adsorbed and held by the chuck, allowing the workpiece to be safely ground, and in the ML process, the modification line is formed at a substantially constant depth from the back surface of the workpiece, thereby preventing the occurrence of microcracks in the workpiece during the transport process and peeling process. [Brief description of the drawings]
[0011] [Figure 1] 1 is a schematic diagram showing an overview of a fly-cutting device according to an embodiment of the present invention; [Diagram 2] 1A is a perspective view of a fly-cutting tool, and FIG. 1B is an enlarged view of a main part of the fly-cutting tool. [Diagram 3] FIG. 11 is a plan view showing the positions of the fly cut lines and the measurement positions of the thickness sensors. [Figure 4] 1A is a plan view of a workpiece, FIG. 1B is a longitudinal sectional view of the workpiece, and FIG. 1C is an enlarged view of a main portion of the workpiece. [Diagram 5] 1A to 1C are schematic diagrams showing a procedure for machining a workpiece having bumps. [Figure 6] 1A to 1C are schematic diagrams showing a procedure for cutting a BG film. [Figure 7] FIG. 4 is a plan view showing a schematic positional relationship between adjacent fly cut lines. [Figure 8] FIG. 4 is a side view showing a schematic positional relationship between a fly-cutting tool and a chuck. [Figure 9]1A to 1C are schematic diagrams showing a conventional procedure for machining a workpiece with bumps. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] An embodiment of the present invention will be described with reference to the drawings. In the following, when the number, numerical value, amount, range, etc. of components are mentioned, the number is not limited to the specific number, and may be more or less than the specific number, unless otherwise specified or when it is clearly limited to a specific number in principle.
[0013] In addition, when referring to the shape or positional relationship of components, etc., this includes things that are substantially similar or approximate to those shapes, etc., unless otherwise specified or considered to be clearly different in principle.
[0014] In addition, the drawings may exaggerate characteristic parts to make the features easier to understand, and the dimensional ratios of the components may not be the same as the actual ones. In addition, in cross-sectional views, hatching of some components may be omitted to make the cross-sectional structure of the components easier to understand.
[0015] A silicon workpiece 7 (described later) is supplied to a fly-cutting device 1 shown in Fig. 1. The fly-cutting device 1 includes cutting means 2 and a chuck 3.
[0016] The cutting means 2 includes a fly-cutting tool 21, a tool spindle 22, and a spindle feed mechanism 23.
[0017] 2(a) and (b), the fly-cutting tool 21 includes a ring frame 21a attached to the lower end of the tool spindle 22, and a tool bit 21b attached to the outer periphery of the ring frame 21a. The ring frame 21a is attached to the tool spindle 22 via, for example, a bolt. The tool bit 21b is attached to the ring frame 21a via a bolt 21c, so that when the tool bit 21b is worn out, only the tool bit 21b can be replaced. The tool bit 21b is, for example, a single diamond.
[0018] The tool spindle 22 is configured to be rotated around a rotation axis 22a in the direction of arrow A in Fig. 1. An induction motor is used for the rotation of the tool spindle 22. Note that the rotation direction of the tool spindle 22 is not limited to the direction of arrow A in Fig. 1, and may be the opposite direction.
[0019] The spindle feed mechanism 23 raises and lowers the tool spindle 22 in the vertical direction. The spindle feed mechanism 23 is composed of, for example, a plurality of linear guides that guide the moving direction of the tool spindle 22, and a ball screw slider mechanism that raises and lowers the tool spindle 22. The spindle feed mechanism 23 is interposed between the tool spindle 22 and a column 24.
[0020] The chuck 3 includes a chuck spindle 31. The chuck spindle 31 is configured to be rotatably driven around a rotation shaft 31a in the direction of arrow B in Fig. 1. Note that the rotation direction of the chuck spindle 31 is not limited to the direction of arrow B in Fig. 1, and may be the opposite direction.
[0021] The chuck 3 has an adsorbent 32 made of a porous material such as alumina embedded in its upper surface. The pores of the adsorbent 32 have a roughness of, for example, #400 or #800. The chuck 3 has a conduit (not shown) that runs through the inside and reaches the surface. The conduit is connected to a vacuum source, a compressed air source, or a water supply source via a rotary joint (not shown). When the vacuum source is activated, the workpiece 7 placed on the adsorbent 32 is adsorbed and held on the holding surface 3a of the chuck 3. When the compressed air source or water supply source is activated, the adsorption between the workpiece 7 and the holding surface 3a is released.
[0022] The fly-cutting device 1 includes a cooling water nozzle 4. The cooling water nozzle 4 supplies cooling water such as pure water to a fly-cutting line L where the cutting tool 21b cuts a BG film 75, which will be described later.
[0023] The fly-cutting device 1 is equipped with a thickness sensor 5. The thickness sensor 5 is an in-process gauge that measures the thickness of the workpiece 7, and specifically, as shown in Fig. 3, one measuring head 51 measures the height of the workpiece 7, and the other measuring head 52 measures the height of the chuck 3, and the workpiece 7 relative to the chuck 3 can be measured during processing from the difference between the two.
[0024] The operation of the fly-cutting device 1 is controlled by a control unit 6. The control unit 6 controls each of the components constituting the fly-cutting device 1. The control unit 6 is composed of, for example, a CPU, a memory, and the like. The functions of the control unit 6 may be realized by controlling using software, or may be realized by operating using hardware.
[0025] The control unit 6 also functions as a cutting time prediction unit that calculates the time for the BG film 75 to reach the finished thickness based on the measurement value of the thickness sensor 5, the rotation speed of the tool spindle 22, the rotation speed of the chuck spindle 31, and the descent speed of the spindle feed mechanism 23.
[0026] As shown in Figures 4(a) and (b), the workpiece 7 has a plurality of chips (not shown) with bumps 71 formed on its surface 72. Specifically, the workpiece 7 has a plurality of chips formed only in a central region 73 on the surface 72 of the workpiece 7, and each chip has a bump 71 formed thereon as an electrical contact. In other words, the chips and bumps 71 are not formed in an outer peripheral region 74 of the workpiece 7. Hereinafter, the central region 73 will be referred to as the bump region 73. The height of the bumps 71 is, for example, 100 µm or less.
[0027] A BG film 75 is attached to the front surface 72 side of the workpiece 7 so as to cover the entire surface. The BG film 75 protects the chips and bumps 71 during cutting and grinding of the back surface 76, which will be described later. As shown in Figures 4(b) and (c) , the bump region 73 of the BG film 75 is relatively higher than the outer peripheral region 74 in accordance with the height of the bumps 71.
[0028] Next, a series of steps for machining the workpiece 7 will be described with reference to FIG.
[0029] [BG film attached] First, using a known film attachment device, the BG film 75 is attached to the surface 72 of the workpiece 7. The BG film 75 is made of a base material 75a and an adhesive 75b, and for example, the base material 75a is made of polyolefin and the adhesive 75b is made of acrylic.
[0030] [BG film cutting] Next, the fly-cutting device 1 is used to cut the upper surface 75c of the BG film 75. Specifically, first, the back surface 76 of the workpiece 7 is sucked and held by the chuck 3. Next, with the tool spindle 22 and the chuck spindle 31 both rotating, the spindle feed mechanism 23 cuts the cutting tool 21b into the BG film 75 while supplying cooling water from the cooling water nozzle 4.
[0031] As shown in Figures 6(a) to 6(c) and 7(a), the cutting tool 21b cuts the top surface 75c of the BG film 75 from the center to the outer periphery. If the cutting tool 21b cuts the BG film 75 from the outer periphery to the center, the periphery of the BG film 75 that the cutting tool 21b contacts may elastically deform and may not be cut into the desired shape, whereas by cutting the BG film 75 from the center to the outer periphery, the cutting tool 21b can stably cut the BG film 75. The various cutting conditions are, for example, a rotational speed of the tool spindle 22 of 3000 rpm, a rotational speed of the chuck spindle 31 of 1 rpm, and a descending speed of the spindle feed mechanism 23 of 0.2 µm / s.
[0032] In addition, the amount of the BG film 75 removed by the cutting tool 21b in one cutting (the size of the fly cut line L) is 12 μm in thickness (depth) under the above-mentioned cutting conditions. Furthermore, as shown in Figures 7(a) to (c), after the cutting tool 21b cuts the BG film 75, the amount of rotation (0.3 mm) of the BG film 75 during one rotation of the cutting tool 21b corresponds to the pitch interval between adjacent fly cut lines L.
[0033] As shown in FIG. 8, the rotation axis 31a of the chuck 3 is inclined with respect to the rotation axis 22a of the tool spindle 22, and the holding surface 3a of the chuck 3 is formed in a convex shape with the center higher than the outer periphery. That is, in the range where the bit 21b cuts the BG film 75, the chuck 3 and the tool spindle 22 are approximately parallel, while the chuck 3 is separated from the tool spindle 22 on the opposite side of the range where the bit 21b cuts the BG film 75 across the rotation center of the chuck 3. As a result, a gap is secured between the BG film 75 and the bit 21b until the bit 21b returns to the center of the BG film 75 after cutting out from the outer periphery of the BG film 75, so that the bit 21b is prevented from contacting the BG film 75 at an unintended position. In FIG. 7, the escape amount, which is the distance from the lower end of the holding surface 3a to the rotation center of the chuck 3, is set to 60 μm.
[0034] The timing to finish cutting the BG film 75 is determined by the following procedure. That is, the thickness sensor 5 measures the thickness of the workpiece 7 relative to the chuck 3 during processing. The control unit 6 calculates the time until the measurement value of the thickness sensor 5 reaches a preset finish thickness of the workpiece 7 based on the measurement value of the thickness sensor 5, the rotation speed of the tool spindle 22, the rotation speed of the chuck spindle 31, and the descending speed of the spindle feed mechanism 23. When that time has elapsed, the control unit 6 determines that the thickness of the workpiece 7 being processed has reached the finish thickness, and stops the feed by the spindle feed mechanism 23, as shown in FIG. 6(d).
[0035] 3, the thickness sensor 5 measures the height of the workpiece 7 at a point different from the nearest flycut line L, so it is necessary to consider the positional relationship between the measurement position of the thickness sensor 5 and the nearest flycut line L. For example, since the thickness of the workpiece 7 at the measurement position of the thickness sensor 5 in FIG. 3 is about 12 μm thicker than the thickness of the workpiece 7 at the nearest flycut line L, the measurement value of the thickness sensor 5 may be corrected to approximately match the thickness of the workpiece 7 at the nearest flycut line L by subtracting about 12 μm from the measurement value of the thickness sensor 5. The shape of the BG film 75 after flycutting (i.e., the total amount removed by flycutting) can be arbitrarily changed according to the height of the bumps 71.
[0036] When the workpiece 7 reaches the finishing thickness, the upper surface 75c of the BG film 75 is a spiral curved surface, and further, as shown in Fig. 6(d), a step 77 is formed at the nearest fly cut line L. Then, as shown in Fig. 6(e), by performing a spark out in which the tool spindle 22 and the chuck spindle 31 are rotated while the spindle feed mechanism 23 is stopped, the upper surface 75c of the BG film 75 is smoothly finished.
[0037] In this way, by removing the central region 73 of the upper surface 75c of the BG film 75, which is formed to be relatively thicker than the peripheral region 74, with the bit 21b, the thickness of the workpiece 7 including the BG film 75 can be made approximately uniform over the entire surface.
[0038] [Workpiece grinding] Next, the workpiece 7 is transferred to a known grinding device, and the back surface of the workpiece 7 is ground with a grinding wheel 81. At this time, since the top surface 75c of the BG film 75 has been fly-cut, the entire top surface 75c of the BG film 75 is attracted and held substantially flat by the grinding chuck 82 regardless of the bumps 71, so that vacuum leakage at the outer periphery of the workpiece 7 and flapping of the workpiece 7 during grinding are suppressed, and the back surface 76 of the workpiece 7 after grinding is formed substantially flat.
[0039] [Laser dicing] Next, the work 7 is transferred to a known laser dicing device, and laser dicing (ML) is performed in which a laser having a wavelength that transmits the work 7 is focused inside the work 7 to form modified lines 78 in a lattice shape in a plan view on the work 7. The modified lines 78 become starting points for dividing the work 7 when the work 7 is divided into individual pieces. Since the upper surface 75c of the BG film 75 is fly-cut, the BG film 75 is adsorbed and held substantially flat by the ML chuck 83 regardless of the bumps 71, and the back surface 76 of the work 7 is ground substantially flat, so that the modified lines 78 can be stably formed to a predetermined depth from the back surface 76 of the work 7.
[0040] [Work transport] Next, the back surface 76 of the workpiece 7 is sucked and held by a chuck 84 of a known transport arm, and the workpiece 7 is transported to a dicing (DC) tape application device. At this time, since the modification lines 78 are uniformly formed at a predetermined depth from the back surface 76 of the workpiece 7, even if the workpiece 7 is sucked with negative pressure, no cracks are generated in the workpiece 7, and the workpiece 7 can be transported safely.
[0041] [DC tape attached, BG film peeled off] Next, using a known DC tape application device, the workpiece 7 transferred to the chuck 85 is applied to a dicing frame 87 via the DC tape 86. The DC tape 86 is applied by a rolling roller 88 pressing the DC tape 86 against the back surface 76 of the workpiece 7. At this time, since the modification lines 78 are uniformly formed at a predetermined depth from the back surface 76 of the workpiece 7, even if the rolling roller 88 presses the workpiece 7, no cracks are generated in the workpiece 7, and the DC tape 86 can be safely applied.
[0042] Thereafter, the BG film 75 is peeled off from the workpiece 7 using a known peeling device. The BG film 75 is peeled off from the front surface 72 of the workpiece 7 by rolling up the peeling tape 89 that is pressure-bonded to the BG film 75. At this time, since the modification line 78 is uniformly formed at a predetermined depth from the back surface 76 of the workpiece 7, no cracks are generated in the workpiece 7 even when the BG film 75 is peeled off from the workpiece 7, and the DC tape 86 can be safely attached.
[0043] As described above, the flycutting device 1 according to an embodiment of the present invention is a flycutting device 1 that cuts the upper surface 75c of a BG film 75 attached to a workpiece 7 including a bump region 73 having bumps 71 formed on a surface 72 and an outer peripheral region 74 around the bump region 73, and is equipped with a flycutting tool 21, a tool spindle 22 to which the flycutting tool 21 is attached at its lower end and which can be raised and lowered while rotating the flycutting tool 21, and a chuck 3 that rotatably holds the workpiece 7, and is configured so that the flycutting tool 21 cuts the upper surface 75c of the BG film 75 from the center toward the outer periphery.
[0044] According to this configuration, the central region 73 of the BG film 75 is cut relatively thinner than the outer peripheral region 74, so that when the upper surface 75c side of the BG film 75 is adsorbed and held by the chuck 3, the entire surface of the BG film 75 can be adsorbed and held by the chuck 3. This allows the workpiece 7 to be ground safely. In addition, since the modification line 78 is formed at an approximately constant depth from the back surface 76 of the workpiece 7 in the ML process, the occurrence of microcracks in the workpiece 7 can be suppressed when the workpiece 7 is transported, when the DC tape 86 is applied, or when the BG film 75 is peeled off.
[0045] In addition, the fly-cutting device 1 is configured such that the fly-cutting tool 21 includes a ring frame 21a attached to the tool spindle 22, and a cutting tool 21b that is attached to the outer periphery of the ring frame 21a and is capable of cutting the BG film 75.
[0046] According to this configuration, the tool bit 21b can be attached to the tool spindle 22 via the ring frame 21a.
[0047] In addition, in the fly-cutting device 1, the rotation axis 31a of the chuck 3 is set at a predetermined angle, and the holding surface 3a of the chuck 3 that holds the workpiece 7 is formed in a convex shape with the center higher than the outer periphery.
[0048] According to this configuration, a gap is secured between the BG film 75 and the bite 21b after the bite 21b cuts through the outer periphery of the BG film 75 to the outside and returns to the center of the BG film 75, thereby preventing the bite 21b from contacting the BG film 75 in an unintended position.
[0049] The fly cutter 1 is also configured to include a cooling water nozzle 4 that supplies cooling water to the upper surface 75c of the BG film 75.
[0050] According to this configuration, when the BG film 75 is cut, the temperature of the BG film 75 can be prevented from rising excessively.
[0051] The fly-cutting device 1 is also configured to include a thickness sensor 5 that measures the thickness of the BG film 75 during cutting by the fly-cutting tool 21, and a control unit 6 that calculates the time it takes for the BG film 75 to reach the finished thickness based on the measurement value of the thickness sensor 5, the rotation speed of the fly-cutting tool 21, the rotation speed of the chuck 3, and the descent speed of the tool spindle 22.
[0052] According to this configuration, the finished thickness of the BG film 75 can be appropriately controlled.
[0053] Furthermore, the present invention can be modified in various ways other than those described above without departing from the spirit of the present invention, and it goes without saying that the present invention extends to such modifications. [Explanation of symbols]
[0054] 1: Fly cutting device 2:Cutting means 21: Flycut tool 21a: Ring frame 21b :byte 21c: Bolt 22: Tool spindle 22a: Rotating shaft 23: Spindle feed mechanism 24: Column 3: Zipper 3a: Holding surface 31: Chuck spindle 31a: Rotating shaft 32: Adsorbent 4: Cooling water nozzle 5: Thickness sensor 51, 52: Measuring head 6: Control section 7: Work 71: Bump 72 :Surface 73: Bump area 74: Outer area 75: BG film 75a: Base material 75b: Adhesive 75c:Top surface 76: Back side 77: Step 78: Reformation line L: Fly cut line
Claims
1. A flycutting device for cutting an upper surface of a protective film attached to a workpiece, the upper surface of the protective film including a bump region on which bumps are formed and an outer peripheral region around the bump region, A fly-cutting tool; a tool spindle having a lower end attached to the fly-cutting tool and capable of ascending and descending while rotating the fly-cutting tool; A chuck that rotatably holds the workpiece; Equipped with A fly-cutting device, characterized in that the fly-cutting tool cuts the upper surface of the protective film from the center toward the outer periphery.
2. The fly-cutting tool comprises: a ring frame attached to the tool spindle; a cutting tool attached to an outer periphery of the ring frame and capable of cutting the protective film; 2. The flycutting device according to claim 1, further comprising:
3. The rotation axis of the chuck is inclined at a predetermined angle, 3. The flycutting device according to claim 1, wherein the holding surface of the chuck for holding the workpiece is formed in a convex shape with a center higher than an outer periphery.
4. 4. The fly-cutting device according to claim 1, further comprising a cooling water nozzle for supplying cooling water to an upper surface of the protective film.
5. a thickness sensor for measuring a thickness of the protective film during cutting by the fly-cut tool; a cutting time prediction unit that calculates a time for the protective film to reach a finished thickness based on the measurement value of the thickness sensor, the rotation speed of the fly-cutting tool, the rotation speed of the chuck, and the descending speed of the tool spindle; 5. The fly-cutting device according to claim 1, further comprising:
Citation Information
Patent Citations
Wafer processing method of processing wafer having bumps formed thereon and apparatus for processing wafer
JP2009206475A
Wafer grinding method
JP2013021017A
Setup method of bit cutting device
JP2015107535A
Cutting tool device
JP2015208796A
Processing method of wafer
JP2018182129A