Method for detecting surface condition of raw material melt, method for producing single crystal, and CZ single crystal production apparatus
The use of two CCD cameras for parallax-based detection of solidification and melting in single crystal production improves accuracy and efficiency, addressing the limitations of conventional visual inspection methods.
Patent Information
- Application Number
- JP2021031774
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-01
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2041-03-01
AI Technical Summary
Conventional methods for detecting solidification and completion of melting in single crystal production using the Czochralski method are inaccurate and labor-intensive, failing to provide comprehensive views of the crucible interior and relying on visual inspection, which can lead to crucible damage and reduced productivity.
The method employs two CCD cameras to capture images of the melt surface from different angles, utilizing parallax data to automatically detect solidification and melting completion, reducing operator workload and enhancing detection accuracy.
This approach allows for precise and automated detection of solidification and melting, preventing crucible damage and increasing single crystal production efficiency by reducing delays in detecting these critical process stages.
Smart Images

Figure 0007571618000001 
Figure 0007571618000002 
Figure 0007571618000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for detecting the surface state of a raw material melt in single crystal production by the CZ method (Czochralski method), a single crystal production method, and a CZ single crystal production apparatus, and more particularly to a method for detecting solidification and a method for detecting completion of melting in a single crystal production apparatus in a preparation process for pulling a single crystal. [Background technology]
[0002] In a single crystal pulling apparatus using the Czochralski method, in order to produce a plurality of single crystal rods from the same crucible (quartz crucible), it is known to grow and pull a single crystal, and then additionally supply (hereinafter also referred to as "recharge") an amount of solid raw material corresponding to the decrease in the molten raw material into the crucible through a supply pipe, melt it, and then grow and pull the next single crystal again. If the solid raw material is directly added to the molten liquid in the crucible during recharge, the molten liquid may scatter, causing problems such as the raw material adhering to the outside of the crucible or to the supply pipe.
[0003] Therefore, a technique has been adopted in which, after the initial single crystal is pulled up, the surface of the melt remaining in the crucible is solidified to some extent, and raw material is supplied to this solidified surface by recharging, and then melted. Conventional techniques include a method in which an operator visually monitors the solidification state of the melt surface, or a method in which a signal detected by a diameter control visual sensor is processed by image processing, as in Patent Document 1. Disclosed methods for detecting the completion of melting include a method in which an operator periodically visually monitors the condition inside the quartz crucible, a method in which the image inside the crucible is captured by a two-dimensional CCD camera and then binarized and detected from the number of white pixels (Patent Document 2), a method in which the completion of melting is detected by using a change in the fluctuation range of the molten metal surface temperature data or by detecting when the binarized image data of the inside of the furnace camera becomes all 0 (black) (Patent Document 3), and a method in which the completion of melting is detected by using a change in the carbon monoxide concentration in the exhaust gas (Patent Document 4). Patent document 5 discloses a technology that uses two CCD cameras as a means of detecting the position of raw materials during the melting process. The purpose of this technology is to measure distance based on the principle of triangulation using the difference in how the two cameras see (parallax). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 3632427 [Patent Document 2] JP 2000-264780 A [Patent Document 3] Patent No. 3704710 [Patent Document 4] Patent No. 6390606 [Patent Document 5] JP 2017-77981 A Summary of the Invention [Problem to be solved by the invention]
[0005] First, in the case of detecting solidification, the conventional technology uses a visual sensor for diameter control, and therefore only the camera field of view required for detecting the diameter of the crystal can be obtained, making it impossible to grasp the solidification status of the entire crucible. In addition, since the main purpose is to detect the diameter of the crystal, the imaging conditions such as the aperture and shutter speed of the camera are generally adjusted so that the contrast between the meniscus ring and the melt is high. Furthermore, after binarization to stabilize the diameter detection, the edge of the meniscus ring is extracted as a diameter signal from a certain scanning direction in the inspection area, and this signal is used to control the crystal diameter to the desired diameter. However, the solidification formed on the melt surface has a problem that it is difficult to appear as a change in the diameter value because the brightness of the meniscus ring part during diameter detection is low. In addition, the direction in which the solidification stretches is not uniform, so the method of extracting the edge from a certain scanning direction is not suitable for detecting solidification, and so there were problems with detecting solidification with the conventional technology.
[0006] Next, regarding detection of the completion of melting, the above-mentioned example of the conventional method using a visual sensor judges the completion of melting based on the number of white or black pixels in the image after binarization processing, but there was a problem with the accuracy of the timing of detecting the completion of melting. In any case, there has been a demand for a method that can detect the timing of solidification and completion of melting with high accuracy. If solidification progresses too far, it will damage the quartz crucible, and a delay in discovering the completion of melting will lead to a decrease in the productivity of single crystals with that equipment. There is also a demand for reducing the operator's work, such as visual inspection.
[0007] The present invention has been made in consideration of the above problems, and aims to provide a method for detecting the surface condition of a raw material melt, a method for manufacturing a single crystal, and a CZ single crystal manufacturing apparatus, which can automatically detect the timing of solidification and completion of melting of the raw material melt with high accuracy and reduce the burden on the operator in single crystal manufacturing by the CZ method. [Means for solving the problem]
[0008] In order to achieve the above object, the present invention provides a method for detecting a surface state of a raw material melt in a quartz crucible in a single crystal production process by a CZ method, the method comprising the steps of: An arbitrary identical inspection area on the surface of the raw material melt in the quartz crucible is photographed from different directions at the same time using two CCD cameras to obtain a measurement image of the inspection area; The present invention provides a method for detecting the surface condition of a raw material melt, which is characterized by automatically detecting at least one of the solidification timing, when the raw material melt changes from a completely molten state to a state in which a solid is formed on the surface of the raw material melt, and the melting completion timing, when the raw material melt changes from a state in which a solid is formed on the surface of the raw material melt to a completely molten state, using parallax data of the measurement images from the two CCD cameras.
[0009] Such a detection method of the present invention allows the use of parallax data to easily and reliably grasp changes in the state of the raw material melt in the quartz crucible, and achieves high detection accuracy. Moreover, it is possible to similarly detect solidification and completion of melting. Therefore, it is possible to prevent damage to the quartz crucible due to excessive solidification, and a decrease in device productivity due to a delay in discovering completion of melting. Furthermore, because solidification and completion of melting are detected automatically, visual monitoring can be omitted, and the workload of the operator can be reduced.
[0010] At this time, the parallax rate obtained by dividing the parallax data within the inspection area by the area of the inspection area can be used as the parallax data of the measurement image.
[0011] In this manner, the solidification or completion of melting of the raw material melt can be easily detected by using the parallax ratio.
[0012] The solidification timing may be detected when the parallax ratio is 10% or more, and the melting completion timing may be detected when the parallax ratio remains 3% or less for 5 minutes or more.
[0013] With these criteria, the timing of solidification or completion of melting can be grasped more appropriately and stably, and erroneous detections such as determining that solidification has occurred when it has not, or determining that melting has been completed when there is still raw material or solidified residue remaining, can be more reliably prevented.
[0014] After the single crystal is pulled, and before the raw material is recharged, the solidification timing is detected; The timing at which the melting is completed can be detected while the recharged raw material is being melted and before the next single crystal is pulled.
[0015] In this way, when multiple single crystals are produced by recharging, the timing of solidification or completion of melting can be detected simply and reliably, thereby improving the productivity of single crystals.
[0016] The present invention also provides a method for producing a single crystal by the CZ method, which comprises pulling a single crystal from a raw material melt obtained by melting a raw material contained in a quartz crucible with a heater, the method comprising the steps of: After pulling the single crystal, the raw material is recharged and melted, and then the next single crystal is pulled. The present invention provides a method for producing a single crystal, characterized in that when the solidification timing or the melting completion timing is automatically detected by the method for detecting the surface condition of the raw material melt of the present invention, the power of the heater, the position of the quartz crucible, and the position of the heater are automatically controlled to be in accordance with the conditions for the next process.
[0017] According to the manufacturing method of the present invention, when manufacturing a plurality of single crystals by recharging, the single crystal manufacturing apparatus can be operated simply and efficiently, and single crystals can be pulled with high productivity.
[0018] The present invention also provides a CZ single crystal manufacturing apparatus that includes a quartz crucible for accommodating a raw material, and a heater for melting the raw material in the quartz crucible to form a raw material melt, and that pulls a single crystal from the raw material melt, Two CCD cameras that simultaneously capture images of an arbitrary identical inspection area on the surface of the raw material melt in the quartz crucible from different directions; an image processing unit that obtains parallax data of the measurement images of the inspection area obtained by photographing the measurement images with the two CCD cameras; The apparatus further includes at least one of a solidification detection processing unit and a melting completion detection processing unit, the solidification detection processing unit automatically detects, from parallax data of the measurement image, a solidification timing at which the raw material changes from a completely molten state to a state in which a solid is formed on a surface of the raw material melt, The present invention provides a CZ single crystal manufacturing apparatus, characterized in that the melting completion detection processing unit automatically detects the melting completion timing at which the raw material melt changes from a state in which a solidification is formed on the surface to a completely molten state from the parallax data of the measurement image.
[0019] The device of the present invention can easily and reliably detect changes in the state of the raw material melt (solidification or completion of melting) with high detection accuracy. This makes it possible to prevent damage to the quartz crucible due to excessive solidification, prevent a decrease in the productivity of the device due to a delay in discovering the completion of melting, and reduce the workload of the operator.
[0020] At this time, the parallax data of the measurement image may be a parallax ratio obtained by dividing the parallax data within the inspection area by the area of the inspection area.
[0021] With this, it becomes possible to easily detect the solidification and completion of melting of the raw material melt.
[0022] The solidification timing may be detected when the parallax ratio is 10% or more, and the melting completion timing may be detected when the parallax ratio remains 3% or less for 5 minutes or more.
[0023] With these criteria, the timing of completion of solidification or melting can be grasped more appropriately and stably, and erroneous detection can be prevented more reliably.
[0024] The apparatus further includes a control unit for controlling the power of the heater, the position of the quartz crucible, and the position of the heater, The control unit can automatically control the power of the heater, the position of the quartz crucible, and the position of the heater so that they meet the conditions for the next process based on detection of the solidification timing by the solidification detection processing unit or the melting completion timing by the melting completion detection processing unit.
[0025] Such a device can be operated simply and efficiently to pull single crystals with high productivity. Effect of the Invention
[0026] As described above, the method for detecting the surface state of the raw material melt, the method for producing a single crystal, and the CZ single crystal production apparatus of the present invention can easily and reliably grasp the state change of the raw material melt (solidification or completion of melting) with high detection accuracy. This makes it possible to prevent damage to the quartz crucible caused by excessive solidification and a decrease in productivity of the pulled single crystal caused by a delay in discovering the completion of melting, and also reduces the workload of the operator. [Brief description of the drawings]
[0027] [Figure 1] FIG. 1 is a schematic diagram showing an example of a CZ single crystal manufacturing apparatus according to the present invention. [Diagram 2] FIG. 2 is an image diagram showing an example of an image captured by one of the CCD cameras. [Diagram 3] 4 is a graph showing a change in parallax ratio when solidification is formed after pulling up a single crystal in Example 1. [Figure 4] 11 is a graph showing a change in parallax ratio when monitoring the completion of melting after the raw material is charged in Example 2. [Diagram 5] 13 is a graph showing a change in output (diameter data) of a diameter detection visual sensor when solidification is formed after pulling up a single crystal in a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] As described above, there has been a demand for a method capable of detecting the solidification and completion of melting of the raw material melt when pulling a single crystal by the CZ method (particularly when recharging is performed). The inventors conducted extensive research and found that, in detecting solidification, when observing the melt in its molten state, there are no distinctive edges, so the appearance of the two CCD cameras on the left and right is the same, and the parallax is almost zero. However, when solidification is formed, linear patterns with contrast in various directions appear on the solidified surface, resulting in a large amount of parallax. This is because the angles of the two CCD cameras are different, and when solidification occurs, the detection positions are photographed differently, which results in the parallax of the two CCD cameras. The same idea is also applied to detecting the completion of melting; when the raw material is completely melted and gone, the distinctive patterns disappear, and the parallax obtained decreases. The present inventors focused on the increase or decrease in the amount of data relating to this parallax (for example, the number of pixels where parallax occurs) and considered that this could be applied to detection of the completion of solidification or melting, leading to the completion of the present invention.
[0029] Hereinafter, the present invention will be described with reference to the drawings. However, the present invention is not limited to the embodiments. FIG. 1 shows an outline of an example of a CZ single crystal manufacturing apparatus according to the present invention. This apparatus 20 has a main chamber 1 and a pull chamber 2, and a carbon purge tube 3 is disposed from the bottom of the pull chamber 2 to the top of the main chamber 1. In the main chamber 1, a quartz crucible 6 containing raw material 4 (including solidified raw material melt) and raw material melt 5 and a graphite crucible 7 disposed outside the quartz crucible 6 are supported by a support shaft 8 so as to be movable up and down. A cylindrical heater 9 made of, for example, a carbon material for melting the raw material 4 is disposed around the quartz crucible 6 and the graphite crucible 7, and a heat insulating member 10 is disposed around the heater 9. The heater 9 can be driven by means not shown, and its position can be adjusted.
[0030] A monitoring window 12 is provided at the top of the main chamber 1, and two CCD cameras (also simply called cameras) 11 are provided outside the monitoring window 12 to capture images of the surface condition of the raw material melt 5 in the quartz crucible 6 through the monitoring window 12. These two CCD cameras 11 are capable of simultaneously capturing images of any identical inspection area on the surface of the raw material melt 5 from different directions. Furthermore, it is provided with an image processing section 13, a solidification detection processing section 14, a melting completion detection processing section 15, and a control section 16, which can be implemented as, for example, a computer (program, etc.). This computer is connected to the CCD camera 11, the heater 9 (and its driving means), and the support shaft 8, and can automatically process images from the CCD camera 11, and issue commands for adjusting the power and position of the heater 9 and adjusting the vertical movement of the support shaft 8 (adjusting the positions of the quartz crucible 6 and the graphite crucible 7).
[0031] Each part will be described in more detail below. The two cameras 11 are not particularly limited as long as they can simultaneously obtain measurement images of the inspection area, and a dedicated camera for checking the surface state of the raw material melt can be provided, or a CCD camera for detecting the raw material position or diameter, as has been conventionally used, can be used. The type and arrangement of the cameras can be appropriately set so that a wider camera field of view can be obtained for the surface of the raw material melt in the quartz crucible 6.
[0032] Here, the image captured by the camera 11 will be described. FIG. 2 shows an example of an image (captured image) captured by one of the cameras. The outer frame indicates the range of the camera's field of view (captured image). Also captured is the purge tube 3, which has an opening, and what is captured through the opening is the surface of the raw material melt 5 (raw material melt surface monitoring area). An inspection area is arbitrarily set (here, the area surrounded by a dotted line), and it can be seen that part of the surface of the raw material melt 5 is captured within the inspection area. The other camera, positioned at a different angle, also simultaneously captures the same inspection area. In the present invention, the image of this part of the inspection area is called a measurement image.
[0033] The image processing unit 13 acquires parallax data of the measurement images of the inspection area obtained by photographing with the two cameras 11. First, let us explain parallax. Generally, by performing stereo matching on images captured by two CCD cameras, the difference in position (parallax) between corresponding locations in two images can be obtained. Parallax is used to measure distance based on the principle of triangulation, but this invention focuses on the quantity of parallax data. Here, the "parallax data of the measurement image" in the present invention will be described. As the "parallax data of the measurement image", for example, a parallax ratio, which is a value obtained by dividing the "parallax data in the inspection area" by the "area in the inspection area", can be used. As described above, the inspection area is set within a range where the raw material melt 5 in the quartz crucible 6 can be monitored through the monitoring window 12, and for example, the number of pixels of the parallax in the inspection area divided by the number of pixels for the area can be used as the parallax ratio to detect the completion of solidification and melting.
[0034] A more detailed explanation will be given below. As described above, when the surface of the raw material melt is not solidified, there is no characteristic edge, and the appearance from the two cameras on the left and right appears the same at first glance, and the parallax is almost zero (normally, parallax occurs since the two cameras are photographed separately, but there is no difference between the two measurement images for the inspection area in the melt state). However, when solidification is formed, a contrasting linear pattern appears on the formed solidified surface, so that the parallax can be clearly obtained. That is, in the photographed inspection area, the difference (parallax) in the position of the corresponding place (the linear pattern, etc.) between the two measurement images taken by the two cameras can be clearly obtained. The total number of points (e.g., pixels) occupied by such places seen at different positions in the inspection area (all of those places if there are multiple places) can be regarded as "parallax data in the inspection area". And, the "area in the inspection area" can be regarded as the number of points (pixels) occupied by the inspection area, and the value of the "parallax data in the inspection area" divided by the value of the "area in the inspection area" as described above is the parallax rate (one example of "parallax data of the measurement image"). If such data is utilized, the measurement principle is simple and the data can be easily obtained from a measurement image, and therefore the solidification or completion of melting of the raw material melt can be easily detected. The criteria for determining disparity (criteria for determining whether pixels in two measurement images are the same or different) are not particularly limited and can be set appropriately.
[0035] The solidification detection processing unit 14 automatically detects the solidification timing when the raw material changes from a completely melted state to a solidification formed on the surface of the raw material melt 5, based on the parallax data (parallax ratio) of the measurement image obtained by the image processing unit. The detection of the solidification timing can be set, for example, when the parallax ratio becomes 10% or more. In this way, solidification can be stably detected.
[0036] On the other hand, the melting completion detection processing unit 15 automatically detects the melting completion timing when the state where the surface of the raw material melt 5 is solidified changes to a completely melted state from the parallax data (parallax rate) of the measurement image. The melting completion timing can be detected, for example, when the parallax rate remains at 3% or less for 5 minutes or more. Since small unmelted raw material may float in the raw material melt, if there is no parallax for about 5 minutes, it can be sufficiently determined that melting is complete.
[0037] By using such criteria (thresholds), the timing of solidification or complete melting can be more appropriately grasped, and erroneous detection can be more reliably prevented. However, the criteria are not limited to these and can be determined as appropriate. The solidification detection processing unit 14 and the melting completion detection processing unit 15 may be provided as at least one of them, or both. It is preferable to provide both, since it is possible to appropriately detect both the solidification timing and the melting completion timing.
[0038] The control unit 16 automatically controls the power of the heater 9, the position of the quartz crucible 6, and the position of the heater 9 to be the conditions for the next process based on the detection of the solidification timing by the solidification detection processing unit 14 or the melting completion timing by the melting completion detection processing unit 15. In particular, in an apparatus used for producing a plurality of single crystals by recharging, there are conditions such as the power and position of the heater 9 and the position of the quartz crucible 6 suitable for each case of solidifying the surface of the raw material melt when recharging the raw material after pulling the single crystal, completely melting the recharged or solidified raw material, and pulling the next single crystal after complete melting. In the case of detecting the solidification timing by the solidification detection processing unit 14, various adjustments of the heater 9 and the quartz crucible 6 can be controlled by the control unit 16 so as to be in accordance with the set conditions suitable for the next process of recharging the raw material and completely melting the raw material, and in the case of detecting the melting completion timing by the melting completion detection processing unit 15, so as to be in accordance with the set conditions suitable for the next process of pulling the single crystal. Automatic control is more preferable.
[0039] The CZ single crystal manufacturing apparatus 20 of the present invention as described above can easily detect the solidification of the raw material melt, the completion of melting, or both with high detection accuracy. Therefore, particularly in the production of multiple single crystals by raw material recharge, it is possible to simply and reliably prevent the raw material melt from being solidified more than necessary or the completion of melting from being not noticed, which can damage the quartz crucible and reduce the productivity of single crystal production. Moreover, since the detection can be performed automatically, visual observation by an operator, which was previously performed, can be omitted or reduced.
[0040] Next, a method for detecting the surface condition of the raw material melt and a method for manufacturing a single crystal according to the present invention using the CZ single crystal manufacturing apparatus 20 shown in Fig. 1 will be described. A process for manufacturing a plurality of single crystals by recharging the raw material while detecting the surface condition of the raw material melt will be described. When pulling a single crystal using the CZ single crystal manufacturing apparatus 20, an inert gas such as Ar is supplied from above the pull chamber 2 and exhausted from below the main chamber 1, so that both chambers 1 and 2 are filled with the inert gas under reduced pressure. In addition, the quartz crucible 6 contains a raw material such as polycrystalline silicon, which is heated and melted by a heater 9 to become raw material melt 5. After that, a wire is gradually lowered from above the pull chamber 2, and a seed crystal attached to the lower end of the wire is immersed in (comes into contact with) the raw material melt 5 in the quartz crucible 6.
[0041] The quartz crucible 6 is rotated at a predetermined speed via a support shaft 8 by a motor or the like, while the wire is slowly wound upward while rotating around its axis in the opposite direction to the quartz crucible 6. As a result, a single crystal is pulled up while growing, following the seed crystal, and a necked section, a cone section, a straight body section, and finally a tail section are formed before being pulled up into the pull chamber 2.
[0042] After the single crystal is pulled as described above, before the next step of recharging, the heater 9 and the quartz crucible 6 are controlled to the heater power, crucible position, and heater position for solidification. After the control is performed as specified, monitoring of solidification is started. That is, the parallax rate is automatically obtained one after another from the measured image of the inspection area by the two cameras 11, the image processing unit 13, and the solidification detection processing unit 14. When a specified standard is reached (for example, when the parallax rate is 10% or more), the solidification timing is automatically detected. When such a solidification timing is detected, the control unit 16 automatically controls the heater power, etc., for melting, and additional raw material is added by recharging.
[0043] After the input of the raw material is completed, the raw material is melted while monitoring the completion of melting. That is, the parallax rate is automatically obtained again from the measured image of the inspection area by the two cameras 11, the image processing unit 13, and the solidification detection processing unit 14. Then, when a predetermined standard is reached (for example, when the parallax rate remains at 3% or less for 5 minutes or more), the melting completion timing is automatically detected. When such a melting completion timing is detected, the control unit 16 automatically controls the heater power, etc. to the desired level for pulling the single crystal, and the next single crystal is pulled. This series of tasks is carried out automatically.
[0044] Such a detection method and manufacturing method makes it possible to easily and accurately grasp the solidification and completion of melting of the raw material melt, while manufacturing single crystals one after another with high productivity, and also reduces the burden on the operator. EXAMPLES
[0045] The present invention will be described in more detail below with reference to examples and comparative examples of the present invention, but the present invention is not limited to these. Example 1 Using the CZ single crystal manufacturing apparatus 20 of the present invention shown in FIG. 1, the detection method of the present invention was carried out for the solidification timing in the solidification formation process of the raw material melt after the single crystal was pulled up and before the raw material was recharged. The experiment was carried out under the manufacturing conditions of crucible aperture: 800 mm, raw material melt weight: 400 kg, with two CCD cameras attached outside the monitoring window of the main chamber as shown in Figure 1. The image of monitoring the raw material melt surface is the same as in Figure 2. In order to be able to confirm the raw material melt surface of the same inspection area from the opening in the purge tube, the field of view of the CCD camera was set to approximately 500 mm in the X direction and approximately 375 mm in the Y direction, and the inspection area for solidification and completion of melting was set to approximately 300 mm in the X direction and 100 mm in the Y direction (450 × 150 pixels, area 67,500 pixels) in both cases.
[0046] Figure 3 shows the change in the parallax rate when solidification occurs after pulling a single crystal. The horizontal axis represents the elapsed time from an arbitrary point in the process, and the vertical axis represents the parallax rate within the inspection area for monitoring solidification. In the molten state, there is almost no information in the form of positional differences between corresponding locations between the two measurement images, so the parallax rate is stable at around 0. However, the moment solidification spreads over the surface of the raw material melt, linear patterns with contrast in various directions appear, causing the parallax rate to increase sharply. When the threshold for detecting the solidification timing was set to 10% or more, the solidification timing was detected in 212 minutes. For verification purposes, an operator simultaneously visually monitored the situation and determined that the solidification occurred at approximately the same time as described above (the "solidification point" in Figure 3, 211 min).
[0047] Example 2 After Example 1 was completed, raw material was added, and the detection method of the present invention was carried out on the melting completion timing during the process of melting the raw material.
[0048] FIG. 4 shows the change in the parallax ratio when monitoring the completion of melting after the raw material is added. The horizontal axis represents the elapsed time from an arbitrary point in the process, and the vertical axis represents the parallax ratio within the inspection area for monitoring the completion of melting. The reason why the parallax ratio does not decrease suddenly like during solidification in Example 1 is because small lumps of unmelted raw material become free in the quartz crucible in the latter half of melting. However, once the material is completely molten, the parallax ratio stabilizes at approximately 0. The threshold for detecting the completion of melting was set to 3% or less for approximately 5 minutes, and the timing of the completion of melting was detected at 406 minutes ("Point at which completion of melting was detected" in FIG. 4). For verification purposes, an operator simultaneously visually monitored the melting and determined that the melting was completed at approximately the same time as above (405 min).
[0049] (Comparative Example) When the solidification detection in Example 1 was performed, the solidification detection was also performed using a conventional visual sensor for diameter detection. At this time, the field of view of the camera was approximately 220 mm in the X direction and approximately 165 mm in the Y direction, and the solidification detection area was approximately 80 mm in the X direction and approximately 80 mm in the Y direction (582 × 582 pixels). The scanning direction for detecting the edge to detect solidification was from the quartz crucible wall toward the center, and solidification was detected as complete when the diameter data, which is the output signal of the diameter detection visual sensor, reached 150 mm or more.
[0050] The change in output in this case is shown in Figure 5. The horizontal axis represents the elapsed time from an arbitrary point in the process, and the vertical axis represents the output (diameter data) of the visual sensor for diameter detection. Even when solidification actually occurred, no change in the output data was observed, and solidification could not be detected. Since priority is given to the imaging conditions and binarization process so that the meniscus part with the highest brightness in the melt can be stably detected for diameter control, it is not expected that the difference in contrast between the melt and solidified part during solidification monitoring will result in a change in output value that can be used to detect solidification. It may be possible to detect this by changing the imaging conditions or the threshold value for the binarization process depending on the process, but this becomes complicated. In contrast, in the present invention, as in the first embodiment, detection can be performed simply and with high accuracy.
[0051] The present invention is not limited to the above-described embodiment. The above-described embodiment is merely an example, and any configuration that is substantially the same as the technical idea described in the claims of the present invention and that provides similar effects is included in the technical scope of the present invention. [Explanation of symbols]
[0052] 1...Main chamber, 2...Pull chamber, 3...Purge tube, 4...raw material, 5...raw material melt, 6...quartz crucible, 7...graphite crucible, 8...Support shaft, 9...Heater, 10...Heat insulating member, 11...CCD camera (2 units), 12: monitoring window; 13: image processing section; 14: solidification detection processing section; 15...melting completion detection processing section, 16...control section, 20...CZ single crystal manufacturing apparatus.
Claims
1. A method for producing a single crystal by a CZ method, in which a single crystal is pulled from a raw material melt obtained by melting a raw material contained in a quartz crucible with a heater, comprising the steps of: An arbitrary identical inspection area on the surface of the raw material melt in the quartz crucible is photographed simultaneously from different directions using two CCD cameras to obtain a measurement image of the inspection area; When using parallax data of the measurement images of the two CCD cameras, one or more of a solidification timing when the raw material melt changes from a completely molten state to a state where a solid is formed on the surface of the raw material melt, and a melting completion timing when the raw material melt changes from a state where a solid is formed on the surface of the raw material melt to a completely molten state are automatically detected, A method for detecting the state of the surface of a raw material melt, characterized in that a parallax rate obtained by dividing the number of pixels in the inspection area where parallax occurs by the number of pixels in the area of the inspection area is used as the parallax data of the measurement image.
2. 2. The method for detecting the state of the surface of a raw material melt according to claim 1, wherein the solidification timing is detected when the parallax rate becomes 10% or more.
3. 3. The method for detecting the surface state of a raw material melt according to claim 1, wherein the melting completion timing is detected when the parallax rate remains at or below 3% for 5 minutes or more.
4. After pulling the single crystal, before recharging the raw material, the solidification timing is detected; 4. A method for detecting the surface state of a raw material melt as described in any one of claims 1 to 3, characterized in that the melting completion timing is detected while the recharged raw material is melting and before the next single crystal is pulled up.
5. A method for producing a single crystal by the CZ method, which comprises pulling a single crystal from a molten material obtained by melting a raw material contained in a quartz crucible by a heater, After pulling the single crystal, the raw material is recharged and melted, and then the next single crystal is pulled.
5. A method for producing a single crystal, comprising the steps of: automatically detecting the solidification timing or the melting completion timing by the method for detecting the surface state of the raw material melt according to any one of claims 1 to 4; and automatically controlling the power of the heater, the position of the quartz crucible, and the position of the heater to be conditions for a next process.
6. A CZ single crystal manufacturing apparatus comprising a quartz crucible for accommodating a raw material, and a heater for melting the raw material in the quartz crucible to form a raw material melt, and pulling a single crystal from the raw material melt, Two CCD cameras for simultaneously photographing an arbitrary identical inspection area on the surface of the raw material melt in the quartz crucible from different directions; an image processing unit that obtains parallax data of the measurement image from the measurement image of the inspection area obtained by photographing the two CCD cameras; The apparatus further includes at least one of a solidification detection processing unit and a melting completion detection processing unit, the solidification detection processing unit automatically detects, from parallax data of the measurement image, a solidification timing at which the raw material changes from a completely molten state to a state in which a solid is formed on a surface of the raw material melt, the melting completion detection processing unit automatically detects, from parallax data of the measurement image, a melting completion timing at which the raw material melt has changed from a state in which a solid has been formed on a surface thereof to a completely melted state, A CZ single crystal manufacturing apparatus, characterized in that the parallax data of the measurement image is a parallax rate obtained by dividing the number of pixels in the inspection area where parallax occurs by the number of pixels in the area of the inspection area.
7. 7. The CZ single crystal manufacturing apparatus according to claim 6, wherein the solidification timing is detected when the parallax rate becomes 10% or more.
8. 8. The CZ single crystal manufacturing apparatus according to claim 6, wherein the melting completion timing is detected when the parallax ratio remains at or below 3% for 5 minutes or more.
9. Further comprising a control unit for controlling the power of the heater, the position of the quartz crucible, and the position of the heater; The CZ single crystal manufacturing apparatus according to any one of claims 6 to 8, characterized in that the control unit automatically controls the power of the heater, the position of the quartz crucible, and the position of the heater to meet the conditions for the next process based on the detection of the solidification timing by the solidification detection processing unit or the melting completion timing by the melting completion detection processing unit.
Citation Information
Patent Citations
Governor free control device for combined plant
JP1988090606A
Melting detection method and detector for use in semiconductor single crystal pulling device
JP2000264780A
Method for manufacturing single crystal
JP2017077981A
Method for supplying raw material and method for manufacturing silicon single crystal