Gas Sensors
A gas sensor with a movable membrane section and through hole design mitigates thermal stress on the solid electrolyte layer, preventing damage and ensuring sensor reliability.
Patent Information
- Application Number
- JP2021090825
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-31
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-05-31
AI Technical Summary
The solid electrolyte layer in existing gas sensors is prone to damage due to thermal stress when heated to high temperatures.
The gas sensor design includes a substrate with a cavity and a movable membrane section, where the solid electrolyte layer is positioned on a movable part that can move along the substrate's thickness direction, alleviating thermal stress through a through hole formation.
This design effectively suppresses damage to the solid electrolyte layer by allowing it to expand freely, reducing the risk of cracking and maintaining sensor functionality.
Smart Images

Figure 0007591976000001 
Figure 0007591976000002 
Figure 0007591976000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to gas sensors. [Background technology]
[0002] The gas sensor described in WO 2017 / 014033 (Patent Document 1) has a substrate, an insulating layer, a solid electrolyte layer, and a microheater. A cavity penetrating the substrate in the thickness direction is formed in the substrate. The insulating layer is disposed on the substrate. The insulating layer has a portion on the substrate surrounding the cavity (hereinafter referred to as the "peripheral portion"), and a portion on the cavity and connected to the peripheral portion (hereinafter referred to as the "membrane portion"). The solid electrolyte layer is on the membrane portion. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2017 / 014033 Summary of the Invention [Problem to be solved by the invention]
[0004] During operation of the gas sensor described in Patent Document 1, the solid electrolyte layer is heated to a high temperature (for example, to about 500° C.) by the microheater. As a result, in the gas sensor described in Patent Document 1, the solid electrolyte layer may be damaged by thermal stress.
[0005] The present disclosure provides a gas sensor capable of preventing a solid electrolyte layer from being damaged due to thermal stress. [Means for solving the problem]
[0006] The gas sensor of the present disclosure includes a substrate, an insulating layer disposed on the substrate, and a solid electrolyte layer. A cavity penetrating the substrate in a thickness direction is formed in the substrate. The insulating layer has a peripheral portion disposed on the substrate around the cavity, and a membrane portion located on the cavity and connected to the peripheral portion. The membrane portion includes a movable portion. The movable portion is displaceable along the thickness direction of the substrate by forming a through hole penetrating the membrane portion around the movable portion in the thickness direction of the substrate. The solid electrolyte layer is disposed on the movable portion. Effect of the Invention
[0007] According to the gas sensor of the present disclosure, it is possible to prevent the solid electrolyte layer from being damaged due to thermal stress. [Brief description of the drawings]
[0008] [Figure 1A] FIG. 2 is a plan view of the gas sensor 100. [Figure 1B] 1 is a plan view of the gas sensor 100 in which the insulating layer 70 and the porous metal layer 80 are omitted. [Diagram 2] FIG. 1B is a cross-sectional view taken along line II-II in FIG. 1A. [Diagram 3] FIG. 1B is a cross-sectional view taken along line III-III in FIG. 1A. [Figure 4] 3A to 3C are process diagrams illustrating a method for manufacturing the gas sensor 100. [Diagram 5] FIG. 11 is a cross-sectional view illustrating a first insulating layer forming step S2. [Figure 6] FIG. 11 is a cross-sectional view for explaining a wiring forming step S3. [Figure 7] FIG. 11 is a cross-sectional view illustrating a second insulating layer forming step S4. [Figure 8] FIG. 11 is a cross-sectional view illustrating a porous oxide layer forming step S5. [Figure 9] FIG. 11 is a cross-sectional view illustrating a first porous metal layer forming step S6. [Figure 10] FIG. 11 is a cross-sectional view illustrating a solid electrolyte layer forming step S7. [Figure 11] FIG. 11 is a cross-sectional view for explaining the patterning step S8. [Figure 12] FIG. 11 is a cross-sectional view illustrating a third insulating layer forming step S9. [Figure 13] FIG. 11 is a cross-sectional view illustrating the second porous metal layer forming step S10. [Figure 14] FIG. 11 is a cross-sectional view for explaining a through hole forming step S11. [Figure 15] 1 is a cross-sectional view of a gas sensor 100 according to a first modified example. [Figure 16] FIG. 11 is a plan view of the gas sensor 100 according to Modification 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The details of the embodiments of the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are designated by the same reference numerals, and redundant description will not be repeated.
[0010] (Configuration of the gas sensor according to the embodiment) The configuration of a gas sensor according to an embodiment (hereinafter referred to as "gas sensor 100") will be described below. The gas sensor 100 is, for example, an oxygen / humidity sensor. However, the gas sensor 100 is not limited to this.
[0011] FIG. 1A is a plan view of the gas sensor 100. FIG. 1B is a plan view of the gas sensor 100, in which the insulating layer 70 and the porous metal layer 80 are omitted. FIG. 2 is a cross-sectional view taken along II-II in FIG. 1A. FIG. 3 is a cross-sectional view taken along III-III in FIG. 1A. In FIG. 1A, the wiring 30 is indicated by a dotted line. As shown in FIGS. 1A, 1B, 2, and 3, the gas sensor 100 includes a substrate 10, an insulating layer 20, a wiring 30, a porous oxide layer 40, a porous metal layer 50, a solid electrolyte layer 60, an insulating layer 70, and a porous metal layer 80.
[0012] The substrate 10 has a first main surface 10a and a second main surface 10b. The first main surface 10a and the second main surface 10b are end surfaces in the thickness direction of the substrate 10. The second main surface 10b is the opposite surface to the first main surface 10a. A cavity C is formed in the substrate 10. The cavity C penetrates the substrate 10 along the thickness direction of the substrate 10. The cavity C has a rectangular shape in a plan view (when viewed along the thickness direction of the substrate 10 from the first main surface 10a side). The substrate 10 is formed of, for example, single crystal silicon.
[0013] The insulating layer 20 is disposed on the substrate 10. More specifically, the insulating layer 20 is disposed on the first main surface 10a. The insulating layer 20 has, for example, a first layer 21, a second layer 22, a third layer 23, and a fourth layer 24.
[0014] The first layer 21 is disposed on the substrate 10 (first main surface 10a). The first layer 21 is formed of, for example, silicon oxide. The second layer 22 is disposed on the first layer 21. The second layer 22 is formed of, for example, silicon nitride. The third layer 23 is disposed on the second layer 22. The third layer 23 is formed of, for example, silicon oxide. The fourth layer 24 is disposed on the third layer 23. The fourth layer 24 is formed of, for example, silicon oxide.
[0015] A portion of the insulating layer 20 that is disposed on the substrate 10 around the cavity C is referred to as a peripheral portion 20a. A portion of the insulating layer 20 that is located above the cavity C is referred to as a membrane portion 20b. The membrane portion 20b is connected to the peripheral portion 20a. As a result, the membrane portion 20b is supported above the cavity C.
[0016] The wiring 30 is disposed in the insulating layer 20. More specifically, the wiring 30 is disposed on the third layer 23 and covered by the fourth layer 24. The periphery of the wiring 30 is covered by a barrier layer 31. The barrier layer 31 ensures adhesion between the insulating layer 20 and the wiring 30. The wiring 30 is made of, for example, platinum. The barrier layer 31 is made of, for example, titanium oxide. Note that the portion of the barrier layer 31 disposed on the third layer 23 is referred to as a first portion 31a, and the portion of the barrier layer 31 covering the wiring 30 is referred to as a second portion 31b.
[0017] The wiring 30 has a heater portion 30a, an end portion 30b, and a connection portion 30c. The heater portion 30a is formed by meandering the wiring 30. The heater portion 30a is disposed in the membrane portion 20b. The end portion 30b is disposed in the peripheral portion 20a. The connection portion 30c connects the heater portion 30a and the end portion 30b.
[0018] The porous oxide layer 40 is disposed on the insulating layer 20. The porous oxide layer 40 is formed of, for example, tantalum oxide. Since the porous oxide layer 40 is porous, it serves as a flow path for a gas to be detected by the gas sensor 100 (a gas to be detected).
[0019] The porous metal layer 50 is disposed on the porous oxide layer 40. The porous metal layer 50 is formed of, for example, platinum. The porous metal layer 50 has an electrode portion 50a, an end portion 50b, and a connection portion 50c. The electrode portion 50a is located on the membrane portion 20b with the porous oxide layer 40 interposed therebetween. The end portion 50b is located on the peripheral portion 20a with the porous oxide layer 40 interposed therebetween. The connection portion 30c connects the electrode portion 50a and the end portion 50b.
[0020] The solid electrolyte layer 60 is disposed on the porous metal layer 50. More specifically, the solid electrolyte layer 60 is disposed on the electrode portion 50a. The solid electrolyte layer 60 has ion conductivity. The solid electrolyte layer 60 is formed of, for example, yttria-stabilized zirconia.
[0021] The insulating layer 70 is disposed on the insulating layer 20 so as to cover the porous oxide layer 40, the porous metal layer 50, and the solid electrolyte layer 60. However, the insulating layer 70 has an opening that at least partially exposes the upper surface of the solid electrolyte layer 60. The insulating layer 70 is, for example, a layer in which a layer made of silicon oxide and a layer made of tantalum oxide are stacked.
[0022] The pad portion 30d and the pad portion 50d are disposed on the insulating layer 70. The pad portion 30d is electrically connected to the end portion 30b through an opening (not shown) formed in the insulating layer 20 (fourth layer 24) and the insulating layer 70 so as to expose the end portion 30b. The pad portion 50d is electrically connected to the end portion 50b through an opening (not shown) formed in the insulating layer 70 so as to expose the end portion 50b.
[0023] The porous metal layer 80 has an electrode portion 80a, a pad portion 80b, and a connection portion 80c. The electrode portion 80a is disposed on the solid electrolyte layer 60. The pad portion 80b is disposed on the insulating layer 20 with the insulating layer 70 interposed therebetween. The connection portion 80c connects the electrode portion 80a and the pad portion 80b.
[0024] A through hole TH is formed in the membrane portion 20b and the insulating layer 70 on the membrane portion 20b. The through hole TH penetrates the membrane portion 20b and the insulating layer 70 along the thickness direction of the substrate 10. The membrane portion 20b has a movable portion 20c. The through hole TH is formed around the movable portion 20c. This allows the movable portion 20c to be displaced along the thickness direction of the substrate 10 with the base end side of the movable portion 20c as a fulcrum. The through hole TH is, for example, U-shaped. The heater portion 30a, the electrode portion 50a, the solid electrolyte layer 60, and the electrode portion 80a are on the movable portion 20c.
[0025] The width of the wiring 30 constituting the connection portion 30c at the base end of the movable portion 20c is greater than the width of the wiring 30 constituting the heater portion 30a.
[0026] (Operation of the gas sensor 100 according to the embodiment) The following describes the operation of the gas sensor 100. Here, the operation of the gas sensor 100 will be described taking as an example the case of detecting oxygen gas in a detection target gas.
[0027] When a current flows through the wiring 30, the heater section 30a generates heat by resistance. This heats the solid electrolyte layer 60, causing it to exhibit ion conductivity. When the solid electrolyte layer 60 is made of yttria-stabilized zirconia, the solid electrolyte layer 60 is heated to about 500° C. by the heater section 30a.
[0028] The pad portion 50d and the pad portion 80b are connected to the negative and positive electrodes of a power source, respectively. The detected gas passes through the porous oxide layer 40 and the electrode portion 50a and reaches the interface between the electrode portion 50a and the solid electrolyte layer 60. Oxygen gas in the detected gas that reaches the interface between the electrode portion 50a and the solid electrolyte layer 60 receives electrons from the electrode portion 50a and becomes oxygen ions.
[0029] These oxygen ions pass through the solid electrolyte layer 60 and reach the interface between the solid electrolyte layer 60 and the electrode section 80a. The oxygen ions that reach the interface between the solid electrolyte layer 60 and the electrode section 80a release electrons to the electrode section 80a and become oxygen gas. This causes a current to flow between the pad section 50d and the pad section 80b. This current is proportional to the concentration of oxygen gas in the detected gas. Therefore, by detecting this current, the concentration of oxygen gas in the detected gas can be measured.
[0030] (Method of Manufacturing the Gas Sensor 100 According to the Embodiment) A method for manufacturing the gas sensor 100 will now be described.
[0031] Fig. 4 is a process diagram showing a method for manufacturing the gas sensor 100. As shown in Fig. 4, the method for manufacturing the gas sensor 100 includes a preparation step S1, a first insulating layer forming step S2, a wiring forming step S3, a second insulating layer forming step S4, a porous oxide layer forming step S5, a first porous metal layer forming step S6, a solid electrolyte layer forming step S7, a patterning step S8, a third insulating layer forming step S9, a second porous metal layer forming step S10, a through-hole forming step S11, and a cavity forming step S12.
[0032] In the preparation step S1, a substrate 10 is prepared. Note that the substrate 10 prepared in the preparation step S1 does not have a cavity C formed therein.
[0033] Fig. 5 is a cross-sectional view for explaining the first insulating layer forming step S2. As shown in Fig. 5, in the first insulating layer forming step S2, a first layer 21, a second layer 22, and a third layer 23 are formed in sequence. The first layer 21, the second layer 22, and the third layer 23 are formed, for example, by using a CVD (Chemical Vapor Deposition) method.
[0034] 6 is a cross-sectional view for explaining the wiring formation step S3. As shown in FIG. 6, in the wiring formation step S3, a wiring 30 and a barrier layer 31 are formed. In the wiring formation step S3, first, a first portion 31a is formed. The first portion 31a is formed by depositing and patterning a material constituting the barrier layer 31. This deposition is performed by using, for example, a sputtering method. This patterning is performed by forming a mask using a photolithography method and etching using the mask.
[0035] In the wiring formation process S3, secondly, the wiring 30 is formed. The wiring 30 is formed by depositing and patterning a material constituting the wiring 30. This deposition is performed, for example, by sputtering. This patterning is performed by forming a mask using photolithography and etching using the mask. In the wiring formation process S3, thirdly, the second portion 31b is formed. The second portion 31b is formed by depositing and patterning a material constituting the barrier layer 31. This deposition is performed, for example, by sputtering. This patterning is performed by forming a mask using photolithography and etching using the mask.
[0036] Fig. 7 is a cross-sectional view for explaining the second insulating layer forming step S4. As shown in Fig. 7, in the second insulating layer forming step S4, a fourth layer 24 is formed. The fourth layer 24 is formed, for example, by using a CVD method. Fig. 8 is a cross-sectional view for explaining the porous oxide layer forming step S5. As shown in Fig. 8, in the porous oxide layer forming step S5, a porous oxide layer 40 is formed. The porous oxide layer 40 is formed, for example, by using a vapor deposition method.
[0037] Fig. 9 is a cross-sectional view for explaining the first porous metal layer forming step S6. As shown in Fig. 9, in the first porous metal layer forming step S6, a porous metal layer 50 is formed. The porous metal layer 50 is formed by using, for example, a sputtering method.
[0038] FIG. 10 is a cross-sectional view for explaining the solid electrolyte layer forming step S7. As shown in FIG. 10, in the solid electrolyte layer forming step S7, the solid electrolyte layer 60 is formed. The solid electrolyte layer 60 is formed by forming and patterning a material constituting the solid electrolyte layer 60. The film is formed by using, for example, a sputtering method. The patterning is performed by, for example, dry etching. FIG. 11 is a cross-sectional view for explaining the patterning step S8. As shown in FIG. 11, in the patterning step S8, the porous oxide layer 40 and the porous metal layer 50 are patterned. The patterning is performed by, for example, dry etching.
[0039] FIG. 12 is a cross-sectional view for explaining the third insulating layer forming step S9. As shown in FIG. 12, in the third insulating layer forming step S9, an insulating layer 70 is formed. The insulating layer 70 is formed by, for example, a sputtering method. The insulating layer 70 is etched to form an opening for exposing the solid electrolyte layer 60. FIG. 13 is a cross-sectional view for explaining the second porous metal layer forming step S10. As shown in FIG. 13, in the second porous metal layer forming step S10, a porous metal layer 80 is formed. The porous metal layer 80 is formed by forming and patterning a material constituting the porous metal layer 80. This film formation is performed by, for example, a sputtering method. This patterning is performed by, for example, dry etching.
[0040] Fig. 14 is a cross-sectional view for explaining the through hole forming step S11. As shown in Fig. 14, in the through hole forming step S11, a through hole TH is formed in the insulating layer 20 and the insulating layer 70. The through hole TH is formed by, for example, dry etching. In the cavity forming step S12, a cavity C is formed. The cavity C is formed by, for example, wet etching. In this manner, the gas sensor 100 having the structure shown in Figs. 1A, 1B, 2, and 3 is formed.
[0041] (Effects of the gas sensor according to the embodiment) The effects of the gas sensor 100 according to the embodiment will be described below.
[0042] When the gas sensor 100 detects a gas to be detected, the heater section 30a heats the solid electrolyte layer 60. If the membrane section 20b restricts the thermal expansion of the solid electrolyte layer 60 when the solid electrolyte layer 60 is heated by the heater section 30a, the solid electrolyte layer 60 may crack due to thermal stress. This is noticeable when the solid electrolyte layer 60 is made of a material that requires high heating temperature, such as yttria-stabilized zirconia.
[0043] However, in the gas sensor 100, the membrane portion 20b has a movable portion 20c, and the solid electrolyte layer 60 is disposed on the movable portion 20c. The movable portion 20c is displaceable along the thickness direction of the substrate 10 due to the through holes TH formed around the periphery thereof. Therefore, when the solid electrolyte layer 60 is heated, the movable portion 20c is displaced to relieve the thermal stress applied to the solid electrolyte layer 60, and the solid electrolyte layer 60 is less likely to crack.
[0044] In the gas sensor 100, the width of the wiring 30 constituting the connection portion 30c at the base end of the movable portion 20c is larger than the width of the wiring 30 constituting the heater portion 30a. Therefore, in the gas sensor 100, breakage of the wiring 30 due to displacement of the movable portion 20c is suppressed.
[0045] (Variation 1) FIG. 15 is a cross-sectional view of the gas sensor 100 according to the first modification. As shown in FIG. 15, the insulating layer 20 may further include a fifth layer 25 disposed on the fourth layer 24 and a sixth layer 26 disposed on the fifth layer 25. The fifth layer 25 is made of, for example, silicon nitride. The sixth layer 26 is made of, for example, silicon oxide. The gas sensor 100 may further include a wiring 90. The wiring 90 is made of, for example, platinum. The wiring 90 is disposed in the insulating layer 20. More specifically, the wiring 90 is disposed on the fifth layer 25 and is covered by the sixth layer 26.
[0046] A barrier layer 91 is disposed around the wiring 90. The barrier layer 91 is formed of, for example, titanium oxide, and ensures adhesion between the barrier layer 91 and the insulating layer 20 (the fifth layer 25 and the sixth layer 26). The wiring 90 has a portion that is disposed in a serpentine manner in the movable part 20c, and this portion constitutes a temperature sensor part 90a.
[0047] (Variation 2) Fig. 16 is a plan view of the gas sensor 100 according to Modification 2. The through hole TH may be formed in a curved shape in plan view as shown in Fig. 16. This makes it possible to suppress stress concentration around the movable part 20c.
[0048] Although the embodiment of the present disclosure has been described above, the above-mentioned embodiment can be modified in various ways. The scope of the present invention is not limited to the above-mentioned embodiment. The scope of the present invention is defined by the claims, and is intended to include all modifications within the meaning and scope equivalent to the claims. [Explanation of symbols]
[0049] 10 substrate, 10a first main surface, 10b second main surface, 20 insulating layer, 20a peripheral portion, 20b membrane portion, 20c movable portion, 21 first layer, 22 second layer, 23 third layer, 24 fourth layer, 25 fifth layer, 26 sixth layer, 30 wiring, 30a heater portion, 30b end portion, 30c connection portion, 30d pad portion, 31 barrier layer, 31a first portion, 31b second portion, 40 porous oxide layer, 50 porous metal layer, 50a electrode portion, 50b end portion, 50c connection portion, 50d pad portion, 60 solid electrolyte layer, 70 insulating layer, 80 porous metal layer, 80a electrode portion, 80b pad portion, 80c connection portion, 90 wiring, 90a temperature sensor portion, 91 barrier layer, 90a Temperature sensor section, 100 Gas sensor, C cavity, S1 Preparation process, S2 First insulating layer forming process, S3 Wiring forming process, S4 Second insulating layer forming process, S5 Porous oxide layer forming process, S6 First porous metal layer forming process, S7 Solid electrolyte layer forming process, S8 Patterning process, S9 Third insulating layer forming process, S10 Second porous metal layer forming process, S11 Through-hole formation process, S12 cavity formation process, TH through-hole.
Claims
1. A substrate; an insulating layer disposed on the substrate; A solid electrolyte layer; The substrate has a cavity formed therein, the cavity penetrating the substrate in a thickness direction, the insulating layer has a peripheral portion disposed on the substrate around the cavity, and a membrane portion over the cavity and connected to the peripheral portion; The membrane portion includes a movable portion, the movable portion is displaceable along the thickness direction by forming a through hole penetrating the membrane portion around the movable portion in the thickness direction, the solid electrolyte layer is disposed on the movable part, The gas sensor, wherein the through hole is formed in a curved shape in a plan view.
2. 2. The gas sensor according to claim 1, wherein the solid electrolyte layer is made of yttria-stabilized zirconia.
3. Further comprising wiring disposed in the insulating layer, The wiring includes a heater portion disposed in the movable portion and a heater portion disposed in the peripheral portion. and a connection portion connecting the heater portion and the end portion, The width of the wiring constituting the connection portion at the base end of the movable portion is 3. The gas sensor according to claim 1, wherein the width of the first wiring is larger than that of the second wiring.
Citation Information
Patent Citations
Gas sensor and gas detector
JP1996247981A
Method for driving hydrogen gas sensor device, and hydrogen gas sensor device using the same
JP2016085131A
Nitroxide based gas sensor, oxygen pump, gas sensor device, manufacturing method of gas sensor device, and sensor network system
JP2017191021A
Gas sensor and gas sensing apparatus
KR1020180085186A
Nanopore-containing substrates with aligned nanoscale electronic elements and methods of making and using same