Steel processing method and rolling part manufacturing method

By controlling the strain ratio εx/εx' during rolling or forging processes, the method addresses the issue of gaps in rolling components, improving their fatigue life and adhesion, thus enhancing the performance of components like bearings.

JP7595735B2Active Publication Date: 2024-12-06SANYO SPECIAL STEEL CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023202877
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-12-26
Filing Date
2023-11-30
Publication Date
2024-12-06
Estimated Expiration
2043-11-30

AI Technical Summary

Technical Problem

Existing methods for manufacturing rolling components fail to effectively control the deformation phenomenon of nonmetallic inclusions and the surrounding matrix, leading to gaps that reduce the rolling fatigue life of components like bearings.

Method used

A method is developed to control the strain ratio εx/εx' by applying compressive stress during the rolling or forging process, using a rolling or forging analysis model to determine the reduction rate, ensuring the strain ratio remains below a predetermined value to enhance adhesion between the matrix and nonmetallic inclusions.

Benefits of technology

This approach results in rolling components with improved rolling fatigue life by reducing gaps and enhancing adhesion at the interface, thereby extending the lifespan of components such as bearings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595735000003
    Figure 0007595735000003
  • Figure 0007595735000004
    Figure 0007595735000004
  • Figure 0007595735000005
    Figure 0007595735000005
Patent Text Reader

Abstract

To manufacture a rolling component of an excellent rolling life.SOLUTION: A steel material machining method for applying compression stress to a base material made of a steel material including a nonmetal inclusion to machine it into a shape different from that of the base material is characterized by determining a rolling reduction when the compression stress is applied to the steel material using a distortion ratio εx / εx' as a management index, in which εx' denotes distortion in the extending direction of a contact when the contact between the nonmetal inclusion and a host phase of the steal material reaches a reversal position where the direction of shearing stress is reversed, and εx denotes distortion when a contact corresponding part of a steel material having no nonmetal inclusion corresponding to the contact reaches the reversal position where the direction of shearing stress is reversed.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a processing method for applying compressive stress to a steel material containing nonmetallic inclusions to perform processing. [Background technology]

[0002] In recent years, with the increasing performance of various mechanical devices, mechanical parts and equipment that require a long rolling fatigue life are becoming increasingly The operating environment in these facilities has become extremely severe, and the lifespan of these machine parts and devices must be improved. There is a strong demand for improved reliability. It is known that steel parts such as bearings inevitably contain foreign matter called non-metallic inclusions due to the manufacturing processes of steel, such as the refining process, casting process, and solidification process.

[0003] Furthermore, in steel parts such as bearings manufactured through rolling and forging processes, gaps may form around nonmetallic inclusions. It is believed that these gaps occur at the interface due to differences in deformability between the nonmetallic inclusions and the parent steel. For example, when the steel part is a bearing, the above-mentioned gaps may promote crack generation in the bearing part that is subjected to rolling fatigue during use, and may become the starting point of the cracks. Similar issues exist in rolling parts other than bearings that require a good rolling fatigue life.

[0004] Therefore, in order to improve the rolling fatigue life of rolling parts such as bearings, it is effective to reduce the gaps around the non-metallic inclusions.

[0005] Patent Document 1 discloses a method for manufacturing a ring-shaped mechanical component having a rolling part with excellent rolling fatigue life, characterized in that, in the manufacture of a mechanical component having a rolling part on which a rolling part rolls on the inner diameter of a ring-shaped material, the rolling part on which the rolling part rolls is formed on the inner diameter surface of the ring-shaped material by forging in which a compressive hydrostatic stress of 1.5 times or more the yield stress of the material is applied to the inner diameter surface of the ring-shaped material on which the rolling part is to be formed, resulting in a compressive strain of 0.10 or more in plastic strain in the rolling direction of the rolling part. As a result, voids present at the interface between non-metallic inclusions in the steel and the steel parent phase tend to close, making it possible to manufacture a mechanical component with excellent rolling fatigue life.

[0006] Patent Document 2 discloses a method for manufacturing a ring-shaped mechanical component, which includes a step of forming rolling parts by cold forging by applying a hydrostatic stress of at least 1000 MPa to the inner diameter surface of a ring-shaped processed base material to be subjected to cold forging to form rolling parts, using upper and lower punches that smoothly reduce in diameter toward their tips, and discloses that the action of the hydrostatic stress causes voids present at the interface between non-metallic inclusions in the steel and the steel parent phase to tend to close. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Patent No. 5896713 [Patent Document 2] Patent No. 5669128 [Patent Document 3] Patent No. 2923095 [Patent Document 4] JP 2014-55346 A [Non-patent literature]

[0008] [Non-Patent Document 1] Light Metals / Vol.42 No.2(1992) Present status of finite element analysis in plastic processing [Non-Patent Document 2] Kobe Steel Techniques / Vol.48 No.1 (Apr.1998) Special issue on plastic processing. Effect of entry side calculation region length on plate thickness distribution in steady plate rolling analysis. Summary of the Invention [Problem to be solved by the invention]

[0009] In the above-mentioned Patent Documents 1 and 2, in order to close gaps that already exist inside a steel part or a preform, a certain level of hydrostatic compressive stress or compressive strain is simply applied to the steel part or preform, and the deformation phenomenon of nonmetallic inclusions and the surrounding base material is not controlled, so it is difficult to evaluate the effect of closing the gaps.

[0010] An object of the present invention is to provide a method for producing a rolling part having an excellent rolling life by controlling the deformation phenomenon of the nonmetallic inclusions and parent phase contained in a steel material. [Means for solving the problem]

[0011] In order to solve the above problems, a steel processing method is provided in which a compressive stress is applied to a base material made of a steel material containing nonmetallic inclusions, and the base material is processed into a shape different from that of the base material, the method being characterized in that a reduction ratio when applying a compressive stress to the steel material is determined using a strain ratio εx / εx' as a control index, where εx' is the strain in the extension direction of a contact point between a nonmetallic inclusion and a base phase of the steel material when the contact point reaches a reversal position where the direction of the shear stress is reversed, and εx is the strain in the extension direction of a contact point corresponding to the contact point of a steel material without nonmetallic inclusions when the contact point reaches a reversal position where the direction of the shear stress is reversed.

[0012] (2) The method for processing a steel material according to (1) above, characterized in that the compressive stress is imparted to the steel material by a rolling or forging roll.

[0013] (3) A method for processing a steel material according to the above (2), characterized in that a reduction ratio of a rolling or forging roll for suppressing the distortion ratio εx / εx' to a predetermined value or less is obtained in advance by a rolling or forging analysis model, and the steel material is rolled or forged at the reduction ratio.

[0014] (4) A method for manufacturing a rolling part, comprising processing a semi-finished product manufactured by the method for processing a steel material according to any one of (1) to (3) above into a shape of the rolling part. Effect of the Invention

[0015] According to the present invention, by controlling the deformation phenomenon of the parent phase and non-metallic inclusions contained in the steel material, it is possible to provide rolling parts such as bearings having an excellent rolling life. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is an explanatory diagram for explaining a rolling analysis method. [Diagram 2] 1 shows a shear stress distribution in the plate model 11 obtained at a certain timing during rolling. [Diagram 3] FIG. 2 is an explanatory diagram of a leading region and a reversing region. [Figure 4] FIG. 1 is a schematic diagram of a contact point between a nonmetallic inclusion and a parent phase for explaining a distortion ε′. [Diagram 5] FIG. 1 is a schematic diagram of ring rolling. [Figure 6] 1 is a graph showing the relationship between strain εx (εx') and rolling reduction (Example). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] The present inventors have discovered a processing method for steel, in which compressive stress is applied to a base material made of steel containing non-metallic inclusions, and the base material is processed into a shape different from that of the base material, which can provide rolling parts such as bearings having an excellent rolling life by controlling the deformation phenomenon of the non-metallic inclusions and base phase contained in the steel.

[0018] Rolling parts include parts that require a good rolling fatigue life, such as bearings, gears, hub units, continuously variable transmissions, constant velocity joints, crank pins, piston pins, and the like.

[0019] The present inventors have clarified a method for controlling the deformation phenomenon of nonmetallic inclusions and parent phase contained in a steel material when the steel material is rolled, by analyzing the rolling analysis model based on a known rigid-plastic finite element method (see Non-Patent Document 1). CAE analysis was used for the rolling analysis.

[0020] CAE analysis is an abbreviation of Computer Aided Engineering, and is an analytical method to evaluate (simulate) design problems of a product that is reproduced on a computer. CAE analysis is realized by a computer program.

[0021] Fig. 1 is an explanatory diagram for explaining a rolling analysis method. The relationship between the gap generation behavior around the nonmetallic inclusion L and the strain when a sheet model 11 is rolled using a pair of upper and lower rolls 12 is analyzed. The contact condition between the nonmetallic inclusion L and the parent phase is defined by the shear friction coefficient, and the shear stress and strain history when the nonmetallic inclusion L passes from the entry side to the exit side of the rolls 12 are obtained. Here, the strain refers to the plastic strain at the contact point between the nonmetallic inclusion L and the parent phase in the stretching direction of the sheet model 11 (the X-axis direction in Fig. 1).

[0022] The parameters to be given to the rolling analysis model include, in addition to the contact conditions (shear friction coefficient) between the nonmetallic inclusions L and the parent phase described above, representative examples include plate thickness, hot or cold conditions (temperature, etc.), positions and sizes of the nonmetallic inclusions, positions and sizes of gaps existing around the nonmetallic inclusions, rolling reduction, physical property data of the material (Young's modulus, Poisson's ratio, stress-strain curve), roll diameter and peripheral speed of the rolling rolls, and shear friction coefficient between the rolling rolls and the plate model. The rolling reduction is the degree of rolling processing expressed as a percentage, and is calculated by the formula (h1-h2) / h1, where h1 and h2 are the thicknesses of the material before and after rolling, respectively. These parameters can be ascertained by prior analysis of the properties of the steel material used in rolling parts such as bearings. When two or more nonmetallic inclusions L are present, it is desirable to assume the rolling part after machining and target the nonmetallic inclusion L that is located closer to the surface of the rolling part. This is because it is believed that the shorter the distance from the nonmetallic inclusion L to the surface of the rolling part, the greater the relative harmfulness it poses to the rolling part.

[0023] FIG. 2 shows the shear stress distribution of the plate model 11 acquired at a certain timing during rolling, with the magnitude and positive and negative of the shear stress color-coded. From the shear stress distribution, it is possible to identify the position where the direction of the shear stress reverses (hereinafter also referred to as the reversal position). In other words, from the shear stress distribution in FIG. 2, it is possible to grasp the position where the positive and negative of the shear stress changes, that is, the reversal position. The dotted line in the figure indicates the reversal position of the nonmetallic inclusion L.

[0024] The concept of the reversal position can be defined by the backward movement zone and the pre-deformation zone. In other words, the reversal position is located at the boundary between the backward movement zone and the pre-deformation zone. The backward movement zone will be described with reference to FIG. 3. The speed of the sheet model 11 at the roll entry side (point A) is V A The speed of the plate model 11 at the exit (point B) is V B When defined as above, V A and V B The magnitude relationship of V A <V B The velocity V of the plate model 11 N The point (point N) where the speed becomes equal to the peripheral speed V of the roll is called the neutral point, and the area in front of the neutral point (the roll exit side) is the leading zone, and the area behind the neutral point (the roll entry side) is the astern zone. The definitions of the leading zone and the astern zone are also described in Patent Document 3.

[0025] The pre-deformation region is a region on the inlet side of the rolling rolls 12 where the plate thickness starts to decrease before the rolled material comes into contact with the rolling rolls 12 due to the force of the rolls 12 pulling the material in. Since it is technically common knowledge that the rolled material deforms before it comes into contact with the rolls, that is, it is pre-deformed (for example, see Non-Patent Document 2), a detailed explanation will be omitted.

[0026] The inventors then focused on ε', which is the strain in the longitudinal direction (x-axis direction) of the plate model 11 when the nonmetallic inclusion L reaches the reversal position. More specifically, as shown in the schematic diagram of Fig. 4, they focused on the contact point between the nonmetallic inclusion L and the parent phase when the nonmetallic inclusion L reaches the reversal position, and found ε', which is the strain at this contact point in the x-axis direction, from the strain history.

[0027] A similar rolling analysis is also performed on a uniform plate model that does not include nonmetallic inclusions L, and εx, which is the strain in the longitudinal direction (x-axis direction) of the plate model 11 when the contact corresponding part corresponding to the above-mentioned contact reaches the reversal position, is found, and the strain ratio εx / εx' is calculated. That is, εx, which is the strain in the x-axis direction of the contact corresponding part that has reached the reversal position, is found from the strain history, and the strain ratio εx / εx' is calculated.

[0028] Both strain εx and strain εx' increase due to rolling, but the extent of the increase differs depending on the presence or absence of nonmetallic inclusions, so it is possible to evaluate the behavior of gap generation by the strain ratio εx / εx'. The inventors have discovered that by performing rolling using the strain ratio εx / εx', which allows the evaluation of the behavior of gap generation, as a control index, it is possible to manufacture rolling parts with high adhesion between the parent phase and the nonmetallic inclusion interface and excellent fatigue life.

[0029] Specifically, the above-mentioned rolling analysis is performed multiple times while changing the reduction ratio, and thus the relationship between the reduction ratio, the distortion ratio εx / εx', and the final gap area (hereinafter also referred to as correlation information) can be grasped. Here, if the acceptance criteria for the final gap area are determined in advance, the appropriate range of the distortion ratio εx / εx' (corresponding to "not more than a predetermined value" as described in the claims) can be grasped from the correlation information. The acceptance criteria for the final gap area can be appropriately set according to the application of the rolled material, etc. Specifically, information such as "setting the distortion ratio εx / εx' to not more than a predetermined value" can be obtained as quantitative information for reducing the harmfulness of the gap. In addition, for rolling parts, a final gap area ratio of 8 to 9% or less is generally recommended.

[0030] The final gap area ratio (%) is the gap area ratio calculated after the rolling process is completed, and can be calculated by (gap cross-sectional area / non-metallic inclusion cross-sectional area) × 100. The final gap area ratio (%) is also obtained as an output value from the rolling analysis. It goes without saying that the gap cross-sectional area is the "cross-sectional area of ​​the gap in the X-Z cross section" in FIG. 4, and the non-metallic inclusion cross-sectional area is the "cross-sectional area of ​​the non-metallic inclusion in the X-Z cross section" in FIG. 4. Note that the gap cross-sectional area is preferably the "gap cross-sectional area" when the plate model 11 is cut at the center position of the non-metallic inclusion L in the plate width direction (normal direction to the paper surface in FIG. 1). From the correlation information, the reduction ratio for setting the distortion ratio εx / εx' to a predetermined value or less can be obtained. The predetermined value varies depending on the parameters given to the rolling analysis model, and is not limited in this specification. Therefore, by rolling the steel material based on the determined rolling reduction, it is possible to manufacture a semi-finished product for a rolling part having high adhesion between the parent phase and the non-metallic inclusions and excellent fatigue life. By processing the shape of this semi-finished product, it is possible to manufacture a rolling part having excellent fatigue life.

[0031] In the above embodiment, the rolling process of plate-shaped steel material has been described, but the present invention is not limited to this and can also be applied to ring rolling. Here, ring rolling refers to "a forging process in which the thickness of a ring-shaped steel material in the radial direction is reduced using several rolls to expand the diameter of the ring," and is classified as a type of rotary forging among plastic processing.

[0032] Fig. 5 is a schematic diagram of ring rolling. Referring to the figure, the forging roll is composed of a driving roll 21 and a driven roll 22. The driving roll 21 rotates by being applied with a rotational force from a driving source (not shown). The ring-shaped steel material 20 is sandwiched between the driving roll 21 and the driven roll 22, and by pressing the driven roll 22 in the Z-axis direction toward the ring-shaped steel material 20, the driven roll 22 rotates due to frictional force, and the inner diameter of the ring-shaped steel material 20 can be plastically deformed in the diameter expansion direction.

[0033] In this ring rolling, by carrying out CAE analysis using a forging analysis model, correlation information corresponding to the correlation information described above can be obtained. Based on the correlation information, the rolling reduction ratio for setting the distortion ratio εx / εx' to a predetermined value or less can be grasped.

[0034] (Example) The present invention will be specifically described with reference to examples. Using the above-mentioned rolling analysis model, the relationship between the distortion ratio εx / εx' and the rolling reduction ratio was analyzed by CAE, and the distortion ratio εx / εx' and the rolling reduction ratio for reducing the final gap area ratio to 8% or less were investigated. DEFORM-3D manufactured by Scientific Forming Technologies was used as the analysis software for the CAE analysis.

[0035] The parameters given to the model are the rolling reduction ratio, the contact condition of the nonmetallic inclusion L and the parent phase (shear friction coefficient): 0.3, the thickness of the plate model 11: 50 mm, the Young's modulus of the plate: 206 GPa, the Poisson's ratio of the plate: 0.3, JPEG0007595735000001.jpg14128 Position of nonmetallic inclusion: 1 mm from the surface, φ of nonmetallic inclusion: 1 mm, temperature condition of hot rolling: 1000°C, inclusion and parent phase: close contact (no gap), roll diameter of rolling roll: φ250 mm, roll peripheral speed: 12.6 rad / s, shear friction coefficient of rolling roll and plate model: 0.7, etc. The nonmetallic inclusion was defined as a rigid body. In this example, the acceptance standard for the final gap area ratio (%) was set to 8% or less.

[0036] The relationship between the strain εx (εx') and the reduction ratio is shown in the graph of FIG. 6. The strain εx is plotted as a black square, and the strain εx' is plotted as a black circle. In the figure, the horizontal axis is the reduction ratio (%), and the vertical axis is the strain εx (εx'). The relationship between the strain εx and the reduction ratio was fitted to a linear function, and a relational equation of y = 0.0030x - 0.018 was obtained (correlation coefficient: 0.98). Similarly, the relationship between the strain εx' and the reduction ratio was fitted to a linear function, and a relational equation of y = 0.0099x - 0.0035 was obtained (correlation coefficient: 0.98). The strain ratio εx / εx' when the reduction ratio is 2 (%), 5 (%), 10 (%), 20 (%), and 40 (%) was obtained from the above relational equation, and summarized in Table 1 together with the output final gap area ratio (%). [Table 1]

[0037] From these results, it was found that the final gap area ratio can be reduced to 8% or less by setting the strain ratio εx / εx' to 0.13 or less. Therefore, in this embodiment, it was found that by determining the rolling reduction ratio to set the strain ratio εx / εx' to 0.13 or less, it is possible to manufacture a material with high adhesion between the matrix and non-metallic inclusion interfaces and excellent fatigue life. If the parameters given to the rolling analysis model change, it is sufficient to perform the analysis process again to obtain the appropriate strain ratio εx / εx'. [Explanation of symbols]

[0038] 11 Board Model 12 Rolling mill L Nonmetallic inclusions 20 Ring-shaped steel material 21 Driving Roll 22 Follower roll

Claims

1. A method of manufacturing a rolling part, comprising processing a semi-finished product manufactured by a predetermined steel processing method into a shape of a rolling part, comprising the steps of: The method for processing the specified steel material is a method for applying compressive stress to a base material made of a steel material containing non-metallic inclusions, and processing the base material into a shape different from that of the base material, and the method for manufacturing a rolling part is characterized in that in this steel processing method, a distortion ratio εx / εx' is used as a control index to determine a rolling reduction rate when applying compressive stress to the steel material. Here, εx' is the strain in the extension direction of a contact point between a nonmetallic inclusion and the parent phase of a steel material when the contact point reaches a reversal position where the direction of the shear stress is reversed, and εx is the strain in the extension direction of a contact corresponding part of a steel material without nonmetallic inclusions when the contact corresponding part reaches a reversal position where the direction of the shear stress is reversed.

2. The method for manufacturing a rolling component according to claim 1, wherein the compressive stress is imparted to the steel material by a rolling or forging roll.

3. 3. The method for manufacturing a rolling part according to claim 2, characterized in that a reduction ratio of a rolling or forging roll for suppressing the distortion ratio εx / εx' to a predetermined value or less is obtained in advance by a rolling or forging analysis model, and the steel material is rolled or forged at the reduction ratio.

Citation Information

Patent Citations

  • Method and apparatus for manufacturing hose with reinforcing ribs of rigid resin

    JP1981069128A

  • transformer

    JP1983096713A

  • Roll for rolling, grinding method therefor and metal sheet rolling method

    JP1995265912A

  • Method and device for detecting inclusion with nonlinear ultrasonic wave

    JP2006284428A

  • Method for manufacturing machine component superior in rolling fatigue life

    JP2013121600A