Gas sensor and method for manufacturing the same
By depositing the porous metal layer at an angle to the substrate surface and using shared vapor deposition equipment, the method lowers manufacturing costs and ensures uniformity, addressing the need for specialized equipment in existing gas sensors.
Patent Information
- Application Number
- JP2021084657
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-19
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-05-19
AI Technical Summary
The formation of the first porous metal layer in existing gas sensors requires specialized sputtering equipment due to low vacuum conditions, leading to increased manufacturing costs.
The method involves forming the porous metal layer by depositing its constituent material in a direction inclined to the normal of the substrate surface, using a general-purpose vapor deposition apparatus, and forming the porous oxide layer using the same method, allowing for shared equipment and reduced costs.
This approach reduces manufacturing costs and maintains in-plane uniformity of the porous metal layer thickness while enabling the use of general-purpose equipment, and the helical structure helps relieve thermal stress on the solid electrolyte layer.
Smart Images

Figure 0007591973000001 
Figure 0007591973000002 
Figure 0007591973000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a gas sensor and a method for manufacturing a gas sensor. [Background technology]
[0002] International Publication No. WO 2017 / 014033 (Patent Document 1) describes a gas sensor. The gas sensor described in Patent Document 1 includes a substrate, an insulating layer, a microheater, a porous oxide layer, a first porous metal layer, a solid electrolyte layer, and a second porous metal layer.
[0003] A cavity is formed in the substrate. The cavity penetrates the substrate along the thickness direction. An insulating layer is disposed on the substrate. A microheater is disposed in a portion of the insulating layer above the cavity (hereinafter referred to as a "membrane portion"). A porous oxide layer is disposed on the membrane portion. A first porous metal layer is disposed on the porous oxide layer. A solid electrolyte layer is disposed on the first porous metal layer. A second porous metal layer is disposed on the solid electrolyte layer. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2017 / 014033 Summary of the Invention [Problem to be solved by the invention]
[0005] In the gas sensor described in Patent Document 1, the first porous metal layer is formed by sputtering. However, when forming the first porous metal layer by sputtering, special conditions (sputtering at a low vacuum) are required, so a general-purpose sputtering device cannot be used. As a result, a dedicated sputtering device must be introduced to form the first porous metal layer, which increases the manufacturing cost.
[0006] The present disclosure has been made in view of the problems of the conventional techniques as described above. More specifically, the present disclosure provides a gas sensor and a method for manufacturing the gas sensor that can reduce manufacturing costs. [Means for solving the problem]
[0007] The method for manufacturing a gas sensor according to the present disclosure includes the steps of forming an insulating layer on a main surface of a substrate, forming a porous oxide layer on the insulating layer, and forming a porous metal layer on the porous oxide layer. The step of forming the porous metal layer is performed by depositing a constituent material of the porous metal layer in a direction inclined with respect to the normal to the main surface.
[0008] The gas sensor of the present disclosure includes a substrate, an insulating layer disposed on the substrate, wiring disposed in the insulating layer, a porous oxide layer, a first porous metal layer disposed on the porous oxide layer, a solid electrolyte layer disposed on the first porous metal layer, and a second porous metal layer disposed on the solid electrolyte layer. The substrate has a cavity penetrating the substrate in the thickness direction. The insulating layer has a membrane portion on the cavity. The wiring has a heater portion disposed in the membrane portion. The porous oxide layer is disposed on the membrane portion. The first porous metal layer is composed of a plurality of spiral structures. Each of the plurality of spiral structures extends in a spiral shape along the thickness direction. Effect of the Invention
[0009] According to the gas sensor and the method for manufacturing the gas sensor of the present disclosure, the manufacturing cost can be reduced. [Brief description of the drawings]
[0010] [Figure 1] 1 is a cross-sectional view of a gas sensor 100. FIG. [Diagram 2] 2 is a schematic diagram showing the internal structure of a porous oxide layer 50. FIG. [Diagram 3] 2 is a schematic diagram showing the internal structure of a porous metal layer 60. FIG. [Figure 4] 3A to 3C are process diagrams illustrating a method for manufacturing the gas sensor 100. [Diagram 5] FIG. 11 is a cross-sectional view illustrating a first insulating layer forming step S2. [Figure 6] FIG. 11 is a cross-sectional view illustrating a first wiring forming step S3. [Figure 7] FIG. 11 is a cross-sectional view illustrating a second insulating layer forming step S4. [Figure 8] FIG. 11 is a cross-sectional view illustrating a second wiring forming step S5. [Figure 9] FIG. 11 is a cross-sectional view illustrating a third insulating layer forming step S6. [Figure 10] FIG. 11 is a cross-sectional view illustrating a porous oxide layer forming step S7. [Figure 11] FIG. 13 is a schematic diagram for explaining the mechanism by which a helical structure 51 is formed in the porous oxide layer forming step S7. [Figure 12] FIG. 11 is a cross-sectional view illustrating a first porous metal layer forming step S8. [Figure 13] FIG. 11 is a cross-sectional view for illustrating a solid electrolyte layer forming step S9. [Figure 14] FIG. 11 is a cross-sectional view for explaining the patterning step S10. [Figure 15] FIG. 11 is a cross-sectional view illustrating a fourth insulating layer forming step S11. [Figure 16] FIG. 11 is a cross-sectional view illustrating the second porous metal layer forming step S12. [Figure 17] 4 is a graph showing the relationship between the deposition direction of the constituent material of the porous metal layer 60 and the relative density of the porous metal layer 60. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The details of the embodiments of the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are designated by the same reference numerals, and redundant description will not be repeated.
[0012] (Configuration of the gas sensor according to the embodiment) A gas sensor according to an embodiment (hereinafter referred to as "gas sensor 100") will be described below.
[0013] Fig. 1 is a cross-sectional view of a gas sensor 100. As shown in Fig. 1, the gas sensor 100 has a substrate 10, an insulating layer 20, a wiring 30, and a wiring 40. The gas sensor 100 further has a porous oxide layer 50, a porous metal layer 60, a solid electrolyte layer 70, an insulating layer 80, and a porous metal layer 90.
[0014] The substrate 10 is made of, for example, single crystal silicon. The substrate 10 has a main surface 10a and a main surface 10b. The main surface 10a and the main surface 10b are end surfaces of the substrate 10 in the thickness direction. The main surface 10b is the surface opposite to the main surface 10a. A cavity 10c is formed in the substrate 10. The cavity 10c penetrates the substrate 10 along the thickness direction.
[0015] The insulating layer 20 is disposed on the substrate 10. More specifically, the insulating layer 20 is formed on the main surface 10a. The insulating layer 20 has a first layer 21, a second layer 22, a third layer 23, a fourth layer 24, a fifth layer 25, and a sixth layer 26.
[0016] The first layer 21 is made of, for example, silicon oxide. The first layer 21 is disposed on the substrate 10 (on the main surface 10a). The second layer 22 is made of, for example, silicon nitride. The second layer 22 is disposed on the first layer 21. The third layer 23 and the fourth layer 24 are made of, for example, silicon oxide. The third layer 23 is disposed on the second layer 22. The fourth layer 24 is disposed on the third layer 23.
[0017] The fifth layer 25 is formed of, for example, silicon nitride. The fifth layer 25 is disposed on the fourth layer 24. The sixth layer 26 is formed of, for example, silicon oxide. The sixth layer 26 is disposed on the fifth layer 25.
[0018] The insulating layer 20 has a membrane portion 27. The membrane portion 27 is a portion of the insulating layer 20 located above the cavity 10c.
[0019] The wiring 30 is disposed in the insulating layer 20. More specifically, the wiring 30 is disposed on the third layer 23 and is covered by the fourth layer 24. The wiring 30 is formed of, for example, platinum. The periphery of the wiring 30 is covered by an adhesion layer 31. The adhesion layer 31 is formed of, for example, titanium oxide. The adhesion layer 31 ensures adhesion between the insulating layer 20 and the wiring 30. The adhesion layer 31 has a first portion 31a and a second portion 31b. The first portion 31a is disposed on the third layer 23. The wiring 30 is disposed on the first portion 31a. The second portion 31b covers the wiring 30.
[0020] The wiring 30 has a heater portion 32. The heater portion 32 is disposed within the membrane portion 27 and is a portion of the wiring 30 that meanders in a plan view. The heater portion 32 generates heat by resistance heating when electricity is applied thereto.
[0021] The wiring 40 is disposed in the insulating layer 20. More specifically, the wiring 40 is disposed on the fifth layer 25 and is covered by the sixth layer 26. The wiring 40 is formed of, for example, platinum. The periphery of the wiring 40 is covered by an adhesion layer 41. The adhesion layer 41 is formed of, for example, titanium oxide. The adhesion layer 41 ensures adhesion between the insulating layer 20 and the wiring 40.
[0022] The wiring 40 has a temperature sensor section 42. The temperature sensor section 42 is disposed within the membrane section 27, and is a portion of the wiring 40 that meanders in a plan view. The temperature sensor section 42 overlaps with the heater section 32 in a plan view. The temperature sensor section 42 functions as a resistance temperature detector. That is, the temperature near the temperature sensor section 42 is measured by measuring the change in the electrical resistance value of the wiring 40 that constitutes the temperature sensor section 42.
[0023] The porous oxide layer 50 is disposed on the insulating layer 20. More specifically, the porous oxide layer 50 is disposed on the membrane portion 27. FIG. 2 is a schematic diagram showing the internal structure of the porous oxide layer 50. As shown in FIG. 2, the porous oxide layer 50 is preferably composed of a plurality of helical structures 51. The helical structures 51 extend in a helical shape along the thickness direction of the substrate 10. That is, the helical structures 51 extend along the thickness direction of the substrate 10 while rotating around a central axis along the thickness direction of the substrate 10.
[0024] 1, the porous metal layer 60 is disposed on the porous oxide layer 50. The porous metal layer 60 is made of, for example, platinum. The porous metal layer 60 is the cathode.
[0025] The relative density of the porous metal layer 60 is preferably 0.5 or more. The relative density of the porous metal layer 60 is a value obtained by dividing the density of the porous metal layer 60 by the density of the constituent materials of the porous metal layer 60. The density of the porous metal layer 60 is a value obtained by dividing the weight of the porous metal layer 60 by the apparent volume of the porous metal layer 60 (the sum of the volume of the constituent materials of the porous metal layer 60 and the volume of the voids in the porous metal layer 60).
[0026] Fig. 3 is a schematic diagram showing the internal structure of the porous metal layer 60. As shown in Fig. 3, the porous metal layer 60 is preferably composed of a plurality of spiral structures 61. The spiral structures 61 extend in a spiral shape along the thickness direction of the substrate 10. That is, the spiral structures 61 extend along the thickness direction of the substrate 10 while rotating around a central axis along the thickness direction of the substrate 10.
[0027] 1, the solid electrolyte layer 70 is disposed on the porous metal layer 60. The solid electrolyte layer 70 is made of an oxygen ion conductor. The solid electrolyte layer 70 is made of, for example, yttria-stabilized zirconia.
[0028] The insulating layer 80 is disposed on the insulating layer 20 so as to cover the porous oxide layer 50, the porous metal layer 60, and the solid electrolyte layer 70. However, the insulating layer 80 has an opening that partially exposes the solid electrolyte layer 70. The insulating layer 80 is, for example, a layer in which a silicon oxide layer and a tantalum oxide layer are stacked.
[0029] The porous metal layer 90 is disposed on a portion of the solid electrolyte layer 70 that is exposed from the insulating layer 80. The porous metal layer 90 is made of, for example, platinum. The porous metal layer 90 is an anode.
[0030] When energized, the heater section 32 generates heat and heats the solid electrolyte layer 70. This causes the solid electrolyte layer 70 to exhibit oxygen ion conductivity. The gas around the gas sensor 100 passes through the porous oxide layer 50 and reaches the porous metal layer 60. Oxygen gas in the gas that reaches the porous metal layer 60 receives electrons from the porous metal layer 60, generating oxygen ions.
[0031] The oxygen ions move within the solid electrolyte layer 70 due to the voltage between the porous metal layer 60 and the porous metal layer 90. The oxygen ions that reach the porous metal layer 90 release electrons to the porous metal layer 90 and become oxygen gas. At this time, a current flows between the porous metal layer 60 and the porous metal layer 90. Since this current is proportional to the concentration of oxygen gas, the gas sensor 100 can detect the concentration of oxygen gas in the gas surrounding the gas sensor 100 by detecting this current. The concentration of water vapor in the gas surrounding the gas sensor 100 can also be detected in a similar manner.
[0032] (Method of Manufacturing Gas Sensor According to the Embodiment) A method for manufacturing the gas sensor 100 will now be described.
[0033] Fig. 4 is a process diagram showing a method for manufacturing the gas sensor 100. As shown in Fig. 4, the method for manufacturing the gas sensor 100 includes a preparation step S1, a first insulating layer forming step S2, a first wiring forming step S3, a second insulating layer forming step S4, a second wiring forming step S5, a third insulating layer forming step S6, a porous oxide layer forming step S7, a first porous metal layer forming step S8, a solid electrolyte layer forming step S9, a patterning step S10, a fourth insulating layer forming step S11, a second porous metal layer forming step S12, and a cavity forming step S13.
[0034] In the preparation step S1, a substrate 10 is prepared. The substrate 10 prepared in the preparation step S1 does not have a cavity 10c formed therein.
[0035] Fig. 5 is a cross-sectional view for explaining the first insulating layer forming step S2. As shown in Fig. 5, in the first insulating layer forming step S2, a first layer 21, a second layer 22, and a third layer 23 are formed in sequence. The first layer 21, the second layer 22, and the third layer 23 are formed, for example, by using a CVD (Chemical Vapor Deposition) method.
[0036] 6 is a cross-sectional view for explaining the first wiring forming step S3. In the first wiring forming step S3, as shown in FIG.
[0037] In the first wiring formation process S3, first, the first portion 31a is formed by depositing and patterning a material constituting the adhesion layer 31. The deposition is performed by, for example, sputtering. The patterning is performed by, for example, forming a mask using photolithography and etching using the mask.
[0038] Secondly, in the first wiring formation process S3, the wiring 30 is formed by depositing and patterning the constituent material of the wiring 30. This deposition is performed by, for example, sputtering. This patterning is performed by, for example, forming a mask using photolithography and etching using the mask.
[0039] Thirdly, in the first wiring formation process S3, the second portion 31b is formed by depositing and patterning the constituent material of the adhesion layer 31. This deposition is performed by, for example, sputtering. This patterning is performed by, for example, forming a mask using photolithography and etching using the mask.
[0040] FIG. 7 is a cross-sectional view for explaining the second insulating layer forming step S4. As shown in FIG. 7, in the second insulating layer forming step S4, a fourth layer 24 and a fifth layer 25 are formed in sequence. The fourth layer 24 and the fifth layer 25 are formed, for example, by a CVD method. FIG. 8 is a cross-sectional view for explaining the second wiring forming step S5. As shown in FIG. 8, in the second wiring forming step S5, a wiring 40 and an adhesive layer 41 are formed. The wiring 40 and the adhesive layer 41 are formed by the same method as the wiring 30 and the adhesive layer 41.
[0041] 9 is a cross-sectional view for explaining the third insulating layer forming step S6. As shown in FIG 9, in the third insulating layer forming step S6, a sixth layer 26 is formed. The sixth layer 26 is formed by using, for example, a CVD method.
[0042] Fig. 10 is a cross-sectional view for explaining the porous oxide layer forming step S7. The arrows in Fig. 10 indicate the deposition direction of the constituent material of the porous oxide layer 50. As shown in Fig. 10, in the porous oxide layer forming step S7, the porous oxide layer 50 is formed. The porous oxide layer 50 is formed by depositing the constituent material of the porous oxide layer 50. This deposition is performed from a direction inclined with respect to the normal line of the main surface 10a. During this deposition, it is preferable that the substrate 10 is rotated one or more times around a rotation axis (see dotted line in Fig. 10) along the normal line of the main surface 10a.
[0043] Fig. 11 is a schematic diagram for explaining the mechanism by which the helical structure 51 is formed in the porous oxide layer forming step S7. The arrows in Fig. 11 indicate the deposition direction of the constituent material of the porous oxide layer 50. As shown in Fig. 11, as the deposition of the constituent material of the porous oxide layer 50 starts, agglomeration nuclei 52 made of the constituent material of the porous oxide layer 50 are formed on the insulating layer 20.
[0044] The material for the porous oxide layer 50 is deposited in a direction inclined with respect to the normal to the main surface 10a. Therefore, the material for the porous oxide layer 50 is not deposited in the shadow of the agglomeration nuclei 52. As a result, the material for the porous oxide layer 50 is deposited on the agglomeration nuclei 52 along the deposition direction (see the dotted line in FIG. 11). During the deposition of the material for the porous oxide layer 50, the substrate 10 is rotated around a rotation axis along the normal to the main surface 10a. Therefore, the direction in which the material for the porous oxide layer 50 is deposited is also changed in accordance with this rotation. As a result, a helical structure 51 is formed.
[0045] FIG. 12 is a cross-sectional view for explaining the first porous metal layer forming step S8. The arrows in FIG. 12 indicate the deposition direction of the constituent material of the porous metal layer 60. As shown in FIG. 12, in the first porous metal layer forming step S8, the porous metal layer 60 is formed. The porous metal layer 60 is formed by depositing the constituent material of the porous metal layer 60 from a direction inclined with respect to the main surface 10a. This deposition is preferably performed from a direction inclined by 80° or more and less than 90° with respect to the main surface 10a. During this deposition, it is preferable that the substrate 10 is rotated one or more times around a rotation axis (see dotted line in FIG. 11) along the normal line of the main surface 10a. As a result, a helical structure 61 is formed.
[0046] The porous oxide layer forming step S7 and the first porous metal layer forming step S8 are preferably performed using the same deposition apparatus.
[0047] FIG. 13 is a cross-sectional view for explaining the solid electrolyte layer forming step S9. As shown in FIG. 13, in the solid electrolyte layer forming step S9, a solid electrolyte layer 70 is formed. The solid electrolyte layer 70 is formed by forming and patterning a material constituting the solid electrolyte layer 70. The film is formed by, for example, sputtering. The patterning is performed by, for example, dry etching. FIG. 14 is a cross-sectional view for explaining the patterning step S10. As shown in FIG. 14, in the patterning step S10, the porous oxide layer 50 and the porous metal layer 60 are patterned. The patterning is performed by, for example, dry etching.
[0048] Fig. 15 is a cross-sectional view for explaining the fourth insulating layer forming step S11. As shown in Fig. 15, in the fourth insulating layer forming step S11, an insulating layer 80 is formed. The insulating layer 80 is formed by, for example, sputtering. Note that the insulating layer 80 is etched to form an opening that partially exposes the solid electrolyte layer 70.
[0049] Fig. 16 is a cross-sectional view for explaining the second porous metal layer forming step S12. As shown in Fig. 16, in the second porous metal layer forming step S12, a porous metal layer 90 is formed. The porous metal layer 90 is formed by forming and patterning a material constituting the porous metal layer 90. This film formation is performed by, for example, sputtering. This patterning is performed by, for example, dry etching.
[0050] In the cavity forming step S13, the cavity 10c is formed by, for example, wet etching. In this manner, the gas sensor 100 having the structure shown in FIG.
[0051] (Effects of the gas sensor and the manufacturing method thereof according to the embodiment) The effects of the gas sensor 100 and the method for manufacturing the gas sensor 100 will be described below.
[0052] When attempting to form the porous metal layer 60 by sputtering, it is necessary to perform the sputtering under conditions of low vacuum, and therefore a general-purpose sputtering device cannot be used. That is, when attempting to form the porous metal layer 60 by sputtering, a dedicated sputtering device capable of performing sputtering under conditions of low vacuum is required, which increases the manufacturing cost.
[0053] On the other hand, in the manufacturing method of the gas sensor 100, the porous metal layer 60 is formed by depositing the constituent material of the porous metal layer 60 from a direction inclined with respect to the main surface 10a. This deposition can be realized by using a general-purpose deposition apparatus. In addition, in the manufacturing method of the gas sensor 100, the porous oxide layer 50 is also formed by the same method as the porous metal layer 60, so that the deposition apparatus used for forming the porous metal layer 60 can be also used for forming the porous oxide layer 50. Therefore, the gas sensor 100 and the manufacturing method of the gas sensor 100 can reduce manufacturing costs.
[0054] When the porous metal layer 60 is formed by sputtering, it is necessary to perform the sputtering under conditions of a low degree of vacuum, which may result in a low in-plane uniformity in the thickness of the porous metal layer 60. On the other hand, in the method for manufacturing the gas sensor 100, the substrate 10 is rotated about an axis of rotation along the normal to the main surface 10a when vapor deposition is performed. Therefore, according to the gas sensor 100 and the method for manufacturing the gas sensor 100, the in-plane uniformity in the thickness of the porous metal layer 60 is maintained even if vapor deposition is performed from a direction inclined with respect to the normal to the main surface 10a.
[0055] In addition, in the manufacturing method of the gas sensor 100, since the substrate 10 is rotated around a rotation axis along the normal line of the main surface 10a during deposition, the porous metal layer 60 is composed of a plurality of spiral structures 61.
[0056] When the gas sensor 100 is in operation, the solid electrolyte layer 70 is heated to a high temperature (when the solid electrolyte layer 70 is made of yttria-stabilized zirconia, it is heated to about 500° C.), and thermal stress acts on the solid electrolyte layer 70. In the gas sensor 100, the helical structure 61 acts like a spring to relieve the thermal stress acting on the solid electrolyte layer 70, thereby preventing the solid electrolyte layer 70 from being damaged by the thermal stress.
[0057] Fig. 17 is a graph showing the relationship between the deposition direction of the constituent material of the porous metal layer 60 and the relative density of the porous metal layer 60. In Fig. 17, the horizontal axis represents the angle (unit: °) between the deposition direction of the constituent material of the porous metal layer 60 and the normal line of the main surface 10a, and the vertical axis represents the relative density (no unit) of the porous metal layer 60. As shown in Fig. 17, by depositing the constituent material of the porous metal layer 60 from a direction inclined by 80° or more and less than 90° with respect to the main surface 10a, the relative density of the porous metal layer 60 can be made 0.5 or less.
[0058] As the relative density of the porous metal layer 60 decreases, the number of voids in the porous metal layer 60 increases, which increases the deformability of the porous metal layer 60 and facilitates the relaxation of thermal stress applied to the solid electrolyte layer 70. Therefore, by depositing the constituent material of the porous metal layer 60 from a direction inclined at an angle of 80° or more and less than 90° with respect to the main surface 10a (setting the relative density of the porous metal layer 60 to 0.5 or less), damage to the solid electrolyte layer 70 due to thermal stress is suppressed.
[0059] Although the embodiment of the present disclosure has been described above, the above-mentioned embodiment can be modified in various ways. The scope of the present invention is not limited to the above-mentioned embodiment. The scope of the present invention is defined by the claims, and is intended to include all modifications within the meaning and scope equivalent to the claims. [Explanation of symbols]
[0060] 10 substrate, 10a, 10b main surface, 10c cavity, 20 insulating layer, 21 first layer, 22 second layer, 23 third layer, 24 fourth layer, 25 fifth layer, 26 sixth layer, 27 membrane portion, 30 wiring, 31 adhesion layer, 31a first portion, 31b second portion, 32 heater portion, 40 wiring, 41 adhesion layer, 42 temperature sensor portion, 50 porous oxide layer, 51 helical structure, 52 aggregation nucleus, 60 porous metal layer, 61 helical structure, 70 solid electrolyte layer, 80 insulating layer, 90 porous metal layer, 100 gas sensor, S1 preparation step, S2 first insulating layer forming step, S3 first wiring forming step, S4 second insulating layer forming step, S5 second wiring forming step, S6 third insulating layer forming step, S7 porous oxide layer forming step, S8 First porous metal layer forming step, S9 solid electrolyte layer forming step, S10 patterning step, S11 fourth insulating layer forming step, S12 second porous metal layer forming step, S13 cavity forming step.
Claims
1. forming an insulating layer on a major surface of a substrate; forming a porous oxide layer on the insulating layer; forming a porous metal layer on the porous oxide layer; the step of forming the porous metal layer is carried out by depositing a constituent material of the porous metal layer in a direction inclined with respect to a normal line of the main surface, The method for manufacturing a gas sensor, wherein the step of forming the porous oxide layer is performed by depositing a constituent material of the porous oxide layer in a direction inclined with respect to a normal line of the main surface.
2. 2. The method for manufacturing a gas sensor according to claim 1, wherein the step of forming the porous metal layer is performed while rotating the substrate at least once around a rotation axis along a normal line to the main surface.
3. 3. The method for manufacturing a gas sensor according to claim 1, wherein the step of forming the porous metal layer is performed by depositing a constituent material of the porous metal layer from a direction inclined at an angle of 80° or more and less than 90° with respect to a normal to the main surface.
4. The method for manufacturing a gas sensor according to claim 1 , wherein the step of forming the porous metal layer and the step of forming the porous oxide layer are performed in the same deposition apparatus.
Citation Information
Patent Citations
Limiting current-type oxygen sensor and its manufacture
JP1999304754A
Electrode
JP2002170557A
Glancing Angle Deposition of Thin Films
JP2002509188A
Sputtering apparatus
JP2006104525A
Limiting current type gas sensor
WO2017014033A1