Method for manufacturing circuit-embedded substrate

The method improves alignment accuracy between the circuit and electrode pads in film heaters by using ultrasonic welding and misalignment absorbing regions with bent shapes, addressing positional deviations and increasing yield rates.

WO2024224826A1PCT designated stage expired Publication Date: 2024-10-31NISSHA PRINTING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/008746
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-27
Filing Date
2024-03-07
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Conventional manufacturing methods for film heaters face challenges in aligning electrode pads and embedded thin metal wires, leading to positional deviations and reduced yield rates due to separate processes for pad placement and wire embedding.

Method used

A method that involves arranging electrode pads parallel to each other on a film, embedding a thin metal wire with an arbitrary pattern using ultrasonic welding, and incorporating misalignment absorbing regions with bent shapes to improve alignment accuracy between the circuit and electrode pads.

Benefits of technology

The method enhances the precision of alignment between the circuit and electrode pads, thereby increasing the rate of non-defective products by absorbing misalignment and allowing for consistent embedding positions despite potential shifts in pad placement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024008746_31102024_PF_FP_ABST
    Figure JP2024008746_31102024_PF_FP_ABST
Patent Text Reader

Abstract

[Problem] To provide a method for manufacturing a circuit-embedded substrate, said method being capable of improving a non-defective rate by improving the accuracy of positioning between a circuit and an electrode pad. [Solution] This method comprises: preparing a film; arranging two electrode pads on the film along a first direction; forming a circuit by embedding the circuit into the film using an ultrasonic welding machine, said circuit comprising one thin metal wire and having a functional part of an arbitrary pattern, two wiring parts led out from both ends of the functional part, and two end parts extending from the wiring part to the opposite side from the functional part, partially overlapping the electrode pad, and constituting two displacement absorption regions; and connecting the electrode pads and the thin metal wire thereon to each other. The ultrasonic welding machine has: a horn for embedding the thin metal wire into the film by melting a contact surface with the thin metal wire of the film by ultrasonic vibration; and a thin metal wire drawn out through the inside of the horn. The displacement absorption regions are constituted by a bent-shaped end and have a width for absorbing the positional deviation in a first direction between the electrode pad and the circuit.
Need to check novelty before this filing date? Find Prior Art

Description

Manufacturing method of circuit-embedded substrate

[0001] The present invention relates to a method for manufacturing a circuit-embedded substrate.

[0002] A film heater in which a single thin metal wire is embedded in a film with a given pattern is known (see, for example, Patent Document 1). Referring to Fig. 10 , such a film heater 100 includes a film 200, rectangular first and second electrode pads 500 and 600 arranged parallel to each other at a distance along the Y direction on the periphery of the film 200, and a circuit 400 formed of a single thin metal wire 300 embedded in the film 200. The circuit 400 includes a heater section 450 having a given pattern, a first wiring section 430 and a second wiring section 440 respectively drawn from both ends of the heater section 450, and first and second end sections 410 and 420 extending from the first wiring section 430 and the second wiring section 440 respectively in the opposite direction from the heater section 450 (the +X direction in the figure) and overlapping the first electrode pad 500 and the second electrode pad 600, respectively. The circuit 400 is embedded by applying ultrasonic vibrations using an ultrasonic welding machine to melt the contact surface of the film 200 with the thin metal wires 300. For example, the circuit 400 can be embedded in the following order starting from the first end 410: the first wiring section 430, the heater section 450, the second wiring section 440, and the second end 420.

[0003] The first end 410 and the second end 420 straddle the first electrode pad 500 and the second electrode pad 600, respectively, in the X direction. The upper surfaces of the first electrode pad 500 and the second electrode pad 600 are electrically connected to the thin metal wires 300 that contact the upper surfaces of the first end 410 and the second end 420. When a voltage is applied to the first electrode pad 500 and the second electrode pad 600, a current is generated in the circuit 400, and the heater section 450 generates heat.

[0004] Japanese Patent Application Laid-Open No. 2022-066706

[0005] In the conventional manufacturing method for the film heater 100, the electrode pads 500, 600 are first placed on the film 200, and the corners of the film 200 are then placed against a jig (not shown). Then, the thin metal wires 300 are embedded in the film 200 so that the first end 410 and the second end 420 overlap the electrode pads 500, 600. Because the placement of the electrode pads 500, 600 and the embedding of the thin metal wires 300 are separate processes, the following misalignments occur: (1) misalignment of the electrode pads, (2) misalignment of the embedded thin metal wires, and (3) misalignment of the electrode pads and the embedded thin metal wires. In this manufacturing method, for example, if the placement locations of the electrode pads 500, 600 are misaligned in the +Y direction in FIG. 10( a), the embedded position of the thin metal wires 300 will be relatively misaligned in the −Y direction in FIG. 10( a). In other words, the conventional manufacturing method has had the problem that it is difficult to improve the yield rate because it is difficult to align the electrode pads 500, 600 with the circuit 400.

[0006] The present invention has been made to solve the above-mentioned problems, and aims to provide a method for manufacturing a circuit-embedded substrate that can improve the yield rate by increasing the alignment accuracy between the circuit and the electrode pads.

[0007] A first invention for achieving the above object includes a preparation step of preparing a film; an arrangement step of arranging first electrode pads and second electrode pads in parallel to each other at intervals along a first direction on a peripheral edge portion on a first main surface of the film; and a circuit formation step of forming a circuit having a functional portion made of one thin metal wire arranged on the first main surface and having an arbitrary pattern, a first wiring portion drawn out from one of both ends of the functional portion, a second wiring portion drawn out from the other of both ends of the functional portion, and first end portions extending from the first wiring portion and the second wiring portion respectively to the opposite side of the functional portion, partially overlapping the first electrode pad and the second electrode pad, and constituting a first misalignment absorption region and a second end portion forming a second misalignment absorption region, by embedding the functional portion, the first wiring portion and the second wiring portion, and portions of the first end portion and the second end portion that do not overlap the first electrode pad and the second electrode pad, into the first main surface of the film using an ultrasonic welding machine; a connecting step of electrically connecting the first electrode pads and the second electrode pads to the thin metal wires located on the first electrode pads and the second electrode pads, respectively; the ultrasonic welding machine has a horn that applies ultrasonic vibrations to melt the contact surface of the film with the thin metal wires and embed the thin metal wires in the first main surface of the film, and the thin metal wires that pass through the inside of the horn and are continuously drawn out from the tip of the horn onto the first main surface of the film; and the first and second misalignment absorption regions are formed by first and second curved ends and have widths that absorb misalignment in a first direction between the first and second electrode pads and the circuit, respectively.

[0008] According to this manufacturing method, even if the embedded positions of the first and second electrode pads and the first and second end portions are misaligned in the first direction relative to each other, the first and second end portions have portions that overlap with the first and second electrode pads, respectively, because the first and second end portions have a curved shape and a width that absorbs the misalignment in the first direction between the first and second electrode pads and the circuit. Therefore, the alignment accuracy between the electrode pads and the circuit is improved, and the yield rate can be improved.

[0009] A second invention is a method for manufacturing a circuit-embedded substrate according to the first invention, wherein the bent shape is a zigzag shape or a U-shape in plan view.

[0010] According to the method for manufacturing a circuit-embedded substrate of the present invention, it is possible to improve the accuracy of alignment between the circuit and the electrode pads, thereby improving the yield rate.

[0011] 5 is a schematic perspective view showing an embodiment of a manufacturing method for a circuit-embedded substrate. A partially enlarged view showing an example of a first end and a second end. An enlarged view showing a state in which an electrode pad is misaligned in the +X direction. A partially enlarged view showing another example of the first end and the second end. An enlarged view showing a state in which an electrode pad is misaligned in the +X direction. An enlarged view showing a state in which an electrode pad is further misaligned in the +X direction from that in FIG. 5. An enlarged view showing a state in which an electrode pad is misaligned in the -X direction. An enlarged view showing a state in which an electrode pad is misaligned in the +X direction in a conventional film heater. An enlarged view showing a state in which an electrode pad is misaligned in the -X direction in a conventional film heater. (a) A schematic plan view showing a conventional film heater. (b) A-A cross-sectional view of (a).

[0012] (Overview of Circuit-Embedded Substrate) Referring to FIG. 1( f ), the circuit-embedded substrate 1 includes a film 2, a circuit 4 formed of a single thin metal wire 3 disposed on a first main surface 2 a of the film 2, a first electrode pad 5, and a second electrode pad 6. The circuit 4 includes a functional portion 45, a first wiring portion 43, a second wiring portion 44, a first end portion 41, and a second end portion 42. The functional portion 45 has an arbitrary pattern. The first wiring portion 43 is drawn out from one end 45 a of the functional portion 45. The second wiring portion 44 is drawn out from the other end 45 b of the functional portion 45. The first end portion 41 extends from the first wiring portion 43 toward the opposite side of the functional portion 45 (in the −Y direction) and overlaps the first electrode pad 5. The second end portion 42 extends from the second wiring portion 44 toward the opposite side of the functional portion 45 (in the −Y direction) and overlaps the second electrode pad 6. In this embodiment, the first end portion 41 and the second end portion 42 have a zigzag shape (an example of a bent shape) in a plan view.

[0013] The functional portion 45, the first wiring portion 43, and the second wiring portion 44 are embedded in the first main surface 2a of the film 2. The portions of the first end portion 41 and the second end portion 42 that overlap the electrode pads 5, 6 are not embedded in the first main surface 2a, while the remaining portions are embedded. In other words, the thin metal wires 3 located above the electrode pads 5, 6 are not embedded in the first main surface 2a, while the thin metal wires 3 that are not located above the electrode pads 5, 6 are embedded.

[0014] In this embodiment, the functional portion 45 is a heat-generating portion, and the circuit-embedded substrate 1 is a film heater. For example, by applying a positive voltage to the first electrode pad 5 and a negative voltage to the second electrode pad 6, a current is generated in the circuit 4 made of the thin metal wires 3, causing the functional portion 45 to heat up. The functional portion 45 has two ends 45a, 45b connected to the first wiring portion 43 and the second wiring portion 44, respectively, and has a loop-shaped pattern. More specifically, the functional portion 45 has a pattern shape that extends from the connection portion 45a with the first wiring portion 43 in the +X direction, then extends in the +Y direction, the −X direction, the −Y direction, and the +X direction to reach the connection portion 45b with the second wiring portion 44. In this way, the functional portion 45 has the connection portions 45a, 45b with the first wiring portion 43 and the second wiring portion 44, and has an arbitrary pattern that extends from the connection portions 45a, 45b in the XY plane.

[0015] The film 2 can have any shape, and in this embodiment, it is rectangular. The film 2 can be transparent, opaque, or colored transparent. Examples of materials that can be used for the film 2 include thermoplastic resins such as ethylene-based resins, propylene-based resins, polyolefin-based resins, thermoplastic polyester-based resins, polyamide-based resins, polyvinyl chloride, polycarbonate, and ABS resin. The film 2 may contain two or more of these. The film 2 can be appropriately added with inorganic fine powders or organic fillers, dispersants, antioxidants, compatibilizers, UV stabilizers, antiblocking agents, antistatic agents, and the like. The thickness of the film 2 is, for example, 0.05 mm to 1 mm.

[0016] The thin metal wires 3 can be made of conductive materials such as copper, iron, gold, copper-nickel, nickel-chromium, and iron-nickel-chromium. From the viewpoints of electrical resistance, durability, and cost, it is preferable to use copper or a copper alloy made by combining copper with zinc, lead, tin, silver, aluminum, nickel, beryllium, zirconium, or a combination of two or more elements. The diameter of the thin metal wires 3 is, for example, 0.01 mm to 0.5 mm. By making the diameter as small as possible, for example, 0.01 mm to 0.2 mm, the thin metal wires 3 can be made less noticeable.

[0017] The circuit 4 may be formed of a conductive wire consisting of thin metal wires 3 and an insulating coating layer covering the wires. The insulating coating layer is made of an insulating resin, such as polyester, polyethylene, polyurethane, polyvinyl chloride, polyamide, polyimide, polyesterimide, polyamideimide, or fluororesin. The diameter of the conductive wire is, for example, 0.05 mm to 0.3 mm.

[0018] The two electrode pads 5 and 6 may be made of conductive materials such as copper, phosphor bronze, brass, Corson alloy, nickel, and molybdenum. These materials may be used as base materials plated with nickel, tin, gold, silver, copper, or other materials. The electrode pads 5 and 6 may have dimensions of, for example, 5 mm x 10 mm and a thickness of, for example, 0.1 mm. While the electrode pads 5 and 6 are rectangular in this embodiment, they are not limited thereto. For example, they may be polygonal, circular, elliptical, or L-shaped.

[0019] (Method of Manufacturing Circuit-Embedded Substrate) One embodiment of a method of manufacturing such a circuit-embedded substrate 1 will be described with reference to Fig. 1. The method of manufacturing the circuit-embedded substrate 1 includes a preparation step (not shown) of preparing a film 2, an arrangement step (Fig. 1(a)) of arranging first electrode pads 5 and second electrode pads 6 on the peripheral portion of a first main surface 2a of the film 2, a circuit formation step (Figs. 1(b) to 1(e)) of forming a circuit 4 using an ultrasonic welder 7, and a connection step (Fig. 1(f)) of electrically connecting a first end 41 and a second end 42 of the circuit 4 to the electrode pads 5, 6.

[0020] In the preparation step, the film 2 may be fixed on a stage (not shown). A jig (not shown) may also be used to facilitate alignment of the film 2. In the placement step, the first electrode pad 5 and the second electrode pad 6 are placed on the periphery of the first main surface 2a of the film 2. In other words, they are placed side by side in the X direction (first direction) along one side of the film 2 that is parallel to the X direction. The two electrode pads 5 and 6 are rectangular and are placed parallel to each other with a gap in between along the X direction. The two electrode pads 5 and 6 each serve as a terminal portion of the circuit-embedded substrate 1. The two electrode pads 5 and 6 can be fixed on the first main surface 2a using, for example, an adhesive or the like.

[0021] 1(b), ultrasonic welding machine 7 used in the circuit formation process includes an oscillator (not shown) that generates ultrasonic vibrations, a horn 71 that propagates the ultrasonic vibrations from the oscillator, and thin metal wires 3. By applying ultrasonic vibrations, horn 71 melts the contact surface of film 2 with thin metal wires 3 and can embed thin metal wires 3 in first main surface 2a of film 2. Thin metal wires 3 pass through the inside of horn 71 and are continuously drawn out from tip 71a of horn 71 onto first main surface 2a of film 2.

[0022] In the circuit formation process, as shown in FIG. 1B, first, a predetermined length of the fine metal wire 3 is pulled out from the horn 71 and embedded in the first main surface 2a of the film 2, forming a first end 41 by extending the fine metal wire 3 in a zigzag pattern across the first electrode pad 5. At this time, the bent portion of the zigzag pattern is embedded in the first main surface 2a, and the portion of the fine metal wire 3 overlapping the first electrode pad 5 is not embedded in the first main surface 2a but contacts the upper surface of the first electrode pad 5. Next, as shown in FIG. 1C, the fine metal wire 3 is pulled out a predetermined length from the embedded end of the first end 41 toward the +Y direction and embedded in the first main surface 2a to form a first wiring portion 43. Next, the fine metal wire 3 is pulled out a predetermined length from the embedded end 43a of the first wiring portion 43 and embedded in the first main surface 2a in an arbitrary pattern extending in the XY plane to form a functional portion 45. The embedded end 43a of the first wiring portion 43 serves as the starting end of the functional portion 45. In other words, the end 43a of the first wiring portion 43 becomes one 45a of both ends of the functional portion 45 (see FIG. 1(d)). Next, as shown in FIG. 1(d), the thin metal wire 3 is pulled out by a predetermined length from the horn 71, and extends from the end 45b of the functional portion 45 in the -Y direction and is embedded in the first main surface 2a to form the second wiring portion 44. The end 45b of the functional portion 45 is the starting end of the second wiring portion 44 and becomes the other of both ends of the functional portion 45. Next, as shown in FIG. 1(e), the thin metal wire 3 is pulled out by a predetermined length from the embedded end 44a of the second wiring portion 44 and is embedded in the first main surface 2a, and forms the second end 42 spanning over the second electrode pad 6 in a zigzag shape. At this time, the zigzag bent portions are embedded in the first main surface 2a, and the thin metal wires 3 overlapping the second electrode pads 6 are not embedded in the first main surface 2a but are in contact with the upper surfaces of the second electrode pads 6. After the second end portions 42 are formed, the thin metal wires 3 are cut at the embedded ends of the second end portions 42. Cutting methods can be used, for example, with a cutter or nippers. Finally, in the connection process, as shown by point P in FIG. 1( f ), the two electrode pads 5, 6 are electrically connected to the thin metal wires 3 located above (in contact with) the two electrode pads 5, 6. For the connection, known metal joining techniques such as welding (resistance welding, ultrasonic welding, laser welding, etc.), soldering, brazing, etc. can be used.It should be noted that there may be a plurality of locations where the electrode pads 5, 6 are electrically connected to the thin metal wires 3. In this manner, the circuit-embedded substrate 1 can be obtained.

[0023] (First embodiment of misalignment absorbing region) Referring to Fig. 2, the first end 41 and the second end 42 respectively constitute a first misalignment absorbing region 41a and a second misalignment absorbing region 42a. The first misalignment absorbing region 41a and the second misalignment absorbing region 42a are regions indicated by dashed lines in the figure. Fig. 2 shows a state where there is no misalignment between the first electrode pad 5 and the second electrode pad 6 and the first end 41 and the second end 42. The first misalignment absorbing region 41a has a width W 41 The second misalignment absorbing region 42a has a width W 42 These widths W 41 , W 42 is equal to the width of the zigzag shape of the end portions 41 and 42, and the width W of the two electrode pads 5 and 6 5 , W 6 Naturally, the width W of the positional deviation absorbing regions 41a and 42a is set to be larger than 41 , W 42 If the width W of the electrode pads 5 and 6 is increased, the allowable positional deviation of the electrode pads 5 and 6 in the X direction also increases. 5 , W 6 When the distance S between the electrode pads 5 and 6 is 10 mm, the width W 41 , W 42 may each be 15 mm.

[0024] As shown in FIG. 3, even if the positions of the electrode pads 5 and 6 are shifted by d in the +X direction, the positional deviation absorbing regions 41a and 42a each have a width W 41 , W 42 Since the misalignment absorbing regions 41a and 42a have a width W 41 , W 42By having this, even if the positions of the electrode pads 5, 6 relative to the film 2 are shifted by d in the X direction, the ends 41, 42 will overlap the electrode pads 5, 6. Therefore, the embedding positions of the ends 41, 42 do not need to take into account the positional shift of the electrode pads 5, 6. In other words, the ends 41, 42 can be embedded in the same positions every time the circuit-embedded substrate 1 is manufactured. In this way, it is possible to align the ends 41, 42 with the electrode pads 5, 6 without considering the positional shift of the electrode pads 5, 6, thereby improving the yield rate.

[0025] (Second embodiment of misalignment absorbing region) Referring to Fig. 4, the bent shape of the first end 41 and the second end 42 may be U-shaped in a plan view. The first end 41 and the second end 42 respectively constitute a first misalignment absorbing region 41a and a second misalignment absorbing region 42a. Fig. 4 shows a state in which there is no misalignment between the first end 41 and the second end 42 and the first electrode pad 5 and the second electrode pad 6.

[0026] The first positional deviation absorbing region 41a has a width W 41 The second misalignment absorbing region 42a has a width W 42 These widths W 41 , W 42 are equal to the width of the U-shape of the end portions 41 and 42, and satisfy the following formulas (1) and (2), respectively. 5 , S 6 are the intervals between the two thin metal wires 3 that straddle each of the electrode pads 5 and 6 in the Y direction. 41 = (2 × W 3 ) + S 5 ... (1) W 42 = (2 × W 3 ) + S 6 ...(2) When the thin metal wire 3 and the electrode pads 5 and 6 are ultrasonically welded together, the width W of each of the first positional deviation absorbing region 41a and the second positional deviation absorbing region 42a is 41 , W 42 and the width W of the two electrode pads 5 and 6 5 , W 6When soldering the thin metal wire 3 to the electrode pads 5 and 6, it is necessary to fix the thin metal wire 3 by placing solder on both sides of the thin metal wire 3 (in other words, by placing solder at positions that sandwich the thin metal wire 3). 5 (W 6 ) > W 41 (W 42 The width W of the electrode pads 5 and 6 5 , W 6 Whereas, the width (diameter) W of the metal thin wire 3 3 and the interval S 5 , S 6 are set to values ​​that satisfy the following equations (3) and (4): 5 = 2W 3 +S 5 ... (3) W 6 = 2W 3 +S 6 ...(4) That is, the width W of the electrode pads 5 and 6 5 , W 6 and the width (diameter) W of the metal thin wire 3 3 Once this is determined, the interval S 5 , S 6 can be calculated from the above equations (3) and (4). For example, the width W 5 (=width W 6 ) of the electrode pads 5, 6 is 5 mm, and the width (diameter) W 3 When the metal thin wire 3 has a diameter of 0.5 mm, the distance S 5 (=S 6 ) is 5 - 1 = 4 mm.

[0027] In this way, the interval S 5 , S 6 By forming the first misalignment absorbing region 41a and the second misalignment absorbing region 42a in a U-shape with a gap therebetween, for example, as shown in FIG. 5, the electrode pads 5 and 6 are spaced apart by a distance d (=W 5 / 2 = W 6 Even if the positions of the thin metal wires 3 are misaligned by 1 / 2, there will be overlapping portions between the thin metal wires 3 and the electrode pads 5, 6 (portions where the thin metal wires 3 straddle the electrode pads 5, 6). In other words, the accuracy of aligning the electrode pads 5, 6 with the ends 41, 42 is improved, and the yield rate can be improved.

[0028] 6 and 7, even if the electrode pads 5 and 6 are shifted by d+d / 2 in the ±X directions, there will be overlapping portions between the thin metal wire 3 and the electrode pads 5 and 6 as long as the shapes of the first end 41 and the second end 42 satisfy the above formulas (3) and (4). In FIGS. 6 and 7, one thin metal wire 3 overlaps the edge portion of each of the electrode pads 5 and 6. As can be seen from FIGS. 6 and 7, the allowable range of positional shift of the electrode pads 5 and 6 in the X direction is d+d / 2. Here, d=W 5 / 2 (=W 6 / 2), so W 5 / 2+W 5 / 4 = 3W 5 / 4 (=3W 6 / 4).

[0029] 8 and 9, the first end 410 and the second end 420 of the conventional film heater 100 are straight. In FIGS. 8 and 9, the electrode pads 500 and 600 are misaligned in the X direction, but there are portions where the thin metal wire 300 and the electrode pads 500 and 600 overlap. The amount of misalignment of the electrode pads 500 and 600 in FIGS. 8 and 9 is half the width (W 500 / 2,W 600 That is, the allowable range of positional deviation of the electrode pads 500 and 600 in the X direction is half the width of the electrode pads 500 and 600 (W 500 / 2,W 600 / 2).

[0030] In this way, by changing the shape of the first end 41 and the second end 42 from the conventional straight line to a U-shape that satisfies the above formulas (3) and (4), the tolerance for positional deviation in the X direction of the electrode pads 5 and 6 increases by 1.5 times. In other words, it becomes easier to align the first end 41 and the second end 42 with the electrode pads 5 and 6, thereby improving the yield rate.

[0031] In the above two embodiments, the embedded position of the thin metal wire 3 is not shifted and the electrode pads 5, 6 are shifted, but the manufacturing method of the present invention can achieve the same effects as the above embodiments even in a configuration where the electrode pads 5, 6 are not shifted and the embedded position of the thin metal wire 3 is shifted. Also, in a configuration where both the positions of the electrode pads 5, 6 and the embedded position of the thin metal wire 3 are shifted, the manufacturing method of the present invention can achieve the same effects as the above embodiments.

[0032] 1: Circuit-embedded substrate 2: Film 2a: First main surface 3: Thin metal wire 4: Circuit 41: First end 41a: First misalignment absorbing region 42: Second end 42a: Second misalignment absorbing region 43: First wiring portion 44: Second wiring portion 45: Functional portion 5: First electrode pad 6: Second electrode pad 7: Ultrasonic welder 71: Horn 100: Film heater 200: Film 300: Thin metal wire 400: Circuit 410: First end 420: Second end 430: First wiring portion 440: Second wiring portion 450: Heater portion 500: First electrode pad 600: Second electrode pad 700: Adhesive layer

Claims

a placement step of placing first and second electrode pads parallel to each other at intervals along a first direction on the periphery of a first main surface of the film; and a circuit formation step of embedding, into the first main surface of the film, the functional section, which is made of a single thin metal wire arranged on the first main surface and has an arbitrary pattern, a first wiring section drawn out from one of both ends of the functional section, a second wiring section drawn out from the other of both ends of the functional section, and a first end constituting a first misalignment absorption region and a second end constituting a second misalignment absorption region, the first wiring section and the second wiring section extending to the opposite side of the functional section, respectively, partially overlapping the first electrode pad and the second electrode pad, respectively, by the functional section, the first wiring section and the second wiring section, and portions of the first end and the second end that do not overlap the first electrode pad and the second electrode pad, using an ultrasonic welder; a connecting step of electrically connecting the first electrode pads and the second electrode pads to the thin metal wires located on the first electrode pads and the second electrode pads, respectively; the ultrasonic welding machine has a horn that applies ultrasonic vibrations to melt the contact surface of the film with the thin metal wires and embed the thin metal wires in the first main surface of the film, and the thin metal wires pass through the inside of the horn and are continuously drawn out from a tip of the horn onto the first main surface of the film; and the first and second misalignment absorbing regions are formed by the first end and the second end that are bent, and each have a width that absorbs misalignment in the first direction between the first electrode pads and the second electrode pads and the circuit.

2. The method for manufacturing a circuit-embedded board according to claim 1, wherein the bent shape is a zigzag shape or a U-shape in a plan view.

Citation Information

Patent Citations

  • sheet heater

    JP1990008894U

  • Method of manufacturing non-contact communication medium, non-contact communication medium, and method of connecting antenna and circuit device

    JP2014096125A

  • Film heater

    JP2019169417A

  • Film heater and manufacturing method thereof

    JP2022066706A