Chemical coolant for aerosol fire extinguishing agent and preparation method
By combining organic flame retardant and metal inorganic salts that can undergo decomposition reactions in chemical coolant, the problem of energy waste of hot aerosol fire extinguishing agent is solved, and more efficient fire extinguishing and cooling effects are achieved, and the stability of the finished product is improved.
Patent Information
- Application Number
- PCT/CN2023/098896
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-12
- Filing Date
- 2023-06-07
- Publication Date
- 2024-11-21
AI Technical Summary
The chemical coolant of existing hot aerosol fire extinguishing agents has limited effect in flame reduction and cooling, and has failed to make full use of the heat generated during the fire extinguishing process, resulting in waste of energy.
Chemical coolant composed of 30%-69% organic flame retardant, 30%-69% metal inorganic salts that can undergo decomposition reactions and 1%-10% binder, through organic flame retardant and metal inorganic The combined action of salt can achieve heat absorption and cooling and produce fire-extinguishing active substances, enhance fire-extinguishing capacity, and improve the stability of the finished product through binders.
While ensuring the smoke-removing and cooling effect, the fire extinguishing ability of the aerosol fire extinguishing agent is improved, the cooling effect is enhanced, the stability of the chemical coolant is improved, the powdering phenomenon is avoided, and the spraying temperature and fire extinguishing time are reduced.
Smart Images

Figure PCTCN2023098896-FTAPPB-I100001
Abstract
Description
Chemical coolant for aerosol fire extinguishing agent and preparation method thereof Technical Field
[0001] The invention belongs to the technical field of chemical coolants, and particularly relates to a chemical coolant for aerosol fire extinguishing agent and a preparation method thereof. Background Art
[0002] When thermal aerosol fire extinguishing agents burn, they produce large amounts of non-combustible gases such as N2, CO2, and water vapor, as well as solid oxide particles such as potassium and strontium. The non-combustible gases can reduce the concentration of combustible gases and oxygen in the fire scene, suppressing the flames. The oxide solid particles can capture HO·, H·, and O· free radicals, reducing the concentration of active free radicals in the fire scene to achieve chemical suppression and extinguish fires, thus extinguishing fires from multiple dimensions. Furthermore, with technological advances, the corrosiveness and environmental pollution of thermal aerosol fire extinguishing agents produced are becoming increasingly less, and their application is also becoming increasingly widespread. However, thermal aerosol fire extinguishing agents require combustion during fire extinguishing, which is a highly exothermic reaction. During spraying, their maximum temperature can reach around 1000°C, posing significant safety hazards and secondary disasters. Therefore, to reduce safety hazards, it is necessary to block or absorb the heat generated during the combustion of thermal aerosol fire extinguishing agents.
[0003] At present, the method of combining hot aerosol fire extinguishing agent with coolant to reduce the spraying temperature is generally adopted. Commonly used coolants are divided into physical coolants and chemical coolants. Chinese patent CN102872557B discloses a physical cooling method to replace the chemical coolant of aerosol fire extinguishing device. By installing a physical deceleration agent and a physical coolant above the cartridge, the chemical coolant is replaced to achieve rapid cooling and ensure rapid airflow circulation; Chinese patent CN101716404B discloses a cooling filter layer of hot aerosol fire extinguishing equipment, in which a chemical coolant is loaded on the cooling layer module, so that the chemical coolant does not damage the structural layer of the cooling module when participating in the reaction. US Patent No. US20120273714A1 discloses a catalytic chemical coolant for aerosols and its preparation method. The catalytic chemical coolant is prepared using heat-absorbing cooling materials such as manganese oxalate and potassium permanganate, along with processing aids such as metal oxides or hydroxides and stearates, and a binder comprising an alkali metal silicate and a water-soluble polymer in a solution. The coolant also includes a surface coating made of a hydroxymethyl or hydroxyethyl cellulose film. The catalytic chemical coolant exhibits high strength and excellent cooling effectiveness, and eliminates toxic gases from fire extinguishing products. Chinese Patent No. CN110755776B discloses a method for assembling a hot aerosol coolant and a hot aerosol generator. The method combines or uses a physical coolant made of cast iron, ceramic, or graphite with a chemical coolant such as basic magnesium carbonate or calcium carbonate. The hot aerosol coolant undergoes a strong exothermic reaction with the hot aerosol generator, effectively absorbing heat and cooling the air, thereby minimizing the impact on combustion and injection performance.
[0004] However, the chemical coolants currently prepared for hot aerosol fire extinguishing agents only consider their flame extinguishing and temperature reduction functions, while the large amount of heat generated during the fire extinguishing process is not fully utilized, resulting in a certain amount of energy waste.
[0005] Summary of the Invention
[0006] In response to the above technical problems, the present invention provides a chemical coolant for aerosol fire extinguishing agents and a preparation method. Based on the idea that hot aerosol fire extinguishing agents generate a large amount of heat during the combustion and spraying process, and fully utilizing this heat to produce new aerosols with fire extinguishing capabilities, a new chemical coolant is prepared, which can improve the fire extinguishing capability while ensuring the flame extinguishing and cooling effect.
[0007] In order to achieve the above object, the present invention provides a chemical coolant for aerosol fire extinguishing agent, which is composed of 30%-69% organic flame retardant, 30%-69% metal inorganic salt and 1%-10% binder.
[0008] Preferably, the organic flame retardant is any one of dicyandiamide, melamine, melamine cyanurate, melamine orthophosphate, melamine borate, melamine phosphate or melamine pyrophosphate.
[0009] Preferably, the metal inorganic salt is a K / Na / Mg / Ca / Sr inorganic salt that can undergo a decomposition reaction.
[0010] Preferably, the inorganic salt of K / Na / Mg / Ca / Sr that can undergo decomposition reaction is any one of potassium carbonate, potassium bicarbonate, sodium carbonate, sodium bicarbonate, magnesium carbonate, magnesium bicarbonate, calcium carbonate, calcium bicarbonate, strontium carbonate or strontium bicarbonate.
[0011] Preferably, the binder is any one of ethyl cellulose, phenolic resin, epoxy resin, hydroxypropyl methyl cellulose, polyvinyl alcohol or dextrin.
[0012] The present invention also provides a method for preparing a chemical coolant for an aerosol fire extinguishing agent, which specifically comprises the following steps:
[0013] (1) Weighing an organic flame retardant, a metal inorganic salt, and a binder, sieving and mixing them several times to obtain a mixture;
[0014] (2) adding anhydrous methanol to the mixture and mixing to obtain a wet material;
[0015] (3) sieving the wet material to form granules, and then drying and sieving it again to obtain coolant granules;
[0016] (4) Pressing the coolant particles to obtain a finished coolant product.
[0017] Preferably, the sieve in step (1) is 100 mesh, and the sieving times are 3-5 times.
[0018] Preferably, the mass of the anhydrous methanol in step (2) accounts for 10-20% of the weight of the mixture.
[0019] Preferably, the sieve in step (3) is 20 mesh, and the drying condition is 55-65° C. for 12-24 hours, until the volatile content is less than 1%.
[0020] Preferably, the pressing condition in step (4) is 10 MPa, and the diameter of the finished coolant product is 6 mm and the height is 5.5 mm.
[0021] The beneficial effects of the present invention are as follows: K / Na / Mg / Ca / Sr inorganic salts capable of undergoing decomposition reactions are used as the main components of the coolant. The decomposition reaction undergoes an endothermic decomposition reaction and simultaneously produces fire-extinguishing active metal substances, thereby improving the fire extinguishing ability of the aerosol fire extinguishing agent while reducing smoke and temperature. The organic flame retardant used in combination also undergoes a thermal decomposition reaction at around 300°C to absorb heat and simultaneously produce non-combustible gases such as NH3, N2, CO2, and water vapor, which can reduce the concentration of combustible gas and oxygen and cover the flame, thereby enhancing the cooling and fire extinguishing capabilities. In addition, the selected organic flame retardant also has a certain degree of adhesion, and cooperates with the adhesive to bond the metal inorganic salt, thereby improving the adhesion of the chemical coolant, preventing the metal inorganic salt from pulverizing, and improving the stability of the finished chemical coolant during storage, transportation, and use, thereby ensuring the cooling effect on the aerosol fire extinguishing agent. DETAILED DESCRIPTION
[0022] The technical solutions of the present invention are further explained below with reference to specific embodiments. It is worth noting that the following embodiments are only preferred embodiments of the present invention and should not be construed as limiting the present invention. The scope of protection of the present invention shall be determined by the claims. Any modifications or substitutions made to the technical solutions of the present invention by those skilled in the art without creative effort shall fall within the scope of protection of the present invention.
[0023] Example 1
[0024] (1) Weighing 50% potassium carbonate, 45% dicyandiamide, and 5% phenolic resin with a mesh size less than 100, passing through a 100-mesh sieve three times, and dry-mixing the mixture to obtain a uniform mixture;
[0025] (2) Weighing 14% anhydrous methanol and adding it to the mixture, mixing evenly to obtain a wet material;
[0026] (3) passing the wet material through a 20-mesh screen to granulate, and then drying at 55° C. for 12 h to 24 h until the volatile matter content is less than 1%, thereby obtaining chemical coolant granules;
[0027] (4) The coolant particles were placed in a tablet press and pressed at 10 MPa to obtain a finished chemical coolant product with a diameter of 6 mm and a height of 5.5 mm. The finished product was in a cylindrical shape.
[0028] Example 2
[0029] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% potassium bicarbonate, 45% melamine and 5% ethyl cellulose to prepare a finished chemical coolant.
[0030] Example 3
[0031] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% sodium carbonate, 45% melamine cyanurate and 5% epoxy resin to prepare a finished chemical coolant.
[0032] Example 4
[0033] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% sodium bicarbonate, 45% melamine orthophosphate and 5% polyvinyl alcohol to prepare a finished chemical coolant.
[0034] Example 5
[0035] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% magnesium carbonate, 45% focused melamine phosphate and 5% hydroxypropyl methylcellulose to prepare a finished chemical coolant.
[0036] Example 6
[0037] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% magnesium bicarbonate, 45% melamine and 5% dextrin to prepare a finished chemical coolant.
[0038] Example 7
[0039] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% potassium carbonate, 45% dicyandiamide and 5% ethyl cellulose to prepare a finished chemical coolant.
[0040] Example 8
[0041] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 50% magnesium hydroxide, 45% dicyandiamide and 5% ethyl cellulose to prepare a finished chemical coolant.
[0042] Example 9
[0043] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 30% potassium carbonate, 60% dicyandiamide and 10% phenolic resin to prepare a finished chemical coolant.
[0044] Example 10
[0045] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 69% potassium carbonate, 30% dicyandiamide and 1% phenolic resin to prepare a finished chemical coolant.
[0046] Comparative Example 1
[0047] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 95% dicyandiamide and 5% ethyl cellulose to prepare a finished chemical coolant.
[0048] Comparative Example 2
[0049] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 99% melamine and 1% phenolic resin to prepare a finished chemical coolant.
[0050] Comparative Example 3
[0051] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 95% potassium carbonate and 5% dextrin to prepare a finished chemical coolant.
[0052] Comparative Example 4
[0053] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 80% potassium carbonate and 20% dextrin to prepare a finished chemical coolant.
[0054] Comparative Example 5
[0055] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 20% sodium bicarbonate, 79% dicyandiamide and 1% dextrin to prepare a finished chemical coolant.
[0056] Comparative Example 6
[0057] The method and steps are the same as those in Example 1, wherein the raw materials are replaced with 79% sodium bicarbonate, 20% dicyandiamide and 1% dextrin to prepare a finished chemical coolant.
[0058] Results test:
[0059] 70 g of the finished chemical coolant and physical coolant (Φ6 ceramic balls) prepared in Examples 1-10 and Comparative Examples 1-6 were each assembled with 50 g of a K-type aerosol fire extinguishing agent charge (homemade, 73% KNO3 + 27% reducing agent) into a small fire extinguishing device. A discharge experiment was conducted. The device was weighed before and after the experiment, and the discharge volume was obtained by the weight difference before and after. Simultaneously, the temperature at 0.5 cm from the device nozzle was measured during the discharge experiment.
[0060] The finished chemical coolants prepared in Examples 1-10 and Comparative Examples 1-5 were placed in a high humidity test at a humidity of 85% and a temperature of 25° C. The powdering of the finished chemical coolants was observed and recorded after 12 h, 24 h, and 1 week.
[0061] The results are shown in the table below:
[0062] The results are shown in Table 1: Compared with physical coolants, the chemical coolants prepared in Examples 1-10 have lower spraying temperatures, shorter fire extinguishing times, and higher spraying volumes during the spraying experiments. Moreover, after the high humidity experiment, the finished chemical coolants did not pulverize, and their storage resistance was improved. However, in Comparative Examples 1 and 2, organic flame retardants were used as the active ingredients of the chemical coolants without metallic inorganic salts. Although the spraying volumes were increased compared to those in Comparative Examples 1-10, the spraying temperatures were significantly increased, the cooling effects were poor, and the fire extinguishing failed. Comparative Examples 3 and 4 used metallic organic salts as the active ingredients of the chemical coolants without the addition of organic flame retardants. Although both had good cooling and fire extinguishing effects, they were prone to pulverization. Comparative Examples 5 and 6 respectively use metal inorganic salts with too low or too high content to prepare chemical coolants. The coolant with a high metal inorganic salt content has better cooling and fire extinguishing effects, while the coolant with a low metal inorganic salt content has relatively poor cooling and fire extinguishing effects. In addition, both coolants are prone to pulverization, and the higher the inorganic salt content, the more likely it is to pulverize.
Claims
1. A chemical coolant for an aerosol fire extinguishing agent, characterized in that: It consists of 30%-69% organic flame retardant, 30%-69% metal inorganic salt and 1%-10% binder.
2. The chemical coolant for an aerosol fire extinguishing agent according to claim 1, characterized in that: The organic flame retardant is any one of dicyandiamide, melamine, melamine cyanurate, melamine orthophosphate, melamine borate, melamine phosphate or melamine pyrophosphate.
3. The chemical coolant for an aerosol fire extinguishing agent according to claim 1, characterized in that: The metal inorganic salt is a K / Na / Mg / Ca / Sr inorganic salt that can undergo a decomposition reaction.
4. The chemical coolant for an aerosol fire extinguishing agent according to claim 3, characterized in that: The inorganic salt that can undergo decomposition reaction of K / Na / Mg / Ca / Sr is any one of potassium carbonate, potassium bicarbonate, sodium carbonate, sodium bicarbonate, magnesium carbonate, magnesium bicarbonate, calcium carbonate, calcium bicarbonate, strontium carbonate or strontium bicarbonate.
5. The chemical coolant for aerosol fire extinguishing agent according to claim 1, characterized in that: The binder is any one of ethyl cellulose, phenolic resin, epoxy resin, hydroxypropyl methyl cellulose, polyvinyl alcohol or dextrin.
6. A method for preparing a chemical coolant for an aerosol fire extinguishing agent comprising any one of claims 1 to 5, characterized in that: The following steps are involved: (1) weighing an organic flame retardant, a metal inorganic salt, and a binder, sieving and mixing them multiple times to obtain a mixture; (2) adding anhydrous methanol to the mixture and mixing to obtain a wet material; (3) sieving the wet material into granules, and then drying and sieving it again to obtain coolant granules; (4) The coolant particles are pressed to obtain a coolant product.
7. The preparation method according to claim 6, characterized in that: The sieve described in step (1) is 100 mesh, and the sieving times is 3-5 times.
8. The preparation method according to claim 6, characterized in that: The mass of the anhydrous methanol described in step (2) accounts for 10-20% of the mass of the mixture.
9. The preparation method according to claim 6, characterized in that: The sieve described in step (3) is 20 mesh, and the drying condition is drying at 55-65° C. for 12-24 hours until the volatile content is less than 1%.
10. The preparation method according to claim 6, characterized in that: The pressing condition in step (4) is 10 MPa, and the diameter of the finished coolant is 6 mm and the height is 5.5 mm.
Citation Information
Patent Citations
Novel anti-aging aerogel generating agent and preparation process thereof
CN101745195A
Preparation method of self-temperature sensing type fire extinguishing patch and self-temperature sensing type fire extinguishing patch prepared by reparation method
CN108992831A
Self-temperature-sensing fire extinguishing patch and preparation method thereof
CN113426060A
Chemical coolant for aerosol fire extinguishing agent and preparation method thereof
CN116570874A
Preparation of Fire-Extinguishing Material
GB1190132A
Cited By
Lithium ion battery fire extinguishing agent and preparation process
CN120420635A