Avalanche photodetector (variant) and method for manufacturing same (variant)
The avalanche photodetector design addresses inefficiencies in carrier transfer by separating amplification and conversion sections and using a notch and groove structure to enhance sensitivity and reduce dark current, achieving improved signal multiplication and carrier suppression.
Patent Information
- Application Number
- JP2021555095
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-03-12
- Filing Date
- 2020-03-04
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-03-04
AI Technical Summary
Conventional avalanche photodetectors suffer from inefficiencies in transferring optical carriers from the optical conversion section to the avalanche amplifier section, leading to reduced threshold sensitivity and increased dark current.
The avalanche photodetector design separates the avalanche amplification from the light converter by placing a multiplication layer across a conductive wafer, with a notch etched in the multiplication layer and a contact layer formed at its bottom, and uses a groove filled with highly doped polycrystalline silicon to facilitate efficient carrier movement and reduce dark current.
This design enhances threshold sensitivity and reduces dark current, allowing for improved signal multiplication and suppression of parasitic charge carriers, thereby increasing the device's efficiency.
Smart Images

Figure 0007578293000001 
Figure 0007578293000002 
Figure 0007578293000003
Abstract
Description
[Technical field]
[0001] The claimed invention relates to avalanche photodetectors (APDs), which are high-speed, highly sensitive instruments widely used in LiDAR, communication systems, machine vision, robotics, medicine, biology, environmental monitoring, and the like. [Background technology]
[0002] A conventional avalanche photodetector (APD) comprises several semiconductor layers disposed on a semiconductor wafer.
[0003] A group of semiconductor layers forms the photoconversion region, where signal photons are absorbed and free carriers, i.e. electrons and electron holes, are generated. These photogenerated charge carriers then pass into another group of semiconductor layers, the avalanche amplifier, within which an area is formed where the electric field strength is sufficient for avalanche multiplication of the charge carriers.
[0004] To reduce the dark current of the avalanche amplifier and thereby increase the threshold sensitivity of the APD, the area occupied by the avalanche amplifier can be made smaller than the area occupied by the photoconverter.
[0005] In the APD disclosed in U.S. Pat. No. 9,035,410 and Russian Patent No. 2,641,620, both the avalanche amplifier section, which comprises two layers - a contact layer and a multiplication layer - and the photoconverter section are located on the same wafer, and the area of the photoconverter section is larger than the area of the amplifier section.
[0006] The parameters of such devices can be additionally optimized, i.e., the threshold sensitivity can be improved by reducing the area of the avalanche amplifier. In the APD according to Russian Patent No. 2,641,620, the multiplication layer is made of a semiconductor material having the same conductivity type as the signal photoconverter, faces the wafer and is joined to the autonomous photoconverter, which makes it possible to reduce the excessive background noise caused by photocarriers traveling from the photoconverter to the avalanche amplifier via an external electric circuit (see U.S. Patent No. 9,035,410).
[0007] Shortcomings of the prior art In the APD of Russian Patent No. 2,641,620, the multiplication layer is separated from the photoconversion section, which prevents the photocarriers generated in the photoconversion section from reaching the multiplication layer, resulting in a loss of the amplified optical signal, which in turn reduces the threshold sensitivity, which is a basic parameter of the APD. Summary of the Invention [Problem to be solved by the invention]
[0008] The objective of the present disclosure is to create an avalanche photodetector (APD) with high threshold sensitivity that is not limited by the inefficiency of photocarrier transfer from the photoconversion section to the avalanche amplification section. Furthermore, proposed embodiments of the claimed APD allow for a reduction in its dark current.
[0009] By solving these problems, it will be possible to improve the threshold sensitivity of APD, which is its fundamental parameter. [Means for solving the problem]
[0010] The claimed invention includes an avalanche photodetector (APD) and a method for fabricating the same, which allows for more efficient transfer of photocarriers from a photoconverter to an avalanche amplifier by placing a multiplication layer over the entire conductive wafer. At least one avalanche amplifier contact layer is formed in a specific area of the multiplication layer. The multiplication layer outside the contact layer thus functions as a photoconverter. As a result, photocarriers generated in the photoconverter pass unimpeded into the multiplication region of the avalanche amplifier. A first electrode and a second electrode of the avalanche photodetector are placed on the contact layer and the wafer, respectively.
[0011] To mitigate the effect of parasitic charge carriers near the surface on the avalanche amplifier, a notch is etched into the multiplication layer and an avalanche amplifier contact layer is formed at the bottom of the notch, deepening the multiplication region relative to the top surface of the photoconversion region.
[0012] To reduce dark current in the APD from adjacent wafer regions, a closed trench is etched into the multiplication layer surface with a depth equal to or greater than the thickness of the multiplication layer but less than the combined thickness of the wafer and multiplication layer, and a photodetector is formed inside the region bounded by the trench, which is filled with heavily doped polycrystalline silicon of the same conductivity type as the multiplication layer.
[0013] To increase efficiency, the semiconductor wafers should be made of low resistivity materials.
[0014] Preferably, both the wafer and the multiplication layer are made of the same semiconductor material.
[0015] The multiplication layer on the wafer surface can be created using epitaxy techniques, and the contact layer can be created by doping the multiplication layer with a dopant that forms a layer of opposite conductivity.
[0016] The grooves preferably have a width of 1.5 μm to 2.0 μm.
[0017] A high resistance layer can be provided between the contact layer of the avalanche amplifier and the first electrode.
[0018] The objects, features, and advantages of the present invention will be further pointed out in the detailed description and the accompanying drawings. [Brief description of the drawings]
[0019] [Figure 1] 1 is a schematic transverse cross-sectional view of a claimed APD according to a first embodiment, comprising a semiconductor wafer 101, a multiplication layer 102 covering the entire surface of the semiconductor wafer having the same conductivity type as the multiplication layer, a dielectric layer 103 covering the multiplication layer 102 surface and a sidewall of a notch 104 having a depth of 0.5-2.5 μm for a contact layer 105, and a contact layer 105 made by diffusion from highly doped polycrystalline silicon having an opposite conductivity to that of the multiplication layer, at least one avalanche amplifier 106 and a photo-converter 107 outside the avalanche amplifier, a first electrode 108 located on the highly doped polycrystalline silicon filling the notch 104 and on the transparent dielectric layer 103, and a second electrode 109 formed on a bottom surface of the semiconductor wafer 101. [Figure 1A] 1A and 1B are diagrams showing a process of placing a multiplication layer 102 on a silicon wafer 101. [Figure 1B] 1A and 1B are diagrams illustrating a process of placing a dielectric layer 103 on a multiplication layer 102. [Figure 1C] FIG. 1 illustrates a process for forming the avalanche amplifier 106 region by creating a contact layer 105 by diffusion from heavily doped polycrystalline silicon filling a 0.5-2.5 μm deep notch 104 having an opposite conductivity to that of the multiplication layer, forming at least one avalanche amplifier 106 and a photoconverter 107 outside the avalanche amplifier. [Figure 1D]FIG. 1 illustrates a process of forming a first electrode 108 made of a transparent conductive material on the surface of the highly doped polycrystalline silicon and dielectric layer 103 filling the notch 104. [Figure 1E] 1A to 1C are diagrams showing a process of forming a second electrode 109 on a semiconductor wafer 101. [Diagram 2] The semiconductor wafer 201 includes a multiplication layer 202 covering the entire surface of the semiconductor wafer having the same conductivity type as the multiplication layer, a dielectric layer 203 covering the multiplication layer 202 surface and the sidewall of a notch 204 for a contact layer 205, and a contact layer 205 filling the notch 204 with a depth of 0.5 to 2.5 μm and made by diffusion from highly doped polycrystalline silicon having a conductivity opposite to that of the multiplication layer, and at least one avalanche amplification section 206 and a photoconversion section 207 are formed, and further includes a multiplication layer 202 having a width of 1.5 μm to 2.0 μm and a depth of 1.5 μm to 2.0 μm. 2 is a schematic cross-sectional view of a claimed APD according to a second embodiment, comprising: a closed trench 210, the thickness of which is equal to or greater than the thickness of the multiplication layer but less than the total thickness of the wafer and multiplication layer combined, filled with heavily doped polysilicon of the same conductivity type as the multiplication layer and surrounding the avalanche amplification section and the photo-conversion section; a high-resistivity layer 211 formed on the highly doped polysilicon filling the notch 204; a transparent electrode 208 formed on the surface of the high-resistivity layer 211 and the dielectric layer 203; and a second electrode 209 formed on the semiconductor wafer 201. [Figure 2A] 2 is a diagram showing a process of placing a multiplication layer 202 on a silicon wafer 201. FIG. [Figure 2B] FIG. 2 illustrates the process of forming a blocked trench 210 filled with highly doped polycrystalline silicon of the same conductivity type as the multiplication layer, allowing a photodetector to be formed inside the area bounded by said trench. [Figure 2C] 2A and 2B are diagrams illustrating a process of placing a dielectric layer 203 on a multiplication layer 202. [Figure 2D]FIG. 2 illustrates a process for forming the avalanche amplifier 206 region by creating a contact layer 205 by diffusion from heavily doped polycrystalline silicon filling a 0.5-2.5 μm deep notch 204 having an electrical conductivity opposite to that of the multiplication layer, forming at least one avalanche amplifier 206 and a photoconverter 207 outside the avalanche amplifier. [Figure 2E] 13A and 13B are diagrams showing a process of forming a high resistance layer 211 on a contact layer 205 of an avalanche amplifier section 206. [Figure 2F] FIG. 2 illustrates a process of forming a first electrode 208 made of a transparent conductive material on the surface of the highly doped polycrystalline silicon and dielectric layer 203 filling the notch 204. [Figure 2G] 2A to 2C are diagrams showing a process of forming a second electrode 209 on a semiconductor wafer 201. [Figure 3A] 2 is a schematic top view of an APD according to a second embodiment, which includes a single avalanche amplifier 206 and a groove 210. FIG. [Figure 3B] 1 is a schematic top view of an APD according to a second embodiment, which includes three avalanche amplifiers 206 and a groove 210. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] Reference markings used throughout this disclosure and the accompanying drawings, with the exception of the numeral 100 (incident light), consist of three numerals, the first numeral being the figure number and the last two numerals designating a particular element of the design.
[0021] For example, in FIG. 2, marking 206 refers to element number 06 (see list below).
[0022] The following markings are used to refer to specific elements of the design: 01‐ Wafer, 02- Multiplication layer, 03- Dielectric layer, 04- Notch filled with highly doped polycrystalline silicon; 05- Contact layer, 06- Avalanche amplifier, 07- Optical conversion section, 08- First transparent electrode, 09- Second electrode, 10 – Obstructed sulcus, 11- High resistance material layer.
[0023] FIG. 1 is a schematic cross-sectional view of a claimed APD according to a first embodiment, comprising a semiconductor wafer 101, a multiplication layer 102 covering the entire surface of the semiconductor wafer having the same conductivity type as the multiplication layer, a dielectric layer 103 covering the surface of the multiplication layer 102, a notch 104 filled with highly doped polycrystalline silicon, and a contact layer 105 made by diffusing dopants from the highly doped polycrystalline silicon having an opposite conductivity to that of the multiplication layer, in which at least one avalanche amplifier 106 and a photo-conversion section 107 outside the avalanche amplifier are formed, and further comprising a first electrode 108 made of a transparent material located on top of the highly doped polycrystalline silicon filling the notch 104 and on the dielectric layer 103, and a second electrode 109 formed on the bottom surface of the semiconductor wafer 101.
[0024] A method for manufacturing an APD as shown in FIG. 1 is further illustrated by FIGS. 1A, 1B, 1C, 1D, 1E, and 1F and includes the following sequence of steps.
[0025] Depositing on a silicon wafer 101 a multiplication layer 102 of the same conductivity type as the wafer (see FIG. 1A).
[0026] Providing a dielectric layer 103 on top of the multiplication layer 102 (see FIG. 1B).
[0027] Forming one or more avalanche amplifier 106 regions in the multiplication layer by etching a 0.5-2.5 μm deep notch 104 in both the dielectric layer 103 and the multiplication layer 102, covering its sidewalls with a dielectric layer, and filling it with highly doped polycrystalline silicon (see FIG. 1C).
[0028] A step of forming a contact layer 105 by diffusing dopants from heavily doped polycrystalline silicon having an opposite conductivity to that of the multiplication layer filling the notch 104, whereby at least one avalanche amplification section 106 and a photoconversion section 107 outside the avalanche amplification section are formed (see FIG. 1D).
[0029] Forming a first electrode 108 made of a transparent conductive material on the surface of the highly doped polycrystalline silicon filling the notch 104 and on the surface of the dielectric layer 103 (see FIG. 1E).
[0030] Forming a second electrode 109 on the bottom surface of the semiconductor wafer 101 (see FIG. 1F).
[0031] The exemplary APD according to FIG. 18 cm -3 On a p+ type silicon wafer 101 having a dopant concentration higher than 15 ~10 17 cm -3 The multiplication layer 102 may be fabricated using a method that includes forming by epitaxy a multiplication layer 102 having a width of 5-7 μm, made of p-type silicon with a dopant concentration of 1000 .5-2.5 μm. A notch 104 having a depth of 0.5-2.5 μm is etched into both the dielectric layer 103 and the multiplication layer 102, the sidewalls of which are covered with a dielectric layer, and then the notch 104 ... 18 cm -3At least one avalanche amplifier 106 is formed on the surface of the multiplication layer by filling it with highly doped polycrystalline silicon having a dopant concentration higher than that of the multiplication layer 102 and an opposite conductivity to that of the multiplication layer 102, and then diffusing said dopant into the multiplication layer 102 to form a contact layer 105, and a photoconverter layer 107 is formed outside the avalanche amplifier 106. A first electrode 108 made of a transparent material of ITO or AZO type is formed on the surface of the highly doped polycrystalline silicon filling the notch 104 and the dielectric layer 104, while a second electrode 109, which is an aluminum foil having a thickness of about 0.5 to 1.0 μm, is formed on the bottom side of the semiconductor wafer 101.
[0032] An APD such as that shown in FIG. 1 operates as follows.
[0033] In contrast to electrode 109, electrode 108 is applied with a positive voltage sufficient to trigger impact ionization in multiplication layer 102 of avalanche amplifier 106, multiplying the free charge carriers.
[0034] Incident light 100 falling on the surface of the photo-conversion section 107 is absorbed and free charge carriers, i.e. electrons and electron-holes, are generated. The photoinduced free electrons (photoelectrons) in the photo-conversion section 107 are driven by the superposition of electric fields, one percolating from the avalanche amplification section 106 and the other induced by the first electrode 108 in the photo-conversion section, to drift towards the avalanche multiplication layer 102 where they are multiplied and generate the output signal of the APD, while the holes travel into the wafer 101. The photoinduced photoelectrons in the non-depleted area of the photo-conversion section 107 are collected in the depleted area of the photo-conversion section by diffusion caused by the concentration gradient of free electrons in the photo-conversion section.
[0035] In order to mitigate the effect of parasitic charge carriers near the surface on the avalanche amplifier, a notch 104 is etched in the multiplication layer, and a contact layer 105 of the avalanche amplifier 106 is formed at the bottom of the notch 104, thereby deepening the multiplication region relative to the top surface of the photoconverter region. At the same time, photocarriers from the actual recorded long-wavelength signal can efficiently enter the avalanche amplifier region from the photoconverter, while the inflow of dark carriers from the dielectric-photoconverter interface is prevented.
[0036] FIG. 2 shows a semiconductor wafer 201, a multiplication layer 202 covering the entire surface of the semiconductor wafer having the same conductivity type as the multiplication layer, a dielectric layer 203 covering the surface of the multiplication layer 202, a notch 204 filled with highly doped polycrystalline silicon, and a contact layer 205 filling the notch 204 to a depth of 0.5 to 2.5 μm and made by diffusing dopants from highly doped polycrystalline silicon having a conductivity opposite to that of the multiplication layer, in which at least one avalanche amplification section 206 and a photoconversion section 207 located outside the avalanche amplification section are formed, and further 2 is a schematic transverse cross-sectional view of a claimed APD according to a second embodiment, comprising: a closed groove 210 having a width of 1.5 μm to 2.0 μm and a depth equal to or greater than the thickness of the multiplication layer but less than the total thickness of the wafer and multiplication layer combined, filled with highly doped polycrystalline silicon of the same conductivity type as the multiplication layer, and surrounding the avalanche amplification section and the photoconversion section; a high-resistance layer 211 formed on the highly doped polycrystalline silicon filling the notch 204; a transparent electrode 208 formed on the surfaces of the high-resistance layer 211 and the dielectric layer 203; and a second electrode 209 formed on the semiconductor wafer 201.
[0037] A method for manufacturing an APD as shown in FIG. 2 is further illustrated by FIGS. 2A, 2B, 2C, 2D, 2E, 2F, 2G, and 2H, and includes the following sequence of steps.
[0038] Depositing on a silicon wafer 201 a multiplication layer 202 of the same conductivity type as the wafer (see FIG. 2A).
[0039] Etching a closed trench 210 on the surface of the multiplication layer 202 having a depth equal to or greater than the thickness of the multiplication layer but less than the total thickness of the wafer and the multiplication layer combined, and filling it with heavily doped polycrystalline silicon of the same conductivity type as the multiplication layer 202 so as to allow the formation of a photodetector inside the area bounded by said trench (see FIG. 2B).
[0040] Providing a dielectric layer 203 over the multiplication layer 202 and the notch 204 (see FIG. 2C).
[0041] Forming one or more avalanche amplifier 206 regions in the multiplication layer by etching a 0.5-2.5 μm deep notch 204 in both the dielectric layer 203 and the multiplication layer 202, covering its sidewalls with a dielectric layer, and filling it with highly doped polycrystalline silicon (see FIG. 2D).
[0042] A step of forming a contact layer 205 by diffusing dopants from heavily doped polycrystalline silicon having an opposite conductivity to that of the multiplication layer filling the notch 204, whereby at least one avalanche amplifier section 206 and a photoconversion section 207 outside the avalanche amplifier section are formed (see FIG. 2E).
[0043] Forming a high resistance layer 211 on the surface of the highly doped polycrystalline silicon filling the notch 204 (see FIG. 2F).
[0044] Forming a first electrode 208 made of a transparent conductive material on top of the high resistance layer 211 and the dielectric layer 203 (see FIG. 2G).
[0045] Forming a second electrode 209 on the bottom surface of the semiconductor wafer 201 (see FIG. 2H).
[0046] The exemplary APD according to FIG. 18 cm -3 On a p+ type silicon wafer 201 having a dopant concentration higher than 15 ~10 17 cm -3 The multiplication layer 202 may be fabricated using a method that includes forming by epitaxy a multiplication layer 202 having a width of 5-7 μm, made of p-type silicon with a dopant concentration of 1000 μm. A closed trench 210 is then etched on the surface of the multiplication layer 202, having a width of 1.5 μm-2.0 μm and a depth equal to or greater than the thickness of the multiplication layer but less than the total thickness of the wafer and multiplication layer combined, and filled with highly doped polycrystalline silicon of the same conductivity type as the multiplication layer 202, so as to allow the formation of a photodetector inside the area bounded by said trench. A notch 0.5-2.5 μm deep is etched in both the dielectric layer and the multiplication layer, the sidewalls of which are covered with a dielectric layer and then etched at a depth of 1000 μm. 18 cm -3 At least one avalanche amplifier 205 is formed on the surface of the multiplication layer 202 by filling it with highly doped polycrystalline silicon having a dopant concentration higher than that of the multiplication layer 202 and an opposite conductivity to that of the multiplication layer 202, and then diffusing said dopant into the multiplication layer 202 to form a contact layer 205, and a photoconversion layer 207 is formed outside the avalanche amplifier 206. A high resistance layer 211 made of highly resistive polycrystalline silicon is formed on the highly doped polycrystalline silicon filling the notch 204. A first electrode 207 made of a transparent material of ITO or AZO type is formed on both the high resistance layer 211 and the dielectric layer 203, while a second electrode 208, which is an aluminum foil having a thickness of about 0.5 to 1.0 μm, is formed on the bottom surface of the semiconductor wafer 201.
[0047] The APD according to the embodiment as shown in Fig. 2, i.e. with blocked trenches 210, is characterized by the fact that it is possible to suppress the inflow of parasitic charge carriers from adjacent regions into the avalanche amplifier. To effectively suppress such parasitic currents, the trenches with a depth exceeding the thickness of the multiplication layer will be filled with highly doped polycrystalline silicon of the same conductivity type as the multiplication layer. The smaller dark current in the APD leads to a further improvement in the threshold sensitivity.
[0048] The highly resistive layer 211 located over the heavily doped polycrystalline silicon filling the notch 104 provides negative feedback when the avalanche forms, making it possible to achieve higher multiplication factors, especially when operating in the so-called "Geiger" mode.
Claims
1. 1. A method for manufacturing an avalanche photodetector, comprising the steps of: - forming a multiplication layer over the entire surface of a semiconductor wafer; - covering the entire surface of said multiplication layer with a dielectric layer; - forming at least one avalanche amplifier on a specific area of the top surface of the multiplication layer and on the dielectric layer by etching a notch in both the dielectric layer and the multiplication layer, the sidewalls of the notch being covered with a dielectric layer; filling said notch with highly doped polycrystalline silicon having an electrical conductivity opposite to that of the multiplication layer, followed by diffusing dopants from said polycrystalline silicon areas into said multiplication layer to form the contact layer of said at least one avalanche multiplication part and the photoconversion part formed outside said notch; - placing a first electrode made of a transparent material on both the surface of said highly doped polycrystalline silicon and on the surface of said dielectric layer; - forming a second electrode on a bottom surface of the semiconductor wafer.
2. 1. A method for manufacturing an avalanche photodetector, comprising the steps of: - forming a multiplication layer over the entire surface of a semiconductor wafer; - etching a blocked trench extending on the surface of the multiplication layer in order to form an avalanche amplifier and a photoconverter inside the area bounded by the blocked trench, the depth of the trench being equal to or greater than the thickness of the multiplication layer but less than the total thickness of the wafer and multiplication layer combined; - filling said blocked trenches with highly doped polycrystalline silicon of the same conductivity type as said multiplication layer; - covering the entire surface of the multiplication layer and the closed grooves with a dielectric layer; - forming at least one avalanche amplifier on the upper surface of the multiplication layer and the dielectric layer, inside the area bounded by the closed trench, by etching a notch in both the dielectric layer and the multiplication layer, the sidewalls of the notch being covered with a dielectric layer; filling said notch with highly doped polycrystalline silicon having an electrical conductivity opposite to that of the multiplication layer, followed by diffusing dopants from said polycrystalline silicon areas into said multiplication layer to form the contact layer of said at least one avalanche multiplication part and the photoconversion part formed outside said notch; - providing a highly resistive layer on the surface of said highly doped polycrystalline silicon filling said notch; - depositing on the surface of both said highly resistive layer and said dielectric layer a first electrode made of a transparent material; - forming a second electrode on a bottom surface of the semiconductor wafer.
3. The method according to claim 1 or 2, wherein the semiconductor wafer is made of a low resistivity material.
4. The method of any one of claims 1 to 3, wherein the wafer and the multiplication layer are both made of the same semiconductor material.
5. The method according to any one of claims 1 to 4, wherein the multiplication layer is formed on the wafer surface using an epitaxy method.
6. The method of any one of claims 1 to 4, wherein a notch having a depth of 0.5 μm to 2.5 μm is etched into the dielectric layer and the multiplication layer.
7. The method of claim 2, wherein the blocked grooves have a width between 1.5 μm and 2.0 μm.
8. 3. The method of claim 2, wherein a highly resistive layer is deposited on the highly doped polysilicon before the first electrode is deposited.
9. 1. An avalanche photodetector, comprising: a semiconductor wafer; an epitaxial multiplication layer covering the surface of the semiconductor wafer; a dielectric layer covering the surface of said epitaxial multiplication layer; a photoconversion part located outside at least one avalanche multiplication part formed on the epitaxial multiplication layer and a contact layer of the avalanche multiplication part; a contact layer of the avalanche multiplier, made by diffusion of dopants from highly doped polycrystalline silicon of opposite conductivity to that of the multiplication layer, filling a notch in both the dielectric layer and the multiplication layer, the notch being flanked by a dielectric layer; a first electrode made of a transparent material and placed on the surface of said highly doped polycrystalline silicon and on the surface of said dielectric layer; a second electrode formed on a bottom surface of the semiconductor wafer.
10. 10. The avalanche photodetector of claim 9, wherein the notch etched into the dielectric layer and the multiplication layer has a depth of between 0.5 μm and 2.5 μm.
11. 1. An avalanche photodetector, comprising: a semiconductor wafer; an epitaxial multiplication layer covering the entire surface of the semiconductor wafer; a dielectric layer covering the surface of said epitaxial multiplication layer; a photoconversion part located outside at least one avalanche multiplication part formed on the epitaxial multiplication layer and a contact layer of the avalanche multiplication part; a contact layer of the avalanche multiplier made by diffusion of dopants from highly doped polycrystalline silicon of opposite conductivity to that of the multiplication layer, filling a notch etched in both the dielectric layer and in the multiplication layer, the side of which is lined with dielectric; a first electrode made of a transparent material and placed on the surface of the dielectric layer and on the highly resistive layer on the highly doped polycrystalline silicon; a second electrode formed on a bottom surface of the semiconductor wafer; a closed trench formed on the multiplication layer, the depth of which is equal to or greater than the thickness of the multiplication layer, but less than the total thickness of the wafer and multiplication layer combined, and which is filled with highly doped polycrystalline silicon of the same conductivity type as the multiplication layer, the trench being located around the avalanche amplifier and the photoconverter.
12. 12. The avalanche photodetector of claim 11, wherein the notch etched into the dielectric layer and the multiplication layer has a depth of between 0.5 μm and 2.5 μm.
13. The avalanche photodetector of claim 12, wherein the groove has a width between 1.5 μm and 2.0 μm.
Citation Information
Patent Citations
Avalanche photodiode
JP1987033482A
Structure of semiconductor photomultiplier
JP2008311651A
High-sensitivity high-resolution detectors and arrays
JP2008544496A