Manufacturing method of multi-functional composite non-woven fabric, and multi-functional composite non-woven fabric manufactured thereby
Patent Information
- Application Number
- PCT/KR2023/021553
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-02
- Filing Date
- 2023-12-26
- Publication Date
- 2024-11-07
Smart Images

Figure KR2023021553_07112024_PF_FP_ABST
Abstract
Description
Method for manufacturing a multifunctional composite nonwoven fabric and a multifunctional composite nonwoven fabric manufactured therefrom
[0001] The present invention relates to a method for manufacturing a multifunctional composite nonwoven fabric and a multifunctional composite nonwoven fabric manufactured therefrom, and more particularly, to a method for manufacturing a multifunctional composite nonwoven fabric and a multifunctional composite nonwoven fabric manufactured therefrom, characterized in that a first sheet layer manufactured in the form of any one of a long-fiber web, a short-fiber nonwoven fabric and a long-fiber nonwoven fabric is laminated and intertwined with a second sheet layer manufactured in the form of any one of a short-fiber web, a film and an ultra-fine fiber web.
[0002] Non-woven fabric refers to a fiber structure manufactured by forming a thin felt-like web by arranging fibers in parallel or irregular directions without going through a weaving process, and then combining them. Therefore, the web refers to the stage before the fibers are combined to manufacture the non-woven fabric, and the non-woven fabric refers to the form in which the fibers that make up the web are combined.
[0003] The above nonwoven fabric is made up of intertwined fibers, allowing for a wide range of uses due to its lack of longitudinal and transverse directionality. In particular, its applications have recently expanded to include filters, nonwoven rolls, and artificial leather, leading to its widespread use.
[0004]
[0005] Typically, there are various methods for manufacturing nonwoven fabrics, and the types of nonwoven fabrics are broadly classified into staple fiber nonwoven fabrics and long fiber nonwoven fabrics manufactured using a spunbond method. Referring to Fig. 1, the manufacturing process of staple fiber nonwoven fabrics will be described. Typically, when manufacturing nonwoven fabrics, staple fibers pass through a carding machine (10) to form a carded web (20). This carding process is a process for forming a carded web (20) in which staple fibers are oriented in a horizontal direction relative to the plane of the nonwoven sheet to be manufactured. In order to uniformly form the staple fibers forming the carded web (20), a mixed fiber process for uniformly mixing the staple fibers may be performed prior to the carding process.
[0006] The above carded web (20) is supplied to a cross lapper (30) and is vertically laminated on a conveyor belt (40) that runs in the machine direction (MD) from the cross lapper (30) to form a forming web (50). That is, after the carded web (20) is laminated on a conveyor belt (40) that runs in the machine direction and rotates from the cross lapper (30) in the vertical direction of the machine direction, a non-woven fabric is formed through a binding process such as needle punching. In addition, the short-fiber non-woven fabric can also be manufactured through a process such as thermal bonding or spunlace.
[0007] And, long-fiber nonwoven fabrics can be manufactured by a spunbond method, etc. In the spunbond nonwoven fabric manufacturing method, multifilament yarns spun from a spinning block are cooled and solidified in a cooling chamber, then supplied to a high-pressure air ejector, and are continuously stretched through a stretching tube or high-pressure air pipe and an opening means, and then laminated in the form of a web on a net conveyor. The laminated web as described above can be manufactured by simultaneously applying heat and pressure using a calendar roll to combine the multifilament yarns to give them a certain thickness and physical properties, and then winding them.
[0008]
[0009] Nonwoven fabrics manufactured as described above are used in a variety of fields. However, when actually used in products in each field, they must be manufactured with properties and structures appropriate for each product's intended use. Recently, demand for multilayer nonwoven fabrics, designed to achieve a variety of desired functions by laminating multiple nonwoven fabrics, is increasing.
[0010] As a prior art related to such multilayer nonwoven fabrics, Japanese Patent No. 3587831 proposes a multilayer nonwoven fabric having a first fiber layer and a second fiber layer including latent crimped fibers laminated as a surface sheet used on a skin-contacting surface of an absorbent article, wherein the first fiber layer and the second fiber layer are partially heat-fused at a plurality of locations, and the multilayer nonwoven fabric is manufactured by heat-treating the multilayer fibers, wherein a plurality of raised portions are formed in the first fiber layer. In addition, Korean Patent Laid-Open Publication No. 10-2004-0012353 proposes a method for manufacturing a multi-composite laminate nonwoven fabric for civil engineering, characterized by combining a) a lower layer containing a long-fiber nonwoven fabric, b) a middle layer in which heat-shrinkable polypropylene-based short-fiber fibers are introduced from the left and right sides in a range of 40 to 50 degrees with respect to the mechanical traveling direction of the lower layer and alternately and repeatedly laminated, and c) an upper layer positioned on the middle layer and in which polypropylene-based short-fiber fibers are laminated.
[0011]
[0012] According to the above-described prior art, a nonwoven fabric exhibiting elasticity must be manufactured using a composite yarn of the sheath-core or side-by-side type that has elasticity by compositely spinning two or more types of polymers. However, a web manufactured using such yarn is prone to fibers getting caught in the needles and breaking during needle punching. In addition, an elastic nonwoven fabric manufactured using such a composite yarn has the problem of a complicated manufacturing process, which increases the manufacturing cost.
[0013]
[0014]
[0015] The problem to be solved by the present invention is to provide a method for manufacturing a multifunctional composite nonwoven fabric, characterized in that a first sheet layer made of any one of a long-fiber web, a short-fiber nonwoven fabric, and a long-fiber nonwoven fabric and a second sheet layer made of any one of a short-fiber web, a film, and an ultra-fine fiber web are laminated, a multifunctional composite nonwoven fabric is manufactured by laminating a composite sheet layer by laminating the first sheet layer multiple times in a cross-lapper, and then joining the first and second sheet layers by interlacing the first and second sheet layers through a fiber fastening process, and a multifunctional composite nonwoven fabric manufactured thereby.
[0016] The method for manufacturing a multifunctional composite nonwoven fabric of the present invention for solving the above problem comprises: a first step of preparing a first sheet layer having a predetermined thickness and width; a second step of preparing a second sheet layer having a predetermined thickness and width; a third step of laminating the first sheet layer prepared in the first step and the second sheet layer prepared in the second step to manufacture a composite sheet layer; a fourth step of supplying the composite sheet layer manufactured in the third step to a cross-lapper and laminating it multiple times in a sheet form to manufacture a laminated sheet layer; a fifth step of manufacturing a composite nonwoven fabric by interweaving the first sheet layer and the second sheet layer of the laminated sheet layer manufactured in the fourth step through a fiber fastening process; And a sixth step of winding the composite nonwoven fabric manufactured in the fifth step; wherein the first sheet layer may be any one of a long-fiber web, a short-fiber nonwoven fabric, and a long-fiber nonwoven fabric, wherein the short-fiber nonwoven fabric is a spunlace or heat-bonded nonwoven fabric, and the long-fiber nonwoven fabric is a spunbond nonwoven fabric, and the long-fiber web, short-fiber nonwoven fabric, and long-fiber nonwoven fabric may be manufactured from polypropylene fiber, polyester fiber, nylon fiber, aramid fiber, and may be manufactured from general yarn or split yarn.
[0017]
[0018] In addition, the fiber fastening process in the fifth step is any one of a needle punching process, a thermal bonding process, a water jet process, and a steam jet process, the second sheet layer has any one of a short fiber web, a film, and an ultrafine fiber web, the short fiber web or film constituting the second sheet layer may be made of a thermoplastic elastomer, the ultrafine fiber web constituting the second sheet layer may be a meltblown web or nanofiber web made of a thermoplastic polymer, the width of the second sheet layer may be smaller than or equal to the width of the first sheet layer, the thickness of the first sheet layer is 0.1 to 3.5 mm, the thickness of the second sheet layer is 0.1 to 2.0 mm, and the sixth step is preferably performed at 80 to 150°C for 100 to 900 seconds.
[0019] The multifunctional composite nonwoven fabric manufactured by the present invention can manufacture a multifunctional composite nonwoven fabric having excellent elasticity, elastic recovery, and filtering effect by laminating and interlocking a first sheet layer manufactured from any one of a long-fiber web, a short-fiber nonwoven fabric, and a long-fiber nonwoven fabric with a second sheet layer manufactured from any one of a short-fiber web, a film, and an ultra-fine fiber web, and then bonding them through a fiber fastening process. In addition, the multifunctional composite nonwoven fabric manufactured as described above has excellent formability so that it can be applied to various purposes such as artificial leather, nonwoven rolls, or filters.
[0020]
[0021] Figure 1 is a manufacturing process diagram of a single-fiber nonwoven fabric according to the prior art.
[0022] Figure 2 is a flow chart of a method for manufacturing a multifunctional composite nonwoven fabric according to the present invention.
[0023] Figure 3 is a needle punching process diagram for manufacturing a multifunctional composite nonwoven fabric according to the present invention.
[0024] Figure 4 is a photograph of a multifunctional composite nonwoven fabric according to the present invention.
[0025]
[0026] In this application, it should be understood that terms such as “include,” “have,” or “comprising” are intended to specify the presence of a feature, number, step, component, part, or combination thereof described in the specification, and do not preclude the possibility of the presence or addition of one or more other features, numbers, steps, operations, components, parts, or combinations thereof. In addition, unless otherwise defined, all terms used herein, including technical or scientific terms, have the same meaning as commonly understood by a person of ordinary skill in the art to which the present invention pertains. Terms defined in commonly used dictionaries should be interpreted as having a meaning consistent with the meaning they have in the context of the relevant art, and shall not be interpreted in an idealized or excessively formal sense unless explicitly defined in this application.
[0027]
[0028] Hereinafter, the method for manufacturing a multifunctional composite nonwoven fabric according to the present invention and the multifunctional composite nonwoven fabric manufactured therefrom will be described in detail. Figure 1 attached to the present invention is a process diagram for manufacturing a short-fiber nonwoven fabric according to the prior art, Figure 2 is a flow chart for a method for manufacturing a multifunctional composite nonwoven fabric according to the present invention, Figure 3 is a needle punching process diagram for manufacturing a multifunctional composite nonwoven fabric according to the present invention, and Figure 4 is a photograph of a multifunctional composite nonwoven fabric according to the present invention.
[0029]
[0030] The multifunctional composite nonwoven fabric according to the present invention has excellent elasticity, elastic recovery, and filtering effect, and can be used as a base material for manufacturing filters, nonwoven rolls, or artificial leather.
[0031]
[0032] A filter is a structure that filters out foreign substances in liquids or gases, and can be manufactured with various materials and shapes. A non-woven roll is a roll manufactured using non-woven fabric. It is mainly used when removing impurities from the surface of a base material such as an iron plate or when treating it with medicine or oil. In addition, non-woven fabric is widely used as a base material for manufacturing artificial leather. Artificial leather is an artificial material created to replace the appearance and properties of natural leather, and can be widely used as a material to replace natural leather.
[0033]
[0034] The method for manufacturing a multifunctional composite nonwoven fabric according to the present invention preferably includes, as illustrated in FIG. 2, a first step of preparing a first sheet layer having a predetermined thickness and width; a second step of preparing a second sheet layer having a predetermined thickness and width; a third step of laminating the first sheet layer prepared in the first step and the second sheet layer prepared in the second step to manufacture a composite sheet layer; a fourth step of supplying the composite sheet layer manufactured in the third step to a cross-lapper and laminating the sheet layers multiple times to manufacture a laminated sheet layer; a fifth step of manufacturing a composite nonwoven fabric by interweaving the first sheet layer and the second sheet layer through a fiber fastening process in the laminated sheet layer manufactured in the fourth step; and a sixth step of winding the composite nonwoven fabric manufactured in the fifth step.
[0035]
[0036] Looking at this in detail, the first step is a step of preparing a first sheet layer (80) having a certain thickness and width, and it may be preferable for the first sheet layer (80) to be composed of any one of a long-fiber web, a short-fiber nonwoven fabric, and a long-fiber nonwoven fabric.
[0037]
[0038] The above-mentioned long-fiber web is a web manufactured using long fibers as a preliminary step in manufacturing a long-fiber nonwoven fabric, and refers to a state before the fibers constituting the long-fiber web are combined. In addition, the above-mentioned long-fiber nonwoven fabric refers to a form in which the fibers constituting the long-fiber web are combined through a fiber-fastening process such as needle punching.
[0039] In addition, a short-fiber nonwoven fabric is a nonwoven fabric manufactured using short fibers rather than long fibers, and refers to a form in which the fibers constituting the short-fiber nonwoven fabric are combined through a fiber fastening process.
[0040] According to the present invention, it may be preferable that the single-fiber nonwoven fabric is a spunlace nonwoven fabric or a thermal bonding nonwoven fabric, and the long-fiber nonwoven fabric is a spunbond nonwoven fabric.
[0041] The above spunlace nonwoven fabric refers to a nonwoven fabric manufactured by intertwining and binding constituent fibers using water spray, and the above heat-bonded nonwoven fabric refers to a nonwoven fabric manufactured by bonding a web containing thermoplastic synthetic fibers by melting the web using heat. The above spunbond nonwoven fabric refers to a nonwoven fabric manufactured by continuously bonding melted and spun long fibers.
[0042]
[0043] According to the present invention, the long fiber web, short fiber nonwoven fabric and long fiber nonwoven fabric constituting the first sheet layer (80) are preferably made of a thermoplastic polymer material, such as one of nylon, polyester, polypropylene and aramid fiber.
[0044]
[0045] In addition, the long fiber web, short fiber nonwoven fabric, and long fiber nonwoven fabric constituting the first sheet layer (80) may be a mixture of two or more types of fibers manufactured from thermoplastic polymer materials such as nylon, polyester, polypropylene, and aramid fibers.
[0046]
[0047] According to the present invention, the long fiber web, short fiber nonwoven fabric and long fiber nonwoven fabric constituting the first sheet layer (80) can be manufactured from general yarn or split yarn.
[0048] In the present invention, the fiber manufactured solely from the thermoplastic polymer material is referred to as a general fiber, and the split fiber refers to a fiber in which a heterogeneous polymer resin is composed of multiple pieces on the fiber cross-section, and which is subsequently divided into individual pieces through post-processing such as splitting. The split fiber as described above is a fiber that can be manufactured with a single-yarn fineness of 0.5 denier or less, and is one of the most commercially used ultrafine fibers along with island-in-the-sea yarn.
[0049]
[0050] The long-fiber web manufactured as a split yarn as described above is manufactured in the form of an ultra-fine yarn, and thus has an excellent feel and can exhibit excellent performances such as a feeling of fullness and flexibility. In particular, by manufacturing the long-fiber web as a split yarn, chemical treatment to remove marine components, such as with island-in-the-sea yarn, is unnecessary, and when manufacturing artificial leather, it can produce artificial leather that has a feel similar to natural leather and can replace it. In addition, in the present invention, the general yarn refers to a fiber, not a split yarn.
[0051]
[0052] The thickness of the first sheet layer (80) manufactured as described above may preferably be 0.1 to 3.5 mm. That is, when the multifunctional composite nonwoven fabric according to the present invention is used as artificial leather, the thickness of the first sheet layer (80) may preferably be 0.1 mm in order to manufacture the artificial leather with a thin thickness. In particular, when the multifunctional composite nonwoven fabric according to the present invention is used for purposes such as a filter, the thickness of the first sheet layer (80) may preferably be 3.5 mm in order to maximize the filtering effect by increasing the thickness.
[0053]
[0054] According to the present invention, the second step is a step of preparing a second sheet layer (70) to be laminated together with the first sheet layer (80), and it is preferable that the second sheet layer (70) be manufactured in the form of any one of a single fiber web, a film, and an ultrafine fiber web.
[0055]
[0056] That is, when the use of the multifunctional composite nonwoven fabric according to the present invention is artificial leather or a nonwoven roll, it may be preferable to use a short-fiber web or film manufactured using a thermoplastic elastomer as the second sheet layer (70). When the short-fiber web or film manufactured using a thermoplastic elastomer is used as the second sheet layer (70) as described above, it is possible to impart elasticity and elastic recovery properties to the manufactured multifunctional composite nonwoven fabric.
[0057]
[0058] The thermoplastic elastomer (TPE) mentioned above, like thermoplastic synthetic resins, refers to a material that can be injection-molded or extruded by applying heat. After cooling, it regains its original high-elasticity properties, making it recyclable.
[0059] According to the present invention, the thermoplastic elastomer constituting the second sheet layer (70) may be composed of any one of a thermoplastic polyurethane elastomer, a thermoplastic olefin-based elastomer, and a thermoplastic polyamide-based elastomer.
[0060]
[0061] The above thermoplastic polyurethane elastomer refers to an elastomer having a urethane bond in its molecular structure, which is a compound synthesized through an addition reaction of isocyanate and polyol. The above thermoplastic polyurethane elastomer has high resilience, excellent compressive strain, and excellent impact, wear, and tear properties, and refers to a synthetic resin produced through a polymerization reaction of diisocyanate and one or more diols. The TPU provides flexibility without using a plasticizer, as well as a wide range of hardness and high elasticity.
[0062]
[0063] Thermoplastic olefin elastomers can be manufactured as binary alloys by blending ethylene-propylene comonomer as an impact modifier with the general-purpose resin polypropylene. Furthermore, ternary alloys can be manufactured by adding small amounts of polyethylene. These thermoplastic olefin elastomers are manufactured and sold by manufacturers of ethylene-propylene diene monomer (EPDM), including DUPONT, Exxon, Goodrich, and Dow Chemical.
[0064]
[0065] Also, thermoplastic polyamide elastomer refers to a multi-block copolymer in which crystalline polyamide forms a hard segment and a rubber-like polyether or polyester with a low glass transition temperature forms a soft segment. The thermoplastic polyamide elastomer was first produced by Atofina in 1983 and released under the trade name Pebax. Afterwards, Evonik Degussa GmbH of Germany developed a polyamide-b-polyether with polyamide-12 as a hard segment and released it under the trade name VESTAMID E, and EMS-Grivory AG of Switzerland released a thermoplastic polyamide elastomer with nylon 6 and nylon 12 as hard segments under the trade name Grilamide.
[0066]
[0067] In addition, that is, when the multifunctional composite nonwoven fabric according to the present invention is used as a filter, it is preferable to use an ultrafine fiber web manufactured using a thermoplastic polymer such as polyester or polypropylene as the second sheet layer (70). The ultrafine fiber web refers to an ultrafine fiber web manufactured by a process such as meltblown or electrospinning. When an ultrafine fiber web is used as the second sheet layer (70) as described above, a filtering effect capable of removing foreign substances from the ultrafine fiber web can be imparted.
[0068]
[0069] According to the present invention, the second sheet layer (70) prepared in the second step may be manufactured as a single-fiber web or film manufactured using a thermoplastic elastomer. In addition, the second sheet layer (70) prepared in the second step may also be manufactured as an ultrafine fiber web manufactured using a thermoplastic polymer.
[0070]
[0071] As described above, the thickness of the second sheet layer (70) prepared through the second step is preferably 0.1 to 2.0 mm. That is, in order to smoothly perform the lamination process when laminating the first sheet layer (80) and the second sheet layer (70) in the subsequent third step, and to smoothly perform the bonding of the first sheet layer (80) and the second sheet layer (70), the thickness of the second sheet layer (70) is preferably 0.1 to 2.0 mm.
[0072]
[0073] According to the present invention, the second sheet layer (70) prepared in the second step may have a color. That is, when the second sheet layer (70) has a color as described above, it can be laminated on one side of the first sheet layer (80) and heat-treated to color the multifunctional composite nonwoven fabric produced, thereby imparting color.
[0074]
[0075] After preparing the first sheet layer (80) and the second sheet layer (70) as described above, a third step is performed in which the first sheet layer (80) prepared in the first step and the second sheet layer (70) prepared in the second step are laminated to manufacture a composite sheet layer (85).
[0076] The third step is to form a composite sheet layer (85) by sequentially stacking the first sheet layer (80) and the second sheet layer (70) using a conventional nonwoven web forming device.
[0077] The third step can be performed by laminating one of the long-fiber web, short-fiber nonwoven fabric, and long-fiber nonwoven fabric constituting the first sheet layer (80) and one of the short-fiber web, film, and ultra-fine fiber web constituting the second sheet layer (70), and at this time, the width of the second sheet layer (70) is preferably smaller than or equal to the width of the first sheet layer (80).
[0078] That is, when the use of the multifunctional composite nonwoven fabric according to the present invention is artificial leather or a filter, it may be preferable to provide the width of the second sheet layer (70) to be smaller than the width of the first sheet layer (80) in order to provide a concentration gradient of the thermoplastic elastomer constituting the second sheet layer (70) along the cross-section of the multifunctional composite nonwoven fabric being manufactured. When the width of the second sheet layer (70) is provided to be smaller than the width of the first sheet layer (80) as described above, a portion of the first sheet layer (80) is laminated with the second sheet layer (80), thereby providing a concentration gradient of the thermoplastic elastomer constituting the second sheet layer (70) along the cross-section of the multifunctional composite nonwoven fabric being manufactured.
[0079]
[0080] In addition, when the use of the multifunctional composite nonwoven fabric according to the present invention is a nonwoven fabric roll, the first sheet layer (80) and the second sheet layer (70) are laminated with the same width, so that the second sheet layer (70) is laminated on the entire surface of the first sheet layer (80), and the multifunctional composite nonwoven fabric can be manufactured so that the fibers constituting the first sheet layer (80) and the second sheet layer (70) have the same concentration along the cross-section of the manufactured multifunctional composite nonwoven fabric.
[0081]
[0082] After performing the above third step, as the fourth step, the composite sheet layer (85) manufactured in the third step is supplied to a cross lapper (30) and folded multiple times in a sheet shape to manufacture a laminated sheet layer (60). This corresponds to a process of forming a molded web (50) by supplying a carded web (20) to a cross lapper (30) and stacking it vertically on a conveyor belt (40) in the conventional technology, as illustrated in FIG. 1.
[0083]
[0084] As described above, the composite sheet layer (85) manufactured in the third step is fed into the cross lapper (30) and dropped vertically onto the conveyor belt (40) that runs in the machine direction, thereby stacking the composite sheet layer (85) in a direction perpendicular to the machine direction. The laminated sheet layer (60) manufactured through the fourth step as described above is then subjected to the fifth step, which is the fiber fastening process, to intertwine the first sheet layer (80) and the second sheet layer (70), thereby manufacturing a composite nonwoven fabric (90).
[0085]
[0086] The fourth step above is to manufacture a laminated sheet layer (60) by placing the composite sheet layer (85) manufactured in the third step into a cross-lapper (30) and dropping the composite sheet layer (85) onto a conveyor belt (40) moving in the machine direction while stacking the composite sheet layer (85) on top in a direction perpendicular to the machine direction.
[0087]
[0088] That is, a composite sheet layer (85) manufactured by stacking the first sheet layer (80) prepared in the first step and the second sheet layer (70) prepared in the second step multiple times is supplied to a cross lapper (30) and folded multiple times into a sheet shape, thereby manufacturing a laminated sheet layer (60).
[0089]
[0090] After performing the fourth step as described above, it is also possible to add a step of adjusting the weight per unit area (㎡) by drafting the manufactured laminated sheet layer (60).
[0091] A typical nonwoven web forming device includes a draft module, which uses a plurality of rollers to draft and stretch the laminated sheet layer (60). Through the draft process, the laminated sheet layer (60) is uniformed and the weight per unit area (㎡) is controlled. The draft ratio in the draft module can be adjusted in various ways according to user settings.
[0092]
[0093] The laminated sheet layer (60) manufactured through the above-mentioned fourth step is then manufactured as a composite nonwoven fabric (90) by interlocking the first sheet layer (80) and the second sheet layer (70) constituting the laminated sheet layer (60) through a fiber fastening process in the fifth step.
[0094] The above fiber fastening process refers to a process for intertwining and binding the fibers that constitute the laminated sheet layer (60) manufactured in the fourth step. According to the present invention, the fiber fastening process may be any one of a needle punching process, a thermal bonding process, a water jet process, and a steam jet process that are repeatedly performed on the upper or lower portion of the laminated sheet layer (60).
[0095]
[0096] As a fiber fastening process, the needle punching process refers to a process of manufacturing a composite nonwoven fabric (90) by moving a needle with a barb up and down and passing the laminated sheet layer (60) through the up and down movement area of the needle, thereby intertwining the fibers constituting the laminated sheet layer (60) together.
[0097] The needle punching process performed in the fifth step above refers to a process of interlocking and joining the laminated sheet layers (60) manufactured in the fourth step above in a needle punching machine (100), as illustrated in FIG. 3.
[0098] According to the present invention, the fifth step can be performed through a needle punching process that is repeatedly performed on the upper or lower part of the laminated sheet layer (60) in which the first sheet layer (80) and the second sheet layer (70) are laminated, as illustrated in FIG. 3.
[0099] That is, when the first sheet layer (80) is composed of a long fiber web and the second sheet layer (70) is composed of a thermoplastic elastomer film, the long fiber web constituting the first sheet layer (80) and the thermoplastic elastomer film constituting the second sheet layer (70) are needle-punched from the top to the bottom of the laminated sheet layer (60) by a downward punching unit (110) provided on one side of the needle punching machine (100), so that the long fibers constituting the long fiber web of the laminated sheet layer (60) penetrate downward through the thermoplastic elastomer film and interlace with the thermoplastic elastomer film, thereby allowing the long fibers to be laminated.
[0100]
[0101] When the first sheet layer (80) is made of a short-fiber nonwoven fabric or a long-fiber nonwoven fabric, and the second sheet layer (70) is made of a short-fiber web, the fibers constituting the first sheet layer (80) and the second sheet layer (70) can be intertwined and fastened by a downward punching unit (110) provided on one side of a needle punching machine (100). In addition, when the second sheet layer (70) is made of a microfiber web, the first sheet layer (80) and the second sheet layer (70) can be intertwined and fastened by the same method.
[0102]
[0103] After being punched by the downward punching part (110) as described above, the first sheet layer (80) and the second sheet layer (70) can be interlocked and more tightly fastened by needle punching from the bottom to the top by the upward punching part (120) provided on one side of the downward punching part (110).
[0104]
[0105] The needle punching performed in the fifth step above is performed by first needle-punching the upper part of the laminated sheet layer (60) and then needle-punching the lower part, or in the opposite order, so that the first sheet layer (80) and the second sheet layer (70) are intertwined and integrated (laminated), thereby manufacturing a composite nonwoven fabric (90).
[0106]
[0107] That is, first, the laminated sheet layer (60) is transferred to the downward punching unit (110) so that the upper surface of the laminated sheet layer (60) is needle-punched. Thereafter, as illustrated in FIG. 3, while the laminated sheet layer (60) is transferred to the upward punching unit (120), needle-punching is performed from the lower side of the laminated sheet layer (60) to the upper side by the upward punching unit (120), so that the components constituting the laminated sheet layer (60) are interlocked and combined.
[0108] In addition, when the second sheet layer (70) is composed of a thermoplastic elastomer film, the long fibers constituting the first sheet layer (80) can be connected by intertwining the long fibers with the thermoplastic elastomer film while penetrating downward through the thermoplastic elastomer film.
[0109]
[0110] As described above, the laminated sheet layer (60) needle-punched by the downward punching unit (110) is then transferred to the upward punching unit (120), and needle-punching is performed from the lower portion of the laminated sheet layer (60) to the upper portion by the upward punching unit (120), so that the long fiber web or long fiber support fabric constituting the first sheet layer (80) and the short fiber web, film or ultra-fine fiber web constituting the second sheet layer (70) can be intertwined and joined.
[0111] By repeatedly performing needle punching as described above, the first sheet layer (80) and the second sheet layer (70) constituting the laminated sheet layer (60) can be densely and uniformly laminated.
[0112]
[0113] According to the present invention, the fiber bonding process performed in the fifth step may also be performed by a thermal bonding process, a water jet process, a steam jet process, or the like.
[0114] The above thermal bonding process refers to a process of manufacturing a composite nonwoven fabric (90) by heating and melting some of the fibers constituting the laminated sheet layer (60) and bonding them, and the water jet process refers to a process of manufacturing a composite nonwoven fabric (90) by intertwining the fibers constituting the laminated sheet layer (60) together using water sprayed at high pressure.
[0115] In particular, the steam jet process is a process developed by Kuraray Co., Ltd. of Japan, which uses high-pressure steam to three-dimensionally interlace a web. It refers to a method of interlacing and combining the constituent fibers of the web in three dimensions by spraying high-pressure air onto the web through the grooves of an air knife.
[0116]
[0117] That is, a composite nonwoven fabric (90) can be manufactured by interlocking the first sheet layer (80) and the second sheet layer (70) of the laminated sheet layer (60) through any one of the needle punching process, thermal bonding process, water jet process, and steam jet process as a fiber fastening process through the fifth step.
[0118]
[0119] According to the present invention, when manufacturing a composite nonwoven fabric (90) by intertwining the first sheet layer (80) and the second sheet layer (70) through a needle punching process or a water jet process as the fiber fastening process, a heat treatment process may be additionally included.
[0120] That is, since the composite nonwoven fabric (90) manufactured by the needle punching process or the water jet process is in a state where its structural structure is stressed by an external force, it is necessary to remove this stress to prevent deformation of the composite nonwoven fabric (90) that may occur in the future. Therefore, in the fifth step, the stress applied to the composite nonwoven fabric (90) manufactured by the needle punching process or the water jet process is removed by heat treating the surface. In addition, through the heat treatment, the surface of the composite nonwoven fabric (90) can be flattened and uniformed at the same time.
[0121] As shown in Fig. 3, a composite nonwoven fabric (9) manufactured by a needle punching process is transferred to a heat treatment device (200), and then a step of heat treating the composite nonwoven fabric (90) to remove stress is performed.
[0122] The above heat treatment can be performed using a heat treatment device (200) such as a tenter, and at this time, the heat treatment may preferably be performed at 80 to 150°C for 100 to 900 seconds. That is, the composite nonwoven fabric (90) transferred to the heat treatment device (200) is heat treated at 80 to 150°C for 100 to 900 seconds, thereby removing the stress applied to the structure of the composite nonwoven fabric (90) and flattening and uniforming the surface.
[0123] In addition, the composite nonwoven fabric (9) manufactured by the water jet process can be dried simultaneously through heat treatment.
[0124]
[0125] After the above 5th step, the 6th step of winding the manufactured composite nonwoven fabric (90) using a roll or the like is performed, thereby completing the manufacture of a multifunctional composite nonwoven fabric according to the present invention as shown in FIG. 4.
[0126]
[0127] The multifunctional composite nonwoven fabric manufactured as described above according to the present invention can exhibit excellent elasticity by being manufactured by laminating and interweaving thermoplastic elastomer in the form of a single fiber web or film as the second sheet layer (70). In particular, it has excellent elastic recovery force in both the horizontal and vertical directions, and thus has the characteristic of being applicable to applications such as artificial leather and nonwoven rolls. In addition, the multifunctional composite nonwoven fabric can be manufactured by laminating and interweaving ultrafine fiber webs as the second sheet layer (70), and thus imparting excellent filtering properties.
[0128]
[0129] Although the present invention has been described with reference to the experimental examples illustrated in the drawings, these are merely exemplary, and those skilled in the art will understand that various modifications and equivalent other experimental examples are possible from the examples. Furthermore, those skilled in the art to which the present invention pertains will understand that the present invention can be easily modified into other specific forms without changing the technical spirit or essential characteristics of the present invention. Therefore, it should be understood that the embodiments described above are exemplary in all respects and not restrictive, and the true technical protection scope of the present invention should be determined by the technical spirit of the appended claims.
[0130]
[0131] [Explanation of symbols]
[0132] 10: Carding machine
[0133] 30: Crossrapper
[0134] 40: Conveyor belt
[0135] 60: Laminated sheet layer
[0136] 70: Second sheet layer
[0137] 80: 1st sheet layer
[0138] 85: Composite sheet layer
[0139] 90: Composite nonwoven fabric
Claims
1. Step 1: preparing a first sheet layer having a certain thickness and width; A second step of preparing a second sheet layer having a certain thickness and width; A third step of manufacturing a composite sheet layer by laminating the first sheet layer prepared in the first step and the second sheet layer prepared in the second step; A fourth step of supplying the composite sheet layer manufactured in the third step to a cross-lapper and folding it multiple times in a sheet form to manufacture a laminated sheet layer; A fifth step of manufacturing a composite nonwoven fabric by interlocking the first sheet layer and the second sheet layer through a fiber fastening process in the laminated sheet layer manufactured in the fourth step; and A method for manufacturing a multifunctional composite nonwoven fabric, comprising a sixth step of winding the composite nonwoven fabric manufactured in the fifth step.
2. In claim 1, A method for manufacturing a multifunctional composite nonwoven fabric, characterized in that the first sheet layer is any one of a long-fiber web, a short-fiber nonwoven fabric, and a long-fiber nonwoven fabric.
3. In claim 2, A method for producing a multifunctional composite nonwoven fabric, characterized in that the long-fiber web, short-fiber nonwoven fabric or long-fiber nonwoven fabric is produced from any one of polypropylene fiber, polyester fiber, nylon fiber and aramid fiber.
4. In claim 1, A method for manufacturing a multifunctional composite nonwoven fabric, characterized in that the second sheet layer has the form of any one of a single fiber web, a film, and an ultra-fine fiber web.
5. In claim 1, A method for manufacturing a multifunctional composite nonwoven fabric, characterized in that the fiber fastening process in the fifth step is any one of a needle punching process, a thermal bonding process, a water jet process, and a steam jet process.
6. A multifunctional composite nonwoven fabric manufactured by the method for manufacturing a multifunctional composite nonwoven fabric according to any one of claims 1 to 5.
Citation Information
Patent Citations
Filtrating medium for air filter, streamer-shaped filter using the same, and manufacturing method of filterating medium for air filter
JP2008055270A
Manufacturing method of non-woven fabric for hidden surface type artificial leather
KR100500745B1
Bubble for artificial leather and method for producing same
KR101505632B1
Apparatus based on artificial intelligence for providing recommendation by determining similar situation data
KR1020220121095A
Manufacturing method of multi-functional non-woven fabric and multi-functional non-woven fabric prepared therefrom
KR102599166B1