Tank component and method for producing such a tank component

A multi-layer tank component with a high-strength steel outer wall and nickel-containing stainless steel inner wall, combined with internal high-pressure forming, addresses the challenges of hydrogen tank stability and embrittlement, achieving reliable and efficient hydrogen storage.

WO2024199798A1PCT designated stage expired Publication Date: 2024-10-03BAYERISCHE MOTOREN WERKE AG
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/053353
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-02-09
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Hydrogen tanks for vehicles require high pressure stability, resistance to hydrogen embrittlement, and efficient, cost-effective manufacturing, as existing technologies struggle to meet these demands.

Method used

A tank component with a multi-layer design featuring a high-strength steel outer wall and a nickel-containing stainless steel inner wall, where the outer wall absorbs mechanical stresses and the inner wall prevents hydrogen embrittlement, combined with an internal high-pressure forming method to shape the component.

Benefits of technology

The solution provides a pressure-stable, resistant tank component that withstands high pressures and prevents hydrogen embrittlement, ensuring operational reliability and efficient manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024053353_03102024_PF_FP_ABST
    Figure EP2024053353_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a tank component (1) having a length extent from a first tank end (3) to a second tank end (4) and a width extent (5) orthogonal to said length extent (2), wherein the tank component (1) tapers at the first (3) and at the second tank end (4) with respect to a tank centre part lying geometrically between said tank ends (3, 4) in the direction of the length extent (2), wherein the tank component (1) has a tank outer wall (6) and a tank inner wall (7) and wherein the tank inner wall (7) is in contact over its entire area with the tank outer wall (6) and the tank outer wall (6), at least substantially, completely covers the tank inner wall (7), and wherein the tank outer wall (6) consists of a high-strength steel material which has a yield strength greater than 1500 MPa and less than 2500 MPa and furthermore the tank inner wall (7) consists of a steel material which is different from the steel material of the tank outer wall in terms of its composition and has a nickel content of more than 5%, wherein the tank outer wall (6), at least on average, has a wall thickness of more than 2 mm and less than 10 mm and the tank inner wall, at least one average, has a wall thickness of less than 1 mm and more than 0.1 mm.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Tank component and method for producing such a tank component

[0002] The invention relates to a tank component, in particular a tank base body for receiving and storing a pressurized medium, such as hydrogen. It is generally known from the prior art to use so-called internal high-pressure forming for shaping metal components. Such internal high-pressure formed components, particularly those with special requirements, can also have two layers. DE 10 2016 208 690 A1 discloses a tube with a first and a second metal layer, which is produced using an internal high-pressure forming process.

[0003] In vehicles that have a hydrogen tank for storing hydrogen, high demands are placed on this hydrogen tank. A hydrogen tank must be particularly pressure-stable and able to withstand a pressure in the range of 1600 bar for a long time. Furthermore, this tank must be resistant or insensitive to hydrogen diffusion and hydrogen embrittlement. Furthermore, as with any commercial application, the efficient, and in particular cost-effective, provision of such functions is of great importance. Against this background, it is an object of the invention to provide a tank component that has a high level of operational reliability during scheduled operation and that can be manufactured efficiently, and further to provide a manufacturing method for producing such a tank component.This object is achieved by an article according to patent claim 1 and by a manufacturing method according to patent claim 3, wherein preferred developments of the invention are each the subject of the dependent patent claims.

[0004] For the purposes of the invention, a tank component is understood to be a component intended for use in a tank device, i.e., a device for holding a liquid or gaseous storage medium and preferably for holding liquefied hydrogen. In particular, a tank component that essentially encloses a tank volume of the tank device must meet particular requirements with regard to its resistance to the storage medium. Hydrogen storage devices, in particular, are subject to stringent requirements with regard to resistance to hydrogen embrittlement and pressure and temperature resistance. A bottle shape, as is generally known from diving or gas cylinders, has proven to be a suitable design for such a tank component.Figuratively speaking, the finished tank component has a longitudinal extension from a first tank end to a second tank end and a width extension orthogonal to this longitudinal extension. The tank component is preferably designed as an at least substantially hollow-cylindrical component, with the cylinder axis preferably running along this longitudinal extension. Furthermore, the tank component is tapered at this first and at this second tank end; preferably, the two tank ends are designed symmetrically to one another. Further preferably, the section of the tank component arranged between the two tank ends is to be understood as the tank center part, and preferably at least this tank center part is designed as a hollow-cylindrical body, preferably with a circular cross-sectional area.

[0005] The tank component has an outer tank wall and an inner tank wall, wherein the inner tank wall is in full contact with the outer tank wall, at least in sections, and further preferably, the outer tank wall covers the inner tank wall, at least substantially, completely or over its entire surface. Figuratively speaking, the wall of the tank component, which surrounds the interior volume intended to accommodate the storage medium, can be designed as a multi-layer, i.e., at least a two-layer component, wherein the inner tank wall forms a first layer and the outer tank wall forms a second layer of this tank component.It is proposed that the tank inner and outer walls be adapted to the respective requirements placed on them, so that the tank outer wall is designed in particular to absorb mechanical stresses, in particular to absorb pressure forces from the storage medium, and the tank inner wall is designed in particular to chemically securely absorb the storage medium, in particular to prevent hydrogen embrittlement on the tank outer wall.

[0006] The tank outer wall comprises a high-strength steel material as one component, or is made of such a steel material, wherein a high-strength steel material within the meaning of this invention has a yield strength greater than 1500 MPa, preferably greater than 1750 MPa, and more preferably less than 2500 MPa, preferably less than 2250 MPa, and particularly preferably at least substantially equal to 2000 MPa. Steel materials with such a yield strength can still be formed to a sufficient extent and have sufficient strength to withstand compressive forces, such as those that can occur, in particular, during hydrogen storage.Furthermore, the tank component has the tank inner wall, which has as one component a steel material whose composition differs from that of the steel material of the tank outer wall, and furthermore, the tank inner wall consists of this steel material, which differs from that of the steel material of the tank outer wall. Furthermore, the steel material of the tank inner wall has a nickel content of more than 5%, preferably more than 10%, and more preferably more than 12%, and more preferably, the nickel content is less than 50%, preferably less than 30%, and particularly preferably less than 20%. In particular, a nickel content in a steel material in the stated range leads to good resistance to hydrogen embrittlement for this material.In particular, a steel material of the described type makes it possible for the tank inner wall to protect the tank outer wall or, in other words, the tank inner wall is particularly resistant to hydrogen and protects the tank outer wall, which contributes significantly to the stability of a tank facility, from hydrogen embrittlement.

[0007] Furthermore, the tank outer wall has, at least in sections, or at least substantially or at least on average, a wall thickness of more than 2 mm and less than 10 mm. The wall thickness of the tank outer wall is preferably oriented towards the pressure at which the storage medium is to be stored in the tank device and towards the geometric configuration of the tank component. The proposed tank inner wall has, at least in sections, or at least substantially or at least on average, a wall thickness of less than 1 mm and more than 0.1 mm, preferably more than 0.2 mm, and more preferably less than 0.6 mm.

[0008] In a preferred embodiment, the steel material of the tank's inner wall is stainless steel, preferably rust-proof stainless steel. In particular, stainless steel with the proposed nickel content exhibits particularly high resistance to substances, especially hydrogen, thus enabling the construction of a particularly durable tank system.

[0009] Furthermore, a method for producing a tank component is proposed, wherein the tank component is designed as previously described. The proposed method comprises at least the following steps:

[0010] - providing a tank outer wall of the tank component, wherein the tank outer wall represents, at least substantially, the outer shape of the tank component,

[0011] - Inserting a tank inner wall blank into the tank outer wall,

[0012] - Incorporating the tank outer wall into a tank component mold,

[0013] - applying an internal forming high pressure to the tank inner wall blank so that the tank inner wall blank adheres, at least largely or completely, to the tank outer wall and thus forms the tank inner wall,

[0014] - Forming the tank component from the tank component mold. The tank outer wall is provided in an at least substantially fully formed state, so that it already has, at least substantially, the outer contour of the tank component. The tank inner wall blank has a shape, particularly at the beginning of the proposed process, so that it can be inserted or inserted into the tank outer wall.

[0015] The tank outer wall, in particular with the tank inner wall blank inserted therein, is inserted into the tank component mold or accommodated therein. Furthermore, after the tank outer wall has been inserted into the tank component mold, the mold is closed so that the tank component mold supports the tank outer wall from the outside and thus counteracts deformation of the latter, in particular during hydroforming of the tank inner wall blank into the tank inner wall.

[0016] After the tank outer wall has been incorporated into the tank component mold, the tank inner wall blank is subjected to an internal forming high pressure at least once, wherein this internal forming high pressure prevails in particular in a forming medium which is introduced into the tank inner wall blank. Furthermore, the internal high pressure forming process can be carried out by repeatedly applying such internal forming high pressure and, more preferably, different internal forming pressures can be applied at different forming stages. In particular, the internal forming high pressure is selected such that the tank inner wall blank adheres, at least largely or completely, to the tank outer wall and thus forms the tank inner wall. In particular, if such internal forming high pressure is applied multiple times, a multi-stage forming of the tank inner wall blank into the tank inner wall is achieved.

[0017] In a preferred embodiment of the invention, the material of the tank inner wall blank is stainless steel. This stainless steel is preferably rust-proof stainless steel. Stainless steel, in particular, has proven to be a particularly suitable material, especially in connection with the use of the tank inner wall in a hydrogen storage device.

[0018] In a preferred embodiment of the invention, at least the tank component mold is heated to a forming temperature, preferably at least during the application of the internal forming high pressure to the tank inner wall blank. This application of the internal forming high pressure is understood to include, in particular, such internal forming high pressure in a multi-stage forming process as well as in a single-stage forming process. A forming temperature is selected from a range in which this forming temperature is greater than 100°C and less than 1000°C. It should also be noted that the manufacturing process can also take place at room temperature or at a temperature below the proposed range.In particular, by heating the tank component mold, better degrees of deformation can be achieved than without such heating; furthermore, such a forming temperature can also be provided via the medium which is introduced into the tank inner wall blank to apply the internal forming high pressure, and in particular when forming with a forming temperature from the proposed range, an improvement in the manufacturing process can be achieved.

[0019] In a preferred embodiment of the invention, in the method for producing the tank component, the internal forming high pressure is applied to the tank inner wall blank using a liquid forming medium. The forming medium is preferably heated to an internal forming temperature, at least while the internal forming high pressure is applied, wherein the internal forming temperature is greater than 100°C and less than 1000°C. It should also be noted that forming the tank inner wall blank is also possible outside the proposed temperature range for the internal forming temperature, preferably at room temperature. In particular, heating to the internal forming temperature by the liquid forming medium enables improved forming of the tank inner wall blank into the tank inner wall.

[0020] In a preferred embodiment of the invention, the method for producing the tank component utilizes a multi-stage method for forming the tank inner wall blank into the tank inner wall. In such a multi-stage forming method, at least one internal forming preforming pressure is applied prior to the application of the internal forming high pressure. This internal forming preforming pressure can also be considered internal forming high pressure within the meaning of this invention. Preferably, the internal forming preforming pressure is reduced again, and subsequently, another internal forming preforming pressure or the internal forming pressure is applied, with which the tank inner wall blank is fully pressed against the tank outer wall, thus forming the tank inner wall. A high degree of forming can be achieved, in particular, through a multi-stage method.

[0021] In the following, individual features and developments of the invention are explained in more detail with reference to the figures, whereby combinations of features other than those shown are also possible, it shows: Fig.1 : schematically shows the production of a tank component for storing hydrogen in a motor vehicle in a sectional view, production steps divided into a) to e),

[0022] Fig.2: a schematic manufacturing process for producing a tank component of the described type.

[0023] In the figure, tank component 1 has a longitudinal extension 2 from a first tank end 3 to a second tank end 4 and a width extension 5 orthogonal to this longitudinal extension 2, wherein the tank component 1 is tapered at the first 3 and second 4 tank ends with respect to a tank center section located geometrically in the direction of the longitudinal extension between these tank ends 3, 4. In this case, the tank center section has a circular, hollow cylindrical shape, wherein the illustrated longitudinal extension 2 forms the cylinder axis of this tank center section. Figuratively speaking, the tank outer wall 6 and thus the tank component 1 have a bottle-like geometry.

[0024] The tank component 1 has an outer tank wall 6. In Figure 1 a), the inner tank wall 7 is shown in its unformed state, i.e., as a tank inner wall blank 10. The proposed manufacturing method shapes this inner tank wall blank 10 in such a way that the inner tank wall 7 is created and is in full contact with the outer tank wall 6. In the finished state, the outer tank wall 6 therefore at least substantially completely covers the inner tank wall 7, so that the inner tank wall 7 is completely covered by the outer tank wall from the radial outside and is also in contact with it, forming a two-layer tank wall. In this sense, at least substantially is to be understood in particular as meaning that the inner tank wall 7 is not covered by the outer tank wall 6 only at its end faces, in particular at the first 3 and second 4 tank ends.

[0025] The illustrated tank outer wall 6 consists of a high-strength steel material which has a yield strength of approximately 2000 MPa. This high-strength tank outer wall 6 achieves the supporting function which is necessary due to the high compressive strength to be achieved. The tank inner wall blank 10 and thus the tank inner wall 7 consists of a steel material which differs in composition from the steel material of the tank outer wall 6. This material of the tank inner wall 7 has a nickel content of more than 5%, whereby such a nickel content has a positive effect on the tank inner wall 7 being insensitive to hydrogen embrittlement and hydrogen diffusion. The tank outer wall 6 has an average wall thickness of approximately 5 mm; deviations from this wall thickness arise in particular from the deformation of the tank outer wall at the tapered first 3 and second 4 tank ends.The tank inner wall 7, on the other hand, has on average a smaller wall thickness than the tank outer wall 6, this wall thickness of the tank inner wall being approximately 0.5 mm.

[0026] In Figures 1 b) to e), in particular the designations for the first 3 and second 4 tank ends as well as the longitudinal 2 and width 5 extensions are not shown any further; this is done to improve the clarity of the figures.

[0027] In other words, Figure 1 a) shows how the tank outer wall 6 is prepared during production of the tank component. This sectional view therefore does not show a finished product of the tank component 1, but rather an intermediate product during production which is subject to further processing. Figure 1 a) shows that the tank outer wall 6 already has the outer shape of the tank component 1, i.e. the outer shape of the pressure vessel of a hydrogen storage device. The tank inner wall 10, which is still unformed at this stage, has already been inserted into this tank outer wall 6 made of high-strength steel as the tank inner wall blank 7, which protects the tank outer wall 6 against hydrogen embrittlement during normal operation of the tank component.

[0028] In Figure 1 b) it can be seen how the tank outer wall 6 with the tank inner wall blank 7 accommodated therein is received in the tank component mold 8, the tank component mold 8 being designed in several parts and being open for inserting and receiving the tank outer wall 6 in the tank component mold 8.

[0029] Figure 1 c) shows how the tank component mold 8 is transferred from its open state, shown in Figure 1 b), to the closed state. In the closed state, the tank component mold 8 supports the tank outer wall 6 from the outside.

[0030] Figure 1 d) shows how the tank component mold 8, in the closed state, supports the tank outer wall 6 from the outside. It can also be seen how the tank inner wall blank is filled with a medium 9 for internal high-pressure forming and thus for applying internal forming high pressure. Figure 1 e) shows that in the closed tank component mold 8, the tank inner wall blank 7 has been formed into the tank inner wall 10 by means of the internal forming high pressure in the medium, so-called forming medium 9, or rather, this has pressed against the tank outer wall 6 and thus formed the tank inner wall 10, which is supported from the outside by the tank outer wall 6 and is completely covered by it. In order to form the tank component 1 from the tank component mold 8 (not shown), the multi-part tank component mold 8 is opened.

[0031] Figure 2 shows a schematic process sequence for producing a tank component 1.

[0032] In a first method step 101, the tank outer wall 6 of the tank component 1 is provided, wherein the tank outer wall 6 already has, at least substantially, the outer shape of the tank component.

[0033] In a second process step 102, the tank inner wall blank 7 is inserted into this tank outer wall 6.

[0034] In a third method step 103, the tank outer wall 6 with the tank inner wall blank 7 accommodated therein is received in a multi-part tank component mold 8.

[0035] In a fourth method step 105, the tank inner wall blank 7 is filled with a forming medium for applying internal forming high pressure and then subjected to this internal forming high pressure. By applying the internal forming high pressure to the tank inner wall blank 7, the tank inner wall blank 7 is formed into the tank inner wall 10, which is then pressed against the tank outer wall 6 from the inside.

[0036] In a fifth method step 105, the tank component 1 is formed from the multi-part tank component mold.

Claims

Claims 1. Tank component (1) having a longitudinal extension from a first tank end (3) to a second tank end (4) and a width extension (5) orthogonal to this longitudinal extension (2), wherein the tank component (1) is tapered at the first (3) and at the second tank end (4), compared to a tank middle part lying geometrically in the direction of the longitudinal extension (2) between these tank ends (3, 4), wherein the tank component (1) has a tank outer wall (6) and a tank inner wall (7), and wherein the tank inner wall (7) is in full contact with the tank outer wall (6) and the tank outer wall (6) completely covers the tank inner wall (7), and wherein the tank outer wall (6) consists of a high-strength steel material which has a yield strength which is greater than 1500 MPa and less than 2500 MPa, and furthermore the tank inner wall consists (7) made of a steel material which is different in composition from the steel material of the tank outer wall,and has a nickel content of more than 5%, wherein the tank outer wall (6), at least on average, has a wall thickness of more than 2 mm and less than 10 mm and the tank inner wall, at least on average, has a wall thickness of less than 1 mm and more than 0.1 mm., 2. Tank component according to claim 1, characterized in that the steel material of the tank inner wall (7) is a stainless steel material.

3. A method for producing a tank component according to one of the preceding claims, comprising the steps: - providing a tank outer wall (6) of the tank component (1), wherein the tank outer wall represents, at least substantially, the outer shape of the tank component, - Inserting a tank inner wall blank into the tank outer wall, - Recording the tank outer wall with the tank inner wall blank in a tank component mold, - applying an internal forming high pressure to the tank inner wall blank so that the tank inner wall blank adheres, at least largely or completely, to the tank outer wall and thus forms the tank inner wall, - Forming the tank component from the tank component mold.

4. A method for producing a tank component according to claim 3, characterized in that the tank component mold is heated to a forming temperature which is greater than 100 °C and less than 1000 °C at least during the application of the internal forming high pressure.

5. A method for producing a tank component according to one of claims 3 or 4, characterized in that the internal forming high pressure is applied to the tank inner wall blank with a liquid forming medium, that the forming medium, at least during the application of the internal forming high pressure, is heated to an internal forming temperature which is greater than 100° C and which is less than 1000° C.

6. A method for producing a tank component according to one of claims 3 to 5, characterized in that before the internal forming high pressure is applied, at least one internal forming preforming pressure is applied and then reduced again.

Citation Information

Patent Citations

  • anti-vibration tube

    DE102016208690A1

  • Method for manufacturing a pressure vessel and pressure vessel

    DE102019134165A1

  • Method for manufacturing hydrogen tank

    JP2018083391A

  • High pressure gas container and manufacturing method for high pressure gas container

    US20140197179A1

  • Improved method to produce high-resistance composite vessels with inner metal liner and vessels made by said method

    US20160377228A1