Method for detecting blockage of injection pipe, method for clearing blockage of injection pipe, and melting equipment

By installing a thermometer inside the cast tube to detect clogs and using an impact applying device, the method addresses inefficiencies in clog detection and clearing, ensuring efficient and safe operation of metal smelting furnaces.

JP7582734B2Active Publication Date: 2024-11-13HYUGA SEIRENSHO KK
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021012867
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-02-19
Filing Date
2021-01-29
Publication Date
2024-11-13
Estimated Expiration
2041-01-29

AI Technical Summary

Technical Problem

Existing methods for detecting and clearing clogs in cast tubes feeding raw materials to metal smelting furnaces are inefficient, inaccurate, and pose safety risks, leading to increased energy consumption and reduced productivity.

Method used

Install a thermometer inside the cast tube at a specific position away from the bottom surface to detect clogging by monitoring temperature changes, and use an impact applying device to clear clogs automatically.

Benefits of technology

Accurate and timely detection of clogs prevents unnecessary temperature rises, reduces energy consumption, and enhances safety by minimizing manual intervention and equipment damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007582734000001
    Figure 0007582734000001
  • Figure 0007582734000002
    Figure 0007582734000002
  • Figure 0007582734000003
    Figure 0007582734000003
Patent Text Reader

Abstract

To provide a melting facility of performing metal refining where the clogging of a material charge pipe charging material to a melting furnace is swiftly and correctly detected, thus the productivity and safety of the facility are satisfactorily maintained.SOLUTION: In a method for detecting material charge pipe clogging in a melting facility 10 for metal refining where a material charge pipe 3 charging material is installed in the upper part of a melting furnace (electric furnace 1), the material charge pipe 3 is a cylindrical pipe comprising a downward inclination part. At the inside of the downward inclination part of the material charge pipe 3, a thermometer 34 is installed in a position separated from the inner wall bottom face of the downward inclination part. Also, based on the variation of the temperature in the material charge pipe 3 measured by the thermometer 34, the clogging of the material charge pipe 3 is detected.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for detecting blockages in a source pipe that feeds raw materials into a melting furnace in a melting facility for metal smelting, a method for clearing blockages in the source pipe, and a melting facility for metal smelting that is capable of detecting blockages in the source pipe. [Background technology]

[0002] In many metal smelting processes such as ferronickel smelting, for example, as shown in Fig. 1, a process is carried out in which high-temperature raw materials are continuously fed into a melting furnace such as an electric furnace 1 through a feed pipe 3. During such raw material feeding process, depending on the properties of the raw materials being fed, the feed pipe may become clogged with raw materials, preventing smooth feeding of the raw materials.

[0003] For example, when the above-mentioned clogging of raw materials occurs in the feed pipe 3 installed in the electric furnace 1 as shown in Fig. 1, a phenomenon occurs in which the mountain-shaped stack 61A formed in the furnace immediately below the feed pipe 3 shrinks as shown in Fig. 4. When this happens, an unnecessary increase in the furnace temperature due to radiant heat from the layer below (slag layer 5) is induced, and the productivity and safety of the production equipment including the electric furnace 1 may decrease.

[0004] The clogging of the dumping pipe can be detected, for example, by the increase or decrease in the remaining amount (stored amount) of burnt ore 6 in the batcher bin 2 installed on the upper part of the dumping pipe 3 shown in Fig. 1. However, since a batcher bin usually has two to four dumping pipes (not shown in Fig. 1), it is not possible to know which of the multiple dumping pipes is clogged by the above detection means.

[0005] In order to detect which of the multiple injection pipes is clogged, the only way was to check inside the furnace through an inspection hatch on the furnace cover of the electric furnace 1 and visually check the degree of shrinkage of the mountain-like stack. However, the field of view of the inspection hatch on the furnace is narrow and there are often many blind spots, so it is sometimes difficult to visually identify the location of the clog, and there are often problems with the safety of the inspection worker. In this case, the only way to clear the clog is to apply an external force to all of the injection pipes that may be clogged in sequence.

[0006] Regarding the above-mentioned method of applying an external force to all the tubes in sequence to deal with the blockage of the source tube, it may take a long time to identify the clogged tube and to clear the blockage, and it may be unavoidable that the cost is reduced due to the energy loss caused by the unnecessary temperature rise on the furnace and in the exhaust gas. Therefore, it is not necessarily a preferable method in terms of the speed of response.

[0007] As a means for detecting the above-mentioned clogging of the chute, Patent Document 1 proposes a method for detecting clogging inside the pipe by measuring the temperature of the outer surface of the chute, which is not fitted with refractory material. However, if there is a part inside the chute where refractory material is not installed, the heat dissipated from the chute increases, and energy loss increases. In addition, the heat shortens the life of the chute. In addition, in order to eliminate the clogging after detection, it is necessary to apply an impact to the chute from the outside, but this impact is also problematic in that it is likely to cause poor contact between the thermometer installed outside the chute and the chute.

[0008] Also, Patent Document 2 proposes a method of installing a displacement sensor between the source pipe and the electrode, calculating the amount of electrode displacement, and estimating clogging of the source pipe when the amount of displacement exceeds a threshold. However, this method has problems such as problems caused by dust adhering to the displacement sensor, vibrations in the factory building, and malfunctions caused by electrode displacement due to factors other than clogging of raw materials. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2016-098401 A [Patent Document 2] JP 2014-105940 A Summary of the Invention [Problem to be solved by the invention]

[0010] The present invention aims to maintain the productivity and safety of a melting facility for metal refining by quickly and accurately detecting clogging of a feed pipe that feeds raw materials into a melting furnace. [Means for solving the problem]

[0011] The present inventors have conducted extensive research to solve the above problems, and have discovered that by installing a thermometer at a specific appropriate position inside the injection pipe, clogging of the injection pipe can be detected early and the above problems can be solved, leading to the completion of the present invention.

[0012] (1) A method for detecting blockage of a source pipe in a melting facility for refining metals, in which a source pipe for feeding raw materials is installed above a melting furnace, said source pipe being a cylindrical tube including a downwardly sloping portion, and a thermometer being installed inside the downwardly sloping portion of said source pipe at a position spaced apart from the bottom surface of the inner wall of said downwardly sloping portion, and a blockage of the source pipe is detected based on fluctuations in temperature inside the source pipe measured by said thermometer.

[0013] According to the "method of detecting plugging of a feed pipe" in (1), by installing a thermometer at an appropriate position in the feed pipe that feeds raw materials into the melting furnace of the melting equipment, plugging of the feed pipe can be detected quickly and accurately. This prevents unnecessary increases in the furnace lid temperature and exhaust gas temperature of the melting furnace, and maintains the productivity and safety of the melting equipment including the melting furnace. More specifically, according to the present invention, by quickly detecting and dealing with plugging of the feed pipe before the above-mentioned mountain-like stack shrinks, it is possible to prevent an increase in the radiated heat associated with an increase in the exhaust gas and furnace lid temperatures, and improve the energy consumption rate of the melting equipment. In addition, by preventing an increase in the flue and furnace lid temperatures, it is possible to extend the life of the equipment. In addition, since it is no longer necessary for an operator to perform a confirmation task by directly visually inspecting the inside of the furnace, it is possible to reduce the workload of the operator and improve safety.

[0014] (2) A method for detecting a clog in a feed pipe described in (1), in which the thermometer is installed in a position where it comes into contact with the fluid consisting of the raw material when the flow rate per unit time of the raw material flowing inside the downwardly inclined portion is a predetermined standard flow rate, and where it no longer comes into contact with the fluid when the flow rate falls below the predetermined amount.

[0015] In the "method of detecting clogging of the injecting pipe" in (2), the installation position of the thermometer in the detection method in (1) is optimized according to the fluctuation of the actual flow rate of the raw material in each injecting pipe to be used. This makes it possible to further improve the detection accuracy in each injecting pipe.

[0016] (3) A method for detecting blockage of an injection source pipe described in (1) or (2), in which the injection source pipe is judged to be clogged when the temperature inside the injection source pipe measured by the thermometer drops below a predetermined value.

[0017] According to the "method of detecting clogging of a feed pipe" in (3), the method described in (1) or (2) can be carried out simply and with sufficiently high accuracy based on an easily set criterion. Also, by appropriately setting the above-mentioned predetermined value, clogging of the feed pipe can be detected with high accuracy before the pile-like stack in the furnace shrinks and an unnecessary increase in the furnace temperature due to radiant heat from the lower layer is induced.

[0018] (4) A method for detecting blockage of an injection source pipe described in (1) or (2), in which the injection source pipe is judged to be clogged if the decrease in temperature inside the injection source pipe measured by the thermometer continues for more than a predetermined period of time.

[0019] According to the "method for detecting clogging of a feed pipe" in (4), the method described in (1) or (2) can be carried out simply and with sufficiently high accuracy based on an easily set criterion. Also, by appropriately setting the above-mentioned predetermined time, clogging of the feed pipe can be detected with high accuracy before the pile-like stack in the furnace shrinks and an unnecessary increase in the furnace temperature due to radiant heat from the lower layer is induced.

[0020] (5) The method for detecting plugging of a source pipe according to any one of (1) to (4), wherein the melting furnace is an electric furnace, and the melting facility for metal smelting is part of a ferronickel manufacturing facility.

[0021] According to the "method for detecting clogging of an injection source pipe" of (5), in a ferronickel production facility where measures against clogging of an injection source pipe are often essential, the above-mentioned effects of the method for detecting clogging of an injection source pipe described in any one of (1) to (3) can be enjoyed, and the productivity and safety of the ferronickel production facility can be well maintained.

[0022] (6) A method for clearing a blockage in an injector pipe detected by a method for detecting a blockage in an injector pipe described in any one of (1) to (5), wherein an impact application device for applying a mechanical impact to the injector pipe is installed outside the injector pipe upstream of a position where the thermometer is installed, and when a blockage in the injector pipe is detected by the method for detecting a blockage in the injector pipe, the impact application device is activated to clear the blockage in the injector pipe.

[0023] According to the "method for clearing blockages in a water supply pipe" in (6), while enjoying the above-mentioned effects of the method for detecting blockages in a water supply pipe described in any one of (1) to (5), blockages in the water supply pipe can be automatically avoided or quickly cleared. In addition, since manual striking is no longer necessary, the work burden on workers and the dangers associated with the work can be significantly reduced while maintaining or improving the standard of maintenance and management work for the water supply pipe.

[0024] (7) A melting facility for metal refining in which a source pipe for feeding raw materials is installed above a melting furnace, the source pipe being a cylindrical tube including a downwardly sloping portion, and a thermometer being installed inside the downwardly sloping portion of the source pipe at a position spaced from the bottom surface of the inner wall of the downwardly sloping portion.

[0025] According to the "melting equipment" in (7), by installing a thermometer at an appropriate position in the feed pipe that feeds the raw material into the melting furnace of the melting equipment, clogging of the feed pipe can be detected quickly and accurately. This makes it possible to prevent unnecessary increases in the furnace cover temperature and exhaust gas temperature of the melting furnace, and to maintain the productivity and safety of the melting equipment including the melting furnace.

[0026] (8) The melting equipment described in (7), wherein the thermometer is installed in a position where it comes into contact with the fluid consisting of the raw material when the flow rate per unit time of the raw material flowing inside the downwardly inclined portion is a predetermined standard flow rate, and where it no longer comes into contact with the fluid when the flow rate falls below the predetermined amount.

[0027] In the "melting equipment" of (8), the installation position of the thermometer in the melting equipment of (7) is optimized according to the fluctuation of the actual flow rate of the raw material in each of the feed pipes. This makes it possible to further improve the detection accuracy of each feed pipe.

[0028] (9) A melting equipment as described in (7) or (8), in which an impact application device that applies a mechanical impact to the source pipe is installed outside the source pipe, upstream of the position where the thermometer is installed.

[0029] The "melting equipment" of (9) can avoid or quickly eliminate blockages in the source pipe while enjoying the above-mentioned effects of the melting equipment described in (7) or (8). Also, since manual striking is no longer necessary, the workload of workers and the dangers associated with the work can be significantly reduced while maintaining or improving the standard of maintenance and management work for the source pipe.

[0030] (10) The melting facility according to any one of (7) to (9), wherein the melting furnace is an electric furnace, and the melting facility for metal smelting is part of a ferronickel manufacturing facility.

[0031] According to the "melting equipment" of (10), in a ferronickel production facility where measures against clogging of the injection source pipe are likely to be essential, the above-mentioned effects of the melting equipment described in any one of (7) to (9) can be enjoyed, and the productivity and safety of the ferronickel production facility can be well maintained.

[0032] (11) A method for producing ferronickel, comprising melting raw materials using the melting equipment described in (10).

[0033] According to the "method for producing ferronickel" of (11), the above-mentioned effects provided by the melting equipment described in (10) can be enjoyed, and ferronickel can be produced with good productivity and safety. Effect of the Invention

[0034] According to the present invention, in a melting facility for refining metals, clogging of a feed pipe through which raw materials are fed into a melting furnace can be detected quickly and accurately, thereby maintaining the productivity and safety of the facility at a good level. [Brief description of the drawings]

[0035] [Figure 1] 1 is a schematic diagram showing an example of the configuration of a melting facility to which the "method for detecting clogging of a source pipe" of the present invention can be applied. [Diagram 2] FIG. 2 is a cross-sectional view of a source pipe installed in the melting equipment. [Diagram 3] FIG. 3 is a schematic diagram showing a state in which damage has occurred in the refractory of the injection pipe in FIG. 2. [Figure 4] 2 is a schematic diagram showing the state of a mountain-like pile of material inside the furnace when a blockage of the injection pipe occurs in the melting equipment of FIG. 1. FIG. [Diagram 5] FIG. 2 is a schematic diagram showing an example of a thermometer installation mode in a source pipe in the "melting equipment" of the present invention. [Figure 6] 6 is a schematic diagram showing the state of the flow of the raw material in the source pipe when clogging occurs in the source pipe in the "melting facility" of FIG. 5. FIG. [Figure 7] FIG. 2 is a schematic diagram showing an example of a state in which a source pipe branches off from the lower part of a batcher bin located at the upper part of an electric furnace. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] The following describes specific embodiments of the method for detecting plugging of a source pipe and the melting equipment according to the present invention. Note that the present invention is not limited to the following embodiments, and can be embodied in other embodiments without departing from the scope of the present invention.

[0037] <Melt equipment and source pipe clogging detection method> The "method for detecting clogging of a raw material (calcined ore) in a melting facility 10 for metal smelting, for example, as shown in FIG. 1, in which a raw material (calcined ore 6) is introduced into the melting facility 10, above a melting furnace (electric furnace 1). A representative example of a melting facility for metal smelting to which the "method for detecting clogging of a raw material (calcined ore) in the present invention can be applied is a ferronickel manufacturing facility. Of course, the present invention is not limited to application to a ferronickel manufacturing facility, and can be implemented in various melting facilities.

[0038] Also, a specific example of a melting furnace to which the "method for detecting clogging of a feed pipe" of the present invention can be suitably applied is the "three-phase AC electrode type circular electric furnace" disclosed in Patent Document 2. The melting equipment and melting furnace as the embodiment of the present invention are not necessarily limited to the above-mentioned ferronickel manufacturing equipment and electric furnace, and the present invention is a technology that can be widely applied to all melting equipment in which a feed pipe for feeding raw materials is installed above the melting furnace, as described above. However, the following will describe in detail the embodiment in which the melting equipment to which the present invention is applied is a ferronickel manufacturing equipment and an electric furnace that constitutes it.

[0039] [Melting equipment] As shown in FIG. 2, the melting equipment 10 of the present invention is characterized in that a thermometer 34 is installed inside the downwardly inclined portion 31 of the input pipe 3, which is the input pipe for the raw material (calcined ore 6) to the electric furnace 1.

[0040] The installation position of the thermometer 34 may be any position spaced a predetermined distance from the bottom surface of the inner wall of the downwardly inclined portion 31. Melting equipment for metal refining in which a source pipe for introducing raw materials is installed above a melting furnace such as an electric furnace 1, and in which the thermometer 34 is installed at the above-mentioned position inside the source pipe, which is a cylindrical pipe configured to include the downwardly inclined portion 31, falls within the technical scope of the present invention. In such melting equipment, the "method for detecting clogging of a source pipe" of the present invention can be implemented.

[0041] The melting equipment 10, which is a manufacturing equipment for ferronickel, has a source pipe 3 for feeding burnt ore 6 into an electric furnace 1 in which electrodes 11 and 12 are installed. The source pipe 3 is a cylindrical pipe in which a refractory material 33 such as castable is installed on the substantially entire inner wall of a metal shell 32, which is an outer shell part made of metal or the like. As shown in FIG. 1, the source pipe 3 is configured to include a downwardly inclined portion 31 (see FIG. 2) as shown in FIG. 1 and FIG. 2, since it is necessary to drop the burnt ore 6 stored in the batcher bin 2 to an appropriate position horizontally separated from directly below the batcher bin 2. The "method for detecting clogging of the source pipe" of the present invention can be implemented in various melting equipment by installing a thermometer 34 in advance at an appropriate position inside the downwardly inclined portion 31 of the source pipe 3 as shown in FIG. 5 and FIG. 6.

[0042] Furthermore, the "method for detecting blockage of a raw material injection pipe" of the present invention can quickly detect the location of a blockage of raw materials (calcined ore) even in a melting facility in which multiple injection pipes 3, preferably a large number (for example, three or more) of injection pipes 3 are installed for one electric furnace (melting furnace) 1, and therefore exerts a particularly favorable effect in a melting facility in which such a large number of injection pipes 3 are installed.

[0043] The installation position of the thermometer 34 in the injection pipe 3 for carrying out the "method for detecting clogging of the injection pipe" of the present invention is inside the downwardly inclined portion 31 and at a predetermined distance from the bottom surface of the inner wall of the downwardly inclined portion, as shown in FIG. 5. FIG. 6 is a schematic diagram showing the state of flow of the ore 6 in the injection pipe when clogging of the ore 6 occurs in the injection pipe 3 in the "melting facility" of FIG. 5. For example, the "method for detecting clogging of the injection pipe" of the present invention can be carried out by installing the thermometer 34 at the position shown in FIG. 5 and FIG. 6, that is, at the position where the contact state between the thermometer 34 and the flowing ore 6 changes depending on the presence or absence of clogging.

[0044] The above-mentioned "position where the contact state between the thermometer and the flowing ore changes" is, more specifically, the position where the thermometer comes into contact with the fluid made of raw materials when the flow rate per unit time of the raw materials flowing inside the downwardly inclined portion 31 is a predetermined standard flow rate, and where the thermometer no longer comes into contact with the fluid when the flow rate falls below the predetermined amount.

[0045] More specifically, as shown in Figures 5 and 6, the thermometer 34 is installed in a position where it comes into contact with the burnt ore 6 during normal operation, and where it does not come into contact with the burnt ore 6 or at least the amount of contact is reduced when the burnt ore 6 clogs the inside of the injection pipe 3. It is more preferable that the installation position is in the vicinity of the lower end of the downward inclined portion 31. By installing the thermometer 34 in the vicinity of the lower end of the downward inclined portion 31, the occurrence of the clogging of the burnt ore 6 in almost the entire inside of the injection pipe 3 can be detected more reliably.

[0046] As described above, by optimizing the installation position of the thermometer 34 according to the fluctuation of the actual flow rate of the raw material in each of the target injection pipes, it is possible to detect with higher accuracy whether or not the clog of the ore 6 occurs in the injection pipe 3 based on the fluctuation of the temperature sensed by the thermometer 34. There is no particular limitation on the type of the thermometer 34, but a thermocouple can be preferably used.

[0047] Moreover, the melting equipment 10 is preferably provided with an impact device 35 for applying a mechanical impact to the source pipe 3 outside the source pipe 3. The impact device 35 is a device for applying a mechanical impact to the source pipe 3 that has become clogged and blocked. The impact device 35 is installed outside the source pipe 3, upstream of the position where the thermometer 34 is provided.

[0048] The impact device 35 may be installed at any position upstream of the thermometer 34, but for example, as shown in FIG. 2, it is preferable to install the impact device 35 at the elbow portion of the injection pipe 3, which is located upstream of the thermometer 34. The elbow portion refers to the bent portion of the injection pipe 3 or its adjacent area, as shown in FIG. 2, and is a portion where the flow direction of the flowing burnt ore 6 changes. The elbow portion is also a portion of the injection pipe where clogging is relatively likely to occur. By providing the impact device 35 at this elbow portion, the injection pipe clogging, which occurs relatively frequently at the elbow portion, can be eliminated without manual labor, and dangerous manual labor such as hitting the elbow with a hammer can be reduced accordingly.

[0049] The impact applying device 35 is not limited to the elbow portion, but is preferably provided at any location where operational experience indicates that there is a risk of the source pipe becoming clogged. For example, the location where the downwardly inclined portion changes to a gentler angle is a location where there is a risk of the source pipe becoming clogged. By providing the impact applying device 35 at any location where there is a risk of the source pipe becoming clogged, the manual work performed by the operator can be more efficiently reduced.

[0050] Furthermore, the impact device 35 may be any device capable of shaking off the raw material (in this example, burnt ore 6) that has become blocked inside the source pipe 3, and for example, an air vibrator or an air knocker driven by air pressure can be suitably used.

[0051] In addition, the thermometer 34 and the impact application device 35 are electrically connected to a control unit (not shown), and the temperature information inside the source pipe 3 transmitted from the thermometer 34 is received by the control unit.When the control unit determines that a blockage has occurred, it is preferable that the control unit causes the impact application device 35 to apply an impact to the source pipe 3.

[0052] [How to detect blockage of injection pipe] In an electric furnace 1 having a smelting pipe 3 with a thermometer 34 installed in the above-mentioned manner, when a blockage of the ore 6 occurs inside the smelting pipe 3, the temperature detected by the thermometer 34 in the smelting pipe 3 gradually drops. When an operator who performs the "method for detecting blockage of a smelting pipe" of the present invention confirms a drop in the temperature detected by the thermometer 34, the operator can eliminate the blockage of the smelting pipe 3 by applying an external force such as vibration to the smelting pipe 3, thereby preventing an increase in the furnace cover temperature and exhaust gas temperature of the electric furnace 1. In addition, even if a plurality of smelting pipes 3 are installed in the electric furnace 1, the clogged smelting pipe can be identified.

[0053] The criterion for determining whether or not the injection source pipe 3 is clogged based on the fluctuation of the temperature sensed by the thermometer 34 is that the above temperature is equal to or lower than a predetermined value, i.e., a threshold value predefined according to the operating conditions, and thus it can be determined that the injection source pipe 3 is clogged. Alternatively, it may be determined that the injection source pipe 3 is clogged when the above temperature continues to decrease for a predetermined time or more, such as about 10 to 30 minutes.

[0054] The judgment criteria for each of the above temperatures can be specifically determined, for example, by carrying out a test in advance to correspond the temperature fluctuations measured by the thermometer 34 to the shrinkage of the mountain-like stack 61A formed directly below the source pipe 3 as observed through an inspection hatch provided on the furnace cover of the electric furnace 1, or to the increase / decrease in the remaining amount (stored amount) of burnt ore 6 in the batcher bin 2, as shown in the examples described later.

[0055] Furthermore, when a blockage in the injection source pipe 3 is detected by any of the above methods or by a judgment based on other predetermined standards related to temperature fluctuation, an alarm is sounded to notify the operator, and the operator can apply some external force to the injection source pipe 3 from outside the injection source pipe 3 to remove the blockage. The means for applying the external force is not particularly limited. An operator may manually apply a blow with a hammer or the like, or a simple device for applying a blow may be additionally installed.

[0056] In addition, clogging of the injection pipe 3 also occurs due to damage (damaged portion 33A) of the refractory 33 inside the injection pipe 3 as shown in Fig. 3. If the clogged portion of the injection pipe 3 is not known and the injection pipe is struck unnecessarily, the damage (damaged portion 33A) of the refractory inside the injection pipe progresses, but by installing a thermometer 34 in the injection pipe 3 and carrying out the present invention to accurately know the clogged portion, unnecessary impact from the outside of the injection pipe 3 can be reduced, and as a result, the progress of damage at the damaged portion 33A of the refractory 33 inside the injection pipe 3 can be suppressed, and the occurrence of clogging of the injection pipe 3 can be reduced.

[0057] <How to clear a clogged injection pipe> Furthermore, as described above, the present invention can be embodied as a "method for clearing blockages in a source pipe" having a unique aspect by installing the impact applying device 35 at a predetermined position of the source pipe 3. In the "method for clearing blockages in a source pipe" which is one embodiment of the present invention, blockages in the source pipe detected by the "method for detecting blockages in a source pipe" of the present invention described above can be automatically avoided or quickly cleared. Specifically, when the above-mentioned control unit detects a drop in temperature sensed by the thermometer 34 and determines that a blockage has occurred, it operates the impact applying device 35 to perform an operation to clear the blockage in the source pipe, thereby avoiding or quickly clearing the blockage in the source pipe.

[0058] In the "method for clearing a clog in a water injection pipe", when a clog occurs in the water injection pipe 3, the clog can be cleared by operating the impact applying device 35 installed upstream of the water injection pipe 3 from the position where the thermometer 34 is installed. In this case, starting from the time when it is determined that a clog has occurred, the impact applying device 35 may be operated only once to apply only one impact to the water injection pipe, or it may be operated at a predetermined interval (for example, one-minute intervals) to apply multiple impacts to the water injection pipe 3.

[0059] <Application to ferronickel production> The main raw material used in the production of ferronickel is nickel oxide ore. This nickel oxide ore is first dried by reducing the moisture content of the ore, which is called dried ore. This dried ore is calcined and partially reduced using a rotary kiln or the like. In this specification, the high-temperature material discharged from the rotary kiln after the calcination and partial reduction treatment is called calcined ore.

[0060] In the production of ferronickel, the calcined ore 6 is temporarily stored in the batcher bin 2 installed on the top of the electric furnace 1. The calcined ore stored in the batcher bin 2 is generally at a temperature of about 500°C to 800°C. The calcined ore 6 stored in the batcher bin 2 is then fed to the electric furnace 1 through the feed pipe 3. The calcined ore 6 is melted and reduced in the furnace, and separated into metal and slag according to specific gravity. Since the specific gravity of the slag is smaller than that of the metal, a slag layer 5 is formed above the metal layer 4 as shown in FIG. 1.

[0061] The cinders 6 fed into the electric furnace 1 form a mountain-shaped stack 61A on the slag, with the top located near the bottom of the feed pipe 3. The stack 61A formed on the slag layer 5 gradually shrinks as it melts from the bottom. However, cinders 6 are constantly fed from the bottom of the feed pipe 3 as the stack 61A shrinks, so the cinders 6 fed from the feed pipe 3 can maintain the shape of the mountain-shaped stack 61A in the furnace.

[0062] The metal and slag held in the electric furnace 1 are tapped intermittently from holes at different heights. The slag is mainly used to adjust the composition of the steel smelting process, and the metal is cast after the sulfur is removed in the next process and is mainly used as a raw material for stainless steel.

[0063] Here, the temperature of the burnt ore 6 is the temperature in the injection pipe, and is generally about 500°C to 800°C. Inside the batcher bin 2 and the injection pipe 3, a refractory material 33 such as castable is installed, which protects the injection pipe 3 itself and suppresses the dissipation of heat to the outside of the injection pipe 3. However, as shown in FIG. 3, if a part of the refractory material 33 is damaged by wear or the like, the burnt ore may clog the injection pipe starting from the damaged part 33A. Even if the refractory material 33 covering the inner wall of the injection pipe 3 is in a sound state, clogging may occur inside the injection pipe 3 depending on the properties of the burnt ore 6.

[0064] If the injection pipe 3 is left clogged for a long time due to any of the above reasons, the mountain-shaped stack 61A melts continuously from the bottom and gradually shrinks. When the shrinkage progresses beyond a certain level, the surface of the slag layer 5 (molten metal surface) becomes exposed at the foot part 5A of the mountain-shaped stack 61A, as shown in Figure 4. When the molten metal surface, which is usually covered by burnt ore, becomes exposed as shown in Figure 4, the radiant heat of the slag and the heat exchange between the slag and the gas above it cause the lid temperature and exhaust gas temperature of the electric furnace 1 to rise at an accelerated rate.

[0065] In regard to the above-mentioned undesirable temperature rise, by applying the "method for detecting clogging of the injection source pipe" of the present invention and the "melting equipment" of the present invention to the manufacturing method and manufacturing equipment of ferronickel, the occurrence of clogging of the injection source pipe 3 and its occurrence position can be detected quickly and accurately, and the productivity and safety of the ferronickel manufacturing can be maintained well. EXAMPLES

[0066] The present invention will be explained in more detail below by showing examples of test operations, but the present invention is not limited to the following examples in any way.

[0067] In an electric furnace 1A having electrodes 11A, 12A, and 13A as shown in FIG. 7, three injection pipes 3A, 3B, and 3C branched off from the bottom of a batcher bin 2A installed on the furnace of the electric furnace 1A. A thermometer (thermocouple) was installed in the injection pipe 3A, which has the gentlest downward slope and is close to the center of the furnace. The thermometer was installed near the bottom end of the downward slope. Initially, the temperature measured by this thermometer fluctuated between 500°C and 800°C, but after two hours, it was confirmed that the temperature continued to drop for more than one hour. At this point, when the inside of the electric furnace 1A was checked, it was confirmed that the inside of the injection pipe 3A, where the thermometer was installed, was filled with burnt ore.

[0068] When an external impact was applied to the elbow of the pipe, the blockage was cleared and the supply of the ore resumed. After this point, the temperature on the thermometer quickly returned to the original range of 500°C to 800°C.

[0069] One hour later, it was confirmed that the temperature was continuing to drop, and by checking inside the furnace, it was confirmed that the injection pipe was clogged. However, since no temperature rise in the furnace lid or exhaust gas was confirmed, temperature measurement was continued without applying external force. As a result, two hours later, the temperature of the injection pipe was confirmed to fluctuate between 400℃ and 500℃, and at the same time, the temperature rise in the furnace lid and exhaust gas flue was also confirmed, so at this point, external force was applied to the injection pipe as above to remove the blockage. After this work, the thermometer value quickly returned to its original range of 500℃ to 800℃.

[0070] Next, in the subsequent operation, an air knocker (SK-60LPS manufactured by Seishin) was installed as an impact device at the elbow of the injection pipe and operation was continued. During this operation, it was decided that there was a possibility that the injection pipe was clogged if the 10-minute average moving average value of the thermometer continued to drop for one hour or if the 10-minute average value fell below 500°C, and when this was decided, the impact device was automatically operated by the above-mentioned control mechanism, and it was confirmed that it was possible to deal with the clogged injection pipe before the furnace roof temperature and exhaust gas temperature rose due to the clogged injection pipe. [Explanation of symbols]

[0071] 1. 1A electric furnace (melting furnace) 11, 12, 11A, 12A, 13A electrode 2, 2A Batcher Bin 3, 3A, 3B, 3C projection tube 31 Downward Slope 32 Metal Shell 33 Refractories 34 Thermometer 35 Impact Apparatus 4 Metal Layer 5 Slag layer 6 Burnt ore (raw material) 61 Laminated material (burnt ore) 10 Melting equipment

Claims

1. A method for detecting clogging of a feed pipe in a metal smelting facility in which a feed pipe for feeding raw materials is installed above a melting furnace, comprising: The source pipe is a cylindrical pipe including a downwardly inclined portion, A thermometer is installed inside the downwardly inclined portion of the injection pipe, Detecting a blockage of the injection pipe based on a change in temperature in the injection pipe measured by the thermometer; the thermometer is installed at a position where it comes into contact with a fluid made of the raw material when the flow rate per unit time of the raw material flowing inside the downwardly inclined portion is a predetermined standard flow rate, and where it does not come into contact with the fluid when the flow rate becomes equal to or less than the predetermined rate. How to detect blockage of injection pipe.

2. When the temperature in the injection pipe measured by the thermometer falls below a predetermined value, it is determined that the injection pipe is clogged.

2. The method for detecting blockage of a source pipe according to claim 1.

3. When the temperature inside the injection pipe measured by the thermometer continues to decrease for a predetermined period of time or more, it is determined that the injection pipe is clogged.

2. The method for detecting blockage of a source pipe according to claim 1.

4. The melting furnace is an electric furnace, and the melting facility for metal smelting is part of a ferronickel manufacturing facility.

4. A method for detecting blockage of a source pipe according to claim 1.

5. A method for clearing a clog in an injection source pipe, the method for clearing a clog in an injection source pipe detected by the method for detecting a clog in an injection source pipe according to any one of claims 1 to 4, comprising the steps of: an impact applying device that applies a mechanical impact to the injection source pipe is installed on the outside of the injection source pipe upstream of a position where the thermometer is installed; When a blockage in the injection pipe is detected by the method for detecting a blockage in the injection pipe, the impact applying device is operated to eliminate the blockage in the injection pipe. How to clear a clogged injection pipe.

6. A melting facility for metal smelting, in which a feed pipe for feeding raw materials is installed above a melting furnace, The source pipe is a cylindrical pipe including a downwardly inclined portion, A thermometer is installed inside the downwardly inclined portion of the injection pipe, the thermometer is installed at a position where it comes into contact with a fluid made of the raw material when the flow rate per unit time of the raw material flowing inside the downwardly inclined portion is a predetermined standard flow rate, and where it does not come into contact with the fluid when the flow rate becomes equal to or less than the predetermined rate. Melting equipment.

7. an impact applying device that applies a mechanical impact to the injection source pipe is installed on the outside of the injection source pipe upstream of a position where the thermometer is installed; 7. The melting installation according to claim 6.

8. The melting furnace is an electric furnace, and the melting facility for metal smelting is part of a ferronickel manufacturing facility. Melting installation according to claim 6 or 7.

9. A method for producing ferronickel, comprising melting raw materials using the melting equipment according to claim 8.

Citation Information

Patent Citations

  • Blockage detection method of raw-material charging chute forsealed type electric furnace

    JP1987210389A

  • Device and method for detecting blockage of material inputting pipe in three-phase ac electrode type circular electric furnace

    JP2014105940A

  • Method for detecting clogging of sintered ore chute, and sintered ore chute provided with clogging detection function

    JP2016098401A

  • Melting tank

    JP2017155997A