Method for preparing cellulose nanofibers by combining deep eutectic solvent pretreatment and ultrasonic crushing

TWI946014BActive Publication Date: 2026-11-11NAT SUN YAT SEN UNIV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
TW114131594
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-08-19
Publication Date
2026-11-11
Estimated Expiration
2045-08-18

Smart Images

  • Figure TWG2TB001920766_001
    Figure TWG2TB001920766_001
  • Figure TWG2TB001920766_002
    Figure TWG2TB001920766_002
  • Figure TWG2TB001920766_003
    Figure TWG2TB001920766_003
Patent Text Reader

Abstract

A method for preparing nanocellulose addresses the significant environmental impact of conventional methods. The method includes: mixing potassium carbonate and glycerol to prepare a eutectic solvent; diluting the eutectic solvent to prepare a diluted eutectic solvent solution; pretreating a biomass containing lignin, hemicellulose, and cellulose with the diluted eutectic solvent solution, dissolving at least a portion of the lignin and hemicellulose in the diluted eutectic solvent solution; washing the pretreated biomass with a washing solution to remove the diluted eutectic solvent solution; and ultrasonically crushing the washed biomass to break down the cellulose and obtain nanocellulose. This method reduces environmental pollution and lowers wastewater treatment costs.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for preparing nanocellulose, comprising: Potassium carbonate and glycerol are mixed to prepare a deep eutectic solvent; The eutectic solvent is diluted to prepare a eutectic solvent dilution with a volume concentration of 5% to 15%; a biomass raw material containing lignin, hemicellulose and cellulose is pretreated with the eutectic solvent dilution to dissolve at least a portion of the lignin and hemicellulose in the eutectic solvent dilution. The pretreated biomass raw material is cleaned with a cleaning solution to remove the eutectic solvent diluent; and the cleaned biomass raw material is ultrasonically crushed to break down the cellulose in the biomass raw material and obtain nanocellulose.

2. The method for preparing nanocellulose as described in claim 1, wherein, The deep eutectic solvent system is prepared by mixing potassium carbonate and glycerol and heating to 80-100°C.

3. The method for preparing nanocellulose as described in claim 1, wherein, In this eutectic solvent, the molar ratio of potassium carbonate to glycerol is 1:

5.

4. The method for preparing nanocellulose as described in claim 1, wherein, The pretreatment time of the biomass raw material with the eutectic solvent diluent is 30 to 180 minutes.

5. The method for preparing nanocellulose as claimed in claim 1, wherein, The temperature at which the biomass raw material is pretreated with the eutectic solvent diluent is 70–90°C.

6. The method for preparing nanocellulose as claimed in claim 1, wherein, When the biomass is pretreated with the eutectic solvent diluent, the solid-liquid ratio of the biomass to the eutectic solvent diluent is 2 g: 30 mL.

7. The method for preparing nanocellulose as claimed in claim 1, wherein, The cleaning solution is 75% ethanol by volume.

8. The method for preparing nanocellulose as claimed in claim 1, wherein, The ultrasonic crushing time for the cleaned biomass raw material is 30 to 90 minutes.

9. The method for preparing nanocellulose as claimed in claim 1, wherein, The biomass raw material is rice straw.

Citation Information

Patent Citations

  • Method for preparing cellulose-based conductive film through combination of eutectic solvent and ultrasound

    CN116410497A

  • Grape vine lignin extraction method and lignin carboxymethyl cellulose composite film

    CN118085326A

  • Methods for manufacturing a composite material from biomass

    TW202407054A

  • Polyester Depolymerisation

    US20250115733A1