Measuring device and method for determining when to replace glass responsive membrane
The measuring device uses membrane resistance and temperature monitoring to determine the optimal replacement time for glass response membranes in hydrofluoric acid systems, enhancing accuracy and reducing replacement frequency.
Patent Information
- Application Number
- JP2022527559
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-05-29
- Filing Date
- 2021-04-09
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2041-04-09
AI Technical Summary
Existing pH meters using glass response membranes in hydrofluoric acid-containing wastewater systems fail to accurately determine when to replace the membranes due to variable acid concentration and environmental conditions, leading to premature or delayed replacement.
A measuring device that monitors the membrane resistance value and environmental temperature to provide a replacement index, using calibration curves and threshold values to determine the optimal time for membrane replacement.
Accurately determines the lifespan of glass response membranes in hydrofluoric acid environments, reducing unnecessary replacements and minimizing measurement anomalies.
Smart Images

Figure 0007580460000001 
Figure 0007580460000002 
Figure 0007580460000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a measuring device and a method for determining when to replace a glass responsive membrane. [Background technology]
[0002] When hydrofluoric acid is contained in wastewater from semiconductor factories, it is necessary to neutralize the hydrofluoric acid before discharging the wastewater into the environment. For this reason, a pH meter is placed in the flow path through which such liquid flows to constantly monitor the pH of the wastewater. A glass electrode with a glass response membrane is generally used as a pH meter. The glass response membrane becomes thinner and thinner as it is dissolved by hydrofluoric acid, and eventually dissolves completely (a hole appears).
[0003] Even if the glass responsive membrane melts and becomes thinner, it can be used for measurements without any problems until a hole appears and the internal liquid comes into contact with the liquid sample to be measured. Therefore, there is a problem that it is not realized that the glass responsive membrane needs to be replaced until a hole appears in the glass responsive membrane and measurements become impossible. In addition, because the concentration of hydrofluoric acid contained in wastewater and the like is not constant even in the same location, it is difficult to uniformly estimate the lifespan of the responsive glass membrane from the thickness of the glass, etc., and then replace the responsive glass membrane. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-072714 A Summary of the Invention [Problem to be solved by the invention]
[0005] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to determine the time to replace a responsive glass film used to measure a sample containing hydrofluoric acid. The inventors noticed that there is a relationship between the thickness of the glass response membrane and the resistance value of the glass response membrane, in that the greater the thickness, the greater the resistance value, and came up with the idea of determining when to replace the glass response membrane based on the membrane resistance value of the glass response membrane. In addition, considering that the resistance value of the glass response membrane changes depending on the temperature of the environment in which the glass response membrane is placed, we considered using the temperature of the environment in which the glass response membrane is placed to determine when to replace the glass response membrane. [Means for solving the problem]
[0006] That is, the measuring device of the present invention is a measuring device for measuring the hydrogen ion concentration of a liquid sample containing hydrofluoric acid, and is characterized in that it comprises a glass electrode having a glass responsive membrane for measuring the hydrogen ion concentration in the liquid sample, a membrane resistance measuring unit for measuring the membrane resistance value of the glass responsive membrane, a temperature measuring unit for measuring the temperature of the environment in which the glass responsive membrane is placed, and an output unit for outputting an exchange index for replacing the glass responsive membrane based on the membrane resistance value and the temperature.
[0007] With such a measuring device, even if the hydrofluoric acid concentration or temperature of the environment in which the responsive glass film is placed is not constant, it is possible to determine the time to replace the responsive glass film. As a result, even when continuously measuring the hydrogen ion concentration of a liquid sample containing hydrofluoric acid, it is possible to reduce the time and cost required to frequently replace the responsive glass membrane by overestimating its lifespan, and to reduce the risk of sudden measurement abnormalities.
[0008] In order to save the user the trouble of determining when to replace the glass response film, it is preferable to further comprise a determination unit that determines the time to replace the glass response film based on the film resistance value and the temperature.
[0009] A specific embodiment of the present invention includes, for example, converting the film resistance value into a film resistance value at a predetermined temperature based on the temperature, and determining the time to replace the glass response film based on this converted value.
[0010] It is preferable that the measurement device further includes a storage unit that stores a correlation between the film resistance value and the temperature measured by the temperature measurement unit.
[0011] The storage section may further store a correlation between a composition of the glass responsive film and the film resistance value.
[0012] In order to make it easier for the user to notice when it is time to replace the glass responsive membrane, it is preferable to issue a warning when the converted value falls below a preset threshold value.
[0013] In order to reduce the frequency of replacement of the glass responsive film, it is preferable to make the glass responsive film less soluble in hydrofluoric acid, for example by containing one or more elements selected from the group consisting of scandium, yttrium, titanium, zirconium, hafnium, niobium, and tantalum. Effect of the Invention
[0014] According to the present invention, it is possible to determine the time to replace a glass responsive membrane used to measure a liquid sample containing hydrofluoric acid, and therefore in cases where it is necessary to constantly monitor the pH of a liquid sample containing hydrofluoric acid, the frequency of replacing the glass responsive membrane can be reduced compared to the conventional method. [Brief description of the drawings]
[0015] [Figure 1] 1 is a schematic diagram showing an entire measuring device according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a schematic diagram showing a glass responsive membrane and its surrounding area according to the embodiment. [Diagram 3] 1 is a graph showing changes in the film resistance value (actual measured value) of a glass responsive film. [Figure 4]4 is a graph showing the relationship between the film resistance value and temperature of a glass responsive film. [Diagram 5] 11 is a graph showing changes in film resistance value after temperature correction. [Explanation of symbols]
[0016] 1. Measurement equipment 2. Glass electrode 21. Glass responsive membrane 3...Reference electrode 6. Film resistance measurement section 7...Temperature measurement section 8... Judgment section 9...Storage section S: Liquid sample DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The measuring device 1 according to this embodiment is disposed in a wastewater flow path from a semiconductor factory or the like that may contain hydrofluoric acid, for example, as shown in FIG. 1, and monitors whether the hydrofluoric acid is being appropriately neutralized by continuously measuring the hydrogen ion concentration in the wastewater.
[0018] Specifically, the measuring device 1 includes a glass electrode 2 equipped with a glass response membrane, a reference electrode 3 used together with the glass electrode 2, a calculation unit 4 that calculates an ion concentration by measuring the potential difference output from the glass electrode and the reference electrode, and a display unit 5 that displays the ion concentration calculated by the calculation unit 4. The calculation unit 4 is configured using a computer having, for example, a CPU, a memory, an input / output interface, an AD converter, etc.
[0019] The glass electrode 2 and the reference electrode 3 are arranged so as to be immersed in the liquid sample S flowing through the aforementioned drainage flow path P. In this embodiment, as shown in Figures 1 and 2, a composite electrode in which the glass electrode 2 and the reference electrode 3 are integrally formed is used.
[0020] The glass electrode 2 includes, for example, an internal liquid, a housing for containing the internal liquid, an internal electrode provided so as to be immersed in the internal liquid, and a glass responsive membrane 21 disposed between the internal liquid and a liquid sample. In this embodiment, as shown in Fig. 2, a chip-replaceable glass responsive membrane 21 is used in which the glass responsive membrane 21 is attached to a separate member that is detachable from the housing, and the member is screwed into, for example, a screw hole formed in the housing to fix the glass responsive membrane 21.
[0021] The comparative electrode 3 includes, for example, an internal liquid, a housing that contains the internal liquid, an internal electrode that is provided so as to be immersed in the internal liquid, and a liquid junction 31 that electrically connects the internal liquid and the liquid sample. The liquid junction 31 is formed, for example, of a ceramic plate or the like that is disposed inside a through-hole formed in the housing. In this embodiment, the liquid junction 31 is also a chip-replaceable liquid junction 31 that is attached to a separate member that is detachable from the housing, and that is fixed by screwing the member together with the liquid junction 31 into, for example, a screw hole formed in the housing.
[0022] The measuring device 1 of this embodiment further includes a film resistance measuring unit 6 that measures the film resistance value of the glass responsive film 21, a temperature measuring unit 7 that measures the temperature of the environment in which the glass responsive film 21 is placed, and a judgment unit 8 that judges when to replace the glass responsive film based on the film resistance value measured by the film resistance measuring unit 6 and the temperature measured by the temperature measuring unit 7.
[0023] The film resistance measuring unit 6 includes an insulation resistance meter 61 that measures the electrical resistance of the glass responsive film 21, and a film resistance calculation unit. The insulation resistance meter 61 includes a conductive material such as a platinum wire that is immersed in the liquid sample S in the same manner as the glass electrode 2. The film resistance calculation unit includes a voltmeter that detects the voltage between the conductive material and the inner electrode of the glass electrode via the glass responsive film when a current is passed through the conductive material, and calculates the resistance value of the glass responsive film based on the voltage value detected by the voltmeter. Alternatively, the film resistance calculation unit includes an ammeter that detects the current that flows between the conductive material and the inner electrode of the glass electrode via the glass responsive film when a voltage is applied to the conductive material, and calculates the resistance value of the glass responsive film based on the current value detected by the ammeter. In this embodiment, the calculation unit 4 also functions as a membrane resistance calculation unit.
[0024] The temperature measurement unit 7 includes a temperature sensor 71 and a temperature calculation unit. In this embodiment, the temperature sensor 71 is provided near the glass responsive membrane 21 of the glass electrode 2 to measure the temperature of the liquid sample S near the glass responsive membrane 21. In this embodiment, the calculation unit 4 also functions as the temperature calculation unit.
[0025] When the thickness of the glass responsive membrane 21 decreases, the membrane resistance value of the glass responsive membrane 21 decreases. The judgment unit 8 is configured to utilize this relationship and judge that it is time to replace the glass responsive membrane 21 when the membrane resistance value of the glass responsive membrane 21 measured by the membrane resistance measurement unit 6 becomes smaller than a preset threshold value.
[0026] The threshold value is preset according to the composition of the glass responsive film 21, for example, by referring to past measurement data, and may be, for example, an average film resistance value 24 hours before the glass responsive film 21 melts and develops a hole, based on the past measurement data. The measuring device 1 may further include a memory unit 9 for storing the threshold value.
[0027] In addition to the threshold value, the storage unit 9 may store, for example, an equation or a table showing the correlation between the film resistance value and the temperature.
[0028] Another factor that affects the degree of dissolution of the glass-responsive film 21 is, for example, the composition of the glass-responsive film 21. Specifically, by making the glass-responsive film 21 contain one or more elements selected from, for example, scandium, yttrium, titanium, zirconium, hafnium, niobium, and tantalum, it is possible to suppress the degree of dissolution (dissolution rate) by hydrofluoric acid to a lower level compared to the glass-responsive film 21 that does not contain these elements. The mechanism by which the hydrofluoric acid resistance is improved by adding these elements is thought to be as follows. Trivalent rare earth elements such as scandium or yttrium have a higher electronegativity than lanthanoids such as lanthanum (La) that are added to tighten the glass mesh network of the glass responsive film. Therefore, by replacing a part of the lanthanoids contained in the glass responsive film with trivalent rare earth elements such as scandium or yttrium, the glass network can be tightened and strengthened. As a result, it is believed that the hydrofluoric acid resistance of the glass responsive film is improved. Tetravalent elements such as titanium, zirconium, and hafnium have a larger ionic radius than the main elements such as silicon that form the glass network. Therefore, these elements have a larger oxygen coordination number and stronger bond strength with oxygen than silicon, etc. For this reason, it is believed that the addition of these elements strengthens the glass network and improves the hydrofluoric acid resistance of the glass responsive film. Pentavalent elements such as tantalum and niobium have a larger number of bonds (5 bonds) than silicon, the main element that forms the glass network (4 bonds). Therefore, by adding these elements, the glass network is cross-linked and strengthened, which is thought to contribute to improving the hydrofluoric acid resistance of the glass responsive film.
[0029] In this way, it is considered that the dissolution speed by hydrofluoric acid varies depending on the composition of the glass responsive film 21. Therefore, the storage unit 9 may store an equation or a table expressing the correlation between the composition of the glass responsive film 21 and the film resistance value.
[0030] When the membrane resistance value becomes equal to or smaller than the threshold value, the thickness of the glass responsive membrane 21 becomes small, and it can be predicted that a hole will be formed in the glass responsive membrane 21 within 24 hours, for example. Therefore, the measuring device 1 according to this embodiment further includes an output unit that outputs a warning when the determining unit 8 determines that the membrane resistance value becomes equal to or smaller than the threshold value. The display unit 5 may also function as the output unit.
[0031] The procedure and method for determining the time to replace the glass responsive membrane 21 using the measuring device 1 configured in this manner are as follows. The film resistance value of the responsive glass film 21 is measured by the film resistance measuring unit 6. An example of the film resistance value of the responsive glass film 21 measured by the film resistance measuring unit 6 is shown in FIG. 3. The graph in FIG. 3 shows the results of using two Horiba Advanced Techno hydrofluoric acid resistant pH electrodes (product number 7123) and measuring the film resistance value of the responsive glass film 21 of these electrodes with an insulation resistance meter (Agilent 433913) twice a day for about 125 hours. The graph in FIG. 3 shows that the film resistance value fluctuates greatly from measurement to measurement. From such a graph waveform with large fluctuations, it is difficult to estimate the period until the responsive glass film 21 melts and develops a hole (the lifespan of the responsive glass film) and to determine when to replace the responsive glass film 21.
[0032] In order to investigate the cause of the large fluctuations in the film resistance value in the graph of Fig. 3, a certain day in the graph is taken as an example. The first measurement on this day was taken at 9 am, and the temperature of the measurement environment at this time was 19.5°C. The second measurement on the same day was taken at 5 pm, and the temperature of the measurement environment at this time was 22.8°C. From this, the inventors considered that such a large fluctuation in the graph waveform was caused by the temperature around the glass responsive film 21 changing for each measurement.
[0033] Therefore, the inventor attempted to use the temperature measurement unit 7 to measure the environment in which the glass responsive membrane 21 is placed, for example the temperature of the liquid sample S around the glass responsive membrane 21, at the same time as measuring the membrane resistance value, and to correct the membrane resistance value using the measured temperature.
[0034] The present inventors have investigated the relationship between the film resistance value of the responsive glass film 21 and temperature, and as a result, for example, for the responsive glass film 21 used in the above-mentioned hydrofluoric acid-resistant pH electrode (product number 7123) manufactured by Horiba Advanced Techno, obtained a calibration curve showing the correlation between the film resistance value and temperature as shown in Fig. 4. This calibration curve was obtained from the results of measuring the film resistance value of the responsive glass film 21 at each temperature using three identical glass electrodes 2. The black circles in Fig. 4 represent the average film resistance values of the three glass electrodes 2.
[0035] Therefore, by using this calibration curve to temperature-correct the film resistance value in the graph of Fig. 3 and converting it into a film resistance value at a predetermined temperature (e.g., 25°C), for example, a graph like Fig. 5 was obtained. In the graph of Fig. 5, the fluctuation of the film resistance value is suppressed by correcting the change in the film resistance value due to temperature, and a graph waveform that makes it easy to estimate the lifespan of the glass responsive film 21 can be obtained.
[0036] Therefore, in this embodiment, the determination unit 8 performs temperature correction on the film resistance value measured by the film resistance measurement unit 6, for example, as shown in Fig. 5, using a calibration curve or the like stored in the memory unit 9. Furthermore, the determination unit 8 compares the corrected film resistance value with a threshold value stored in the memory unit 9 and determines whether the film resistance value after temperature correction is equal to or smaller than the threshold value, thereby determining whether it is time to replace the glass response film 21.
[0037] In this embodiment, the threshold value stored in the memory unit 9 is set based on the membrane resistance value of a glass responsive membrane 21 of the same composition whose membrane resistance was measured in the past on the same drainage flow path P as described above, for example, by referring to the membrane resistance value at the time when a hole was developed in the glass responsive membrane 21 after 24 hours and it became unusable.
[0038] For glass response membranes 21 having a different composition, a calibration curve for the composition of the glass response membrane 21 can be further created, and the judgment unit 8 can further correct the film resistance value after temperature correction based on this calibration curve, thereby making it possible to more accurately determine the time to replace the glass response membrane.
[0039] In this embodiment, when the judgment unit 8 judges that it is time to replace the glass response membrane 21, the output unit issues a warning to the user as an indication for replacing the glass response membrane, for example, to urge the user to replace the glass response membrane 21.
[0040] According to the measuring device 1 and the method for determining when to replace a glass responsive membrane configured in this manner, the time to replace the glass responsive membrane 21 is determined not only based on the membrane resistance value of the glass responsive membrane 21 but also on the temperature of the environment in which the glass responsive membrane 21 is placed. Therefore, even if the temperature of the environment in which the glass responsive membrane 21 is placed is not constant, the time to replace the glass responsive membrane 21 can be accurately determined. As a result, even when continuously measuring the hydrogen ion concentration of a liquid sample S containing hydrofluoric acid, it is possible to save the trouble and cost of frequently replacing the glass responsive membrane 21 by overestimating the usage period of the glass responsive membrane 21.
[0041] Since the memory unit 9 stores equations and tables that express the correlation between the composition of the glass response film 21 and the film resistance value, the time to replace the glass response film 21 can be determined more accurately based on the composition of the glass response film 21.
[0042] The present invention is not limited to the above-described embodiment. For example, the judgment unit may be made to use machine learning to learn data on previously measured film resistance values, and to predict trends in changes in film resistance values depending on the time of day or the day of the week, and to estimate the time until the glass responsive film dissolves and a hole is formed based on the predicted trends.
[0043] For example, the dissolution rate of the glass-responsive film may be calculated from the slope of a graph of the corrected film resistance value as shown in FIG. 5, and the replacement time may be predicted from the calculated dissolution rate and a preset threshold value.
[0044] In the above-described embodiment, a method of correcting the film resistance value using a calibration curve that represents the correlation between the composition of the glass response film and the film resistance value has been described. However, the present invention is not limited to this method, and the threshold value may be set using an equation or table that represents the correlation between the composition of the glass response film and the threshold value.
[0045] The threshold can be set for various time spans depending on the environment in which the measurement device is used, such as when a hole appears in the glass responsive membrane after 24 hours, but also when a hole appears after a few hours or after two days. In the above embodiment, the case where the threshold value is set for each composition of the glass responsive film has been described, but the threshold value may be set regardless of the composition of the glass responsive film.
[0046] In the above embodiment, the film resistance value was converted into a resistance value at a predetermined temperature. However, the predetermined temperature may be converted into, for example, an average value of temperatures measured by a temperature measuring unit over a predetermined period of time.
[0047] In the above embodiment, the determination unit of the measuring device determines the time to replace the glass response membrane based on the membrane resistance value and temperature of the glass response membrane, but the user (person) may determine the time to replace the glass response membrane. For example, the output unit of the measuring device may be configured to output a replacement index for determining the time to replace the glass response membrane, such as displaying the replacement index on a screen. In this case, the replacement index may be the membrane resistance value and the temperature, and may further include their threshold values. With such a configuration, the user (person) can determine the time to replace the glass response membrane based on the output replacement index.
[0048] In the above-mentioned embodiment, a glass response membrane that is detachable from the housing is used, and only the glass response membrane is replaced, but this is not limited to the above, and a glass electrode in which the glass response membrane and the housing are integrally formed may be used, and the entire glass electrode may be replaced when replacing. In this case, instead of a composite electrode in which the glass electrode and the reference electrode are integrated, the glass electrode and the reference electrode may be provided separately.
[0049] Depending on the type of glass responsive membrane used, the glass responsive membrane may be colored. In the case of a colored glass responsive membrane, it is thought that the color will also become lighter when the glass responsive membrane is dissolved by hydrofluoric acid and the thickness is reduced. Specifically, it can be created by intentionally adding colored elements such as lanthanoid elements such as Ce, Nd, Pr, and Er, transition metal elements such as Ni and Cu, and elements with mixed valence such as V, Ti, Cr, and Mn to the composition of the glass responsive membrane. In particular, the lanthanoid elements reduce resistance and improve water resistance and responsiveness, so it is possible to create a glass responsive membrane by replacing part of the added La, which is an essential element of the glass responsive membrane, with these elements. Therefore, a color monitoring unit may be further provided that measures the spectral reflectance of the glass responsive film and monitors the chromaticity of the glass responsive film, and the time to replace the glass responsive film may be determined based on the chromaticity as well as the film resistance value described above. The time to replace the glass responsive film may be estimated not only by a device for monitoring the chromaticity but also by a human visual inspection during maintenance, by comparing the color with a color sample prepared in advance. As a specific method of judgment, for example, a threshold value may be set in advance for the chromaticity of the glass response membrane for each type of glass response membrane, and if the chromaticity falls below the threshold value, the judgment unit may judge that the glass response membrane needs to be replaced. Furthermore, the film resistance may be further corrected based on the chromaticity using an equation or table that expresses the correlation between the film resistance and chromaticity, or the chromaticity may be used as an index independent of the film resistance, and it may be determined that it is time to replace the glass response film when, for example, either the film resistance or the chromaticity falls below a threshold value.
[0050] In addition, various modifications and combinations of the embodiments may be made as long as they do not go against the spirit of the present invention. [Industrial Applicability]
[0051] According to the present invention, it is possible to determine the time to replace a glass responsive membrane used to measure a liquid sample containing hydrofluoric acid, and therefore in cases where it is necessary to constantly monitor the pH of a liquid sample containing hydrofluoric acid, the frequency of replacing the glass responsive membrane can be reduced compared to the conventional method.
Claims
1. A measurement device for measuring a hydrogen ion concentration of a liquid sample containing hydrofluoric acid, comprising: a glass electrode having a glass responsive membrane for measuring a hydrogen ion concentration in the liquid sample; A membrane resistance measuring unit for measuring a membrane resistance value of the glass responsive membrane; A temperature measuring unit that measures the temperature of the environment in which the glass responsive film is placed; an output unit that outputs a replacement index for replacing the glass response film based on the film resistance value and the temperature; A determination unit that determines when to replace the glass response film based on the film resistance value and the temperature, The measuring device according to claim 1, wherein the determining unit further uses a correlation between a composition of the glass responsive film and the film resistance value when determining the time to replace the glass responsive film.
2. The measuring device described in Claim 1, characterized in that the judgment unit converts the film resistance value into a film resistance value at a predetermined temperature based on the temperature, and judges the time to replace the glass response film based on this converted value.
3. 3. The measuring device according to claim 1, further comprising a storage unit that stores a correlation between the film resistance value and the temperature measured by the temperature measuring unit.
4. 4. The measuring device according to claim 3, wherein the memory section further stores a correlation between the composition of the glass responsive film and the film resistance value.
5. 3. The measuring device according to claim 2, wherein a warning is issued when the converted value falls below a preset threshold value.
6. 6. The measuring device according to claim 1, wherein the responsive glass film contains one or more elements selected from the group consisting of scandium, yttrium, titanium, zirconium, hafnium, niobium, and tantalum.
7. A measuring device as described in any one of claims 1 to 6, characterized in that the judgment unit judges the time to replace the glass response film based on the chromaticity or color of the glass response film in addition to the correlation between the film resistance value, the temperature, and the composition of the glass response film and the film resistance value.
8. A method for determining when to replace a glass response membrane of a glass electrode for measuring a hydrogen ion concentration in a liquid sample containing hydrofluoric acid, comprising: Measure the film resistance of the glass responsive film; measuring the temperature of the environment in which the glass responsive membrane is located; When determining the time to replace the glass response film based on the film resistance value and the temperature, The method for determining the time to replace a glass responsive film further comprises using a correlation between the composition of the glass responsive film and the film resistance value.
Citation Information
Patent Citations
glass
JP1984162147A
Ph meter with self-diagnosing function
JP1985205345A
Method and apparatus for detecting crack generated at detecting end of measuring instrument for ph or the like
JP1987261950A
Ph meter with life-prediction display