Gate interface engineering with doped layers

By forming a silicon layer with dopants and controlled oxidation, followed by high-k dielectric material integration, the method addresses gate leakage and quality issues in high dielectric constant materials, enhancing device performance and yield.

JP7562709B2Active Publication Date: 2024-10-07APPLIED MATERIALS INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2022577138
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-06-17
Filing Date
2021-06-08
Publication Date
2024-10-07
Estimated Expiration
2041-06-08

AI Technical Summary

Technical Problem

The challenge lies in maximizing the performance of high dielectric constant materials in gate structures while addressing issues such as gate leakage and poor quality oxide layers, which are exacerbated by device scaling, particularly in silicon oxide gate dielectrics and high-k materials.

Method used

A method involving the formation of a silicon layer with dopants, followed by controlled oxidation and removal of sacrificial oxides, and the use of high-k dielectric materials, all performed under controlled conditions to limit oxidation spread and enhance quality.

Benefits of technology

This approach results in high-quality gate oxides that suppress excessive oxidation, improve electrical and thermal performance, and reduce gate leakage, enabling better device yield and reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562709000001
    Figure 0007562709000001
  • Figure 0007562709000002
    Figure 0007562709000002
  • Figure 0007562709000003
    Figure 0007562709000003
Patent Text Reader

Abstract

A processing method may be performed to fabricate a semiconductor structure. The method may include forming a silicon layer over a semiconductor substrate. The forming may include forming the silicon layer incorporating a dopant. The method may include oxidizing a portion of the silicon layer while maintaining the portion of the silicon layer in contact with the semiconductor substrate. The oxidation may drive a portion of the dopant through the silicon layer into the semiconductor substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0001] This application claims priority to U.S. patent application Ser. No. 63 / 040,107, entitled "GATE INTERFACE ENGINEERING WITH DOPED LAYER," filed Jun. 17, 2020, which is incorporated by reference in its entirety.

[0002]

[0002] The present technology relates to semiconductor systems, processes, and equipment. More specifically, the present technology relates to processes for strengthening gate structures. [Background technology]

[0003]

[0003] The performance of logic gates is related to the properties of the materials used as well as the thickness and area of ​​the structural layers. However, as some gate properties are tailored to accommodate device scaling, challenges arise. For example, for silicon oxide gate dielectrics, reducing the thickness can improve capacitance, increase channel mobility, and speed up device performance. However, as the thickness continues to decrease, gate leakage can affect devices and reduce device yield. Furthermore, the reduced oxide can degrade and cause shorts. To reduce the effective oxide thickness while limiting the impact on gate leakage, high-k materials have been employed for the gate dielectric. However, efforts to maximize the use of certain high-k materials have been limited by morphology issues associated with forming the high-k materials.

[0004]

[0004] Thus, there is a need for improved systems and methods that can be used to maximize the performance of high dielectric constant materials and enable the production of high quality devices and structures. These and other needs are addressed by the present technique. Summary of the Invention

[0005]

[0005] A processing method may be performed to fabricate a semiconductor structure. The method may include forming a silicon layer over a semiconductor substrate. The forming may include forming the silicon layer incorporating a dopant. The method may include oxidizing a portion of the silicon layer while maintaining the portion of the silicon layer in contact with the semiconductor substrate. The oxidation may drive a portion of the dopant through the silicon layer into the semiconductor substrate.

[0006] In some embodiments, the silicon layer may be formed by atomic layer deposition or epitaxial growth. The dopant may be or may include one or more of nitrogen, phosphorus, or fluorine. The silicon layer may be formed to a thickness of about 5 nm or less. A sacrificial oxide may be formed by oxidizing a portion of the silicon layer, and the method may also include removing the sacrificial oxide. The removing may include an in situ dry chemical process. The removing may be performed in a first processing chamber, and the method may also include forming an oxygen-containing material. The method may include transferring the semiconductor substrate from the first processing chamber to a second processing chamber. The method may include forming a high-k dielectric material overlying the oxygen-containing material. Prior to forming the high-k dielectric material, the method may include introducing reactive ligands to the oxygen-containing material using a nitrogen-containing precursor or an oxygen-containing precursor.

[0007]

[0007] The nitrogen-containing precursor may be or may include ammonia. The high-k dielectric material may be or may include at least one element selected from the group including hafnium, zirconium, silicon, lanthanum, aluminum, titanium, or strontium. The method may be performed in one or more process chambers without exposing the semiconductor substrate to air. The silicon layer may be epitaxially formed on the semiconductor substrate, and the semiconductor substrate may be or may include silicon germanium. A sacrificial oxide may be formed by oxidizing a portion of the silicon layer, and forming the sacrificial oxide may include a first oxidation process. In the method, oxidizing the portion of the silicon layer in contact with the semiconductor substrate may include a second oxidation process different from the first oxidation process. Oxidizing the portion of the silicon layer in contact with the semiconductor substrate may include providing a nitrogen-oxygen containing precursor to the semiconductor substrate. Oxidizing the portion of the silicon layer in contact with the semiconductor substrate may be performed at a temperature of about 750°C or less.

[0008] Some embodiments of the present technique may include a method of forming a semiconductor structure. The method may include removing an oxide from a surface of a substrate contained in a semiconductor processing chamber. The substrate may be or may include a silicon germanium fin. The method may include forming a silicon layer over a semiconductor substrate. The forming may include forming a silicon layer incorporating nitrogen, fluorine, or phosphorus as a dopant. The method may include oxidizing the silicon layer to form a sacrificial oxide. The oxidation may cause a portion of the dopant to diffuse through the silicon layer to the semiconductor substrate. The method may include removing the sacrificial oxide. The method may include providing nitrous oxide to the substrate to form an oxygen-containing material. The method may include pretreating the oxygen-containing material by contacting the substrate with a nitrogen-containing precursor. The method may include forming a high-k dielectric material overlying the pretreated oxygen-containing material.

[0009] In some embodiments, the removing may include an in situ dry chemical process. The removing may be performed in the first processing chamber. The method may also include transferring the substrate from the first processing chamber to a second processing chamber prior to forming the high-k dielectric material. The silicon layer may be formed by atomic layer deposition or epitaxial growth, and the silicon layer may be formed to a thickness of about 5 nm or less. Forming the sacrificial oxide may include delivering an oxygen-containing precursor and a hydrogen-containing precursor to the substrate to form the oxygen-containing material.

[0010]

[0010] Some embodiments of the present technique may include a method of forming a semiconductor structure. The method may include removing a native oxide from a surface of a substrate contained in a semiconductor processing chamber. The substrate may include silicon germanium. The method may include forming a silicon layer over the semiconductor substrate. The forming may include forming a silicon layer incorporating a dopant. The method may include oxidizing a portion of the silicon layer to form a sacrificial oxide while maintaining the portion of the silicon layer in contact with the semiconductor substrate. The oxidation may drive a portion of the dopant through the silicon layer and into the semiconductor substrate. The method may include removing the sacrificial oxide.

[0011]

[0011] The above techniques may provide numerous advantages over conventional systems and techniques. For example, the process may allow for the incorporation of dopants into the channel region of a semiconductor structure, producing a high quality oxide layer for the gate oxide. Additionally, the fabrication of the gate oxide may limit oxidation extending to underlying layers. These and other embodiments, along with their many advantages and features, are described in more detail in conjunction with the following description and accompanying drawings.

[0012] A further understanding of the nature and advantages of the disclosed technology may be realized by reference to the remaining portions of the specification and the drawings. [Brief description of the drawings]

[0013] [Figure 1]FIG. 1 illustrates a top view of an exemplary processing system in accordance with an embodiment of the present technique. [Diagram 2] 1A-1D illustrate selected steps in a method of forming a semiconductor structure in accordance with embodiments of the present technique. [Figure 3A-3F] 1 is a schematic cross-sectional view illustrating an exemplary substrate according to an embodiment of the present technology; [Figure 3G-3I] 1 is a schematic cross-sectional view illustrating an exemplary substrate according to an embodiment of the present technology; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014]

[0016] Some figures are included as schematics. It should be understood that the figures are for illustrative purposes and should not be considered to scale unless scale is explicitly stated. Furthermore, as schematics, the figures are provided to aid in understanding and may not include all aspects or information as compared to realistic representations and may include exaggerated material for illustrative purposes.

[0015]

[0017] In the accompanying figures, similar components and / or features may be labeled with the same reference label. Additionally, various components of the same type may be distinguished by following the reference label with a letter that distinguishes the similar components. When only a first reference label is used herein, the description applies to any one of the similar components having the same first reference label, regardless of the letter.

[0016]

[0018] As the dimensions of logic gate structures shrink, new material structures are required to obtain improvements. High-k dielectrics increase the dielectric constant of the gate stack compared to conventional gate stacks using materials such as silicon oxide. However, as with silicon oxide, decreasing the thickness of the material increases the gate leakage. For example, decreasing the effective oxide thickness increases the gate leakage. Thus, the inverse relationship between gate leakage and effective oxide thickness can limit the performance of transistors and fabricated devices.

[0017]

[0019] In a FinFET structure, the gate oxide on top of the fin can serve many functions. For example, the gate oxide can form a conductive channel region under the gate. Defects or holes in the gate oxide, such as from poor quality oxide, can cause shorts and damage to the structure. Additionally, the gate oxide can inhibit the diffusion of germanium in the PFET or P-MOS regions of the device. Prior art techniques often use wet oxidation techniques, such as Chemox, in conjunction with other oxidation methods to form the gate oxide. Prior art techniques produce poor quality oxide layers that can be poorly controlled and can cause oxidation to overextend into the fin. This can result in a less robust germanium oxide material that can be more susceptible to damage from thermal or electrical stress. The present technique overcomes these issues by forming a controlled gate oxide layer from a defined silicon-containing material. This gate oxide layer can inhibit over-oxidation of the SiGe fin material and can provide improved electrical and thermal performance over prior art techniques. The present technique also provides a mechanism for incorporating dopants into the channel region and other substrate structures with overlying layers.

[0018]

[0020] While the remaining disclosure will always identify specific deposition and treatment processes using the disclosed technology, it will be readily understood that the systems and methods are equally applicable to a variety of other processes that may be performed in the described chambers. Thus, the present technology should not be considered limited to use with only the described treatment and deposition processes. Before describing the steps of an exemplary process sequence according to the present technology, the present disclosure will describe one possible system that can be used with the present technology to perform certain elements of a deposition or treatment step. It should be understood that the present technology is not limited to the described equipment, and the described processes may be performed in any number of processing chambers and systems.

[0019]

[0021] FIG. 1 illustrates a top view of one embodiment of a deposition, etch, bake, and / or cure chamber processing system 100 according to an embodiment. The tool or processing system 100 illustrated in FIG. 1 may include multiple process chambers 114A-D, a transfer chamber 110, a service chamber 116, an integrated metrology chamber 117, and a pair of load lock chambers 106A-B. The process chambers may include any number of structures or components and any number or combination of process chambers. It should be understood that the system 100 is not intended to limit the tools in which the chambers for performing the processes described below may be incorporated. Any tool including any number of chambers may be used in accordance with some embodiments of the present technique.

[0020]

[0022] The transfer chamber 110 may include a robotic transport mechanism 113 for transporting substrates between chambers. The transport mechanism 113 may have a pair of substrate transport blades 113A each attached to a distal end of an extendable arm 113B. The blades 113A may be used to transport individual substrates into and out of process chambers. In a process, one of the substrate transport blades, such as blade 113A of the transport mechanism 113, may retrieve a substrate W from one of the load lock chambers, such as chambers 106A-B, and transport the substrate W to a first stage of processing, such as the processing processes described below, for example, in chambers 114A-D. The chambers may be included to perform individual or multiple steps of the described techniques. For example, one or more chambers may be configured to perform a deposition or formation step, while one or more other chambers may be configured to perform one or more of the pre-processing steps and / or post-processing steps described. Any number of configurations are encompassed by the present technology, which may also perform any number of additional fabrication steps typically performed in semiconductor processing.

[0021]

[0023] If a chamber is occupied, the robot may wait until processing is complete and then remove the processed substrate from the chamber with one blade 113A and insert a new substrate with a second blade (not shown). Once the substrate has been processed, it may then be moved to a second stage of processing. At each move, the transport mechanism 113 may generally have one blade carrying a substrate and one blade that is empty to perform a substrate swap. The transport mechanism 113 may wait at each chamber until the swap can be accomplished.

[0022]

[0024] Once processing is completed in the process chambers, the transport mechanism 113 may remove the substrate W from the last process chamber and transport the substrate W to a cassette in the load lock chambers 106A-B. From the load lock chambers 106A-B, the substrate may be moved into the factory interface 104. The factory interface 104 may be operable to transfer substrates between the pod loaders 105A-D and the load lock chambers 106A-B, which are generally in a clean environment at atmospheric pressure. The clean environment of the factory interface 104 may generally be provided through an air filtration process, such as HEPA filtration. The factory interface 104 may also include a substrate orienter / aligner (not shown) that may be used to properly align the substrate prior to processing. At least one substrate robot, such as robots 108A-B, may be positioned in the factory interface 104 to transport substrates between various locations / locations in the factory interface 104 and other locations associated therewith. The robots 108A-B may be configured to move along a track system within the factory interface 104 from a first end to a second end of the factory interface 104.

[0023]

[0025] The processing system 100 may further include an integrated metrology chamber 117 for providing control signals that may provide adaptive control for any of the processes being performed in the processing chambers. The integrated metrology chamber 117 may include any of a variety of metrology devices for measuring various film properties such as thickness, roughness, composition, etc., and the metrology devices may further be capable of automatically characterizing lattice parameters such as critical dimensions, sidewall angles, and feature heights under vacuum.

[0024]

[0026] Each of the processing chambers 114A-D may be configured to perform one or more process steps in the fabrication of semiconductor structures, and any number and combination of processing chambers may be used in the multi-chamber processing system 100. For example, any of the processing chambers may be configured to perform a number of substrate processing steps, including any number of deposition processes, including cyclical layer deposition, atomic layer deposition, chemical vapor deposition, physical vapor deposition, and other steps, including etching, pre-cleaning, pre-treatment, post-treatment, annealing, plasma treatment, degassing, orientation, and other substrate processes. Some specific processes that may be performed in any of the chambers, or any combination of the chambers, may be metal deposition, surface cleaning and preparation, thermal annealing, such as rapid thermal processing, and plasma treatment. Any other process may be similarly performed in a specific chamber incorporated within the multi-chamber processing system 100, including any of the processes described below that would be readily understood by one of ordinary skill in the art.

[0025]

[0027] FIG. 2 illustrates a method 200 for forming a semiconductor structure, the steps of which may be performed, for example, in one or more chambers incorporated in the multi-chamber processing system 100 as described above, or in any other multi-chamber system. The method 200 may include one or more steps prior to the initiation of the described method steps, including front-end processing, deposition, etching, polishing, cleaning, or any other steps that may be performed prior to the described steps. The method may include many optional steps illustrated in the figures, which may or may not be specifically related to the method of the present technology. For example, many of the steps are described to provide a broader range of structure formation processes, but are not critical to the present technology, or may be performed by alternative methodologies as described further below. The method 200 illustrates steps illustrated generally in FIGS. 3A-3I, which illustrations are described in conjunction with the steps of the method 200. It should be understood that FIG. 3 illustrates only a partial schematic diagram, and the substrate may include any number of transistor sections and additional materials having the aspects shown in the figures.

[0026]

[0028] Method 200 may include optional steps for developing the semiconductor structure to a particular manufacturing step. In some embodiments, method 200 may be performed on a base structure, but in some embodiments, the method may be performed subsequent to other material formation. As shown in FIG. 3A, the semiconductor structure may represent device 300 after certain processing has been completed. For example, substrate 305 may be a planar material, or may be a structured device that may include one or more materials configured as or defining posts, trenches, or other structures as well understood to be encompassed by the present technology. Substrate 305 may include any number of materials including silicon, silicon germanium, or silicon-containing materials such as oxides, nitrides, and carbides of silicon, as well as any other material that may be incorporated into a structure. In some embodiments encompassed by the present technology, substrate 305 may be part of a silicon germanium fin, such as may be associated with a FinFET structure, or may be part of a P-MOS region. Prior to method 200, a layer of silicon germanium may be formed on a silicon substrate, or other substrate, and patterned to form a fin structure. An insulating dielectric may be formed around the fins and a trim process may be performed to thin the tops of the fins. It should be understood that the figures are not to any particular scale.

[0027]

[0029] Following this processing, or as a result of the transfer of the substrate, the substrate 305 may include native oxide 310 or residual particulate material on the surface of the silicon germanium, as shown in FIG. 3A. The exposed material on the surface of the substrate 305 may be etched, planarized, or otherwise processed to produce an intermittent pattern in some embodiments. Although illustrated as a single example, it should be understood that the device 300 may include smaller sections of a larger process integration that may include any number of additional sections that may be similar to or different from the objects illustrated. For example, an N-MOS region may be positioned adjacent to the illustrated structure and may include any amount of patterning or steps performed in conjunction with or apart from the described methods. The substrate 305 may be contained or positioned in a processing region of a semiconductor processing chamber, and the method 200 may be performed to fabricate a semiconductor material, such as a high-k dielectric material, in the substrate.

[0028]

[0030] The method 200 may include, in optional step 205, removing the native oxide 310 from the substrate 305. Removing the native oxide 310 may be performed by any number of processes. For example, reduction may be performed by using a hydrogen-containing precursor, which may reduce the oxide to ensure a relatively clean surface of the silicon germanium. Additionally, the process may include a plasma process or treatment that may include a fluorine-containing precursor and a hydrogen-containing precursor. The fluorine-containing precursor may be or include nitrogen trifluoride as well as any other fluorine-containing precursor. The hydrogen-containing precursor may be characterized by an amine group [-NH2] or other nitrogen- or hydrogen-containing group. For example, the hydrogen-containing precursor may be or include a nitrogen-hydrogen-containing precursor such as ammonia as one non-limiting example. The plasma may be generated locally or in a remote plasma region that may be fluidly coupled to the substrate processing region. The flow rate of the fluorine-containing precursor and the flow rate of the hydrogen-containing precursor may be controlled to maintain an atomic flow ratio of hydrogen to fluorine of less than 1:2. The oxide 310 or residual material may be removed by plasma effluents 315, as shown in FIG. 3B, which process may also include a heat treatment to remove by-products from the etching process.

[0029]

[0031] The removal of the native oxide in step 205 may be by an in situ dry chemical process that may not expose the substrate surface to air or an oxygen-containing environment. The removal of the native oxide in step 205 may be performed in a first processing chamber in some embodiments of the method 200. The method 200 may include transferring the substrate from the first processing chamber to a second processing chamber prior to forming the high-k dielectric material, as described below. The method 200 may include performing the steps in one or more processing chambers without exposing the substrate surface to air or atmosphere, such as by maintaining a vacuum in the system 100 while transferring the substrate between one or more chambers for the steps of the method 200. Maintaining an integrated vacuum may advantageously reduce the formation of unwanted oxides as well as contamination of the surface. The transfer may be performed between one or more chambers on a single platform, or between chambers on multiple platforms. However, by utilizing a single platform, it may be better ensured that exposure of the substrate to an oxygen environment is avoided.

[0030]

[0032] In step 210, a silicon-containing material may be formed or deposited on the pretreated or cleaned substrate surface. For example, as shown in FIG. 3C, a layer of silicon, or a silicon-containing material such as doped silicon, alloyed silicon, or silicon-metalloid or silicon and metal materials may be formed or deposited by any number of methods to form a layer 320 overlying the surface of the substrate 305. In some non-limiting embodiments, silicon may be conformally epitaxially grown on the surface of the silicon germanium fin. Additionally, an atomic layer deposition process may be performed to produce a silicon layer that is conformally deposited or formed on the substrate. Conformal formation may allow for more control over the thickness than conventional deposition techniques. The layer may be formed to any height, and relatively high quality silicon may be produced. For example, the silicon layer 320 may be formed to a height of several angstroms or nanometers in various embodiments. In some embodiments, the layer can be formed to a thickness of about 10.0 nm or less, and can be formed to a thickness of about 8.0 nm or less, about 5.0 nm or less, about 4.0 nm or less, about 3.0 nm or less, about 2.0 nm or less, about 1.0 nm or less, about 9 Å or less, about 8 Å or less, or less.

[0031]

[0033] In some embodiments, the silicon layer may be formed as amorphous silicon and may include dopant materials during the formation process. As shown in FIG. 3C, dopant particles 321 may be incorporated into the silicon layer during deposition. The dopant may be provided as an additional precursor that may further interact with one or more silicon-containing precursors or other deposition precursors or carrier gases to incorporate the dopant particles into the silicon material being formed. Exemplary dopant materials may be nitrogen, phosphorus, fluorine, or any other material that may be incorporated into the silicon structure. Although the material may be provided in any number of forms, the material may be provided in a more easily dissociable form to limit additional material incorporation into the silicon layer. For example, exemplary precursors may include diatomic nitrogen, nitrogen trifluoride, fluorine, hydrogen fluoride, phosphine, or any other nitrogen-, fluorine-, or phosphorus-containing material.

[0032]

[0034] Following the formation of the silicon layer, a portion of the layer may be oxidized in step 215. The oxidation may be performed in any number of ways, and may completely oxidize the layer, although the oxidation may not extend completely through the silicon layer. The oxidation step 215 may generate a sacrificial oxide 322 by converting a portion of the silicon layer 320, up to the entire silicon layer, to silicon oxide. The oxidation step 215 may oxidize a portion of the silicon layer 320 while maintaining the portion of the silicon layer 320 at least partially in contact with the semiconductor substrate 305. For example, a controlled oxidation may be performed to limit the oxidation from spreading through the silicon-containing layer. Step 215 may include a thermal-based reaction with steam, such as an in-situ steam generation process, in which oxidation occurs at a slower rate compared to conventional thermal techniques. Additionally, the oxidation may use hydrogen and oxygen together as a thermal oxidation process, and additional precursors may also be used. For example, in some embodiments, an oxygen-containing precursor, such as a nitrogen-oxygen-containing precursor, may be used. For example, nitrous oxide, or other nitrogen-oxygen containing precursors, and / or additional precursors, such as hydrogen, can be used to oxidize portions of the silicon-containing material.

[0033]

[0035] The nitrogen can act as an oxygen carrier and may not become part of the interface or substrate. The process can also be performed slowly, which can result in more controlled oxidation, and can be controlled to maintain a particular thickness of silicon along the surface of the substrate 305. Following the formation of the sacrificial oxide, a number of other manufacturing steps can be performed, including the formation of a dummy poly mask, followed by the formation of a dummy gate in the substrate. After processing has been performed, a gate oxide formation process can be performed, as described further below.

[0034]

[0036] The oxidation process may also be used to facilitate additional steps. For example, by incorporating a dopant into the silicon layer, the oxidation process may be used to thermally drive the dopant 321 through the silicon layer and into the underlying substrate, as shown in FIG. 3D. For example, the temperature of the oxidation may allow the dopant material to fully diffuse through the silicon layer and become incorporated into the underlying material. Incorporating fluorine, nitrogen, or phosphorus into the substrate, such as the underlying channel region, which may be beneath the gate being formed, may improve the operational performance and reliability of the device being formed. While doping may be performed during the formation of the underlying channel region, incorporating the dopant following the oxidation step may ensure high quality formation throughout the channel region. Furthermore, formation may be performed without excessive incorporation of other components of the dopant material, such as hydrogen, or other components of the dopant, provided in the form of a precursor.

[0035]

[0037] One or more removal steps may be performed in optional step 220 to remove the sacrificial oxide covering the retained silicon 320. As shown in FIG. 3E, the retained silicon may be characterized by a thickness sufficient to maintain coverage over the silicon germanium substrate material. For example, in some embodiments, the silicon layer 320 may be maintained at about 5 nm or less, and may be maintained at about 4 nm or less, about 3 nm or less, about 2 nm or less, about 1 nm or less, about 5 Å or less, or less. The removal step may include a selective etch, such as an oxide-selective etch. In some embodiments, a plasma etching process may be performed, such as using a fluorine-containing precursor and a hydrogen-containing precursor. The removal step may include any of the steps described above, such as by utilizing nitrogen trifluoride and ammonia plasma etching, which may include additional heat treatments or sublimation steps. Additional or alternative fluorine and hydrogen-containing precursors may also be used in some embodiments. By performing an oxide-selective etch process in step 220, portions of the underlying silicon may be maintained or substantially maintained.

[0036]

[0038] After the silicon cap material is exposed, a second oxidation step may be performed to oxidize the remaining silicon layer material covering the silicon germanium fin. In optional step 225, any of the previous oxidation steps may be performed to produce an oxygen-containing material 324 shown in FIG. 3F, such as silicon oxide. In some embodiments, the remaining silicon material may be completely converted to silicon oxide, and no residual silicon layer may remain. In some embodiments, the oxidation may utilize nitrous oxide and hydrogen, as described above. This allows the oxidation to be tightly controlled to substantially confine the silicon material, while limiting or preventing over-oxidation to silicon germanium material. Such a thermal oxidation process may provide many advantages, as described above. For example, unlike wet oxidation, this oxidation may produce high quality oxide and limit germanium diffusion.

[0037]

[0039] Furthermore, some conventional oxidation processes, including wet and dry oxidation processes, can cause excessive oxidation to silicon germanium, producing germanium oxide materials. Germanium oxide can be characterized by fewer stable bonds compared to silicon oxide, and as a result, subsequent processes can break the bonds of germanium oxide. This can damage the oxide formed or reduce the quality of the interface between materials, which can limit the efficiency of the transistor or damage the device. Forming a high quality oxide can advantageously protect the structure during subsequent steps. For example, conventional processes that produce low density oxides can be further degraded during additional manufacturing steps. Additional high-k dielectric steps, which can include high temperature processes, can be performed as described below, as well as subsequent manufacturing. For example, flash annealing can be performed at up to 1000° C. at some point in manufacturing. A lower quality or density oxide can further promote diffusion of germanium due to a more porous oxide structure. A denser thermal oxide process according to some embodiments of the present technology can protect against diffusion during subsequent manufacturing steps. By maintaining controlled oxidation according to embodiments of the present technique, high quality oxide material with specific depths can be provided at any of the reduced thicknesses mentioned above.

[0038]

[0040] The formed oxygen-containing material may be of high quality and highly ordered, meaning a crystallographic structure that is free or substantially free of defects. This may provide an interface that may prevent additional materials from closely accessing the channel region, thus preventing leakage. The resulting oxygen-containing material 324 may include silicon dioxide. The formed oxygen-containing material 324 may have a thickness of up to about 5 Å, and may have a thickness of about 5 Å or more, about 10 Å or more, about 15 Å or more, about 20 Å or more, about 25 Å or more, about 30 Å or more, or more.

[0039]

[0041] The method 200 may include, in optional step 230, delivering a pretreatment precursor to the substrate. The pretreatment precursor may be or may include a nitrogen-containing precursor or an oxygen-containing precursor. The precursor may contact the substrate and may form or introduce reactive ligands to the exposed surface of the substrate, shown as ligands 325 in FIG. 3G. Unlike the prior art, the present technology may utilize a pretreatment configured to provide ordered growth of high-k dielectric material in a subsequent step.

[0040]

[0042] The pretreatment precursor may be or may include any nitrogen-containing precursor or oxygen-containing precursor. The oxygen-containing precursor may be characterized by a hydroxyl group [-OH] and may be incorporated into the surface of the oxygen-containing material 324 of the substrate. The nitrogen-containing precursor may be characterized by an amine group [-NH2] or other nitrogen-containing group. For example, the nitrogen-containing precursor may be or may include a nitrogen-hydrogen-containing precursor, such as ammonia as one non-limiting example, or a nitrogen-oxygen-containing precursor, or any other precursor containing nitrogen.

[0041]

[0043] The surface termination in some embodiments may be or may include a hydroxyl or amine group terminated surface. Method 200 may then include forming a high-k dielectric material overlying the oxygen-containing material in optional step 235. While the present technique may encompass any formation or deposition of a high-k material, in some embodiments, forming step 235 may be or may include atomic layer deposition, which may utilize any number of atomic layer deposition chambers. Formation, if performed, may be performed directly after pre-treating the substrate or oxygen-containing material surface, and may be performed in the same chamber as pre-treatment, or in an additional chamber, such as an additional chamber incorporated in the same system, such as system 100. In some embodiments, vacuum conditions may be maintained while the substrate is transferred from the pre-treatment chamber to the deposition or formation chamber, which may limit exposure of the substrate to air.

[0042]

[0044] When an atomic layer deposition process is performed to form a high-k dielectric material, a metal-containing precursor may be provided to the substrate to react with the pretreated surface. For example, a transition metal-containing precursor, a poor metal-containing precursor, or a lanthanide metal-containing precursor may be provided to the process chamber to interact with reactive ligands exposed on the substrate from the pretreatment. An oxygen-containing precursor may then be provided in a second step, followed by purging the metal-containing precursor, etc. This may produce an atomic layer deposition oxide layer, such as layer 330a shown in FIG. 3H. In one non-limiting example, a hafnium-containing precursor may be provided in a first step and an oxidizer may be provided in a second step to produce a hafnium oxide film. The additional metal-containing precursor may include a zirconium-containing precursor to produce a zirconium-containing material, and any other number of metal-containing precursors to produce additional metal oxide structures. For the hafnium-containing precursor, and similarly for any alternative metal, the precursor may be or include a halogen-containing precursor, an oxygen-containing precursor, a hydrogen-containing precursor, or a carbon-containing precursor, all of which incorporate hafnium.

[0043]

[0045] For the oxidizing agent, any oxygen-containing precursor that can react with the metal-containing material can be used. For example, the oxygen-containing precursor can be or include water, diatomic oxygen, ozone, hydroxyl-containing precursors or alcohols, nitrogen-oxygen-containing precursors, plasma-enhanced oxygen, including local or remote enhanced oxygen, or any other material containing oxygen that can be incorporated with a metal, such as hafnium, to produce a metal oxide material layer covering the substrate. Again, any of the metal-containing materials mentioned above can be used in embodiments of the present technology and can include any of the grouped metals, which may include, but are not limited to, for example, hafnium, zirconium, silicon, lanthanum, aluminum, titanium, strontium, or combinations of these materials, such as hafnium silicate.

[0044]

[0046] When pretreatment according to embodiments of the present technology is performed, the structure of the metal-containing material can be formed or deposited in an ordered manner to produce a more uniform grain structure. This can be produced by forming reactive ligands of the pretreatment precursor on the more structured surface material, such as the higher quality silicon or silicon oxide, produced by embodiments of the present technology. Furthermore, further improvements can be obtained by performing the pretreatment exposure under specific conditions.

[0045]

[0047] The pretreatment may be performed at a temperature configured to activate the precursor and / or the surface of the substrate. For example, in situations where a nitrogen-hydrogen containing precursor may be used as the pretreatment precursor, the substrate may be maintained at a temperature of about 300° C. or higher while delivering the precursor. Similarly, pretreatment with an oxygen-containing precursor may also be performed while maintaining the substrate temperature at 300° C. or higher. In any pretreatment step, the substrate may also be maintained at a temperature of about 400° C. or higher, about 500° C. or higher, about 600° C. or higher, about 700° C. or higher, about 800° C. or higher, or higher. If the temperature for the pretreatment is reduced to about 500° C. or lower, the effect may be reduced. Similarly, if the temperature is increased to about 700° C. or higher, nucleation may not be improved and excess precursor may be incorporated into the surface, reducing device mobility. As a result, in some embodiments, the temperature may be maintained at about 500° C. to about 700° C. during the pretreatment.

[0046]

[0048] Similar temperature ranges can affect one or both of the oxidation steps, allowing careful control of both the amount of silicon cap material maintained in the first oxidation and limiting excessive oxidation in the second oxidation. To control the slow ingress of oxygen into the silicon material, the temperature can be maintained at about 900° C. or less, and can be maintained at about 850° C. or less, about 800° C. or less, about 750° C. or less, about 700° C. or less, about 650° C. or less, about 600° C. or less, or less.

[0047]

[0049] Similarly, exposure time can affect the amount of nitrogen-containing precursor incorporated, so that to limit mobility loss in the fabricated device, the exposure of the precursor can be about 3 minutes or less, and in some embodiments, the exposure time can be about 2.5 minutes or less, about 2 minutes or less, about 1.5 minutes or less, about 1 minute or less, about 45 seconds or less, about 30 seconds or less, about 15 seconds or less, or less. Once an appropriate amount of amine groups is incorporated, formation can be performed. Formation, including atomic layer formation, can be performed at any temperature, but in some embodiments, atomic layer deposition can be performed at a temperature similar to or less than the temperature at which pretreatment is performed, regardless of whether the steps are performed in the same chamber or in a different chamber. For example, atomic layer deposition can be performed at a second temperature relative to the pretreatment temperature, and the formation temperature can be about 500° C. or less in embodiments, about 450° C. or less, about 400° C. or less, about 350° C. or less, about 300° C. or less, about 250° C. or less.

[0048]

[0050] After the layer of high-k material is formed or deposited, one or more post-treatment processes may be performed. In some embodiments, the substrate may be transferred from the deposition chamber to another chamber or set of chambers to post-treat the material in optional step 240. As described above, the transfer may be performed in a single processing system having multiple chambers, and thus the transfer from or between any of these chambers may be performed while maintaining vacuum conditions. The method 200 may then include one or more additional post-treatment processes, as described in optional step 245. The post-treatment process may include one or more processes performed in one or more chambers, including multiple chambers on the same cluster tool. The post-treatment process may include oxidation, nitridation, and / or thermal annealing.

[0049]

[0051] As mentioned above, a pretreatment step may be performed to provide sufficient termination sites to provide the aforementioned uniform growth while limiting the incorporation of excess precursor into the substrate. For example, incorporated nitrogen interfaces may reduce the mobility of the fabricated transistor, or the speed at which carriers can move through the structure. Although the above-mentioned pretreatment may further improve the scaling of the high-k film, if not controlled, the pretreatment may actually reduce the mobility of the device. However, in some embodiments, one post-treatment may include oxidizing the high-k material formed with a second oxygen-containing precursor to a first oxygen-containing precursor that may be used in the pretreatment step.

[0050]

[0052] For example, an oxidation step utilizing any of the oxygen-containing precursors described above can be performed to further oxidize the film after formation. The deposition or formation of a high-k film may result in a porous film, or a film containing voids in its structure. The oxidation step may penetrate the film with oxygen species to fill the voids as exemplified by layer 330b, and may also generate oxide material, such as optional layer 320, at the interface of the high-k material if not formed in a previous step described above. This may improve the interface of the underlying layer from the amine end groups and improve the mobility performance of the device. To limit excessive increase in thickness of the underlying oxide layer, the oxidation step may be performed for a limited time and may be performed within any of the time ranges described above.

[0051]

[0053] If used, the post-treatment step may further include contacting the substrate with a second nitrogen-containing precursor to the pre-treatment nitrogen-containing precursor. The second nitrogen-containing precursor may include any of the nitrogen-containing precursors described above, including nitrogen gas and any of the nitrogen-containing precursors described elsewhere. The second nitrogen-containing precursor may include a plasma-activated or enhanced nitrogen-containing precursor, thermally activated nitrogen, or any other nitrogen precursor, which may incorporate nitrogen radicals or nitrogen atoms into the high-k structure and stabilize the film or stabilize the film toward an equilibrium state. Unlike an oxidation step, nitridation may not increase the thickness of an underlayer such as silicon oxide, and may slightly increase the dielectric constant value of the resulting film.

[0052]

[0054] Nitrogen incorporation can be controlled to limit incorporation into the film to maintain structural and electrical properties. In some embodiments, post-treatment nitridation can incorporate up to about 20 atomic % nitrogen in the surface region of the high-k film, and can incorporate up to about 15 atomic % nitrogen, up to about 10 atomic % nitrogen, up to about 8 atomic % nitrogen, up to about 6 atomic % nitrogen, up to about 4 atomic % nitrogen, up to about 2 atomic % nitrogen, or less. In some embodiments, incorporation of about 3 atomic % to about 7 atomic % can maintain a higher dielectric constant value than higher nitrogen incorporations and make the film more stable than lower nitrogen incorporations. Surface region can refer to the exposed surface of the material, but nitrogen incorporation can extend to any distance within the film and can be consistent, or can form a reduction gradient throughout the material.

[0053]

[0055] Although the post-treatment oxidation or nitridation can be carried out at any of the temperatures previously mentioned, in some embodiments, the post-treatment oxidation and / or nitridation can be carried out at a temperature range of about 500° C. or less, and can be carried out at a temperature range of about 400° C. or less, about 300° C. or less, about 200° C. or less, about 100° C. or less, depending on the process being performed.

[0054]

[0056] A post-treatment anneal may be performed following any of the steps, including any of the post-treatment steps described. The post-treatment anneal may be performed in any chamber in which a previous step is performed, or may involve transfer to a different chamber, such as, for example, a chamber configured to perform a rapid thermal anneal process. Again, the chamber may be integrated on the same platform as other chambers, which may allow transfer between chambers while maintaining vacuum conditions. The post-treatment anneal may further align the bonds of the film and further stabilize the film. In embodiments, the post-treatment anneal may be performed at a temperature that may, in some embodiments, be above the deposition temperature or oxidation temperature. For example, the post-treatment anneal may be performed at a temperature of about 400° C. or greater, and in embodiments, may be performed at a temperature of about 500° C. or greater, about 600° C. or greater, about 700° C. or greater, about 800° C. or greater, about 900° C. or greater, or greater.

[0055]

[0057] By performing pre-treatment, oxidation, and / or post-treatment according to embodiments of the present technique, improved high-k materials and semiconductor structures can be produced. The layer of high-k material can be produced to any thickness, including up to about a few nanometers. However, due to the favorable grain structure produced by the present technique, the effective oxide thickness can be produced thinner without loss to gate leakage performance. The high-k materials produced according to the present technique can be characterized by a dielectric constant value of about 10 or more, and can be characterized by a dielectric constant value of about 15 or more, about 20 or more, about 21 or more, about 22 or more, about 23 or more, about 24 or more, about 25 or more, or more.

[0056]

[0058] The present technology further allows for improved dielectric constants compared to the prior art. Furthermore, due to the grain structure produced, the gate leakage current associated with the film may be about 10 times lower than that of a silicon oxide film of similar thickness, the gate leakage current may be about 100 times lower than that of a silicon oxide film of similar thickness, about 1,000 times lower than that of a silicon oxide film of similar thickness, about 5,000 times lower than that of a silicon oxide film of similar thickness, about 10,000 times lower than that of a silicon oxide film of similar thickness, about 20,000 times lower than that of a silicon oxide film of similar thickness, about 50,000 times lower than that of a silicon oxide film of similar thickness, about 100,000 times lower than that of a silicon oxide film of similar thickness, or less. By producing a film according to an embodiment of the present technology, a formed film having a beneficial morphology may be produced, and the electrical properties of the film may be improved compared to the prior art.

[0057]

[0059] In the foregoing specification, for purposes of explanation, numerous details have been set forth in order to provide an understanding of various embodiments of the present technology. However, it will be apparent to one of ordinary skill in the art that particular embodiments may be practiced without some of these details or with additional details.

[0058]

[0060] Although several embodiments have been disclosed, those skilled in the art will recognize that various modifications, alternative configurations, and equivalents may be used without departing from the spirit of the embodiments. Moreover, a number of well-known processes and elements have not been described in order to avoid unnecessarily obscuring the technology. Thus, the above description should not be considered as limiting the scope of the technology.

[0059]

[0061] Where a range of values ​​is provided, it is understood that each intervening value between the upper and lower limit of that range, to the smallest fraction of the unit of the lower limit, is also specifically disclosed, unless the context clearly dictates otherwise. Any narrower range between any stated value or unstated intervening value in a stated range and any other stated or intervening value in that stated range is included. The upper and lower limits of these smaller ranges may be independently included or excluded in the range, and each range in which either or both limits are included in the smaller ranges is also included in the technology, subject to any specifically excluded limit in the stated range. When one or both limits are included in a stated range, ranges excluding one or both of those included limits are also included.

[0060]

[0062] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural references unless the context clearly dictates otherwise. Thus, for example, reference to "a layer" includes a plurality of such layers, reference to "the precursor" includes a reference to one or more precursors and equivalents thereof known to those skilled in the art, and so forth.

[0061]

[0063] Additionally, as used in this specification and the claims that follow, the terms "comprise," "comprising," "contain," "containing," "include," and "including" specify the presence of stated features, integers, components, or steps, but do not exclude the presence or addition of one or more other features, integers, components, steps, operations, or groups.

Claims

1. 1. A method for forming a semiconductor structure, comprising: Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating a dopant forming a silicon layer over a semiconductor substrate; oxidizing a portion of the silicon layer, the oxidation driving a portion of the dopant through the silicon layer and into the semiconductor substrate; Including, The method, wherein the silicon layer is formed to a thickness of about 5 nm or less.

2. The method of claim 1 , wherein the silicon layer is formed by atomic layer deposition or epitaxial growth.

3. 10. The method of claim 1, wherein the dopants include one or more of nitrogen, phosphorus, or fluorine.

4. A method for forming a semiconductor structure, comprising: Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating a dopant forming a silicon layer over a semiconductor substrate; oxidizing a portion of the silicon layer, the oxidation driving a portion of the dopant through the silicon layer and into the semiconductor substrate to form a sacrificial oxide; removing the sacrificial oxide, the removal comprising an in-situ dry chemical process and performed in a first processing chamber; forming an oxygen-containing material; transferring the semiconductor substrate from the first processing chamber to a second processing chamber; forming a high-k dielectric material overlying the oxygen-containing material; A method comprising:

5. 5. The method of claim 4, further comprising prior to forming the high-k dielectric material, introducing reactive ligands into the oxygen-containing material using a nitrogen-containing precursor or an oxygen-containing precursor.

6. 6. The method of claim 5, wherein the nitrogen-containing precursor comprises ammonia.

7. 5. The method of claim 4, wherein the high-k dielectric material comprises at least one element selected from the group consisting of hafnium, zirconium, silicon, lanthanum, aluminum, titanium, and strontium.

8. 10. The method of forming a semiconductor structure of claim 1, performed in one or more processing chambers without exposing the semiconductor substrate to atmosphere.

9. A method for forming a semiconductor structure, comprising: Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating a dopant forming a silicon layer over a semiconductor substrate; oxidizing a portion of the silicon layer, the oxidation driving a portion of the dopant through the silicon layer and into the semiconductor substrate; Including, The method of claim 1, wherein the silicon layer is epitaxially formed on the semiconductor substrate, the semiconductor substrate comprising silicon germanium.

10. A sacrificial oxide is formed by oxidizing a portion of the silicon layer, the forming of the sacrificial oxide comprising a first oxidation process, the method further comprising: oxidizing a portion of the silicon layer in contact with the semiconductor substrate, the second oxidation process being different from the first oxidation process; 10. The method of claim 1 comprising:

11. A method for forming a semiconductor structure, comprising the steps of: Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating a dopant forming a silicon layer over a semiconductor substrate; oxidizing a portion of the silicon layer, the oxidation driving a portion of the dopant through the silicon layer and into the semiconductor substrate; Including, The method, wherein oxidizing the portion of the silicon layer in contact with the semiconductor substrate comprises delivering a nitrogen-oxygen containing precursor to the semiconductor substrate.

12. 12. The method of claim 11, wherein oxidizing the portion of the silicon layer in contact with the semiconductor substrate occurs at a temperature of about 750°C or less.

13. 1. A method for forming a semiconductor structure, comprising: removing oxides from a surface of a substrate contained in a semiconductor processing chamber, the substrate comprising a silicon germanium fin; Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating nitrogen, fluorine, or phosphorus as a dopant forming a silicon layer over a semiconductor substrate; oxidizing the silicon layer to form a sacrificial oxide, the oxidation causing a portion of the dopant to diffuse through the silicon layer and into the semiconductor substrate; removing the sacrificial oxide; providing nitrous oxide to the substrate to form an oxygen-containing material; pretreating the oxygen-containing material by contacting the substrate with a nitrogen-containing precursor; forming a high-k dielectric material overlying the pretreated oxygen-containing material; The method includes:

14. The method of claim 13 , wherein the removing comprises an in-situ dry chemical process.

15. The removing is performed in a first processing chamber, and further comprising: transferring the substrate from the first processing chamber to a second processing chamber prior to forming the high-k dielectric material.

15. The method of forming a semiconductor structure of claim 14, comprising:

16. 14. The method of forming a semiconductor structure of claim 13, wherein the silicon layer is formed by atomic layer deposition or epitaxial growth, and the silicon layer is formed to a thickness of about 5 nm or less.

17. 14. The method of forming a semiconductor structure of claim 13, wherein forming the sacrificial oxide comprises delivering an oxygen-containing precursor and a hydrogen-containing precursor to the substrate to form an oxygen-containing material.

18. 1. A method for forming a semiconductor structure, comprising: removing native oxide from a surface of a substrate contained in a semiconductor processing chamber, the substrate comprising silicon germanium; Forming a silicon layer over a semiconductor substrate, said forming comprising: Forming a silicon layer incorporating a dopant forming a silicon layer over a semiconductor substrate; oxidizing a portion of the silicon layer to form a sacrificial oxide while maintaining a portion of the silicon layer in contact with the semiconductor substrate, the oxidation driving a portion of the dopant through the silicon layer and into the semiconductor substrate; and oxidizing a portion of the silicon layer to form a sacrificial oxide while maintaining a portion of the silicon layer in contact with the semiconductor substrate. removing the sacrificial oxide; and wherein the silicon layer is formed to a thickness of about 5 nm or less.

Citation Information

Patent Citations

  • Manufacture of semiconductor integrated circuit

    JP1995235547A

  • Semiconductor device manufacturing method

    JP2015133412A