Method for repairing junction
The semiconductor wafer bonding repair method addresses unbonded areas by using a laser beam to restore bonds, ensuring effective bonding and preventing damage, thus overcoming issues of inadequate irradiation and pressure in the bonding process.
Patent Information
- Application Number
- PCT/JP2024/016927
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-15
- Filing Date
- 2024-05-07
- Publication Date
- 2024-11-21
AI Technical Summary
In semiconductor wafer bonding processes, unbonded portions occur due to inadequate laser light irradiation and pressure issues, leading to wasted parts and adverse effects like flapping and peeling during subsequent processing steps.
A bonding repair method using a laser beam to specifically target and repair unbonded areas, limiting heat and light exposure to prevent further damage and ensure a strong bond between semiconductor wafers.
This method effectively forms a good bonded state between semiconductor wafers by repairing unbonded portions with precise laser irradiation, preventing heat and light-related adverse effects and ensuring proper bonding even in areas initially missed by the bonding process.
Smart Images

Figure JP2024016927_21112024_PF_FP_ABST
Abstract
Description
Joint repair method
[0001] The present invention relates to a joining technique using laser light.
[0002] There are semiconductor device manufacturing technologies that include a process for bonding two semiconductor wafers (hereinafter referred to as a "bonding process"). For example, Patent Document 1 describes a technology in which two semiconductor wafers are stacked one on top of the other, and pressure is applied from the back side of one wafer using gas or liquid while the back side of the other wafer receives pressure to sandwich the two semiconductor wafers, and in this state, laser light is irradiated onto the opposing surfaces of the semiconductor wafers to bond them together.
[0003] In recent years, such bonding processes have been used in semiconductor device manufacturing technology when sealing sensors (acceleration sensors, gyro sensors, etc.) and micromachines (actuators, etc.) within devices, and when manufacturing semiconductor devices with a three-dimensional structure in which chips are stacked.
[0004] Patent Application No. 2022-92779
[0005] On the other hand, in the above-mentioned bonding process, as described in Patent Document 1, a holding part may be required to hold the semiconductor wafers when the overlapping semiconductor wafers are clamped. In this case, the portion of the semiconductor wafer held by the holding part cannot be irradiated with laser light even if bonding is required at that portion, and that portion remains unbonded. If such an unbonded portion occurs, the portion may be wasted or may have adverse effects on processing and equipment in subsequent processes (such as a cutting process) (adverse effects due to flapping or peeling of the semiconductor wafer).
[0006] Furthermore, even if it is possible to irradiate the portion held by the holding part with laser light in some way, in the previous process (the process of clamping the semiconductor wafer), it may not be possible to apply appropriate pressure to the portion held by the holding part, resulting in a poor bond and an unbonded portion. This problem can also occur when the entire semiconductor wafer is heated and bonded while being clamped. Specifically, when a holding part such as the one described above is required, the same problem can occur in the portion held by the holding part, even if bonding is required at that portion, because the pressure required for clamping is insufficient.
[0007] Therefore, an object of the present invention is to provide a technology that enables a good bond to be formed between objects to be bonded, such as semiconductor wafers, even if unbonded portions may occur during a bonding process of the objects to be bonded.
[0008] The bond repair method of the present invention repairs the bonded state at an unjoined portion by irradiating a laser beam onto the unjoined portion when an unjoined portion occurs in at least a part of the joint target portion during a joining process in which two objects to be joined are joined at a joint target portion set on the opposing surfaces of the two objects.
[0009] According to the above-described bond repair method, the use of laser light makes it possible to limit the heated area to the unbonded portion, and as a result, it is possible to repair the bonded state of the unbonded portion while preventing the adverse effects of heat and light from reaching portions other than the unbonded portion.
[0010] According to the present invention, even if an unbonded portion may occur in the bonding process, it is possible to form a good bonded state between the objects to be bonded.
[0011] FIG. 1(A) is a cross-sectional view conceptually illustrating an example of two objects to be joined in a joining process, and FIG. 1(B) is a plan view illustrating the two objects to be joined, excluding one of the objects to be joined. FIGS. 2(A) and 2(B) are conceptual diagrams illustrating an example of a joining device used in the joining process, with FIG. 2(A) illustrating a state in which a second stage is raised, and FIG. 2(B) illustrating a state in which the second stage is lowered. FIG. 3 is a conceptual diagram illustrating a state in which an unjoined portion occurs in a joining target portion. FIG. 4(A) is a conceptual diagram illustrating an example of a bond repair device used in a bond repair method according to an embodiment, and FIG. 4(B) is a plan view illustrating an example of a first support unit used in the embodiment. FIG. 5(A) is a plan view conceptually illustrating an arrangement of the objects to be joined on a support mechanism provided in the bond repair device, and FIG. 5(B) is a plan view conceptually illustrating an arrangement of the objects to be joined when the objects to be joined are rotated in a circumferential direction. 6A and 6B are conceptual diagrams respectively showing a detour portion and a linear portion that are reset as welding targets to avoid inclusions.
[0012] [1] Bonding Process [1-1] Bonding Objects Figures 1(A) and 1(B) are a cross-sectional view and a plan view conceptually illustrating an example of two bonding objects 101 and 102 to be bonded in a bonding process. The bonding objects 101 and 102 are base materials composed of substrates such as semiconductor wafers. Note that Figure 1(A) is a cross-sectional view taken along line IA-IA shown in Figure 1(B). Also, Figure 1(B) is a plan view showing one of the two bonding objects 101 and 102, the bonding object 102, excluding the other.
[0013] In the examples of FIGS. 1A and 1B, the joining target 101 includes a plurality of device regions Rd that are to be separated by cutting along cutting lines Ct. Each device region Rd becomes a base portion of a device after being separated. Each device region Rd is provided with a recess 103 that forms a cavity within the device. Here, the cavity is an enclosed space for sealing an element 104 that performs the function of the device. The element 104 is a sensor (such as an acceleration sensor or a gyro sensor), a micromachine (such as an actuator), an electronic circuit, etc.
[0014] After the elements 104 are placed in the recesses 103 of each device region Rd in the bonding object 101, the bonding object 102 is bonded to the bonding object 101 in a state in which all of the recesses 103 are blocked. As a result, cavities are formed in each device region Rd, and the elements 104 are sealed in the cavities. Furthermore, the bonding object 102 becomes a lid portion of the device when the bonding object 101 is cut along the cutting line Ct and separated into individual pieces together with the bonding object 101.
[0015] 1A, the bonding of the bonding objects 101 and 102 is performed at a bonding target portion Pt set in their opposing surfaces 101a and 102a. In the example of FIG. 1B, in order to bond the entire periphery of the recess 103 in each device region Rd, a rectangular linear portion Pt1 for bonding the periphery of the recess 103 along the cutting line Ct is set as the bonding target portion Pt. The bonding at this linear portion Pt1 is necessary to maintain the cavity as an airtight space in each device obtained by the singulation, even after the device is singulated by cutting along the cutting line Ct.
[0016] 1(B) , an annular linear portion Pt2 for joining the entire peripheries of the objects to be joined 101 and 102 is also set as the joining target portion Pt at the peripheral portion Re of the objects to be joined 101 and 102. The joining at the linear portion Pt2 is necessary to prevent fluttering at the peripheral portion Re of the objects to be joined 101 and 102 that may occur during the cutting process (cutting at the cutting line Ct).
[0017] In the joining process, the joining target portion Pt having the above-described pattern shape is irradiated with laser light to join the two objects to be joined 101 and 102. Specifically, the joining process is performed using a joining device as described below.
[0018] The shapes of the objects to be joined 101 and 102 and the pattern shape of the joining target portion Pt are not limited to those described above, and can be changed as appropriate depending on the shape and size of the device to be manufactured, the joining position, line, area, etc. Furthermore, the joining of the objects to be joined 101 and 102 is not limited to being performed by irradiating the joining target portion Pt with laser light, and may be changed as appropriate to being performed by heating the entire objects to be joined 101 and 102, with a pressurized area for the objects to be joined 101 and 102 as the joining target portion Pt.
[0019] [1-2] Bonding Apparatus Fig. 2(A) is a conceptual diagram showing an example of a bonding apparatus used in the bonding process. In the example of Fig. 2(A), the bonding apparatus includes a chamber mechanism 1, a sealing mechanism 2, a pressure mechanism 3, a laser light source 4, and a control unit 5. The configuration of each unit will be specifically described below.
[0020] <Chamber Mechanism 1> The chamber mechanism 1 has a first chamber component 11, a second chamber component 12, and a drive unit 13 that drives at least one of these components.
[0021] The first chamber component 11 and the second chamber component 12 are components that form an enclosed space (hereinafter referred to as "chamber 10") for carrying out the bonding process, and are configured so that the chamber 10 can be selectively formed or opened by moving the chamber 11 and the second chamber component 12 relatively close to or farther apart in the vertical direction. More specifically, this is as follows.
[0022] The first chamber component 11 is composed of a first cylindrical portion 111 and a first stage 112 that is supported tightly inside the first cylindrical portion 111. The first cylindrical portion 111 is disposed with its central axis aligned with the vertical direction, and the first stage 112 is supported horizontally by the first cylindrical portion 111. The first stage 112 is a stage that is transparent to laser light and is made of, for example, quartz.
[0023] The second chamber component 12 is composed of a second cylindrical portion 121 disposed above the first cylindrical portion 111 and coaxial with the first cylindrical portion 111, a second stage 122 supported inside the second cylindrical portion 121 with no gap between them so as to be movable up and down, and a drive unit 123 that moves the second stage 122 up and down. The upper end of the first cylindrical portion 111 and the lower end of the second cylindrical portion 121 are in contact with each other with no gap between them, thereby forming a chamber 10 between the first stage 112 and the second stage 122 as shown in Figures 2(A) and 2(B). Note that Figure 2(A) shows a state in which the second stage 122 is raised, and Figure 2(B) shows a state in which the second stage 122 is lowered.
[0024] 2(B) , by lowering the second stage 122 to bring it into surface contact with the back surface 102b of the objects to be bonded 102, when pressure is applied to the back surface 101b of the objects to be bonded 101 from the first stage 112 side (the lower side in the example of FIG. 2(B) ) by the pressure mechanism 3 described below, the pressure can be received on the back surface 102b side (the upper side in the example of FIG. 2(B) ) of the objects to be bonded 102. In this way, in this bonding apparatus, the second stage 122 can function as a support part that receives pressure on the back surface 102b side of the objects to be bonded 102.
[0025] The drive unit 13 is a part that moves at least one of the first chamber component 11 and the second chamber component 12 in the vertical direction, thereby moving these components relatively closer to or farther apart.
[0026] <Sealing mechanism 2> The sealing mechanism 2 is a mechanism that divides the space within the chamber 10 into a plurality of regions (hereinafter referred to as "chamber regions") and seals between adjacent chamber regions (see FIG. 2(B)). Specifically, the sealing mechanism 2 divides the space within the chamber 10 into a first chamber region R1 facing the back surface 101b of the object to be joined 101 and a second chamber region R2 adjacent to the first chamber region R1, and seals between these chamber regions. More specifically, it works as follows.
[0027] The sealing mechanism 2 is composed of a flange 21 and a retaining portion 22. Here, the flange 21 is an annular portion that protrudes from a position on the inner surface of the first cylindrical portion 111 that is higher than the first stage 112 (i.e., a position closer to the second cylindrical portion 121) toward the central axis of the first cylindrical portion 111, and extends to a position where it can face peripheral portions Re of the objects to be joined 101 and 102 when the objects to be joined 101 and 102 are placed in the chamber 10. The retaining portion 22 is composed of an annular sealing member (such as an O-ring), and is installed on the upper surface of the tip of the flange 21 so as to be able to support the peripheral portions Re of the objects to be joined 101 and 102 over the entire circumference when the objects to be joined 101 and 102 are placed in the chamber 10.
[0028] According to such a sealing mechanism 2, when the second stage 122 descends and comes into contact with the back surface 102b of the workpieces 102, the entire periphery Re of the workpieces 101 and 102 is sandwiched between the second stage 122 and the holder 22. As a result, as shown in Fig. 2(B) , the space within the chamber 10 is divided into a first chamber region R1 and a second chamber region R2, and the space between these chamber regions is sealed.
[0029] <Pressure Mechanism 3> The pressure mechanism 3 is a mechanism that applies pressure to the back surface 101b of the object to be joined 101 by increasing the internal pressure of the first chamber region R1. Specifically, the pressure mechanism 3 is a mechanism that uses a gas or a liquid as a pressure transmission medium 30, and applies pressure to the back surface 101b of the object to be joined 101 while the pressure transmission medium 30 is in contact with the back surface 101b. More specifically, it is as follows.
[0030] The pressurizing mechanism 3 can adjust the internal pressure for each chamber region formed by dividing the chamber 10 with the sealing mechanism 2, can reduce the pressure in each chamber region, and can also pressurize the first chamber region R1 using a pressure transmission medium 30. Pressurization of the first chamber region R1 is achieved by supplying the pressure transmission medium 30 (gas or liquid) to the first chamber region R1 using, for example, a compression pump. The pressurizing mechanism 3 then makes the internal pressure of the first chamber region R1 higher than the internal pressure of the second chamber region R2, and utilizes the difference between the internal pressures to apply pressure to the back surface 101b of the object to be joined 101.
[0031] <Laser light source 4> The laser light source 4 is a part that emits laser light, and is disposed below the first stage 112 that is transparent to laser light. The laser light source 4 is capable of scanning the laser light in a horizontal plane along the pattern shape of the welding target portion Pt while irradiating the welding objects 101 and 102 with laser light via the first stage 112. Furthermore, the laser light source 4 is capable of focusing the laser light on the welding location (position of the welding target portion Pt) of the welding objects 101 and 102.
[0032] <Controller 5> The controller 5 is composed of a processing device such as a CPU or a microcomputer, and controls various operating parts (such as the chamber mechanism 1, the pressurizing mechanism 3, and the laser light source 4) of the bonding apparatus. Specifically, the controller 5 performs control along the following flow to carry out the bonding process.
[0033] The control unit 5 first brings the first chamber component 11 and the second chamber component 12 close to each other and combines them to form the chamber 10 (see FIG. 2A). Here, the objects to be joined 101 and 102 are placed on the holder 22 before the chamber 10 is formed.
[0034] Next, the control unit 5 controls the pressurizing mechanism 3 to reduce the internal pressure of the entire chamber 10 until the chamber 10 is in a vacuum state. At this time, the peripheral portions Re of the objects to be bonded 101 and 102 are not yet sandwiched between the second stage 122 and the holder 22, and are therefore free from the seal. This allows the gas present between the objects to be bonded 101 and 102 to flow out (into the chamber 10) through the gap between the objects to be bonded 101 and 102. This also reduces the internal pressure between the objects to be bonded 101 and 102.
[0035] Thereafter, the control unit 5 lowers the second stage 122 to contact the back surface 102b of the objects to be joined 102, thereby sandwiching the entire periphery Re of the objects to be joined 101 and 102 between the second stage 122 and the holding unit 22 (see FIG. 2B ). As a result, a first chamber region R1 and a second chamber region R2 are formed, and the space between them is sealed.
[0036] In this state, the control unit 5 controls the pressurizing mechanism 3 to increase the internal pressure of the first chamber region R1 while maintaining the second chamber region R2 in a vacuum state. As a result, the internal pressure of the first chamber region R1 becomes higher than the internal pressure of the second chamber region R2, and a pressure corresponding to the difference between the internal pressures is applied to the back surface 101b of the workpieces 101. As a result, the workpieces 101 and 102 are sandwiched between the pressure transmission medium 30 and the second stage 122 (pressurizing step). At this time, by changing the internal pressure of the first chamber region R1, the pressure applied to the back surface 101b of the workpieces 101 can be changed to a desired value. The internal pressure of the first chamber region R1 may be set to a value lower than atmospheric pressure, approximately the same as atmospheric pressure, or higher than atmospheric pressure, as long as it is higher than the internal pressure of the second chamber region R2.
[0037] After the pressure mechanism 3 applies pressure to the rear surface 101b of the objects to be joined 101, the control unit 5 maintains this state and controls the laser light source 4 to irradiate the welding target portions Pt of the objects to be joined 101 and 102 with laser light. At this time, the control unit 5 scans the laser light in a horizontal plane along the pattern shape of the welding target portions Pt. In this way, the welding process for joining the two objects to be joined 101 and 102 is executed by the joining device.
[0038] The above-mentioned joining device is not limited to a device that joins the joining objects 101 and 102 by irradiating laser light onto a joining target portion Pt having a pattern shape, but may be appropriately modified to a device that joins the joining objects 101 and 102 by heating the entire joining objects 101 and 102, with the pressure application area for the joining objects 101 and 102 as the joining target portion Pt.
[0039] [1-3] Occurrence of Unbonded Portion In the above-described bonding apparatus, when the bonding process is performed, the entire periphery Re of the bonding objects 101 and 102 is sandwiched between the second stage 122 and the holding portion 22 (see FIGS. 1(B) and 2(B)). Therefore, as shown in FIG. 3, when the laser beam is irradiated onto the bonding target portion Pt, the presence of the sealing mechanism 2 including the holding portion 22 prevents the laser beam from being irradiated onto the portion of the bonding target portion Pt that is set on the periphery Re (the annular linear portion Pt2). As a result, this portion becomes an unbonded portion Pu. If such an unbonded portion Pu occurs, it becomes impossible to prevent fluttering at the periphery Re of the bonding objects 101 and 102 that may occur during the cutting process (cutting along the cutting line Ct).
[0040] Furthermore, not only when the joining process is performed using the above-described joining device, but also when two joining objects 101 and 102 are clamped while overlapping each other, if a holding part for holding the joining objects 101 and 102 is required, a part of the joining target portion Pt may be hidden by the holding part (and the mechanism including it). In that case, the laser light cannot be irradiated onto the part of the joining target portion Pt that is hidden by the holding part, and this part becomes an unjoined portion Pu. When such an unjoined portion Pu occurs, not only the above-described fluttering problem but also problems such as the part where the unjoined portion Pu occurs being wasted and adverse effects (such as peeling) on processing and the equipment in subsequent steps may occur.
[0041] Furthermore, even if it were possible to irradiate the laser light to the portion of the welding target portion Pt that is hidden by the holding portion (and the mechanism including it) in some way, in the previous process (the process of clamping the welding objects 101 and 102), it would be impossible to apply appropriate pressure to the portion held by the holding portion, which could result in a poor welding at that portion, turning it into an unwelded portion Pu. This problem can also occur when the welding objects 101 and 102 are clamped and then heated as a whole to be welded, if a holding portion such as the one described above is required, because the pressure required for clamping will be insufficient at the portion held by the holding portion.
[0042] Therefore, even when an unbonded portion Pu may occur in the bonding process, in order to enable a good bonded state to be formed between the objects to be bonded 101 and 102, the present inventors propose a bond repair method for repairing the bonded state at the unbonded portion Pu by irradiating the unbonded portion Pu with laser light. The bond repair method will be specifically described below.
[0043] In addition to the reasons mentioned above, other possible reasons for the occurrence of the unbonded portion Pu include a foreign object being caught between the two objects to be bonded 101 and 102, preventing the objects to be bonded 101 and 102 from coming into close contact with each other, or a temporary insufficient output of the laser light source 4, resulting in an insufficient power of the laser light required for bonding. A bond repair method for repairing the bonded state of the unbonded portion Pu caused by these reasons will be described in a second modified example below.
[0044] [2] Bond Repair Method The bond repair method according to the embodiment can be performed using the following bond repair device.
[0045] 4A is a conceptual diagram showing an example of a bond repair device. The bond repair device includes a support mechanism 6, a laser light source 7, and a control unit 8.
[0046] The support mechanism 6 is a mechanism including a first support part 61 and a second support part 62, and supports the objects to be joined 101 and 102 after the above-described joining step has been performed by sandwiching them from the back surface 101b and 102b sides between the first support part 61 and the second support part 62. The support mechanism 6 may be provided with a pressurizing function for sandwiching and pressing the objects to be joined 101 and 102 while supporting them with the first support part 61 and the second support part 62.
[0047] In this embodiment, the first support portion 61 is arranged so as to be located on the laser light incident side (on the back surface 101b side of the object to be joined 101 in the example of FIG. 4A ) with respect to the objects to be joined 101 and 102. A support portion having a window 61w formed therein for passing the laser light from the laser light source 7 is used as the first support portion 61. Specifically, the window 61w is formed in the first support portion 61 so that at least a part of the unjoined portion Pu can be seen through the window 61w when the objects to be joined 101 and 102 are sandwiched between the first support portion 61 and the second support portion 62.
[0048] Fig. 4(B) is a plan view showing an example of the first support portion 61 used in the embodiment. Here, Fig. 4(B) shows the first support portion 61 that can be used to repair the joined state of the unjoined portion Pu when the annular linear portion Pt2 of the weld target portion Pt shown in Fig. 1(B) becomes an unjoined portion Pu (in other words, when the unjoined portion Pu occurs on the peripheral portions Re of the two objects to be welded 101 and 102).
[0049] Specifically, the first support portion 61 is composed of a main body portion 611, an annular portion 612, and a beam portion 613. Here, the main body portion 611 is a portion that contacts a central region of the back surface 101b of the joining object 101 that is inside the peripheral edge portion Re (see FIG. 4A). The annular portion 612 is a portion that contacts an annular region of the back surface 101b of the joining object 101 that includes the outer periphery and is narrower than the peripheral edge portion Re (see FIG. 4A). The beam portion 613 is a portion that connects the annular portion 612 to the main body portion 611 at at least one location (see FIG. 4B). The region surrounded by the main body portion 611, the annular portion 612, and the beam portion 613 forms a window 61w of the first support portion 61. 4(B) shows the first support portion 61 in which an annular portion 612 is connected to a main body portion 611 at four locations by four beam portions 613 that are equally spaced around the center point of the first support portion 61, resulting in the formation of four windows 61w. Note that the configuration of the first support portion 61 (the shape and number of the windows 61w, etc.) is not limited to that shown in FIG. 4(B) and can be changed as appropriate to suit the shape of the unwelded portion Pu generated in the weld target portion Pt, etc.
[0050] The laser light source 7 is a part that emits laser light, and is capable of irradiating the laser light through a window 61w of the first support part 61 toward the objects to be joined 101 and 102 supported by the support mechanism 6. Specifically, the laser light source 7 is capable of irradiating the laser light through the window 61w of the first support part 61 onto the unjoined portion Pu visible through the window 61w. The laser light source 7 is also capable of scanning the laser light in a horizontal plane along the pattern shape of the unjoined portion Pu (here, the pattern shape of the annular linear portion Pt2). Furthermore, the laser light source 4 is capable of focusing the laser light on the joining location (the position of the unjoined portion Pu) of the objects to be joined 101 and 102.
[0051] The control unit 8 is configured with a processing device such as a CPU or a microcomputer, and controls various operating units (such as the support mechanism 6 and the laser light source 7) included in the bond repair device. Specifically, the bond repair method is carried out by the control unit 8 performing control along the following flow.
[0052] The control unit 8 first supports the objects to be joined 101 and 102 with the support mechanism 6 (support step; see FIG. 4A ). At this time, the objects to be joined 101 and 102 are positioned so that at least a part of the unjoined portion Pu is visible through the window 61w of the first support part 61, as shown in FIG. 5A . At this time, the control unit 8 may control the support mechanism 6 to clamp the objects to be joined 101 and 102 with the first support part 61 and the second support part 62.
[0053] Thereafter, the control unit 8 controls the laser light source 7 to irradiate the unbonded portion Pu visible through the window 61w of the first support portion 61 with laser light (repair step). At this time, the control unit 8 scans the laser light in a horizontal plane along the pattern shape of the unbonded portion Pu (here, the pattern shape of the annular linear portion Pt2). This repairs the bonded state of the portion of the unbonded portion Pu visible through the window 61w of the first support portion 61. In this way, the bond repair method for repairing the bonded state of the unbonded portion Pu is executed by the bond repair device.
[0054] According to this type of bond repair method, the heating area can be limited to the unbonded portion Pu by using laser light, and as a result, the bonded state of the unbonded portion Pu can be repaired while preventing the adverse effects of heat and light from reaching portions other than the unbonded portion Pu.
[0055] Furthermore, according to the first support portion 61, the periphery of the unbonded portion Pu seen through the window 61w can be supported by the edge of the window 61w (the main body portion 611, the annular portion 612, and the beam portion 613), thereby increasing the degree of adhesion between the two objects to be bonded 101 and 102 at the unbonded portion Pu. Therefore, by irradiating the unbonded portion Pu seen through the window 61w with laser light, it is possible to repair the bonded state of the unbonded portion Pu to a good one.
[0056] [3] Modified Examples [3-1] First Modified Example In the repair step of the above-described bond repair method, laser light can be irradiated onto the portion of the unbonded portion Pu that is visible through the window 61w of the first support portion 61, but on the other hand, laser light cannot be irradiated onto the portion of the unbonded portion Pu that is hidden by the beam portion 613, and the bonded state of that portion cannot be repaired (see Figure 5 (A)).
[0057] Therefore, after the repair step is performed, the objects 101 and 102 to be joined may be rearranged by rotating them in the circumferential direction so that the portion of the unjoined portion Pu that was hidden by the beam portion 613 is visible through the window 61w, as shown in Fig. 5(B) . Note that in Fig. 5(B) , the repaired portion of the unjoined portion Pu is indicated by a thick solid line. Then, the above-described repair step may be performed again on the portion of the unjoined portion Pu that was hidden by the beam portion 613.
[0058] According to this bond repair method, even if the bonded state of all portions of the unbonded portion Pu cannot be repaired by a single repair step, it is possible to repair the bonded state of all portions of the unbonded portion Pu by rearranging the objects to be bonded 101 and 102 and performing the repair step again. Furthermore, such re-execution of the repair step can be repeated by rearranging the objects to be bonded 101 and 102 each time until the bonded state of all portions of the unbonded portion Pu can be repaired.
[0059] In addition, the joint repair method of this modified example may be appropriately modified so that, instead of rotating the objects to be joined 101 and 102 circumferentially and repositioning them, the first support portion 61 of the joint repair device is rotated circumferentially (in other words, the objects to be joined 101 and 102 are rotated circumferentially relative to the first support portion 61), so that the portion of the unjoined portion Pu that was hidden by the beam portion 613 can be seen through the window 61w.
[0060] [3-2] Second Modification As described above, possible reasons for the occurrence of the unwelded portion Pu include a foreign object being caught between the two objects to be welded 101 and 102, preventing the objects to be welded 101 and 102 from coming into close contact with each other, or a temporary shortage of the power of the laser light required for welding due to an insufficient output from the laser light source 4. Meanwhile, with regard to the unwelded portion Pu that may occur for these reasons, unlike the case of the above-described embodiment (i.e., the case where it is clear that the portion of the weld target portion Pt that is held by the holding portion will become the unwelded portion Pu), at the time the welding process is completed, it is unclear whether or not the unwelded portion Pu has actually occurred, and even if the unwelded portion Pu has occurred, it is unclear where the unwelded portion Pu has occurred.
[0061] Therefore, even if an unbonded portion Pu may occur for these reasons, the inventor further proposes the following bond repair method to enable the formation of a good bonded state between the objects to be bonded 101 and 102.
[0062] First, the welding state of the welding target portion Pt after the welding process is inspected to identify an unwelded portion Pu occurring in the welding target portion Pt (identification step). Next, the unwelded portion Pu identified in the identification step is irradiated with a laser beam to repair the welding state of the unwelded portion Pu (repair step).
[0063] As a specific example, consider the case where a joining process is performed using the joining device shown in Figure 2 (A), and an unjoined portion Pu occurs in an area where pressure can be applied by the pressure transmission medium 30 (an area where laser light can be irradiated; in other words, an area other than the part where laser light irradiation is prevented by the presence of the sealing mechanism 2 including the holding portion 22).
[0064] First, consider a case where the cause of the unbonded portion Pu is insufficient power of the laser beam. In this case, after the unbonded portion Pu is identified in the identification step, the objects to be bonded 101 and 102 are clamped and pressed together using the bonding device (see FIG. 2A ) used in the bonding process again (pressure step), and then, in the repair step, the unbonded portion Pu is irradiated with laser light in a state where the insufficient power of the laser beam has been resolved, thereby repairing the bonded state of the unbonded portion Pu.
[0065] Next, consider a case where the unwelded portion Pu is caused by a foreign object (inclusion) sandwiched between the objects to be welded 101 and 102. In this case, after the welding process is performed, a bulge with its apex located at the position of the inclusion occurs on the back surface 102b of the object to be welded 102. By observing the back surface 102b of the object to be welded 102 with a camera, such a bulge can be observed as an interference fringe. Therefore, in the identification step, by observing the back surface 102b of the object to be welded 102 with a camera, a portion of the welding target portion Pt that overlaps with the interference fringe observed by the camera can be identified as the unwelded portion Pu. Furthermore, the center position of the interference fringe can be identified as the position of the inclusion.
[0066] In this case, too, the bonding state of the unbonded portion Pu can be repaired by reusing the bonding device (see FIG. 2(A)) used in the bonding process. However, since the unbonded portion Pu is caused by an inclusion, it cannot be removed, and therefore the bulge with the inclusion as its apex cannot be eliminated. Furthermore, if an inclusion is located on the unbonded portion Pu, it is difficult to improve the bonding state of the unbonded portion Pu even if a laser beam is directly irradiated onto the unbonded portion Pu caused by the inclusion.
[0067] Therefore, before the repair step is performed, a pressure greater than the pressure applied to the back surface 101b of the objects 101 when the objects 101 and 102 are clamped in the joining process is applied by the pressure transmission medium 30 (pressure step). This shrinks the bulge as much as possible, and the contact area between the objects 101 and 102 around the inclusion can be increased.
[0068] Then, in the repair step, the bulge is kept in a state of being shrunk as much as possible by the pressurizing step, and the laser light is irradiated while avoiding the location of the inclusion identified in the identification step, thereby repairing the bonded state at the unbonded portion Pu.
[0069] Here, if the inclusion is located at a position shifted from the unjoined portion Pu, the bulge can be made as small as possible in the above-mentioned pressure application step to reduce the influence of the inclusion, and then the unjoined portion Pu can be repaired by irradiating the laser light directly onto the unjoined portion Pu.
[0070] On the other hand, if an inclusion is located on the unwelded portion Pu, the laser beam is irradiated at a position shifted from the unwelded portion Pu to avoid the position of the inclusion, thereby complementing the repair of the welded state at the shifted position. As an example, as shown in FIG. 6A , a detour portion Pt3 that bypasses the position of the inclusion is reset as the weld target portion Pt, and the laser beam is irradiated to the detour portion Pt3, thereby complementing the repair of the welded state at the unwelded portion Pu. Note that in FIG. 6A , the portion of the weld target portion Pt that has been welded is indicated by a thick solid line (the same applies to FIG. 6B ). As another example, as shown in FIG. 6B , another linear portion Pt4 is reset as the weld target portion Pt along a portion of the weld target portion Pt that includes the unwelded portion Pu (including a portion that has already been welded), and the linear portion Pt4 is irradiated with the laser beam, thereby complementing the repair of the welded state at the unwelded portion Pu (see FIG. 6B ).
[0071] The irradiation of laser light onto the unjoined portion Pu in the repair step includes not only cases where laser light is irradiated directly onto the unjoined portion Pu to repair the joined state of the unjoined portion Pu, but also cases where it is necessary to avoid inclusions even when laser light is not irradiated directly onto the unjoined portion Pu, and the repair of the joined state at the unjoined portion Pu can be complemented by irradiating laser light at a position shifted from the unjoined portion Pu to avoid the inclusions.
[0072] [3-3] Third Modification Example When the cause of the unbonded portion Pu is a foreign object (inclusion) sandwiched between the objects to be bonded 101 and 102, the method for repairing the bonded state at the unbonded portion Pu in the above-described second modification example involves performing a pressurizing step before performing the repair step, thereby shrinking the bulge caused by the inclusion as much as possible and increasing the contact area between the objects to be bonded 101 and 102 around the inclusion. However, instead of or in parallel with the pressurizing step, a pre-processing step such as the one described below may be performed.
[0073] Specifically, before the repair step is performed, the inclusion at the position identified in the identification step is irradiated with a pretreatment laser beam to heat and deform the inclusion, or to sublimate the inclusion by a phenomenon such as ablation (pretreatment step). This reduces the height of the bulge, and as a result, increases the contact area between the objects to be welded 101 and 102 around the inclusion.
[0074] Furthermore, when the inclusions are heated and deformed with laser light in the pretreatment step, a pressure application step can be performed in parallel, so that the heated inclusions can be pressed with pressure and deformed efficiently, thereby reducing the height of the bulge.
[0075] Furthermore, when the inclusions are sublimated by laser light in the pretreatment step, the pressurization step can be performed in parallel to the pretreatment step, so that the gas generated by the sublimation can be pushed out into the cavity by pressure, and as a result, the bulge can be eliminated. If the bulge can be eliminated, it becomes possible to irradiate the unbonded portion Pu with laser light directly without avoiding the inclusions in the repair step.
[0076] The above-described embodiments and modifications should be considered to be illustrative in all respects and not restrictive. The scope of the present invention is defined not by the above-described embodiments and modifications, but by the claims. Furthermore, the scope of the present invention is intended to include all modifications that are equivalent to the scope of the claims and fall within the scope thereof.
[0077] Furthermore, from the above-described embodiments and modifications, each step constituting the bond repair method may be extracted individually as a subject of the invention, or a bond repair device used in the bond repair method or each part of the bond repair device (such as the first support part 61) may be extracted individually. Furthermore, a combination of these with a part of a bonding process or a bonding device may be extracted as a subject of the invention.
[0078] REFERENCE SIGNS LIST 1 chamber mechanism 2 sealing mechanism 3 pressure mechanism 4 laser light source 5 control unit 6 support mechanism 7 laser light source 8 control unit 10 chamber 11 first chamber component 12 second chamber component 13 drive unit 21 flange 22 holding unit 30 pressure transmission medium 61 first support unit 61w window 62 second support unit Ct cutting line Pt joining target unit Pu unjoined unit R1 first chamber region R2 second chamber region Rd device region Re peripheral portion 101, 102 joining object 101a, 102a opposing surface 101b, 102b rear surface 103 recess 104 element 111 first cylindrical portion 112 first stage 121 second cylindrical portion 122 second stage 123 drive unit 611 main body portion 612 Annular portion 613 Beam portion Pt1, Pt2, Pt4 Linear portion Pt3 Detour portion
Claims
1. A method for repairing a joint, in which when an unjoined portion occurs in at least a part of a joining target portion during a joining process in which two objects to be joined are joined at a joining target portion set on the opposing surfaces of the objects, the method repairs the joint state at the unjoined portion by irradiating the unjoined portion with laser light.
2. A bond repair method as described in claim 1, comprising: a supporting step of supporting the two objects to be joined by sandwiching them from their back sides with a first supporting part and a second supporting part, using as the first supporting part a supporting part that allows at least a part of the unjoined part to be seen through a window for passing laser light; and a repair step of repairing the bonded state of the unjoined part by irradiating the unjoined part with laser light through the window after the supporting step.
3. A joint repair method as described in claim 2, in which, when the unjoined portion occurs on the peripheral portions of the two objects to be joined, the first support portion is a support portion that includes a main body portion in contact with a central region of the back surface that is inside the peripheral portion, an annular portion in contact with an annular region along the outer periphery of the back surface, and a beam portion connecting the annular portion to the main body portion, and the area surrounded by these forms the window.
4. A joint repair method as described in claim 3, wherein after the repair step is performed, the two objects to be joined are rotated circumferentially relative to the first support portion, thereby exposing a portion of the unjoined portion that was hidden by the beam portion through the window, and then the repair step is performed again on that portion.
5. A bonding repair method as described in claim 1, comprising: a pressurizing step of applying pressure to the back surface of one of the two objects to be joined while a pressure transmission medium, gas or liquid, is in direct contact with the back surface of the other object to be joined, and receiving the pressure by a support part on the back surface side of the other object to be joined, thereby clamping the two objects to be joined; and a repair step of repairing the bonded state of the unjoined portion by irradiating the unjoined portion from the back surface side of one of the objects to be joined with laser light while clamping the two objects to be joined by the pressurizing step.
6. A bonding repair method as described in claim 5, wherein the pressurizing step is also used in the bonding process, and in the pressurizing step performed when repairing the unbonded portion, a pressure greater than the pressure applied in the pressurizing step performed before the repair is applied to the back surface of one of the bonding objects by using a pressure transmission medium of gas or liquid.
7. A bond repair method according to any one of claims 1 to 6, comprising: an identification step of identifying the unbonded portion generated in the bond target portion by inspecting the bonded state at the bond target portion after the bonding process; and a repair step of repairing the bonded state at the unbonded portion by irradiating the unbonded portion identified in the identification step with laser light.
8. A bond repair method as described in claim 7, wherein in the identifying step, the unjoined portion is identified, and if the cause of the unjoined portion is an inclusion, the position of the inclusion is identified, and in the repair step, the bonded state of the unjoined portion is repaired by irradiating laser light while avoiding the position of the inclusion identified in the identifying step.
9. A bond repair method according to any one of claims 1 to 6, comprising: an identifying step of identifying the unbonded portion generated in the bond target portion by inspecting the bonded state at the bond target portion after the bonding process, and identifying the position of the inclusion if the cause of the unbonded portion is an inclusion; a pre-processing step of irradiating the inclusion at the position identified in the identifying step with a laser beam to deform or sublimate the inclusion; and a repair step of repairing the bonded state at the unbonded portion by irradiating the unbonded portion identified in the identifying step with a laser beam after the pre-processing step.
Citation Information
Patent Citations
Game machine
JP2022092779A
Manufacturing method of thin film device and bonding method of glass substrate
JP2005338281A
Joint device
JP2022078625A
Processing device
WO2021025119A1