Gas Sensor Element
The gas sensor element's through hole design with a recessed inner wall surface improves adhesion, preventing moisture-induced peeling and structural damage, ensuring durability by eliminating gaps between ceramic layers and conductive materials.
Patent Information
- Application Number
- JP2022048059
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-03-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-03-24
AI Technical Summary
Gas sensor elements experience peeling due to gaps between the inner circumferential surface of through holes and conductor portions, which allow moisture to reach the heat generating part, leading to structural damage from pressure increases caused by evaporating water vapor.
The gas sensor element incorporates a through hole design with a recessed inner wall surface that enhances adhesion between the ceramic layer and conductive material, preventing gaps and reducing the likelihood of peeling by ensuring the conductive paste fills the recessed area effectively.
This configuration significantly reduces the occurrence of peeling and structural damage by minimizing gaps, thereby enhancing the durability and reliability of the gas sensor element.
Smart Images

Figure 0007581274000003 
Figure 0007581274000004 
Figure 0007581274000005
Abstract
Description
[Technical field]
[0001] The present invention relates to a gas sensor element. [Background technology]
[0002] Conventionally, gas sensors that measure gas components in a measurement gas such as an automobile exhaust gas are known. The gas sensor has a gas sensor element that includes, for example, a plurality of laminated ceramic layers and a detection part formed on one side in the longitudinal direction. In such a gas sensor element, a heater layer including a heat generating part is formed between the ceramic layers. Conductive parts such as a current-carrying terminal of the heat generating part and a detection electrode may be provided on one side and the other side of one or more ceramic layers. For this reason, a through hole is formed in the ceramic layer to electrically connect these conductive parts in the thickness direction.
[0003] Patent Document 1 discloses a gas sensor element including a first ceramic layer having a first through hole formed therein and a second ceramic layer having a second through hole formed therein, laminated on the first ceramic layer. In this gas sensor element, a first conductor is formed on the inner peripheral surface of the first through hole, and a second conductor is formed on the inner peripheral surface of the second through hole, so that electrical contact is achieved between the first conductor and the second conductor. Patent Document 2 discloses a gas sensor element including a through hole penetrating the front and back surfaces, and a ceramic sheet having a conductive pattern that electrically connects the front and back surfaces. In this gas sensor element, an insulating paste is printed on the inner wall surface of the through hole, and a conductive layer paste is printed thereon so that the front and back surfaces are electrically connected. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2008-046112 A [Patent Document 2] Patent No. 4421756 Summary of the Invention [Problem to be solved by the invention]
[0005] The gas sensor element having the configuration disclosed in Patent Document 1 may have a gap between the inner circumferential surface of the through hole and the conductor. When liquid components such as moisture present in this gap move through the heater layer to reach the heat generating part and its vicinity, and evaporate due to the heat of the heat generating part to become water vapor, etc., the pressure increases locally. This may cause peeling in the internal structure of the gas sensor element, leading to damage to the gas sensor element. This also applies to the gas sensor element having the configuration disclosed in Patent Document 2. In other words, the liquid components present between the inner circumferential surface of the through hole and the insulating paste may move through the insulating paste and heater layer to reach the heat generating part and its vicinity, evaporate with the rise in the surrounding temperature, and the pressure may increase locally, causing similar peeling. In this way, when the ceramic forming the inner circumferential surface of the through hole and the member printed on the inner circumferential surface or filled in the through hole are made of different materials, if a gap occurs between the two, moisture that may cause peeling may enter there, leading to damage to the gas sensor element.
[0006] In one aspect, the present invention has been made in consideration of the above circumstances, and its object is to provide a gas sensor element in which gaps are unlikely to occur between the inner wall surface of the through hole formed in the ceramic layer and the material in contact therewith. [Means for solving the problem]
[0007] In order to solve the above-mentioned problems, the present invention employs the following configuration.
[0008] The gas sensor element according to the first aspect of the present invention includes a heating portion and a ceramic layer. The ceramic layer has a first surface and a second surface opposite to the first surface, and is configured to be heated by the heating portion. The ceramic layer has a through hole penetrating the ceramic layer in a thickness direction from the first surface to the second surface, and forming a through hole for electrically connecting the first surface side and the second surface side. The through hole is defined by a first inner wall surface extending in the thickness direction, and a second inner wall surface that is continuous with the first inner wall surface and defines a recess recessed toward the inside of the ceramic layer from the first inner wall surface. When the thickness of the ceramic layer is 1, the length of the first inner wall surface to the innermost position of the recess based on the position closest to the central axis of the through hole is 0.05 to 0.20.
[0009] According to the first aspect, a recess is formed in a through hole for a through hole penetrating the ceramic layer in the thickness direction, the recess having a recess recessed toward the inside of the ceramic layer. The maximum depth of the recess, based on the position closest to the central axis of the through hole, is set to 0.05 to 0.20 with respect to the thickness of the ceramic layer. This improves the adhesion between the first and second inner wall surfaces of the ceramic that define the through hole and the different material when the through hole is formed by the ceramic layer and a different material, making it difficult for gaps to occur between them.
[0010] A gas sensor element according to a second aspect of the present invention is the gas sensor element according to the first aspect, wherein when a thickness of the ceramic layer is defined as 1, a length of the first inner wall surface from a position closest to a central axis of the through hole to an innermost position of the recess is not less than 0.10 and not more than 0.20.
[0011] A gas sensor element according to a third aspect of the present invention is the gas sensor element according to the first or second aspect, wherein the second inner wall surface is continuous around the entire circumference of the through hole, and the recess is defined by the second inner wall surface so as to be annular when viewed from the first surface side.
[0012] According to a third aspect, the recess is formed so as to continue over the entire circumference around the central axis of the through hole, which can further improve the adhesion between the ceramic and the different material.
[0013] A gas sensor element according to a fourth aspect of the present invention is the gas sensor element according to any one of the first aspect to the third aspect, wherein the second inner wall surface is present at least one of a position biased toward the first surface side and a position biased toward the second surface side in the thickness direction.
[0014] A gas sensor element according to a fifth aspect of the present invention is the gas sensor element according to any one of the first to fourth aspects, wherein the second inner wall surface is present in a plurality of portions along the thickness direction.
[0015] A gas sensor element according to a sixth aspect of the present invention is the gas sensor element according to any one of the first to fifth aspects, further comprising a conductive portion having electrical conductivity and formed so as to fill the inside of the through hole.
[0016] A gas sensor element according to a seventh aspect of the present invention is the gas sensor element according to any one of the first to sixth aspects, wherein the heat generating portion is disposed on the first surface side of the ceramic layer, and the through hole electrically connects the heat generating portion and an element on the second surface side of the ceramic layer.
[0017] A gas sensor element according to an eighth aspect of the present invention is the gas sensor element according to any one of the first to seventh aspects, and is configured to measure a concentration of nitrogen oxides in a measurement gas. Effect of the Invention
[0018] According to the present invention, a gas sensor element is provided in which gaps are unlikely to occur between the inner wall surface of the through hole formed in the ceramic layer and a different material in contact therewith, and therefore peeling is unlikely to occur in the internal structure. [Brief description of the drawings]
[0019] [Figure 1]FIG. 1 is a schematic cross-sectional view illustrating a configuration of a sensor element according to an embodiment. [Diagram 2] FIG. 2 is a schematic diagram showing an example of a schematic planar arrangement of a heat generating portion and its surroundings. [Diagram 3] FIG. 13 is a schematic diagram showing another example of a schematic planar arrangement of a heat generating portion and its surroundings. [Figure 4] FIG. 4 is a partial cross-sectional view of a lead portion according to one embodiment. [Diagram 5] FIG. 4 is a partial cross-sectional view of the periphery of a through hole according to one embodiment. [Figure 6] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to another embodiment. [Figure 7A] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a modified example. [Figure 7B] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a modified example. [Figure 7C] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a modified example. [Figure 7D] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a modified example. [Figure 7E] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a modified example. [Figure 8] FIG. 11 is a partial cross-sectional view of the periphery of a through hole according to a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] An embodiment according to one aspect of the present invention (hereinafter, also referred to as "the present embodiment") will be described below with reference to the drawings. However, the present embodiment described below is merely an example of the present invention in every respect. It goes without saying that various improvements and modifications can be made without departing from the scope of the present invention. In other words, in implementing the present invention, a specific configuration according to the embodiment may be appropriately adopted. Note that the components shown in each figure may be shown in a deformed form for the convenience of explanation, and do not necessarily represent the actual size relationship of each component.
[0021] 1. Configuration of gas sensor element FIG. 1 is a schematic cross-sectional view showing an example of the configuration of the gas sensor element 100 according to the present embodiment. The gas sensor element 100 has, for example, a long and narrow plate shape extending along the longitudinal direction, and is formed, for example, in a rectangular parallelepiped shape. The gas sensor element 100 shown in FIG. 1 has a front end and a rear end as ends in the longitudinal direction, and in the following description, the front end is the end on the left side of FIG. 1, and the rear end is the end on the right side of FIG. 1. As shown in FIG. 1, the direction from the front to the back of the paper is the left-right direction of the gas sensor element 100. However, the shape of the gas sensor element 100 is not limited to this example, and may be appropriately selected depending on the embodiment. The orientation of the gas sensor element 100 during use is not limited to the orientation specified in FIG. 1.
[0022] The gas sensor element 100 has a structure in which six layers, a first substrate layer 1, a second substrate layer 2, a third substrate layer 3, a first solid electrolyte layer 4, a spacer layer 5, and a second solid electrolyte layer 6, which are made of solid electrolyte layers, are laminated in this order from the bottom in the cross-sectional view of FIG. 1. That is, the gas sensor element 100 includes a laminated body made of the first solid electrolyte layer 4, the second solid electrolyte layer 6, and the spacer layer 5. The solid electrolytes forming the six layers, the first substrate layer 1, the second substrate layer 2, the third substrate layer 3, the first solid electrolyte layer 4, the spacer layer 5, and the second solid electrolyte layer 6, may be dense. The term "dense" refers to a porosity of 5% or less.
[0023] The gas sensor element 100 is manufactured, for example, by performing processes such as predetermined processing and printing of wiring patterns on ceramic green sheets corresponding to each layer, stacking them, and further firing them to integrate them. As an example, the gas sensor element 100 is a laminate of a plurality of ceramic layers. Hereinafter, the layers 1 to 6 may be referred to as "ceramic layers" without distinguishing between them. In this embodiment, the upper surface of the second solid electrolyte layer 6 constitutes the upper surface of the gas sensor element 100, the lower surface of the first substrate layer 1 constitutes the lower surface of the gas sensor element 100, and each side surface of the layers 1 to 6 constitutes each side surface of the gas sensor element 100.
[0024] [Measurement gas flow section] At the front end side of the gas sensor element 100, between the lower surface of the second solid electrolyte layer 6 and the upper surface of the first solid electrolyte layer 4, a gas inlet 10, a first diffusion rate-controlling section 11, a buffer space 12, a second diffusion rate-controlling section 13, a first internal void 20, a third diffusion rate-controlling section 30, a second internal void 40, a fourth diffusion rate-controlling section 16, and a third internal void 17 are formed adjacent to each other and communicated with each other in this order.
[0025] The gas inlet 10, the buffer space 12, the first internal space 20, the second internal space 40, and the third internal space 17 are spaces provided by hollowing out the spacer layer 5, and are spaces (internal spaces) within the gas sensor element 100 that are bounded at the top by the underside of the second solid electrolyte layer 6 and at the bottom by the upper surface of the first solid electrolyte layer 4.
[0026] The first diffusion rate-controlling portion 11 is provided as two horizontally elongated slits (the opening has a long side direction perpendicular to the drawing). The second diffusion rate-controlling portion 13, the third diffusion rate-controlling portion 30, and the fourth diffusion rate-controlling portion 16 are each provided as a hole whose length extending in the direction perpendicular to the drawing is shorter than that of the first internal space 20, the second internal space 40, and the third internal space 17, respectively.
[0027] As illustrated in FIG. 1, the second diffusion rate-controlling section 13, the third diffusion rate-controlling section 30, and the fourth diffusion rate-controlling section 16 may be provided as two horizontally elongated slits (the opening has a long side direction perpendicular to the drawing) like the first diffusion rate-controlling section 11, but are not limited thereto. For example, the fourth diffusion rate-controlling section 16 may be provided as one horizontally elongated slit (the opening has a longitudinal direction perpendicular to the drawing) formed as a gap with the lower surface of the second solid electrolyte layer 6. That is, the fourth diffusion rate-controlling section 16 may be in contact with the upper surface of the first solid electrolyte layer 4. The second diffusion rate-controlling section 13, the third diffusion rate-controlling section 30, and the fourth diffusion rate-controlling section 16 will be described later. The portion (internal space) from the gas inlet 10 to the third internal space 17 is referred to as the measurement gas flow section 7.
[0028] [Reference gas introduction space] A reference gas introduction space 43 is provided at a position farther from the front end side than the measurement gas flow section 7, between the upper surface of the third substrate layer 3 and the lower surface of the spacer layer 5, and at a position defined by the side surface of the first solid electrolyte layer 4. A reference gas such as the atmosphere is introduced into the reference gas introduction space 43. However, the configuration of the gas sensor element 100 is not limited to this example. As another example, the first solid electrolyte layer 4 may be configured to extend to the rear end of the gas sensor element 100, and the reference gas introduction space 43 may be omitted. In this case, the atmosphere introduction layer 48 may be configured to extend to the rear end of the gas sensor element 100.
[0029] [Atmospheric introduction layer] The air introducing layer 48 is made of porous alumina, and is configured so that the reference gas is introduced through the reference gas introducing space 43. In addition, the air introducing layer 48 is formed so as to cover the reference electrode 42.
[0030] [Reference electrode] The reference electrode 42 is formed so as to be sandwiched between the upper surface of the third substrate layer 3 and the first solid electrolyte layer 4, and is surrounded by an air introduction layer 48 connected to the reference gas introduction space 43. The reference electrode 42 is used to measure the oxygen concentrations (oxygen partial pressures) in the first internal space 20, the second internal space 40, and the third internal space 17. Details will be described later.
[0031] [Gas inlet] The gas inlet 10 is a portion of the measurement gas flow section 7 that opens to the external space. The measurement gas is introduced into the gas sensor element 100 from the external space through the gas inlet 10. In this embodiment, as illustrated in FIG. 1, the gas inlet 10 is disposed on the front surface of the gas sensor element 100. That is, the measurement gas flow section 7 is configured to have an opening at the front end of the gas sensor element 100. However, it is not essential that the measurement gas flow section 7 has an opening on the front surface of the gas sensor element 100, that is, that the gas inlet 10 is disposed on the front surface of the gas sensor element 100. As long as the gas sensor element 100 can introduce the measurement gas from the external space into the measurement gas flow section 7, the gas inlet 10 may be disposed on the right side surface or the left side surface of the gas sensor element 100, for example.
[0032] When the gas inlet 10 is disposed on the front surface of the gas sensor element 100, the measurement gas flow section 7 may be blocked by a dense ceramic layer on each side surface (right side surface and left side surface) of the gas sensor element 100. The ceramic layer may be made of a material such as zirconia (ZrO2). When the measurement gas flow section 7 is blocked by a dense ceramic layer on each side surface of the gas sensor element 100, the gas sensor element 100 is configured to take in the measurement gas from the external space into the gas sensor element 100 through the gas inlet 10.
[0033] However, it is not essential for the gas sensor element 100 to block the measurement gas flow portion 7 on each side of the gas sensor element 100 with a dense ceramic layer. Also, it is not essential for the gas sensor element 100 to be provided with the gas inlet 10. That is, it is sufficient for the gas sensor element 100 to be able to take in the measurement gas from the external space into the measurement gas flow portion 7, and it is not essential for the gas sensor element 100 to take in the measurement gas from the external space through the gas inlet 10. For example, the gas sensor element 100 may take in the measurement gas from the external space into the measurement gas flow portion 7 without providing the gas inlet 10 by leaving at least one of the side surfaces 59 of the spacer layer 5 open instead of being blocked by a dense ceramic layer.
[0034] [First diffusion-controlled part] The first diffusion rate-controlling portion 11 is a portion that applies a predetermined diffusion resistance to the measurement gas taken in through the gas inlet 10.
[0035] [Buffer space] The buffer space 12 is a space provided for guiding the measurement gas introduced from the first diffusion rate-controlling portion 11 to the second diffusion rate-controlling portion 13 .
[0036] [Second diffusion-controlled section] The second diffusion rate-controlling portion 13 is a portion that imparts a predetermined diffusion resistance to the measurement gas introduced from the buffer space 12 into the first internal space 20 .
[0037] When the measurement gas is introduced from the outside of the gas sensor element 100 into the first internal space 20, the measurement gas is suddenly taken into the gas sensor element 100 from the gas inlet 10 due to pressure fluctuations of the measurement gas in the external space (exhaust pressure pulsations if the measurement gas is automobile exhaust gas), but is not introduced directly into the first internal space 20, but is introduced into the first internal space 20 after the concentration fluctuations of the measurement gas are canceled through the first diffusion rate-controlling part 11, the buffer space 12, and the second diffusion rate-controlling part 13. As a result, the concentration fluctuations of the measurement gas introduced into the first internal space can be almost negligible.
[0038] [First internal space] The first internal space 20 is provided as a space for adjusting the oxygen partial pressure in the measurement gas introduced through the second diffusion rate-controlling part 13. The oxygen partial pressure is adjusted by the operation of the main pump cell 21.
[0039] [Main pump cell] The main pump cell 21 is an electrochemical pump cell including an inner pump electrode 22, an outer pump electrode 23, and a second solid electrolyte layer 6 sandwiched between these electrodes. The inner pump electrode 22 has a ceiling electrode portion 22a provided on almost the entire surface of a lower surface 62 of the second solid electrolyte layer 6 adjacent to (facing) the first internal space 20. The outer pump electrode 23 is provided in a region of an upper surface 63 of the second solid electrolyte layer 6 corresponding to the ceiling electrode portion 22a in a manner adjacent to the external space.
[0040] The inner pump electrode 22 is formed across the upper and lower solid electrolyte layers (the second solid electrolyte layer 6 and the first solid electrolyte layer 4) that define the first internal space 20, and the spacer layer 5 that provides the side walls. Specifically, a ceiling electrode portion 22a is formed on the lower surface 62 of the second solid electrolyte layer 6 that provides the ceiling surface of the first internal space 20, and a bottom electrode portion 22b is formed on the upper surface of the first solid electrolyte layer 4 that provides the bottom surface. Then, side electrode portions (not shown) are formed on the side wall surfaces (inner surfaces) of the spacer layer 5 that constitute both side wall portions of the first internal space 20 so as to be connected to the ceiling electrode portion 22a and the bottom electrode portion 22b. That is, the inner pump electrode 22 is arranged in a tunnel-shaped structure at the arrangement portion of the side electrode portion.
[0041] The inner pump electrode 22 and the outer pump electrode 23 are formed as porous cermet electrodes (for example, cermet electrodes made of Pt and ZrO2 containing 1% Au). The inner pump electrode 22, which comes into contact with the measurement gas, is used to measure nitrogen oxides (NO x ) are formed using materials that have weakened reducing ability against the components.
[0042] The gas sensor element 100 is configured to be able to pump oxygen in the first internal space 20 out to the external space or pump oxygen in the external space into the first internal space 20 by applying a desired pump voltage Vp0 between the inner pump electrode 22 and the outer pump electrode 23 in the main pump cell 21 and flowing a pump current Ip0 in a positive or negative direction between the inner pump electrode 22 and the outer pump electrode 23.
[0043] [Oxygen partial pressure detection sensor cell for main pump control] In addition, in order to detect the oxygen concentration (oxygen partial pressure) in the atmosphere in the first internal space 20, the inner pump electrode 22, the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, and the reference electrode 42 constitute an oxygen partial pressure detection sensor cell 80 for controlling the main pump (i.e., an electrochemical sensor cell).
[0044] The gas sensor element 100 is configured to be able to identify the oxygen concentration (oxygen partial pressure) in the first internal space 20 by measuring the electromotive force V0 in the main pump control oxygen partial pressure detection sensor cell 80. Furthermore, the pump current Ip0 is controlled by feedback controlling Vp0 so that the electromotive force V0 is constant. This allows the oxygen concentration in the first internal space 20 to be kept at a predetermined constant value.
[0045] [Third diffusion-controlled section] The third diffusion rate-controlling section 30 is a section that applies a predetermined diffusion resistance to the measurement gas whose oxygen concentration (oxygen partial pressure) has been controlled by the operation of the main pump cell 21 in the first internal space 20, and guides the measurement gas to the second internal space 40.
[0046] [Second internal space] The second internal space 40 is provided as a space for further adjusting the oxygen partial pressure in the measurement gas introduced through the third diffusion-controlling part 30. The oxygen partial pressure is adjusted by the operation of the auxiliary pump cell 50.
[0047] [Auxiliary pump cell] The auxiliary pump cell 50 is an auxiliary electrochemical pump cell including an auxiliary pump electrode 51, an outer pump electrode 23 (not limited to the outer pump electrode 23, but any appropriate electrode on the outside of the gas sensor element 100 will suffice), and the second solid electrolyte layer 6. The auxiliary pump electrode 51 has a ceiling electrode portion 51a provided on substantially the entire lower surface of the second solid electrolyte layer 6 facing the second internal space 40.
[0048] The auxiliary pump electrode 51 is disposed in the second internal space 40 in a tunnel-shaped structure similar to the inner pump electrode 22 provided in the first internal space 20. That is, a ceiling electrode portion 51a is formed on the lower surface 62 of the second solid electrolyte layer 6 that provides the ceiling surface of the second internal space 40, and a bottom electrode portion 51b is formed on the upper surface of the first solid electrolyte layer 4 that provides the bottom surface of the second internal space 40. Side electrode portions (not shown) connecting the ceiling electrode portion 51a and the bottom electrode portion 51b are formed on both wall surfaces of the spacer layer 5 that provide the side walls of the second internal space 40. As a result, the auxiliary pump electrode 51 has a tunnel-shaped structure.
[0049] Like the inner pump electrode 22, the auxiliary pump electrode 51 is also made of a material with a weakened ability to reduce nitrogen oxide components in the measurement gas.
[0050] The gas sensor element 100 is configured so that, by applying a desired voltage Vp1 between the auxiliary pump electrode 51 and the outer pump electrode 23 in the auxiliary pump cell 50, oxygen in the atmosphere within the second internal space 40 can be pumped out to the external space or pumped in from the external space into the second internal space 40.
[0051] [Oxygen partial pressure sensor cell for controlling auxiliary pump] In addition, in order to control the oxygen partial pressure in the atmosphere within the second internal space 40, the auxiliary pump electrode 51, the reference electrode 42, the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, and the third substrate layer 3 constitute an oxygen partial pressure detection sensor cell 81 for controlling the auxiliary pump (i.e., an electrochemical sensor cell).
[0052] The auxiliary pump cell 50 pumps with the variable power supply 52, the voltage of which is controlled based on the electromotive force V1 detected by the auxiliary pump control oxygen partial pressure detection sensor cell 81. As a result, the oxygen partial pressure in the atmosphere in the second internal space 40 is adjusted to NO x The partial pressure is controlled to a low level that has virtually no effect on the measurement of
[0053] In addition, the pump current Ip1 is used to control the electromotive force of the main pump control oxygen partial pressure detection sensor cell 80. Specifically, the pump current Ip1 is input as a control signal to the main pump control oxygen partial pressure detection sensor cell 80, and the electromotive force V0 is controlled so that the gradient of the oxygen partial pressure in the measurement gas introduced from the third diffusion rate-controlling portion 30 into the second internal space 40 is always constant. x When used as a sensor, the oxygen concentration in the second internal space 40 is maintained at a constant value of about 0.001 ppm by the action of the main pump cell 21 and the auxiliary pump cell 50.
[0054] [4th diffusion-controlled section] The fourth diffusion rate-controlling section 16 is a section that imparts a predetermined diffusion resistance to the measurement gas whose oxygen concentration (oxygen partial pressure) has been controlled by the operation of the auxiliary pump cell 50 in the second internal space 40, and guides the measurement gas to the third internal space 17.
[0055] [Third internal void] The third internal space 17 absorbs nitrogen oxides (NO x The space is provided for carrying out the process related to the measurement of NO concentration. xThe concentration is measured by the operation of the measuring pump cell 41. In this embodiment, after the oxygen concentration (oxygen partial pressure) is adjusted in advance in the first internal space 20, the oxygen partial pressure of the measurement gas introduced into the second internal space 40 through the third diffusion rate-controlling section 30 is further adjusted by the auxiliary pump cell 50. This makes it possible to keep the oxygen concentration of the measurement gas introduced from the second internal space 40 to the third internal space 17 constant with high accuracy. Therefore, the gas sensor element 100 according to this embodiment can measure NO x It becomes possible to measure the concentration.
[0056] [Measurement pump cell] The measurement pump cell 41 measures the nitrogen oxide concentration in the measurement gas in the third internal space 17. The measurement pump cell 41 is an electrochemical pump cell including a measurement electrode 44, an outer pump electrode 23, a second solid electrolyte layer 6, a spacer layer 5, and a first solid electrolyte layer 4. In the example shown in FIG. 1 , the measurement electrode 44 is provided on an upper surface of the first solid electrolyte layer 4 adjacent to (facing) the third internal space 17.
[0057] [Measurement electrode] The measurement electrode 44 is a porous cermet electrode. The measurement electrode 44 detects NO 2 present in the atmosphere in the third internal space 17. x Reduce NO x It also functions as a reduction catalyst. In one example shown in FIG. 1, the measurement electrode 44 is exposed in the third internal space 17. In another example, the measurement electrode 44 may be covered with a diffusion rate limiting portion. The diffusion rate limiting portion may be composed of a porous membrane mainly composed of alumina (Al2O3). The diffusion rate limiting portion is configured to prevent NO 2 from flowing into the measurement electrode 44 from being mixed with the NO 2 x It also acts as a protective film for the measurement electrode 44.
[0058] The gas sensor element 100 is configured so that the measurement pump cell 41 can pump out oxygen produced by decomposition of nitrogen oxides in the atmosphere surrounding the measurement electrode 44, and detect the amount of oxygen produced as a pump current Ip2.
[0059] In order to detect the oxygen partial pressure around the measurement electrode 44, a measurement pump control oxygen partial pressure detection sensor cell 82 (i.e., an electrochemical sensor cell) is configured by the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, the measurement electrode 44, and the reference electrode 42. The variable power supply 46 is controlled based on the voltage (electromotive force) V2 detected by the measurement pump control oxygen partial pressure detection sensor cell 82.
[0060] The measurement gas introduced into the third internal space 17 reaches the measurement electrode 44 under conditions in which the oxygen partial pressure is controlled. Nitrogen oxides in the measurement gas around the measurement electrode 44 are reduced (2NO→N2+O2) to generate oxygen. The generated oxygen is then pumped by the measurement pump cell 41, and the voltage Vp2 of the variable power supply is controlled so that the control voltage V2 detected by the measurement pump control oxygen partial pressure detection sensor cell 82 is constant. Since the amount of oxygen generated around the measurement electrode 44 is proportional to the concentration of nitrogen oxides in the measurement gas, the pump current Ip2 in the measurement pump cell 41 is used to calculate the nitrogen oxide concentration in the measurement gas.
[0061] In addition, the measurement electrode 44, the first solid electrolyte layer 4, the third substrate layer 3, and the reference electrode 42 are combined to form an electrochemical sensor cell to form an oxygen partial pressure detection means, thereby detecting NO in the atmosphere around the measurement electrode 44. x It is possible to detect the electromotive force corresponding to the difference between the amount of oxygen generated by the reduction of the components and the amount of oxygen contained in the reference atmosphere, which makes it possible to determine the concentration of nitrogen oxide components in the measurement gas.
[0062] [Sensor cell] An electrochemical sensor cell 83 is formed by the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, the outer pump electrode 23, and the reference electrode 42. The gas sensor element 100 is configured to be able to detect the oxygen partial pressure in the measurement gas outside the sensor by the electromotive force Vref obtained by the sensor cell 83.
[0063] In the gas sensor element 100 having the above-mentioned configuration, the main pump cell 21 and the auxiliary pump cell 50 are operated to always maintain the oxygen partial pressure at a constant low value (NO x Therefore, the gas sensor element 100 can detect the NO concentration in the measurement gas in a manner substantially proportional to the concentration of nitrogen oxides in the measurement gas. x The nitrogen oxide concentration in the measurement gas can be determined based on a pump current Ip2 that flows when oxygen generated by reduction of the nitrogen oxide is pumped out of the measurement pump cell 41.
[0064] [heater] Furthermore, the gas sensor element 100 includes a heater 70 that adjusts the temperature by heating and keeping the gas sensor element 100 warm. The heater 70, except for a heater electrode 71 described later, is disposed at a position closer to the lower surface of the gas sensor element 100 than to the upper surface of the gas sensor element 100 in the thickness direction of the gas sensor element 100 (the vertical direction in FIG. 1). However, the position of the heater 70 is not limited to this example, and may be appropriately selected depending on the embodiment.
[0065] The heater 70 mainly includes a heater electrode 71, a heat generating portion 72 (72a, 72b), a lead portion 73, and a heater insulating layer 74. In the example shown in Fig. 1, the heater 70 further includes a pressure dissipation hole 75. As described below, the lead portion 73 is formed as a pair of through holes that penetrate the first substrate layer 1 and the second substrate layer 2 in their thickness direction to electrically connect the lower surface side of the first substrate layer 1 and the upper surface side of the second substrate layer 2 (see Figs. 2 and 3).
[0066] The heater electrode 71 is an electrode formed in a manner to contact the lower surface (the lower surface of the gas sensor element 100) of the first substrate layer 1. By connecting the heater electrode 71 to an external power source, it is possible to supply power from the outside to the heat generating portion 72 via the lead portion 73.
[0067] The heating portion 72 is an electric resistor sandwiched between the second substrate layer 2 and the third substrate layer 3 from above and below, that is, a resistive heating element provided between the second substrate layer 2 and the third substrate layer 3. The heating portion 72 generates heat when power is supplied from a heater power source (not shown) provided outside the gas sensor element 100 through the heater electrode 71 and the lead portion 73, which are a current path, and heats and keeps warm the solid electrolyte that forms the gas sensor element 100.
[0068] The heat generating part 72 is made of Pt or contains Pt as a main component. The heat generating part 72 is embedded in a predetermined area on the side of the gas sensor element 100 where the measured gas flow part 7 is provided, so as to face the measured gas flow part 7 in the element thickness direction. The heat generating part 72 is provided to have a thickness of, for example, about 10 μm to 20 μm.
[0069] 2 is a schematic diagram showing an example of a schematic planar arrangement of the heat generating portion 72 and its periphery. As shown in FIG. 2, the heat generating portion 72 has a meandering portion 72a that meanders in front of the gas sensor element 100, and a pair of straight portions 72b that extend linearly from both ends of the meandering portion 72a toward the rear end of the gas sensor element 100. The shape of the meandering portion 72a is not limited to the example shown in FIG. 2, and may be, for example, a shape as shown in FIG. 3. The pair of straight portions 72b are provided so as to have substantially the same shape, that is, so that both have the same resistance value. The rear ends of the straight portions 72b are connected to a pair of through holes that constitute the lead portions 73.
[0070] The heating portion 72 can adjust the temperature of the entire gas sensor element 100 to a temperature at which the solid electrolyte is activated. That is, in the gas sensor element 100, current is passed through the heater electrode 71 to cause the heating portion 72 to generate heat, thereby heating and keeping each portion of the gas sensor element 100 at a predetermined temperature. Specifically, the gas sensor element 100 is heated so that the temperature of the solid electrolyte and electrodes in the vicinity of the measurement gas flow portion 7 becomes, for example, about 700°C to 900°C (or 750°C to 950°C).
[0071] The heater insulating layer 74 is an insulating layer formed in a manner to cover the heat generating portion 72, and is, for example, an insulating layer formed of an insulator such as alumina (Al2O3) on the upper and lower surfaces of the heat generating portion 72. The heater insulating layer 74 is formed for the purpose of obtaining electrical insulation between the second substrate layer 2 and the heat generating portion 72, and between the third substrate layer 3 and the heat generating portion 72. The heater insulating layer 74 has a thickness of about 70 μm to 110 μm, and is provided at a position separated from the tip surface and side surface of the gas sensor element 100 by about 200 μm to 700 μm. However, the thickness of the heater insulating layer 74 does not need to be constant, and may be different between a portion where the heat generating portion 72 is present and a portion where the heat generating portion 72 is not present.
[0072] Pressure relief hole 75 is a portion that penetrates third substrate layer 3 and is provided so as to communicate with reference gas introduction space 43, and is formed for the purpose of mitigating an increase in internal pressure that accompanies an increase in temperature within heater insulation layer 74. However, providing pressure relief hole 75 is not essential, and pressure relief hole 75 does not necessarily have to be provided.
[0073] [Through hole] 4 is a partial cross-sectional view showing the lead portion 73 and its surrounding structure. Although not limited thereto, in this embodiment, the lead portion 73 is formed in the form of a through hole that electrically connects the lower surface 203 side of the first substrate layer 1 and the upper surface 200 side of the second substrate layer 2, that is, electrically connects the lower surface 203 side and the upper surface 202 side of the first substrate layer 1, and the lower surface 201 side and the upper surface 200 side of the second substrate layer 2, respectively. The through hole in this embodiment is composed of a through hole H1 penetrating the first substrate layer 1, a through hole H2 penetrating the second substrate layer 2, and a conductive part P1 formed to fill the insides of the through holes H1 and H2. The through hole H1 penetrates the first substrate layer 1 in the thickness direction from the upper surface 202 to the lower surface 203 of the first substrate layer 1. The through hole H2 penetrates the second substrate layer 2 in the thickness direction from the upper surface 200 to the lower surface 201 of the second substrate layer 2, and is positioned so as to communicate with the through hole H1 when the first substrate layer 1 and the second substrate layer 2 are stacked.
[0074] The conductive portion P1 is formed to fill the inside of the through hole H1, and may be formed continuously on the periphery defining the through hole H1 on the lower surface 203 of the first substrate layer 1. Similarly, the conductive portion P1 is formed to fill the inside of the through hole H2, and may be formed continuously on the periphery defining the through hole H2 on the upper surface 200 of the second substrate layer 2. This makes the electrical connection between the heater electrode 71 and the pair of straight line portions 72b of the heat generating portion 72 more reliable.
[0075] The conductive portion P1 is formed by firing a conductive paste mainly composed of Pt together with the ceramic green sheets corresponding to the first substrate layer 1 and the second substrate layer 2, although this is not limited thereto. That is, the conductive portion P1 is formed integrally with the first substrate layer 1 and the second substrate layer 2. According to the inventors' study, a gap is often generated between the inner wall surface defining the through holes H1, H2 and the conductive portion P1 due to the difference in shrinkage rate when the conductive paste forming the conductive portion P1 and the ceramic green sheets are heated and integrated. A liquid component such as moisture may penetrate into this gap from the outside of the gas sensor element 100. As described above, since the heater insulating layer 74 is a porous body such as alumina, the penetrated liquid component may move inside or at the interface of the heater insulating layer 74 and reach the heat generating portion 72 and its vicinity. When the surrounding temperature rises due to the heat generation of the heat generating portion 72, the liquid component that reaches the heat generating portion 72 and its vicinity evaporates there and becomes water vapor or the like. This causes a localized increase in pressure, which may result in separation of the internal structure of the gas sensor element 100, including the heater 70, and may lead to damage to the gas sensor element 100.
[0076] As a result of intensive research, the inventors have found that the breakage of the gas sensor element 100 caused by the intrusion of liquid components can be suppressed by increasing the adhesion between the conductive portion P1 and the inner wall surface of the ceramic layer that defines the through holes H1 and H2 and preventing the intrusion of liquid components. That is, the inventors have found that the anchor effect between the ceramic green sheet and the conductive paste can be improved by forming at least one recess in a predetermined depth range on the inner wall surface that defines the through holes H1 and H2. This configuration may be applied to both the first substrate layer 1 and the second substrate layer 2, or may be applied to at least one of them. Hereinafter, the second substrate layer 2 and the through hole H2 will be described as an example. The upper surface 200 and the lower surface 201 of the second substrate layer 2 are examples of the first surface and the second surface of the present invention, respectively. Note that the following description can be similarly applied to the first substrate layer 1 and the through hole H1, and in this case, the upper surface 202 and the lower surface 203 of the first substrate layer 1 are examples of the first surface and the second surface of the present invention, respectively.
[0077] 5 is a cross-sectional view of the vicinity of through hole H2 of the second substrate layer 2. As described above, through hole H2 penetrates the second substrate layer 2 in the thickness direction from the upper surface 200 to the lower surface 201. The shape of through hole H2 in the top view of the second substrate layer 2 is not particularly limited, and may be approximately circular, oval, rectangular, etc. An axis that passes through the geometric center of this shape and extends in the thickness direction of the second substrate layer 2 is defined as the central axis A1 of through hole H2.
[0078] 5, the through hole H2 is defined by an upper first inner wall surface 210, a second inner wall surface 212 continuous therewith, and a lower first inner wall surface 211. The upper first inner wall surface 210 and the lower first inner wall surface 211 are surfaces extending generally along the thickness direction of the second substrate layer 2, with the upper first inner wall surface 210 continuing to the upper surface 200 and the lower first inner wall surface 211 continuing to the lower surface 201. The second inner wall surface 212 is a surface continuing at its upper end to the upper first inner wall surface 210 and at its lower end to the lower first inner wall surface 211, and defines a recess 220 recessed toward the inside of the second substrate layer 2 further than the upper first inner wall surface 210 and the lower first inner wall surface 211. In this embodiment, the second inner wall surface 212 is continuous in a constant shape around the entire circumference of the through hole H2 at a certain position in the thickness direction of the second substrate layer 2. As a result, the recess 220 in this embodiment is defined by the second inner wall surface 212 so as to have a roughly constant depth around the entire circumference of the through hole H2 and to be annular in top view. However, the configuration of the second inner wall surface 212 is not limited to this, and the shape may vary along the circumferential direction of the through hole H2, or may be discontinuous rather than continuous around the entire circumference of the through hole H2.
[0079] According to the inventors' study, when the thickness L1 of the second substrate layer 2 is 1, the above-mentioned anchor effect is effectively exhibited when the depth L2 to the innermost position of the recess 220 is 0.05 or more and 0.20 or less, and the above-mentioned anchor effect is more effectively exhibited when the depth L2 is 0.10 or more and 0.20 or less. Here, the depth L2 to the innermost position of the recess 220 is the maximum depth of the recess 220 determined based on the position closest to the central axis A1 among the upper first inner wall surface 210 and the lower first inner wall surface 211 in a cross section of the second substrate layer 2 that includes the central axis A1 and is parallel to the longitudinal direction of the second substrate layer 2. The depth L2 relative to the thickness L1 is determined based on a cross-sectional photograph of the second substrate layer 2 captured by an electron microscope (SU-1510, manufactured by Hitachi High-Technologies Corporation). That is, in the above cross-sectional photograph, the depth L2 can be the distance between the position of a pixel identified as the position closest to the central axis A1 among the upper first inner wall surface 210 and the lower first inner wall surface 211, and the position of a pixel identified as the position farthest from the central axis A1 among the second inner wall surface 212. Meanwhile, the thickness L1 can be the average value of the distance along the thickness direction from the position of a pixel identified as the upper surface 200 to the position of a pixel identified as the lower surface 201, for 10 randomly selected points in the above cross-sectional photograph.
[0080] By setting the maximum depth of the recess 220 within the above range, the conductive paste for forming the conductive portion P1 can easily enter the recess 220. Furthermore, the relative unevenness formed by the upper first inner wall surface 210, the second inner wall surface 212, and the lower first inner wall surface 211 creates an anchor effect between the conductive paste and these wall surfaces, making it possible to absorb the difference in shrinkage between the ceramic layer and the conductive paste.
[0081] For reasons described later, it is preferable that the second inner wall surface 212 exists at a position biased toward either the upper surface 200 side or the lower surface 201 side in the thickness direction of the second substrate layer 2, but is not limited thereto. That is, the second inner wall surface 212 may exist at any position in the thickness direction of the second substrate layer 2 except for positions continuous with the upper surface 200 and the lower surface 201. In addition, there may be two or more second inner wall surfaces 212 in the thickness direction. In addition, the shape of the second inner wall surface 212 in a cross-sectional view of the second substrate layer 2 (i.e., the shape of the recess 220) is not particularly limited and can be selected appropriately.
[0082] <2. How to form through holes> Below, an example of a method for manufacturing the gas sensor element 100, including a method for forming the through hole (lead portion 73) according to this embodiment, will be described, but the method for forming the lead portion 73 and the method for manufacturing the gas sensor element 100 are not limited to this.
[0083] First, the ceramic green sheets to be the ceramic layers of the gas sensor element 100 are prepared in the same number as the ceramic layers of the gas sensor element 100. That is, in this embodiment, six ceramic green sheets are prepared. As described above, the ceramic green sheets contain a solid electrolyte as a ceramic component. The thicknesses of these ceramic green sheets may all be the same or may differ depending on the layer to be formed.
[0084] Next, through holes are formed in each of the six ceramic green sheets for use in positioning during printing or lamination. The through holes can be formed by punching the ceramic green sheets in the thickness direction using, for example, a punching device. The through holes H1 in the first substrate layer 1 and the through holes H2 in the second substrate layer 2 for the lead portions 73 may also be formed at this stage. For example, when forming the recesses 220 described above in the second substrate layer 2, the through holes H2 and the recesses 220 may be formed in a single punching operation using a punching device that forms the upper first inner wall surface 210, the lower first inner wall surface 211, and the second inner wall surface 212 in a single punching operation. In addition, the recesses 220 may be formed by chipping an appropriate portion of the inner wall surface after forming the through holes defined by the inner wall surface extending generally parallel to the thickness direction using the punching device.
[0085] Next, the ceramic green sheets to become the third substrate layer 3, the first solid electrolyte layer 4, the spacer layer 5, and the second solid electrolyte layer 6 are printed with the required patterns and dried. The printing can be performed by a known method such as screen printing. The drying can also be performed by a known method.
[0086] Before or after the printing and drying process, or in parallel with the printing and drying process, the through holes H1 of the ceramic green sheet to be the first substrate layer 1 and the through holes H2 of the ceramic green sheet to be the second substrate layer 2 are filled with conductive paste to be the conductive parts P1. At this time, if there is a recess 220 near the filling side, the conductive paste will more reliably enter the recess 220, and the adhesion between the conductive paste and the ceramic layer will be improved. This is the reason why it is preferable that the second inner wall surface 212 is present at a position biased toward either the upper surface 200 side or the lower surface 201 side. This applies not only to the case where the second inner wall surface 212 is formed in the ceramic green sheet to be the second substrate layer 2, but also to the case where the second inner wall surface is formed in the ceramic green sheet to be the first substrate layer 1.
[0087] Before, after, or in parallel with the printing and drying process, a heating portion 72 and a heater insulating layer 74 are formed on the upper surface of the ceramic green sheet to be the second substrate layer 2. These can be formed by printing and drying a heater paste and an insulator paste for forming the heating portion 72 (72a, 72b). More specifically, an insulating paste is printed on the surface in a predetermined pattern and thickness, and dried. Next, a heater paste is printed on the insulating paste in a predetermined pattern and thickness, and dried. Furthermore, an insulating paste is printed on the heater paste in a predetermined pattern and thickness, and dried. For example, a Pt paste and a paste mainly composed of Pt can be used as the heater paste, and for example, a paste mainly composed of Al2O3 can be used as the insulating paste.
[0088] After printing the patterns on the six ceramic green sheets and drying them, they are aligned with each other, stacked in a predetermined order, and pressed under predetermined temperature and pressure conditions to form a laminate with six ceramic layers. This laminate contains a plurality of unfired gas sensor elements 100, which are cut into pieces and fired at a predetermined firing temperature to obtain individual gas sensor elements 100. In the obtained gas sensor element 100, a conductive portion P1 is formed so as to fill the internal space of the through hole H1 and the through hole H2, thereby forming the lead portion 73.
[0089] <3. Features> According to the above embodiment, it is possible to improve the adhesion between the inner wall surface that defines the through hole for forming the through hole and the conductive paste that is filled therein by a simple method. This makes it possible to prevent the occurrence of a gap between the ceramic layer and the conductive part, and to suppress the peeling of the internal components of the gas sensor element 100 caused by the evaporation of the liquid component that has penetrated therein. Therefore, it is possible to provide a gas sensor element 100 that is less likely to break.
[0090] <4. Modifications> Although the embodiments of the present invention have been described above, the above description of the embodiments is merely an example of the present invention in every respect. Various improvements and modifications may be made to the above embodiments. Regarding each component of the above embodiments, components may be omitted, replaced, or added as appropriate. Furthermore, the shape and dimensions of each component of the above embodiments may be modified as appropriate depending on the embodiment. For example, the following modifications are possible. In the following, the same reference numerals are used for components similar to those of the above embodiments, and the description of the same points as those of the above embodiments is omitted as appropriate. The following modifications may be combined as appropriate.
[0091] (1) The gas sensor element 100 of the above embodiment includes the first substrate layer 1. However, the first substrate layer 1 may be omitted, and the second substrate layer 2 may be configured as the bottommost ceramic layer in FIG.
[0092] (2) The through holes H1 and H2 are not limited to being filled with the conductive paste of the above embodiment. For example, as shown in Fig. 6, the inner wall surfaces of the through holes H1 and H2 may be covered with an insulating paste P2, and the insides of the through holes H1 and H2 may be filled with a conductive paste that will become the conductive portion P1, thereby forming the lead portion 73.
[0093] Even in such a case, by forming through holes including recesses in at least one of the first substrate layer 1 and the second substrate layer 2, it is possible to prevent gaps from occurring between the ceramic layer and the insulating paste P2, which is a different material, and therefore it is possible to avoid peeling due to evaporation of the liquid component. Note that since the conductive paste and the insulating paste P2 have high adhesion, it is more important not to generate gaps between the ceramic layer and the part made of a different material that contacts it.
[0094] (3) The cross-sectional shape of the inner wall surface defining the through hole H2 (H1) is not limited to the shape of the above embodiment, and may be changed as appropriate. For example, the cross-sectional shape of the inner wall surface of the through hole H2 (H1) can be a shape that defines the recesses 220, 220a, and 220b as shown in Figs. 7A to 7E, and in either case, the depth L2 can be specified in the same manner as in the above embodiment. Fig. 7A is an example in which a recess 220 having substantially the same cross-sectional shape as in the above embodiment is formed biased toward the lower surface side, not the upper surface side, of the ceramic layer. Fig. 7B is an example in which the recess 220a is formed on the upper surface side of the ceramic layer, and the recess 220b is formed on the lower surface side. In this case, the recess 220a can be defined by the upper second inner wall surface 212, and the recess 220b can be defined by the lower second inner wall surface 214. Furthermore, a first inner wall surface that is continuous with the upper second inner wall surface 212 and the lower second inner wall surface 214 at both ends can be defined as an intermediate first inner wall surface 213.
[0095] 7C to 7E are examples of recesses 220 having different cross-sectional shapes. As shown in FIG. 7C, the second inner wall surface 212 may itself be uneven in cross-sectional view. Also, the cross-sectional shape of the recesses 220 may not only have corners, but also be smoothly curved as shown in FIG. 7D. Furthermore, the cross-sectional shape of the recesses 220 may have multiple corners as shown in FIG. 7E. In any of the cases shown in FIG. 7C to 7E, these recesses 220 may be formed not only on the upper surface side of the ceramic layer, but also at a middle position in the thickness direction, or on the lower surface side, or may be formed in multiple. Also, when multiple recesses 220 are formed, their shapes may be different from each other.
[0096] The gas sensor element 100 of the above embodiment may further include a porous protective layer covering the front end portion and its periphery. The porous protective layer is, for example, a porous ceramic body such as alumina. By providing the porous protective layer, it is possible to prevent moisture in the measurement gas from penetrating into the gas sensor element 100 and exerting an undesirable effect on the gas sensor element 100. EXAMPLES
[0097] Examples of the present invention will be described in detail below, but the present invention is not limited to these examples.
[0098] <Experiment 1> As shown in FIG. 1, five gas sensor elements were prepared in which six ceramic layers were laminated and heaters were formed. These gas sensor elements had different configurations of a pair of lead parts that penetrate the first substrate layer and the second substrate layer and connect the electric resistor of the heating part and the heater electrode, but had a common configuration except for this point. Specifically, the cross-sectional shapes of the inner wall surface of the through hole of the second substrate layer for forming the lead part were made to be the cross-sectional shapes shown in FIG. 5, FIG. 6, FIG. 7A, FIG. 7B, and FIG. 8, respectively, and were used as the gas sensor elements of Examples 1 to 4 and Comparative Example 1. The gas sensor element of Example 2 had the same cross-sectional shape of the inner wall surface of the through hole of the second substrate layer as the gas sensor element of Example 1, but was different from the gas sensor element of Example 1 in that the inner wall surfaces of the through holes of the first substrate layer and the second substrate layer were covered with an insulating paste. In the gas sensor element according to Comparative Example 1, the through hole of the second substrate layer was defined by a generally flat inner wall surface that did not define a recess and extended generally parallel to the thickness direction of the second substrate layer. In the gas sensor elements according to Examples 1 to 4, the depth of the recess determined by the method according to the above embodiment was 0.15 when the thickness of the second substrate layer was set to 1.
[0099] The rear end side including the pair of lead portions of the gas sensor elements according to Examples 1 to 4 and Comparative Example 1 was immersed in water and left for 4 hours. After that, they were taken out of the water and the water adhering to the surface was wiped off. Then, a voltage of 12V was applied to the heating portion via the heater electrode for 30 seconds, and it was confirmed whether or not peeling occurred between the second substrate layer and the third substrate layer including the heating portion and the heater insulating layer surrounding it. The results were evaluated into the following three levels, A to C. A: The voltage application under the above conditions was repeated several times, but no peeling was observed. B: Peeling was confirmed upon the second voltage application. C: Peeling was confirmed upon the first voltage application.
[0100] The results of Experiment 1 are shown in Table 1 below. As shown in Table 1, in Examples 1 to 4, the resistance to peeling was significantly improved compared to Comparative Example 1. Moreover, from the results of Example 2, it was confirmed that the resistance to peeling was improved even when the material in contact with the inner wall surface of the through hole was a material other than the conductive paste. The effectiveness of the present invention was confirmed by the above Experiment 1. [Table 1]
[0101] <Experiment 2> In the gas sensor element according to Example 1, gas sensor elements were prepared in which the depth of the recess with respect to the thickness of the second substrate layer was changed to 0.05, 0.10, 0.20, and 0.25, respectively, and these were designated as the gas sensor elements according to Examples 5 to 7 and Reference Example 1, respectively. These gas sensor elements were immersed in water under the same conditions as in Experiment 1, and then the moisture on the surface was wiped off. A voltage was applied under the same conditions as in Experiment 1, and it was confirmed whether peeling occurred or not in the same manner as in Experiment 1. The results were evaluated on the above-mentioned three levels of A to C.
[0102] The results of Experiment 2 are shown in Table 2 below. As shown in Table 2, in Examples 1, 6 and 7, the resistance to peeling was significantly improved. In Example 5, the peeling resistance was inferior to Examples 1, 6 and 7, possibly because the depth of the recesses was relatively shallow, but it was improved compared to Comparative Example 1 and Reference Example 1. In Reference Example 1, peeling occurred. This is thought to be because the conductive paste did not sufficiently penetrate into the recesses. The effectiveness of the present invention was confirmed by the above Experiment 2. [Table 2] [Explanation of symbols]
[0103] 100: gas sensor element; 4: first solid electrolyte layer; 6: second solid electrolyte layer; 5...spacer layer, 7...measurement gas flow section (internal space), 11...first diffusion rate-controlling section (diffusion rate-controlling section), 13...second diffusion rate-controlling section (diffusion rate-controlling section), 30...third diffusion rate-controlling section (diffusion rate-controlling section), 16...fourth diffusion rate-controlling section (diffusion rate-controlling section), 20…First internal void, 40…Second internal void (vacant room), 17…Third internal void, 72...heat generating portion, 73...lead portion, 74...heater insulating layer, 200...Top surface (first surface), 201...Bottom surface (second surface), 202...Top surface (first surface), 203...Bottom surface (second surface) 210: upper first inner wall surface; 211: lower first inner wall surface; 212: (upper) second inner wall surface; 220: recess; A1: central axis; H1...Through hole, H2...Through hole, P1...Conductive part
Claims
1. A heating portion; a plurality of laminated ceramic layers configured to be heated by the heat generating portion and forming an internal space into which a gas to be measured is introduced from an external space; a measurement electrode to which the measurement gas introduced into the internal space reaches; Equipped with the plurality of ceramic layers include a first ceramic layer having a first surface, a second surface opposite to the first surface, and a through hole penetrating the first ceramic layer in a thickness direction from the first surface to the second surface, the through hole forming a through hole for electrically connecting the first surface side and the second surface side; The first ceramic layer forms one ceramic layer between the first surface and the second surface, the through hole is defined by a first inner wall surface extending in the thickness direction and a second inner wall surface that is continuous with the first inner wall surface and defines a recess that is recessed toward an inside of the first ceramic layer more than the first inner wall surface, The second inner wall surface is formed at a position not continuous with the first surface and the second surface, When the thickness of the first ceramic layer is 1, the length of the first inner wall surface from the position closest to the central axis of the through hole to the innermost position of the recess is 0.05 to 0.
20. Gas sensor element.
2. When the thickness of the first ceramic layer is 1, the length of the first inner wall surface from the position closest to the central axis of the through hole to the innermost position of the recess is 0.10 or more and 0.20 or less. The gas sensor element according to claim 1 .
3. the second inner wall surface is continuous around the entire circumference of the through hole, and the recess is defined by the second inner wall surface so as to be annular when viewed from the first surface side; 3. The gas sensor element according to claim 1.
4. The second inner wall surface is present at least one of a position biased toward the first surface side and a position biased toward the second surface side in the thickness direction. The gas sensor element according to claim 1 .
5. The second inner wall surface is present in a plurality of parts along the thickness direction. The gas sensor element according to claim 1 .
6. A conductive portion having electrical conductivity and formed so as to fill the inside of the through hole. Further comprising: The gas sensor element according to claim 1 .
7. the heat generating portion is disposed on the first surface side of the first ceramic layer, the through hole electrically connects the heat generating portion and an element on the second surface side of the first ceramic layer. The gas sensor element according to claim 1 .
8. configured to measure a concentration of nitrogen oxides in a measurement gas; The gas sensor element according to claim 1 .
Citation Information
Patent Citations
Circuit board and method for manufacturing it
JP2002208763A
Circuit board and its manufacturing method
JP2006319314A
Gas sensor and its manufacturing method
JP2008046112A
Sensor element, sensor element manufacturing method and gas sensor
JP2008157927A
Wiring substrate, mounting structure, and production process of wiring substrate
JP2010034258A