TWI946261BActive Publication Date: 2026-11-11CHINA STEEL
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
TW114152056
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-12-30
Publication Date
2026-11-11
Estimated Expiration
2045-12-29

Smart Images

  • Figure TWG2TB001921013_001
    Figure TWG2TB001921013_001
  • Figure TWG2TB001921013_002
    Figure TWG2TB001921013_002
Patent Text Reader

Abstract

A binder for iron shot briquetting, iron shot briquetting, and a method for manufacturing the same are disclosed. The binder for iron shot briquetting comprises bentonite and steel mill solids. The steel mill solids have a particle size of less than 150 micrometers. The weight ratio of bentonite to steel mill solids is between 1:2 and 2:1. The method for manufacturing iron shot briquetting includes a mixing step to obtain an admixture; the admixture includes the binder for iron shot briquetting described above; the admixture is placed in a steel mold; a pressure of 250 kg / cm² to 1100 kg / cm² is applied to the admixture in the steel mold to form briquettes; and the briquettes are placed in a natural environment to form iron shot briquettes, wherein the room temperature crushing strength of the iron shot briquettes is greater than 400 kg / cm².
Need to check novelty before this filing date? Find Prior Art

Claims

1. A binder for iron shot briquetting, comprising: A piece of soap clay; And a steel plant solid waste, wherein the particle size of the steel plant solid waste is less than 150 micrometers; wherein the weight ratio of the bentonite to the steel plant solid waste is between 1:2 and 2:

1.

2. The binder for iron shot agglomeration as described in claim 1, wherein the particle size of the steel mill solids is less than 150 micrometers.

3. The binder for iron shot agglomeration as described in claim 1, wherein the steel mill solids, by weight percent, comprise: Fe2O3 < 50%; CaO < 11%; SiO2 < 8%; Al2O3 < 5%; MgO < 3%; K₂O + Na₂O < 0.5%; The remaining portion is a mixture of impurities such as electrostatic precipitate ash, blast furnace ash, and sintering ash, which are unavoidable during the steelmaking process.

4. A method for manufacturing iron shot briquettes, comprising: A mixture is subjected to a blending step to obtain a blend; The composition, by weight percentage, comprises: a binder for iron shot briquetting as described in any one of claims 1 to 3, wherein the amount of the binder is 6% to 16%; placing the mixture in a steel mold; applying a pressure of 250 kg / cm² to 1100 kg / cm² to the mixture located in the steel mold to form a briquetted material; and placing the briquetted material in a natural environment to form an iron shot briquetted material, wherein the room temperature crushing strength of the iron shot briquetted material is greater than 400 kg / cm².

5. The method for manufacturing iron shot briquettes as described in claim 4, wherein the components, by weight percentage, further include: An iron sand, wherein the amount of iron sand used is 79.5% to 88.5%; wherein the metallic iron content of the iron sand is greater than 70%; And a water, wherein the amount of water used is 4% to 8%.

6. The method for manufacturing iron shot briquettes as described in claim 5, wherein the mixing step comprises: The iron sand and the binder are mixed to form a premix; Add the water to the premix; The water and the premix are mixed and stirred at room temperature to obtain the mixture.

7. The method for manufacturing iron sand blocks as described in claim 4, wherein the diameter of the steel mold is 4 cm.

8. A method for manufacturing iron shot briquettes as described in claim 4, wherein placing the briquettes in the natural environment comprises: The block was left to stand for 7 days.

9. The method for manufacturing iron sand agglomerates as described in claim 4, wherein the particle size of the iron sand is less than 8 mm.

10. An iron sand agglomerate, which is made by the method of manufacturing iron sand agglomerates as described in any one of claims 4 to 9, wherein the reduction pulverization rate of the iron sand agglomerate is between 10% and 17%.