High-insulation and low-corrosion vaporization propellant for non-pressure-storage perfluorohexanone fire-extinguishing apparatus and preparation method
By using the vaporization propellant prepared by non-metal salt or metal salt oxidant, the problems of poor electrical insulation and strong corrosiveness in the existing technology are solved, the effects of high insulation and low corrosiveness are achieved, and the perfluorohexanone fire extinguishing technology is expanded. The application scope of the device.
Patent Information
- Application Number
- PCT/CN2023/092037
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-14
- Filing Date
- 2023-05-04
- Publication Date
- 2024-10-17
AI Technical Summary
The vaporized propellant of existing non-storage perfluorohexanone fire extinguishing devices has problems with poor electrical insulation and strong corrosiveness, which limits its application in precision instrument locations and new energy scenarios with high electrical insulation requirements.
Use a vaporization propellant composed of 30-90% non-metal salt oxidant and/or metal salt oxidant, 10-50% reducing agent, and 1-20% binder, and prepare it by drying, crushing, mixing, granulating and drying , improve the electrical insulation and reduce the corrosion of the residue after spraying.
A vaporized propellant with high insulation and low corrosiveness is achieved, which is suitable for precision instruments and new energy scenarios, and improves the application scope of perfluorohexanone fire extinguishing devices.
Smart Images

Figure CN2023092037_17102024_PF_FP_ABST
Abstract
Description
A high-insulation, low-corrosion vaporized propellant for non-pressurized perfluorohexanone fire extinguishing device and its preparation method Technical Field
[0001] The invention belongs to the technical field of fire fighting and extinguishing, and particularly relates to a high-insulation and low-corrosion vaporized propellant for a non-pressure stored perfluorohexanone fire extinguishing device and a preparation method thereof. Background Art
[0002] Perfluorohexanone fire extinguishing agent is a new environmentally friendly, colorless, and non-toxic fire extinguishing agent. It has a boiling point of 49.2°C at standard atmospheric pressure, a freezing point of -108°C, and a dielectric strength of ≥110kV, demonstrating its extremely high insulation properties. At room temperature, the agent is in liquid form, significantly improving its storage, transportation, and handling, eliminating the risk of frostbite. Upon discharge from the nozzle, the agent rapidly transforms into a gaseous state, leaving no residue after evaporation. It is non-toxic and harmless to humans, with an ODP of 0, a GWP of 1, and an ALT of 0.014 years (5 days) in the atmosphere. Its extinguishing concentration is 4-6%, making it an excellent alternative to halon and HFC-based fire extinguishing agents. Perfluorohexanone fire extinguishing agent primarily extinguishes flames through physical cooling, and also has oxygen isolation and chemical inhibition properties. Its fire extinguishing mechanisms include cooling, temperature reduction, oxygen isolation, and chemical inhibition. For a long time, perfluorohexanone was mainly used in large-scale pressure-storage fire extinguishing systems. However, with the rapid development of emerging industries such as new energy and power storage, and the urgent need for fire safety, micro / small non-pressure-storage perfluorohexanone fire extinguishing devices have begun to emerge. Existing non-pressure-storage perfluorohexanone fire extinguishing devices use vaporized propellant as a power source to propel the spraying of perfluorohexanone. There are two main forms. The first form is that the vaporized propellant is only used as a power source. The perfluorohexanone and the vaporized propellant are separated by a piston inside the device. The gas generated by the vaporized propellant pushes the piston to spray the perfluorohexanone. This form has the problem of complex device structure. The second form is that the vaporized propellant is installed in the agent chamber. The gas generated by the vaporized propellant after activation causes the agent chamber to open holes or rupture. This type of device has a simple structure and a wider range of applications, becoming the main trend in the development of non-pressure-storage perfluorohexanone fire extinguishing devices. For example, Chinese patent CN214860780U discloses a perfluorohexanone internal pressure storage fire extinguishing device, and Chinese patent CN215309854U discloses a non-pressure storage perfluorohexanone fire extinguishing device.
[0003] When the vaporized propellant is installed in the agent bin, the structure of the fire extinguishing device will be simplified, and the process requirements and costs will be reduced. Therefore, it has become the main production trend of non-pressurized perfluorohexanone fire extinguishing devices. At present, non-pressurized perfluorohexanone fire extinguishing devices mainly use aerosol fire extinguishing agents specifically used for fire extinguishing as vaporized propellants. For example, the non-pressurized perfluorohexanone fire extinguishing device disclosed in Chinese patent CN113509663A uses the heat generated by the combustion of the aerosol gas-generating charge to destroy the packaging of the perfluorohexanone material package, and causes it to be sprayed outward under the pressure of the aerosol to achieve fire extinguishing. However, this type of vaporized propellant is a K-type aerosol fire extinguishing agent. The solid residue after spraying is highly active and has poor electrical insulation after absorbing moisture. At the same time, after the non-storage pressure perfluorohexanone fire extinguishing device is activated, the solid residue from the combustion of the vaporized propellant will be sprayed out along with the perfluorohexanone fire extinguishing agent. After the perfluorohexanone is vaporized, the solid residue will adhere to the surface of the protected object. After a long period of high humidity, the solid residue will absorb moisture and form an alkaline electrolyte liquid film, which has poor electrical insulation and strong corrosiveness. Moreover, with the development and progress of science and technology, more and more precision instrument sites, power systems, and new energy scenarios with high electrical insulation requirements have emerged. In these sites, the traditional non-storage pressure perfluorohexanone fire extinguishing devices constructed with K-type aerosol fire extinguishing agent as the vaporized propellant have poor applicability, which seriously restricts their scope of application.
[0004] Summary of the Invention
[0005] In order to solve the above technical problems, the present invention provides a high-insulation, low-corrosion vaporized propellant for non-pressurized perfluorohexanone fire extinguishing equipment and a preparation method. The vaporized propellant mainly improves the electrical insulation and reduces the corrosiveness of the sediment or residue after spraying in two ways: first, the oxidant uses a non-metallic salt oxidant, and the residue after combustion is a non-conductive neutral substance such as solid carbon residue; second, the oxidant uses a metal salt oxide whose solid residue after spraying is highly stable and not easily soluble in water.
[0006] The technical solution adopted in the present invention is as follows:
[0007] The invention provides a high-insulation and low-corrosion vaporization propellant for a non-pressure-storage perfluorohexanone fire extinguishing device, which is composed of 30-90% of a non-metallic salt oxidant and / or a metallic salt oxidant, 10-50% of a reducing agent, and 1-20% of an adhesive.
[0008] Preferably, the non-metallic salt oxidant is any one of ammonium nitrate, ammonium perchlorate, ammonium chlorate, urea peroxide, guanidine nitrate, ammonium dinitramide, trinitramide, 3,4-dinitraminofurazan, and hexanitrohexaazaisowurtzitane.
[0009] Preferably, the metal salt oxidant is any one of strontium nitrate, barium nitrate, magnesium nitrate, calcium nitrate, nickel nitrate, silver nitrate, zinc nitrate, lead nitrate, and ammonium dichromate.
[0010] Preferably, the reducing agent is any one of hexamethylenetetramine, dicyandiamide, melamine, 5-aminotetrazole, bis(5-tetrazolyl)amine, N-guanyl urea dinitramide, triaminoguanidine nitrate, and nitroguanidine.
[0011] Preferably, the binder is any one of phenolic resin, shellac, carboxymethyl cellulose, sodium carboxymethyl cellulose, polyvinyl alcohol, polyester polyether, polyvinyl chloride, polyvinyl acetate, fluororubber, hydroxyl-terminated polybutadiene, carboxyl-terminated polybutadiene, acrylic resin, hydroxypropyl methylcellulose, melamine formaldehyde resin, polycaprolactone, and polyethylene glycol.
[0012] The present invention also provides a method for preparing a high-insulation, low-corrosion vaporized propellant for a non-pressurized perfluorohexanone fire extinguishing device, which specifically comprises the following steps:
[0013] (1) Take the oxidizing agent, reducing agent and binder, dry and grind them separately, and pass them through a sieve for later use;
[0014] (2) Weigh various raw materials according to their mass fraction and dry mix them until uniform;
[0015] (3) spraying the solvent into the mixture in step (2), mixing while spraying, and granulating the mixture after mixing evenly;
[0016] (4) Drying the particles obtained in step (3) until the solvent content is less than 1% to obtain a vaporized propellant.
[0017] Preferably, the sieve aperture in step (1) is 100 mesh, and the sieve aperture in step (3) is 20 mesh.
[0018] Preferably, the solvent in step (3) is any one of water, anhydrous ethanol, anhydrous acetone, and ethyl acetate, and the amount used is 5-20% of the total mass of the raw materials.
[0019] Preferably, the drying condition in step (4) is drying at 45-55° C. for 20-30 h.
[0020] The beneficial effects of the present invention are:
[0021] 1. The present invention adopts non-metallic salts or metal salts with stable solid residues after spraying as oxidants to prepare a vaporizing propellant suitable for perfluorohexanone fire extinguishing device. The solid residues generated after combustion by using non-metallic salts as oxidants are mainly substances such as residual carbon, which have no conductive ions and are insoluble in water or are neutral after dissolving. Therefore, the vaporizing propellant and the fire extinguishing device have the advantages of high insulation and low corrosion. The metal salt with stable solid residues after combustion is adopted as the oxidant. The stable metal salt remaining after combustion is almost insoluble in water or reacts with water and still exists in the form of the original metal salt solid. Therefore, the vaporizing propellant has very weak corrosiveness and few conductive ions, thereby having good electrical insulation. Therefore, the vaporizing propellant and the corresponding non-pressure storage perfluorohexanone fire extinguishing device have the advantages of high insulation and low corrosion, thereby improving the adaptability to precision instrument sites, power systems, and new energy scenarios with high requirements for electrical insulation.
[0022] 2. In the present invention, the raw materials of the oxidant, reducing agent, and adhesive are controlled to be about 100 mesh. The vaporized propellant particles formed after granulation are passed through a 20-mesh sieve to form small particles with a diameter of about 6 mm and a height of about 5.5 mm. By increasing the size of the particles, the sensitivity of the raw materials to external energy is reduced, thereby improving the safety of the vaporized propellant. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] FIG1 is a comparison diagram of the copper plates of Example 1, Example 12 and Comparative Example 1. DETAILED DESCRIPTION
[0024] The present invention is further described below with reference to the accompanying drawings and specific embodiments. It should be noted that the following embodiments are only preferred embodiments of the present invention and are not intended to limit the present invention. The scope of protection of the present invention shall be subject to the contents of the claims. Any modification or equivalent substitution of the technical solution of the present invention by those skilled in the art without making any creative work shall fall within the scope of protection of the present invention.
[0025] Example 1
[0026] (1) Weigh 65% ammonium nitrate, 30% nitroguanidine, and 5% polyvinyl alcohol, dry and grind them separately, and pass them through a 100-mesh sieve for later use;
[0027] (2) The above raw materials were placed in a mixer and dry-mixed for 30 minutes until uniform. Then, 8% water was added to the mixer by spraying, and mixed while adding to ensure that the water and solid raw materials were fully and evenly mixed to prevent local dilution. After the mixing was completed, the mixture was passed through a 20-mesh sieve for granulation to obtain small particles with a diameter of about 6 mm and a height of about 5.5 mm;
[0028] (3) The small particles were transferred to a dryer and dried at 50° C. for 24 h until the moisture content was less than 1%, thereby preparing a vaporized propellant.
[0029] Example 2
[0030] Weigh 70% of ammonium dinitramide, 20% of 5-aminotetrazole, and 10% of fluororubber, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0031] Example 3
[0032] Weigh 30% of carbamide peroxide, 50% of hexamethylenetetramine, and 20% of carboxymethyl cellulose, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0033] Example 4
[0034] Weigh 40% of trinitramide, 50% of dicyandiamide, and 10% of polyvinyl chloride, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0035] Example 5
[0036] Weigh 50% of 3,4-dinitraminofurazan, 35% of melamine, and 15% of polyvinyl acetate, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0037] Example 6
[0038] Weigh 85% of hexanitrohexaazaisowurtzitane, 10% of triaminoguanidine nitrate, and 5% of melamine formaldehyde resin, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0039] Example 7
[0040] Weigh 60% ammonium perchlorate, 45% 5-aminotetrazole, and 5% hydroxy-terminated polybutadiene, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0041] Example 8
[0042] Weigh 80% of ammonium chlorate, 10% of N-guanyl urea dinitramide, and 10% of acrylic resin, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0043] Example 9
[0044] Weigh 65% guanidine nitrate, 30% nitroguanidine, and 5% polyvinyl alcohol, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0045] Example 10
[0046] Weigh 65% strontium nitrate, 25% bis(5-tetrazolyl)amine, and 10% hydroxypropyl methylcellulose, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0047] Example 11
[0048] Weigh 80% of ammonium dichromate, 10% of N-guanyl urea dinitramide, and 10% of acrylic resin, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0049] Example 12
[0050] Weigh 20% hexanitrohexaazaisowurtzitane, 50% strontium nitrate, 20% nitroguanidine, and 10% phenolic resin, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0051] Example 13
[0052] Weigh 30% of 3,4-dinitraminofurazan, 40% of silver nitrate, 20% of 5-aminotetrazole, and 10% of hydroxy-terminated polybutadiene, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0053] Example 14
[0054] Weigh 60% of trinitramide, 20% of ammonium dichromate, 20% of 5-aminotetrazole, and 10% of phenolic resin, dry and grind them separately, and pass them through a 100-mesh sieve for later use; other methods and steps are the same as those in Example 1.
[0055] Comparative Example 1
[0056] 70% potassium nitrate, 20% dicyandiamide, and 10% phenolic resin were weighed and a vaporizing propellant was prepared according to the method and steps described in Example 1.
[0057] Comparative Example 2
[0058] 20% strontium nitrate, 50% potassium nitrate, 20% guanidine nitrate, and 10% phenolic resin were weighed and a vaporizing propellant was prepared according to the method and steps described in Example 1.
[0059] Verification results:
[0060] The vaporized propellants from Examples 1-10 and Comparative Examples 1-2 were installed in a perfluorohexanone fire extinguishing device. The discharged solid residue was collected using a PVC plate and a copper plate, respectively. To test electrical insulation, the solid residue was allowed to absorb moisture for 24 hours at a temperature of 35°C and a relative humidity of 90%, and then its electrical resistance was measured. To test corrosion, the solid residue was allowed to absorb moisture for 24 hours at a temperature of 30°C and a relative humidity of 85%, and the corrosion of the copper plate was observed. The results are shown in Table 1:
[0061] Table 1 Electrical insulation and corrosiveness of vaporized propellants under different formulations
[0062] As can be seen from the data in Table 1, in Examples 1-10, after using a non-metallic salt oxidant or a metal salt oxidant with a stable solid residue after spraying, the electrical insulation of the residue after the perfluorohexanone fire extinguishing device is significantly improved and the corrosiveness is significantly reduced; after spraying, the vaporized propellant prepared with the non-metallic salt oxidant is found to have a resistance value greater than 2200 megohms after moisture absorption testing, and the copper plate has no obvious discoloration (as shown in the copper plate of Example 1 in Figure 1); after spraying, the vaporized propellant prepared with the metal salt oxidant has a resistance value ranging from hundreds of megohms to 2200 megohms, and the copper plate only has slight discoloration (as shown in the copper plate of Example 12 in Figure 1); When the commonly used K-type aerosol fire extinguishing agent and S-type aerosol fire extinguishing agent are used as the vaporized propellant, the resistance after spraying and moisture absorption is only 0-20 megohms, and the copper plate changes color significantly (as shown in the copper plate of the comparative example in Figure 1), indicating that the vaporized propellant prepared by the present invention can effectively replace the vaporized propellant (aerosol fire extinguishing agent) of the existing perfluorohexanone fire extinguishing device, while achieving rapid destruction of the agent chamber, reducing the corrosiveness of the solid residue and improving the electrical insulation, thereby helping to expand the application scope of the perfluorohexanone fire extinguishing device, so that it can be well applied in precision instrument places, power systems, and new energy scenarios with high electrical insulation requirements.
Claims
1. A highly insulating and low-corrosive vaporized propellant for a non-pressurized perfluorohexanone fire extinguishing device, characterized in that: The invention is composed of 30-90% of non-metallic salt oxidant and / or metallic salt oxidant, 10-50% of reducing agent and 1-20% of adhesive.
2. A highly insulating and low-corrosive vaporized propellant for a non-pressurized perfluorohexanone fire extinguishing device according to claim 1, characterized in that: The non-metallic salt oxidant is any one of ammonium nitrate, ammonium perchlorate, ammonium chlorate, urea peroxide, guanidine nitrate, ammonium dinitramide, trinitramide, 3,4-dinitraminofurazan, and hexanitrohexaazaisowurtzitane.
3. The high-insulation, low-corrosion vaporized propellant for non-pressurized perfluorohexanone fire extinguishing device according to claim 1, characterized in that: The metal salt oxidant is any one of strontium nitrate, barium nitrate, magnesium nitrate, calcium nitrate, nickel nitrate, silver nitrate, zinc nitrate, lead nitrate and ammonium dichromate.
4. The high-insulation, low-corrosion vaporized propellant for non-pressurized perfluorohexanone fire extinguishing device according to claim 1, characterized in that: The reducing agent is any one of hexamethylenetetramine, dicyandiamide, melamine, 5-aminotetrazolyl, bis(5-tetrazolyl)amine, N-guanyl urea dinitramide, triaminoguanidine nitrate, and nitroguanidine.
5. The high-insulation, low-corrosion vaporized propellant for non-pressurized perfluorohexanone fire extinguishing device according to claim 1, characterized in that: The adhesive is any one of phenolic resin, shellac, carboxymethyl cellulose, sodium carboxymethyl cellulose, polyvinyl alcohol, polyester polyether, polyvinyl chloride, polyvinyl acetate, fluororubber, hydroxyl-terminated polybutadiene, carboxyl-terminated polybutadiene, acrylic resin, hydroxypropyl methylcellulose, melamine formaldehyde resin, polycaprolactone, and polyethylene glycol.
6. A method for preparing a highly insulating and low-corrosive vaporized propellant for a non-pressurized perfluorohexanone fire extinguishing device, characterized in that: The following steps are involved: (1) taking an oxidizing agent, a reducing agent and a binder, drying and crushing them respectively, and passing them through a sieve for later use; (2) Weigh various raw materials according to their mass fraction and mix them until uniform; (3) spraying the solvent onto the mixture in step (2), mixing while spraying, and granulating the mixture after the mixture is evenly mixed; (4) Drying the particles obtained in step (3) until the solvent content is less than 1% to obtain a vaporized propellant.
7. The preparation method according to claim 6, characterized in that: The mesh size of the sieve in step (1) is 100 mesh, and the mesh size of the sieve in step (3) is 20 mesh.
8. The preparation method according to claim 6, characterized in that: The solvent in step (3) is any one of water, anhydrous ethanol, anhydrous acetone and ethyl acetate, and the amount used is 5-20% of the total mass of the raw materials.
9. The preparation method according to claim 6, characterized in that: The drying condition in step (4) is drying at 45-55° C. for 20-30 hours.
10. The preparation method according to claim 9, characterized in that: The drying condition is drying at 50° C. for 24 hours.
Citation Information
Patent Citations
Extinguishment combination with hot gas sol
CN101376049A
Rapid and efficient aerosol fire extinguishing agent and preparation method thereof
CN105597259A
Low-temperature S-type aerosol fire extinguishing agent
CN106621165A
S-shaped hot aerosol fire extinguishing agent
CN108355293A
Low-combustion-temperature and environment-friendly hot aerosol fire extinguishing agent
CN110384888A