Welded cover for laminated core
The welding cover for laminated cores addresses spatter adhesion by covering the outer surface near the welding groove with a replaceable copper alloy part, ensuring effective spatter prevention and cost-effective maintenance.
Patent Information
- Application Number
- JP2021019820
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-10
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2041-02-10
AI Technical Summary
Conventional welding covers for laminated cores fail to prevent spatter from adhering to the outer circumferential surface near the welding groove, risking contamination and additional processing difficulties.
A welding cover for laminated cores that covers a predetermined range of the outer peripheral surface near the welding groove while exposing the welding position, using a replaceable copper or copper alloy cover part to suppress spatter adhesion.
Effectively prevents spatter from adhering to the outer circumferential surface of laminated cores during welding, allowing for easy replacement of worn parts and reducing manufacturing costs.
Smart Images

Figure 0007579167000001 
Figure 0007579167000002 
Figure 0007579167000003
Abstract
Description
[Technical Field]
[0001] SUMMARY OF THE INVENTION An embodiment of the present invention relates to a weld cover for a laminated core. [Background technology]
[0002] Conventionally, laminated cores have been known, in which thin-plate-shaped core pieces are stacked. Such laminated cores have weld grooves recessed from the outer periphery and extending in the stacking direction, and the core pieces are fixed in a stacked state by welding at welding positions set within the weld grooves. Since spatter is generated during welding, Patent Document 1, for example, proposes placing a weld cover in the weld groove to prevent spatter generated during welding from adhering to the laminated core. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Laid-Open No. 2011-87386 Summary of the Invention [Problem to be solved by the invention]
[0004] It is believed that by using the above-described welding cover, spatter scattered from the welding position can be prevented from adhering to the surface of the laminated core. However, if the material melted at the welding position flows around the welding cover, it may adhere to the outer peripheral surface near the welding groove as spatter.
[0005] Therefore, a welding cover for a laminated core is provided that can suppress the risk of spatter adhering to the outer peripheral surface of the laminated core in the vicinity of the welding groove. [Means for solving the problem]
[0006] The welding cover for a laminated core according to the embodiment is for a laminated core used when welding the laminated core, and the laminated core has a welding groove formed therein that is recessed from the outer peripheral surface and extends in the stacking direction, and has a portion that contacts the surface of the welding groove, and covers a predetermined area of the outer peripheral surface on the side of the welding groove while exposing the welding position formed within the welding groove. [Brief explanation of the drawings]
[0007] [Figure 1] FIG. 1 is a diagram showing a schematic example of the configuration of a laminated core; [Figure 2] 1 is a diagram schematically illustrating an example of a configuration of a welding groove and an example of a welding mode. [Figure 3] FIG. 1 is a diagram showing an example of a state in which a welding cover is attached to a laminated core; [Figure 4] FIG. 1 is a diagram schematically illustrating an example of the configuration of a welding cover. [Figure 5] FIG. 10 is a diagram illustrating an example of the configuration of a cover portion. [Figure 6] FIG. 1 is a diagram illustrating an example of the configuration of a main body portion; [Figure 7] FIG. 10 is a diagram schematically illustrating an example of the shape of a main body portion. [Figure 8] FIG. 1 is a diagram schematically illustrating an example of the configuration of a base portion; [Figure 9] FIG. 10 is a diagram schematically illustrating an example of a welding mode with a welding cover attached. [Figure 10] FIG. 10 is a diagram schematically illustrating another configuration example of the cover portion. [Figure 11] Diagram 1 showing another example of the welding cover configuration [Figure 12] Diagram 2 showing another example of the welding cover configuration DETAILED DESCRIPTION OF THE INVENTION
[0008] An embodiment will be described below. First, an example of the configuration of a laminated core 1 to be welded and the welding method will be described with reference to Fig. 1 and Fig. 2. As shown in Fig. 1, the laminated core 1 is formed by stacking core pieces 2, which are formed, for example, by punching thin strip-shaped electromagnetic steel sheets into an annular shape using a press (not shown). Hereinafter, in the stacking direction of the core pieces 2, the upper side in the figure will be referred to as the upper end of the laminated core 1, and the lower side in the figure will be referred to as the lower end of the laminated core 1.
[0009] The electrical steel sheet may have a relatively high silicon content and a relatively thin thickness to improve high-frequency characteristics, and as is well known, the surface of the electrical steel sheet is covered with an insulating coating.
[0010] In this embodiment, the laminated core 1 is formed by stacking a plurality of roughly annular core pieces 2 to form, for example, three blocks 2A to 2C, and stacking the blocks 2A to 2C while shifting them relative to one another in the circumferential direction, a process known as rotation stacking. This suppresses variations in height and weight in the circumferential direction that may occur due to uneven thickness of the electromagnetic steel sheets that serve as the base material. Note that the stacking mode of the core pieces 2 is not limited to this.
[0011] The laminated core 1 has a hollow portion 4 on its inner circumferential side for accommodating a rotor (not shown), and multiple slots 5 that open toward the hollow portion 4 and accommodate windings (not shown). On the other hand, multiple lugs 6 for fixing the laminated core 1 to a housing (not shown) are provided on the outer circumferential side of the laminated core 1 at three equally spaced locations around the periphery of the laminated core 1. However, the shapes, number, and positions of the hollow portions 4, slots 5, and lugs 6 are merely examples, and are not limited to the example configuration shown in FIG. 1.
[0012] Additionally, a plurality of welding grooves 7 for welding the laminated core pieces 2 together are formed on the outer peripheral surface of the laminated core 1, extending along the lamination direction from the upper end to the lower end of the laminated core 1. In this embodiment, the welding grooves 7 are formed at six locations that are equally spaced in the circumferential direction of the laminated core 1.
[0013] As shown in Fig. 2, the welding groove 7 is formed so as to be on the inner periphery side of an imaginary line (CL) extending from the outer periphery of the laminated core 1, in other words, so as to be recessed from the outer periphery of the laminated core 1 as a whole. Hereinafter, the direction roughly along the outer periphery of the laminated core 1 will be referred to as the width direction of the welding groove 7. The welding groove 7 has a protrusion 8 formed roughly in the center of the width direction, which protrudes relatively toward the outer periphery. This protrusion 8 corresponds to the welding position.
[0014] Both sides of the protrusion 8 are recessed relatively inward, forming recesses 9 that connect to the outer circumferential surface on the sides of the welding groove 7. In this embodiment, the recesses 9 are formed in a smooth curve, and the welding groove 7 is generally ω-shaped. However, the welding groove 7 can also be formed in a shape that does not form the protrusion 8, such as a shape that is curvedly recessed from the outer circumferential surface or a shape that has a partially flat portion. In that case, the welding position is approximately at the center in the width direction.
[0015] The width (W7) of weld groove 7, the width (W8) of convex portion 8, and the width (W9) of each concave portion 9 can be set as appropriate. However, the gap (ΔL) between the tip of convex portion 8 and imaginary line (CL) is set to a length that prevents weld bead 10 formed at the tip of convex portion 8 during welding from protruding beyond imaginary line (CL).
[0016] In this embodiment, the laminated core 1 is welded by so-called MAG (Metal Active Gas) welding using a welding torch 11. In this MAG welding, a magnetic material 12 serving as an electrode material is supplied through a cylindrical body 11a with a bottom that opens toward the welding position, and welding is performed by moving the welding torch 11 along the welding groove 7 while supplying a shielding gas (G) to shield the magnetic material 12 and the welding position. The magnetic material 12 is supplied by a rotating reel 13 in the amount required for each welding. The shielding gas (G) is, for example, carbon dioxide gas alone or a mixture of carbon dioxide gas and an inert gas.
[0017] During welding, the core pieces 2 and magnetic material 12 melt, which can generate spatter such as slag and metal particles. If the spatter scatters and adheres to the laminated core 1, it may become mixed in as foreign matter during the winding process or varnish impregnation process that follow the welding. Furthermore, spatter adhering to the outer peripheral surface affects the external shape of the laminated core 1, which could cause problems when it is housed in a housing.
[0018] Therefore, if spatter adheres to the laminated core 1, it is necessary to remove the spatter. However, although it depends on the size, if the spatter is approximately 0.5 mm or larger, it will firmly adhere to the laminated core 1. In such cases, removing the spatter requires a great deal of effort.
[0019] Therefore, in this embodiment, when welding the laminated core 1, in order to prevent spatter from adhering to the laminated core 1, particularly to the outer surface of the laminated core 1 near the welding groove 7, a welding cover 20 is attached at a position corresponding to the welding groove 7 of the laminated core 1 as shown in Figure 3.
[0020] In this embodiment, the welding cover 20 is attached to the laminated core 1 using a mounting portion 14, on which the laminated core 1 is placed during welding, and which has a diameter larger than that of the laminated core 1, and an upper lid 15, which is placed on the upper end of the laminated core 1. This upper lid 15 constitutes part of a pressurizing machine used to remove burrs caused by punching and to determine the height (H1) of the laminated core 1. The laminated core 1 is placed on the mounting portion 14 with presser plates 16 attached to the upper and lower ends in the lamination direction. These presser plates 16 are intended to prevent the core pieces 2 from shifting when the laminated core 1 is transferred from the lamination process to the welding process.
[0021] More specifically, during welding, the lower end of the welding cover 20 is supported by a support portion 30 fixed in a housing portion 14a recessed from the outer circumferential surface of the mounting portion 14. The support portion 30 has a shaft 31 at a position that sandwiches the lower end of the base portion 23 of the welding cover 20 from both sides, and supports the welding cover 20 in a state in which it can rotate around the shaft 31. In the present embodiment, the welding cover 20 is basically attached to the mounting portion 14, is attached to the laminated core 1 during welding, and is released from the attachment when the welding is completed.
[0022] Additionally, the welding cover 20 is fixed with its upper end pressed against the laminated core 1 by a pressing portion 40 provided on the top lid 15. This pressing portion 40 includes a plate portion 41 that covers the base portion 23 of the welding cover 20 from the outside, and a pressing bar 43 with rollers 42 that press the plate portion 41 toward the laminated core 1. Additionally, a sloped portion 44 is formed on the surface of the plate portion 41, sloping gradually downward and toward the front of the figure.
[0023] During welding, the welding cover 20 is rotated to a position where the upper end of the base portion 23 is on the back side of the plate portion 41, and in that state the top lid 15 is moved downward as shown in the figure. At this time, in the pressing portion 40, the rollers 42 attached to the pressing bar 43 gradually climb the slopes 44 as the top lid 15 moves, thereby pressing the plate portion 41 toward the laminated core 1. As a result, the welding cover 20 is attached while being pressed against the laminated core 1.
[0024] Although not shown, the mounting portion 14 is formed with a number of accommodation portions 14a corresponding to the number of welding grooves 7, and a support portion 30 is disposed in each accommodation portion 14a. Therefore, during welding, each of the multiple welding grooves 7 can be covered with a welding cover 20, and it is possible to handle situations where multiple welding grooves 7 are welded simultaneously.
[0025] This welding cover 20 includes a cover portion 21, a main body portion 22, and a base portion 23, and is formed in a shape that covers the outer peripheral surface of the side of the welding groove 7 while exposing the welding position set in the welding groove 7. More specifically, as shown in Fig. 4, the welding cover 20 is composed of two cover portions 21 arranged on the sides of the welding groove 7 facing the welding position in the welding groove 7, two main body portions 22 to which each cover portion 21 is replaceably and detachably attached, and a base portion 23 having an opening 23a that exposes the entire welding groove 7 of the laminated core 1, and to which the two main body portions 22 are replaceably and detachably attached on either side of the opening 23a.
[0026] 5, the cover portion 21 is formed in the shape of a flat rectangular plate from a copper material. That is, the cover portion 21 is formed in a simple shape that makes it relatively easy to process when manufacturing the cover portion 21. However, the cover portion 21 is not limited to a copper material, and can be formed from, for example, a copper alloy material, a copper-plated material, a gold-plated material, a silver-plated material, a tin-plated material, a chrome-plated material, a titanium material, a stainless steel material, or a combination thereof.
[0027] The cover portion 21 is provided with through holes 21a at, for example, two locations in the longitudinal direction for screwing to the main body portion 22. In this embodiment, the cover portion 21 is attached to the main body portion 22 with SUS screws. The length (L21) of the cover portion 21 is set to be longer than the length of the welding groove 7 in the lamination direction, that is, the height (H1) of the laminated core 1. The width (W21) and thickness (D21) of the cover portion 21 are set so that the longitudinal ends of the cover portion 21 come into contact with the surfaces of the welding grooves 7 when the cover portion 21 is attached to the main body portion 22, as will be described later.
[0028] 6, the main body 22 includes a flat mounting portion 22a for mounting to the base portion 23, and an inclined portion 22b having a flat inclined surface that slopes from the mounting portion 22a toward the welding groove 7. The mounting portion 22a has through holes 22c formed in, for example, two locations in the longitudinal direction for screwing the main body 22 to the base portion 23, and the inclined portion 22b has screw holes 22d formed in, for example, two locations at positions corresponding to the through holes 21a of the cover portion 21. In this embodiment, the main body 22 is mounted to the base portion 23 with stainless steel screws.
[0029] In this embodiment, the main body 22 is made of a soft iron material. That is, the main body 22 is made of a material that is relatively easy to process into its shape. However, the main body 22 is not limited to a soft iron material, and other materials can also be used. The length (L22) of the main body 22 is set to be longer than the length of the weld groove 7 in the lamination direction. The width (W22a) of the attachment portion 22a is set appropriately within a range that allows attachment to the base portion 23.
[0030] The width (W22b) of the inclined portion 22b is shorter than the width (W21) of the cover portion 21, and is set so that when the cover portion 21 is attached, the end portion of the cover portion 21 comes into contact with the surface of the welding groove 7. As shown enlarged in Fig. 7, the lower end surface 22e of the inclined portion 22b is formed in a shape corresponding to the surface shape of the portion connecting the welding groove 7 to the outer peripheral surface. Note that Fig. 7 shows a portion of the welding groove 7.
[0031] In this embodiment, the lower end surface 22e includes the boundary position (P) between the welding groove 7 and the outer peripheral surface of the laminated core 1, and is formed with a width (W22e) that covers from a position slightly within the welding groove 7 to a predetermined range of the outer peripheral surface to the side of the welding groove 7. However, as long as the lower end surface 22e includes the boundary position (P), it can be formed into a shape that does not overlap the welding groove 7 or a shape that overlaps the welding groove 7. Furthermore, because the main body 22 is made of a soft iron material, it is easy to form it into a shape that corresponds to the shape of the outer peripheral surface of the laminated core 1 and the shape of the welding groove 7, both in terms of manufacturing and cost.
[0032] Furthermore, a wall portion 22f is formed at the end of the mounting portion 22a on the inclined portion 22b side, i.e., at the upper end of the inclined portion 22b. This wall portion 22f is the portion with which the short-side end of the cover portion 21 comes into contact when the cover portion 21 is mounted to the main body portion 22. Then, by mounting the cover portion 21 with the short-side end in contact with the wall portion 22f, the relative positions of the cover portion 21 and the main body portion 22 are determined.
[0033] That is, the inclined surface of inclined portion 22b and wall portion 22f function as a positioning structure that determines the attachment position of cover portion 21. In addition, through hole 22c also functions as a positioning structure. As a result, by bringing lower end surface 22e of inclined portion 22b into contact with the surface of laminated core 1, the end of cover portion 21 protruding from inclined portion 22b is positioned so as to contact the surface of weld groove 7.
[0034] As shown in Fig. 8, the base portion 23 is formed in a generally flat plate shape. This base portion 23 is made of, for example, stainless steel, and is attached to a position corresponding to the welding groove 7 of the laminated core 1 with the cover portion 21 and the main body portion 22 attached. The size of the base portion 23 is arbitrary, but the width (W23a) of the opening 23a formed in the center is set to be larger than the width (W7) of the welding groove 7 and the length (L23a) is set to be larger than the length of the welding groove 7, that is, the height (H1) of the laminated core 1.
[0035] On the left and right sides of this opening 23a in the drawing, screw holes 23b for attaching the main body 22 are formed in, for example, two locations each. The base 23 has a pressing surface 23c formed at its upper end in the drawing that is pressed by the pressing portion 40, and a block portion 23d formed at its lower end in the drawing that is supported by the support portion 30. The pressing surface 23c is formed in a position that does not overlap with the opening 23a, and as shown in a side view, the front surface side on the left side in the drawing and the back surface side on the right side in the drawing are flat.
[0036] Block portion 23d is formed, for example, in a block shape, and as shown in a side view, has through-hole 23e for passing shaft 31 through, and spring groove 23f that opens to the back side and to which a spring (not shown) is attached. This spring presses welding cover 20 in a direction away from laminated core 1. Therefore, by moving top lid 15 upward after welding is completed, welding cover 20 is opened. In other words, the attachment state to laminated core 1 is released.
[0037] Next, the operation of the above-described welding cover 20 will be described. As mentioned above, if spatter is generated during welding and adheres to the laminated core 1, it becomes necessary to remove the adhered spatter. If the scattering of spatter can be suppressed at this time, it is thought that the adhesion of spatter to the laminated core 1 can be suppressed.
[0038] However, it is possible that the heat generated during welding will cause the melted material to travel around the welding cover 20 and adhere to the laminated core 1. Furthermore, since the laminated core 1 is made up of multiple stacked core pieces 2, slight irregularities may occur within the welding groove 7, potentially forming a slight gap between the welding cover 20 and the welding groove 7. When welding is performed by MAG welding as in this embodiment, the post-sealing gas (G) may promote the movement of the melted material.
[0039] Therefore, in this embodiment, when welding the laminated core 1, the welding cover 20 having the above-described configuration is attached to the laminated core 1 in a state in which the end of the cover portion 21 contacts the surface of the welding groove 7 on the side of the welding position, as shown in Fig. 9, and in which the lower end surface 22e of the inclined portion 22b of the main body portion 22 continuously covers the welding groove 7 from the edge to the outer circumferential surface. At this time, the welding cover 20 is attached in a state in which the cover portion 21 is in close contact with the surface of the welding groove 7 by the pressing portion 40, and in which the lower end surface 22e of the main body portion 22 is in close contact with a predetermined range from the edge of the welding groove 7 to the outer circumferential surface. Note that the base portion 23 is not shown in Fig. 9 to simplify the explanation.
[0040] As a result, when welding is performed using welding torch 11, cover portion 21 prevents spatter that scatters directly from the welding position from adhering to the outer peripheral surface of laminated core 1. Even if the molten material flows around cover portion 21 due to its own weight or shielding gas (G), main body portion 22 covers the outer peripheral surface near welding groove 7, including the boundary position with welding groove 7, and therefore prevents spatter from adhering to the outer peripheral surface.
[0041] Incidentally, the welding cover 20 needs to be heat resistant because it is exposed to high temperatures during welding, but it is expected that it will wear out with repeated use. Therefore, if the entire welding cover 20 were made of, for example, a copper material, machining would be required to form it into a shape corresponding to the welding groove 7 and the outer circumferential surface, and it is expected that it would be expensive as a consumable item.
[0042] Therefore, in this embodiment, the portion of the welding cover 20 that faces the welding position, requires heat resistance, and may be worn away by heat and contact during welding, is made into a separate, replaceable cover portion 21. Furthermore, by forming the cover portion 21 into a roughly rectangular plate shape, processing of the cover portion 21 is made easy.
[0043] As a result, machining is not required, and when replacement is required, only the cover portion 21 needs to be replaced, so the welding cover 20 can be manufactured and used within a practical range as a consumable item. Furthermore, by forming the cover portion 21 from a copper material or the like, a decrease in durability is also suppressed.
[0044] According to the embodiment described above, the following effects can be obtained. The welding cover 20 is used when welding a laminated core 1 having a welding groove 7 recessed from the outer peripheral surface and extending in the stacking direction, and has a cover portion 21 that contacts the surface of the welding groove 7, and a main body portion 22 that covers a predetermined range of the outer peripheral surface on the side of the welding groove 7 while exposing the welding position formed within the welding groove 7.
[0045] As a result, when welding, by attaching welding cover 20 to laminated core 1, cover portion 21 comes into contact with the surface of welding groove 7 on the side of the welding position, and a predetermined range from the edge of welding groove 7 to the outer circumferential surface is covered by main body portion 22. This prevents spatter generated during welding from adhering to the outer circumferential surface near welding groove 7 and prevents molten material from wrapping around and adhering as spatter.
[0046] Furthermore, welding cover 20 includes main body 22 that covers the outer peripheral surface in a predetermined range including the boundary position (P) between welding groove 7 and the outer peripheral surface, and cover 21 that is detachably attached to main body 22 and contacts the surface of welding groove 7 on the side of the welding position along the stacking direction. As a result, even if cover 21 is worn down due to wear caused by heat or contact during welding, simply replacing cover 21 eliminates the need to replace main body 22 or base 23. Therefore, welding cover 20 can be manufactured and used within a practical range as a consumable item.
[0047] At this time, the cover portion 21 of the welded cover 20 is formed in a rectangular plate shape. This eliminates the need for cutting out or other processes when manufacturing the cover portion 21, thereby reducing the manufacturing cost of the cover portion 21.
[0048] Furthermore, the welding cover 20 has an inclined surface and a wall 22f on the main body 22 as a positioning structure for determining the position for attaching the cover 21. This makes it easy to position the cover 21 in the same position when replacing it, that is, to attach the cover 21 to a position where it contacts the surface of the welding groove 7.
[0049] The cover portion 21 of the welding cover 20 is made of copper, copper alloy, copper-plated, gold-plated, silver-plated, tin-plated, chrome-plated, titanium, stainless steel, or a combination of these materials, which provides heat resistance to high temperatures during welding and resistance to damage caused by collisions with scattered spatter.
[0050] Furthermore, welding cover 20 is not limited to the above-described configuration example, and other configurations are possible. For example, cover portion 21 may have a curved end on the side that contacts welding groove 7 as shown in Shape Example 1 of Fig. 10, a chamfered end on the side that contacts welding groove 7 as shown in Shape Example 2, or a pointed end on the side that contacts welding groove 7 as shown in Shape Example 3.
[0051] Even with this shape, it is possible to obtain the same effects as in the embodiment, such as being able to prevent spatter from adhering due to wraparound by contacting the surface of the welding groove 7. Furthermore, because the end portion has a relatively simple shape, it is possible to prevent an excessive increase in the processing load and manufacturing costs.
[0052] Furthermore, although the embodiment illustrates a configuration in which the cover part 21 is screwed to the main body part 22 from the welding position side, the cover part 21 may be attached to the main body part 22 from the side opposite to the welding position. This makes the surface of the cover part 21 on the welding position side flat, making it possible to prevent spatter from adhering to the screws and holes.
[0053] 11, the welding cover 20 can be configured to have a packing 50 provided on the lower end surface 22e of the main body 22. In this case, the packing 50 can be made of, for example, a fluorine-based or silicone-based rubber material. With this configuration, even if there is a small gap between the welding cover 20 and the outer peripheral surface of the laminated core 1, the gap is filled with the packing 50, thereby suppressing the adhesion of spatter to the outer peripheral surface near the welding groove 7. Note that the base 23 is not shown in FIG. 11.
[0054] 12, the welding cover 20 can be configured to include a main body 22 that is shaped to continuously cover the area from the surface of the welding groove 7 on the side of the welding position to the outer circumferential surface of the side of the welding groove 7 while exposing the welding position. That is, for example, the area from the outer circumferential surface of the side of the welding groove 7 to the position where the cover part 21 contacts the surface of the welding groove 7 in FIG. 9 of the embodiment can be covered by the bottom surface 22g of the main body 22, in other words, the area can be covered solely by the main body 22. Note that the base part 23 is not shown in FIG. 12.
[0055] This configuration also makes it possible to suppress adhesion of spatter to the outer peripheral surface near the weld groove 7. In this case, by providing a thin cover portion 21 on the surface of the main body portion 22 on the welding position side, it is also possible to suppress wear of the main body portion 22. Furthermore, a configuration in which a packing 50 is provided on the bottom surface 22g of the main body portion 22 can also be used.
[0056] Although the embodiment illustrates a laminated core 1 for a stator, the welding cover 20 can also be applied when welding an iron core for a rotor, for example. Furthermore, the laminated core 1 is not limited to those used in motors, but can also be used for generators.
[0057] Although several embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be embodied in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included within the scope and spirit of the invention, and are also included in the scope of the invention and its equivalents as defined in the claims. [Explanation of symbols]
[0058] In the drawings, 1 denotes a laminated core, 7 denotes a welding groove, 20 denotes a welding cover, 21 denotes a cover portion, 22 denotes a main body portion, 23 denotes a base portion, and 50 denotes a packing.
Claims
1. A welding cover for a laminated core used when welding a laminated core, The laminated core has weld grooves formed therein that are recessed from the outer circumferential surface and extend in the lamination direction, a main body portion covering the outer circumferential surface in a predetermined range including a boundary position between the welding groove and the outer circumferential surface; a cover portion that is detachably attached to the main body portion and contacts a surface on a side of the welding position of the weld groove along a lamination direction; A welding cover for a laminated core has a portion that contacts the surface of the weld groove, exposing the weld position formed in the weld groove, while covering a predetermined range from the edge of the weld groove to the outer peripheral surface to the side of the weld groove with the main body in contact.
2. 2. A welded cover for a laminated core according to claim 1, wherein said body portion is provided with a positioning structure for determining a position for attaching said cover portion.
3. 3. The welded cover for a laminated core according to claim 1 or 2, wherein the cover portion is formed from a copper material, a copper alloy material, a copper-plated material, a gold-plated material, a silver-plated material, a tin-plated material, a chrome-plated material, a titanium material, a stainless steel material, or a combination of these materials.
4. 4. The weld cover for a laminated core according to claim 1, further comprising a packing provided at a portion covering the outer peripheral surface on the side of the weld groove for sealing a gap between the outer peripheral surface and the portion.
5. 5. The weld cover for a laminated core according to claim 1, which continuously covers from the surface of the weld groove to the outer peripheral surface on the side of the weld groove while exposing the weld position.
Citation Information
Patent Citations
The stator of rotary electric machine
JP1979171107U
JP1989118878U
JP1991047666U
Stacked stator core and manufacturing method therefor
JP2011087386A
Iron core and method for manufacturing the same
JP2019106813A