Prepreg with metal layer, method for manufacturing laminate, and method for manufacturing prepreg with metal layer
Patent Information
- Application Number
- JP2022576711
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Priority Date
- 2022-01-19
- Filing Date
- 2022-01-19
- Publication Date
- 2024-11-20
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional copper foils with carriers face handling difficulties due to the thinness of the ultra-thin copper layer, leading to waste and reduced work efficiency, as they require a carrier layer for support which is eventually discarded.
A prepreg with a metal layer of 11 μm or less, where the semi-cured prepreg acts as a carrier, eliminating the need for a separate carrier layer, and allowing for the direct application of a metal layer without a carrier, enabling easier handling and reduced waste.
This approach reduces waste and increases work efficiency by eliminating the need for a carrier layer, facilitating the production of multilayer boards and improving handling during transportation, while also addressing the challenges of thin copper foil handling and reducing defects like wrinkles and tears.
Abstract
Description
Prepreg with metal layer, laminate manufacturing method, and method for manufacturing prepreg with metal layer
[0001] The present invention relates to a prepreg with a metal layer, a method for producing a laminate, and a method for producing a prepreg with a metal layer.
[0002] Copper foils with carriers have been known for some time. For example, Japanese Patent Laid-Open No. 2019-31739 discloses a copper foil with carriers that includes a carrier layer, an intermediate layer provided on the carrier layer, a release layer provided on the intermediate layer, and an ultrathin copper layer provided on the release layer.
[0003] Such a carrier-attached copper foil is placed on a prepreg and heated to make the carrier layer and intermediate layer peelable from the release layer, and the carrier layer and intermediate layer are then removed, leaving only the ultra-thin copper layer.
[0004] Conventional carrier-attached copper foils are made easier to handle by providing a carrier. The ultra-thin copper layer itself is extremely difficult, or in fact impossible, to handle due to its thinness. Therefore, a carrier is provided to make it easier to handle.
[0005] The present invention provides a technique for eliminating waste and increasing work efficiency compared to conventional copper foils with carriers.
[0006] The prepreg with a metal layer according to the present invention comprises: a metal layer having a thickness of 11 μm or less; and a semi-cured prepreg provided with the metal layer, and does not necessarily require a carrier layer for supporting the metal layer.
[0007] In the prepreg with a metal layer according to the present invention, the prepreg may have a fiber layer and a resin layer provided on the fiber layer, and the resin layer may be in a semi-cured state with an uneven surface.
[0008] In the prepreg with a metal layer according to the present invention, the peak intensity of the largest peak in an XRD measurement of the resin layer of the prepreg may be one-third or less of the peak intensity of the largest peak in an XRD measurement of a prepreg in which the resin layer is completely cured.
[0009] The thickness of the metal layer may be 5 μm or less, or even thinner, 3 μm or less, or even thinner, 1 μm or less.
[0010] A laminate may be produced by laminating the above prepregs with metal layers.
[0011] A method for manufacturing a prepreg with a metal layer may include the steps of: forming a metal layer on a carrier layer having a heat-deteriorating adhesive on its surface; providing a thermosetting prepreg on the surface of the metal layer opposite the carrier layer; curing the prepreg and deteriorating the adhesive by heating; and removing the carrier layer and the adhesive.
[0012] The method for producing a prepreg with a metal layer may further include a step of oxidizing a surface of the metal layer opposite to the carrier layer between the step of forming the metal layer and the step of providing the prepreg.
[0013] By adopting an embodiment in which a carrier layer for supporting the metal layer is not provided as in the present invention, waste can be eliminated and work efficiency can be improved compared to a copper foil with a carrier provided with a carrier layer.
[0014] FIG. 1 is a cross-sectional view of a prepreg having a metal layer provided on one side thereof in an embodiment of the present invention. FIG. 2 is a cross-sectional view of a laminated board according to an embodiment of the present invention. FIG. 3 is a cross-sectional view of a laminated board according to an embodiment of the present invention, showing a first manufacturing example thereof. FIG. 4 is a cross-sectional view of a laminated board according to an embodiment of the present invention, showing a second manufacturing example thereof. FIG. 5 is a cross-sectional view of a laminated board according to an embodiment of the present invention, showing a third manufacturing example thereof. FIG. 6 is a cross-sectional view of a prepreg having a metal layer provided on both sides thereof in an embodiment of the present invention. FIG. 7 is a cross-sectional view illustrating a process for manufacturing a prepreg having a metal layer provided on one side thereof in an embodiment of the present invention. FIG. 8 is a cross-sectional view illustrating a process for manufacturing a prepreg having a metal layer provided on both sides thereof in an embodiment of the present invention. FIG. 9 is a cross-sectional view of a prepreg having a metal layer provided with an adhesive layer in an embodiment of the present invention. FIG. 10 is a cross-sectional view of a prepreg having a metal layer provided with an oxide layer in an embodiment of the present invention. FIG. 11 is a cross-sectional view illustrating an example of a method for manufacturing a prepreg having a metal layer according to an embodiment of the present invention. FIG. 12 is a cross-sectional view illustrating another example of a method for manufacturing a prepreg having a metal layer according to an embodiment of the present invention. FIG. 13A is an SEM image (2000x magnification) of a resin layer in a state where semi-curing at 120°C has not progressed much. FIG. 13B is an SEM image (5000x magnification) of a resin layer in a state where semi-curing at 120°C has not progressed much. FIG. 14A is an SEM image (2000x magnification) of a resin layer in a moderate semi-cured state at 150°C. FIG. 14B is an SEM image (5000x magnification) of a resin layer in a moderate semi-cured state at 150°C. FIG. 15A is an SEM image (2000x magnification) of a resin layer in a cured state. FIG. 15A is an SEM image (5000x magnification) of a resin layer in a cured state. FIG. 16 shows the results of XRD measurement of a resin layer in a state where semi-curing at 120°C has not progressed much. FIG. 17 shows the results of XRD measurement of a resin layer in a moderate semi-cured state at 150°C. Fig. 18 shows the results of XRD measurement of a resin layer in an advanced cured state at 190°C. Fig. 19 is a cross-sectional view of a prepreg according to an example embodiment of the present invention. Fig. 20A is a plan view showing an example of a first fiber layer that can be used in an embodiment of the present invention.Fig. 20B is a plan view showing an example of a second fiber layer that can be used in the embodiment of the present invention. Fig. 21 is a cross-sectional view of a prepreg according to another example of the embodiment of the present invention.
[0015] EMBODIMENTS <<Configuration>> As shown in FIG. 1, a prepreg 100 with a metal layer according to this embodiment may include a metal layer 20 having a thickness of 11 μm or less and a semi-cured prepreg 10 provided with the metal layer 20. The prepreg 100 with a metal layer according to this embodiment does not include a carrier layer for supporting the metal layer 20. The metal layer 20 is, for example, a metal foil such as copper foil. An adhesive layer 30 may be provided between the metal layer 20 and the prepreg 10 (see FIG. 9). Patent Document 1 (
[0016] ) states that "the thickness of the carrier is preferably 100 to 2000 μm, more preferably 300 to 1800 μm, and even more preferably 400 to 1100 μm." However, the thickness of the metal layer 20 according to this embodiment is significantly thinner than the thickness of the carrier.
[0016] In this embodiment, the term "semi-cured state" refers to a state in which, unlike a liquid, the prepreg has a certain shape but is not completely solidified and can be deformed, for example, by pressing. By using prepreg 10 in a semi-cured state, it is possible to achieve a state in which the metal layer 20 can be embedded. Note that prepreg 10 may not be in a semi-cured state, but may be in a cured state.
[0017] A resin material can be used as the material for the prepreg 10. For example, an epoxy resin can be used as this resin material. However, the resin material is not limited to this, and other resin materials such as unsaturated polyester resin, vinyl ester resin, bismaleimide resin, benzoxazine resin, triazine resin, phenol resin, urea resin, melamine resin, polyimide resin, polyolefin resin, aliphatic polyamide resin, semi-aromatic polyamide resin, aromatic polyester resin, polycarbonate resin, and polystyrene resin can also be used.
[0018] In this embodiment, the semi-cured prepreg 10 serves as a substitute for the conventional carrier layer, eliminating the need for a carrier layer. Conventionally, a carrier layer has been provided to facilitate handling, such as transportation. Without a carrier layer, problems such as wrinkles and tears in the copper foil occur during transportation, making the carrier layer an essential component.
[0019] Such a carrier layer is ultimately discarded, resulting in waste. On the other hand, according to the present embodiment, the semi-cured prepreg 10 functions as a carrier layer without providing such a carrier layer, which is extremely advantageous in that it allows for easy handling, such as transportation. Note that the prepreg 10 of the present embodiment does not necessarily need to be in a semi-cured state, and may be a completely cured solid.
[0020] This embodiment is also extremely useful when manufacturing a multilayer board (multilayer wiring board) 200 as shown in Fig. 2. Conventionally, a copper foil with a carrier was laminated on a prepreg 10, and then the carrier layer was removed. On the other hand, this embodiment is extremely useful in that a multilayer board can be formed by simply stacking prepregs 100 with metal layers, eliminating the need to remove the carrier layer.
[0021] That is, as shown in Fig. 3, since no carrier layer is provided, a multilayer board can be formed simply by stacking metal layer-attached prepregs 100. Note that, as shown in Fig. 4, the metal layer-attached prepregs 100 may be stacked after appropriate circuits have been formed.
[0022] Also, as shown in FIG. 5, a multilayer board 200 may be manufactured by stacking prepregs 100 with metal layers while embedding part or all of the circuit (see the prepregs 100 with metal layers in the middle and bottom of FIG. 5).
[0023] As shown in Fig. 6, metal layers 20 may be provided on both sides of the prepreg 10. Note that such a prepreg 10 is not formed from a metal foil with a carrier having a carrier layer. In this embodiment, the prepreg 10 is provided with a metal layer 20 that does not have a carrier layer.
[0024] One reason why a carrier layer is required is that the company that provides the copper foil and the company that manufactures the circuit board are different companies, but the inventors of this application have an environment (company) where these operations can be performed together. As a result, copper foil can be applied to semi-cured prepreg 10 in-house, and multilayer boards can be manufactured and circuits designed in that state.
[0025] As shown in Fig. 19 , the prepreg 100 of this embodiment may have a first fiber layer 170 formed of first fibers 171, and a second fiber layer 180 formed of second fibers 181 and spaced apart from the first fiber layer 170 in the thickness direction. A resin material may be provided on the side of the first fiber layer 170 facing the second fiber layer 180 (upper side in Fig. 19 ) and on the side of the first fiber layer 170 opposite to the second fiber layer 180 (lower side in Fig. 19 ), thereby forming a resin layer 160. Furthermore, as shown in Fig. 21 , fiber layers such as the first fiber layer 170 and the second fiber layer 180 may be embedded in the resin layer 160.
[0026] As shown in Fig. 20A, the first fiber layer 170 may be formed by weaving first fibers 171. Similarly, as shown in Fig. 20B, the second fiber layer 180 may be formed by weaving second fibers 181. Note that three or more fiber layers may be provided, and up to the nth fiber layer (where "n" is an integer of 3 or more) may be provided, with a resin layer provided corresponding to each fiber layer.
[0027] Examples of the fibers that can be used include glass fibers, liquid crystal polyester fibers, aromatic polyamide fibers, PBO (polyparaphenylene benzobis oxazole) fibers, PPS (polyphenylene sulfide) fibers, carbon fibers, etc. Examples of the glass material for the glass fibers include T-glass, S-glass, D-glass, E-glass, NE-glass, C-glass, H-glass, ARG-glass, and quartz glass.
[0028] The resin layer 160 of a semi-cured prepreg 100 containing fiber layers such as the first fiber layer 170 and the second fiber layer 180 may have an uneven surface, as shown in FIGS. 14A and 14B. The fiber layer may be embedded in the semi-cured resin layer 160 (see FIG. 21), forming an uneven surface on the resin layer 160 where the fiber layer is located. Semi-cured prepregs 100 having such an uneven surface have a desirable hardness and are highly suitable for embedding patterned circuits. The inclusion of a fiber layer also provides shape stability. Note that FIGS. 13A and 13B show prepregs 100 at a lower temperature than FIGS. 14A and 14B, and the semi-curing has not yet progressed to an adequate state. FIGS. 15A and 15B show prepregs 100 in a cured state, where the uneven surface is no longer visible. 13A and 13B, a prepreg 100 including a resin layer 160 having an uneven surface can be provided by lowering the temperature. Alternatively, a prepreg may be selected after confirming that the resin layer 160 has an uneven surface, or conditions under which the resin layer 160 has an uneven surface may be selected, and mass production may be carried out according to the selected conditions.
[0029] Furthermore, the XRD measurement results showed high peak values at the low temperature of 120°C (see FIG. 16) when the semi-cured state was not sufficient, and at the high temperature of 190°C (see FIG. 18) when the cured state was advanced. However, it was also confirmed that the peak values were smaller in the semi-cured state shown in FIGS. 14A and 14B (see FIG. 18). Furthermore, compared with the case shown in FIG. 18 where the cured state was advanced, the peak intensity in the semi-cured state shown in FIG. 18 was about one-quarter. For this reason, it is beneficial to use a semi-cured prepreg in which the peak intensity of the largest peak in the XRD analysis (the peak around 44 degrees in FIGS. 17 and 18) is one-third or less (preferably one-quarter or less) of the peak intensity in the cured state.
[0030] According to this embodiment, it is also possible to employ a thin metal layer 20, and the thickness of the metal layer 20 may be 10 μm or less, 8 μm or less, 5 μm or less, 3 μm or less, or 1 μm or less. The thinner the metal layer 20, the greater the need for a carrier layer. However, in this embodiment, the metal layer 20 without a carrier layer is provided directly on the semi-cured prepreg 10, thereby eliminating the need for a carrier layer.
[0031] As an example, as shown in FIG. 7 , a prepreg with a metal layer can be manufactured by transporting a semi-cured prepreg 10 by a transport unit 310 such as a belt conveyor, and providing a metal layer 20 made of copper foil or the like on the prepreg 10 by a supply unit 320 such as a supply roller.
[0032] When providing the metal layer 20 on both sides, the metal layer 20 may be provided on one side of the prepreg 10 as shown in FIG. 7, and then the prepreg 10 with the metal layer 20 provided on one side may be inverted and another metal layer 20 may be provided (see FIG. 8).
[0033] The configuration may be reversed, and a prepreg with a metal layer may be manufactured by transporting the metal layer using a transport unit 310 such as a belt conveyor while providing resin to the metal layer using a supply unit 320 such as a supply roller (see FIGS. 7 and 8).
[0034] An oxide layer 15, which is formed by oxidizing a portion of the metal layer 20, may be provided on the surface of the metal layer 20 facing the prepreg 10 (see FIG. 10 ). When the metal layer 20 is made of copper, the oxide layer 15 may be made of copper oxide. The copper oxide may be cuprous oxide (copper(I) oxide) or cupric oxide (copper(II) oxide). Since cupric oxide is generated by further oxidizing cuprous oxide, the ratio of cuprous oxide to cupric oxide may be adjusted by adjusting the degree of oxidation of cuprous oxide, or the metal layer 20 may be made of only cupric oxide. Instead of the oxide layer 15 of the metal layer 20, a reduction layer, which is formed by reducing the metal layer 20, may be provided.
[0035] In this embodiment, the following aspects can be provided: (1) Semi-hardened prepreg CCL (Cupper Clad Laminate). (2) CCL with a metal foil (metal layer) of 11 μm or less. (3) Semi-hardened CCL including an electroless plating layer, a metal paste layer of the same type, or both. (4) Semi-hardened CCL including an electroless plating layer without including any palladium components. (5) Semi-hardened prepreg CCL in which the adhesive layer is made of an oxide precipitated from the metal foil to form an anchor.
[0036] According to this embodiment, for example, the following effects can be obtained. Since there is no need to separately procure and use uncured prepreg (raw material) and metal foil, the cost of cutting each material (prepreg, metal foil), the labor required for prepreg edge processing, the labor required for temperature and humidity control (such as refrigeration), and corrosion prevention management are eliminated, resulting in significant cost reductions. In addition, damage due to defective products in these processes is eliminated. Furthermore, the handling process and the carrier material used for that process are also unnecessary. Therefore, the layup process for overlapping these components is also unnecessary. Furthermore, the misalignment of the inner and outer layer circuits and the leakage of resin from both ends during pressure and heat application, i.e., resin dripping, which occurred in conventional methods, can be reduced, thereby improving quality stability in the process. Furthermore, when using CCL with thin metal foil, there is no need to use expensive metal foil with a carrier, and various processes involved can be omitted.
[0037] Furthermore, conventionally, it has been extremely difficult to manufacture CCLs using copper foils as thin as 12 μm or less, and no CCLs with metal layers of 10 μm or less have been available as products. Even if such CCLs were possible, they would have to be manufactured using an electroless plating process, which poses the problem of a lack of established technology for creating anchors with sufficient peel strength. In addition, palladium residue remains during the electroless plating process, which can potentially cause serious defects such as migration when the CCL is later formed into a circuit. However, this embodiment can solve these problems.
[0038] In this embodiment, the following manufacturing method is provided as an example (see FIG. 11).
[0039] A carrier plate 130 forming a flat carrier layer is prepared and coated with a thermally degradable adhesive 140 (i.e., adhesive strength weakens with heat) (see S1 in Figure 11 ). A plating inducer, which converts non-conductors such as silver or palladium into conductors, is mixed on top of the carrier plate 130 and applied to form a plating layer 110. The plating layer 110 is formed by electroless plating or electrolytic plating. Once the plating layer 110 has a certain thickness, electrodes may be attached and electrolytic plating may be performed to increase the thickness. The plating layer 110 may be made of, for example, copper foil. An anchor may be formed on the copper foil surface using a method used by conventional copper foil manufacturers, or a browning treatment may be used. Alternatively, an oxide may be precipitated on top of the finished copper plating layer to form an oxide layer 115 (e.g., in the case of copper, a treatment is performed to precipitate cuprous oxide or cupric oxide on the surface) (see S2 in Figure 11 ). Note that the precipitation of oxide on top of the plated copper foil may result in unevenness or cavities on the upper surface. The carrier layer may be made of resin, metal, ceramic, or other materials.
[0040] For example, a copper foil plating layer 110 is brought into contact with a prepreg (a soft thermosetting resin sheet known as a green material) 120, which is then pressurized and heated (see S3 in Figure 11). The adhesive 140 on the carrier side is decomposed by thermal degradation, while oxides deposited on the upper side of the metal plating, which form irregularities and cavities, penetrate the soft prepreg, creating a strong peel strength and forming an integrated structure. The prepreg eventually hardens under the influence of heat, and the resulting metal-clad laminate can be easily peeled off from the carrier plate (see S4 in Figure 11).
[0041] In this embodiment, as another example, the following manufacturing method is provided (see FIG. 12).
[0042] A carrier plate 130 for forming a carrier layer having a surface that peels easily, such as a mirror surface, is prepared. A plating layer 110 is formed on the mirror surface of the carrier plate 130 by electrolytic plating or electroless plating (see S11 in FIG. 12).
[0043] At this time, the upper surface of the plated layer 110 is oxidized, and when oxides are precipitated on the upper surface of the plated layer 110, irregularities and cavities are formed on the upper surface, forming an oxide layer 115 (see S12 in FIG. 12).
[0044] For example, a copper foil plating layer 110 is brought into contact with a prepreg (a soft thermosetting resin sheet known as green material) 120, and pressure and heat are applied (see S13 in Figure 12). At this time, the oxides deposited on the upper side of the metal plating, which are irregularities and cavities, penetrate into the soft prepreg, creating a strong peel strength and integrating it. The prepreg eventually hardens under the influence of heat, and the resulting metal-clad laminate can be easily peeled off from the carrier plate (see S14 in Figure 12).
[0045] The CCLs obtained in this manner are useful not only for copper foil CCLs with thicknesses exceeding 11 μm, but also for metal-clad laminates with thicknesses of 11 μm or less. Even with copper foils as thin as a few μm, it is possible to produce thin copper foil CCLs that have sufficient peel strength and address the problems associated with palladium, particularly migration. When the copper foil is oxidized (i.e., the oxide layer 115 is provided), the anchor surface is formed by the unevenness of the insulating oxide precipitate, while the cross section of the unoxidized copper foil is essentially free of unevenness. This results in a smooth, flat surface on the conductor layer side, reducing electrical resistance and improving high-frequency characteristics. Furthermore, the presence of such an oxide layer 115 allows for the formation of circuits with cross sections closer to square or rectangular than conventional shapes during etching (clear cuts). This allows for currents closer to the design value to flow through the formed circuits.
[0046] Furthermore, this method does not leave a plating-inducing layer, such as silver or palladium, anywhere on the CCL, which was previously required in the electroless plating process, and it can produce CCL with sufficient peel strength to act as an anchor on the oxide deposit surface. This allows for the production of metal-clad laminates without using thin metal foils, which are particularly difficult to handle. Creating an anchor through the deposition of insulating materials such as oxide results in a smooth, flat conductor layer, which increases electrical resistance on the anchor surface of the conductor layer and improves frequency characteristics. Of course, metal-clad laminates with thicknesses of 10 μm or more are also possible. This method is applicable to the production of substrates with any thickness of metal layer and any thickness and number of layers.
[0047] The prepreg with a metal layer in the above-described embodiment may be provided with electronic components such as semiconductor elements, capacitors, and resistors. These electronic components may be encapsulated in a sealing portion to provide electronic equipment (including packages) such as IC packages and electronic devices. Such electronic equipment may be incorporated into any mounting device, such as automobiles, airplanes, ships, helicopters, personal computers, and home appliances. Products in this embodiment may include any objects, such as electronic components, devices, electrical appliances, communication equipment, and cars.
[0048] The above-mentioned description of the embodiment, the modified examples, and the disclosure of the drawings are merely examples for explaining the invention described in the claims, and the invention described in the claims is not limited by the above-mentioned description of the embodiment or the disclosure of the drawings.
[0049] 10 Prepreg 20 Metal layer 100 Prepreg with metal layer 200 Multilayer board
Claims
1. A metal layer having a thickness of 11 μm or less; an oxide layer provided on the metal layer; A prepreg provided on the oxide layer; Equipped with No carrier layer is provided to support the metal layer, A prepreg with a metal layer, wherein the oxide layer does not contain anything other than copper or copper oxide.
2. The prepreg has a fiber layer and a resin layer provided on the fiber layer, 2. The prepreg with a metal layer according to claim 1, wherein the surface of the resin layer is in a semi-cured state and has an uneven shape.
3. 3. The prepreg with a metal layer according to claim 1, wherein a peak intensity of a maximum peak in an XRD measurement of a resin layer of the prepreg is ⅓ or less of a peak intensity of a maximum peak in an XRD measurement of a prepreg in which the resin layer is completely cured.
4. The prepreg with a metal layer according to claim 1 , wherein the metal layer has a thickness of 5 μm or less.
5. The prepreg with a metal layer according to claim 1 , wherein the metal layer has a thickness of 3 μm or less.
6. The prepreg with a metal layer according to claim 1 , wherein the metal layer has a thickness of 1 μm or less.
7. The prepreg with a metal layer according to claim 1 , wherein the metal layer is provided on both sides of the prepreg.
8. A method for producing a laminate by laminating a prepreg with a metal layer according to any one of claims 1 to 7.
9. forming a metal layer on a carrier layer having a thermally degradable adhesive on its surface; providing a thermosetting prepreg on a surface of the metal layer opposite the carrier layer; a step of curing the prepreg and degrading the adhesive by heating; removing the carrier layer and the adhesive; A method for producing a prepreg with a metal layer comprising the steps of:
10. 10. The method for producing a prepreg with a metal layer according to claim 9, further comprising a step of oxidizing or reducing a surface of the metal layer opposite to the carrier layer between the step of forming the metal layer and the step of providing the prepreg.
11. forming a metal layer on a carrier layer having a mirror surface; providing a thermosetting prepreg on a surface of the metal layer opposite the carrier layer; removing the carrier layer; A method for producing a prepreg with a metal layer comprising the steps of:
12. The method for producing a prepreg with a metal layer according to any one of claims 9 to 11, wherein the step of forming the metal layer is carried out by electroless plating or electrolytic plating.