Method for producing optical laminate with pressure-sensitive adhesive layer
By alternately stacking optical laminates with intervening films and using a twisted blade end mill followed by a twisted file, the method addresses release liner lifting in optical laminate cutting, achieving high-quality and defect-free optical laminates.
Patent Information
- Application Number
- JP2023060508
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-04-04
- Publication Date
- 2024-10-24
- Estimated Expiration
- 2041-09-21
AI Technical Summary
The issue of release liner lifting during end face cutting of optical laminates with adhesive layers is not effectively addressed in existing manufacturing methods, leading to defects and inefficiencies.
A method involving the alternately stacking of optical laminates with adhesive layers and intervening films, using an end mill with twisted blades for cutting, and subsequent finishing with a twisted file to suppress release liner lifting.
This approach effectively suppresses release liner lifting and adhesive layer defects, ensuring high-quality optical laminates with improved yield and dimensional accuracy.
Smart Images

Figure 0007573061000002 
Figure 0007573061000003 
Figure 0007573061000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a pressure-sensitive adhesive layer-attached optical laminate. [Background technology]
[0002] In image display devices such as mobile phones and notebook personal computers, various optical laminates (e.g., polarizing plates) are used to realize image display and / or improve the performance of the image display. Typically, the optical laminate has an adhesive layer for bonding a front plate (e.g., a cover glass) as one outermost layer, and another adhesive layer for bonding the optical laminate to an image display panel as the other outermost layer. In practice, release liners are temporarily attached to these adhesive layers in a peelable manner to protect these adhesive layers until they are actually used. In recent years, it has been desired to process the shape of the optical laminate into a desired shape. Examples of such processing methods include end face cutting using an end mill. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2001-54845 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the cutting process of the end face of the pressure-sensitive adhesive layer-attached optical laminate, lifting of the temporarily attached release liner may occur. The present invention has been made to solve such problems, and a main object of the present invention is to provide a simple method for producing a pressure-sensitive adhesive layer-attached optical laminate in which lifting of the release liner is suppressed. [Means for solving the problem]
[0005] A method for manufacturing an optical laminate with an adhesive layer according to an embodiment of the present invention includes forming a workpiece by alternating stacking a plurality of optical laminates with an adhesive layer and a plurality of intervening films, and cutting the outer peripheral surface of the workpiece, wherein cutting the workpiece includes cutting with an end mill, and cutting with the end mill includes cutting with a twist file. In one embodiment, the thickness of the intervening film is 75 μm to 1000 μm. In one embodiment, the intervening film is made of a polyester resin. In one embodiment, the pressure-sensitive adhesive layer-attached optical laminate includes an optical film, a first pressure-sensitive adhesive layer having a thickness of 50 μm or more and arranged on one side of the optical film, a first release liner releasably attached temporarily to the first pressure-sensitive adhesive layer, a second pressure-sensitive adhesive layer arranged on the other side of the optical film, and a second release liner releasably attached temporarily to the second pressure-sensitive adhesive layer, the release strength of the first release liner being greater than the release strength of the second release liner. In one embodiment, the optical film includes, in order from the first pressure-sensitive adhesive layer side, a polarizer and a retardation layer. In one embodiment, the end mill has a twisted blade and a pocket area per blade of 5 mm 2 That's all. In one embodiment, the end mill has an outer diameter of 10 mm to 20 mm. In one embodiment, the cutting with the end mill includes rough cutting with an end mill having a helical blade and finish cutting with a helical file. Effect of the Invention
[0006] According to an embodiment of the present invention, a workpiece is formed by alternately stacking multiple optical laminates with adhesive layers and multiple intervening films, and the outer peripheral surface of the workpiece is cut, thereby realizing a simple method for manufacturing an optical laminate with adhesive layers in which lifting of the release liner is suppressed. [Brief description of the drawings]
[0007] [Figure 1] 4 is a schematic front view of a main portion illustrating a method of forming a workpiece in a manufacturing method according to an embodiment of the present invention. FIG. [Diagram 2] FIG. 1 is a schematic cross-sectional view illustrating an example of a pressure-sensitive adhesive layer-attached optical laminate that can be used in a production method according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a schematic perspective view illustrating an outline of a cutting process in a manufacturing method according to an embodiment of the present invention. [Figure 4] 1 is a schematic perspective view for explaining the structure of an end mill having a twisted blade that can be used for cutting in a manufacturing method according to an embodiment of the present invention. FIG. [Diagram 5] 1 is a schematic plan view seen from the rotation axis direction to explain the pocket area of an end mill having a twisted blade that can be used for cutting in a manufacturing method according to an embodiment of the present invention. FIG. [Figure 6] 1 is a schematic perspective view for explaining the structure of a twisted file that can be used for end face processing in a manufacturing method according to an embodiment of the present invention. FIG. [Figure 7] 1 is a schematic diagram illustrating a twist file having no clearance angle in one aspect of a manufacturing method according to an embodiment of the present invention. FIG. [Figure 8] FIG. 7 is a schematic cross-sectional view of a main portion for explaining the depth and pitch of projections and recesses of the file portion in the twist file of FIG. 6.
[0008] Hereinafter, specific embodiments of the present invention will be described with reference to the drawings, but the present invention is not limited to these embodiments. Note that the drawings are schematic for ease of viewing, and the ratios of length, width, thickness, and the like, as well as angles, etc. in the drawings are different from the actual ones.
[0009] A method for producing an optical laminate with a pressure-sensitive adhesive layer according to an embodiment of the present invention includes alternately stacking a plurality of optical laminates with a pressure-sensitive adhesive layer and a plurality of intervening films to form a workpiece, and cutting the outer peripheral surface of the workpiece. In an embodiment of the present invention, an optical laminate with a pressure-sensitive adhesive layer in which lifting of the release liner is suppressed (as a result, defects in the pressure-sensitive adhesive layer are suppressed) can be easily realized by alternately stacking a plurality of optical laminates with a pressure-sensitive adhesive layer and a plurality of intervening films to form a workpiece. The optical laminate with a pressure-sensitive adhesive layer typically includes an optical film, a first pressure-sensitive adhesive layer having a thickness of 50 μm or more and arranged on one side of the optical film, a first release liner releasably temporarily attached to the first pressure-sensitive adhesive layer, a second pressure-sensitive adhesive layer arranged on the other side of the optical film, and a second release liner releasably temporarily attached to the second pressure-sensitive adhesive layer. In one embodiment, the release force of the first release liner is greater than the release force of the second release liner. Each step of the manufacturing method will be described below in order.
[0010] A. Formation of the Work A-1. Overview First, a workpiece is formed. In an embodiment of the present invention, as shown in FIG. 1, a workpiece W is formed by alternately stacking a plurality of pressure-sensitive adhesive layer-attached optical laminates 100, 100, ... and a plurality of intervening films 120, 120, .... By alternately stacking the pressure-sensitive adhesive layer-attached optical laminates and the intervening films, lifting of the release liner can be significantly suppressed. In particular, lifting of the second release liner having a small peel strength (weak adhesive strength) can be effectively suppressed. The pressure-sensitive adhesive layer-attached optical laminates 100 may be stacked so that the first release liner 30 is on the upper side, or the second release liner 50 is on the upper side. Preferably, the pressure-sensitive adhesive layer-attached optical laminates 100 are stacked so that the first release liner 30 is on the upper side. With such a configuration, lifting of the second release liner can be even more effectively suppressed. The total thickness of the workpiece is, for example, 5 mm to 50 mm. The pressure-sensitive adhesive layer-attached optical laminate and the intervening film are stacked so that the workpiece has such a total thickness. The number of pressure-sensitive adhesive layer-attached optical laminates included in the workpiece can vary depending on the thickness of the pressure-sensitive adhesive layer-attached optical laminate. The number of pressure-sensitive adhesive layer-attached optical laminates is, for example, 5 to 100. The intervening film 120 is typically stacked so as to be the upper and lower outermost layers of the workpiece as shown in FIG. 1. That is, in the workpiece, the number of intervening films 120 is one more than the number of pressure-sensitive adhesive layer-attached optical laminates 100. With this configuration, the formation of a pressing mark on the pressure-sensitive adhesive layer-attached optical laminate by clamping during cutting can be suppressed. In the embodiment of the present invention, since the workpiece includes the intervening film, the number of pressure-sensitive adhesive layer-attached optical laminates obtained from the same thickness of the workpiece is smaller than that of a normal manufacturing method, while the lifting of the release liner is significantly suppressed, and as a result, defects in the pressure-sensitive adhesive layer are significantly suppressed. That is, the embodiment of the present invention is based on a technical idea opposite to that of a normal manufacturing method, which is premised on increasing the yield.
[0011] A-2. Optical laminate with pressure-sensitive adhesive layer FIG. 2 is a schematic cross-sectional view for explaining an example of an optical laminate with a pressure-sensitive adhesive layer. The pressure-sensitive adhesive layer-attached optical laminate 100 of the illustrated example includes an optical film 10, a first pressure-sensitive adhesive layer 20 arranged on one side of the optical film 10, a first release liner 30 releasably attached temporarily to the first pressure-sensitive adhesive layer 20, a second pressure-sensitive adhesive layer 40 arranged on the other side of the optical film 10, and a second release liner 50 releasably attached temporarily to the second pressure-sensitive adhesive layer. When the pressure-sensitive adhesive layer-attached optical laminate is applied to an image display device, typically, the second release liner 50 (effectively, the second pressure-sensitive adhesive layer 40) is arranged on the image display panel side. When the pressure-sensitive adhesive layer-attached optical laminate is actually used, the first release liner 30 and the second release liner 50 are peeled off and removed. Typically, the first adhesive layer 20 can be used to bond a front plate (e.g., a cover glass); the second adhesive layer 40 can be used to bond the adhesive layer-attached optical laminate to an image display device (essentially, an image display panel).
[0012] The optical film 10 may be any suitable optical film that can be used in applications requiring cutting. The optical film may be a film composed of a single layer, or may be a laminate. Specific examples of optical films composed of a single layer include a polarizer and a retardation film. Specific examples of optical films composed as a laminate include a polarizing plate (typically a laminate of a polarizer and a protective film), a conductive film for a touch panel, a surface-treated film, and a laminate in which the optical film composed of these single layers and / or the optical film composed as a laminate are appropriately laminated according to the purpose (for example, an anti-reflection circular polarizing plate, a polarizing plate with a conductive layer for a touch panel). In the illustrated example, the optical film 10 includes a polarizer 11 and a retardation layer 12 in this order from the first pressure-sensitive adhesive layer 20 side. Therefore, the optical film 10 in the illustrated example may be an anti-reflection circular polarizing plate.
[0013] The first pressure-sensitive adhesive layer 20 preferably has a storage modulus G′ at 25° C. of 1.0×10 5 (Pa) ~ 2.5 × 10 5(Pa), and more preferably 1.1×10 5 (Pa) ~ 2.3 × 10 5 (Pa), and more preferably 1.2×10 5 (Pa) ~ 2.0 × 10 5 (Pa). The storage modulus can be determined, for example, by dynamic viscoelasticity measurement. The first adhesive layer 20 may have any suitable configuration as long as it has adhesiveness and transparency that can be used for optical applications and has the desired storage modulus. Specific examples of adhesives constituting the first adhesive layer include acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives. An adhesive having the desired storage modulus can be prepared by adjusting the type, number, combination, and compounding ratio of monomers forming the base resin of the adhesive, as well as the compounding amount of the crosslinking agent, reaction temperature, reaction time, and the like. The base resin of the adhesive may be used alone or in combination of two or more types. From the viewpoints of transparency, processability, durability, and the like, an acrylic adhesive is preferred. Details of the adhesive constituting the adhesive layer are described, for example, in JP 2014-115468 A, and the description of the publication is incorporated herein by reference.
[0014] The thickness of the first pressure-sensitive adhesive layer 20 is 50 μm or more, as described above, preferably 70 μm to 1000 μm, more preferably 100 μm to 700 μm, and even more preferably 200 μm to 600 μm.
[0015] A commonly known and commonly used configuration in the industry can be adopted for the second pressure-sensitive adhesive layer 40. The thickness of the second pressure-sensitive adhesive layer 40 can be, for example, 10 μm to 50 μm, or, for example, 10 μm to 30 μm.
[0016] Any appropriate release liner may be used for each of the first release liner 30 and the second release liner 50. Specific examples include plastic films, nonwoven fabrics, or papers whose surfaces are coated with a release agent. Specific examples of the release material include silicone-based release agents, fluorine-based release agents, and long-chain alkyl acrylate-based release agents. Specific examples of the plastic film include polyethylene terephthalate (PET) films, polyethylene films, and polypropylene films. The thickness of the release liner may be, for example, 10 μm to 100 μm.
[0017] In one embodiment, the release strength of the first release liner 30 is greater than the release strength of the second release liner 50. With such a configuration, the effect of the embodiment of the present invention (i.e., suppression of lifting of the release liner) becomes significant. The release strength of the first release liner 30 is preferably 0.05 N / 10 mm to 0.5 N / 10 mm; the release strength of the second release liner 50 is preferably 0.01 N / 10 mm to 0.02 N / 10 mm; the difference in release strength ("first release liner" - "second release liner") is preferably 0.03 N / 10 mm to 0.45 N / 10 mm.
[0018] A-3.Interposition film The thickness of the intervening film 120 is preferably 75 μm to 1000 μm, more preferably 150 μm to 750 μm, further preferably 200 μm to 600 μm, and particularly preferably 300 μm to 500 μm. If the intervening film is too thin, the effect of suppressing lifting may be insufficient, and alternate lamination with the pressure-sensitive adhesive layer-attached optical laminate may be difficult. If the intervening film is too thick, productivity may be insufficient.
[0019] The intervening film 120 may be any appropriate resin film as long as the effects of the embodiment of the present invention can be obtained. The intervening film is typically made of a polyester resin, preferably polyethylene terephthalate. With such a configuration, melting of the intervening film during cutting processing is suppressed, so that contamination of the pressure-sensitive adhesive layer-attached optical laminate by molten resin can be suppressed. The intervening film may be made of a (meth)acrylic resin, a polyimide resin, a polyamide resin (e.g., nylon), or the like.
[0020] The elastic modulus of the intervening film is, for example, 2.2 kN / mm 2 ~4.8kN / mm 2 The elastic modulus is measured in accordance with JIS K 6781.
[0021] B. Cutting the outer surface of the workpiece B-1.Overview Next, the outer peripheral surface of the work W is cut. FIG. 3 is a schematic perspective view for explaining the outline of cutting of the outer peripheral surface (hereinafter, sometimes referred to as "cutting process"). As described in the above A-1 with reference to FIG. 1, a plurality of pressure-sensitive adhesive layer-attached optical laminates and a plurality of intervening films are alternately stacked to form the work W as shown in FIG. 3. In the illustrated example, the work W has outer peripheral surfaces 1a, 1b facing each other and outer peripheral surfaces 1c, 1d perpendicular to the outer peripheral surfaces 1a, 1b. The work W is preferably clamped from above and below by a clamping means (not shown). The clamping means (e.g., a jig) may be made of a soft material or a hard material. When made of a soft material, its hardness (JIS A) is preferably 60° to 80°. If the hardness is too high, a pressing mark by the clamping means may remain. If the hardness is too low, a positional deviation may occur due to deformation of the jig, and cutting accuracy may be insufficient. The pressure-sensitive adhesive layer-attached optical laminate is cut into any appropriate shape when forming the work. Specifically, the pressure-sensitive adhesive layer-attached optical laminate may be cut into a rectangular shape as shown in the illustrated example, or may be cut into a shape similar to a rectangular shape (for example, a rectangular shape having a shape that becomes a recess when viewed in a plane in the center of the long side), or may be cut into an appropriate shape depending on the purpose (for example, a circle).
[0022] B-2. End mill The cutting process may be performed by any appropriate means. Specifically, the cutting process may be a so-called full back process, or may be an end mill process as shown in FIG. 3. Hereinafter, the end mill process will be described as a representative example of the cutting process. First, an end mill that can be used in the cutting process will be described.
[0023] As the end mill, an end mill having a twisted blade can be suitably used. FIG. 4 is a schematic perspective view for explaining the structure of an end mill having a twisted blade. As shown in FIG. 4, an end mill 60 having a twisted blade has a rotation axis 61 extending in the stacking direction (vertical direction) of the workpiece W, and a cutting blade 62 configured as the outermost diameter of a main body rotating around the rotation axis 61. In the illustrated example, the cutting blade 62 is configured as the outermost diameter twisted along the rotation axis 61, and shows a right blade right twist. The cutting blade 62 includes a cutting edge 62a, a rake face 62b, and an escape face 62c. The number of blades of the cutting blade 62 can be appropriately set according to the purpose. In the illustrated example, the cutting blade is configured with three blades, but the number of blades may be one continuous blade, two blades, four blades, or five or more blades. The blade angle of the end mill (the twist angle θ of the cutting blade in the illustrated example) is preferably 20° to 70°, and more preferably 30° to 60°. The relief surface of the cutting blade is preferably roughened. Any appropriate treatment can be adopted as the roughening treatment. A representative example is blasting. By roughening the relief surface, adhesion of the adhesive to the cutting blade can be suppressed, and as a result, blocking can be suppressed. The outer diameter of the end mill is preferably 5 mm to 20 mm, and more preferably 10 mm to 20 mm. In this specification, "blocking" refers to a phenomenon in which the adhesive layer-attached optical laminates in the work are bonded to each other by the adhesive on the end surface, and the shavings of the adhesive attached to the end surface contribute to the adhesion of the adhesive layer-attached optical laminates to each other. In addition, the "outer diameter of the end mill" refers to twice the distance from the rotation axis 61 to the cutting edge 62a. The end mill may be a cantilever end mill in which one end (upper end) is held, or a double-supported end mill in which both ends (upper end and lower end) are held.
[0024] The pocket area per tooth of the end mill with a twisted blade is preferably 5 mm 2 More preferably, 10 mm 2 More preferably, it is 11 mm or more. 2 ~40mm 2The pocket ratio per blade of the end mill having a twisted blade is preferably 35% to 55%, more preferably 38% to 52%, and further preferably 42% to 50%. When the pocket area and pocket ratio per blade are within such ranges, the lifting of the release liner can be well suppressed. As shown in FIG. 5, the pocket area means the difference between the area of a virtual circle (circle indicated by a broken line in FIG. 5) having the outer diameter of the end mill as a diameter and the projected area of the end mill body (solid line portion in FIG. 5) when the end mill is viewed from the direction of the rotation axis. The pocket area per blade is obtained by dividing the pocket area by the number of blades. The pocket ratio is obtained by dividing the pocket area by the area of the virtual circle. The pocket area can be obtained by any appropriate image processing. The pocket area depends on the outer diameter and the number of blades of the end mill, but in the embodiment of the present invention, the lifting of the release liner can be well suppressed by optimizing the pocket area regardless of the outer diameter and the number of blades.
[0025] A twisted file may be used as the end mill. FIG. 6 is a schematic perspective view for explaining the structure of the twisted file. The twisted file 70 is typically configured by attaching diamond particles to an end mill having a twisted blade, as shown in FIG. 6. Specifically, the twisted file 70 has a rotation axis 71 extending in the stacking direction (vertical direction) of the workpiece W, and a cutting blade 72 configured as the outermost diameter of a body rotating around the rotation axis 71. Diamond particles are attached to the cutting blade 72, and a file portion 73 is formed. In the illustrated example, the cutting blade 72 is configured as the outermost diameter twisted along the rotation axis 71, and shows a right blade right twist. The cutting blade 72 includes a cutting edge 72a, a rake surface 72b, and an escape surface 72c. The number of blades of the cutting blade 72 can be appropriately set according to the purpose. The cutting blade in the illustrated example is configured with three blades, but the number of blades may be one continuous blade, two blades, four blades, or five or more blades. The twist angle θ is preferably 10° to 70°, more preferably 30° to 60°. The rake angle is preferably 1° to 25°, more preferably 3° to 20°, and even more preferably 3° to 10°. In one embodiment, as shown in FIG. 7, the twist file 70 (substantially the cutting blade 72) does not have a clearance angle. That is, the cutting edge 72a has a flat surface, and a state in which the cutting edge 72a and the processed (cut) surface of the workpiece are in contact with each other can be realized. With this configuration, it is possible to realize an optical laminate with a pressure-sensitive adhesive layer in which crack generation is suppressed even under harsh environments such as a heat shock test. The width B of the flat surface of the cutting edge 72a is preferably 0.1 mm or more, more preferably 0.2 mm to 1.4 mm, and even more preferably 0.4 mm to 1.0 mm. If the width is too small, the crack suppression effect may be insufficient. If the width is too large, it will essentially be equivalent to a bar file, and the effect of a twisted file may not be obtained. Note that Figure 7 is a schematic diagram for ease of viewing, and does not correspond to the twisted file in Figure 6.
[0026] The processing with the twist file may be performed as "normal processing" with the rake face 72b side on the upstream side in the rotation direction, or as "side-end processing" with the relief face 72c side (the back side of the blade) on the upstream side in the rotation direction. With "side-end processing", even if there is a clearance angle (when the width B of the flat surface of the cutting edge 72a is 0: the clearance angle can be, for example, 2 to 25°), the cutting edge 72a and the processed (cut) surface of the workpiece are in contact with each other, so that a sufficient crack suppression effect can be obtained even if there is a clearance angle. "Side-end processing" can be achieved, for example, by reversing the rotation direction of the twist file, or by making the rotation direction of the twist file the same as in normal processing and attaching it in the opposite direction to that in normal processing.
[0027] FIG. 8 is a schematic cross-sectional view of a main part for explaining the uneven shape of the file portion 73. The depth D of the unevenness of the file portion 73 is, for example, 5 μm to 120 μm. The lower limit of the depth D is preferably 8 μm or more, more preferably 15 μm or more. The upper limit of the depth D is preferably 50 μm or less, more preferably 35 μm or less. The pitch P of the unevenness of the file portion 73 is, for example, 5 μm to 250 μm. The lower limit of the pitch P is preferably 10 μm or more, more preferably 25 μm or more. The upper limit of the pitch P is preferably 100 μm or less, more preferably 60 μm or less. The diameter (outer diameter) of the twist file 70 (substantially the cutting blade 72) can be, for example, 2 mm to 12 mm. The length L of the file portion 73 can be, for example, 10 mm to 100 mm. In this specification, the "diameter of the twisted file" refers to twice the distance from the rotation axis 71 to the cutting edge 72a, as in the above-mentioned "diameter of the end mill". The arithmetic mean height (Sa) of the surface of the file portion 73 is preferably 1 μm to 15 μm, more preferably 3 μm to 10 μm. The maximum height (Sz) of the surface of the file portion 73 is preferably 10 μm to 100 μm, more preferably 25 μm to 80 μm. These surface roughnesses can be measured in accordance with the "non-contact (optical probe)" evaluation method of ISO 25178. Specifically, they can be measured with a laser microscope (manufactured by Keyence Corporation, product name "VK-X1000". The particle size of the diamond particles is, for example, 1 μm to 100 μm.
[0028] The grit of the file part of the twisted file can be, for example, #100 or more, preferably #200 or more, and more preferably #500 or more. The grit of the file part can be, for example, #3000 or less, preferably #2500 or less, and more preferably #2200 or less. The grit can be adjusted by the size of the diamond particles, etc.
[0029] B-3. Specific steps for cutting Typically, cutting is performed by rotating the cutting blade of the end mill in contact with the outer circumferential surface of the workpiece while moving the end mill and the workpiece relatively. The end mill rotates and moves relatively to perform cutting. In cutting, only the end mill may be moved, only the workpiece may be moved, or both the end mill and the workpiece may be moved.
[0030] The cutting process may be performed only once or may be performed multiple times (for example, two times, three times, four times or more). In one embodiment, the cutting process is performed only once. In this case, the cutting process is typically performed using an end mill having a twisted blade. In another embodiment, the cutting process is performed twice. In this case, the cutting process preferably includes rough cutting with an end mill having a twisted blade and finish cutting with a twisted file. By performing finish cutting with a twisted file, glue chipping (a state in which the end of the adhesive layer is chipped) can be formed. As a result, so-called glue balls can be significantly suppressed. The amount of glue chipping formed by finish cutting with a twisted file can be, for example, 10 μm to 500 μm. In this specification, the term "glue ball" refers to the adhesive constituting the adhesive layer protruding from the end face during cutting and the protruding adhesive solidifying into granular form. The amount of cutting by finish cutting is typically significantly smaller than the amount of cutting by rough cutting. With such a configuration, the dimensional accuracy of the obtained pressure-sensitive adhesive layer-attached optical laminate can be maintained, and excellent quality (e.g., suppression of lifting and interlayer peeling) can be maintained. For example, the cutting amount by rough cutting is preferably about 0.1 mm to 0.5 mm, and the cutting amount by finish cutting is preferably about 0.01 mm to 0.05 mm.
[0031] The conditions of the cutting process can be appropriately set according to the purpose and the mode of the cutting process. For example, as described above, when the cutting process includes rough cutting by an end mill having a twisted blade and finish cutting by a twisted file, the following cutting conditions can be adopted. The rotation speed of the end mill having a twisted blade in the rough cutting can vary depending on the outer diameter of the end mill. For example, when the outer diameter is 15 mm, the rotation speed is preferably 5000 rpm to 15000 rpm, more preferably 8000 rpm to 10000 rpm; for example, when the outer diameter is 6 mm, the rotation speed is preferably 1000 rpm to 40000 rpm, more preferably 15000 rpm to 25000 rpm. The peripheral speed (independent of the outer diameter) of the end mill having a twisted blade in the rough cutting is preferably 200000 mm / min to 750000 mm / min, more preferably 250000 mm / min to 500000 mm / min. The feed rate of the end mill having a twisted blade in rough cutting is preferably 500 mm / min to 2500 mm / min, more preferably 1000 mm / min to 2000 mm / min. The number of cuts at the cutting point in one rough cut may be one cut, two cuts, three cuts or more. The rotation speed of the twisted file in the finish cut may vary depending on the outer diameter of the twisted file. For example, when the outer diameter is 15 mm, the rotation speed is preferably 2000 rpm to 6000 rpm, more preferably 3000 rpm to 4000 rpm; for example, when the outer diameter is 6 mm, the rotation speed is preferably 5000 rpm to 15000 rpm, more preferably 7000 rpm to 10000 rpm. The peripheral speed of the twist file in the finish cutting (not depending on the outer diameter) is preferably 95000mm / min to 300000mm / min, more preferably 150000mm / min to 200000mm / min. The feed speed of the twist file in the finish cutting is preferably 300mm / min to 2000mm / min, more preferably 500mm / min to 1000mm / min. The number of cuts at the cutting point in one finish cutting can be one cut, two cuts, three cuts or more. EXAMPLES
[0032] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples. The methods for measuring the various properties in the examples are as follows.
[0033] (1) Thickness The thickness of 10 μm or less was measured using an interference film thickness meter (manufactured by Otsuka Electronics, product name "MCPD-3000"), and the thickness of more than 10 μm was measured using a digital micrometer (manufactured by Anritsu, product name "KC-351C"). (2) Release liner lifting A predetermined number of the optical laminates with the adhesive layer after cutting were extracted from the workpiece, and the entire periphery of each optical laminate with the adhesive layer was observed using a magnifying glass or a microscope. The maximum amount of lifting of the first release liner and the second release liner of the predetermined number of optical laminates with the adhesive layer was taken as the "lifting of the release liner" and was evaluated according to the following criteria. A (good): Less than 100 μm B: 100μm or more and less than 500μm C: 500μm or more and less than 900μm D (defective): 900μm or more
[0034] [Example 1] 1. Preparation of optical laminate with adhesive layer As the polarizer, a long polyvinyl alcohol (PVA) resin film was made to contain iodine and uniaxially stretched in the longitudinal direction (MD direction) to obtain a film (thickness 12 μm). A long optically functional film (HC-TAC film) was attached to one side of this polarizer so that the longitudinal directions of the two films were aligned. The HC-TAC film is a film in which a hard coat (HC) layer (2 μm) is formed on a triacetyl cellulose (TAC) film (25 μm), and the film was attached so that the TAC film was on the polarizer side to obtain a laminate of an HC layer / protective layer (TAC film) / polarizer. A normal acrylic adhesive (thickness 5 μm) was used for the attachment. Next, a polycarbonate resin film (refractive index characteristics: nx>ny=nz, in-plane retardation: about 140 nm) was attached as a retardation layer to the polarizer surface of the obtained laminate. The attachment was performed so that the absorption axis of the polarizer and the slow axis of the retardation layer formed an angle of 45°. For bonding, a normal acrylic adhesive (thickness: 5 μm) was used as described above. In this manner, a laminate of HC layer / protective layer (TAC film) / polarizer / retardation layer was obtained. A first adhesive layer (storage modulus: 1.2×10 5 A second adhesive layer (storage modulus: 1.25×10 11 A pressure-sensitive adhesive layer was then formed on the second adhesive layer (a thickness of 20 μm) and a second release liner was temporarily attached to the second adhesive layer. In this manner, a pressure-sensitive adhesive layer-attached optical laminate was produced.
[0035] 2.Cutting The optical laminate with the adhesive layer obtained as described above was punched out into a rectangle of 330 mm x 140 mm. At this time, the punching was performed so that the absorption axis direction of the polarizer was the short side direction. Meanwhile, a PET film with the same size as the punched optical laminate with the adhesive layer and a thickness of 350 μm was prepared and used as an intervening film. The punched optical laminate with the adhesive layer and the intervening film were alternately stacked to form a work (thickness of 5 mm or more). Here, the optical laminate with the adhesive layer and the intervening film were stacked so that the outermost layers on the top and bottom of the work were the intervening films (i.e., so that the intervening film was one more than the optical laminate with the adhesive layer). The entire outer peripheral end surface of the obtained work was cut by an end mill. The twist angle of the end mill was 50°, the rake angle was 5°, and the clearance angle was 15°. Furthermore, the outer diameter of the end mill is 8 mm, the number of teeth is 4, and the area of a virtual circle with the outer diameter as its diameter (hereinafter referred to as the "cross-sectional area" for convenience) is 50.2 mm 2 , the cross-sectional area of each blade is 12.6 mm 2 , Pocket area per blade is 6.4mm 2 The pocket rate per blade was 50.7%. The cutting conditions were an end mill rotation speed of 15,000 rpm (circumferential speed: 380,000 mm / min) and a feed rate of 1,500 mm / min. The cut optical laminate with the pressure-sensitive adhesive layer was subjected to the evaluation in (2) above. The results are shown in Table 1.
[0036] 3. Glue ball When the workpiece (effectively, an optical laminate with an adhesive layer) after cutting with an end mill was visually observed, glue balls were found. This workpiece was further subjected to cutting with a twist file. The twist file had a diameter of 6 mm, 4 blades, a twist angle of 45°, a rake angle of 5°, no clearance angle, a width of the flat surface of the cutting edge of 0.6 mm, and a grit size of the file part of #1000. The cutting conditions were a rotation speed of the twist file of 8000 rpm (circumferential speed: 150000 mm / min) and a feed rate of 900 mm / min. When the workpiece (effectively, an optical laminate with an adhesive layer) after cutting with a twist file was visually observed, the glue balls had been removed to an unrecognizable extent.
[0037] [Examples 2 to 8] A workpiece (substantially an optical laminate with a pressure-sensitive adhesive layer) was cut using an end mill in the same manner as in Example 1, except that the outer diameter and number of teeth of the end mill (resulting in the cross-sectional area, pocket area, and pocket ratio) were changed as shown in Table 1. The results are shown in Table 1.
[0038] For each of Examples 2 to 8, the workpiece (actually, the optical laminate with the pressure-sensitive adhesive layer) after cutting with an end mill was visually observed to have glue beads. Each workpiece was further subjected to cutting with a twisted file. As a result, the glue beads could be removed to an extent that they could not be visually recognized.
[0039] [Comparative Example 1] A workpiece was formed in the same manner as in Example 1, except that no intervening film was used, i.e., only the optical laminate with the adhesive layer was laminated. This workpiece was cut using an end mill in the same manner as in Example 2. The results are shown in Table 1. As shown in Table 1, the lifting was poor in this comparative example, so cutting using a twisted file (evaluation of glue balls) was not performed.
[0040] [Table 1]
[0041] As is clear from Table 1, according to the examples of the present invention, the lifting of the release liner can be suppressed by cutting the workpiece formed by alternately stacking the pressure-sensitive adhesive layer-attached optical laminate and the interposing film with an end mill. Furthermore, by setting the pocket area of the end mill to a predetermined value or more, the lifting of the release liner can be significantly suppressed. [Industrial Applicability]
[0042] The pressure-sensitive adhesive layer-attached optical laminate obtained by the production method according to the embodiment of the present invention can be suitably used in image display devices. [Explanation of symbols]
[0043] W work 10 Optical Film 11 Polarizer 12 Retardation layer 20 First adhesive layer 30 First release liner 40 Second adhesive layer 50 Second release liner 60 End Mill 70 Twist File 100 Optical laminate with pressure-sensitive adhesive layer 120 Intervening Film
Claims
1. The method includes alternately stacking a plurality of pressure-sensitive adhesive layer-attached optical laminates and a plurality of intervening films to form a workpiece, and cutting an outer peripheral surface of the workpiece, The cutting of the workpiece includes cutting with an end mill, and the cutting with the end mill includes cutting with a twist file; The twisted file is constructed by attaching diamond particles to an end mill having a twisted blade, Each of the plurality of pressure-sensitive adhesive layer-attached optical laminates includes an optical film, a first pressure-sensitive adhesive layer having a thickness of 50 μm or more and disposed on one side of the optical film, a first release liner releasably and temporarily attached to the first pressure-sensitive adhesive layer, a second pressure-sensitive adhesive layer disposed on the other side of the optical film, and a second release liner releasably and temporarily attached to the second pressure-sensitive adhesive layer. A method for producing a pressure-sensitive adhesive layer-attached optical laminate.
2. The method according to claim 1, wherein the thickness of the interposing film is from 75 μm to 1000 μm.
3. The method according to claim 1 or 2, wherein the interposing film is made of a polyester resin.
4. The method according to claim 1 , wherein the release strength of the first release liner is greater than the release strength of the second release liner.
5. The method according to claim 4 , wherein the optical film includes a polarizer and a retardation layer in this order from the first pressure-sensitive adhesive layer side.
6. The end mill has a twisted blade and the pocket area per blade is 5 mm 2 The method for producing a semiconductor device according to any one of claims 1 to 5, wherein the method is as described above.
7. The manufacturing method according to any one of claims 1 to 6, wherein the outer diameter of the end mill is 10 mm to 20 mm.
8. The manufacturing method according to claim 1 , wherein the cutting with the end mill includes rough cutting with an end mill having a helical blade and finish cutting with a helical file.
Citation Information
Patent Citations
Laminated film circumferential edge finishing method
JP2001054845A
Diamond coating end mill
JP2002273614A
Diamond-coated end mill
JP2004001115A
Method for manufacturing cut optical laminate having adhesive layer
JP2020134708A
Grinding tool and manufacturing method therefor
WO2016093186A1