Method for manufacturing optical semiconductor apparatus
By etching semiconductor layers to form grooves filled with insulating films, the method addresses the challenge of reducing electrode pad capacitance in optical semiconductor devices, achieving efficient and robust electrode formation.
Patent Information
- Application Number
- PCT/JP2025/017379
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-13
- Publication Date
- 2026-11-19
AI Technical Summary
Existing methods to reduce electrode pad capacitance in optical semiconductor devices either compromise the bonding strength and contact area of the wire or reduce the efficiency of the process flow by forming thick insulating films.
A method involving etching a semiconductor layer to form grooves filled with multiple insulating films, creating a thick insulating structure beneath the electrode pad without increasing overall film thickness, thereby reducing capacitance while maintaining process efficiency.
Reduces electrode pad capacitance effectively without compromising process efficiency, ensuring strong bonding and uniform electrode formation, and simplifying the transfer process.
Smart Images

Figure JP2025017379_19112026_PF_FP_ABST
Abstract
Description
Method for manufacturing optical semiconductor device
[0001] The present disclosure relates to a method for manufacturing an optical semiconductor device.
[0002] Electrode pads are connected to optical devices such as modulators formed on a semiconductor substrate. The capacitance of the electrode pad region is mainly determined by the thickness of the insulating film under the electrode pad and the surface area of the electrode pad. It has been proposed to reduce the capacitance by making the electrode pad mesh-shaped to reduce the surface area (for example, refer to Patent Document 1), but the contact area and bonding strength of the wire bonded to the electrode pad will decrease.
[0003] Japanese Unexamined Patent Publication No. Hei 2-181987
[0004] The capacitance can be reduced by additionally forming a thick insulating film under the electrode pad separately from the insulating film covering the optical device. However, since forming a thick insulating film takes time, there has been a problem that the efficiency of the process flow is reduced.
[0005] The present disclosure has been made to solve the above-mentioned problems, and its object is to obtain a method for manufacturing an optical semiconductor device that can reduce the capacitance of the electrode pad region without reducing the efficiency of the process flow.
[0006] A method for manufacturing an optical semiconductor device according to the present disclosure includes the steps of: forming an optical device on a semiconductor substrate; forming a semiconductor layer on a side of the optical device on the semiconductor substrate; etching the semiconductor layer to form a plurality of first grooves; forming a first insulating film to cover the optical device and fill the first grooves; exposing an upper surface of the semiconductor layer from the first insulating film; etching away the exposed semiconductor layer to form a second groove; forming a second insulating film on the first insulating film to fill the second groove; and forming an electrode pad connected to the optical device on an insulating structure constituted by the first insulating film embedded in the first groove and the second insulating film embedded in the second groove.
[0007] In this disclosure, a semiconductor layer formed on the side of an optical device is etched to form a plurality of first grooves, and these first grooves are filled with a first insulating film covering the optical device. The semiconductor layer is etched away to form second grooves, which are then filled with a second insulating film. An electrode pad is formed on this insulating structure, which is composed of the first insulating film embedded in the first grooves and the second insulating film embedded in the second grooves. This makes it possible to obtain a thick insulating structure without increasing the film thickness of the insulating film. The film deposition time for the insulating film is shortened and the amount of film deposition material is reduced, so the efficiency of the process flow is not reduced. In addition, by forming the electrode pad on a thick insulating structure, the capacitance of the electrode pad region can be reduced.
[0008] This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing a method for manufacturing an optical semiconductor device according to Embodiment 1. This is a plan view showing the electrode pads of an optical semiconductor device according to Embodiment 1. This is a plan view showing a modified example of the electrode pads of an optical semiconductor device according to Embodiment 1. This is a cross-sectional view showing an optical semiconductor device according to Comparative Example 1. This is a cross-sectional view showing an optical semiconductor device according to Comparative Example 2. This is a cross-sectional view showing an optical semiconductor device according to Embodiment 2. This is a cross-sectional view showing an optical semiconductor device according to Embodiment 3. This is a cross-sectional view showing an optical semiconductor device according to Embodiment 4. This is a cross-sectional view showing an optical semiconductor device according to Embodiment 5.
[0009] A method for manufacturing an optical semiconductor device according to an embodiment will be described with reference to the drawings. The same or corresponding components are denoted by the same reference numerals, and repetition of the description may be omitted.
[0010] Embodiment 1 Figures 1 to 7 are cross-sectional views showing a method for manufacturing an optical semiconductor device according to Embodiment 1. First, as shown in Figure 1, an optical device 2 is formed on a semiconductor substrate 1. A semiconductor layer 3 is formed on the side of the optical device 2 on the semiconductor substrate 1. The optical device 2 and the semiconductor layer 3 are etched using a resist pattern 4 formed by a transfer process as a mask.
[0011] Here, the semiconductor substrate 1 is made of n-InP. The optical device 2 has an n-InP cladding layer 5, an absorption layer 6, a p-InP cladding layer 7, and a p-InP layer 8 stacked sequentially on the semiconductor substrate 1. The absorption layer 6 is a quantum well layer made of InGaAsP or AlGaInAs. The semiconductor layer 3 has a current blocking layer 9 and a p-InP layer 8 stacked sequentially on the semiconductor substrate 1. The current blocking layer 9 is made of Fe-InP.
[0012] Next, as shown in Figure 2, the resist pattern 10 formed by the transfer process is used as a mask to etch the semiconductor layer 3 and form a plurality of first grooves 11. The first grooves 11 may be formed partway through the semiconductor substrate 1 or partway through the semiconductor layer 3. In other words, the depth of the first grooves 11 does not have to be the same as the height of the mesa structure of the optical device 2.
[0013] Next, as shown in Figure 3, the first insulating film 12 is formed by sputtering or plasma CVD to cover the optical device 2 and fill the first groove 11. The first insulating film 12 is deposited laterally on the side surface of the first groove 11. Therefore, if the width of the first groove 11 is less than or equal to twice the thickness of the first insulating film 12, the first groove 11 can be filled with the first insulating film 12. The first insulating film 12 is, for example, SiO2 to reduce capacitance. 2 This consists of the above. Furthermore, the first insulating film 12 that grows laterally from the side walls of the opposing first grooves 11 come into contact with each other and become one, eliminating the boundary between them.
[0014] Next, as shown in Figure 4, a portion of the first insulating film 12 is etched to expose the upper surface of the semiconductor layer 3 from the first insulating film 12. At this time, the upper surface of the optical device 2 is also exposed from the first insulating film 12. Next, as shown in Figure 5, the upper surface of the optical device 2 exposed from the first insulating film 12 is covered with a resist pattern 13 formed by the transfer process. In this state, the semiconductor layer 3 exposed from the first insulating film 12 is removed by dry etching or wet etching to form a second groove 14 in the first insulating film 12.
[0015] Next, as shown in Figure 6, a second insulating film 15 is formed on the first insulating film 12 by sputtering or plasma CVD to fill the second groove 14. The second insulating film 15 is deposited laterally on the side surface of the second groove 14. Therefore, if the width of the second groove 14 is less than or equal to twice the thickness of the second insulating film 15, the second groove 14 can be filled with the second insulating film 15. The second insulating film 15 is made of SiN, for example, to prevent moisture absorption. The second insulating films 15 that grow laterally from the side walls of opposing second grooves 14 come into contact with each other and become integrated, eliminating the boundary. The insulating structure 16 is formed by the first insulating film 12 embedded in the first groove 11 and the second insulating film 15 embedded in the second groove 14. For example, the thickness of the first insulating film 12 and the second insulating film 15 is about 1 μm each, while the thickness of the insulating structure 16 is 10 μm.
[0016] Next, as shown in Figure 7, a metal 17 is formed extending from the upper surface of the insulating structure 16 to the upper surface of the optical device 2, and a plating 18 is formed on top of it. The metal 17 is made of, for example, Ti. The plating 18 is made of, for example, Au. As a result, the metal 17 and plating 18 formed on the insulating structure 16 become electrode pads 19 connected to the optical device 2. After that, a bottom electrode 20 is formed on the lower surface of the semiconductor substrate 1.
[0017] Figure 8 is a plan view showing the electrode pad of the optoelectronic device according to Embodiment 1. Below the electrode pad 19, the first insulating film 12 and the second insulating film 15 of the insulating structure 16 are arranged in a stripe pattern. Figure 9 is a plan view showing a modified example of the electrode pad of the optoelectronic device according to Embodiment 1. Below the electrode pad 19, the first insulating film 12 and the second insulating film 15 of the insulating structure 16 are arranged concentrically.
[0018] Next, the effects of this embodiment will be explained in comparison with Comparative Examples 1 and 2. Figure 10 is a cross-sectional view showing an optoelectronic device according to Comparative Example 1. In Comparative Example 1, there are only thin first insulating films 12 and second insulating films 15 between the semiconductor layer 3 and the electrode pad 19. Although it is desirable to increase the thickness of the insulating film below the electrode pad 19, the thickness of the first insulating film 12 and second insulating film 15 covering the device region is determined by design constraints in the device region. Therefore, Comparative Example 1 has the problem of high capacitance.
[0019] Figure 11 is a cross-sectional view showing an optoelectronic device according to Comparative Example 2. In Comparative Example 2, a thick insulating film 21 is formed under the electrode pad 19 in a separate process from the first insulating film 12 and the second insulating film 15 that cover the optical device 2. However, forming the thick insulating film 21 takes time, which reduces the efficiency of the process flow.
[0020] In contrast, in this embodiment, a semiconductor layer 3 formed on the side of the optical device 2 is etched to form a plurality of first grooves 11, and the first grooves 11 are filled with a first insulating film 12 covering the optical device 2. The semiconductor layer 3 is etched away to form second grooves 14, which are filled with a second insulating film 15. An electrode pad 19 is formed on the insulating structure 16 composed of the first insulating film 12 embedded in the first grooves 11 and the second insulating film 15 embedded in the second grooves 14. By embedding the first insulating film 12 in the first grooves 11 and the second insulating film 15 in the second grooves 14 in this way, a thick insulating structure 16 can be obtained without increasing the film thickness of the insulating film. The film deposition time for the insulating film can be shortened, so the efficiency of the process flow does not decrease. The amount of insulating film deposition material can also be reduced. By forming the electrode pad 19 on the thick insulating structure 16, the capacitance of the electrode pad region can be reduced.
[0021] Furthermore, in Comparative Example 2, a resist thick enough to cover the thick insulating film 21 is required for patterning the electrode pad 19. However, as the thickness of the resist increases, the resolution of the transfer pattern decreases, making it impossible to expose complex patterns. The wiring connecting the electrode pad 19 and the optical device 2 drops from the electrode pad 19 to the processing groove and then rises back up to the upper surface of the optical device 2, making it difficult to find the transfer exposure conditions necessary to achieve the desired wiring width at any height. Therefore, forming a thick insulating film 21 as in Comparative Example 2 increases the difficulty of the transfer process. In contrast, in this embodiment, since the height position of the electrode pad 19 is the same as in Comparative Example 1, the film thickness can be freely set with a simple transfer process.
[0022] In addition, a process for forming the first groove 11 is performed separately from the etching process of the optical device 2. Therefore, by adjusting the depth of the first groove 11, the thickness of the insulating structure 16 beneath the electrode pad 19 can be freely set without being limited by the amount of processing of the optical device 2.
[0023] Furthermore, filling the second groove 14 with the second insulating film 15 makes the upper surface of the insulating structure 16 flat. Therefore, the process of forming the electrode pad 19 is simplified, allowing the electrode pad 19 to be formed uniformly and preventing wire breakage of the electrode pad 19. The contact area and bonding strength of the wire bonded to the electrode pad 19 can be ensured. Even if a cavity remains inside the first groove 11 or the second groove 14, capacitance can be reduced, so as long as the upper surface of the insulating structure 16 is flat, there is no problem.
[0024] Furthermore, the wafer after the wafer process is completed is cleaved into a bar, and the bars are stacked and the edges are coated. When the bars are stacked, the semiconductor layer 3 remaining between the electrode pad 19 and the optical device 2 acts as a support, so no stress is applied to the optical device 2.
[0025] Embodiment 2 Figure 12 is a cross-sectional view showing an optical semiconductor device according to Embodiment 2. In Embodiment 1, the width of the first groove 11 was twice the thickness of the first insulating film 12, but in this embodiment, the width of the first groove 11 is twice the sum of the thickness of the first insulating film 12 and the thickness of the second insulating film 15. The first insulating film 12 is formed on the side surface of the first groove 11, but it cannot completely fill the first groove 11, leaving a space. However, the second insulating film 15 formed on top of the first insulating film 12 fills that space. Therefore, if the width of the first groove 11 is twice or less the sum of the thickness of the first insulating film 12 and the thickness of the second insulating film 15, the first groove 11 can be filled with the first insulating film 12 and the second insulating film 15, making the surface of the insulating structure 16 flat. Other configurations and effects are the same as in Embodiment 1.
[0026] Embodiment 3 Figure 13 is a cross-sectional view showing an optoelectronic device according to Embodiment 3. No semiconductor layer 3 remains between the electrode pad 19 and the optical device 2. Therefore, the electrode pad 19 extends from the height of the insulating structure 16 to the upper surface of the optical device 2 without ever dropping down to the processing bottom surface, and is connected to the optical device 2. This makes it possible to reduce the capacitance from the electrode pad 19 to the optical device 2. Other configurations and effects are the same as in Embodiment 1.
[0027] Embodiment 4 Figure 14 is a cross-sectional view showing an optical semiconductor device according to Embodiment 4. While the optical device 2 in Embodiment 1 was an optical modulator, the optical device 2 in this embodiment is a distributed feedback (DFB) laser. The optical device 2 has an n-InP cladding layer 5, an active layer 22, a p-InP cladding layer 7, and a p-InP layer 8 stacked in order on a semiconductor substrate 1. A diffraction grating 23 is formed in the p-InP cladding layer 7. The active layer 22 is a quantum well layer made of AlGaInAs or InGaAsP. The diffraction grating is made of p-InGaAsP. Furthermore, while the optical device 2 in Embodiment 1 had a high mesa structure, the optical device 2 in this embodiment has an embedded structure with a current blocking layer 9 on the side of the active layer 22.
[0028] Thus, even when the optical device 2 is a directly modulated laser with an embedded structure, the capacitance of the electrode pad region can be reduced without compromising the efficiency of the process flow. As a result, the modulation bandwidth can be broadened.
[0029] Embodiment 5 Figure 15 is a cross-sectional view showing an optoelectronic device according to Embodiment 5. While the optical device 2 of Embodiment 1 had a high mesa structure, the optical device 2 of this embodiment has a ridge structure. The optical device 2 has an absorption layer 6, a p-InP cladding layer 7, and a p-InP layer 8 stacked in order on a semiconductor substrate 1. The absorption layer 6 remains over the entire substrate, and only the p-InP layer 8 forms a ridge. Even when the optical device 2 has a ridge structure in this way, the capacitance of the electrode pad area can be reduced without reducing the efficiency of the process flow. In addition, since the first groove 11 is formed in the p-InP layer 8, the thickness of the insulating structure 16 is limited to the thickness of the p-InP layer 8.
[0030] 1. Semiconductor substrate, 2. Optical device, 3. Semiconductor layer, 11. First groove, 12. First insulating film, 14. Second groove, 15. Second insulating film, 16. Insulating structure, 19. Electrode pad
Claims
1. A method for manufacturing an optical semiconductor device, comprising the steps of: forming an optical device on a semiconductor substrate; forming a semiconductor layer on the side of the optical device on the semiconductor substrate; etching the semiconductor layer to form a plurality of first grooves; forming a first insulating film to cover the optical device and fill the first grooves; exposing the upper surface of the semiconductor layer from the first insulating film; etching away the exposed semiconductor layer to form a second groove; forming a second insulating film on the first insulating film to fill the second grooves; and forming an electrode pad connected to the optical device on an insulating structure composed of the first insulating film embedded in the first grooves and the second insulating film embedded in the second grooves.
2. The method for manufacturing an optical semiconductor device according to claim 1, characterized in that the first insulating film is formed on the side surface of the first groove, and the width of the first groove is 2 times or less the thickness of the first insulating film.
3. The method for manufacturing an optical semiconductor device according to claim 1, characterized in that the first insulating film is formed on the side surface of the first groove, and the width of the first groove is less than or equal to twice the sum of the thickness of the first insulating film and the thickness of the second insulating film.
4. The method for manufacturing an optical semiconductor device according to claim 1 or 2, characterized in that the second insulating film is formed on the side surface of the second groove, and the width of the second groove is 2 times or less the thickness of the second insulating film.
5. The method for manufacturing an optical semiconductor device according to any one of claims 1 to 4, characterized in that the electrode pad extends to the upper surface of the optical device without dropping down from the height of the insulating structure.
6. The method for manufacturing an optical semiconductor device according to any one of claims 1 to 5, characterized in that the optical device is an optical modulator.
7. The method for manufacturing an optical semiconductor device according to any one of claims 1 to 5, characterized in that the optical device is a directly modulated laser.
8. The method for manufacturing an optoelectronic device according to any one of claims 1 to 7, characterized in that the optical device has a high mesa structure.
9. The method for manufacturing an optical semiconductor device according to any one of claims 1 to 7, characterized in that the optical device has an embedded structure.
10. The method for manufacturing an optoelectronic semiconductor device according to any one of claims 1 to 7, characterized in that the optical device has a ridge structure.